Method for manufacturing semiconductor device

By injecting ions on the dummy gate structure and spacer during the semiconductor device manufacturing process, changing the etching characteristics, and forming grooves and interlayer insulation patterns at flat bottoms through multiple etching processes, the prior art intermediate insulation patterns are solved. The problem of poor etching has achieved the correct formation of contact holes and the improvement of semiconductor device performance.

CN109841572BActive Publication Date: 2024-12-06SAMSUNG ELECTRONICS CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN201811416261.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2017-11-27
Filing Date
2018-11-26
Publication Date
2024-12-06
Estimated Expiration
2038-11-26

AI Technical Summary

Technical Problem

In the process of manufacturing semiconductor devices, it is difficult to effectively control and adjust the etching characteristics of the inter-insulating pattern, resulting in poor or defects in contact holes, affecting device performance.

Method used

By injecting ions on the dummy gate structure, the spacer and the initial second interlayer insulating pattern, the etching characteristics thereof are changed, and the second groove and interlayer insulating pattern with a flat bottom are formed by multiple etching processes, the spacer is ensured to be The etching rate and thickness of the interlayer insulation pattern are precisely controlled, so as to achieve the correct formation of contact holes.

Benefits of technology

It improves the accuracy of contact hole formation and the electrical characteristics of semiconductor devices, reduces contact unopened defects, and enhances the stability and performance of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN109841572B_ABST
    Figure CN109841572B_ABST
Patent Text Reader

Abstract

A method for manufacturing a semiconductor device, the method comprising: forming a dummy gate structure on a substrate; forming a spacer on the side wall of the dummy gate structure; forming a preliminary first interlayer insulating pattern to fill the gap between adjacent spacers; etching the upper portion of the preliminary first interlayer insulating pattern by a first etching process to form a preliminary second interlayer insulating pattern; implanting ions on the dummy gate structure, the spacer and the preliminary second interlayer insulating pattern by an ion implantation process; etching the upper portion of the preliminary second interlayer insulating pattern by a second etching process to form an interlayer insulating pattern with a flat upper surface; and forming a covering pattern on the interlayer insulating pattern to fill the gap between the spacers.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS

[0002] The entire contents of Korean Patent Application No. 10-2017-0159654, entitled “Method of Manufacturing Semiconductor Device”, filed on November 27, 2017 in the Korean Intellectual Property Office are incorporated herein by reference. Technical Field

[0003] Embodiments relate to methods of manufacturing semiconductor devices. Background Art

[0004] Embodiments relate to methods of manufacturing semiconductor devices. Summary of the invention

[0005] An embodiment can be implemented by providing a method for manufacturing a semiconductor device, the method comprising: forming a dummy gate structure on a substrate; forming a spacer on a side wall of the dummy gate structure; forming a preliminary first interlayer insulating pattern to fill the gap between adjacent spacers; etching an upper portion of the preliminary first interlayer insulating pattern by a first etching process to form a preliminary second interlayer insulating pattern; implanting ions on the dummy gate structure, the spacer and the preliminary second interlayer insulating pattern by an ion implantation process; etching an upper portion of the preliminary second interlayer insulating pattern by a second etching process to form an interlayer insulating pattern having a flat upper surface; and forming a covering pattern on the interlayer insulating pattern to fill the gap between the spacers.

[0006] An embodiment can be implemented by providing a method for manufacturing a semiconductor device, the method comprising: forming a dummy gate structure on a substrate; forming a preliminary first interlayer insulating pattern to fill a gap between the dummy gate structures; etching an upper portion of the preliminary first interlayer insulating pattern by a first etching process to form a preliminary groove having a circular bottom and a preliminary second interlayer insulating pattern below the preliminary groove; injecting ions on the dummy gate structure and the preliminary second interlayer insulating pattern; etching a portion of the preliminary second interlayer insulating pattern by a second etching process to form a groove having a flat bottom and an interlayer insulating pattern below the groove; forming a covering pattern on the interlayer insulating pattern; and replacing the dummy gate structure with a gate structure.

[0007] An embodiment can be implemented by providing a method for manufacturing a semiconductor device, the method comprising: forming a gate structure on a substrate; forming a preliminary interlayer insulating pattern to fill a gap between the gate structures; forming a mask pattern on the gate structure and the preliminary interlayer insulating pattern to cover a contact formation area; using the mask pattern as an etching mask, partially etching an upper portion of the preliminary interlayer insulating pattern to form a groove and an interlayer insulating pattern below the groove; forming a covering pattern on the interlayer insulating pattern to fill the groove; implanting ions on the gate structure, the interlayer insulating pattern and the covering pattern; and etching the interlayer insulating pattern doped with ions to form a contact hole. BRIEF DESCRIPTION OF THE DRAWINGS

[0008] Features will become apparent to those skilled in the art by describing in detail exemplary embodiments with reference to the accompanying drawings, in which:

[0009] Figures 1 to 15 shows cross-sectional views of various stages in a method of manufacturing a semiconductor device according to an example embodiment;

[0010] Figure 16 to Figure 17 cross-sectional views showing stages in a method of manufacturing a semiconductor device according to an example embodiment;

[0011] Figures 18 to 21 shows cross-sectional views of various stages in a method of manufacturing a semiconductor device according to an example embodiment;

[0012] Figure 22 to Figure 29 cross-sectional views showing stages in a method of manufacturing a semiconductor device according to example embodiments; and

[0013] Figure 30 to Figure 32 Cross-sectional views illustrating stages in a method of fabricating a semiconductor device according to example embodiments are shown. DETAILED DESCRIPTION

[0014] In each figure, the left portion shows a cross section of a central portion of a gate structure taken along a second direction, and the right portion illustrates a cross section of an active fin portion of a gate structure taken along a first direction. The first and second directions are parallel to the upper surface of the substrate and perpendicular to each other.

[0015] Figures 1 to 15 Cross-sectional views illustrating stages in a method of fabricating a semiconductor device according to example embodiments are shown.

[0016] refer to Figure 1, the upper portion of the substrate 100 may be partially etched to form the trench 102. When the trench 102 is formed on the substrate 100, an active fin 105 may be formed at the substrate 100. An isolation pattern 104 may be formed to fill a lower portion of the trench 102. A preliminary dummy gate structure 114 may be formed on the active fin 105 and the isolation pattern 104. A spacer 116 may be formed on a sidewall of the preliminary dummy gate structure 114.

[0017] The substrate 100 may include a single crystalline semiconductor material, such as silicon, germanium, or silicon germanium. In one embodiment, the substrate 100 may be a silicon-on-insulator (SOI) substrate or a germanium-on-insulator (GOI) substrate.

[0018] In one implementation, the active fins 105 may extend along a first direction and may be arranged along a second direction.

[0019] In one embodiment, to form the isolation pattern 104, an isolation layer may be formed on the substrate 100 to fully fill the trench 102, and the isolation layer may be planarized to expose the upper surface of the substrate 100. Thereafter, the upper portion of the isolation layer may be removed to expose the upper sidewall of the active fin 105. For example, the isolation layer may include an oxide such as silicon oxide.

[0020] The active fin 105 may include a lower active pattern 105b whose sidewall is surrounded by the isolation pattern 104 and an upper active pattern 105a protruding upward from the isolation pattern 104. The upper active pattern 105a may be provided as an active region. A region where the isolation pattern 104 is formed may be provided as a field region.

[0021] The preliminary dummy gate structure 114 may include a dummy gate insulating pattern 108, a dummy gate pattern 110, and a mask pattern 112. Hereinafter, a method for forming the preliminary dummy gate structure 114 will be described more fully.

[0022] A dummy gate insulating layer may be formed on the surface of the upper active pattern 105a. A dummy gate layer may be formed on the dummy gate insulating layer to completely fill the gap between the upper active patterns 105a. The upper surface of the dummy gate layer may be higher than the upper surface of the upper active pattern 105a.

[0023] In one embodiment, the dummy gate insulating layer may include silicon oxide. In one embodiment, the dummy gate insulating layer may be formed by a thermal oxidation process. When the dummy gate insulating layer is formed by a thermal oxidation process, the dummy gate insulating layer may be formed only on the exposed surface of the upper active pattern 105a. In one embodiment, the dummy gate insulating layer may be formed by a chemical vapor deposition process or an atomic layer deposition process. When the dummy gate insulating layer is formed by a chemical vapor deposition process or an atomic layer deposition process, the dummy gate insulating layer may be conformally formed on the upper active pattern 105a and the isolation pattern 104.

[0024] In one embodiment, the dummy gate layer may include polysilicon. In one embodiment, the dummy gate layer may be formed by a chemical vapor deposition process or an atomic layer deposition process.

[0025] A mask pattern 112 is formed on the dummy gate layer. The dummy gate layer and the dummy gate insulating layer may be patterned using the mask pattern 112 as an etching mask to form a preliminary dummy gate structure 114. For example, the mask pattern 112 may include silicon nitride or silicon oxynitride.

[0026] In one implementation, the preliminary dummy gate structure 114 may extend along the second direction, and a plurality of preliminary dummy gate structures 114 may be arranged along the first direction.

[0027] A spacer layer may be formed on the surface of the preliminary dummy gate structure 114, the isolation pattern 104, and the upper active pattern 105a. The spacer layer may be anisotropically etched to form a spacer 116 on the sidewall of the preliminary dummy gate structure 114. The spacer layer may include silicon nitride or silicon oxynitride. In one embodiment, the spacer layer may be formed by a chemical vapor deposition process or an atomic layer deposition process.

[0028] refer to Figure 2 , the upper portion of the active fin 105 between the spacers 116 may be etched to form a first recess 118. An epitaxial pattern 120 may be formed in the first recess 118 to provide a source / drain region.

[0029] For example, the upper portion of the active fin 105 may be removed by a dry etching process using the preliminary dummy gate structure 114 and the spacer 116 formed on the sidewall of the preliminary dummy gate structure 114 as an etching mask to form the first groove 118 .

[0030] In one implementation, the etching process for forming the first recess 118 may be performed in-situ using the etching process for forming the spacer 116 .

[0031] The epitaxial pattern 120 may be formed by performing a selective epitaxial growth (SEG) process using the surface of the active fin 105 (which corresponds to the bottom of the first groove 118) as a seed. In one embodiment, a plurality of epitaxial patterns 120 parallel to each other in the second direction may contact each other at their sidewalls. In one embodiment, after the epitaxial pattern 120 is formed, an impurity implantation process and a heat treatment process may be further performed to form a source-drain region.

[0032] refer to Figure 3 A preliminary first interlayer insulating layer 130 may be formed on the preliminary dummy gate structures 114, the spacers 116, the epitaxial patterns 120, and the isolation patterns 104. The preliminary first interlayer insulating layer 130 may be formed to completely fill gaps between the preliminary dummy gate structures 114 and cover the preliminary dummy gate structures 114.

[0033] The preliminary first interlayer insulating layer 130 may include silicon oxide. The preliminary first interlayer insulating layer 130 may be formed by a chemical vapor deposition process, a spin-on-glass (SOG) process, or an atomic layer deposition process.

[0034] refer to Figure 4 , the preliminary first interlayer insulating layer 130 may be planarized so that the upper surface of the dummy gate pattern 110 (which is included in the preliminary dummy gate structure 114) is exposed. Therefore, a dummy gate structure 114a in which the dummy gate insulating pattern 108 and the dummy gate pattern 110 are deposited may be formed, and a preliminary first interlayer insulating pattern 130a may be formed between the dummy gate structures 114a.

[0035] The planarization process may include a chemical mechanical polishing (CMP) process and / or an etch-back process. The planarization process may remove the mask pattern 112 .

[0036] refer to Figure 5 , the upper portion of the preliminary first interlayer insulating pattern 130a may be etched by the first etching process to form a preliminary second groove 150 having a rounded or rounded shape. Therefore, a preliminary second interlayer insulating pattern 130b having a relatively protruding upper surface may be formed near the spacer 116. For example, a portion of the preliminary second interlayer insulating pattern 130b adjacent to the spacer 116 may protrude in a direction away from the substrate 100, so that a portion of the preliminary second interlayer insulating pattern 130b not adjacent to the spacer 116 is closer to the substrate 100 than a portion of the preliminary second interlayer insulating pattern 130b adjacent to the spacer 116.

[0037] In one embodiment, the preliminary second groove 150 may have a depth greater than 1 / 2 of the depth of the target second groove to be formed. For example, the preliminary second groove 150 may have a depth of 2 / 3 to 9 / 10 of the target depth of the second groove.

[0038] In the first etching process, the preliminary first interlayer insulating pattern 130a including silicon oxide may be largely etched while the spacer 116 including silicon nitride may be hardly etched. The first etching process may be performed such that an etching selectivity between silicon oxide and silicon nitride is relatively high.

[0039] When the upper portion of the preliminary first interlayer insulating pattern 130a is etched by the first etching process, the portion of the preliminary first interlayer insulating pattern 130a adjacent to the spacer 116 may be less etched than the other portions. Therefore, the bottom of the preliminary second groove 150 may not be flat, and the preliminary second groove 150 may have a deeper shape in the central portion along the first direction. Therefore, along the first direction, the upper surface of the preliminary second interlayer insulating pattern 130b may be higher near or adjacent to the spacer 116 than in the central portion.

[0040] In one embodiment, the preliminary second recess 150 may be formed by an etching process without using plasma. The etching gas used to form the preliminary second recess 150 may include, for example, HF and NH 3 .

[0041] The first etching process may include an etching reaction process and a cleaning process or a post-treatment process for removing reaction by-products after the etching reaction process.

[0042] In one embodiment, the etching reaction process and the purification process may be performed in the same chamber. For example, a cycle consisting of the etching reaction process and the purification process may be repeatedly performed to etch the upper portion of the preliminary first interlayer insulating pattern 130a. The etching reaction process and the purification process may be performed at a relatively high temperature and a relatively high pressure.

[0043] In the first etching process, the chamber pressure, the inflow ratio of the etching gas, the number of cycles and the processing time can be appropriately adjusted. In one embodiment, the chamber pressure can be 1.8 to 3 Torr, and the HF and NH 3 The gas ratio may be 2:1 to 20:1, the number of cycles may be 1 to 10, and / or the processing time may be 1 to 10 seconds.

[0044] In one embodiment, the etching reaction process and the purification process may be performed in different chambers. For example, the etching reaction process may be performed at ambient temperature or a temperature of 10° C. to 30° C. at a relatively low pressure, and the purification process may be performed at a temperature higher than that of the etching reaction process.

[0045] refer to Figure 6ions may be implanted on the dummy gate pattern 110, the spacer 116, and the preliminary second groove 150. Thus, an ion implantation region 151 may be formed under upper surfaces of the dummy gate pattern 110, the spacer 116, and the preliminary second interlayer insulating pattern 130b.

[0046] In one embodiment, ions may be implanted in a vertical direction to the surface of the substrate 100 or in a direction tilted at a predetermined angle to the surface of the substrate 100. When ions are implanted in the vertical direction, ions may be implanted into an upper portion of the preliminary second interlayer insulating pattern 130b while being hardly implanted into a sidewall of the spacer 116.

[0047] The ion implantation process may be performed to change the etching characteristics of the spacer 116 and / or the preliminary second interlayer insulating pattern 130b. For example, the ion-doped spacer 116 may have different etching characteristics from the ion-undoped spacer 116. The ion-doped preliminary second interlayer insulating pattern 130b may have different etching characteristics from the ion-undoped preliminary second interlayer insulating pattern 130b.

[0048] In one embodiment, the ions used for the ion implantation process may include, for example, boron, silicon, arsenic, phosphorus, argon, nitrogen, carbon, oxygen, BF 2 , ions of fluorine, hydrogen, helium, germanium, gallium, krypton, xenon, etc.

[0049] In one embodiment, multiple dopants that are different from each other may be used in the ion implantation process. The multiple dopants may be implanted sequentially or together (eg, simultaneously).

[0050] For example, when boron ions are injected, the etching rate of silicon oxide can be reduced, while the etching rate of silicon nitride can be almost unchanged. For example, the etching of silicon oxide can be slowed down, and the etching selectivity between silicon oxide and silicon nitride can be reduced. Therefore, the etching thickness of the preliminary second interlayer insulating pattern 130b can be accurately adjusted, and the protrusion of the preliminary second interlayer insulating pattern 130b can be removed faster. In one embodiment, when silicon ions are injected, the etching rate of silicon nitride can be increased, while the etching rate of silicon oxide can be almost unchanged. Therefore, the etching rate of the preliminary second interlayer insulating pattern 130b can be increased near the spacer 116 including silicon nitride.

[0051] In one embodiment, the ion implantation process may be performed at a temperature of, for example, -100° C. to 600° C. In one embodiment, an annealing process may be further performed after the ion implantation process.

[0052] refer to Figure 7The bottom of the preliminary second groove 150 may be partially etched by the second etching process to form a second groove 150a having a substantially flat bottom. Thus, a first interlayer insulating pattern 130c having a flat upper surface may be formed.

[0053] In one implementation, the preliminary second interlayer insulating pattern 130 b is etched faster by the second etching process in a region adjacent to the spacer 116 than in a region not adjacent to the spacer 116 .

[0054] An etch selectivity between silicon oxide and silicon nitride in the second etch process may be smaller than an etch selectivity between silicon oxide and silicon nitride in the first etch process.

[0055] In one implementation, an etch rate of the spacers 116 may be increased in the second etch process, or an etch rate of the preliminary second interlayer insulating patterns 130 b may be reduced, compared to the first etch process.

[0056] When the etching rate of the spacer 116 is increased, the etching rate of the preliminary second interlayer insulating pattern 130b in the region adjacent to the spacer 116 may become higher than the etching ratio of other regions. Therefore, the bottom of the second groove 150a may be flattened. When the etching rate of the preliminary second interlayer insulating pattern 130b is reduced, the protrusion of the preliminary second interlayer insulating pattern 130b may be etched faster than other portions. Therefore, the bottom of the second groove 150a may be flattened.

[0057] In one embodiment, the second groove 150a may be formed by an etching process without using plasma. The etching gas used to form the second groove 150a may include HF and NH 3 .

[0058] In one embodiment, the chamber pressure may be 1.8 to 3 Torr, and the HF and NH 3 The gas ratio may be 2:1 to 20:1, the number of cycles may be 1 to 10, and / or the process time may be 1 to 10 seconds.

[0059] In one implementation, the second etching process may be performed under the same conditions as the first etching process.

[0060] In one embodiment, the second etching process may be performed under different conditions from the first etching process. For example, when silicon ions or carbon ions are implanted in the previous process, the HF and NH 3 The gas ratio can be increased and the chamber pressure can be increased to reduce the silicon oxide etch rate.

[0061] When the second etching process is performed, the upper portion of the spacer 116 may be partially etched so that the height of the spacer 116 may be reduced.

[0062] refer to Figure 8 A capping layer may be formed on the dummy gate pattern 110, the spacer 116, and the first interlayer insulating pattern 130c to completely fill the second groove 150a. Thereafter, the capping layer may be planarized so that the upper surfaces of the dummy gate pattern 110 and the spacer 116 are exposed, so that a preliminary first capping pattern 132a is formed in the second groove 150a.

[0063] The capping layer may include silicon nitride. The capping layer may be formed by a chemical vapor deposition process or an atomic layer deposition process.

[0064] Because the bottom of the second groove 150a is flat, the bottom surface of the preliminary first capping pattern 132a may be flat. Therefore, the first interlayer insulating pattern 130c may be hardly interposed between the preliminary first capping pattern 132a and the spacer 116. In one embodiment, the lateral thickness of the first interlayer insulating pattern 130c between the preliminary first capping pattern 132a and the spacer 116 may be equal to or less than 3nm.

[0065] If the second groove has a rounded bottom (unlike the above-described example embodiment), the first interlayer insulating pattern may be inserted between the preliminary first covering pattern and the spacer. Therefore, the preliminary first covering pattern may have a very thin vertical thickness near or adjacent to the sidewall of the spacer. Therefore, the preliminary first covering pattern in the region adjacent to the sidewall of the spacer may be completely removed by subsequent processes. Therefore, the first interlayer insulating pattern under the preliminary first covering pattern may be exposed and may be over-etched.

[0066] However, in example embodiments, the preliminary first capping pattern 132a may have a flat bottom surface. Therefore, the preliminary first capping pattern 132a may not have a thinner portion with a smaller vertical thickness, and may have a uniform vertical thickness throughout the entire portion. Therefore, in subsequent processes, the first interlayer insulating pattern 130c may be sufficiently protected by the preliminary first capping pattern 132a.

[0067] refer to Fig. 9 , the dummy gate pattern 110 may be removed, and the dummy gate insulating pattern 108 under the dummy gate pattern 110 may be removed. Thus, an opening 135 may be formed to expose the surface of the active fin 105. The structure including the opening 135 may be provided as a mold for forming a gate structure. The removal process may include an isotropic etching process.

[0068] The spacer 116 and the preliminary first capping pattern 132a may be partially etched during the formation of the opening 135. Thus, a preliminary second capping pattern 132b having a smaller or reduced height relative to the preliminary first capping pattern 132a may be formed.

[0069] The preliminary second covering pattern 132b may completely cover the upper surface of the first interlayer insulating pattern 130c so that no portion of the first interlayer insulating pattern 130c may be exposed. Therefore, in the process of removing the dummy gate insulating pattern 108, the preliminary second covering pattern 132b may protect the first interlayer insulating pattern 130c so that the first interlayer insulating pattern 130c may not be removed or damaged.

[0070] If the preliminary first covering pattern does not have a flat bottom surface (unlike the example embodiment), the preliminary second covering pattern may be partially removed in the process of forming the opening to expose a portion of the first interlayer insulating pattern. The dummy gate insulating layer and the first interlayer insulating pattern may be formed of silicon oxide, and when the dummy gate insulating layer is removed, the exposed first interlayer insulating pattern may be overetched. Therefore, a deep recess may be formed at the upper surface of the first interlayer insulating pattern.

[0071] refer to Fig.10 , a preliminary gate structure 137 may be formed in the opening 135 .

[0072] For example, a thermal oxidation process may be performed on the upper surface of the active fin 105 exposed through the opening 135 to form an interface layer. A gate insulating layer may be conformally formed on the interface layer, the isolation pattern 104, the spacer 116, and the preliminary second capping pattern 132b. A gate electrode layer may be formed on the gate insulating layer to completely fill the opening 135. Thereafter, the gate electrode layer may be planarized so that the upper surface of the preliminary second capping pattern 132b is exposed. Thus, a preliminary gate structure 137 may be formed in which a preliminary gate insulating pattern 134 and a preliminary gate electrode 136 are deposited.

[0073] The gate insulating layer may include a metal oxide having a higher dielectric constant than silicon nitride. In one embodiment, the gate insulating layer may include, for example, hafnium oxide (HfO 2 ), Tantalum Oxide (Ta 2 O 5 )、ZrO 2 ) etc. The gate insulating layer may be formed by a chemical vapor deposition process or an atomic layer deposition process.

[0074] For example, the gate electrode layer may include a metal such as tungsten, aluminum, copper, tantalum, or titanium, or a nitride thereof. The gate electrode layer may be formed by a chemical vapor deposition process, an atomic layer deposition process, or a physical vapor deposition process.

[0075] refer to Fig.11The preliminary gate insulating pattern 134 and the preliminary gate electrode 136 disposed in the upper portion of the opening 135 may be partially etched to form a third groove 138. Thus, a gate insulating pattern 134a and a gate electrode 136a may be formed in the lower portion of the opening 135.

[0076] In the etching process, the spacer 116 and the preliminary second capping pattern 132b may be partially etched. Thus, the first capping pattern 132c having a height smaller than the preliminary second capping pattern 132b may be formed.

[0077] The first capping pattern 132c may completely cover the first interlayer insulating pattern 130c so that no portion of the first interlayer insulating pattern 130c may be exposed. In addition, no recess may be formed at the upper surface of the first interlayer insulating pattern 130c. Therefore, when the gate insulating pattern 134a and the gate electrode 136a are formed, the first capping pattern 132c may protect the first interlayer insulating pattern 130c.

[0078] refer to Fig.12 , a hard mask layer may be formed on the gate insulating pattern 134a, the gate electrode 136a, and the first capping pattern 132c to fill the third groove 138. Thereafter, the hard mask layer may be planarized so that the upper surface of the first interlayer insulating pattern 130c is exposed to form a first hard mask 140. The first capping pattern 132c may be completely removed by the planarization process.

[0079] Thus, a gate structure 142 may be formed in which the gate insulating pattern 134 a , the gate electrode 136 a , and the first hard mask 140 are deposited in the opening 135 .

[0080] In one embodiment, the hard mask layer may include silicon nitride. The hard mask layer may be formed by a chemical vapor deposition process or an atomic layer deposition process.

[0081] If a recess is to be formed at the upper surface of the first interlayer insulating pattern (unlike the example embodiment), the hard mask layer may partially remain in the recess after the polishing process.

[0082] However, in example embodiments, recesses may not be formed at upper surfaces of the first interlayer insulating patterns 130 c , and the hard mask layer may not remain on the first interlayer insulating patterns 130 c after the polishing process.

[0083] refer to Fig.13 , an etch mask pattern 144 may be formed on the first interlayer insulating pattern 130c and the first hard mask 140. The first interlayer insulating pattern 130c may be etched using the etch mask pattern 144 so that an upper portion of the epitaxial pattern 120 is exposed. Thus, a contact hole 146 may be formed between the gate structures 142.

[0084] The etching mask pattern 144 may include an opening exposing a portion of the first interlayer insulating pattern 130 c for forming a contact hole. The gate structure 142 may also be exposed through the opening.

[0085] In the etching process, the first interlayer insulating pattern 130c between the spacers 116 may be selectively etched. However, when the etching process is performed, the first hard mask 140 formed of silicon nitride and the spacers 116 may be partially etched. Therefore, the upper width of the contact hole 146 may be greater than the lower width thereof. The portion of the contact hole 146 having a relatively large width may be disposed higher than the upper surface of the gate electrode 136a.

[0086] When performing the etching process, if the hard mask layer remains on the first interlayer insulating pattern 130c (unlike the example embodiment), the first interlayer insulating pattern 130c may remain unetched under the hard mask layer. Thus, the contact hole may not expose the epitaxial pattern. Therefore, the contact hole may not be opened, resulting in a contact non-open defect.

[0087] However, in example embodiments, the hard mask layer may not remain on the first interlayer insulating pattern 130c. Therefore, contact non-open defects may be reduced.

[0088] Thereafter, the etch mask pattern 144 may be removed.

[0089] refer to Fig.14 , a conductive layer 148 may be formed on the first hard mask 140 , the spacer 116 , and the first interlayer insulating pattern 130 c to completely fill the contact hole 146 .

[0090] In one implementation, the conductive layer 148 may include a metal such as tungsten, copper, aluminum, etc. The conductive layer 148 may be formed by a chemical vapor deposition process, an atomic layer deposition process, or a physical vapor deposition process.

[0091] refer to Fig.15 , the conductive layer 148 may be planarized so that the upper surface of the first hard mask 140 is exposed to form a contact plug 148a in the contact hole 146. Through the above process, a fin field effect transistor may be formed.

[0092] As described above, the second groove 150a may have a flat bottom, and the bottom surface of the first capping pattern 132c may be flat. Therefore, when performing a process for forming the gate structure 142, the first capping pattern 132c may remain to protect the first interlayer insulating pattern 130c under the first capping pattern 132c. Therefore, when a contact plug is formed by etching the first interlayer insulating pattern 130c, a contact non-open defect may be reduced.

[0093] In addition, when performing the process for forming the gate structure 142, the first interlayer insulating pattern 130c may be hardly consumed. Therefore, the height of the dummy gate structure 114a can be reduced. Therefore, the thickness of the first interlayer insulating pattern 130c to be etched to form the contact hole 146 can be reduced. Therefore, the polishing thickness of the conductive layer 148 in the planarization process for forming the contact plug 148a can be reduced.

[0094] Fig.16 and Fig.17 Cross-sectional views illustrating stages in a method of fabricating a semiconductor device according to example embodiments are shown.

[0095] The method for manufacturing a semiconductor device may be the same as previously described with reference to the prior art except for the process for forming the second groove. Figures 1 to 15 The method of explanation is basically the same.

[0096] like Figure 5 As shown in , this can be done by executing the same Figures 1 to 5 A process substantially the same as or similar to the illustrated process forms a preliminary second interlayer insulating pattern 130 b having a rounded bottom between the spacers 116 on the dummy gate structure 114 a .

[0097] refer to Fig.16 , ions may be implanted on the dummy gate pattern 110 and the spacer 116. Thus, an ion implantation region 151 may be formed at a surface portion of the dummy gate pattern 110 and the spacer 116.

[0098] In one embodiment, ions may be mainly doped on the sidewalls of the spacers 116 and hardly doped on the preliminary second interlayer insulating pattern 130b. In one embodiment, ions may be implanted in a direction inclined at a predetermined angle to the surface of the substrate 100. For example, the ion implantation angle may be -45° to 45°.

[0099] The ion implantation process may be performed to change the etching characteristics of the spacers 116. For example, the spacers 116 doped with ions may have different etching characteristics from the spacers 116 not doped with ions.

[0100] In one embodiment, the ions and temperature in the ion implantation process may be the same as previously described. Figure 6 Those described are essentially the same.

[0101] In one embodiment, multiple dopants that are different from each other may be used in the ion implantation process. The dopants may be implanted sequentially or simultaneously.

[0102] In one implementation, an annealing process may be further performed after the ion implantation process.

[0103] refer to Fig.17 , the bottom of the preliminary second groove 150 may be etched by a second etching process to form a second groove 150a having a substantially flat bottom. Thus, a first interlayer insulating pattern 130c having a flat upper surface may be formed.

[0104] In one implementation, the second etching process may etch the preliminary second interlayer insulating pattern 130b in a region adjacent to the spacer 116 faster than in a region not adjacent to the spacer 116. Thus, the bottom of the second recess 150a may become substantially flat.

[0105] An etch selectivity between silicon oxide and silicon nitride in the second etch process may be smaller than an etch selectivity between silicon oxide and silicon nitride in the first etch process.

[0106] In one embodiment, the process conditions may be adjusted so that the etching rate of the spacer 116 may be increased in the second etching process or the etching rate of the preliminary second interlayer insulating pattern 130b may be reduced compared to the first etching process. In one embodiment, the second etching process may be performed under the same conditions as the first etching process.

[0107] Afterwards, the same procedure as previously referenced can be performed Figures 8 to 15 Thus, a fin field effect transistor can be formed.

[0108] Figures 18 to 21 Cross-sectional views illustrating stages in a method of fabricating a semiconductor device according to example embodiments are shown.

[0109] The method for manufacturing a semiconductor device may be the same as previously described with reference to the prior art except for the process for forming the second groove. Figures 1 to 15 The method of explanation is basically the same.

[0110] like Figure 4 As shown in , this can be done by executing the same Figures 1 to 4 The process described above is substantially the same as or similar to that described above to form a preliminary first interlayer insulating pattern 130 a filling a gap between the spacers 116 on the dummy gate structure 114 a .

[0111] refer to Fig.18 , an upper portion of the preliminary first interlayer insulating pattern 130a may be partially etched to form a preliminary second groove 152 having a rounded bottom. Thus, a preliminary second interlayer insulating pattern 131a having a protrusion adjacent to the spacer 116 may be formed.

[0112] In one embodiment, the depth of the preliminary second groove 152 may be less than 1 / 2 of the depth of the target second groove to be formed. For example, the preliminary second groove 152 may have a depth of 1 / 3 to 1 / 2 of the target depth of the second groove. The etching process may be the same as previously described with reference to Figure 5 The process described is essentially the same.

[0113] Thereafter, ions may be implanted on the dummy gate pattern 110, the spacer 116, and the preliminary second groove 152. Thus, an ion implantation region 151a may be formed under upper surfaces of the dummy gate pattern 110, the spacer 116, and the preliminary second interlayer insulating pattern 131a.

[0114] In one embodiment, the ion implantation process may be similar to that described previously with reference to Figure 6 The process described is essentially the same.

[0115] In one embodiment, the ion implantation process may be similar to that described previously with reference to Fig.16 Therefore, an ion implantation region may be formed only at the upper surface of the dummy gate pattern 110 and on the exposed sidewalls of the spacer 116 .

[0116] refer to Fig.19 , the bottom of the preliminary second groove 152 may be partially etched to form a preliminary third groove 152a having a substantially flat bottom. Thus, a preliminary third interlayer insulating pattern 131b having a flat upper surface may be formed.

[0117] In one embodiment, the etching process can be similar to that previously described with reference to Figure 7 The process described is essentially the same.

[0118] refer to Fig. 20 , the upper portion of the preliminary third interlayer insulating pattern 131b may be partially etched to form a preliminary fourth groove 152b having a round bottom. Thus, a preliminary fourth interlayer insulating pattern 131c protruding near the spacer 116 may be formed.

[0119] In one embodiment, the depth of the preliminary fourth groove 152b may be greater than 1 / 2 of the depth of the target second groove to be formed. For example, the preliminary fourth groove 152b may have a depth of 2 / 3 to 9 / 10 of the target depth of the second groove. The etching process may be the same as previously described. Figure 5 The process described is essentially the same.

[0120] Thereafter, ions may be implanted on the dummy gate pattern 110, the spacer 116, and the preliminary fourth groove 152b. Thus, an ion implantation region 151a may be formed under upper surfaces of the dummy gate pattern 110, the spacer 116, and the preliminary fourth interlayer insulating pattern 131c.

[0121] In one embodiment, the ion implantation process may be similar to that described previously with reference to Figure 6 The process described is essentially the same.

[0122] In one embodiment, the ion implantation process may be similar to that described previously with reference to Fig.16 The process described is essentially the same.

[0123] refer to Fig.21 , the bottom of the preliminary fourth groove 152b may be etched to form the second groove 150a having a substantially flat bottom. Thus, the first interlayer insulating pattern 130c having a flat upper surface may be formed.

[0124] In one embodiment, the etching process can be similar to that previously described with reference to Figure 7 The process described is essentially the same.

[0125] In one implementation, an etching process for forming the preliminary groove, an ion implantation process, and an etching process for forming the groove having a flat bottom may be repeatedly performed through a plurality of cycles to form the second groove 150 a .

[0126] Thereafter, the process is the same as previously referenced Figures 8 to 15 The described processes are basically the same. Thus, a fin field effect transistor can be formed.

[0127] Figure 22 to Figure 29 Cross-sectional views illustrating stages in a method of fabricating a semiconductor device according to example embodiments are shown.

[0128] A plurality of gate structures 142, spacers 116, and first interlayer insulating patterns 130c may be formed on the substrate 100. The spacers 116 may be disposed on sidewalls of the gate structures 142. The first interlayer insulating patterns 130c may fill gaps between the spacers 116.

[0129] In one embodiment, the same method as previously referenced may be performed. Figures 1 to 12 The gate structure 142, the spacer 116, and the first interlayer insulating pattern 130c are formed by performing a process substantially the same as or similar to the process described above. Fig.16 and Fig.17 The process described or previously referenced Figures 18 to 21 The gate structure 142, the spacer 116, and the first interlayer insulating pattern 130c are formed by the illustrated process.

[0130] refer to Fig. 22 and Fig.23An etch mask pattern 160 may be formed on the gate structure 142, the spacer 116, and the first interlayer insulating pattern 130c. The first interlayer insulating pattern 130c may be partially etched using the etch mask pattern 160 to form an insulating pattern 161 on the substrate 100. A preliminary opening 162 may be formed on the insulating pattern 161.

[0131] In one implementation, the etch mask pattern 160 may have a shape that exposes the first interlayer insulating pattern 130 c in a region where the contact hole is not formed, and covers the first interlayer insulating pattern 130 c in a region where the contact hole is formed.

[0132] When the etching process is performed, the first hard mask 140 and the spacer 116 in the region exposed by the etch mask pattern 160 may be partially etched.

[0133] After the etching process, the etch mask pattern 160 may be removed.

[0134] refer to Fig.24 , a capping layer 164 may be formed on the first interlayer insulating pattern 130 c and the first hard mask 140 to fill the preliminary opening 162 .

[0135] In one embodiment, the capping layer 164 may include silicon nitride. The capping layer 164 may be formed by a chemical vapor deposition process or an atomic layer deposition process.

[0136] refer to Fig.25 , the capping layer 164 may be planarized so that the upper surface of the first interlayer insulating pattern 130c is exposed to form a second capping pattern 164a.

[0137] Therefore, the insulating pattern 161 and the second capping pattern 164a may be deposited in a region where a contact hole is not formed. In addition, the first interlayer insulating pattern 130c may remain in a region where a contact hole will be formed in a subsequent process.

[0138] refer to Fig.26 , ions may be implanted on the first interlayer insulating pattern 130c and the second capping pattern 164a. Thus, an ion implantation region may be formed in a region adjacent to upper surfaces of the first interlayer insulating pattern 130c and the second capping pattern 164a.

[0139] The ion implantation process may be performed to change the etching characteristics of the first interlayer insulating pattern 130c and / or the second capping pattern 164a. In an example embodiment, the etching selectivity between silicon oxide and silicon nitride may be increased by the ion implantation process so that the first interlayer insulating pattern 130c may be selectively etched in a subsequent process.

[0140] Furthermore, the ion implantation process may remove a seam that may be generated in the second capping pattern 164 a .

[0141] In one embodiment, ions may be implanted in a direction perpendicular to the surface of the substrate 100. In one embodiment, ions may be implanted in a direction inclined to the surface of the substrate 100. For example, the ion implantation angle may be -45° to 45°.

[0142] In one embodiment, the ions and temperature in the ion implantation process may be the same as previously described. Figure 6 Those described are essentially the same.

[0143] In one embodiment, multiple dopants that are different from each other may be used in the ion implantation process. The dopants may be implanted sequentially or simultaneously.

[0144] In addition, an annealing process may be further performed after the ion implantation process.

[0145] refer to Fig. 27 , the first interlayer insulating pattern 130c may be partially etched to form the preliminary first contact hole 166. The first interlayer insulating pattern 130c may partially remain on the bottom of the preliminary first contact hole 166.

[0146] The second capping pattern 164a may not include a seam. In addition, the second capping pattern 164a may be hardly etched in the etching process. Therefore, over-etching of the second capping pattern 164a (due to the seam) may be prevented in the etching process.

[0147] refer to Fig.28 , the first interlayer insulating pattern 130c remaining on the bottom of the preliminary first contact hole 166 may be etched to form a first contact hole 166a. A surface of the epitaxial pattern 120 may be exposed at the bottom of the first contact hole 166a.

[0148] refer to Fig.29 , a contact plug 170 may be formed in the first contact hole 166a. The process for forming the contact plug 170 may be the same as previously described with reference to Fig.13 The described processes are basically the same. Thus, a fin field effect transistor can be formed.

[0149] Figure 30 to Figure 32 Cross-sectional views illustrating stages in a method of fabricating a semiconductor device according to example embodiments are shown.

[0150] A plurality of gate structures 142, spacers 116, and first interlayer insulating patterns 130c may be formed on the substrate 100. The spacers 116 may be disposed on sidewalls of the gate structures 142. The first interlayer insulating patterns 130c may fill gaps between the spacers 116.

[0151] In one embodiment, the same method as previously referenced may be performed. Figures 1 to 12 The gate structure 142, the spacer 116, and the first interlayer insulating pattern 130c are formed by performing a process substantially the same as or similar to the process described above. Fig.16 and Fig.17 Process described or previous reference Figures 18 to 21 The gate structure 142, the spacer 116, and the first interlayer insulating pattern 130c are formed by the illustrated process.

[0152] Afterwards, the Figure 22 to Figure 25 The insulating pattern 161 and the second capping pattern 164a are deposited in a region where the contact hole is not formed, in the same process as described above.

[0153] refer to Fig.30 , the first interlayer insulating pattern 130c may be partially etched to form the preliminary first contact hole 166. The first interlayer insulating pattern 130c may partially remain on the bottom of the preliminary first contact hole 166.

[0154] Sidewalls of the spacers 116 may be exposed through the preliminary first contact holes 166 .

[0155] refer to Fig.31 ions may be implanted on the sidewalls of the first interlayer insulating pattern 130 c , the first hard mask 140 , the second capping pattern 164 a , and the spacer 116 exposed by the preliminary first contact hole 166 .

[0156] In one implementation, ions may be implanted in a direction inclined to the surface of the substrate 100. For example, the ion implantation angle may be -45° to 45°.

[0157] In one implementation, ions may be implanted onto the sidewalls of the spacers 116 exposed through the preliminary first contact holes 166, while ions may be hardly implanted onto the first interlayer insulating patterns 130c. The ion implantation process may be performed to change etching characteristics of the spacers 116 and the first hard mask 140. For example, the spacers 116 doped with ions may have different etching characteristics from the spacers 116 not doped with ions.

[0158] In one implementation, ions may be implanted in a direction perpendicular to the surface of the substrate 100. Thus, an ion implantation region may be formed under upper surfaces of the first interlayer insulating pattern 130c and the first hard mask 140.

[0159] In one embodiment, the ions and temperature in the ion implantation process may be the same as previously described. Figure 6 Those described are essentially the same.

[0160] In one embodiment, multiple dopants that are different from each other may be used in the ion implantation process. The dopants may be implanted sequentially or simultaneously.

[0161] In one implementation, an annealing process may be further performed after the ion implantation process.

[0162] refer to Fig.32 , the first interlayer insulating pattern 130c remaining on the bottom of the preliminary first contact hole 166 may be etched to form a first contact hole 166a. A surface of the epitaxial pattern 120 may be exposed at the bottom of the first contact hole 166a.

[0163] In the etching process for forming the first contact hole 166a, the second capping pattern 164a may be hardly etched. Therefore, over-etching of the second capping pattern 164a may be prevented in the etching process.

[0164] Afterwards, the same Fig.13 A contact plug is formed in the first contact hole 166a by the same process as described above.

[0165] As described above, the semiconductor device according to example embodiments may be used for a memory device or a logic device including a transistor.

[0166] Embodiments may provide a method of manufacturing a semiconductor device including a transistor.

[0167] Embodiments may provide a method of manufacturing a semiconductor device including a fin field effect transistor having high performance.

[0168] According to example embodiments, a semiconductor device including a fin field effect transistor having excellent electrical characteristics may be manufactured.

[0169] Example embodiments have been disclosed herein, and although specific terms are employed, they are used and interpreted in a general and descriptive sense only, and not for purposes of limitation. In some cases, as will be apparent to one of ordinary skill in the art when filing this application, features, characteristics, and / or elements described in conjunction with a particular embodiment may be used alone or in combination with features, characteristics, and / or elements in other embodiments, unless otherwise specifically noted. Therefore, it will be understood by those skilled in the art that various changes in form and detail may be made without departing from the spirit and scope of the invention as set forth in the appended claims.

Claims

1. A method for manufacturing a semiconductor device, the method include: forming a dummy gate structure on the substrate; forming spacers on sidewalls of the dummy gate structure; forming a preliminary first interlayer insulating pattern to fill gaps between adjacent spacers; etching an upper portion of the preliminary first interlayer insulating pattern by a first etching process to form a preliminary second interlayer insulating pattern; implanting ions on the dummy gate structure, the spacer, and the preliminary second interlayer insulating pattern through an ion implantation process; etching an upper portion of the preliminary second interlayer insulating pattern by a second etching process to form an interlayer insulating pattern having a flat upper surface; as well as forming a capping pattern on the interlayer insulating pattern to fill the gaps between the spacers, The etching selectivity between silicon oxide and silicon nitride in the second etching process is smaller than the etching selectivity between silicon oxide and silicon nitride in the first etching process.

2. The method according to claim 1, in, An upper surface of the preliminary second interlayer insulating pattern has a shape in which a region of the upper surface of the preliminary second interlayer insulating pattern adjacent to the spacer protrudes more than a region of the upper surface of the preliminary second interlayer insulating pattern away from the spacer in a direction away from the substrate.

3. The method according to claim 1, in, The etching gas used in each of the first etching process and the second etching process includes HF and NH 3 .

4. The method according to claim 3, in, In each of the first etching process and the second etching process: The chamber pressure is 1.8 torr to 3 torr, HF and NH 3 The gas ratio is 2:1 to 20:1, The number of cycles ranges from 1 to 10, and The processing time is from 1 to 10 seconds.

5. The method according to claim 1, in, The ions implanted in the ion implantation process include boron, silicon, arsenic, phosphorus, argon, nitrogen, carbon, oxygen, BF 2 , fluorine, hydrogen, helium, germanium, gallium, krypton or xenon ions.

6. The method according to claim 1, in, The ion implantation process includes sequentially or simultaneously implanting a plurality of ions different from each other.

7. The method according to claim 1, in, The ion implantation process includes forming an ion implantation region below surfaces of the dummy gate structure and the preliminary second interlayer insulating pattern.

8. The method according to claim 1, in, The ion implantation process includes forming an ion implantation region below a surface of the dummy gate structure and at a sidewall of the spacer.

9. The method according to claim 1, in, An etching characteristic of at least one of the preliminary second interlayer insulating pattern and the spacer is changed by the ion implantation process.

10. The method according to claim 1, in, Before forming the capping pattern, the first etching process, the ion implantation process, and the second etching process are repeated through a plurality of cycles. 11 . The method of claim 1 , further comprising replacing the dummy gate structure with a gate structure after forming the capping pattern.

12. The method according to claim 11, in, Replacing the dummy gate structure with the gate structure includes: removing the dummy gate structure to form an opening; forming a gate structure layer in the opening and on the capping pattern; and The gate structure layer and the capping pattern are planarized so that the interlayer insulating pattern is exposed to form the gate structure in the opening.

13. The method of claim 11, further comprising forming a contact plug between the gate structures.

14. A method for manufacturing a semiconductor device, the method include: forming a dummy gate structure on the substrate; forming a preliminary first interlayer insulating pattern to fill the gaps between the dummy gate structures; etching an upper portion of the preliminary first interlayer insulating pattern by a first etching process to form a preliminary groove having a round bottom and a preliminary second interlayer insulating pattern under the preliminary groove; implanting ions on the dummy gate structure and the preliminary second interlayer insulating pattern; etching a portion of the preliminary second interlayer insulating pattern by a second etching process to form a groove having a flat bottom and an interlayer insulating pattern below the groove; forming a capping pattern on the interlayer insulating pattern; as well as replacing the dummy gate structure with a gate structure, The etching selectivity between silicon oxide and silicon nitride in the second etching process is smaller than the etching selectivity between silicon oxide and silicon nitride in the first etching process.

15. The method of claim 14, in, Replacing the dummy gate structure with the gate structure includes: removing the dummy gate structure to form an opening; forming a gate structure layer in the opening and on the capping pattern; and The gate structure layer and the capping pattern are planarized so that the interlayer insulating pattern is exposed to form the gate structure in the opening.

16. A method for manufacturing a semiconductor device, the method include: forming a gate structure on a substrate; forming a preliminary interlayer insulating pattern including silicon oxide to fill the gaps between the gate structures; forming a mask pattern on the gate structure and the preliminary interlayer insulating pattern to cover a contact forming region; partially etching an upper portion of the preliminary interlayer insulating pattern using the mask pattern as an etching mask to form a groove and an interlayer insulating pattern below the groove; forming a capping pattern including silicon nitride on the interlayer insulating pattern to fill the groove; implanting ions on the gate structure, the interlayer insulating pattern, and the capping pattern so that the etching selectivity between silicon oxide and silicon nitride is increased; and The interlayer insulating pattern doped with ions is etched to form a contact hole. 17 . The method of claim 16 , further comprising etching a portion of the interlayer insulating pattern before implanting the ions.

18. The method of claim 16, in, The ions include boron, silicon, arsenic, phosphorus, argon, nitrogen, carbon, oxygen, BF 2 , fluorine, hydrogen, helium, germanium, gallium, krypton or xenon ions.

Citation Information

Patent Citations

  • Methods of manufacturing a semiconductor device

    KR1020190061358A

  • Method for forming gate of semiconductor device

    CN101604628A

  • Method for manufacturing semiconductor device

    CN106128958A

  • Semiconductor devices and methods of manufacturing the same

    CN107068565A

  • Semiconductor devices and methods of manufacturing the same

    US20150364574A1