Biodegradable flexible wireless implantable intracerebral heating device and preparation method thereof

By preparing a layered biodegradable material, a wireless implantable intracerebral heating device was fabricated, which solved the problems of needing a second surgery to remove the implanted device and mechanical mismatch. The device achieved biodegradability, flexibility and tissue compatibility, and has precise temperature control and degradation cycle regulation, reducing mechanical damage and infection risks.

CN121944254APending Publication Date: 2026-05-01NANJING UNIV OF POSTS & TELECOMM
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202610193411.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-02-10
Publication Date
2026-05-01

AI Technical Summary

Technical Problem

Existing brain implants require a second surgery for removal and suffer from mechanical mismatch, and traditional devices also have issues with infection risks and insufficient flexibility.

Method used

A flexible, wireless implantable intracerebral heating device is fabricated using layered biodegradable materials, including silk fibroin nanofiber membranes, polylactic acid encapsulation layers, and biodegradable zinc heating layers, through electrospinning and spin coating techniques. The device features a porous structure, wireless heating function, and is driven by an external magnetic field.

Benefits of technology

It achieves biodegradability, flexibility, and tissue compatibility in wireless implantable brain heating devices, avoiding secondary surgery, and features precise temperature control and degradation cycle regulation, reducing mechanical damage and infection risks.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN121944254A_ABST
    Figure CN121944254A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of biomedical engineering and implantable medical instruments, in particular to a biodegradable flexible wireless implantable intracerebral heating device and a preparation method thereof. The device is of a layered structure and sequentially comprises a porous bioprotein substrate layer and a silk protein nanofiber membrane prepared by adopting an electrostatic spinning process from bottom to top, and the crystallinity and degradation rate of the silk protein nanofiber membrane are adjusted through ethanol annealing treatment. And the lower hydrophobic encapsulation layer is positioned on the substrate layer, is made of a biodegradable hydrophobic polymer, preferably polylactic acid (PLA), and is used for isolating biological fluid. And the wireless heating layer is positioned on the lower hydrophobic packaging layer and is formed by depositing a biodegradable metal material, preferably zinc (Zn). And the upper hydrophobic packaging layer covers the wireless heating layer and forms a sealed package for the heating layer together with the lower layer, so that the metal layer is prevented from being corroded by the body fluid too early. The device aims at solving the problems that an existing intracerebral implantation device needs to be taken out through a secondary operation and mechanical mismatch is caused.
Need to check novelty before this filing date? Find Prior Art

Description

A biodegradable flexible wireless implantable intracerebral heating device and its preparation method Technical Field

[0001] This invention relates to the fields of biomedical engineering and implantable medical devices, and in particular to a biodegradable flexible wireless implantable intracerebral heating device and its preparation method. Background Technology

[0002] Treatment of brain diseases (such as brain tumors and neurological disorders) often requires precise local intervention. Traditional physical therapy methods (such as hyperthermia) typically rely on wired implanted probes or large external devices. Wired devices pose a risk of infection from percutaneous leads and restrict patient movement; while traditional rigid implants suffer from severe mechanical mismatch with soft brain tissue, easily causing brain tissue damage or gliosis. Furthermore, existing implantable electronic devices often use non-degradable materials (such as gold, copper, and polyimide), requiring secondary surgery for removal after treatment, increasing medical costs and the risk of brain damage to patients. In recent years, the development of transient electronics technology has provided new ideas for implantable medicine. However, developing a heating device that possesses excellent flexibility and tissue fit, achieves stable wireless control, and ultimately completely degrades into non-toxic byproducts, specifically for the unique microenvironment of the brain, remains a pressing technological challenge. Summary of the Invention

[0003] The technical problem to be solved by the present invention is to provide a biodegradable, flexible, wireless implantable intracranial heating device, which aims to solve the problems of existing intracranial implantable devices requiring secondary surgery for removal and mechanical mismatch.

[0004] To achieve the aforementioned objective, the technical solution of this invention is as follows: a biodegradable flexible wireless implantable intracerebral heating device and its preparation method. This biodegradable flexible wireless implantable intracerebral heating device has a layered structure, consisting of, from bottom to top: a porous biological protein base layer: a silk fibroin nanofiber membrane prepared by electrospinning, which is then annealed with ethanol to adjust its crystallinity and degradation rate. This layer has a porous structure, good air permeability, and can form a conformal fit with the surface of moist brain tissue through water-driven processes.

[0005] Lower hydrophobic encapsulation layer: Located above the base layer, it is made of a biodegradable hydrophobic polymer, preferably polylactic acid (PLA), and is used to isolate biological fluids.

[0006] Wireless heating layer: Located above the lower hydrophobic encapsulation layer, it is formed by the deposition of a biodegradable metallic material, preferably zinc (Zn). This layer is designed as a specific planar coil or disk structure, which generates heat by electromagnetic induction under an external alternating magnetic field.

[0007] Upper hydrophobic encapsulation layer: Covering the wireless heating layer, the material is the same as the lower hydrophobic encapsulation layer. Together with the lower layer, they form a sealed enclosure for the heating layer, preventing body fluids from corroding the metal layer prematurely.

[0008] Preferably, the total thickness of the device is less than 50 μm, and it has excellent flexibility.

[0009] Preferably, the fiber diameter of the silk fibroin base layer is distributed between 300-400 nm, which has good water vapor permeability.

[0010] Preferably, the zinc thickness of the wireless heating layer is 1-10 μm, and the working life and degradation cycle of the control device can be controlled by adjusting the thickness.

[0011] Preferably, the operating life of the device can be controlled from several weeks to several months by adjusting the thickness of the encapsulation layer and the metal layer.

[0012] Preferably, the preparation method of the above-mentioned biodegradable flexible wireless implantable intrabrain heating device includes the following steps: 1) First, a 7% PLA chloroform solution is spin-coated onto a silicon substrate at 300 rpm for 10 s, followed by spin-coating at 800 rpm for 50 s, and then dried at room temperature for 12 h to completely evaporate the solvent to form a first encapsulation layer; 2) Next, a 3 nm chromium adhesion layer and a 3 μm zinc metal layer are sequentially deposited using thermal evaporation technology with the assistance of a mask to construct a patterned wireless heating circuit. Then, a 5% PLA solution is spin-coated on top of the heating layer at 300 rpm for 30 s to form a second encapsulation layer, achieving full encapsulation protection of the zinc layer; 3) Finally, the above-mentioned PLA-Zn-PLA functional layer component is completely peeled off and attached to a silk fibroin substrate using assisted transfer technology. After laser cutting and shaping, a biodegradable flexible wireless implantable intrabrain heating device is obtained.

[0013] The beneficial effects of the present invention are reflected in: (1) The flexible wireless implantable intracerebral heating device provided by the present invention is biodegradable (no need for secondary surgery): all the constituent materials (silk protein, polylactic acid, zinc) can be completely degraded into non-toxic small molecule products such as amino acids, lactic acid, and zinc ions under physiological conditions, and are metabolized or excreted by the body, thus completely eliminating the pain and risk of secondary surgery to remove it.

[0014] (2) The flexible wireless implantable intracerebral heating device provided by the present invention has excellent flexibility and tissue compatibility: the device is thin and light (about 38 μm), which can adapt to the complex curvature of the brain surface and vascular pulsation, reducing mechanical damage and foreign body reaction to fragile brain tissue.

[0015] (3) The flexible wireless implantable intracerebral heating device provided by the present invention can be wirelessly driven and precisely temperature controlled: it is powered wirelessly by an external radio frequency magnetic field, avoiding the risk of infection caused by percutaneous wires. The zinc heating layer responds quickly to the magnetic field, and precise in vivo temperature control (such as the range of 37°C-45°C) can be achieved by adjusting the distance of the external coil or the size of the device.

[0016] (4) The flexible wireless implantable intracerebral heating device provided by the present invention can regulate the degradation cycle: by adjusting the ethanol annealing time and the PLA encapsulation layer thickness, the stable working window of the device in the body (such as more than 15 days) can be preset to meet the needs of different treatment courses. Attached Figure Description

[0017] Figure 1 shows a photograph of the device of the present invention and a diagram illustrating its flexible bending; Figure 2 shows the biodegradation process of the main materials (silk, PLA, zinc) of the device of the present invention; Figure 3 shows a photograph of the device of the present invention undergoing accelerated degradation in vitro under a simulated environment of 60°C PBS buffer; Figure 4 shows the temperature response characteristics of the device of the present invention with different diameters (10, 15, and 25 mm) at different axial working distances; Figure 5 shows the temperature stability test curve of the device of the present invention after multiple on / off cycles at different distances; Figure 6 shows a comparison of the heating performance of the device of the present invention after undergoing 0, 500, and 1000 mechanical bends at a bending radius of 500 μm; Figure 7 shows a comparison of TTC-stained sections of brain tissue after the device of the present invention was implanted into the brain of a mouse. Detailed Implementation

[0018] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of the present invention, and not all of them. Unless otherwise specified, the embodiments and features in the embodiments of this application can be combined with each other. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0019] As shown in Figures 1-7, the present invention provides a biodegradable flexible wireless implantable intracerebral heating device and its preparation method.

[0020] Example 1: This example provides a method for preparing silk protein spinning solution and nanofiber base membrane.

[0021] First, silkworm silk was boiled in a 0.02 M Na₂CO₃ aqueous solution at 100℃ for 120 min to remove sericin. After being repeatedly washed four times with deionized water, it was dried and then dissolved in a 9.3 M LiBr solution at 60℃ with stirring for 4 h. The resulting solution was dialyzed in ultrapure water for 48 h with water changes every 8 h. After centrifugation twice at 18000 rpm (20 min each time) to remove impurities, it was freeze-dried to obtain regenerated silk fibroin sponge. A 5 wt% spinning solution was prepared from the freeze-dried silk fibroin and electrospun under a positive voltage of +10 kV and a negative voltage of -3 kV. The resulting nanofiber membrane was annealed with ethanol for 120 s to induce β-sheet formation, thereby reducing water solubility and improving structural stability, resulting in a flexible base membrane with excellent air permeability and biocompatibility.

[0022] Example 2: This example provides a micro / nano fabrication and device integration method for a polylactic acid (PLA) encapsulation layer and a zinc heating circuit. First, a 7% PLA chloroform solution is spin-coated onto a silicon substrate (parameters: 300 rpm for 10 s, followed by 800 rpm for 50 s), and dried at room temperature for 12 h to completely evaporate the solvent, forming the first encapsulation layer. Next, a 3 nm chromium adhesion layer and a 3 μm zinc metal layer are sequentially deposited using thermal evaporation technology with mask assistance to construct a patterned wireless heating circuit. Subsequently, a 5% PLA solution is spin-coated above the heating layer (parameters: 300 rpm for 30 s) to form the second encapsulation layer, achieving full encapsulation protection of the zinc layer. Finally, using assisted transfer technology, the PLA-Zn-PLA functional layer component is completely peeled off and bonded to the ethanol-annealed silk fibroin substrate prepared in Example 1. Laser cutting then shapes the substrate to obtain a biodegradable, flexible, wireless implantable intracerebral heating device.

[0023] Experiment Example 1: In Vitro Biodegradability Evaluation. This experiment demonstrates the degradation of the device in an in vitro simulated body fluid environment. To predict the long-term degradation behavior of the device in vivo, an accelerated in vitro aging test was designed based on the Arrhenius equation. The device sample was completely immersed in phosphate-buffered saline (PBS, pH 7.4) at 60°C, using high temperature to accelerate hydrolysis and corrosion reactions, simulating the long-term degradation process under physiological conditions at 37°C. The experiment lasted for 14 days, and morphological evolution was recorded on days 1, 8, 10, 12, and 14. The results, as shown in Figure 3, indicate that the device structure was intact in the initial stage; from day 8 onwards, significant corrosion and fracture of the metal mesh appeared; and by day 14, the functional layer structure had completely disintegrated and disappeared. This result not only verifies the excellent biodegradability of the device, but also, according to the Arrhenius equation, this rate ensures that the device can maintain a sufficient therapeutic window at physiological body temperature, followed by safe degradation and excretion, meeting the requirements for implantable medical applications.

[0024] Experiment 2: Wireless Heating Performance and Stability Testing of the Device. Temperature response curves are shown for different working distances (0.5-5 cm) and different device diameters (10, 15, 25 mm). Three sets of devices with diameters of 10, 15, and 25 mm were fabricated and placed above a wireless transmitter. A precision displacement stage was used to strictly control the gradient change of the axial working distance within the range of 0.5 to 5 cm. Under constant power excitation, a high-precision infrared thermal imager was used to record the evolution of the device surface temperature in real time, obtaining temperature response curves for different sizes and distances. The results, shown in Figure 4, indicate that the device saturation temperature is positively correlated with the diameter and decreases nonlinearly with increasing distance.

[0025] The temperature stability under multiple switching cycles (ON / OFF) was then demonstrated by controlling the transmitter to perform multiple cycles of ON / OFF switching excitation. The results, shown in Figure 5, indicate that the device exhibits a rapid thermal response at the millisecond level and a highly consistent heating-cooling trajectory over multiple consecutive cycles, with no significant drift in peak temperature. This confirms that the device possesses excellent thermal stability and tolerance in wireless control mode.

[0026] Experiment 3: Flexibility and Heating Capability Testing under Bending Conditions. This experiment demonstrates the heating stability of the device under large-scale, multiple bending cycles. The device was fixed in a precision mechanical bending testing system with a bending radius of 500 μm and a maximum bending angle of approximately 63°. 0, 500, and 1000 repeated bending cycles were performed. After completing the specified number of cycles, the device was placed above a wireless transmitting coil, and its saturation temperature change was measured within an axial distance range of 0.5 to 5 cm. The test results are shown in Figure 6. With increasing working distance, the temperature response of each group of samples exhibited a non-linear decay. Crucially, compared to the initial state, after 1000 high-intensity bends, the device's temperature response curve showed only a very small deviation, indicating extremely high overall heating performance retention. The results confirm that the internal conductive network and functional materials of the device are tightly integrated, possessing excellent flexibility and mechanical tolerance, sufficient to meet the repeated deformation requirements of practical applications.

[0027] Experiment Example 4: This experiment demonstrates the TTC staining results after device implantation in the mouse brain, proving that the implantation does not cause cerebral ischemia, necrosis, or significant inflammatory response. Mice were randomly divided into the implanted device group (AIMS) and the blank control group (Blank). Fourteen days after surgery, mice were sacrificed, and the entire brain tissue was rapidly dissected and cryo-hardened. Uniformly thick serial sections were prepared along the coronal plane. The sections were completely immersed in 2% TTC (2,3,5-triphenyltetrazolium chloride) phosphate buffer and incubated at 37°C in the dark for 15 to 20 minutes. Mitochondrial dehydrogenase activity reduced the normal tissue to red, followed by fixation with 4% paraformaldehyde and imaging analysis.

[0028] The experimental results, as shown in Figure 7, indicate that the brain slices of the blank control group were uniformly dark red; the tissues surrounding and distal to the implantation site (marked by the dotted line) in the implantation group were bright red, and no pale areas representing ischemic infarction or tissue necrosis were observed. These results confirm that the device has excellent biocompatibility, and the implantation procedure did not induce focal ischemic or necrotic damage to the brain tissue.

[0029] This invention verifies the feasibility of constructing wireless implantable hyperthermia devices based on biodegradable materials. Experimental results show that, through the synergistic design of the silk fibroin substrate and PLA encapsulation layer, the device exhibits excellent electrochemical stability and mechanical flexibility in physiological environments, while achieving complete degradation and non-toxic metabolism within a preset period. This technical solution effectively avoids the risk of secondary surgery and provides a safe and reliable engineered solution for long-term, precise hyperthermia of intracranial malignant tumors.

[0030] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the protection scope of the present invention.

Claims

1. A biodegradable flexible wireless implantable intracerebral heating device, comprising a porous biological protein base layer, a lower hydrophobic encapsulation layer, a wireless heating layer, and an upper hydrophobic encapsulation layer; wherein the porous biological protein base layer is used to form a conformal fit with the surface of brain tissue; the lower hydrophobic encapsulation layer is located on the porous biological protein base layer and is used to isolate biological fluids; the wireless heating layer is located on the lower hydrophobic encapsulation layer and generates heat through eddy currents generated by electromagnetic induction; the upper hydrophobic encapsulation layer covers the wireless heating layer and together with the lower layer constitutes a sealed enclosure for the heating layer.

2. The biodegradable flexible wireless implantable intracerebral heating device according to claim 1, characterized in that, The porous bioprotein substrate layer is a silk protein nanofiber membrane prepared by electrospinning.

3. The biodegradable flexible wireless implantable intracerebral heating device according to claim 2, characterized in that, The lower hydrophobic encapsulation layer and the upper hydrophobic encapsulation layer are made of the same material, which is a biodegradable hydrophobic polymer.

4. The biodegradable flexible wireless implantable intracerebral heating device according to claim 3, characterized in that, The biodegradable hydrophobic polymer is polylactic acid.

5. The biodegradable flexible wireless implantable intracerebral heating device according to claim 1, characterized in that, The total thickness of the porous biological protein base layer, the lower hydrophobic encapsulation layer, the wireless heating layer, and the upper hydrophobic encapsulation layer is less than 50 μm.

6. The biodegradable flexible wireless implantable intracerebral heating device according to claim 2, characterized in that, The fiber diameter of the silk protein base layer is 300-400 nm.

7. The biodegradable flexible wireless implantable intracerebral heating device according to claim 1, characterized in that, The wireless heating layer has a planar coil or disk structure and is formed by deposition of biodegradable metal materials.

8. The biodegradable flexible wireless implantable intracerebral heating device according to claim 1, characterized in that, The biodegradable metallic material is zinc, and the thickness of the zinc is 1-10 μm.

9. A biodegradable flexible wireless implantable intracerebral heating device according to claim 8, characterized in that, The device's operating life and degradation cycle are adjusted by its thickness, and the device's operating life can be controlled from several weeks to several months by adjusting the thickness of the encapsulation layer and the metal layer.

10. A method for preparing a biodegradable flexible wireless implantable intracerebral heating device according to any one of claims 1-9, characterized in that, Includes the following steps: 1) Silkworm silk was boiled in a 0.02 M Na2CO3 aqueous solution at 100℃ for 120 min to remove sericin. After being washed four times with deionized water, it was dried and then dissolved in a 9.3 M LiBr solution at 60℃ and stirred for 4 h. The resulting solution was dialyzed in ultrapure water for 48 h with water changes every 8 h. After centrifugation twice at 18000 rpm for 20 min each time to remove impurities, it was freeze-dried to obtain regenerated silk fibroin sponge. The regenerated silk fibroin sponge was used to prepare a 5 wt% spinning solution, and electrospinning was performed under a positive voltage of +10 kV and a negative voltage of -3 kV to obtain a nanofiber membrane. The obtained nanofiber membrane was annealed with ethanol for 120 s to induce β-sheet formation, resulting in a silk fibroin substrate. 2) First, a 7% PLA chloroform solution was spin-coated onto a silicon substrate at 300 rpm for 10 s, followed by spin-coating at 800 rpm for 50 s, and then dried at room temperature for 12 hours. h) The first encapsulation layer is formed by completely evaporating the solvent; 3) Then, a 3 nm chromium adhesion layer and a 3 μm zinc metal layer are sequentially deposited on the first encapsulation layer using mask thermal evaporation technology to construct a patterned wireless heating circuit. Subsequently, a 5% PLA solution is spin-coated on the heating layer at 300 rpm for 30 s to form the second encapsulation layer, and an integrated PLA-Zn-PLA functional layer component is obtained; 4) Finally, the PLA-Zn-PLA functional layer component is completely peeled off and attached to the silk protein substrate using assisted transfer technology. After laser cutting and shaping, a biodegradable flexible wireless implantable intracerebral heating device is obtained.