A quasi-isostatic electrode sealing mechanism and its use method
By using sealed insulating components and clamping parts in the electrode sealing mechanism, the quasi-isostatic state of the electrode is achieved under high temperature and high pressure environments, solving the problem of stress affecting experimental accuracy in the existing technology, and expanding the scope of brittleness testing. Material testing capabilities.
Patent Information
- Application Number
- CN202010883065.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-08-28
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2040-08-28
Smart Images

Figure CN111970779B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a quasi-isostatic pressure electrode sealing mechanism and a use method thereof, belonging to the technical field of electrode sealing. Background Art
[0002] In the electrochemical experiment of high temperature and high pressure water fluid, the sealing and insulation of the electrode are usually completed by various sealing mechanisms formed by the cooperation of sealing materials such as polytetrafluoroethylene, fluororubber, silicone, epoxy resin, etc., which have certain plasticity, certain strength and good insulation performance, and electrodes. However, in order to ensure the sealing and insulation of the electrode, in the existing various high temperature and high pressure water fluid electrode sealing mechanisms, a large stress (usually including extrusion force and friction force) needs to be applied to the electrode. The stress applied to the material is an important thermodynamic parameter affecting its chemical reaction activity. The type and magnitude of the stress applied to the material largely affect the tendency and rate of the reaction between the material and the high temperature and high pressure water fluid. Therefore, the stress applied to the electrode by the sealing mechanism will undoubtedly change the reaction characteristics of the electrode material in the high temperature and high pressure water fluid, thereby affecting the accuracy of the electrochemical measurement and causing errors in the experimental results. In addition, the stress applied to the electrode by the electrode sealing mechanism is complex and difficult to grasp. Therefore, the error caused by the sealing stress is also difficult to measure and correct. In addition, when brittle materials (such as easily broken mineral materials) are used as electrodes, the stress caused by the electrode sealing mechanism often causes the electrode to break, resulting in the failure of the experiment. Summary of the invention
[0003] Based on the above, the present invention provides a quasi-isostatic electrode sealing mechanism and a method of using the same to solve the technical problems of inaccurate electrochemical measurement results and limited use range caused by existing electrode sealing mechanisms.
[0004] The technical solution of the present invention is: a quasi-isostatic electrode sealing mechanism, used for electrochemical testing of electronic conductivity materials in a high-temperature and high-pressure water fluid environment, the electrode comprising:
[0005] An electrode base, comprising a first base and a second base, wherein the second base is connected to the first base;
[0006] The tested electrode is arranged at an end of the second substrate, the end being the other end opposite to the connection end of the second substrate and the first substrate, and the tested electrode has a testing end, the testing end being the other end opposite to the tested electrode and the end close to the second substrate;
[0007] An electrode lead, one end of which is connected to the electrode to be tested, and the other end of which passes through the electrode base and extends outward;
[0008] A sealed insulating assembly, comprising an insulating sleeve and a fastening member, wherein the insulating sleeve is sleeved on the outer annular surface of the second substrate and the electrode to be tested, and the fastening member is sleeved on the outer surface of the insulating sleeve;
[0009] Among them, in the working state, the electrode under test and the second substrate extend into the fluid of the hydrothermal system, the test end of the electrode under test contacts the fluid, and forms an initial seal by the tiny stress generated by the clamp, and relies on the pressure of the water fluid itself to squeeze the insulating sleeve, thereby achieving a sealing effect under high pressure, so that the electrode under test is in a quasi-isostatic state.
[0010] In one example, the electrode to be tested and the second substrate are cylindrical with the same outer diameter, and the insulating sleeve is tubular.
[0011] In one example, the sealing insulation assembly further includes a protective sleeve, wherein the protective sleeve is sleeved outside the insulation sleeve, and the tightening member is sleeved outside the protective sleeve.
[0012] In one example, the clamping member is a clamping ring, and the clamping ring and the insulating sleeve are in interference connection.
[0013] In one example, the thickness of the outer wall of the protective sleeve near the first substrate end is greater than the thickness of the outer wall near the tested electrode end, and there are two tightening members, which are respectively sleeved on both ends of the protective sleeve.
[0014] In one example, an insulating member is provided between the electrode to be tested and the second substrate, and the electrode lead sequentially passes through the insulating member and the electrode base and then extends outward.
[0015] In one example, the insulating member is made of alumina ceramic or boron nitride.
[0016] In one example, the electrode base is made of titanium or nickel-based alloy.
[0017] In one example, the insulating sleeve is made of fluororubber, polytetrafluoroethylene, talc, boron nitride or pyrophyllite.
[0018] The present invention also provides a method for using a quasi-isostatic electrode, the method comprising:
[0019] Passing the electrode lead through the electrode base and connecting it to one end of the electrode to be tested;
[0020] Putting an insulating sleeve on the outer annular surface of the second substrate and the electrode to be tested;
[0021] The tightening member is sleeved on the outer surface of the insulating sleeve, and pre-pressed to achieve initial sealing between the insulating sleeve, the second substrate and the electrode to be tested;
[0022] The electrode base is fixed on the reactor, and the test end of the electrode to be tested is in contact with the fluid, and the electrode base is fixed on the reactor;
[0023] During the test, the initial seal is formed by the tiny stress generated by the clamp, and the insulating sleeve is squeezed by the pressure of the water fluid itself, thereby achieving a sealing effect under high pressure, so that the electrode under test is in a quasi-isostatic state.
[0024] The beneficial effects of the present invention are as follows: before the test, the working electrode is pre-tightened by the clamping member, so that the insulating sleeve, the second substrate and the electrode to be tested achieve an initial seal; during the electrochemical test, the fluid pressure of the reactor water flow system, especially the fluid contacts and squeezes the outer surface of the insulating sleeve, makes the insulating sleeve more tightly wrap the second substrate and the electrode to be tested, thereby achieving a water pressure seal. Compared with the prior art, this structure has the following two main advantages: First, the electrode to be tested in this structure is in a quasi-isostatic state, which avoids the conventional sealing mechanism causing a large differential stress on the electrode to be tested, causing the electrochemical behavior of the electrode to deviate from the normal state, thereby improving the accuracy of the electrochemical test; second, this mechanism can be used for electrochemical testing of easily breakable brittle materials in high-temperature and high-pressure water fluids, expanding the research objects. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 It is a structural schematic diagram of the quasi-isostatic electrode sealing mechanism;
[0026] Figure 2 A longitudinal cross-sectional view of a quasi-isostatic electrode sealing mechanism;
[0027] Description of reference numerals:
[0028] 10 electrode base, 11 first substrate, 12 second substrate;
[0029] 20 insulation parts;
[0030] 30 tested electrode, 31 testing end;
[0031] 40 electrode leads;
[0032] 50 is a sealing insulation component, 51 is an insulating sleeve, 52 is a protective sleeve, and 53 is a tight hoop ring. DETAILED DESCRIPTION
[0033] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the specific embodiments of the present invention are described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth to facilitate a full understanding of the present invention. However, the present invention can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the present invention, so the present invention is not limited by the specific implementation disclosed below.
[0034] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present invention. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more related listed items.
[0035] See also Figure 1 and Figure 2 An embodiment of the present invention provides a quasi-isostatic electrode sealing structure for electrochemical testing of electronic conductivity materials in a high-temperature and high-pressure water fluid environment. The electrode includes an electrode base 10, an insulating member 20, a tested electrode 30, an electrode lead 40 and a sealed insulating assembly 50.
[0036] The electrode base 10 is installed on the reactor. The electrode base 10 includes a first substrate 11 and a second substrate 12, and the second substrate 12 is connected to the first substrate 11. In one example, the second substrate 12 is vertically connected to the first substrate 11, and the second substrate 12 and the first substrate 11 can be integrally formed. The first substrate 11 is used to be installed on the reactor, and the second substrate 12 is used to extend into the reactor. A through hole is provided on the electrode base 10, and the through hole passes through the first substrate 11 and the second substrate 12. The material of the electrode base 10 can be titanium.
[0037] The insulating member 20 serves to isolate the electrode base 10 from the electrode to be tested 30. The insulating member 20 is stacked on the end of the second substrate 12, which is the other end opposite to the connection end of the second substrate 12 and the first substrate 11. A through hole is provided on the insulating member 20, and the through hole is aligned with the through hole on the electrode base 10. The material of the insulating member 20 can be alumina ceramic or boron nitride.
[0038] The electrode to be tested 30 plays the role of electrochemical testing. The electrode to be tested 30 is installed at the other end of the insulating member 20, which is the other opposite end of the connecting end of the insulating member 20 and the second substrate 12. The electrode to be tested 30 has a test end 31, which is the other opposite end of the electrode to be tested 30 close to one end of the insulating member 20. The test end 31 can be an end face or a part of the electrode to be tested 30 of a predetermined length. In the working state, the test end 31 is located in the high-temperature and high-pressure water fluid in the reactor and contacts with the fluid to obtain a test signal. The material of the electrode to be tested 30 can be a natural single crystal or block conductive mineral, such as yellow copper.
[0039] The electrode lead 40 is used to lead out the test signal. One end of the electrode lead 40 is in contact with the electrode 30 to be tested, and the other end passes through the through holes on the insulating member 20 and the electrode base 10 in sequence and then extends outward. The electrode lead 40 can be a 0.5 mm platinum wire. An insulating ceramic tube can also be set on the electrode lead 40 to play an insulating protection role to avoid direct contact with the electrode base 10, thereby affecting the accuracy of the test.
[0040] The sealing insulation assembly 50 plays the role of preliminarily sealing and fixing the tested electrode 30. The sealing insulation assembly 50 includes an insulation sleeve 51, a protective sleeve 52 and a tight ring.
[0041] The insulating sleeve 51 is sleeved on the outer annular surface of the second substrate 12, the insulating member 20 and the electrode to be tested 30, so that the outer annular surface of the second substrate 12, the insulating member 20 and the electrode to be tested 30 is isolated from the outside. The shape of the insulating sleeve 51 is cylindrical. In the working state, the insulating sleeve 51 is wrapped around the outer annular surface of the second substrate 12, the insulating member 20 and the electrode to be tested 30, so that the second substrate 12, the insulating member 20 and the electrode to be tested 30 are integrally formed into a working electrode. The material of the insulating sleeve 51 can be fluororubber or polytetrafluoroethylene or talc or boron nitride or pyrophyllite.
[0042] The protective sleeve 52 is sleeved on the outside of the insulating sleeve 51 of the insulating sleeve 51 to protect the insulating sleeve 51. The material of the protective sleeve 52 can be a metal material, such as copper. The tight hoop 53 is sleeved on the outer surface of the protective sleeve 52. The tight hoop 53 can be a tight hoop ring, and the tight hoop ring and the insulating sleeve 51 are interference-connected to give pre-pressure to the protective sleeve 52 and the insulating sleeve 51, so as to form the protective sleeve 52, the insulating sleeve 51, the second substrate 12, the insulating member 20 and the tested electrode 30 as a fixed whole. The tight hoop ring can be an integral annular structure or a strip structure, which can be bundled outside the protective sleeve 52. The material of the tight hoop ring can be aluminum. It can also be other metal materials. The number of tight hoop rings can also be multiple, such as 2 or 3, which are respectively tightened on different parts of the protective sleeve 52.
[0043] The thickness of the outer wall of the protective cover 52 near the end of the first substrate 11 is greater than the thickness of the outer wall near the end of the electrode to be tested 30, and gradually transitions from the test electrode end to the end of the first substrate 11. There are two tightening members 53, which are respectively sleeved on the two ends of the protective cover 52. During the test, a tightening ring with a slightly larger inner diameter can be inserted from the test electrode end and gradually moved toward the end of the first substrate 11, and the tightening ring is finally fixed on the end of the protective cover 52 near the first substrate 11, and then another tightening ring with a slightly smaller inner diameter is inserted from the test electrode end and fixed to the outside of the protective cover 52 outside the test end 31. This structure can avoid the problem of the tightening ring squeezing the electrode to be tested 30 during the insertion process, thereby causing inaccurate electrode testing. In addition, since a tightening ring is installed at each end of the protective cover 52, the sealing of the electrode to be tested 30 can also be effectively guaranteed.
[0044] In the quasi-isostatic electrode sealing structure, the tested electrode 30, the insulating member 20 and the second substrate 12 are all cylindrical with the same outer diameter, and the insulating sleeve 51 is tubular. This structure can improve the extrusion sealing effect of the fluid in the hydrothermal system.
[0045] The method of using the above-mentioned quasi-isostatic electrode sealing structure includes: 1. Passing the electrode lead 40 through the electrode base 10 and the insulating member 20 and then connecting it to one end of the electrode 30 to be tested; 2. Sleeving the insulating sleeve 51 on the outer annular surface of the second substrate 12, the insulating member 20 and the electrode 30 to be tested; 3. Sleeving the protective sleeve 52 on the outside of the insulating sleeve 51; 4. Sleeving the tight hoop 53 on the outer surface of the insulating sleeve 51, pre-pressing the protective sleeve 52, the insulating sleeve 51, the second substrate 12, the insulating member 20 and the electrode 30 to be tested to achieve initial sealing; 5. The electrode base 10 is fixedly installed on the reactor, and the second substrate 12, the electrode 30 to be tested, the protective sleeve 52, etc. are extended into the fluid of the hydrothermal system, so that the test end 31 of the electrode 30 to be tested is in contact with the fluid; 6. During the test, the test signal is led out by the electrode lead 40.
[0046] The advantages of the above-mentioned quasi-isostatic electrode sealing mechanism are: before the test, the electrode is pre-tightened by the clamp 53 to achieve an initial seal between the protective sleeve 52, the insulating sleeve 51, the second substrate 12, the insulating member 20 and the electrode 30 to be tested; during the electrochemical test, the fluid pressure of the hydrothermal system of the reactor, especially the fluid contacts and squeezes the outer surface of the protective sleeve 52, makes the protective sleeve 52 and the insulating sleeve 51 more tightly wrap the second substrate 12, the insulating member 20 and the electrode 30 to be tested, thereby achieving a water pressure seal. Compared with the prior art, this structure has the following two advantages: first, the electrode to be tested in this structure is in a quasi-isostatic state, which avoids the conventional sealing mechanism causing a large differential stress on the electrode to be tested, resulting in the electrochemical behavior of the electrode to be tested deviating from the normal state, thereby improving the accuracy of the electrochemical test; second, this mechanism can be used for electrochemical testing of easily broken brittle materials in high-temperature and high-pressure water fluids, expanding the research objects.
[0047] The above-mentioned embodiments only express several implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the patent of the present invention. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.
Claims
1. A quasi-isostatic electrode sealing mechanism for electrochemical testing of electronic conductivity materials in a high-temperature and high-pressure water fluid environment. It is characterized in that The electrode comprises: An electrode base (10) comprises a first base (11) and a second base (12), wherein the second base (12) is connected to the first base (11); The electrode to be tested (30) is arranged at an end of the second substrate (12), the end being the other end opposite to the connection end of the second substrate (12) and the first substrate (11), and the electrode to be tested (30) has a test end (31), the test end (31) being the other end of the electrode to be tested (30) opposite to the end close to the second substrate (12); An electrode lead (40), one end of the electrode lead (40) being connected to the electrode to be tested (30), and the other end of the electrode lead (40) passing through the electrode base (10) and extending outward; A sealed insulating component (50) comprises an insulating sleeve (51) and a tightening member (53), wherein the insulating sleeve (51) is sleeved on the outer annular surfaces of the second substrate (12) and the electrode to be tested (30), and the tightening member (53) is sleeved on the outer surface of the insulating sleeve (51); the sealed insulating component (50) further comprises a protective sleeve (52), wherein the protective sleeve (52) is sleeved outside the insulating sleeve (51), and the tightening member (53) is sleeved outside the protective sleeve (52); the thickness of the outer wall of the protective sleeve (52) near the end of the first substrate (11) is greater than the thickness of the outer wall near the end of the electrode to be tested (30), and there are two tightening members (53), which are respectively sleeved on the two ends of the protective sleeve (52); An insulating member (20) is provided between the electrode to be tested (30) and the second substrate (12), and the electrode lead (40) passes through the insulating member (20) and the electrode base (10) in sequence and then extends outward; in a working state, the electrode to be tested (30) and the second substrate (12) extend into the fluid of the hydrothermal system, the test end (31) of the electrode to be tested (30) contacts the fluid, and an initial seal is formed by the micro stress generated by the tightening member (53), and the insulating sleeve (51) is squeezed by the pressure of the water fluid itself, thereby achieving a sealing effect under high pressure, so that the electrode to be tested is in a quasi-isostatic state.
2. The quasi-isostatic electrode sealing mechanism according to claim 1, It is characterized in that The electrode to be tested (30) and the second substrate (12) are cylindrical with the same outer diameter, and the insulating sleeve (51) is tubular.
3. The quasi-isostatic electrode sealing mechanism according to claim 1, It is characterized in that The tightening member (53) is a tightening ring, and the tightening ring and the insulating sleeve (51) are in interference connection.
4. The quasi-isostatic electrode sealing mechanism according to claim 1, It is characterized in that The material of the insulating member (20) is alumina ceramic or boron nitride.
5. The quasi-isostatic electrode sealing mechanism according to claim 1, It is characterized in that The electrode base (10) is made of titanium or nickel-based alloy.
6. The quasi-isostatic electrode sealing mechanism according to claim 1, It is characterized in that The insulating sleeve (51) is made of fluororubber, polytetrafluoroethylene, talc, boron nitride or pyrophyllite.
7. A method for using the quasi-isostatic electrode sealing mechanism according to any one of claims 1 to 6, It is characterized in that The method comprises: The electrode lead (40) is passed through the electrode base (10) and connected to one end of the electrode to be tested (30); The insulating sleeve (51) is sleeved on the outer annular surface of the second substrate (12) and the electrode to be tested (30); The tightening member (53) is sleeved on the outer surface of the insulating sleeve (51), and pre-pressed so that the insulating sleeve (51), the second substrate (12) and the electrode to be tested (30) achieve initial sealing; The electrode base (10) is fixed on the reaction kettle, and the test end (31) of the electrode to be tested (30) is in contact with the fluid; During the test, an initial seal is formed by the tiny stress generated by the tightening member (53), and the insulating sleeve (51) is squeezed by the pressure of the water fluid itself, thereby achieving a sealing effect under high pressure, and the electrode under test is in a quasi-isostatic state.