One-piece piston ring molding system
By using a positioning device and a position capturing device in the piston ring forming system for overall processing and group grinding of the shaft body, the problems of low production efficiency and unstable quality caused by the numerous processes in the existing technology are solved, and high-precision, large-volume production is achieved. Production and quality improvements.
Patent Information
- Application Number
- CN202010425128.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-05-19
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2040-05-19
AI Technical Summary
The existing piston ring forming system has many processes, resulting in low production efficiency, high equipment costs, unstable quality, and the inability to achieve large-volume simultaneous processing, which affects product accuracy.
Using a positioning device, a preforming device, a position capturing device, a pre-grinding unit, an electroplating device, a finishing grinding unit and an unloading unit, the unified processing and precise forming of multiple piston rings can be achieved through overall processing and group grinding of the shaft body.
It improves product accuracy and yield, reduces the number of equipment and processes, ensures processing benchmarks, and greatly improves the quality and production efficiency of piston rings.
Smart Images

Figure CN111515701B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of piston ring processing, in particular to an integrated piston ring molding system. Background Art
[0002] The piston ring forming system used in the prior art contains many auxiliary processes, including forming and turning the outer circle, ring sorting, grinding and trimming, removing burrs from the outer circle opening, fine grinding, fine grinding of the side, cleaning and degreasing, electroplating clamping, electroplating, outer circle grinding, electroplating unclamping, ring sorting, grinding and trimming, fine grinding, fine grinding of the side, ring sorting and outer circle forming grinding, up to more than a dozen processes, and 11 of them are auxiliary processes. The numerous processes not only reduce the production efficiency and increase the cost of equipment use, but also cause the quality of the piston rings in each process to be subject to uncertainty in human control due to too many processing processes, and the quality is unstable and the defective rate is high. In the existing process processing, the piston rings are processed one by one using single rings, and large-scale synchronous processing cannot be achieved, which undoubtedly reduces the production efficiency of its products and the accuracy of the finished products. Summary of the invention
[0003] The object of the present invention is to provide a piston ring integral molding system to solve the problems raised in the above background technology.
[0004] To achieve the above-mentioned object, the present invention provides the following technical solutions: a piston ring integrated molding system, the system comprising a positioning device, a pre-molding device, a position capturing device, a pre-grinding unit, an electroplating device, a finishing grinding unit and an unloading unit, wherein the positioning device fixes the piston ring to be processed and is processed by the pre-molding device, the pre-grinding unit, the electroplating device, the finishing grinding unit and the unloading device in sequence;
[0005] The positioning device comprises a shaft body and a power assembly connected to the shaft body, the shaft body is sleeved with a plurality of piston rings to be processed and the plurality of piston rings to be processed are clamped by clamping members at both ends of the shaft body, the positioning device is set as a free structure, and the free displacement and axial rotation of the shaft body are realized by the power assembly;
[0006] The preforming device is used to clamp and form the outer circumferential surface of the piston ring to be processed on the shaft body, and form a circular ring structure with a preset outer circumferential surface size;
[0007] The pre-grinding unit includes a grinding wheel 1, which is used to grind the outer cylindrical surface of the piston ring to be processed and form a pre-processed piston ring;
[0008] The electroplating device is used to electroplate the pre-processed piston ring and form a metal coating on the surface of the pre-processed piston ring;
[0009] The finishing grinding unit includes a second grinding wheel, which is used to grind and shape the piston ring with the metal coating;
[0010] The unloading unit is used to unload the piston rings on the shaft body one by one;
[0011] The position capture device captures and records the various ring body positions of the piston ring to be processed which is sleeved on the shaft, and divides the ring bodies of the piston rings to be processed into piston ring groups with a preset number along the axial direction of the shaft after capture. The position capture device also captures and records the various ring body positions of the piston ring with metal coating and the starting point of each piston ring group, which is located at the outer edge of the first-rank piston ring of each piston ring group; the position capture device is electrically connected to the power assembly.
[0012] The pre-grinding unit and the finishing grinding unit both include ceramic grinding wheels. The ceramic grinding wheels in the pre-grinding unit have mesh sizes of 160-200, and the ceramic grinding wheels in the finishing grinding unit have mesh sizes of 100-140.
[0013] The metal plating layer is a chromium layer.
[0014] The power assembly includes a power component and a control component. The power component is connected to the shaft body, and the control component is electrically connected to the position capture device.
[0015] The preforming device comprises two symmetrically arranged clamping members, and both of the two clamping members are formed with semicircular grooves for clamping the piston ring to be processed.
[0016] The first grinding wheel removes 0.1-0.2 mm of the outer diameter of the piston ring to be processed, and the second grinding wheel removes 0.1-0.2 mm of the outer diameter of the piston ring with metal coating.
[0017] It can be seen from the above technical scheme that the present invention uses the shaft of the positioning device to implement the overall processing of multiple piston rings, and combines the position capture device to implement the group grinding of multiple piston rings, which effectively improves the accuracy of the product, and further improves the product accuracy while increasing the production volume, and the yield rate is greatly improved. Specifically:
[0018] 1. The shaft body is sleeved with multiple piston rings, which can realize the unified processing of the piston rings, that is, the processing accuracy of each piston ring on a single shaft body can be improved through pre-grinding, electroplating and finishing grinding;
[0019] Second: Multiple piston rings are polished in groups, so that the size error of piston rings within a unit group is further reduced;
[0020] 3. The position capture device is used to capture and record the piston rings in the pre-grinding, electroplating and finishing grinding stages, which effectively realizes the calibration of the final product, and ensures the dimensional accuracy of the base piston ring located on the inner layer of the piston ring, the uniformity of the metal plating thickness of each piston ring, and the uniformity of the size of each finished piston ring, which greatly improves the quality of the product.
[0021] Fourth: It greatly reduces the number of equipment and production processes in the system, and reduces product errors caused by too many processes and equipment. Compared with traditional processing systems, this system is always located on the same axis from the preforming of the piston ring to the final unloading of the finished product, ensuring the benchmark of processing and improving product quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 It is a schematic diagram of the system structure of the present invention;
[0023] Figure 2 This is a schematic diagram of the distribution of piston ring sections to be processed according to the present invention;
[0024] Figure 3 It is a schematic diagram of the change in the size of the outer cylindrical surface of the piston ring during the pre-grinding, electroplating and finishing grinding processes of the present invention;
[0025] Figure 4 This is a schematic diagram of the structural dimensions of the final finished product piston ring of the present invention. DETAILED DESCRIPTION
[0026] The present invention will be further described below in conjunction with the accompanying drawings:
[0027] like Figure 1-4 The piston ring integral molding system shown in the figure includes a positioning device, a preforming device 1, a position capturing device 4, a pre-grinding unit 2, an electroplating device 7, a finishing grinding unit 3 and an unloading unit. This case realizes the mass production and high-precision production requirements of the piston ring by changing the traditional clamping and positioning method of the piston ring, effectively reduces the processing procedures, reduces the use of equipment, and improves the production efficiency and product quality, as follows:
[0028] In this case, the positioning device is first used to position the ring bodies of multiple piston rings 61 to be processed. The piston rings 61 to be processed are sleeved on the shaft body 5 of the positioning device one by one, and clamped at both ends by clamping members to ensure the tightness of the adjacent piston rings 61 to be processed, and to ensure that there will be no shaking or deviation during the later processing; the positioning device used in this case includes a shaft body 5 and a power component connected to the shaft body 5, and the power component is used to realize the free displacement and self-rotation of the shaft body 5; the power component drives the piston ring 61 to be processed to move, so in order to prevent the position deviation of the piston ring 61 to be processed, in the specific implementation process, the outer diameter of the shaft body 5 is adapted to the inner diameter of the piston ring 61 to be processed, that is, the inner diameter of the piston ring 61 to be processed fits the surface of the shaft body 5, so as to ensure the structural stability after the sleeve connection. It should be emphasized that in this case, multiple piston rings 61 to be processed are sleeved on the shaft body 5, which can not only realize mass production, but also can be combined with the use of the position capture device 4 to capture and record in real time and correct the removal amount of the outer cylindrical surface of the ring body during the grinding process.
[0029] The preforming device 1 is used to clamp and form the outer cylindrical surface of the to-be-processed piston ring 61 on the shaft body 5, and form a circular ring structure with a preset outer cylindrical surface size. The preferred preforming device 1 in this embodiment includes two symmetrically arranged clamping members, namely clamping member 11 and clamping member 2 12, and both clamping members are formed with semicircular grooves for clamping the to-be-processed piston ring 61; in the specific implementation process, the two clamping members are clamped together to form a ring body structure with a roundness less than 0.06 mm for the to-be-processed piston ring 61; it should be pointed out that the to-be-processed piston ring 61 is a semi-sealed structure, that is, an opening portion is formed on its ring body, and the formation of the opening portion allows it to be clamped by two clamping members during preforming and allows the to-be-processed piston ring to have a better roundness, thereby improving the accuracy of subsequent processing.
[0030] The pre-grinding unit 2 includes a grinding wheel 21, which is used to grind the outer peripheral surface of the piston ring 61 to be processed into a pre-processed piston ring 62; the grinding wheel 21 preferably used in this embodiment is a ceramic grinding wheel, and the mesh number of the ceramic grinding wheel is 160-200 meshes.
[0031] The electroplating device 7 is used to electroplate the pre-processed piston ring 62 and form a metal layer on its surface. In this embodiment, the metal plating layer preferably used is a chromium layer.
[0032] The finishing grinding unit 3 includes a grinding wheel 31, which is used to grind the primary processed piston ring 62 with a metal coating into shape, and the polished piston ring is the final finished product; the preferred grinding wheel 31 in this embodiment is a ceramic grinding wheel, and the mesh number of the ceramic grinding wheel is 100-140 meshes.
[0033] The unloading unit is used to unload the piston rings 63 on the shaft body 5 one by one. The present embodiment does not limit the specific unloading device used by the unloading unit. In the specific implementation process, the unloading unit may use a robotic arm, which can realize automatic unloading of the piston rings 63 on the shaft body 5, thereby effectively improving the automation efficiency of this one-piece molding system.
[0034] The above is a structural description of each branch system in the present case. The piston ring is processed through an automated sequence. The positioning device fixes the piston ring 61 to be processed and is processed in sequence through the preforming device 1, the pre-grinding unit 2, the electroplating device 7, the finishing grinding unit 3 and the unloading unit. In the system flow of this processing, the key point to be explained is the coordinated use of the position capture device 4, as follows:
[0035] The position capture device 4 implements capture, recording and control in two stages, namely the pre-grinding stage and the finishing grinding stage;
[0036] Pre-grinding stage:
[0037] At the beginning of this stage, the piston ring 61 to be processed sleeved on the shaft 5 is formed by the preforming device 1. The formed piston ring 61 has a preliminarily formed outer cylindrical surface of the ring body. In order to achieve accurate grinding of the outer cylindrical surface of the piston ring 61 to be processed, the position capture device 4 is used to capture and record the ring body position information of each piston ring 61 to be processed after forming, and the recorded data is uploaded. The position information is recorded as P1; the position capture device 4 processes the recorded ring body position information and divides the various piston rings 61 to be processed on the shaft 5 into piston ring groups with a preset number through a preset division setting. The position information of each piston ring group is recorded as P2, and the position information P2 includes initial point information and end point information; Figure 2As shown, the figure includes intervals S1, S2, ..., SN that divide all the piston rings 61 to be processed into equal numbers, each of which contains a certain preset number of piston rings 61 to be processed. In order to effectively distinguish the piston ring groups, the edge of the first-rank piston ring 61 to be processed in each interval is the starting point, and at the same time, the edge of the first-rank piston ring 61 to be processed in the next interval is the end point; in the figure, the starting point of interval S1 is S11 and the end point is S21, the starting point of interval S2 is S21 and the end point is S31...; in the specific implementation process, in order to effectively control the processing size accuracy of the piston ring group in each interval, the number of piston rings 61 to be processed in the piston ring group is the same; generally, 50 piston rings 61 to be processed are sleeved on a shaft body 5, and grinding is performed on each piston ring group of 5 piston rings 61 to be processed; in implementation, the position capture device 4 uploads the data information after dividing the piston ring group to the processor, and the processor is electrically connected There is a power component, which controls the position of the shaft body 5 relative to the grinding wheel 21 and implements grinding; specifically, during the initial grinding, the interval S1 is first used as a cyclic processing interval, and the shaft body 5 drives the piston ring 61 to be processed to move to the starting point S11. The position capture device 4 has captured the ring body positions of each piston ring 61 to be processed in the interval S1, and the ring body positions include the ring body size at the edge of the starting point S11 and the ring body size at the edge of the piston ring 61 to be processed at the end point S21. The grinding amount M1 of the outer circumferential surface of the ring body required in the interval S1 is obtained according to the preset grinding demand, and the next interval S2 is entered after the grinding is completed; similarly, S2...SN all use the same grinding method; when all the piston rings 61 to be processed on the shaft body 5 are ground, the position capture device 4 is used to recapture and record the position information of the initially processed piston ring 62, and the position information is recorded as P3. The position information P3 includes the position information of the outer circumferential surface of the ring body of each initially processed piston ring 62.
[0038] Complete grinding stage:
[0039] At the beginning of this stage, the initially processed piston ring 62 has been formed with a layer of metal coating by electroplating. At this time, the position information of the initially processed piston ring 62 is captured and recorded by the position capture device 4. The position information is recorded as P4. The position information P4 includes the outer circumferential surface position information of each initially processed piston ring 62 containing a metal coating. Similarly, in the pre-grinding stage, in order to achieve precise grinding of the outer circumferential surface of the initially processed piston ring 62 containing a metal coating, the position capture device 4 processes the recorded ring body position information and divides each initially processed piston ring 62 containing a metal coating on the shaft body 5 into a preset number of positions through a preset division setting. It should be pointed out that the piston ring group corresponds one-to-one to the piston ring group in the pre-grinding stage, that is, the grouping remains unchanged, and the position information of each piston ring group at this time is recorded as P5, and the position information P5 includes the initial point information and end point information of the pre-processed piston ring 62 containing metal plating; during implementation, the position capture device 4 uploads the data information of the position information P5 and P4 to the processor, and the processor is electrically connected to the power component, and the power component controls the position of the shaft 5 relative to the grinding wheel 2 31 and implements grinding, and the grinding amount M2 of the outer cylindrical surface of the ring body within the interval segment of each piston ring group is obtained according to the preset grinding requirement.
[0040] It should be further explained that this case uses a multi-calibration method to achieve precise grinding of the piston ring, specifically: one:
[0042] By sleeve-connecting a plurality of piston rings 61 to be processed on the same shaft body 5, the plurality of piston rings 61 to be processed are polished on the same reference surface, which not only increases the polishing quantity but also improves the precision; two:
[0044] The position capture device 4 captures the ring body position of each piston ring, and implements cyclic grinding for each piston ring group according to the position information, which effectively improves the grinding accuracy;
[0045] 3. Since the finished piston ring includes a base ring body and a metal coating, the base piston ring is first pre-grinded, and then the piston ring containing the metal coating is finished-grinded again on the basis of ensuring the accuracy of all piston rings after pre-grinding. This method effectively ensures the dimensional accuracy of the base piston ring, the uniform thickness of the metal coating of each piston ring, and the uniform size of each finished piston ring, which greatly improves the quality of the product.
[0046] like Figure 4 As shown, after pre-grinding, the piston ring located on the inner ring already has a radius R1 of uniform precision. On this basis, precise grinding after the surface is plated with a metal layer can ensure that the finished piston ring has a radius R2 of uniform precision, and can also ensure that the metal plating has a thickness T of uniform precision.
[0047] The position capture device 4 used in this case uses a machine vision system, which is commonly used in the field of modern mechanical processing. The captured target is converted into an image signal through a camera unit and transmitted to a dedicated image processing system, which is converted into a digital signal based on pixel distribution, brightness, color and other information. The position capture device 4 used in this case is only used to illustrate the location information collection of the piston ring body and the simple processing of the collected signal. The piston ring grouping recognition scheme it uses is an application extension of this image processing system. This case does not further explain its specific circuit control and principle. In the specific implementation process, the position capture device 4 captures and identifies the relative position of the outer cylindrical surface of each piston ring body, and obtains the grinding amount in the interval according to the radius of the first piston ring body and the radius of the last piston ring body in each piston ring group.
[0048] During the implementation of this solution, the closer the number of interval segments is to the number of piston rings 61 to be processed, the higher the accuracy after processing. It can be understood that when each interval segment has only one piston ring 61 to be processed, each piston ring 61 to be processed can be positioned and polished, that is, each piston ring 61 to be processed is a separate cycle processing; however, this implementation method increases the image processing capacity of the position capture device 4, which affects the processing efficiency to a certain extent. Generally, during the processing, 50 piston rings 61 to be processed are sleeved on a shaft body 5, and each 5 piston rings 61 to be processed form an interval segment, and subsequent pre-grinding, electroplating and final grinding are carried out.
[0049] Furthermore, the power assembly includes a power part and a control part, the power part is connected to the shaft body 5, and the control part is electrically connected to the position capture device 4; the power part has a variety of deformation modes, including a rotating device connected to the shaft body 5, generally a variable speed motor can be used, and its output shaft end is connected to the end of the shaft body 5, and in order to realize the free displacement of the shaft body 5 to the preforming device 1, the pre-grinding unit 2, the electroplating device 7, the finishing grinding unit 3 and the unloading device, as well as parallel movement during the pre-grinding and finishing grinding processes, a mechanical arm connected to the end of the shaft body 5 can generally be used.
[0050] Further, the pre-grinding unit 2 and the finishing grinding unit 3 include ceramic grinding wheels, the ceramic grinding wheels in the pre-grinding unit 2 are 160-200 mesh, and the ceramic grinding wheels in the finishing grinding unit 3 are 100-140 mesh. Since the materials of the outer cylindrical surface of the piston ring in the pre-grinding stage and the finishing grinding stage are different, ceramic grinding wheels with different mesh numbers are used accordingly.
[0051] The piston ring one-piece molding system used in this case includes the following process steps:
[0052] S1: Positioning, sleeve the plurality of piston rings 61 to be processed onto the shaft body 5 and clamp and position the plurality of piston rings 61 to be processed;
[0053] S2: Preforming, moving the piston ring 61 to be processed on the shaft body 5 to the preforming device 1 for clamping and forming the outer circumferential surface of the ring body, and forming a circular ring structure with a preset outer circumferential surface size;
[0054] S3: measuring, the positioned piston ring 61 to be processed is moved to the next station, and the position capturing device 4 is used to capture and record the relative position of the outer circumferential surface of the piston ring 61 to be processed;
[0055] S4: pre-grinding, moving the piston ring 61 to be processed which is sleeved on the shaft body 5 after measurement to the next station, and grinding the piston ring 61 to be processed on the shaft body 5 along its axial direction by the pre-grinding unit 2, and obtaining a pre-processed piston ring 62;
[0056] S5: electroplating, electroplating the pre-grinded primary processing piston ring 62 to obtain the primary processing piston ring 62 with a metal coating;
[0057] S6: Finish grinding, move the pre-processed piston ring 62 with metal coating sleeved on the shaft body 5 after electroplating to the next station, and grind it through the finishing grinding unit 3 to obtain the piston ring 63;
[0058] S7: Unclamp and unload the piston ring 63 on the shaft body 5 to complete the operation.
[0059] In step S4, the piston ring 61 to be processed which is sleeved on the shaft body 5 after measurement is moved to the next workstation, and the grinding wheel 21 is used to perform group grinding along the axial direction of the piston ring 61 to be processed on the shaft body 5, wherein the group grinding is to grind each piston ring group after division in a cycle, and in the group grinding process, the initial point where the first-rank piston ring 61 to be processed of each piston ring group is located is used as the starting point for grinding; in step S6, the pre-processed piston ring 62 which is sleeved on the shaft body 5 after electroplating is moved to the next workstation, and the grinding wheel 31 is used to perform group grinding on the outer cylindrical surface of the pre-processed piston ring 62, wherein the group grinding is to grind each piston ring group in a cycle during the pre-grinding process, and in the group grinding process, the initial point where the first-rank piston ring of each piston ring group is located is used as the starting point for grinding.
[0060] The embodiments described above are merely descriptions of preferred implementation modes of the present invention and are not intended to limit the scope of the present invention. Without departing from the design spirit of the present invention, various modifications and improvements made to the technical solutions of the present invention by ordinary technicians in this field should all fall within the protection scope determined by the claims of the present invention.
Claims
1. A piston ring integrated molding system, Features: The system comprises a positioning device, a preforming device, a position capturing device, a pre-grinding unit, an electroplating device, a finishing grinding unit and an unloading unit. The positioning device fixes the piston ring to be processed and is processed by the preforming device, the pre-grinding unit, the electroplating device, the finishing grinding unit and the unloading device in sequence. The positioning device comprises a shaft body and a power assembly connected to the shaft body, the shaft body is sleeved with a plurality of piston rings to be processed and the plurality of piston rings to be processed are clamped by clamping members at both ends of the shaft body, the positioning device is set as a free structure, and the free displacement and axial rotation of the shaft body are realized by the power assembly; The preforming device is used to clamp and form the outer circumferential surface of the piston ring to be processed on the shaft body, and form a circular ring structure with a preset outer circumferential surface size; The pre-grinding unit includes a grinding wheel 1, which is used to grind the outer cylindrical surface of the piston ring to be processed and form a pre-processed piston ring; The electroplating device is used to electroplate the pre-processed piston ring and form a metal coating on the surface of the pre-processed piston ring; The finishing grinding unit includes a second grinding wheel, which is used to grind and shape the piston ring with the metal coating; The unloading unit is used to unload the piston rings on the shaft body one by one; The position capture device captures and records the various ring body positions of the piston ring to be processed which is sleeved on the shaft, and divides the ring bodies of the piston rings to be processed into piston ring groups with a preset number along the axial direction of the shaft after capture. The position capture device also captures and records the various ring body positions of the piston ring with metal coating and the starting point of each piston ring group, which is located at the outer edge of the first-rank piston ring of each piston ring group; the position capture device is electrically connected to the power assembly.
2. The piston ring integral molding system according to claim 1, Features: The pre-grinding unit and the finishing grinding unit both include ceramic grinding wheels. The ceramic grinding wheels in the pre-grinding unit have mesh sizes of 160-200, and the ceramic grinding wheels in the finishing grinding unit have mesh sizes of 100-140.
3. The piston ring integral molding system according to claim 1, Features: The metal plating layer is a chromium layer.
4. The piston ring integral molding system according to claim 1, Features: The power assembly includes a power component and a control component. The power component is connected to the shaft body, and the control component is electrically connected to the position capture device.
5. The piston ring integral molding system according to claim 1, Features: The preforming device comprises two symmetrically arranged clamping members, and both of the two clamping members are formed with semicircular grooves for clamping the piston ring to be processed.
6. The piston ring integral molding system according to claim 1, Features: The first grinding wheel removes 0.1-0.2 mm of the outer diameter of the piston ring to be processed, and the second grinding wheel removes 0.1-0.2 mm of the outer diameter of the piston ring with metal coating.