U-shaped aluminum template punching die
By designing a U-shaped aluminum template punching mold, the problem of low efficiency and low precision in the hole opening process of irregularly shaped aluminum alloy templates is solved, the stable positioning and flatness maintenance of the template are achieved, the mold manufacturing cost is reduced and the cost is avoided scuffs and scratches.
Patent Information
- Application Number
- CN201811206826.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2018-10-17
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2038-10-17
AI Technical Summary
In the construction industry, irregularly shaped aluminum alloy formwork has problems such as low work efficiency, low dimensional accuracy and unguaranteed formwork surface flatness during the drilling process.
A U-shaped aluminum template punching die is designed, including a punch assembly and a die body. It provides positioning, shape retention and flatness through components such as punch connecting plates, punch pressing plates, stamping pins, bearings and mold plates. The maintenance function ensures the stability and accuracy of the template during the punching process.
This mold reduces mold manufacturing costs while ensuring the quality of template processing. It is suitable for U-shaped cross-section templates, ensuring the flatness of the punching part and the smooth movement of the template, avoiding mold wear and surface scratches.
Smart Images

Figure CN109226465B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of aluminum template punching, in particular to an aluminum template punching die. Background Art
[0002] With the continuous innovation and development of modern technology and processes, new building materials are constantly replacing traditional materials and being used in the construction industry. Aluminum alloy formwork is one of the new materials. This material has the advantages of light weight, high strength, corrosion resistance, easy recycling, easy installation, high dimensional accuracy, etc. It is being widely promoted and applied in the construction industry.
[0003] In order to meet the connection requirements during use, aluminum alloy formworks need to be drilled. However, due to different construction projects, the shapes of the designed aluminum alloy formworks vary. Therefore, for irregularly shaped aluminum alloy formworks, holes often need to be drilled, which results in low work efficiency, low dimensional accuracy, and the flatness of the formwork surface cannot be guaranteed. Summary of the invention
[0004] The technical problem to be solved by the invention is to provide a U-shaped aluminum template punching die.
[0005] A U-shaped aluminum template punching die comprises a punch assembly and a die body, wherein the punch assembly consists of a punch connecting plate, a punch pressing plate and a punching pin connected in sequence from top to bottom; a U-shaped cavity penetrating the die body front and back is provided in the die body; the width of the upper cavity of the U-shaped cavity is equal to the width of the lower cavity; the upper cavity is connected to the lower cavity through a side cavity; a punching hole penetrating the die body from top to bottom is provided in the die body, and the punching hole passes through the upper cavity and the lower cavity.
[0006] The U-shaped aluminum template punching die of the present invention has bearings on both sides of the upper cavity and the lower cavity; and a bearing pin is provided in the die body, one on each side and one on the top, passing through the bearing.
[0007] The U-shaped aluminum template punching mold described in the present invention, wherein, an upper mold plate is provided below the upper cavity, and a first punching hole is provided through the center of the upper mold plate; a first pin hole is provided on one side of the upper mold plate; the upper mold plate is fixed to the mold body by a pin passing through the first pin hole; a lower mold plate is provided below the lower cavity, and a second punching hole is provided through the center of the lower mold plate; a second pin hole is provided on one side of the lower mold plate; the lower mold plate is fixed to the mold body by a pin passing through the second pin hole.
[0008] The U-shaped aluminum template punching mold described in the present invention, wherein an upper mold sleeve is provided in the mold body above the upper cavity, and a lower mold sleeve is provided in the mold body below the mold plate; the upper mold sleeve and the lower mold sleeve are both cylindrical, and their inner diameter is equal to the cross-sectional diameter of the stamping pin shaft, and their outer diameter is equal to the diameter of the punching hole in the mold body.
[0009] The U-shaped aluminum template punching die described in the present invention, wherein the cross-section of the punch connecting plate is inverted T-shaped, the upper part of which is a square plate, and the lower part is a circular plate, and the two are made as one piece; a through hole that passes through front and back is provided in the center of the square plate, bolt holes that pass through up and down are provided at the left and right ends of the square plate, and two bolt holes that pass through up and down are symmetrically provided on both sides of the circular plate; a circular groove A is provided at the bottom of the circular plate.
[0010] The U-shaped aluminum template punching die described in the present invention, wherein the punch pressing plate is a circular plate, a through hole is provided in the center thereof, and 6 bolt holes are evenly distributed around it; a circular groove B is provided in the center of the upper surface of the punch pressing plate; the circular groove A and the circular groove B are equal in size.
[0011] The U-shaped aluminum template punching die described in the present invention, wherein the punching pin is in the shape of a cylindrical rod, and the diameter of its head is slightly larger than the diameter of the rod; the diameter of the punching pin head is equal to the diameter of the circular groove A; the head of the punching pin is placed in the space enclosed by the circular groove A and the circular groove B, and the rod of the punching pin passes through the through hole; the punch connecting plate and the punch pressing plate are connected by bolts.
[0012] The U-shaped aluminum template punching die of the present invention, wherein a groove C is provided on the upper surface of the die body.
[0013] The U-shaped aluminum template punching die described in the present invention, wherein a third pin hole is provided on the side of the upper die sleeve; a fourth pin hole is provided on the side of the lower die sleeve; and the upper die sleeve and the lower die sleeve are fixed together with the die body by pins passing through the pin holes.
[0014] The U-shaped aluminum template punching die of the present invention has the left and right ends of the upper cavity and the lower cavity having heights higher than the middle; and the U-shaped aluminum template can be placed in the U-shaped cavity.
[0015] Compared with the prior art, the outstanding effects of the present invention are:
[0016] (1) The mold has the functions of positioning the template punching, maintaining the template shape, and maintaining the flatness of the template punching part. The mold structure is compact and the layout is simple and reasonable. Under the premise of ensuring the quality of template processing, the mold manufacturing cost is reduced to the greatest extent.
[0017] (2) The mold is suitable for U-section templates. When processing the U-section template, the corresponding mold is first installed on the punching equipment. The mold clamping template space is closely matched with the template. When punching, it can effectively support the template cavity, thereby ensuring that the stamping surface and other working surfaces of the template are not deformed before and after stamping, which affects the use of the template. The mold is equipped with a rolling bearing device to ensure that the template moves smoothly in the mold during servo feeding, and at the same time, it can also avoid mold wear and scratches on the template surface.
[0018] The U-shaped aluminum template punching die of the present invention is further described below in conjunction with the accompanying drawings and specific embodiments. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 It is a schematic diagram of the structure of the U-shaped aluminum template punching die of the present invention when punching;
[0020] Figure 2 It is the main view of the punch assembly;
[0021] Figure 3 It is the left view of the punch assembly;
[0022] Figure 4 It is a bottom view of the punch plate;
[0023] Figure 5 It is the front view of the punch plate;
[0024] Figure 6 It is a top view of the punch connecting plate;
[0025] Figure 7 It is the left view of the punch connecting plate;
[0026] Figure 8 It is the front view of the punch connecting plate;
[0027] Fig. 9 is the main view of the upper mold plate;
[0028] Fig.10 is a top view of the upper mold plate;
[0029] Fig.11 is the front view of the lower mold plate;
[0030] Fig.12 is a top view of the lower mold plate;
[0031] Fig.13 It is a front view of a mold body with upper and lower mold plates and upper and lower mold sleeves;
[0032] Fig.14 A top view of a mold body with upper and lower mold plates and upper and lower mold sleeves;
[0033] Fig.15 It is the front view of the mold body without the upper and lower mold plates and the upper and lower mold sleeves;
[0034] Fig.16 It is a top view of the mold body without the upper and lower mold plates and the upper and lower mold sleeves. DETAILED DESCRIPTION
[0035] Combination Figure 1-3 As shown in 13-16, the U-shaped aluminum template punching die includes a punch assembly 1 and a die body 2, wherein the punch assembly is composed of a punch connecting plate 11, a punch pressing plate 12 and a punching pin 13 which are sequentially connected from top to bottom; a U-shaped cavity which passes through the die body 2 from front to back is provided in the die body 2; the width of the upper cavity of the U-shaped cavity is smaller than the width of the lower cavity; the upper cavity is connected to the lower cavity through the side cavity; a punching hole 27 which passes through the die body 2 from top to bottom is provided in the die body 2, and the punching hole 27 passes through the upper cavity and the lower cavity.
[0036] The left and right sides of the upper cavity and the left and right sides of the lower cavity are provided with bearings 4, which can play a guiding role in the aluminum template processing and avoid scratches on the surface of the aluminum template caused by direct contact and friction between the aluminum template and the mold body. The mold body 2 is provided with a bearing pin 21 on the left and right sides, which passes through the bearing up and down. The four corners of the bottom of the mold body 2 are provided with bolt holes 22 for fixing the mold body. One side of the upper surface of the mold body 2 is provided with a fixing hole 29.
[0037] like Figure 1 , 9 As shown in Figure 12, an upper mold plate 5 is provided below the upper cavity, and a first punching hole 52 is provided in the center of the upper mold plate 5; a first pin hole 53 is provided on one side of the upper mold plate 5; the upper mold plate 5 is fixed to the mold body 2 by a pin passing through the first pin hole 53 and the fixing hole 29; a lower mold plate 3 is provided below the lower cavity, and a second punching hole 31 is provided in the center of the lower mold plate 3; a second pin hole 32 is provided on one side of the lower mold plate 3; the lower mold plate 3 is fixed to the mold body 2 by a pin passing through the second pin hole 32 and the fixing hole 29. A transverse rib 51 is provided on each of the left and right sides of the lower surface of the upper mold plate 5, and the upper mold plate 5 is engaged with the mold body 2 through the transverse rib 51. The base of the transverse rib 51 connected to the lower bottom surface of the upper mold plate 5 is slightly narrower than the end, and the edge of the end is subjected to a circular arc transition treatment. The edge of the lower bottom surface of the upper mold plate 5 is subjected to a circular arc transition treatment, which is convenient for taking and placing the mold plate. The cross section of the lower mold plate 3 is in an inverted T shape, with steps 34 on both sides thereof and right-angled trapezoidal protrusions 33 at the bottom of the left and right side surfaces thereof.
[0038] The upper mold plate 5 and the lower mold plate 3 are both made of mold steel, which has better wear resistance, and are detachable from the mold body 2. When they are severely worn in the later stage, they can be directly removed and replaced.
[0039] An upper die sleeve 23 is provided in the die body above the upper cavity, and a lower die sleeve 25 is provided in the die body below the upper die plate 5; both the upper die sleeve 23 and the lower die sleeve 25 are cylindrical, and their inner diameter is equal to the cross-sectional diameter of the stamping pin shaft 13, and their outer diameter is equal to the diameter of the punching hole in the die body 2.
[0040] like Figure 2-8 As shown, the cross-section of the punch connecting plate 11 is inverted T-shaped, with the upper part being a square plate and the lower part being a circular plate, and the two are made as one piece; a through hole 111 is provided in the center of the square plate and runs through from front to back, bolt holes 112 are provided at the left and right ends of the square plate and run through from top to bottom, and two bolt holes 112 are symmetrically provided on both sides of the circular plate and run through from top to bottom; a circular groove A113 is provided at the bottom of the circular plate.
[0041] The punch plate 12 is a circular plate with a through hole 121 in the center and 6 bolt holes 122 evenly distributed around it. A circular groove B123 is provided in the center of the upper surface of the punch plate 12. The diameters of the circular groove A113 and the circular groove B123 are equal.
[0042] The stamping pin 13 is in the shape of a cylindrical rod, and the diameter of its head is slightly larger than the diameter of the rod; the diameter of its rod is 16.5 mm; the diameter of the head of the stamping pin 13 is equal to the diameter of the circular groove A113; the head of the stamping pin 13 is placed in the space enclosed by the circular groove A113 and the circular groove B123, and the rod of the stamping pin 13 passes through the through hole 121; the punch connecting plate 11 and the punch pressing plate 12 are connected by bolts.
[0043] The entire punch assembly is connected to the oil cylinder through the through hole 111 of the punch connecting plate 11.
[0044] like Fig.11 As shown, an elliptical groove C28 with a depth of 1 mm is provided on the upper surface of the mold body 2 for storing cooling lubricating grease.
[0045] A third pin hole 24 is provided on the side of the upper die sleeve 23; a fourth pin hole 26 is provided on the side of the lower die sleeve 25; the upper die sleeve 23 and the lower die sleeve 25 are both fixed to the die body 2 by pins passing through the pin holes.
[0046] The heights of the left and right ends of the upper cavity and the lower cavity are higher than the height of the middle; a U-shaped aluminum template 3 can be placed in the U-shaped cavity. During the punching process of the aluminum template, one end of the aluminum template is clamped by a chuck to pull the aluminum template to move along the U-shaped cavity of the U-shaped aluminum template punching mold, and its moving distance is controlled by a servo motor.
[0047] The embodiments described above are merely descriptions of preferred implementation modes of the present invention and are not intended to limit the scope of the present invention. Without departing from the design spirit of the present invention, various modifications and improvements made to the technical solutions of the present invention by ordinary technicians in this field should all fall within the protection scope determined by the claims of the present invention.
Claims
1. A U-shaped aluminum template punching die, characterized in that: The invention comprises a punch assembly (1) and a die body (2), wherein the punch assembly comprises a punch connecting plate (11), a punch pressing plate (12) and a punch pin (13) which are connected in sequence from top to bottom; a U-shaped cavity which passes through the die body (2) from front to back is provided in the die body (2); the width of the upper cavity of the U-shaped cavity is equal to the width of the lower cavity; the upper cavity and the lower cavity are connected via a side cavity; a punch hole (27) which passes through the die body (2) from top to bottom is provided in the die body (2), and the punch hole (27) passes through the upper cavity and the lower cavity; an upper die plate (5) is provided below the upper cavity, and a first punch hole (52) which passes through the center of the upper die plate (5); a first pin hole (52) is provided on one side of the upper die plate (5) 3); the upper mold plate (5) is fixed to the mold body (2) by a pin passing through the first pin hole (53); a lower mold plate (3) is provided below the lower cavity, and a second punching hole (31) is provided through the center of the lower mold plate (3); a second pin hole (32) is provided on one side of the lower mold plate (3); the lower mold plate (3) is fixed to the mold body (2) by a pin passing through the second pin hole (32); an upper mold sleeve (23) is provided in the mold body above the upper cavity, and a lower mold sleeve (25) is provided in the mold body below the upper mold plate (5); the upper mold sleeve (23) and the lower mold sleeve (25) are both cylindrical, with an inner diameter equal to the cross-sectional diameter of the punching pin shaft (13) and an outer diameter equal to the diameter of the punching hole in the mold body (2); Bearings (4) are provided on both the left and right sides of the upper cavity and the left and right sides of the lower cavity; a bearing pin shaft (21) is provided in the mold body (2) and passes through the bearings up and down; a third pin hole (24) is provided on the side of the upper mold sleeve (23); a fourth pin hole (26) is provided on the side of the lower mold sleeve (25); and the upper mold sleeve (23) and the lower mold sleeve (25) are fixed to the mold body (2) by pins passing through the pin holes.
2. The U-shaped aluminum template punching die according to claim 1, characterized in that: The punch connecting plate (11) has an inverted T-shaped cross section, with an upper portion being a square plate and a lower portion being a circular plate, the two being made in one piece; a through hole extending from front to back is provided in the center of the square plate, bolt holes extending from top to bottom are provided at the left and right ends of the square plate, and two bolt holes extending from top to bottom are symmetrically provided on both sides of the circular plate; a circular groove A (113) is provided at the bottom of the circular plate.
3. The U-shaped aluminum template punching die according to claim 2 is characterized in that: The punch pressing plate (12) is a circular plate having a through hole in the center and 6 bolt holes evenly distributed around it; a circular groove B (123) is provided in the center of the upper surface of the punch pressing plate (12); the diameters of the circular groove A (113) and the circular groove B (123) are equal.
4. The U-shaped aluminum template punching die according to claim 3 is characterized in that: The punch pin (13) is in the shape of a cylindrical rod, and the diameter of its head is slightly larger than the diameter of the rod; the diameter of the head of the punch pin (13) is equal to the diameter of the circular groove A (113); the head of the punch pin (13) is placed in a space enclosed by the circular groove A (113) and the circular groove B (123), and the rod of the punch pin (13) passes through the through hole; the punch connecting plate (11) and the punch pressing plate (12) are connected by bolts.
5. The U-shaped aluminum template punching die according to claim 4, characterized in that: The heights of the left and right ends of the upper cavity and the lower cavity are both higher than the height of the middle part; and a U-shaped aluminum template can be placed in the U-shaped cavity.
Citation Information
Patent Citations
Punching die for punching inner square holes
CN202461303U
Aluminum products frock of punching a hole
CN204770134U
Semi -automatic cavity aluminium alloy piercing press
CN207887714U
U-shaped aluminum template punching die
CN209035257U
Cited By
Aluminum template punching device
CN120885599A