Light-emitting element
The light-emitting element addresses bonding issues in red-emitting VCSELs by using a bonding layer with specific materials and structures, enhancing bonding strength and reducing resistance to improve performance and yield.
Patent Information
- Application Number
- JP2023068757
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-19
- Publication Date
- 2024-10-31
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Red-emitting VCSEL elements face challenges in ensuring strong bonding between semiconductor layers, leading to decreased light-emitting performance due to insufficient bonding strength.
A light-emitting element with a bonding layer between semiconductor layers, composed of materials like metal, Si, or Ge, with specific optical and refractive properties, and a concave-convex structure to enhance bonding strength and reduce electrical resistance.
The solution improves bonding strength, reduces electrical resistance, and enhances temperature characteristics and output light performance by stabilizing the semiconductor layers, allowing for efficient laser oscillation and improved yield.
Smart Images

Figure 2024154745000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to light-emitting devices. [Background technology]
[0002] A vertical cavity surface emitting laser (VCSEL) is a type of semiconductor laser device that resonates light in a direction perpendicular to the substrate surface and emits laser light in the same direction. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2022-38492 A Summary of the Invention [Problem to be solved by the invention]
[0004] In recent years, research and development of VCEL elements that emit red light has been progressing. Red-emitting VCEL elements may have a heterojunction structure in which a semiconductor layer made of GaAs is directly bonded to a semiconductor layer made of a material different from GaAs. In VCEL elements with such a structure, it is difficult to ensure the bonding strength between the two semiconductor layers. Insufficient bonding of these semiconductor layers leads to a decrease in light-emitting performance.
[0005] The present disclosure provides a light-emitting element capable of suppressing deterioration in light-emitting performance. [Means for solving the problem]
[0006] An optical detection device according to one embodiment of the present disclosure includes a first semiconductor layer having a lens with a convex shape, a second semiconductor layer having an active layer and made of a material different from the first semiconductor layer, a first optical reflection layer having a concave mirror facing the lens, a second optical reflection layer facing the first optical reflection layer with the first semiconductor layer and the second semiconductor layer in between, and a bonding layer provided between the first semiconductor layer and the second semiconductor layer.
[0007] The material of the bonding layer may be a metal.
[0008] The material of the bonding layer may be Si or Ge.
[0009] The optical refractive index of the bonding layer may be higher than the optical refractive index of the first optical reflecting layer and lower than the optical refractive index of the second optical reflecting layer.
[0010] The bonding layer may have a first region facing the lens and the concave mirror, and a second region surrounding the first region, and the optical refractive index of the first region may be greater than the optical refractive index of the second region.
[0011] The bonding layer may have a first region facing the lens and the concave mirror, and a second region surrounding the first region, and the attenuation coefficient of the first region may be smaller than the attenuation coefficient of the second region.
[0012] The bonding layer may be an amorphous layer.
[0013] The bonding layer may have a first region facing the lens and the concave mirror, and a second region surrounding the first region, the first region being an amorphous region, and the second region being an oxidized region.
[0014] the light emitting element further includes an electrode electrically connected to the second semiconductor layer via the bonding layer; The bonding layer and the electrode may be integrated together.
[0015] The radius of curvature of the apex of the lens may be set to satisfy the relation d / ω≦4 between the aperture diameter d and the beam waist diameter ω.
[0016] The optical thickness of the bonding layer may be 0.1 to 50 times the oscillation wavelength λ0, and may satisfy k(λ0 / 4)(2r+1) [where r is an integer equal to or less than 100, and 0.9≦k≦1.1].
[0017] The least common multiple of the optical distance from the center of the bonding layer to the inner surface of the second light reflecting layer and the optical distance from the center of the bonding layer to the inner surface of the concave mirror may be within 10% of the oscillation wavelength / 4.
[0018] A cavity length between the first light reflecting layer and the second light reflecting layer may be at least 5 μm or more.
[0019] The difference in lattice constant between the material of the first semiconductor layer and the material of the second semiconductor layer may be 15% or more.
[0020] The energy gap of the first semiconductor layer may be at least 0.8 eV or more.
[0021] The first semiconductor layer may have a higher thermal conductivity than the second semiconductor layer.
[0022] the first light reflecting layer is formed of a laminate of two types of dielectric materials having different light refractive indices; The second light reflecting layer may be formed of a laminate of two types of semiconductors having different optical refractive indices.
[0023] The light emitting device may have a current confinement structure formed by an ion implantation region or a mesa structure.
[0024] The material of the active layer may be InGaN, AlGaN, InGaP, or AlGaInP.
[0025] A plurality of the light emitting elements may be arranged in a two-dimensional array. [Brief description of the drawings]
[0026] [Figure 1] 1 is a cross-sectional view showing a structure of a light-emitting element according to a first embodiment. [Diagram 2] 4 is a cross-sectional view illustrating a step of bonding a first semiconductor layer and a second semiconductor layer. FIG. [Diagram 3] FIG. 4 is a cross-sectional view showing a structure of a light-emitting element according to a modified example of the first embodiment. [Figure 4] FIG. 5 is a cross-sectional view showing the structure of a light-emitting element according to a second embodiment. [Diagram 5] FIG. 11 is a cross-sectional view showing the structure of a light-emitting element according to a third embodiment. [Figure 6] FIG. 11 is a cross-sectional view showing the structure of a light-emitting element according to a fourth embodiment. [Figure 7] FIG. 11 is a cross-sectional view showing the structure of a light-emitting element according to a fifth embodiment. [Figure 8] FIG. 13 is a cross-sectional view showing the structure of a light-emitting element according to a sixth embodiment. [Figure 9] FIG. 13 is a cross-sectional view showing the structure of a light-emitting element according to a seventh embodiment. [Figure 10] FIG. 13 is a cross-sectional view showing the structure of a light-emitting element according to an eighth embodiment. [Figure 11] FIG. 13 is a cross-sectional view showing the structure of a light-emitting element according to a ninth embodiment. [Figure 12] FIG. 23 is a cross-sectional view showing the structure of a light-emitting element according to a tenth embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0027] Hereinafter, an embodiment of the light-emitting device according to the present disclosure will be described with reference to the drawings. Hereinafter, an embodiment in which the light-emitting device is applied to a VCEL device will be described, but the light-emitting device is not limited to the VCEL device. The light-emitting device according to the present disclosure can also be applied to a light-emitting diode (LED) or a laser diode (LD) having a structure in which two semiconductor layers made of different materials are bonded. In addition, in the following embodiment, the main components of the VCEL device will be mainly described, but the VCEL device may have components and functions that are not shown or described. The following description does not exclude components and functions that are not shown or described.
[0028] (First embodiment) Fig. 1 is a cross-sectional view showing the structure of the light-emitting element according to the first embodiment. The light-emitting element 1 shown in Fig. 1 includes a first semiconductor layer 110, a second semiconductor layer 120, a first light reflecting layer 130, a second light reflecting layer 140, a bonding layer 150, an ion-implanted region 160, a first electrode 171, and a second electrode 172. In the following description, two mutually orthogonal in-plane directions are defined as the X direction and the Y direction. The out-of-plane direction orthogonal to the X direction and the Y direction is defined as the Z direction.
[0029] The first semiconductor layer 110 is formed using a material that transmits red light, such as GaN. However, the first semiconductor layer 110 may be made of a material that has an energy gap of at least 0.8 eV. The energy gap of the first semiconductor layer 110 is preferably 1.2 eV, and more preferably 1.7 eV.
[0030] Moreover, the first semiconductor layer 110 has a first main surface 111, a second main surface 112, and a lens 113. The first main surface 111 is a front surface of the first semiconductor layer 110. The second main surface 112 is a rear surface of the first semiconductor layer 110 facing the first main surface 111 in the Z direction. The lens 113 has a convex shape protruding from the second main surface 112. The radius of curvature (ROC) of the apex of the lens 113 is about 50 μm. The lens 113 can be formed, for example, by etching a GaN substrate using a resist as an etching mask.
[0031] The second semiconductor layer 120 is a layer that generates laser oscillation, and is laminated on the first semiconductor layer 110. The second semiconductor layer 120 is made of a different material from the first semiconductor layer 110, for example, GaAs. However, the second semiconductor layer 120 may be made of any material as long as the difference in lattice constant between the second semiconductor layer 120 and the first semiconductor layer 110 is 15% or more.
[0032] Moreover, the second semiconductor layer 120 has a first major surface 121, a second major surface 122, and an active layer 123. The first major surface 121 is a front surface of the second semiconductor layer 120. The second major surface 122 is a rear surface of the second semiconductor layer 120 facing the first major surface 121 in the Z direction. The second major surface 122 is bonded to the first major surface 111 of the first semiconductor layer 110 by a bonding layer 150.
[0033] The active layer 123 is formed on the first principal surface 121 side inside the second semiconductor layer 120. The active layer 123 emits and amplifies spontaneous emission light by carrier recombination. The material of the active layer 123 is, for example, InGaN, AlGaN, InGaP, or AlGaInP. Furthermore, the portion of the second semiconductor layer 120 other than the active layer 123 is, for example, GaAs.
[0034] The first light reflecting layer 130 is laminated on the second principal surface 112 side of the first semiconductor layer 110. The first light reflecting layer 130 functions as a DBR (Distributed Bragg Reflector) that reflects red light. The first light reflecting layer 130 has a structure in which a first layer 131 and a second layer 132 are alternately laminated in the Z direction. The optical refractive index of the first layer 131 is lower than that of the second layer 132. The material of the first layer 131 is, for example, Ti2O5. On the other hand, the material of the second layer 132 is, for example, SiO2. Note that the first light reflecting layer 130 is not limited to a laminate of Ti2O5 and SiO2, and may be a laminate of two types of dielectrics having different optical refractive indexes.
[0035] The first light reflecting layer 130 also has a concave mirror 133. The concave mirror 133 has a concave shape that faces the convex shape of the lenses 113 of the first semiconductor layer 110.
[0036] The second light reflecting layer 140 is laminated on the first major surface 121 side of the second semiconductor layer 120. Like the first light reflecting layer 130, the second light reflecting layer 140 also functions as a DBR that reflects red light. The second light reflecting layer 140 has a structure in which first layers 141 and second layers 142 are alternately laminated in the Z direction. The optical refractive index of the first layer 141 is lower than the optical refractive index of the second layer 142. The material of the first layer 141 is, for example, Al. 0.9 On the other hand, the material of the second layer 132 is, for example, Al 0.5 The second light reflecting layer 140 can be formed by epitaxially growing AlGaAs. 0.9 GaAs and Al 0.5 The layer is not limited to a laminate with GaAs, but may be a laminate of two types of semiconductors with different optical refractive indices.
[0037] The bonding layer 150 is provided between the first major surface 121 of the first semiconductor layer 110 and the second major surface 122 of the second semiconductor layer 120. The bonding layer 150 is a layer for strengthening the bonding between the first semiconductor layer 110 and the second semiconductor layer 120. The bonding layer 150 is, for example, a metal layer containing a metal such as Hf. It is desirable that the thickness t of the bonding layer 150 is 10 nm or less. In this embodiment, the bonding layer 150 is an Hf layer having a thickness t of about 5 nm. Here, the bonding process between the first semiconductor layer 110 and the second semiconductor layer 120 will be described with reference to FIG. 2.
[0038] 2 is a cross-sectional view for explaining a bonding process between the first semiconductor layer 110 and the second semiconductor layer 120. In this embodiment, first, a metal film 150a is formed on the first major surface 111 of the first semiconductor layer 110. The metal film 150a is, for example, a Hf film. The metal film 150a can be formed by, for example, sputtering or vapor deposition.
[0039] Next, a metal film 150b is formed on the second major surface 122 of the second semiconductor layer 120. The metal film 150b is a film formed of the same material as the metal film 150a. Therefore, the metal film 150b can be formed by sputtering or vapor deposition, similar to the metal film 150a. Note that the second light reflecting layer 140 and the ion implantation region 160 may already be formed on the first major surface 121 of the second semiconductor layer 120 before the metal film 150b is formed.
[0040] Finally, the metal film 150a and the metal film 150b are bonded together. As a result, the metal film 150a and the metal film 150b become the bonding layer 150. The bonding layer 150 bonds the first semiconductor layer 110 and the second semiconductor layer 120 together, as shown in FIG.
[0041] The ion implantation region 160 is an insulating region in which ions such as boron (B) are implanted in a part of the second light reflecting layer 140 and a part of the second semiconductor layer 120. The ion implantation region 160 is provided in an outer peripheral region surrounding the central region of each of the second light reflecting layer 140 and the second semiconductor layer 120. The current flowing through the second semiconductor layer 120 cannot pass through the ion implantation region 160 and is concentrated in the central region of the second semiconductor layer 120, which is a non-ion implantation region. This forms a current confinement structure.
[0042] The first electrode 171 is provided on the first semiconductor layer 110. The first electrode 171 includes a metal such as Ti, Pt, or Au. The first electrode 171 is electrically connected to an external circuit.
[0043] The second electrode 172 is provided on the second light reflecting layer 140. The material of the second electrode 172 is a transparent conductive material such as ITO. The second electrode 172 is formed in a circular shape having an opening that exposes the central region of the second light reflecting layer 140.
[0044] Here, the operation of the light emitting element 1 configured as above will be described. When a voltage is applied between the first electrode 171 and the second electrode 172, a current flows from the first semiconductor layer 110 to the second semiconductor layer 120. In the second semiconductor layer 120, the ion implantation region 160 is an insulating region, so that a current is injected into the central region of the second semiconductor layer 120 surrounded by the ion implantation region 160. This injected current generates spontaneous emission light due to carrier recombination in the active layer 123. The spontaneous emission light travels in the stacking direction (Z direction) of the light emitting element 1, and is repeatedly reflected between the second light reflecting layer 140 and the first light reflecting layer 130.
[0045] Since the first light reflecting layer 130 and the second light reflecting layer 140 are configured to reflect red light, the wavelength component of red light in the spontaneous emission light forms a standing wave between the first light reflecting layer 130 and the second light reflecting layer 140, and is amplified by the active layer 123. When the injection current exceeds a threshold value, the light forming the standing wave causes laser oscillation. The laser light (see the arrow in FIG. 1) thus generated is emitted after passing through the second light reflecting layer 140. The light emitting element 1 may be configured so that the laser light is emitted after passing through the first light reflecting layer 130. A light source unit in which a plurality of light emitting elements 1 are arranged in a two-dimensional array may be configured.
[0046] Since the light emitting element 1 is formed with a concave mirror 133, the resonator length L OR can be set to 20 μm. Here, the resonator length L OR 1, is the distance between the inner surface of concave mirror 133 and the flat inner surface of second light reflecting layer 140. The inner surface of concave mirror 133 is a surface that contacts lens 113. On the other hand, the inner surface of second light reflecting layer 140 faces the inner surface of concave mirror 133 with first semiconductor layer 110 and second semiconductor layer 120 interposed therebetween, and is a surface that contacts first main surface 121 of second semiconductor layer 120.
[0047] As described above, the light-emitting element 1 forms a resonator by the active layer 123, the first light reflecting layer 130, and the second light reflecting layer 140. To form this resonator, the least common multiple of the optical distance from the center of the bonding layer 150 to the inner surface of the second light reflecting layer 140 and the optical distance from the center of the bonding layer 150 to the inner surface of the concave mirror 133 is preferably the oscillation wavelength λ0 / 4, but may be at least within 10% of the oscillation wavelength λ0 / 4.
[0048] The concave mirror 133 reduces the cavity length L OR Since the length of the cavity L can be increased, the longitudinal mode interval becomes shorter than 2 nm and becomes narrower. OR Each oscillation mode that can oscillate is called a longitudinal mode. Among the longitudinal modes, those that match the gain spectrum determined by the active layer 123 can oscillate as a laser. The spacing between the longitudinal modes is determined by the cavity length L OR The longer the cavity length, the narrower the cavity becomes. OR When the cavity length L is long, the laser can oscillate at a wavelength with the highest gain. As a result, even if a part of the light is absorbed by the bonding layer 150 (metal layer) formed between the first light reflecting layer 130 and the second light reflecting layer 140, the laser can oscillate. OR is not limited to 20 μm, but may be at least 5 μm or more.
[0049] According to the present embodiment described above, the first semiconductor layer 110 and the second semiconductor layer 120 are bonded together by the bonding layer 150. This improves the bonding strength compared to when these two semiconductor layers made of different materials are directly bonded together. This makes it possible to suppress a decrease in light emission performance.
[0050] In this embodiment, the bonding layer 150 is a metal layer, which makes it possible to reduce the electrical resistance at the bonding interface between the bonding layer 150 and the first semiconductor layer 110 and at the bonding interface between the bonding layer 150 and the second semiconductor layer 120.
[0051] Furthermore, in this embodiment, GaN, which has a higher thermal conductivity than the material of the second semiconductor layer 120, is used as the material of the first semiconductor layer 110. This allows for improved temperature characteristics and higher output of emitted light.
[0052] 3 is a cross-sectional view showing the structure of a light-emitting device according to a modified example of embodiment 1. Here, the same components as those in embodiment 1 are given the same reference numerals, and detailed description thereof will be omitted.
[0053] 3 has a mesa structure in which the ion implantation region 160 of the light emitting element 1 according to the first embodiment is removed by etching such as RIE (Reactive Ion Etching). In the mesa structure, the second semiconductor layer 120 has a protrusion 124 protruding from the first major surface 121. The active layer 123 is formed in the protrusion 124. In addition, the second light reflecting layer 140 is provided on the protrusion 124.
[0054] In the light emitting device 1a according to this modification, the current flowing through the second semiconductor layer 120 is concentrated in the protrusion 124. Therefore, a current confinement structure can be realized in this modification as well.
[0055] Second embodiment 4 is a cross-sectional view showing the structure of a light-emitting device according to embodiment 2. Again, the same components as those in embodiment 1 are given the same reference numerals, and detailed description thereof will be omitted.
[0056] The light-emitting element 2 shown in FIG. 4 differs from the light-emitting element 1 according to the first embodiment in that the first semiconductor layer 110 and the second semiconductor layer 120 are bonded together using a bonding layer 151. The bonding layer 151 can be formed using a low energy gap material or a low effective mass material. Specifically, the material of the bonding layer 151 is a semiconductor such as Si or Ge. The thickness t of the bonding layer 151 is about 5 nm.
[0057] In this embodiment, a Si film or a Ge film is formed on each of the first major surface 121 of the first semiconductor layer 110 and the second major surface 122 of the second semiconductor layer 120. Then, the Si films or the Ge films are bonded to each other to complete the bonding layer 151. The bonding layer 151 forms a tunnel junction between the first semiconductor layer 110 and the second semiconductor layer 120.
[0058] According to the present embodiment described above, the first semiconductor layer 110 and the second semiconductor layer 120 form a tunnel junction by the junction layer 151. Therefore, the junction strength is improved compared to when the first semiconductor layer 110 and the second semiconductor layer 120 are directly bonded to each other. Therefore, it is possible to suppress a decrease in light emission performance.
[0059] In this embodiment, the bonding layer 151 is formed of a low energy gap material such as Si or Ge, thereby generating a tunnel effect. Therefore, the electrical resistance at the bonding interface between the bonding layer 151 and the first semiconductor layer 110 and at the bonding interface between the bonding layer 151 and the second semiconductor layer 120 can be reduced.
[0060] Also in this embodiment, GaN, which has high thermal conductivity, is used as the material for the first semiconductor layer 110. This allows for improved temperature characteristics and higher output of emitted light.
[0061] Furthermore, in this embodiment, the resonator length L OR Since the longitudinal mode spacing is increased, the longitudinal mode spacing can be narrowed. This makes it easier to combine the gain and the yield rate improved.
[0062] In the light emitting device 2 according to this embodiment, similarly to the modification of the first embodiment, a mesa structure as shown in Fig. 3 may be provided instead of the ion implantation region 160. In this case, a current confinement structure can be realized.
[0063] Third embodiment FIG. 5 is a cross-sectional view showing the structure of the light-emitting element according to the third embodiment. Here too, the same components as those in the first embodiment are denoted by the same reference numerals, and detailed descriptions thereof are omitted.
[0064] In the light-emitting element 3 according to the present embodiment, the first semiconductor layer 110 and the second semiconductor layer 120 are joined using the joining layer 152. Further, in the light-emitting element 3 according to the present embodiment, the ion implantation region 160 is formed on the first main surface 111 of the second semiconductor layer 120, and the second light reflection layer 140 has a mesa structure.
[0065] The joining layer 152 is an antireflection layer. The refractive index n0 of the joining layer 152 is higher than the refractive index n1 of the first light reflection layer 130 and smaller than the refractive index n2 of the second light reflection layer 140. The material of the joining layer 152 is, for example, SiN.
[0066] In the present embodiment, SiN films are formed on the first main surface 121 of the first semiconductor layer 110 and the second main surface 122 of the second semiconductor layer 120, respectively. Then, the joining layer 152 is completed by joining the SiN films together. The first semiconductor layer 110 and the second semiconductor layer 120 are joined by the joining layer 152.
[0067] According to the present embodiment described above, the first semiconductor layer 110 and the second semiconductor layer 120 are joined by the joining layer 152. Therefore, the joining strength is improved as compared with the case where the first semiconductor layer 110 and the second semiconductor layer 120 are directly joined. Thus, it is possible to suppress a decrease in light-emitting performance.
[0068] Further, in the present embodiment, the relationship n1 < n0 < n2 holds among the refractive index n0 of the joining layer 152, the refractive index n1 of the first light reflection layer 130, and the refractive index n2 of the second light reflection layer 140. Therefore, it is possible to suppress reflection at the joining interface due to the refractive index difference between the first semiconductor layer 110 and the second semiconductor layer 120, which are made of different materials.
[0069] Also in this embodiment, GaN, which has high thermal conductivity, is used as the material for the first semiconductor layer 110. This allows for improved temperature characteristics and higher output of emitted light.
[0070] Furthermore, in this embodiment, the resonator length L OR Since the longitudinal mode spacing is increased, the longitudinal mode spacing can be narrowed. This makes it easier to combine the gain and the yield rate improved.
[0071] (Fourth embodiment) 6 is a cross-sectional view showing the structure of a light-emitting device according to embodiment 4. Here, the same components as those in embodiment 3 are given the same reference numerals, and detailed description thereof will be omitted.
[0072] In the light emitting element 4 according to this embodiment, the first semiconductor layer 110 and the second semiconductor layer 120 are bonded to each other using the bonding layer 153. The bonding layer 153 has a first region 153a and a second region 153b. The thickness of each of the first region 153a and the second region 153b is about 5 nm. The refractive index of the first region 153a is greater than the refractive index of the second region 153b.
[0073] The first region 153a is a conductive region made of a metal such as Ti. The second region 153b is an insulating region made of SiO2. The first region 153a is disposed at a position facing the lens 113 and the concave mirror 133. The width w1 in the X direction of the first region 153a is approximately equal to the aperture diameter d. The aperture diameter d is the diameter of a circular region surrounded by the ion-implanted region 160 in the first semiconductor layer 110 as shown in FIG. 6. The aperture diameter d is also approximately equal to the width in the X direction of the second light reflecting layer 140.
[0074] According to the present embodiment described above, the first semiconductor layer 110 and the second semiconductor layer 120 are bonded together by the bonding layer 153. This improves the bonding strength compared to when the first semiconductor layer 110 and the second semiconductor layer 120 are directly bonded together. This makes it possible to suppress a decrease in light emission performance.
[0075] In this embodiment, the bonding layer 153 is divided into a first region 153a and a second region 153b having a refractive index difference. The first region 153a having a high refractive index is disposed in the central region of the bonding layer 153, and the second region 153b having a low refractive index is disposed in the peripheral region of the bonding layer 153 surrounding the first region 153a. Therefore, when the wavelength component of the red light is repeatedly reflected between the first light reflecting layer 130 and the second light reflecting layer 140, an optical path is easily formed in the first region 153a. This improves the stability of the transverse mode.
[0076] Also in this embodiment, GaN, which has high thermal conductivity, is used as the material for the first semiconductor layer 110. This allows for improved temperature characteristics and higher output of emitted light.
[0077] Furthermore, in this embodiment, the resonator length L OR Since the longitudinal mode spacing is increased, the longitudinal mode spacing can be narrowed. This makes it easier to combine the gain and the yield rate improved.
[0078] Fifth embodiment 7 is a cross-sectional view showing the structure of a light-emitting device according to embodiment 5. Again, the same components as those in embodiment 3 are given the same reference numerals, and detailed description thereof will be omitted.
[0079] In the light emitting device 5 according to this embodiment, the first semiconductor layer 110 and the second semiconductor layer 120 are bonded to each other using a bonding layer 154. The bonding layer 154 has a first region 154a and a second region 154b. The thickness of each of the first region 154a and the second region 154b is about 10 nm. The attenuation coefficient of the laser oscillation in the first region 154a is smaller than the attenuation coefficient of the laser oscillation in the second region 154b.
[0080] The first region 154a is a semiconductor region made of, for example, Si. The second region 154b is an insulating region made of, for example, a metal such as Au. The first region 154a is disposed at a position facing the lens 113 and the concave mirror 133. The width w2 in the X direction of the first region 154a is approximately equal to the aperture diameter d. The aperture diameter d is the diameter of a circular region surrounded by the ion implantation region 160 in the first semiconductor layer 110 as shown in FIG. 6. The aperture diameter d is also approximately equal to the width in the X direction of the second light reflecting layer 140.
[0081] According to the present embodiment described above, the first semiconductor layer 110 and the second semiconductor layer 120 are bonded together by the bonding layer 154. This improves the bonding strength compared to when the first semiconductor layer 110 and the second semiconductor layer 120 are directly bonded together. This makes it possible to suppress a decrease in light emission performance.
[0082] In this embodiment, the bonding layer 154 is divided into a first region 154a and a second region 154b having a difference in attenuation coefficient. The first region 154a with a low attenuation coefficient is disposed in the central region of the bonding layer 154, and the second region 154b with a high attenuation coefficient is disposed in the peripheral region of the bonding layer 154 surrounding the first region 154a. Therefore, when the wavelength component of the red light is repeatedly reflected between the first light reflecting layer 130 and the second light reflecting layer 140, an optical path is easily formed in the first region 154a. This improves the stability of the transverse mode.
[0083] Also in this embodiment, GaN, which has high thermal conductivity, is used as the material for the first semiconductor layer 110. This allows for improved temperature characteristics and higher output of emitted light.
[0084] Furthermore, in this embodiment, the resonator length L OR Since the longitudinal mode spacing is increased, the longitudinal mode spacing can be narrowed. This makes it easier to combine the gain and the yield rate improved.
[0085] Sixth embodiment 8 is a cross-sectional view showing the structure of a light-emitting device according to embodiment 6. Again, the same components as those in embodiment 3 are given the same reference numerals, and detailed description thereof will be omitted.
[0086] In the light emitting device 6 according to this embodiment, the first semiconductor layer 110 and the second semiconductor layer 120 are bonded to each other using the bonding layer 155. The bonding layer 155 is an amorphous layer having a thickness of about 10 nm. The bonding layer 155 contains, for example, Ga, N, and As.
[0087] According to the present embodiment described above, the first semiconductor layer 110 and the second semiconductor layer 120 are bonded together by the bonding layer 155. This improves the bonding strength compared to when the first semiconductor layer 110 and the second semiconductor layer 120 are directly bonded together. This makes it possible to suppress a decrease in light emission performance.
[0088] In this embodiment, the bonding layer 155 is an amorphous layer. Therefore, carriers are generated in the bonding layer 155 during application of a voltage between the first electrode 171 and the second electrode 172, and the electrical resistance decreases. This makes it possible to reduce the electrical resistance at the bonding interface between the bonding layer 151 and the first semiconductor layer 110 and at the bonding interface between the bonding layer 151 and the second semiconductor layer 120.
[0089] Seventh embodiment 9 is a cross-sectional view showing the structure of a light-emitting device according to embodiment 7. Here, the same components as those in embodiment 6 are given the same reference numerals, and detailed description thereof will be omitted.
[0090] In the light emitting device 7 according to this embodiment, the first semiconductor layer 110 and the second semiconductor layer 120 are bonded to each other using the bonding layer 156. In the light emitting device 6 according to this embodiment, the second semiconductor layer 120 and the second light reflecting layer 140 have a mesa structure. That is, the second semiconductor layer 120 has a protrusion 124, and the second light reflecting layer 140 is formed on the protrusion 124.
[0091] The bonding layer 156 has a first region 156a and a second region 156b. The thickness of each of the first region 156a and the second region 156b is about 10 nm. The first region 156a is an amorphous region containing, for example, Ga, N, and As. The second region 156b is an oxidized region obtained by oxidizing the amorphous region. The first region 156a is disposed at a position facing the lens 113 and the concave mirror 133. The width w3 of the first region 156a in the X direction is approximately the same as the aperture diameter d.
[0092] According to the present embodiment described above, the first semiconductor layer 110 and the second semiconductor layer 120 are bonded together by the bonding layer 156. This improves the bonding strength compared to when the first semiconductor layer 110 and the second semiconductor layer 120 are directly bonded together. This makes it possible to suppress a decrease in light emission performance.
[0093] In this embodiment, the first region 156a disposed in the central region of the bonding layer 156 is an amorphous region, and the second region 156b surrounding the first region 156a is an oxidized region. Therefore, a current confinement structure is also formed in the bonding layer 156. Therefore, when a current passes through the bonding layer 156, it is easily concentrated in the first region 156a.
[0094] Also in this embodiment, GaN, which has high thermal conductivity, is used as the material for the first semiconductor layer 110. This allows for improved temperature characteristics and higher output of emitted light.
[0095] Furthermore, in this embodiment, the resonator length L OR Since the longitudinal mode spacing is increased, the longitudinal mode spacing can be narrowed. This makes it easier to combine the gain and the yield rate improved.
[0096] Eighth embodiment 10 is a cross-sectional view showing the structure of a light-emitting device according to embodiment 8. Here, the same components as those in embodiment 3 are given the same reference numerals, and detailed description thereof will be omitted.
[0097] In the light emitting element 8 according to this embodiment, the first semiconductor layer 110 and the second semiconductor layer 120 are bonded together using the bonding layer 157. The bonding layer 157 is formed integrally with the first electrode 171. The thickness of the bonding layer 157 is preferably 10 nm or less, for example, about 5 nm. The material of the bonding layer 157 is a metal such as Ti.
[0098] In this embodiment, a Ti film is formed on each of the first major surface 121 of the first semiconductor layer 110 and the second major surface 122 of the second semiconductor layer 120. Then, the Ti films are bonded to each other to complete the bonding layer 157. The bonding layer 157 bonds the first semiconductor layer 110 and the second semiconductor layer 120 together via the metal layer.
[0099] According to the present embodiment described above, the first semiconductor layer 110 and the second semiconductor layer 120 are bonded together by the bonding layer 156. This improves the bonding strength compared to when the first semiconductor layer 110 and the second semiconductor layer 120 are directly bonded together. This makes it possible to suppress a decrease in light emission performance.
[0100] In addition, in this embodiment, the bonding layer 156 is a metal layer, which makes it possible to reduce the electrical resistance at the bonding interface between the bonding layer 150 and the first semiconductor layer 110 and at the bonding interface between the bonding layer 150 and the second semiconductor layer 120.
[0101] In this embodiment, the bonding layer 156 is integrated with the first electrode 171. This makes it possible to stabilize the electrical contact characteristics between the first electrode 171 and the second semiconductor layer 120. In addition, when dry etching or wet etching is performed in the manufacturing process of the light-emitting element 8, the bonding layer 156 can function as an etching stop layer.
[0102] Also in this embodiment, GaN, which has high thermal conductivity, is used as the material for the first semiconductor layer 110. This allows for improved temperature characteristics and higher output of emitted light.
[0103] Furthermore, in this embodiment, the resonator length L OR Since the longitudinal mode spacing is increased, the longitudinal mode spacing can be narrowed. This makes it easier to combine the gain and the yield rate improved.
[0104] Ninth embodiment 11 is a cross-sectional view showing the structure of a light-emitting device according to embodiment 9. Here, the same components as those in embodiment 1 are given the same reference numerals, and detailed description thereof will be omitted.
[0105] 11, the radius of curvature of the apex of the lens 113 is larger than that of the light-emitting element 1 according to the first embodiment. In this embodiment, the radius of curvature of the apex of the lens 113 is set to satisfy the relational expression d / ω≦4 between the aperture diameter d and the beam waist diameter ω.
[0106] According to the present embodiment described above, the first semiconductor layer 110 and the second semiconductor layer 120 are bonded to each other by the bonding layer 151, which is a metal layer, in the same manner as in the first embodiment. Therefore, the bonding strength is improved compared to when the first semiconductor layer 110 and the second semiconductor layer 120 are directly bonded to each other. Therefore, it is possible to suppress a decrease in light emission performance.
[0107] In this embodiment, the radius of curvature of the apex of the lens 113 is larger than that of the first embodiment. Therefore, when the wavelength component of the red light is repeatedly reflected between the first light reflecting layer 130 and the second light reflecting layer 140, the radiation angle can be narrowed to make the transverse mode a single mode.
[0108] Also in this embodiment, GaN, which has high thermal conductivity, is used as the material for the first semiconductor layer 110. This allows for improved temperature characteristics and higher output of emitted light.
[0109] Furthermore, in this embodiment, the resonator length L OR Since the longitudinal mode spacing is increased, the longitudinal mode spacing can be narrowed. This makes it easier to combine the gain and the yield rate improved.
[0110] In the light emitting device 9 according to this embodiment, similarly to the modification of the first embodiment, a mesa structure as shown in Fig. 3 may be provided instead of the ion implantation region 160. In this case, a current confinement structure can be realized.
[0111] Tenth embodiment 12 is a cross-sectional view showing the structure of a light-emitting device according to embodiment 10. Here, the same components as those in embodiment 1 are given the same reference numerals, and detailed description thereof will be omitted.
[0112] 12, the first semiconductor layer 110 and the second semiconductor layer 120 are bonded to each other using a bonding layer 158. The bonding layer 158 is a phase shift layer. Specifically, the material of the bonding layer 158 is SiO2. Therefore, in this embodiment, the first electrode 171 is formed on the second semiconductor layer 120.
[0113] The optical thickness of the bonding layer 158 is 0.1 to 50 times the oscillation wavelength λ0, and satisfies k(λ0 / 4)(2r+1) [where r is an integer equal to or less than 100, and 0.9≦k≦1.1].
[0114] In this embodiment, a SiO2 film is formed on each of the first major surface 121 of the first semiconductor layer 110 and the second major surface 122 of the second semiconductor layer 120. Then, the SiO2 films are bonded to each other to complete the bonding layer 158. The bonding layer 158 bonds the first semiconductor layer 110 and the second semiconductor layer 120 together.
[0115] According to the present embodiment described above, the first semiconductor layer 110 and the second semiconductor layer 120 are bonded together by the bonding layer 158. This improves the bonding strength compared to when the first semiconductor layer 110 and the second semiconductor layer 120 are directly bonded together. This makes it possible to suppress a decrease in light emission performance.
[0116] In general, in a VCEL element, the active layer gain changes with respect to wavelength due to a change in the temperature of the active layer. Here, the wavelength at which the active layer gain is at its maximum value is the oscillation wavelength λ0 of the light-emitting element. Therefore, when the temperature of the active layer rises, for example, the active layer gain changes from a to b, and as a result, the oscillation wavelength λ0 also changes from wavelength λa to wavelength λb.
[0117] In the light-emitting device 10 according to this embodiment, when the temperature of the active layer 123 rises, the active layer gain changes from a to b. However, in this embodiment, the bonding layer 158 functions as a phase shift layer. Therefore, at the active layer gain b, the wavelength λb falls in the low light reflection wavelength region. Therefore, the light-emitting device 10 does not oscillate at the wavelength λb. Instead, the light-emitting device 10 oscillates at a wavelength close to the wavelength λa.
[0118] As described above, the bonding layer 158 functions as a phase shift layer, thereby making it possible to control the longitudinal mode, thereby making it possible to stabilize the oscillation wavelength λ0 with respect to the operating temperature and operating current.
[0119] Also in this embodiment, GaN, which has high thermal conductivity, is used as the material for the first semiconductor layer 110. This allows for improved temperature characteristics and higher output of emitted light.
[0120] Furthermore, in this embodiment, the resonator length L OR Since the longitudinal mode spacing is increased, the longitudinal mode spacing can be narrowed. This makes it easier to combine the gain and the yield rate improved.
[0121] In the light emitting device 10 according to this embodiment, similarly to the modification of the first embodiment, a mesa structure as shown in Fig. 3 may be provided instead of the ion implantation region 160. In this case, a current confinement structure can be realized.
[0122] The present technology can be configured as follows. (1) a first semiconductor layer having a lens having a convex shape; a second semiconductor layer having an active layer and made of a material different from that of the first semiconductor layer; a first light reflecting layer having a concave mirror facing the lens; a second light reflecting layer facing the first light reflecting layer with the first semiconductor layer and the second semiconductor layer interposed therebetween; a bonding layer provided between the first semiconductor layer and the second semiconductor layer; A light-emitting element comprising: (2) The light-emitting element according to (1), wherein the material of the bonding layer is a metal. (3) The light-emitting element according to (1), wherein the material of the bonding layer is Si or Ge. (4) The light-emitting element according to (1), wherein the optical refractive index of the bonding layer is higher than the optical refractive index of the first optical reflecting layer and lower than the optical refractive index of the second optical reflecting layer. (5) The light-emitting element described in (1), wherein the bonding layer has a first region facing the lens and the concave mirror and a second region surrounding the first region, and the optical refractive index of the first region is greater than the optical refractive index of the second region. (6) The light-emitting element described in (1), wherein the bonding layer has a first region facing the lens and the concave mirror and a second region surrounding the first region, and the attenuation coefficient of the first region is smaller than the attenuation coefficient of the second region. (7) The light-emitting element according to (1), wherein the bonding layer is an amorphous layer. (8) The light-emitting element described in (1), wherein the bonding layer has a first region facing the lens and the concave mirror and a second region surrounding the first region, the first region being an amorphous region and the second region being an oxidized region. (9) An electrode electrically connected to the second semiconductor layer via the junction layer, The light-emitting element according to (1), wherein the bonding layer and the electrode are integrated. (10) The light-emitting element according to (1), wherein the radius of curvature of the apex of the lens is set to satisfy the relation d / ω≦4, where d is the aperture diameter and ω is the beam waist diameter. (11) The light-emitting element according to (1), wherein the optical thickness of the bonding layer is 0.1 to 50 times the oscillation wavelength λ0, and satisfies k(λ0 / 4)(2r+1), where r is an integer equal to or less than 100, and 0.9≦k≦1.1. (12) The light-emitting element according to any one of (1) to (11), wherein the least common multiple of the optical distance from the center of the bonding layer to the inner surface of the second light reflecting layer and the optical distance from the center of the bonding layer to the inner surface of the concave mirror is within 10% of the oscillation wavelength / 4. (13) The light-emitting device according to any one of (1) to (12), wherein a cavity length between the first light-reflecting layer and the second light-reflecting layer is at least 5 μm or more. (14) The light-emitting device according to any one of (1) to (13), wherein a lattice constant difference between the material of the first semiconductor layer and the material of the second semiconductor layer is 15% or more. (15) The light-emitting element according to any one of (1) to (14), wherein the energy gap of the first semiconductor layer is at least 0.8 eV or more. (16) The light-emitting element according to any one of (1) to (15), wherein the first semiconductor layer has a higher thermal conductivity than the second semiconductor layer. (17) The first light reflecting layer is formed of a laminate of two types of dielectric materials having different light refractive indices, The light-emitting device according to any one of (1) to (16), wherein the second light-reflecting layer is made of a laminate of two types of semiconductors having different optical refractive indices. (18) The light-emitting device according to any one of (1) to (17), which has a current confinement structure formed by an ion-implanted region or a mesa structure. (19) The light-emitting device according to any one of (1) to (18), wherein the material of the active layer is InGaN, AlGaN, InGaP, or AlGaInP. (20) The light-emitting device according to any one of (1) to (19), which is arranged in a two-dimensional array. [Explanation of symbols]
[0123] 1 to 10: Light emitting element 110: First semiconductor layer 113: Lens 120: second semiconductor layer 123:Active layer 130: 1st light reflective layer 133: Concave mirror 140:Second light reflective layer 150~158: Bonding layer 153a, 154a, 156a: 1st area 153b, 154b, 156b: 2nd area 171: 1st electrode
Claims
1. a first semiconductor layer having a lens having a convex shape; A second semiconductor layer having an active layer and made of a material different from that of the first semiconductor layer; a first light reflecting layer having a concave mirror facing the lens; a second light reflecting layer facing the first light reflecting layer with the first semiconductor layer and the second semiconductor layer interposed therebetween; a bonding layer provided between the first semiconductor layer and the second semiconductor layer; A light-emitting element comprising:
2. The light-emitting device according to claim 1 , wherein the material of the bonding layer is a metal.
3. The light-emitting device according to claim 1 , wherein the material of the bonding layer is Si or Ge.
4. The light emitting device according to claim 1 , wherein the optical refractive index of the bonding layer is higher than the optical refractive index of the first optical reflection layer and lower than the optical refractive index of the second optical reflection layer.
5. 2. The light-emitting element according to claim 1, wherein the bonding layer has a first region facing the lens and the concave mirror and a second region surrounding the first region, and the optical refractive index of the first region is greater than the optical refractive index of the second region.
6. 2. The light-emitting element according to claim 1, wherein the bonding layer has a first region facing the lens and the concave mirror and a second region surrounding the first region, and the attenuation coefficient of the first region is smaller than the attenuation coefficient of the second region.
7. The light-emitting device according to claim 1 , wherein the bonding layer is an amorphous layer.
8. 2. The light-emitting element according to claim 1, wherein the bonding layer has a first region facing the lens and the concave mirror and a second region surrounding the first region, the first region being an amorphous region and the second region being an oxidized region.
9. an electrode electrically connected to the second semiconductor layer via the junction layer, The light-emitting device according to claim 1 , wherein the bonding layer and the electrode are integrated together.
10. 2. The light-emitting device according to claim 1, wherein the radius of curvature of the apex of the lens is set so as to satisfy the relation d / ω≦4, where d is an aperture diameter and ω is a beam waist diameter.
11. The optical thickness of the bonding layer is set to be smaller than the oscillation wavelength λ 0 0.1 times or more and 50 times or less, and k(λ 0 2. The light-emitting device according to claim 1, wherein k satisfies 0.9≦k≦1.1, and k is an integer equal to or less than 100. / 4)(2r+1).
12. 2. The light-emitting element according to claim 1, wherein the least common multiple of the optical distance from the center of the bonding layer to the inner surface of the second light-reflecting layer and the optical distance from the center of the bonding layer to the inner surface of the concave mirror is within 10% of the oscillation wavelength / 4.
13. The light-emitting element according to claim 1 , wherein a cavity length between the first light-reflecting layer and the second light-reflecting layer is at least 5 μm or more.
14. The light-emitting device according to claim 1 , wherein a difference in lattice constant between the material of the first semiconductor layer and the material of the second semiconductor layer is 15% or more.
15. The light-emitting device according to claim 1 , wherein the energy gap of the first semiconductor layer is at least 0.8 eV or more.
16. The light-emitting device according to claim 1 , wherein the first semiconductor layer has a higher thermal conductivity than the second semiconductor layer.
17. the first light reflecting layer is formed of a laminate of two types of dielectric materials having different light refractive indices, The light-emitting element according to claim 1 , wherein the second light-reflecting layer is made of a laminate of two types of semiconductors having different optical refractive indices.
18. The light-emitting device according to claim 1 , further comprising a current confinement structure formed by an ion-implanted region or a mesa structure.
19. The light-emitting device according to claim 1 , wherein the material of the active layer is InGaN, AlGaN, InGaP, or AlGaInP.
20. The light-emitting device according to claim 1 , arranged in a two-dimensional array.
Citation Information
Patent Citations
Vertical-cavity surface-emitting laser element and method for manufacturing vertical-cavity surface-emitting laser element
JP2022038492A
Cited By
Method for manufacturing a semiconductor device as well as semiconductor device
DE102025115999A1
Vertical cavity surface emitting laser element and method for producing same
WO2026100262A1