Flat ultra-thin heat pipe with thermal superconductivity

By designing a gradient-increasing vapor space and capillary flow structure in an ultra-thin heat pipe, combined with the capillary structure of copper wire bundles and sintered powder, the problems of low thermal conductivity and low yield are solved, and efficient thermal superconducting performance and Stable and suitable for mass production.

CN111854492BActive Publication Date: 2024-10-11ZUNYI DISHENG ELECTRONIC TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010850022.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-08-21
Publication Date
2024-10-11
Estimated Expiration
2040-08-21

AI Technical Summary

Technical Problem

In the existing technology, ultra-thin heat pipes have low thermal conductivity, unstable thermal conductivity and low yield, making them difficult to apply in mass production.

Method used

Use a heat pipe with a sealed hollow flat space, built-in first capillary structure (copper wire bundle or copper wire braid) and second capillary structure (copper powder sinter), and define the steam flow path as a full section, a transition section and In the empty section, the first capillary structure and the second capillary structure are interconnected and arranged at intervals on the inner wall of the tube to form a steam space with increasing gradient to improve steam flow and capillary water flow effects.

Benefits of technology

It achieves efficient thermal superconducting properties, good anti-gravity capillary flow performance, improves the stability and production yield of the heat pipe, is suitable for large-scale mass production, and maintains excellent thermal superconducting properties under long heat pipe lengths.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111854492B_ABST
    Figure CN111854492B_ABST
Patent Text Reader

Abstract

A flat ultra-thin heat pipe with thermal superconductivity comprises a tube body with a sealed hollow flat space, the two ends of the tube body are evaporation ends and condensation ends, and a full section, a transition section and an empty section are sequentially arranged along the steam flow path, and the steam space from the full section to the transition section and then to the empty section increases in a gradient; a first capillary structure and a second capillary structure are arranged in the tube body, the first capillary structure extends from the evaporation end of the inner wall of the tube body to the condensation end, and the second capillary structure is attached to the inner wall of the tube body along the extension path of the full section to form a closed loop, or extends from the second capillary structure to the transition section. The present invention adopts a capillary structure combination of powder sintering with good characteristics and copper wire bundles or copper wire braids, so that the ultra-thin heat pipe has very good thermal superconductivity on this mixed capillary structure, a large steam space, and can obtain the best capillary water flow at the horizontal and inclined angles, and will not peel off when bent and flattened, and has a high yield during production, and can be applied to large-scale mass production.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of flat heat pipes, and in particular to a flat ultra-thin heat pipe with thermal superconductivity. The heat pipe is mainly used in a CPU heat dissipation module in an ultra-thin notebook, and can also be used in a narrow space as a heat conduction element. Background Art

[0002] A heat pipe is a heat-conducting element that uses the principle of heat conduction and phase change medium to achieve rapid heat transfer properties. The heat of a heating object is quickly transferred to the outside of the heat source through the heat pipe. Its thermal conductivity exceeds that of any known metal and has been widely used in electronic components with large heat output. When the heat pipe is working, the low-boiling-point working medium filled inside the pipe body absorbs the heat generated by the heating electronic components in its evaporation section and then evaporates and vaporizes. The vapor moves to the condensation section with the heat, and liquefies and condenses in the condensation section to release the heat and dissipate the heat of the electronic components. The liquefied working medium flows back to the evaporation section under the action of the capillary structure of the heat pipe wall, continues to evaporate and vaporize, and liquefies and condenses, so that the working medium circulates inside the heat pipe and continuously dissipates the heat generated by the electronic components.

[0003] The capillary structure of the heat pipe known in the art is composed of a woven mesh or sintered powder. The woven mesh is formed by weaving a plurality of metal wires into a planar mesh. The advantage of using a woven mesh is that the holes of the woven mesh are larger, which can provide a larger steam space. The reflux rate of the working liquid in a horizontal state can meet the demand. However, the capillary structure of a general woven mesh is not as good as that of a sintered powder. The working liquid is not easy to reflux quickly in an inclined state. At the same time, the woven mesh in the heat pipe is usually pressed at both ends of the heat pipe (CCI method). After the heat pipe is bent and flattened, the woven mesh will separate from the inner wall of the pipe body, thereby blocking the steam space and causing the characteristics to deteriorate. Using sintered powder The advantage of powder is that the powder is relatively fine, can provide a good capillary reflux speed, and has better anti-gravity ability, that is, it can still have a good capillary reflux speed in a tilted state. However, the thickness of the heat pipe at its heat dissipation end made of sintered powder cannot be accurately controlled, and the sintered powder extending to the heat dissipation end is difficult to make during sintering. At the same time, if the sintered powder is too thick, the steam space will be reduced, and the heat dissipation effect will be poor. If the sintered powder is too thin, the capillary space will be reduced, and the capillary reflux will be poor. If you want to produce a sintered powder structure that meets the requirements of having good steam space and capillary space at the heat dissipation end of the heat pipe, the yield rate is too low and it is not suitable for large-scale production applications.

[0004] Due to the limitation of product structure, heat pipes need to be made very thin. The space inside thin heat pipes is very small. The heat transfer and heat dissipation of heat pipes rely on steam flow and capillary reflux to achieve heat conduction. In the application of heat pipes, to increase the steam flow, more working liquid (pure water) must be filled. How to maximize the capillary space and steam space of the heat pipe is the biggest consideration for the capillary structure design of ultra-thin heat pipes.

[0005] The Chinese patent CN109764708A, which was published on May 17, 2019, has an application number of 201910079829.8 and a patent name of "Heat pipe and its manufacturing method, and equipment containing the heat pipe" (hereinafter referred to as "reference document 1"), which discloses a heat pipe (see attached Figure 1-4 ), the metal mesh 2 is combined with the tube shell 1 to form a gap filled with copper powder between the two, and copper powder is filled in the gap. After the tube shell 1 containing copper powder and the metal mesh 2 is sintered, the copper powder forms a sintered layer to obtain a capillary. It has been found that by adopting this sintering method, a gap filled with copper powder is left between the tube shell 1 and the metal mesh 2, which will cause the metal mesh 2 to be at a certain distance from the tube shell 1, thereby reducing the thermal conductivity. Other existing heat pipes with composite capillary structures can also be referred to. In the process of realizing the present invention, the inventors have found through research and experiments that there are at least the following problems in the prior art: using existing processes and structures, it is impossible to achieve stable and reliable thermal superconducting performance in ultra-thin heat pipes, and the composite capillary structure adopted has a low yield rate and is not suitable for large-scale production applications.

[0006] In view of this, how to solve the problems of low thermal conductivity, unstable thermal conductivity, and low yield rate in the prior art due to process and structural limitations has become a topic to be studied and solved by the present invention. Summary of the invention

[0007] The purpose of the present invention is to solve the problems existing in the prior art, such as low thermal conductivity, unstable thermal conductivity, and low yield of heat pipes due to process and structural limitations. Therefore, a flat ultra-thin heat pipe with thermal superconductivity is provided, so that the ultra-thin heat pipe has excellent thermal conductivity, is easy to mass produce, and has a high yield.

[0008] To achieve the above object, a technical solution adopted by the present invention is: comprising a tube body, one end of the tube body is an evaporation end, and the other end is a condensation end, the tube body has a sealed hollow flat space, the hollow flat space is encapsulated with a working liquid, a first capillary structure and a second capillary structure are arranged in the hollow flat space, the first capillary structure is a copper wire bundle or a copper wire braid, the second capillary structure is a copper powder sintered material, and the remaining space in the hollow flat space except the first capillary structure and the second capillary structure forms a steam space, and its innovation lies in:

[0009] The steam flow path extending from the evaporation end to the condensation end of the tube is defined as a full section, a transition section and an empty section in sequence;

[0010] The first capillary structure extends from the evaporation end of the inner wall of the tube body through the full section, the transition section and the empty section to the condensation end; the first capillary structure is sintered and attached to the inner wall of the tube body;

[0011] The second capillary structure starts from the evaporation end of the inner wall of the tube body and passes through the full section, or passes through the full section and the transition section; the second capillary structure is sintered and attached to the inner wall of the tube body;

[0012] In the full section, the first capillary structure and the second capillary structure are connected to each other in the circumferential direction of the inner wall of the tube body, and form a full arrangement in the circumferential direction of the inner wall of the tube body;

[0013] In the transition section, only the first capillary structure is arranged in the circumferential direction of the inner wall of the tube body, or the first capillary structure and the second capillary structure are arranged in the circumferential direction of the inner wall of the tube body with a gap left in the arrangement in the circumferential direction of the inner wall of the tube body;

[0014] In the empty section, only the first capillary structure is arranged in the circumferential direction of the inner wall of the tube body, and a gap is left in the arrangement in the circumferential direction of the inner wall of the tube body;

[0015] In the full section, the first steam space is formed by the first capillary structure and the second capillary structure; in the transition section, the second steam space is formed by the first capillary structure and the inner wall of the tube body or by the first capillary structure, the second capillary structure and the inner wall of the tube body; in the empty section, the third steam space is formed by the first capillary structure and the inner wall of the tube body; the cross-sectional areas of the first steam space, the second steam space and the third steam space increase in a gradient manner.

[0016] The relevant contents of the present invention are explained as follows:

[0017] 1. In the description of this application, it should be understood that the terms "center", "longitudinal", "lateral", "length", "thickness", "axial", "radial", "circumferential" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing this application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific position, be constructed and operated in a specific position, and therefore cannot be understood as limiting this application. ;

[0018] 2. In addition, the terms "first", "second", and "third" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, a feature defined as "first", "second", and "third" may explicitly or implicitly include at least one of the features. In the description of this application, "multiple" means at least two, such as two, three, etc., unless otherwise clearly and specifically defined.

[0019] 3. In the above technical solution, the first capillary structure is a copper wire bundle or a copper wire braid. The copper wire bundle is a bundle structure composed of copper wires. The copper wire braid can be a 3D braided mesh or a 2D braided mesh or other braided structures. The first capillary structure using a 3D braided mesh structure can have the best capillary water flow effect. The 2D braided mesh or other bundle structures can also have a good capillary water flow effect and also meet the thermal superconductivity requirements of the heat pipe.

[0020] 3. In the above technical solution, at the transition section, the second capillary structure is close to one side of the first capillary structure, and the first capillary structure and the second capillary structure form a continuous transition gap in the circumferential direction of the inner wall of the tube body; at the transition section, the second capillary structure is close to both sides of the first capillary structure, and the second capillary structures on both sides of the first capillary structure form a continuous transition gap in the circumferential direction of the inner wall of the tube body; at the transition section, the second capillary structure is far away from the first capillary structure, and the first capillary structure and the second capillary structure form an interval transition gap in the circumferential direction of the inner wall of the tube body. The above three situations can have steam spaces of nearly equal volume at the transition section.

[0021] 4. In the above technical solution, the first capillary structure is located on the flat surface of the hollow flat space of the tube body to avoid being in a folded and flattened position when flattened, further preventing the first capillary structure from falling off. At the same time, in order to better control the characteristics of the produced heat pipes to be consistent and the quality and performance to be stable, the thickness of the first capillary structure and the second capillary structure are equal.

[0022] 5. In the above technical solution, the thickness range of the first capillary structure and the second capillary structure is between 0.2mm and 0.7mm; the wall thickness range of the tube body is between 0.1mm and 0.3mm, which provides good structural support for creating an ultra-thin heat pipe.

[0023] Due to the application of the above scheme, the present invention has the following advantages and effects compared with the prior art:

[0024] 1. The heat pipe and the mixed capillary structure of the present invention can be filled with more working liquid to increase the steam flow, and a higher steam flow means a higher thermal superconductivity.

[0025] 2. Through the coordinated use of the first capillary structure and the second capillary structure, the capillary phenomenon is improved, so that the flat ultra-thin heat pipe has good capillary water flow and good anti-gravity capillary water flow, and the best capillary water flow at the horizontal and inclined angles can be obtained. At the heat dissipation end, as long as there is a capillary water flow of copper wire bundles or copper wire braids, there is no need to sinter the capillaries, thereby increasing the steam space at the heat dissipation end.

[0026] 3. The capillary structure combination of powder sintering with good characteristics and copper wire bundle or copper wire braid is adopted, so that the thin tube has very good thermal superconductivity on this mixed capillary structure.

[0027] 4. This mixed capillary structure uses a sintering process to sinter the inner wall of the tube body with the sintered powder and the tube body with the copper wire bundle or copper wire braid together, rather than pressing the woven mesh at both ends. Therefore, after bending and flattening during the heat pipe production process, the sintered powder and the copper wire bundle or copper wire braid will not separate from the inner wall of the tube body, avoiding deterioration of characteristics.

[0028] 5. Good mass production and high yield. The above structure is adopted, and the first capillary structure as the copper wire bundle or the copper wire braid runs through, and the second capillary structure is distributed on one side of the full section and the transition section of the first capillary structure. Compared with the existing composite capillary structure, the heat pipe of the present invention has a very high yield during production, which can almost reach the yield of the powder sintered tube, and can be applied to large-scale mass production, and its defective rate is only one thousandth.

[0029] 6. The first capillary structure and the second capillary structure together form a first steam space, a second steam space and a third steam space, so that the steam space at the condensation end is much larger than other parts, and the first capillary structure extends to the third steam space, which is sufficient to meet the capillary water flow here; at the same time, since the steam space from the full section to the transition section and then to the empty section increases in a gradient, after the first evaporation space at the full section forms steam, since the first evaporation space at the full section is small enough, the steam pressure in the first evaporation space is large enough, so that the steam can be better impacted out under the action of high pressure. Therefore, the technical solution of the embodiment of the present invention can also meet the use of heat pipes with very long lengths. The longer the length, the better the thermal superconducting performance. In the prior art, heat pipes exceeding a certain length will almost fail when used. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Attached Figure 1 The cross-section diagram of the flat ultra-thin heat pipe according to the embodiment of the present invention is shown in FIG. Figure 1 ;

[0031] Attached Figure 2 for Figure 1 The cross-sectional diagram of the heat pipe at AA in the middle is a circular tube;

[0032] Attached Figure 3 for Figure 1 Schematic diagram of the cross section of the heat pipe when it is flattened at AA in the middle;

[0033] Attached Figure 4 for Figure 1 A schematic cross-sectional view of the heat pipe at the middle BB when the heat pipe is a circular tube;

[0034] Attached Figure 5 for Figure 1A cross-sectional diagram of the situation when the heat pipe is flattened at the middle BB;

[0035] Attached Figure 6 for Figure 1 Schematic diagram of the cross section when the heat pipe is flattened at the middle BB;

[0036] Attached Figure 7 for Figure 1 Three-section schematic diagram of the situation when the heat pipe is flattened at the middle BB;

[0037] Attached Figure 8 for Figure 1 The cross-sectional diagram of the heat pipe at CC in the middle is a circular pipe;

[0038] Attached Fig. 9 for Figure 1 Schematic diagram of the cross section of the heat pipe when it is flattened at CC in the middle;

[0039] Attached Fig.10 The cross-section diagram of the flat ultra-thin heat pipe according to the embodiment of the present invention is shown in FIG. Figure 2 ;

[0040] Attached Fig.11 The cross-section diagram of the flat ultra-thin heat pipe according to the embodiment of the present invention is shown in FIG. Figure 3 ;

[0041] Attached Fig.12 This is a top view of the horizontal placement of the heat pipe, heating element, and heat sink for the horizontal verification test comparison of Experiment 1;

[0042] Attached Fig.13 This is a front view of the heat pipe, heating element, and heat sink placed at an angle of 90° for the tilt angle verification test comparison of Experiment 2;

[0043] Attached Fig.14 This is the Q-max trend chart obtained after horizontal verification test comparison;

[0044] Attached Fig.15 This is the Q-max trend chart obtained after the tilt angle verification test comparison.

[0045] The various parts of the above drawings are shown as follows:

[0046] 1. Tube body; 101. Evaporation end; 102. Condensation end; 111. Full section; 112. Transition section; 113. Empty section; 121. First steam space; 122. Second steam space; 123. Third steam space; 131. Transition gap;

[0047] 2. The first capillary structure; 3. The second capillary structure;

[0048] 4. Heat generating element; 5. Heat sink. DETAILED DESCRIPTION

[0049] The present invention will be further described below in conjunction with the accompanying drawings and embodiments.

[0050] The present invention will be clearly described below with drawings and detailed descriptions. After understanding the embodiments of the present invention, any person skilled in the art can make changes and modifications based on the techniques taught by the present invention without departing from the spirit and scope of the present invention. Embodiment 1

[0051] As attached Figure 1 To Attachment Fig.10 As shown, the first embodiment of the present invention proposes a flat ultra-thin heat pipe with thermal superconductivity, including a tube body 1, one end of the tube body 1 is an evaporation end 101, and the other end is a condensation end 102, the tube body 1 has a sealed hollow flat space, the hollow flat space is encapsulated with a working liquid, the hollow flat space is provided with a first capillary structure 2 and a second capillary structure 3, the first capillary structure 2 is a copper wire bundle or a copper wire braid, the second capillary structure 3 is a copper powder sintered material, the remaining space in the hollow flat space except the first capillary structure 2 and the second capillary structure 3 forms a steam space, wherein:

[0052] The pipe body 1 is provided with a full section 111, a transition section 112 and an empty section 113 in sequence along the steam flow path extending from the evaporation end 101 to the condensation end 102, and the steam space from the full section 111 to the transition section 112 and then to the empty section 113 increases in a gradient manner;

[0053] The steam flow path of the tube body 1 extending from the evaporation end 101 to the condensation end 102 is defined as a full section 111, a transition section 112 and an empty section 113 in sequence;

[0054] The first capillary structure 2 is a 3D woven mesh composed of copper wires, which is a three-dimensional mesh composed of unit copper wires woven vertically and horizontally and vertically. The first capillary structure 2 extends from the evaporation end 101 of the inner wall of the tube body 1 through the full section 111, the transition section 112 and the empty section 113 to the condensation end 102; the first capillary structure 2 is sintered and attached to the inner wall of the tube body 1;

[0055] The second capillary structure 3 starts from the evaporation end 101 of the inner wall of the tube body 1 and ends at the full section 111 and the transition section 112; the second capillary structure 3 is sintered and attached to the inner wall of the tube body 1;

[0056] On the full section 111, the first capillary structure 2 and the second capillary structure 3 are connected to each other in the circumferential direction of the inner wall of the tube body 1, and form a full arrangement in the circumferential direction of the inner wall of the tube body 1;

[0057] In the transition section 112, the first capillary structure 2 and the second capillary structure 3 are arranged in a spaced or connected manner on the circumferential direction of the inner wall of the tube body 1, and a gap is left in the arrangement on the circumferential direction of the inner wall of the tube body 1. For the schematic diagram of the positions of the first capillary structure 2 and the second capillary structure 3, please refer to the attached Figure 1 and attached Fig.10 ;

[0058] On the empty section 113, only the first capillary structure 2 is arranged in the circumferential direction of the inner wall of the tube body 1, and a gap is left in the circumferential direction of the inner wall of the tube body 1;

[0059] In the full section 111, the first capillary structure 2 and the second capillary structure 3 form a first steam space 121; in the transition section 112, the first capillary structure 2, the second capillary structure 3 and the inner wall of the tube body 1 form a second steam space 122; in the empty section 113, the first capillary structure 2 and the inner wall of the tube body 1 form a third steam space 123; the cross-sectional areas of the first steam space 121, the second steam space 122 and the third steam space 123 increase in a gradient manner. Embodiment 2

[0060] As attached Fig.10 As shown, the second embodiment of the present invention proposes a flat ultra-thin heat pipe with thermal superconductivity, including a tube body 1, one end of the tube body 1 is an evaporation end 101, and the other end is a condensation end 102, the tube body 1 has a sealed hollow flat space, the hollow flat space is encapsulated with a working liquid, the hollow flat space is provided with a first capillary structure 2 and a second capillary structure 3, the first capillary structure 2 is a copper wire bundle or a copper wire braid, the second capillary structure 3 is a copper powder sintered material, the remaining space in the hollow flat space except the first capillary structure 2 and the second capillary structure 3 forms a steam space, wherein:

[0061] The steam flow path of the tube body 1 extending from the evaporation end 101 to the condensation end 102 is defined as a full section 111, a transition section 112 and an empty section 113 in sequence;

[0062] The first capillary structure 2 is a 2D braided mesh composed of copper wires, which is a two-dimensional mesh structure composed of unit copper wires braided vertically and horizontally. The first capillary structure 2 starts from the evaporation end 101 of the inner wall of the tube body 1, passes through the full section 111, the transition section 112 and the empty section 113 and extends to the condensation end 102; the first capillary structure 2 is sintered and attached to the inner wall of the tube body 1;

[0063] The second capillary structure 3 starts from the evaporation end 101 of the inner wall of the tube body 1 and ends at the full section 111; the second capillary structure 3 is sintered and attached to the inner wall of the tube body 1;

[0064] On the full section 111, the first capillary structure 2 and the second capillary structure 3 are connected to each other in the circumferential direction of the inner wall of the tube body 1, and form a full arrangement in the circumferential direction of the inner wall of the tube body 1;

[0065] In the transition section 112, only the first capillary structure 2 is arranged on the circumference of the inner wall of the tube body 1, and a gap is left in the arrangement on the circumference of the inner wall of the tube body 1. For the schematic diagram of the positions of the first capillary structure 2 and the second capillary structure 3, please refer to the attached Fig.11 ;

[0066] On the empty section 113, only the first capillary structure 2 is arranged in the circumferential direction of the inner wall of the tube body 1, and a gap is left in the circumferential direction of the inner wall of the tube body 1;

[0067] In the full section 111, the first capillary structure 2 and the second capillary structure 3 form a first steam space 121; in the transition section 112, the first capillary structure 2 and the inner wall of the tube body 1 form a second steam space 122; in the empty section 113, the first capillary structure 2 and the inner wall of the tube body 1 form a third steam space 123; the cross-sectional areas of the first steam space 121, the second steam space 122 and the third steam space 123 increase in a gradient manner.

[0068] The principle and working process of the flat ultra-thin heat pipe with thermal superconductivity in the embodiment of the present invention are as follows:

[0069] In the flat ultra-thin heat pipe of the embodiment of the present invention, in the hollow flat space of the tube body 1, the remaining space except the first capillary structure 2 and the second capillary structure 3 forms a steam space, and the steam space from the full section 111 to the transition section 112 and then to the empty section 113 increases in a gradient manner, thereby increasing the steam space and improving the steam pressure at the full section 111; the first capillary structure 2 and the second capillary structure 3 in the hollow flat space of the tube body 1 form a capillary water flow space, and the capillary water flow space from the full section 111 to the transition section 112 and then to the empty section 113 decreases in a gradient manner, and the first capillary structure 2 that runs through the empty section 113 provides a good capillary water flow, which is combined with the second capillary structure 3 at the transition section 112 to further enhance the anti-gravity capillary water flow. When the heat pipe is working, in a vacuum environment, the working liquid in the evaporation end 101 is immediately vaporized by heat, and the formed steam diffuses from the evaporation end 101 to the condensation end 202, and the steam diffuses to the condensation end 202 through the first steam space 121, the second steam space 122, and the third steam space 123. After the steam diffused to the condensation end 202 releases heat and condenses into liquid in this section, it flows back to the evaporation end 101 along the first capillary structure 2 and the second capillary structure 3 on the inner wall of the tube body 1, and the reciprocating cycle is performed, thereby quickly transferring heat from the evaporation end to the condensation end and dissipating it.

[0070] By adopting the above embodiment, the heat pipe can have a very high heat conduction efficiency while realizing an ultra-thin heat pipe structure, and still have good heat conduction performance in various use states such as horizontal and inclined, which is mainly achieved by the combination of the following structural characteristics:

[0071] 1. The combination of copper wire bundles or copper wire braids with good water capillary flow effect and sintered powder with better anti-gravity capillary flow is adopted, so that the capillary structure in the heat pipe can have both good water capillary flow effect and better anti-gravity capillary flow performance.

[0072] 2. The combination of copper wire bundles or copper wire braids and sintered powder can obtain the best capillary water flow effect in the horizontal or inclined direction.

[0073] 3. The first capillary structure 2 and the second capillary structure 3 form a first steam space 121, the first capillary structure 2, the second capillary structure 3 or the tube body 1 form a second steam space 122, and the first capillary structure 2 and the tube body 1 form a third steam space 123, so that the steam space at the condensation end 102 is much larger than other parts, and the first capillary structure 2 extends to the third steam space 123, which is sufficient to meet the capillary water flow here; at the same time, since the steam space from the full section 111 to the transition section 112 and then to the empty section 113 increases in a gradient, after the first evaporation space 123 at the full section 111 forms steam, since the first evaporation space 123 at the full section 111 is small enough, the steam pressure in the first evaporation space 123 is large enough, so that the steam can be better impacted out under the action of high pressure, so the technical solution of the embodiment of the present invention can also meet the use of heat pipes with very long lengths. The longer the length, the better the thermal superconducting performance, while the heat pipes in the prior art that exceed a certain length will almost fail when used.

[0074] 4. From the third point, it can be seen that the characteristic of the embodiment of the present invention is that it uses a copper wire bundle or copper wire braid that runs through both ends and a sintered powder that is only sintered to the middle section, so that the heat pipe has very good thermal superconducting properties on this capillary structure.

[0075] 5. This hybrid capillary structure adopts a sintering process to sinter the inner wall of the tube body 1 with the sintered powder and the tube body 1 with the copper wire bundle or copper wire braid together, rather than pressing the braided mesh at both ends. Therefore, after bending and flattening, the sintered powder and the copper wire bundle or copper wire braid will not separate from the inner wall of the tube body 1, avoiding deterioration of characteristics.

[0076] With respect to the above-mentioned embodiment, possible changes of the present invention are described as follows:

[0077] 1. In the above embodiments, the structure and position relationship between the first capillary structure 2 and the second capillary structure 3 at the transition section 112 may be as follows: Figure 5 At the transition section 112, the second capillary structure 3 is close to one side of the first capillary structure 2, and a continuous transition gap 131 is formed on the circumferential direction of the inner wall of the tube body 1 by the first capillary structure 2 and the second capillary structure 3; Figure 6 At the transition section 112, the second capillary structure 3 is close to both sides of the first capillary structure 2, and the second capillary structures 3 on both sides of the first capillary structure 2 form a continuous transition gap 131 on the circumferential direction of the inner wall of the tube body 1; Figure 7 At the transition section 112, the second capillary structure 3 is away from the first capillary structure 2, and a transition gap 131 is formed by the first capillary structure 2 and the second capillary structure 3 on the circumferential direction of the inner wall of the tube body 1. These three situations can have steam spaces of nearly equal volumes.

[0078] 2. In the above-mentioned Embodiment 1 and Embodiment 2, the first capillary structure 2 is a copper wire braid, and this copper wire braid can be a 3D braided mesh. The first capillary structure 2 using a 3D braided mesh structure can have the best water capillary water flow effect, but the present invention is not limited to this. The first capillary structure 2 can also be a 2D braided mesh or other copper wire bundle structure. The 2D braided mesh is a two-dimensional mesh structure composed of unit copper wires woven vertically and horizontally, and the copper wire bundle is a bundle structure composed of copper wires.

[0079] 3. In the above embodiments, the thickness range of the first capillary structure 2 and the second capillary structure 3 is between 0.2 mm and 0.7 mm, and the specific thickness of the first capillary structure 2 and the second capillary structure 3 can be selected from 0.2 mm, 0.3 mm, 0.5 mm, 0.6 mm or 0.7 mm; the wall thickness range of the tube body 1 is between 0.1 mm and 0.3 mm, and specifically, the wall thickness of the tube body 1 can be selected from 0.1 mm, 0.15 mm, 0.2 mm, 0.25 mm or 0.3 mm.

[0080] In order to verify the thermal superconductivity of the embodiment of the present invention, the inventor conducted a thermal conductivity test experiment. In order to ensure the reliability and consistency of the test results, the heat pipes tested were flattened into flat heat pipes with a thickness of 1.5 mm from heat pipes with a specification of Φ8*225 mm, and the body of the heat pipes was a copper pipe. The heat pipes used as the control group are all full-powder heat pipes. The concept of full-powder heat pipes is that the inner wall of the heat pipe is sintered and attached with qualified sintered powder, and the sintered powder is copper powder. The heat pipes of the test group use half-powder + copper mesh heat pipes, that is, the flat ultra-thin heat pipes with thermal superconductivity described in Example 1 of the present invention are used. The first capillary structure 2 made of 3D woven mesh runs through the evaporation end 101 to the condensation end 102 of the heat pipe, and the second capillary structure 3 made of powder sintering is only located in the full section 111 and part of the transition section 112. It should be noted that the heat pipe made of only woven mesh has no thermal superconductivity in the tilted state, so only the full-powder heat pipe is used as the control group for testing.

[0081] During the test, the evaporation end of the flat heat pipe is placed on the heating element 4, and the condensation end of the flat heat pipe is placed on the heat sink 5. The heating power of the heating element 4 can be adjusted. The relevant parameters of the test are explained as follows: P is the heating power of the heating element (W); Tc: heating element temperature (℃); Ta: ambient temperature (℃); Rc: thermal resistance (℃ / W), Rc=(Tc-Ta) / P.

[0082] Experiment 1: Level verification test comparison:

[0083] The heat pipes used in samples 1, 2 and 3 are all-powder heat pipes, and sample 4 uses the flat ultra-thin heat pipe with thermal superconductivity described in Example 1 of the present invention. When conducting a horizontal verification test comparison, the test method is to place the heating element 4, the heat sink 5 and the flat heat pipe horizontally. The top view of the horizontal placement is shown in the attached figure. Fig.12 The test time for each test power is about 600 seconds. The results of the horizontal verification test comparison are shown in Table 1 and Appendix. Fig.14 .

[0084]

[0085] Table 1

[0086] Table 1 shows the results of the horizontal verification test comparison. The Q-max trend chart of the results is shown in the attached Fig.14 , from Table 1 and Appendix Fig.14 It can be seen that:

[0087] 1. In the horizontal test of the full powder sample 1 with a water volume of 0.98cc, the maximum test power is 30W. At the heating power of 30W, its thermal resistance is 2.06℃ / W. After the test power is adjusted to 35W, the measured heating element temperature Tc keeps rising and cannot be stabilized and balanced;

[0088] 2. In the horizontal test of the full powder sample 2 with a water volume of 1.00cc, the maximum test power is 30W. At the heating power of 30W, its thermal resistance is 1.93℃ / W. After the test power is adjusted to 35W and 40W, the measured heating element temperature Tc keeps rising and cannot be stabilized;

[0089] 3. In the horizontal test of the full powder sample 3 with a water volume of 1.04cc, the maximum test power is 35W. At the heating power of 35W, its thermal resistance is 1.79℃ / W. After the test power is adjusted to 40W and 45W, the measured heating element temperature Tc keeps rising and cannot be stabilized;

[0090] 4. In the horizontal test of the semi-powder + copper mesh sample 4 with a water volume of 0.97cc, the maximum test power is 60W. At a heating power of 60W, its thermal resistance is 0.89℃ / W, and when the test power range is between 25W and 60W, the thermal resistance value remains between 0.89 and 0.94.

[0091] Conclusion of Experiment 1: It can be learned from the test data of Experiment 1 that the flat ultra-thin heat pipe with thermal superconductivity described in Example 1 of the present invention can maintain a low and stable thermal resistance under different test powers P (W) in the horizontal verification test comparison, while the full powder sample can only exert its thermal conductivity performance at a lower power, and the thermal resistance value is nearly twice as high as that of Sample 4, indicating that the flat ultra-thin heat pipe of the present invention has good thermal superconductivity in a horizontal state.

[0092] Experiment 2: Tilt angle verification test comparison:

[0093] The heat pipes used in samples 7 and 8 are all-powder heat pipes, and samples 5 and 6 use the flat ultra-thin heat pipes with thermal superconductivity described in Example 1 of the present invention. When performing the tilt angle verification test comparison, the test method is to place the heating element 4 on the top and the heat sink 5 on the bottom, so that the overall tilt angle of the flat heat pipe is 90°, which is used to test the thermal conductivity of the heat pipe at an extreme tilt angle. At the same time, it is required that each test sample has no abnormal sound when the tilt angle is 90° (if the water volume in the heat pipe is too much, there will be a ticking sound during the angle test. This abnormal sound is not allowed in the qualified products of the present invention, so no abnormal sound is required). Please refer to the attached figure for the front view placed at a tilt angle of 90°. Fig.13 The test time for each test power is about 600 seconds. The results of the tilt angle verification test comparison are shown in Table 2 and Appendix. Fig.15 .

[0094]

[0095] Table 2

[0096] Table 2 shows the results of the tilt angle verification test comparison. The Q-max trend chart of the results is shown in the attached Fig.15 , from Table 2 and Appendix Fig.15 It can be seen that:

[0097] 1. In the 90° inclination test with a water volume of 0.97cc, the maximum test power of the semi-powder + copper mesh sample 5 was 35W. At a heating power of 35W, its thermal resistance was 1.64℃ / W. After the test power was adjusted to 40W, the temperature Tc of the heating element kept rising and could not be stabilized;

[0098] 2. In the 90° inclination test with a water volume of 1.0cc, the maximum test power of the semi-powder + copper mesh sample 6 was 40W. At a heating power of 40W, its thermal resistance was 1.61℃ / W. After the test power was adjusted to 45W, the measured heating element temperature Tc kept rising and could not be stabilized;

[0099] 3. In the 90° inclination test with a water volume of 0.98cc, the maximum test power of the full powder sample 7 was 20W. At a heating power of 20W, its thermal resistance was 2.68℃ / W. After the test power was adjusted to 25W, the measured heating element temperature Tc kept rising and could not be stabilized;

[0100] 4. In the 90° inclination test with a water volume of 1.04cc, the maximum test power of the full powder sample 8 was 25W. At a heating power of 25W, its thermal resistance was 2.10℃ / W. After the test power was adjusted to 30W, the measured heating element temperature Tc kept rising and could not be stabilized.

[0101] Conclusion of Experiment 2: It can be learned from the test data of Experiment 2 that in the 90° inclination test comparison of the flat ultra-thin heat pipe with thermal superconductivity described in Example 1 of the present invention, the maximum test power in the simulated use scenario of 90° inclination is 20W higher than that of the full-powder sample, and the full-powder sample is only 20W and 25W, and the thermal resistance value is relatively high, indicating that under the 90° inclination, the full-powder sample only has a heat conduction effect in low-power use, while the flat ultra-thin heat pipe of the present invention can reach 35W and 40W, and even at the maximum test power, the flat ultra-thin heat pipe of the present invention still has a better thermal resistance of 1.64℃ / W and 1.61℃ / W, indicating that the flat ultra-thin heat pipe of the present invention still has better thermal superconductivity under the extreme use condition of 90° inclination, and can satisfy its thermal superconductivity performance at a certain inclination angle.

[0102] The above embodiments are only for illustrating the technical concept and features of the present invention, and their purpose is to enable people familiar with the technology to understand the content of the present invention and implement it accordingly, and they cannot be used to limit the protection scope of the present invention. Any equivalent changes or modifications made according to the spirit of the present invention should be included in the protection scope of the present invention.

Claims

1. A flat ultra-thin heat pipe with thermal superconductivity, comprising a tube body (1), one end of the tube body (1) being an evaporation end (101) and the other end being a condensation end (102), the tube body (1) having a sealed hollow flat space, the hollow flat space encapsulating a working liquid, a first capillary structure (2) and a second capillary structure (3) being arranged in the hollow flat space, the first capillary structure (2) being a copper wire bundle or a copper wire braid, the second capillary structure (3) being a copper powder sintered material, the remaining space in the hollow flat space except the first capillary structure (2) and the second capillary structure (3) forming a steam space, characterized in that: The wall thickness of the tube body (1) ranges from 0.1 mm to 0.3 mm, and the steam flow path extending from the tube body (1) along the evaporation end (101) to the condensation end (102) is defined as a full section (111), a transition section (112), and an empty section (113) in sequence; The first capillary structure (2) extends from the evaporation end (101) of the inner wall of the tube body (1), through the full section (111), the transition section (112) and the empty section (113) to the condensation end (102); the first capillary structure (2) is sintered and attached to the inner wall of the tube body (1); the first capillary structure (2) is located on the flat surface of the hollow flat space of the tube body (1); The second capillary structure (3) starts from the evaporation end (101) of the inner wall of the tube body (1) and passes through the full section (111), or passes through the full section (111) and the transition section (112); the second capillary structure (3) is sintered and attached to the inner wall of the tube body (1); On the full section (111), the first capillary structure (2) and the second capillary structure (3) are connected to each other in the circumferential direction of the inner wall of the tube body (1), and form a full arrangement in the circumferential direction of the inner wall of the tube body (1); On the transition section (112), only the first capillary structure (2) is arranged in the circumferential direction of the inner wall of the tube body (1), or the first capillary structure (2) and the second capillary structure (3) are arranged in a spaced-apart or connected manner in the circumferential direction of the inner wall of the tube body (1), and a gap is left in the arrangement in the circumferential direction of the inner wall of the tube body (1); On the empty section (113), only the first capillary structure (2) is arranged in the circumferential direction of the inner wall of the tube body (1), and a gap is left in the arrangement in the circumferential direction of the inner wall of the tube body (1); In the full section (111), the first capillary structure (2) and the second capillary structure (3) together form a first steam space (121); in the transition section (112), the first capillary structure (2) and the inner wall of the tube body (1) or the first capillary structure (2), the second capillary structure (3) and the inner wall of the tube body (1) together form a second steam space (122); in the empty section (113), the first capillary structure (2) and the inner wall of the tube body (1) together form a third steam space (123); the cross-sectional areas of the first steam space (121), the second steam space (122) and the third steam space (123) increase in a gradient manner; The first capillary structure (2) and the second capillary structure (3) have equal thickness; The thickness of the first capillary structure (2) and the second capillary structure (3) ranges from 0.2 mm to 0.7 mm.

2. The flat ultra-thin heat pipe with thermal superconductivity according to claim 1, characterized in that: The first capillary structure (2) is a 3D woven mesh composed of copper wires, and the 3D woven mesh is a three-dimensional mesh body composed of unit copper wires woven in a vertical and horizontal manner.

3. The flat ultra-thin heat pipe with thermal superconductivity according to claim 1, characterized in that: The first capillary structure (2) is a 2D woven mesh composed of copper wires, and the 2D woven mesh is a two-dimensional mesh structure composed of unit copper wires woven vertically and horizontally.

4. The flat ultra-thin heat pipe with thermal superconductivity according to claim 1, characterized in that: At the transition section (112), the second capillary structure (3) is close to one side of the first capillary structure (2), and a continuous transition gap (131) is formed in the circumferential direction of the inner wall of the tube body (1) by the first capillary structure (2) and the second capillary structure (3).

5. The flat ultra-thin heat pipe with thermal superconductivity according to claim 1, characterized in that: At the transition section (112), the second capillary structure (3) is close to both sides of the first capillary structure (2), and a continuous transition gap (131) is formed in the circumferential direction of the inner wall of the tube body (1) by the second capillary structures (3) on both sides of the first capillary structure (2).

6. The flat ultra-thin heat pipe with thermal superconductivity according to claim 1, characterized in that: At the transition section (112), the second capillary structure (3) is away from the first capillary structure (2), and a transition gap (131) is formed in the circumferential direction of the inner wall of the tube body (1) by the first capillary structure (2) and the second capillary structure (3).