Heat insulation pipeline joint coating structure and construction technology thereof

By adopting a double-layer outer cover structure and a waterproof cap at the insulated pipe fixing port, the problems of sealing and outer cover integrity of the insulated pipe are solved, and the sealing and waterproof performance of the insulated pipe are significantly improved. Ensure long-term stable operation.

CN119042449APending Publication Date: 2024-11-29CHINA PETROLEUM PIPELINE RES INST CO LTD +3
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202310617635.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-29
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

The sealing failure at the replenishment of domestic insulated pipes leads to water inlet and rapid corrosion, threatening the safety of the operation of insulated pipes. Traditional construction technology reduces the integrity of the outer cover layer and the sealing of the insulated layer.

Method used

A double-layer outer protective layer structure is adopted, wherein the first outer protective layer is a phenolic resin board or an epoxy resin board, which is combined with the thermal insulation layer as a foaming template, and the second outer protective layer is a heat shrink belt or an electric heat melt sleeve, through Flexible glue seal ensures the integrity of the outer cover, and a patch tape and waterproof cap are provided between the anti-corrosion layer and the thermal insulation layer to enhance sealing.

Benefits of technology

It improves the sealing and waterproof performance of the insulated pipe fixing ports, ensures the integrity of the outer cover, extends the service life of the insulated pipe, and enhances the reliability of the insulated pipe.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119042449A_ABST
    Figure CN119042449A_ABST
Patent Text Reader

Abstract

The invention provides a heat insulation pipeline joint coating structure and a construction technology thereof.The joint coating structure is arranged in a pipeline joint coating area and sequentially comprises an anti-corrosion layer, a heat insulation layer and an outer protection layer from the outer wall of a pipeline to the outside, and the joint coating structure is characterized in that the heat insulation layer is made of on-site foaming materials, and the outer protection layer comprises a first outer protection layer and a second outer protection layer; the first outer protection layer has waterproof performance and serves as a foaming template of the heat insulation layer; the first outer protection layer is a phenolic resin plate or an epoxy resin plate, the first outer protection layer is bonded with the lap joint area of the pipe body outer protection layer and the lap joint area of the first outer protection layer through flexible glue, and the second outer protection layer is a thermal contraction belt or an electric hot melting sleeve; the joint coating structure is structurally characterized in that a phenolic aldehyde / epoxy resin plate is adopted as a foaming mold and a first outer protection layer, a heat shrinkage belt or an electric hot melting sleeve is adopted as a second outer protection layer, the phenolic aldehyde / epoxy resin plate does not need to be detached in the construction process, construction of the second outer protection layer is facilitated, and the waterproof performance of a heat insulation layer is improved; and meanwhile, the layer also has good sealing performance. In addition, holes do not need to be formed in the surface of the hot melting sleeve and sealed, it is guaranteed that the thermal contraction band or the electric hot melting sleeve integrally and completely guarantees the completeness of an outer protective layer of the heat insulation pipeline, the sealing performance of the repaired mouth of the heat insulation pipeline is enhanced, and the reliability of the repaired mouth of the heat insulation pipeline is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of general corrosion protection and heat insulation pipeline system of metal materials, and specifically relates to a heat insulation pipeline patching structure and a construction process thereof. Background Art

[0002] The quality of the patching of insulated pipes is a key link to ensure the long-term stable operation of the pipeline. The patching of domestic land insulated pipes is generally treated with a similar structure of anti-corrosion layer (epoxy or heat shrink tape) + insulation layer (on-site foaming or insulation tile) + outer sheath (hot melt sleeve or heat shrink tape). Common technologies for patching on-site insulation layers include prefabricated block technology and injection technology. Prefabricated blocks have joints and cannot be integrated with the anti-corrosion layer and outer sheath. Injection molding requires injection holes in the outer sheath, which reduces the integrity of the outer sheath. When foaming with a special mold, the surface of the insulation layer is often damaged. Nearly three decades of engineering applications and field surveys have shown that in the inspection of domestic insulated pipes, a large number of seal failures at the patching points were found, causing water to enter the patching points of the insulated pipes. After water ingress, the insulated pipes showed a dangerous condition of rapid corrosion at the patching points. The depth of the corrosion pits of many projects exceeded 50% of the pipe wall thickness within two or three years of commissioning, and the resulting pipe body corrosion has seriously threatened the safe operation of the insulated pipes.

[0003] The purpose of the present invention is to provide a thermal insulation pipe patching structure and a construction process thereof, so as to ensure the integrity of the thermal insulation pipe outer sheath, enhance the sealing performance of the thermal insulation pipe patching, and improve the reliability of the thermal insulation pipe patching. Summary of the invention

[0004] The heat-insulating pipe patching structure provided by the present invention is arranged in the pipe patching area, and includes three layers of structure, namely, anti-corrosion layer, heat-insulating layer and outer protective layer, from the outer wall of the pipe outward, and is characterized in that the heat-insulating layer is a foaming material in situ, and the outer protective layer includes a first outer protective layer and a second outer protective layer, and the first outer protective layer has waterproof performance and sealing performance and serves as a foaming template for the heat-insulating layer. The first outer protective layer and the outer protective layer overlap area of ​​the pipe body, and the first outer protective layer overlap area are sealed and bonded by flexible double-sided adhesive.

[0005] Furthermore, the foaming material is polyurethane foam.

[0006] Furthermore, the first outer protective layer is a phenolic resin board or an epoxy resin board.

[0007] Furthermore, the second outer protective layer is a heat shrinkable tape or an electric heat-melting sleeve.

[0008] Furthermore, a patching strip and a waterproof cap are provided between the anti-corrosion layer and the heat-insulating layer. The waterproof cap is connected to the patching strip and extends outward to the outside of the outer protective layer.

[0009] Furthermore, the second outer protective layer is a heat shrinkable tape or an electric heat-melting sleeve, and the electric heat-melting sleeve does not need to be opened and has integrity.

[0010] Furthermore, the first outer protective layer is fixedly wrapped around the pipe joint area by using a flexible double-sided adhesive.

[0011] The present invention also provides a construction process of an insulating pipe patching structure, which is used to implement the patching structure of the present invention, and comprises the following steps:

[0012] S1. Carry out pipeline anti-corrosion treatment on the pipeline joint area according to the design documents or relevant construction standards and specifications, and do a good job in coating and testing the anti-corrosion layer;

[0013] S2. Stick the flexible double-sided adhesive tape on the three sides of the first outer sheath for fixing, or stick the flexible double-sided adhesive tape on the overlapping area of ​​the pipe body protective layer and the overlapping area of ​​the first outer sheath;

[0014] S3. Wrap the first outer sheath around the patching area of ​​the pipe. During the operation, ensure that the adhesive layer of the phenolic / epoxy resin board and the overlapped areas on both sides of the patching area of ​​the pipe and the overlapped areas at the head and tail of the phenolic / epoxy resin board itself are tightly attached.

[0015] S4. Drill holes at appropriate locations on the first outer sheath as polyurethane foam injection holes and vents; then conduct a sealing test on the sealed pipe patching area; the test pressure is 0.02MPa. After maintaining the pressure for 2 minutes, apply soapy water on the sealing area. No bubbles should be generated.

[0016] S5. Inject the polyurethane foam material into the pipe patching area from the injection port of the first outer sheath. The polyurethane foam plastic should fill the entire joint without any gaps. After foaming, a small amount of foam should overflow from the foaming hole;

[0017] S6. After foaming, the openings of the first outer sheath are sealed with a viscoelastic tape;

[0018] S7. Install the heat shrink tape or electric heat-melting sleeve in the pipe patching area in accordance with relevant construction standards or specifications.

[0019] Furthermore, the first outer protective layer is a phenolic resin board or an epoxy resin board, which is rectangular and wrapped around the insulated pipe with an overlap of not less than 100 mm. The width of the resin board meets the patching width and overlaps with the insulated pipes on both sides by not less than 50 mm.

[0020] Furthermore, the number of holes drilled on the phenolic resin board or epoxy resin board is 1 to

[0021] 2.

[0022] The insulated pipe patching structure and its construction process provided by the present invention create a double-layer structure of the outer protective layer of the insulated pipe patching. The outer protective layer of the double-layer structure avoids the surface opening and sealing of the hot melt sleeve of the traditional outer protective layer structure, ensuring the overall integrity of the electric hot melt sleeve. For the insulated pipe patching structure, a waterproof layer and an outer protective layer are added, which can effectively improve the sealing of the insulated pipe patching and ensure the long-term stable operation of the insulated pipe. Due to the introduction of the first protective layer, it is more convenient for on-site construction and improves the waterproof performance of the patching. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 It is a cross-sectional view of a thermal insulation pipe patching structure of the present invention.

[0024] Figure 2 The present invention is a schematic diagram of a double-sided adhesive used to fix the first outer protective layer of the phenolic / epoxy resin board of a thermal insulation pipe patching structure.

[0025] In the figure, 1-steel pipe wall, 2-anti-corrosion layer, 3-insulating layer of pipeline body, 4-outer sheath of pipeline body, 5-waterproof cap, 6-patching tape, 7-insulating layer of patching area, 8-phenolic resin board or epoxy resin board, 9-heat shrinkable tape or electric hot melt sleeve, 10-double-sided tape for fixing. DETAILED DESCRIPTION

[0026] In order to enable those skilled in the art to better understand the technical solution of the present disclosure, the present disclosure is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.

[0027] Example 1

[0028] This example is a thermal insulation pipe patching structure.

[0029] The patching structure is arranged in the pipeline patching area, and includes three layers of structure, namely, an anti-corrosion layer, an insulating layer and an outer protective layer, from the outer wall of the pipeline to the outside. It is characterized in that the insulating layer is a field foaming material, and the outer protective layer includes a first outer protective layer and a second outer protective layer. The first outer protective layer has waterproof properties and serves as a foaming template for the insulating layer.

[0030] Furthermore, the foaming material is polyurethane foam.

[0031] Furthermore, the first outer protective layer is a phenolic resin board or an epoxy resin board.

[0032] Furthermore, the second outer protective layer is a heat shrinkable tape or an electric heat-melting sleeve.

[0033] Furthermore, a patching strip and a waterproof cap are provided between the anti-corrosion layer and the thermal insulation layer, and the waterproof cap is connected to the patching strip and extends outward to the outside of the outer protective layer.

[0034] Furthermore, the first outer protective layer is wrapped around the pipe patching area by using double-sided adhesive for fixing.

[0035] The heat-insulating pipe joint patching structure is a three-layer structure of anti-corrosion layer + insulation layer + outer protective layer. The anti-corrosion layer is a common anti-corrosion structure in the market, which can meet the requirements of design documents or relevant construction standards or specifications. The insulation layer is a polyurethane foam layer foamed on site. The outer protective layer adopts a double-layer structure of phenolic / epoxy resin board + heat shrink tape (or electric hot melt sleeve). The cross-sectional view of the heat-insulating pipe joint patching structure is as follows: Figure 1 As shown, its structural feature is that phenolic / epoxy resin board is used as the foaming mold and the first outer protective layer, and heat shrinkable tape or electric hot melt sleeve is used as the second outer protective layer. During the construction process, the phenolic / epoxy resin board does not need to be disassembled, which is convenient for the construction of the second outer protective layer and improves the waterproof performance of the insulation layer. In addition, it is not necessary to open and seal holes on the surface of the hot melt sleeve, ensuring the overall integrity of the heat shrinkable tape or electric hot melt sleeve.

[0036] Example 2

[0037] This example is a test installation process method. Environment: temperature 20.0℃; relative humidity 83.2%, dew point temperature 16.9℃; pipeline diameter is Φ219.1mm, pipeline main body anti-corrosion insulation layer structure: anti-corrosion layer is double-layer FBE, insulation layer is polyurethane foam, outer sheath is PE.

[0038] The specific steps for the construction of thermal insulation pipe patching are as follows:

[0039] S1. Carry out pipeline anti-corrosion treatment on the pipeline joint area according to the design documents, and carry out surface inspection and treatment, anti-corrosion coating, and anti-corrosion layer testing in the joint area;

[0040] S2. Stick the three sides (two long sides and one short side) of the epoxy resin board with double-sided tape;

[0041] S3. Wrap the epoxy resin sheet around the pipe patching area. During the operation, ensure that the epoxy resin sheet and the overlapped areas on both sides of the pipe patching area as well as the overlapped areas at the head and tail of the epoxy resin sheet are tightly attached.

[0042] S4. Drill 1-2 holes at appropriate locations on the epoxy resin board as polyurethane foam injection holes and vent holes. Then conduct a sealing test on the sealed pipe patching area. The test pressure is 0.02MPa. After maintaining the pressure for 2 minutes, apply soapy water to the sealed area and no bubbles are generated.

[0043] S5. Use mechanical high-pressure foaming to inject the polyurethane foam material into the pipe patching area from the injection port of the epoxy resin board. The polyurethane foam plastic should fill the entire joint without any gaps. Ensure that a small amount of foam overflows from the foaming hole after foaming;

[0044] S6. After foaming, the openings of the epoxy resin board are sealed with a viscoelastic tape;

[0045] S7. Install the heat shrink tape in the pipe patching area according to relevant construction standards.

[0046] It is to be understood that the above embodiments are merely exemplary embodiments used to illustrate the principles of the present disclosure, but the present disclosure is not limited thereto. For those of ordinary skill in the art, various modifications and improvements can be made without departing from the spirit and substance of the present disclosure, and these modifications and improvements are also considered to be within the scope of protection of the present disclosure.

Claims

1. An insulated pipe joint patching structure, which is arranged in the pipe joint patching area and includes three layers of structure, namely, an anti-corrosion layer, an insulating layer and an outer protective layer, from the outer wall of the pipe outward, characterized in that: The insulation layer is a field foamed material, and the outer protective layer includes a first outer protective layer and a second outer protective layer. The first outer protective layer has waterproof properties and serves as a foaming template for the insulation layer. The first outer protective layer is sealed and bonded to the overlapping area with the outer protective layer of the pipe body and the overlapping area with the first outer protective layer by using flexible double-sided adhesive.

2. The thermal insulation pipe patching structure according to claim 1, characterized in that: The foaming material is polyurethane foam.

3. The thermal insulation pipe patching structure according to claim 1, characterized in that: The first outer protective layer is a phenolic resin board or an epoxy resin board.

4. The thermal insulation pipe patching structure according to claim 1, characterized in that: The second outer protective layer is a heat shrinkable tape or an electric heat-melting sleeve, and the electric heat-melting sleeve does not need to be opened and has integrity.

5. The thermal insulation pipe patching structure according to claim 1, characterized in that: The first outer protective layer is wound around the pipe patching area by double-sided flexible adhesive.

6. A construction process for a patching structure of an insulated pipe, which is used to implement the patching structure construction process according to any one of claims 1 to 5, comprising the following steps: S1. Carry out pipeline anti-corrosion treatment on the pipeline joint area according to the design documents or relevant construction standards and specifications, and do a good job in coating and testing the anti-corrosion layer; S2. Stick the flexible double-sided adhesive tape on the three sides of the first outer sheath for fixing, or stick the flexible double-sided adhesive tape on the overlapping area of ​​the pipe body protective layer and the overlapping area of ​​the first outer sheath; S3. Wrap the first outer sheath around the patching area of ​​the pipe. During the operation, ensure that the adhesive layer of the phenolic / epoxy resin board and the overlapped areas on both sides of the patching area of ​​the pipe and the overlapped areas at the head and tail of the phenolic / epoxy resin board itself are tightly attached. S4. Drill holes at appropriate locations on the first outer sheath as polyurethane foam injection holes and vents; then conduct a sealing test on the sealed pipe patching area; the test pressure is 0.02MPa, and after maintaining the pressure for 2 minutes, apply soapy water to the sealing area, and no bubbles should be generated; S5. Inject the polyurethane foam material into the pipe patching area from the injection port of the first outer sheath. The polyurethane foam plastic should fill the entire joint without any gaps. After foaming, a small amount of foam should overflow from the foaming hole; S6. After foaming, the openings of the first outer sheath are sealed with a viscoelastic tape; S7. Install the heat shrink tape or electric heat-melting sleeve in the pipe patching area in accordance with relevant construction standards or specifications.

7. The construction process of the thermal insulation pipe patching structure according to claim 6 is characterized in that: The first outer protective layer is a phenolic resin board or an epoxy resin board, which is rectangular and wrapped around the insulated pipe with an overlap of no less than 100mm. The width of the resin board meets the patch width and overlaps with the insulated pipes on both sides by no less than 50mm.

8. The construction process of the thermal insulation pipe patching structure according to claim 6 is characterized in that: The number of holes drilled on the phenolic resin board or epoxy resin board is 1 to 2.

Citation Information

Patent Citations

  • Waterproof type electric hot-melting insulation joint

    CN105953015A

  • A anticorrosive insulation construction for burying ground hot oil line repaired mouth

    CN207762439U

  • Pipeline joint coating structure

    CN217843159U

  • Polyurethane foaming thermal-insulative pipe with polyurea coating as mouth

    CN2818982Y

  • Anticorrosive coating structure for site welded part

    JP2006194368A