A semiconductor discharge tube with negative resistance characteristics and a manufacturing method thereof
By using an N-type diffusion sheet substrate and doping process in the semiconductor discharge tube, P2 and P1 regions are prepared, combined with thinning treatment, a negative resistance characteristic semiconductor discharge tube is formed, which solves the residual pressure high and surge capacity in the prior art. The problem of insufficient results has achieved better surge protection.
Patent Information
- Application Number
- CN201910965826.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-07-01
- Filing Date
- 2019-10-12
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2039-10-12
AI Technical Summary
The existing semiconductor discharge tubes are difficult to achieve negative resistance characteristics in structural design, resulting in high residual voltage, unable to effectively protect the subsequent circuit, and insufficient surge capacity, making it impossible to adapt to a harsh interference environment.
Using an N-type diffusion sheet substrate, the P2 region, P1 region and N1 region are prepared on one side of the substrate through doping process, and the front metal electrode is prepared on the P1 region side. Combined with thinning treatment and metal contact, the negative resistance characteristics are formed. semiconductor discharge tube structure.
It realizes reducing residual voltage and improving surge capacity, so that the device more effectively protects the later-stage circuit when protecting lightning surges, and is suitable for applications with higher surge levels.
Smart Images

Figure CN111223914B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of semiconductor technology, and particularly relates to a method for manufacturing a semiconductor discharge tube with negative resistance characteristics and the semiconductor discharge tube. Background Art
[0002] At present, semiconductor discharge tube (Thyristor Surge Suppresser) is also called: protective thyristor surge suppression thyristor, thyristor surge suppressor, surge suppression thyristor, TSS, solid discharge tube. It is an overvoltage protection device made based on the principle of thyristor. It relies on the breakdown current of the PN junction to trigger the device to conduct and discharge, and a large surge current or pulse current can flow through it. The device itself absorbs surge energy to protect the subsequent circuit from surge damage. The device has been widely used in communication ports and signal ports. Strong surge capability and low residual voltage are the direction of device optimization.
[0003] Improving surge capacity can effectively protect devices from being damaged when subjected to more severe surge interference. Low residual voltage can better eliminate the impact of surge on the subsequent circuit and prevent the back-end circuit from being damaged by residual voltage. At present, when the industry uses diffusers to produce TSS devices, the structure is usually N1P1N2P2 structure (such as Figure 1 ) or P 2 1N 2 1P 2 2N 2 2 Structure (such as Figure 2 ). Among them, N2(P 2 2) The structure is realized by using the original substrate doping. Due to the limitations of the thinning process and diffusion process, N2 (P 2 2) The thickness of the region cannot be very thin, and is generally greater than the minority carrier diffusion length. Due to the long length of the base region, it is difficult for the device to produce a negative resistance effect. This causes the device residual voltage to be high, and the subsequent circuit cannot be well protected. The negative resistance effect can effectively reduce the residual voltage. And according to the semiconductor thermal burnout theory, when a large current is injected, the negative resistance device has a smaller equivalent resistance, and the larger the surge current that can pass through. From the perspective of surge capacity and residual voltage, the stronger the negative resistance characteristic, the better the surge capacity and the lower the residual voltage.
[0004] Therefore, in view of the shortcomings of the above scheme in actual production and implementation, it is modified and improved. At the same time, in the spirit and concept of seeking for excellence, with the assistance of professional knowledge and experience, and after many ingenuity and experiments, the present invention is created, and a method for manufacturing a semiconductor discharge tube with negative resistance characteristics is provided, which can achieve the purpose of reducing residual voltage and improving surge capacity. Summary of the invention
[0005] The invention provides a method for manufacturing a semiconductor discharge tube with negative resistance characteristics, which solves the problems in the prior art.
[0006] The technical solution of the present invention is achieved in this way:
[0007] A semiconductor discharge tube with negative resistance characteristics, characterized in that it includes: a substrate, a P2 region, an N1 region, a P1 region, a front metal electrode, and a back metal electrode; the P2 region is prepared by using a doping process on one side of the substrate; the N1 region is prepared by using a doping process on one side of the P2 region; the P1 region is prepared by using a doping process on one side of the N1 region; the front metal electrode is prepared on one side of the P1 region; and the back metal electrode is prepared by performing a metal contact process on the back side of the substrate after a thinning process.
[0008] The substrate is an N-type diffusion sheet substrate.
[0009] The P1 region, the N1 region and the P2 region are located on the same side of the N-type diffusion sheet substrate.
[0010] The thickness of the P2 region is between 0-30 μm, and the width of the P2 region is smaller than the minority carrier diffusion length of the P2 region.
[0011] The thickness of the substrate after thinning is between 120 μm and 180 μm.
[0012] The method for manufacturing the semiconductor discharge tube having negative resistance characteristics comprises:
[0013] S1: Cutting and unloading the wafer, selecting the substrate;
[0014] S2: P2 region preparation, using a doping process to prepare the P2 region on one side of the substrate;
[0015] S3: Preparation of N1 region: using doping process, N1 region is prepared on one side of P2 region;
[0016] S4: P1 region preparation, using a doping process to prepare the P1 region on one side of the N1 region;
[0017] S5: Prepare the front metal electrode on one side of the P1 area;
[0018] S6: Thinning treatment, thinning the original substrate;
[0019] S7: Performing metal contact processing on the back side of the thinned substrate to produce a back electrode.
[0020] The doping process includes an implantation process and / or a diffusion process.
[0021] In step S5, a front metal electrode is prepared on one side of the P1 region, and NH3 is used to repair the electrode surface morphology.
[0022] In step S7, metal contact treatment is performed on the back side of the thinned substrate, and NH3 is used to repair the surface morphology of the electrode.
[0023] The thinning process in step S6 includes a method of thinning by film sticking, and the film is thinned to a thickness of 120 μm.
[0024] After adopting the above technical solution, the beneficial effect of the present invention is that when the discharge tube device made by the method of the present invention protects against lightning surge, the lower residual voltage is conducive to better protection of the subsequent circuit. The high surge capacity can make the device suitable for higher surge level requirements. The present invention uses the N-type thin film short base region negative resistance longitudinal process to achieve the purpose of reducing the residual voltage and improving the surge capacity. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0026] Figure 1 : Traditional diffuser process cross-sectional structure diagram (N1P1N2P2 structure);
[0027] Figure 2 : Traditional diffuser process cross-sectional structure diagram (P21N21P22N22 structure);
[0028] Figure 3 : An example of a cross-sectional view of a semiconductor discharge tube with negative resistance characteristics;
[0029] Figure 4 : A cross-sectional view of a semiconductor discharge tube with negative resistance characteristics is shown in Figure 1;
[0030] Figure 5 : A cross-sectional view of a semiconductor discharge tube with negative resistance characteristics is shown in Figure 1;
[0031] Figure 6 : A cross-sectional view of a semiconductor discharge tube with negative resistance characteristics is shown in Figure 1;
[0032] Figure 7 : Schematic diagram of the diffusion sheet feeding and cutting;
[0033] Figure 8 : Cross-sectional view of P2 area after preparation;
[0034] Fig. 9 :Schematic diagram of N1 area after process;
[0035] Fig.10 : Schematic diagram of P1 area after process;
[0036] Fig.11 : Rear cross-sectional view of the front electrode;
[0037] Fig.12 : Cross-section diagram after thinning process;
[0038] Fig.13 : Cross-sectional view after back metallization;
[0039] Fig.14 : Traditional TSS current-voltage sweep curve;
[0040] Fig.15 : Negative resistance characteristic TSS current-voltage sweep curve;
[0041] Fig.16 : Comparison of surge residual voltage curves of traditional TSS devices and negative resistance TSS devices.
[0042] Among them: N1-N1 region; N2-N substrate; P1-P1 region; P2-P2 region; P 2 1-P 2 Zone 1; N 2 1–N 2 Zone 1; P 2 2–P 2 Zone 2; N 2 2–N 2 Zone 2. DETAILED DESCRIPTION
[0043] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0044] like Figure 3-Figure 6 are cross-sectional views of semiconductor discharge tubes with negative resistance characteristics of different structures made by the method for manufacturing a semiconductor discharge tube with negative resistance characteristics, and Figure 3 The difference is, Figure 4 The number of P1 zones is several, which are arranged side by side. Figure 3 The difference is, Figure 5 It is composed of two Figure 3 The structure in the figure is set up in reverse, connected by a P-type diffuser in the middle. Figure 4 The difference is, Figure 6 It is composed of two Figure 4 The structure in the figure is set up in reverse, and is connected in the middle by a P-type diffuser.
[0045] The method for manufacturing a semiconductor discharge tube with negative resistance characteristics comprises the following steps:
[0046] Cutting and unloading: Select the appropriate resistivity polishing sheet according to the voltage. Usually <111> Crystal orientation, N-type substrate, feeding. Figure 7 Preparation of P2 area: Use doping process to prepare P2 area. Including but not limited to implantation process, diffusion process, etc. The cross-section diagram after P2 area preparation is as follows Figure 8 .
[0047] N1 region preparation: Use doping process to prepare N1 region. Including but not limited to implantation process, diffusion process, etc. The cross-section diagram after N1 region preparation is as follows Fig. 9 Preparation of P1 area: Use doping process to prepare P1 area. Including but not limited to implantation process, diffusion process, etc. The cross-sectional view after P1 area preparation is as follows Fig.10 . Preparation of the front metal electrode. The cross-section of the device after the front electrode is prepared is as follows Fig.11 . Thinning process, the original substrate is thinned. Generally, CMP or sand blowing process can be used for thinning to a specified thickness. Usually the thickness is around 150 μm. The cross-section of the device after the thinning process is as follows Fig.12 .
[0048] Back metal contact. The cross section after the back metallization process is as follows Fig.13 . Slicing packaging and packaging. Use the packaged device for curve scanning test. Traditional non-negative resistance devices such as Fig.14 . Semiconductor discharge tube devices with negative resistance characteristics such as Fig.15 .
[0049] The surge test of the traditional device and the negative resistance device shows that under the same surge level, the semiconductor discharge tube device with negative resistance characteristic has lower residual voltage. Fig.16 . Adopt N-type substrate thin film short base region negative resistance vertical process.
[0050] The functional structure of the discharge tube manufactured by this method is doped as PNPN type. The surge protection device includes not only unidirectional semiconductor discharge tubes but also bidirectional semiconductor discharge tubes. The thickness of the finished chip is between 30μm and 250μm. The substrate type selects N-type diffusion sheet as the substrate. The P1N1P2N2 structure has the P1N1P2 structure on the same side of the substrate. The P1N1P2 region is prepared using a doping process. The thickness of the P2 region is between 0-30μm, and the width of the P2 region is less than the P2 minority carrier diffusion length. This discharge tube is used as a semiconductor device for surge protection and electrostatic protection. Its operating voltage range is between 6V and 300V. In the VI scanning curve (using 370, QT and other equipment), the semiconductor discharge tube has negative resistance before it is triggered. When the discharge tube device manufactured by this method protects against lightning surges, the lower residual voltage is conducive to better protection of the subsequent circuit. High surge capacity can make the device suitable for higher surge level requirements. This method uses an N-type thin film short base region negative resistance longitudinal process to achieve the purpose of reducing residual voltage and improving surge capacity.
[0051] Based on the above method, a specific implementation method is further described by taking a unidirectional negative resistance characteristic semiconductor discharge tube as an example.
[0052] Wafer cutting, crystal orientation
[111] , arsenic-doped substrate, resistivity 2.0Ω·cm. Then it goes through HF+ No. 1 cleaning process.
[0053] The grown oxide layer is treated with wet oxygen at 900°C for 60 minutes and dry oxygen at 1050°C for 62 minutes.
[0054] Photolithography, then etching and oxidation to form openings, etching the oxide layer with etching solution for 700 seconds to open long base area holes, and then using a stripping solution for wet stripping.
[0055] The pre-implantation oxide layer was grown using 1000°C 60′ O2.
[0056] The boron implantation conditions are 60keV 3.0E14cm-2, followed by annealing activation, the annealing conditions are 1200°C for 40 minutes in N2 atmosphere, and then wet oxygen growth of the oxide layer at 960°C for 40 minutes.
[0057] Photolithography, opening holes in the oxide layer, etching with oxide layer etching solution for 200 seconds, removing the injected protective oxide layer. Then use the degumming solution for wet degumming.
[0058] After phosphorus coating, phosphorus pre-expansion baking is performed.
[0059] Oxidation push-in, the conditions are 850℃+10′H2 / or O2 annealing. Push-in temperature is 1100℃45 minutes nitrogen and oxygen.
[0060] Photolithography, opening holes in the oxide layer, etching with oxide layer etching solution for 300 seconds, removing the injected protective oxide layer. Then use the degumming solution for wet degumming.
[0061] The boron implantation conditions are 20keV 1.0E14cm-2. Then, annealing activation is performed, and the annealing conditions are 960°C for 30 minutes in N2 atmosphere.
[0062] The device was repaired by NH annealing at 400°C for 30 minutes in H2 / N2.
[0063] The front electrode was prepared and then NH3 annealing was used to repair the surface state.
[0064] Surface passivation using LPCVD 425℃ condition
[0065] Contact surfaces are opened by photolithography and etching.
[0066] The film is thinned and the film thickness is 120μm.
[0067] The back electrode was prepared and then NH annealing was used to repair the surface state.
[0068] After that, the chip is diced and tested. After the chip sample is completed, it is packaged using traditional SMB packaging and / or soldering technology.
[0069] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.
Claims
1. A semiconductor discharge tube with negative resistance characteristics, characterized in that: include: Substrate, P2 region, N1 region, P1 region, front metal electrode, back metal electrode; the substrate is an N-type diffusion sheet substrate; the P2 region is prepared by using a doping process on one side of the substrate; the N1 region is prepared by using a doping process on the side of the P2 region away from the substrate; the P1 region is prepared by using a doping process on the side of the N1 region away from the substrate; the front metal electrode is prepared on one side of the P1 region; the back metal electrode is prepared by metal contact treatment on the back of the substrate after thinning treatment; wherein, The P1 region, N1 region and P2 region are located on the same side of the N-type diffusion sheet substrate; The thickness of the P2 region is between 0-30 μm, and the thickness of the P2 region is smaller than the minority carrier diffusion length of the P2 region.
2. The semiconductor discharge tube with negative resistance characteristics according to claim 1, characterized in that: The thickness of the substrate after thinning is between 120 μm and 180 μm.
3. The method for manufacturing a semiconductor discharge tube with negative resistance characteristics according to claim 1 or 2, characterized in that: include: S1: Cutting and unloading the wafer, selecting the substrate; S2: P2 region preparation, using a doping process to prepare the P2 region on one side of the substrate; S3: Preparation of N1 region: using doping process, N1 region is prepared on one side of P2 region; S4: P1 region preparation, using a doping process to prepare the P1 region on one side of the N1 region; S5: Prepare the front metal electrode on one side of the P1 area; S6: Thinning treatment, thinning the original substrate; S7: Performing metal contact processing on the back side of the thinned substrate to produce a back electrode.
4. The method for manufacturing a semiconductor discharge tube having negative resistance characteristics according to claim 3, characterized in that: The doping process includes an implantation process and / or a diffusion process.
5. The method for manufacturing a semiconductor discharge tube with negative resistance characteristics according to claim 3, characterized in that: In step S5, a front metal electrode is prepared on one side of the P1 region.
6. The method for manufacturing a semiconductor discharge tube with negative resistance characteristics according to claim 3, characterized in that: In step S7, metal contact processing is performed on the back side of the thinned substrate.
7. The method for manufacturing a semiconductor discharge tube with negative resistance characteristics according to claim 3, characterized in that: The thinning process in step S6 includes a method of thinning by film sticking, and the film is thinned to a thickness of 120 μm.