Gallium nitride Schottky diode and preparation method thereof

By forming tapered gallium nitride layer protrusions and defect isolation structures in gallium nitride Schottky diodes, the problems of low performance and leakage current caused by dislocations are solved, and the effects of high withstand voltage and low leakage are achieved.

CN112038396BActive Publication Date: 2024-10-15SHANGHAI XINYUANJI SEMICON TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010960821.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-09-14
Publication Date
2024-10-15
Estimated Expiration
2040-09-14

AI Technical Summary

Technical Problem

It is difficult to eliminate dislocations in existing gallium nitride Schottky diodes when growing epitaxial layers, resulting in low device performance, poor withstand voltage characteristics and serious leakage current.

Method used

The MOCVD method is used to form tapered gallium nitride layer protrusions on the composite pattern substrate, and a gallium nitride layer is formed on it. The defect isolation structure is formed by stripping off the etching solution and filling the insulating layer to concentrate and passivate the defects and cut them off. carrier transport path.

Benefits of technology

The withstand voltage characteristics and anti-leakage characteristics of the gallium nitride Schottky diode are improved, and the device performance is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112038396B_ABST
    Figure CN112038396B_ABST
Patent Text Reader

Abstract

The invention provides a gallium nitride Schottky diode and a preparation method thereof. A conical gallium nitride layer protrusion and a gallium nitride layer are formed by an MOCVD method. The doping concentration of the conical gallium nitride layer protrusion is greater than that of the gallium nitride layer, and the conical gallium nitride layer protrusion and the gallium nitride layer form a defect closing area, so that defects are concentrated. In the process of stripping a growth substrate by using an etching solution, a groove can be formed in the defect closing area, and a defect isolation structure is formed by filling an insulating layer, so that the defect is passivated, and the vertical projection of the defect closing area is completely located in the defect isolation structure, so that the transmission path of the carrier is cut off in the vertical direction through the defect isolation structure. Furthermore, the conical gallium nitride layer protrusion can gather carriers to the top of the cone for transmission, so that the current is guided and the carriers can be avoided from passing through the edge defect closing area. The invention can obtain a gallium nitride Schottky diode with high withstand voltage and good anti-leakage characteristics, so as to improve the device performance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a gallium nitride Schottky diode and a preparation method thereof. Background Art

[0002] With the widespread use of high-power devices in various fields such as military and civilian applications, people's demand for Schottky diodes is increasing, and their performance requirements are getting higher and higher. For a long time, people have been using silicon-based Schottky diode devices, but with the development of silicon technology over the years, the performance of the corresponding silicon-based Schottky diodes has approached its theoretical limit.

[0003] As the third generation wide bandgap semiconductor material, GaN has the characteristics of large bandgap width, large breakdown electric field, and high electron drift velocity, making it more suitable for making high-temperature, high-frequency, radiation-resistant and high-power devices, and therefore has attracted much attention. Schottky diodes made of GaN also have excellent characteristics of high temperature resistance, high voltage resistance and low on-resistance, and are an ideal material for making a new generation of Schottky diodes.

[0004] At present, in addition to the problems of GaN materials themselves, the reverse breakdown voltage and leakage current of GaN Schottky diodes are still far from the ideal values ​​in theory. Many research groups around the world are looking for different ways to solve and improve this problem of GaN Schottky diodes from the perspective of structure or process, so as to improve the withstand voltage characteristics of GaN Schottky diodes and reduce their leakage current so that the devices can work at higher power.

[0005] In the prior art, when preparing GaN Schottky diodes, when growing GaN epitaxial layers, some dislocations are inevitably generated in the GaN epitaxial layers. These dislocations reduce the withstand voltage characteristics of the GaN Schottky diodes and cause leakage current, thereby reducing device performance.

[0006] Therefore, it is necessary to provide a novel GaN Schottky diode and a preparation method thereof to improve the withstand voltage characteristics of the GaN Schottky diode and reduce its leakage current phenomenon to improve device performance. Summary of the invention

[0007] In view of the above-mentioned shortcomings of the prior art, an object of the present invention is to provide a gallium nitride Schottky diode and a method for preparing the same, so as to solve the problem of low device performance caused by difficulty in eliminating dislocations in the gallium nitride epitaxial layer in the prior art.

[0008] To achieve the above-mentioned object and other related objects, the present invention provides a method for preparing a gallium nitride Schottky diode, comprising the following steps:

[0009] Providing a composite pattern substrate, the composite pattern substrate comprising a growth substrate, a dielectric layer protrusion and a buffer layer;

[0010] Using MOCVD method, forming a conical gallium nitride layer protrusion on the composite pattern substrate, wherein the cone top of the conical gallium nitride layer protrusion is away from the composite pattern substrate;

[0011] Forming a gallium nitride layer on the conical gallium nitride layer protrusion by using a MOCVD method, wherein the doping concentration of the conical gallium nitride layer protrusion is greater than that of the gallium nitride layer, and the conical gallium nitride layer protrusion and the gallium nitride layer form a defective closure area;

[0012] Using a first etching solution to remove the protrusions of the dielectric layer to form a cavity;

[0013] Using a second etching solution to remove the buffer layer to peel off the growth substrate, and forming a groove in the defect closing area by the second etching solution;

[0014] Depositing an insulating layer to fill the groove to form a defect isolation structure, wherein the vertical projection of the defect closing area is completely located within the defect isolation structure;

[0015] Planarization is performed to reveal the protrusions and defect isolation structure of the gallium nitride layer.

[0016] Optionally, before forming the cavity, the method further includes the steps of forming a temporary supporting substrate on the surface of the gallium nitride layer away from the composite pattern substrate, and forming a metal substrate on the exposed surface of the conical gallium nitride layer protrusion, and then removing the temporary supporting substrate, and separately forming a Schottky anode metal layer in contact with the gallium nitride layer and a cathode metal layer in contact with the metal substrate.

[0017] Optionally, before forming the cavity, the method further includes the steps of sequentially forming a Schottky anode metal layer in contact with the gallium nitride layer and a metal substrate in contact with the Schottky anode metal layer on a surface of the gallium nitride layer away from the composite pattern substrate, and forming a cathode metal layer on the exposed protruding surface of the conical gallium nitride layer.

[0018] Optionally, the conical gallium nitride layer protrusions are arranged at intervals or in contact with each other.

[0019] Optionally, the dielectric layer protrusion includes a SiO2 layer, a SiON x Layer or SiN x The buffer layer includes an AlN layer, an Al x Ga 1-x The defect isolation structure includes a SiO2 layer, a SiONx Layer or SiN x The first etching solution is HF solution or BOE solution, and the second etching solution is KOH solution, NaOH solution or a mixed solution of H2SO4 and H2PO4.

[0020] The present invention also provides a gallium nitride Schottky diode, the gallium nitride Schottky diode comprising:

[0021] Conical GaN layer protrusion;

[0022] A gallium nitride layer, wherein the gallium nitride layer covers the conical gallium nitride layer protrusion, the doping concentration of the conical gallium nitride layer protrusion is greater than that of the gallium nitride layer, and the conical gallium nitride layer protrusion and the gallium nitride layer form a defective closure area;

[0023] The defect isolation structure is covered by the gallium nitride layer, the vertical projection of the defect closing area is completely located in the defect isolation structure, and the defect isolation structure and the conical gallium nitride layer protrusions are arranged alternately.

[0024] Optionally, it further comprises a Schottky anode metal layer in contact with the gallium nitride layer, a metal substrate in contact with the conical gallium nitride layer protrusion, and a cathode metal layer in contact with the metal substrate.

[0025] Optionally, it further includes a Schottky anode metal layer in contact with the gallium nitride layer, a metal substrate in contact with the Schottky anode metal layer, and a cathode metal layer in contact with the conical gallium nitride layer protrusion.

[0026] Optionally, the width of the cone bottom of the conical gallium nitride layer protrusion ranges from 1 μm to 5 μm, and the height of the conical gallium nitride layer protrusion ranges from 1 μm to 5 μm.

[0027] Optionally, the width of the defect isolation structure ranges from 0.2 μm to 2 μm, the height of the defect isolation structure ranges from 0.1 μm to 1.5 μm; and the defect isolation structure includes a tapered defect isolation structure.

[0028] As described above, the gallium nitride Schottky diode and the preparation method thereof of the present invention have the following beneficial effects:

[0029] A conical GaN layer protrusion is formed on the composite pattern substrate by MOCVD method to obtain a conical GaN layer protrusion with high doping, high carrier concentration and high crystal quality, and then a GaN layer is formed on the conical GaN layer protrusion by MOCVD method. Since the conical GaN layer protrusion has a conical morphology, the conical GaN layer protrusion and the GaN layer can form a defective closing area, so that the defects are concentrated;

[0030] In the process of stripping the growth substrate by using an etching liquid, the etching liquid can form a groove in the defect closing area, and a defect isolation structure can be formed by filling the insulating layer, so that the defect is passivated, and the vertical projection of the defect closing area is completely located in the defect isolation structure, so that the transmission path of the carrier can be cut off in the vertical direction through the defect isolation structure;

[0031] Furthermore, since the conical GaN layer protrusion has a conical morphology, the carriers can be gathered to the top of the conical GaN layer protrusion like a funnel to transmit the carriers, so that the current is guided and the carriers can be prevented from passing through the defect closure area with more defects in the edge area;

[0032] The gallium nitride Schottky diode and the preparation method thereof of the present invention can obtain a gallium nitride Schottky diode with high withstand voltage characteristics and good anti-leakage characteristics, thereby improving device performance. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] Figure 1 Shown is a schematic diagram of the process flow for preparing a gallium nitride Schottky diode in an embodiment.

[0034] Figure 2 to Figure 15 It shows a schematic diagram of the structure presented in each step of preparing a gallium nitride Schottky diode in Example 1.

[0035] Fig.16 The scanning electron microscope image of the conical GaN layer protrusion formed in Example 1 is shown.

[0036] Figure 17 to Figure 27 It shows a schematic diagram of the structure presented in each step of preparing a gallium nitride Schottky diode in Example 2.

[0037] Component number description

[0038] 101, 201 composite graphic substrate

[0039] 1011, 2011 Growth substrate

[0040] 1012, 2012 Dielectric layer protrusion

[0041] 1013, 2013 Buffer layer

[0042] 102, 202 Conical GaN layer protrusion

[0043] 103, 203 GaN layer

[0044] 104 Temporary support substrate

[0045] 105, 205 Hollow

[0046] 106, 206 grooves

[0047] 107, 207 Defect Isolation Structure

[0048] 108, 208 bonding metal layer

[0049] 109, 209 Metal substrate

[0050] 110, 210 cathode metal layer

[0051] 111, 211 Schottky anode metal layer

[0052] 112, 212 isolation layer

[0053] A, A' defect closure area

[0054] D, d, D', d' Width

[0055] H, h, H', h' Height DETAILED DESCRIPTION

[0056] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.

[0057] For example, when describing the embodiments of the present invention in detail, for the sake of convenience, the cross-sectional view showing the device structure will not be partially enlarged according to the general scale, and the schematic view is only an example, which should not limit the scope of protection of the present invention. In addition, in actual production, the three-dimensional space dimensions of length, width and depth should be included.

[0058] For ease of description, spatial relational terms such as "under", "below", "below", "below", "above", "on", etc. may be used herein to describe the relationship of one element or feature shown in the drawings to other elements or features. It will be understood that these spatial relational terms are intended to include other directions of the device in use or operation in addition to the directions depicted in the drawings. In addition, when a layer is referred to as being "between" two layers, it can be the only layer between the two layers, or there can be one or more intervening layers. As used herein, "between..." means including the end point values.

[0059] In the context of the present application, a structure in which a first feature is described as being "above" a second feature may include embodiments in which the first and second features are formed in direct contact, and may also include embodiments in which additional features are formed between the first and second features, such that the first and second features may not be in direct contact.

[0060] It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner, and therefore the illustrations only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.

[0061] Embodiment 1

[0062] See also Figures 1 to 16 This embodiment provides a method for preparing a gallium nitride Schottky diode, comprising the following steps:

[0063] Providing a composite pattern substrate 101, wherein the composite pattern substrate 101 includes a growth substrate 1011, a dielectric layer protrusion 1012 and a buffer layer 1013;

[0064] Using MOCVD method, forming a conical GaN layer protrusion 102 on the composite pattern substrate 101, wherein the cone top of the conical GaN layer protrusion 102 is away from the composite pattern substrate 101;

[0065] A gallium nitride layer 103 is formed on the conical gallium nitride layer protrusion 102 by using a MOCVD method, wherein the doping concentration of the conical gallium nitride layer protrusion 102 is greater than that of the gallium nitride layer 103, and the conical gallium nitride layer protrusion 102 and the gallium nitride layer 103 form a defective closing region A;

[0066] The dielectric layer protrusion 1012 is removed by using a first etching solution to form a cavity 105;

[0067] The buffer layer 1013 is removed by using a second etching solution to peel off the growth substrate 1011, and a groove 106 is formed in the defect closing area A by using the second etching solution;

[0068] Depositing an insulating layer to fill the groove 106 to form a defect isolation structure 107, and the vertical projection of the defect closing area A is completely located in the defect isolation structure 107;

[0069] Planarization is performed to expose the GaN layer protrusion 102 and the defect isolation structure 107 .

[0070] In this embodiment, the conical GaN layer protrusion 102 is formed on the composite pattern substrate 101 by MOCVD method to obtain the conical GaN layer protrusion 102 with high doping, high carrier concentration and high crystal quality, and then the GaN layer 103 is formed on the conical GaN layer protrusion 102 by MOCVD method. Since the conical GaN layer protrusion 102 has a conical morphology, the conical GaN layer protrusion 102 and the GaN layer 103 can form the defect closing area A, so that defects such as dislocations are concentrated to obtain defect concentration;

[0071] In the process of stripping the growth substrate 1011 by using the second etching solution, the second etching solution can form the groove 106 in the defect closing area A, and the defect isolation structure 107 can be formed by filling the insulating layer, so that the defect is passivated, and the vertical projection of the defect closing area A is completely located in the defect isolation structure 107, so that the transmission path of the carrier can be cut off in the vertical direction through the defect isolation structure 107;

[0072] Furthermore, since the conical GaN layer protrusion 102 has a conical morphology, the carriers can be gathered to the top of the conical GaN layer protrusion 102 like a funnel for transmission, so that the current is guided and the carriers can be prevented from passing through the defect closing area A where there are more defects in the edge area;

[0073] The method for preparing the gallium nitride Schottky diode of this embodiment can obtain the gallium nitride Schottky diode having high withstand voltage characteristics and good anti-leakage characteristics, thereby improving device performance.

[0074] The specific preparation steps are as follows:

[0075] See also Figure 1 First, the composite pattern substrate 101 is provided. The composite pattern substrate 101 includes a growth substrate 1011, a dielectric layer protrusion 1012 and a buffer layer 1013.

[0076] Specifically, in this embodiment, the dielectric layer protrusion 1012 is located between the growth substrate 1011 and the buffer layer 1013, but it is not limited thereto. In another embodiment, the buffer layer 1013 may also be located below the dielectric layer protrusion 1012, and there is no excessive restriction here. Among them, the growth substrate 1011 may include one or a combination of a sapphire substrate, a Si substrate, a SiC substrate, a ZnO substrate, and a GaN substrate, which can be selected according to needs, and there is no excessive restriction here. In this embodiment, a sapphire substrate is preferably used, but it is not limited thereto.

[0077] As an example, the material of the dielectric layer protrusion 1012 may include SiO2 layer, SiON x Layer or SiN x A combination of one or more layers.

[0078] As an example, the dielectric layer protrusions 1012 are arranged in a spaced arrangement or in contact with each other; when the dielectric layer protrusions 1012 are arranged in a spaced arrangement, they may be in a square, rectangular, elliptical, trapezoidal, or a combination thereof.

[0079] As an example, the buffer layer 103 includes an AlN layer, an Al x Ga 1-x A combination of one or more of an N layer or a ZnO layer.

[0080] Specifically, in this embodiment, the dielectric layer protrusions 1012 are made of SiO2 layer; the dielectric layer protrusions 1012 are arranged at intervals, and the shape of the dielectric layer protrusions 1012 is rectangular, and the width range includes 0.5μm to 3μm, such as 1.0μm, 1.5μm, 2μm, 2.5μm, etc. There are gap grooves between adjacent dielectric layer protrusions 1012, and the width of the gap grooves includes 0.5μm to 2μm, such as 1.0μm, 1.5μm, etc., and the depth range includes 0.5μm to 1μm, such as 0.6μm, 0.8μm, etc. The buffer layer 103 is made of AlN layer. However, the selection of the material and shape of the dielectric layer protrusions 1012 and the buffer layer 103 is not limited to this, and no excessive restrictions are made here.

[0081] Next, see Figure 3 The conical GaN layer protrusion 102 is formed on the composite pattern substrate 101 by using MOCVD method, and the cone top of the conical GaN layer protrusion 102 is far away from the composite pattern substrate 101.

[0082] As an example, the conical GaN layer protrusions 102 are arranged at intervals or in contact with each other.

[0083] Specifically, in this embodiment, the conical GaN layer protrusions 102 are arranged in contact with each other, but are not limited thereto. In another embodiment, by controlling MOCVD process parameters, the conical GaN layer protrusions 102 arranged at intervals may also be formed. No excessive limitation is made here.

[0084] Among them, since the conical GaN layer protrusions 102 have a conical morphology and the adjacent conical GaN layer protrusions 102 are in contact with each other, during the growth process of the adjacent conical GaN layer protrusions 102, a dislocation aggregation area, i.e., a defect closure area A, will be formed between the adjacent conical GaN layer protrusions 102, such as Figure 3and Fig.16 Of course, when the conical GaN layer protrusions 102 are arranged at intervals, the defect closing area A can also be formed in the subsequent GaN layer 103, which will not be described here.

[0085] Next, see Figure 4 A gallium nitride layer 103 is formed on the conical gallium nitride layer protrusion 102 by using an MOCVD method. The doping concentration of the conical gallium nitride layer protrusion 102 is greater than that of the gallium nitride layer 103 , and the conical gallium nitride layer protrusion 102 and the gallium nitride layer 103 form the defect closure area A.

[0086] Specifically, the growth of the gallium nitride layer 103 also adopts the MOCVD method to epitaxially grow from the surface of the conical gallium nitride layer protrusion 102 to the outside to form the gallium nitride layer 103 with a conical morphology, and by controlling the process parameters of the MOCVD method, the following can be finally obtained: Figure 5 The gallium nitride layer 103 has a flat surface as shown, and when the gallium nitride layer 103 is epitaxially grown, the gallium nitride layer 103 also forms a defect aggregation area between adjacent gallium nitride layers 103, that is, the defect closing area A extends into the gallium nitride layer 103, and as the defect closing area A extends along the conical gallium nitride layer protrusion 102 toward the gallium nitride layer 103, the density of defects will gradually weaken until it disappears, so that the defects such as dislocations in the growth process of the conical gallium nitride layer protrusion 102 and the gallium nitride layer 103 can be concentrated through the defect closing area A, thereby reducing the defect probability in other areas.

[0087] See also Figure 6 to Figure 15 As an example, this embodiment also includes the steps of forming a temporary supporting substrate 104 on the surface of the gallium nitride layer 103 away from the composite pattern substrate 101 before forming the cavity 105, and forming a metal substrate 109 on the surface of the exposed conical gallium nitride layer protrusion 102, and then removing the temporary supporting substrate 104, and forming a Schottky anode metal layer 111 in contact with the gallium nitride layer 103 and a cathode metal layer 110 in contact with the metal substrate 109.

[0088] Specifically, Figure 6 First, the temporary support substrate 104 is formed on the surface of the gallium nitride layer 103 to provide support and facilitate subsequent process operations. The material of the temporary support substrate 104 is not overly restricted here and can be selected according to needs.

[0089] Next, see Figure 7, a first etching solution is used to remove the dielectric layer protrusion 1012 to form the cavity 105, wherein the first etching solution includes an HF solution or a BOE solution that reacts with the dielectric layer protrusion 1012, and the type, action time, temperature, etc. of the first etching solution can be selected as needed and are not excessively restricted here.

[0090] Next, see Figure 8 Based on the void 105 , the buffer layer 1013 is removed by a second etching solution to peel off the growth substrate 1011 , and a groove 106 is formed in the defect closing region A by the second etching solution.

[0091] As an example, the second corrosion solution is a KOH solution, a NaOH solution, or a mixed solution of H2SO4 and H2PO4.

[0092] Specifically, the buffer layer 1013 can be removed by the second etching solution to peel off the growth substrate 1011, and because the second etching solution can react with the gallium nitride material, the second etching solution can remove part of the gallium nitride layer 103, especially at the defect closing area A, due to the presence of dislocation, the second etching solution is easy to form the groove 106 here, so as to remove part of the defect dense area and form the groove 106. Among them, since the density of defects decreases from bottom to top, it is preferred that the morphology of the groove 106 includes a cone to further remove the relatively dense defect area at the bottom.

[0093] Next, see Fig. 9 , an insulating layer is deposited to fill the groove 106 to form a defect isolation structure 107 , and the vertical projection of the defect closing area A is completely located within the defect isolation structure 107 .

[0094] As an example, the defect isolation structure 107 includes a SiO2 layer, a SiON x Layer or SiN x A combination of one or more layers.

[0095] Specifically, since the vertical projection of the defect closing region A is completely located within the defect isolation structure 107, the defect isolation structure 107 can completely cut off the carrier transmission path in the vertical direction, thereby effectively avoiding the generation of leakage current and improving the withstand voltage characteristics.

[0096] Next, see Fig.10 , and planarization is performed to expose the GaN layer protrusion 102 and the defect isolation structure 107 .

[0097] Next, see Fig.11A bonding metal layer 108 may be first formed on the exposed surface of the conical gallium nitride layer protrusion 102 , and then the metal substrate 109 may be formed through the bonding metal layer 108 .

[0098] Next, see Fig.12 , using the bonding metal layer 108 and the metal substrate 109 as support, remove the temporary support substrate 104.

[0099] Next, see Fig.13 , Fig.14 and Fig.15 , respectively forming a Schottky anode metal layer 111 in contact with the gallium nitride layer 103 and a cathode metal layer 110 in contact with the metal substrate 109 , wherein the step of forming an isolation layer 112 in the Schottky anode metal layer 111 is also included.

[0100] The preparation of the Schottky anode metal layer 111 and the cathode metal layer 110 is not limited thereto, and the order of preparation can be changed according to specific preparation requirements, and no excessive restrictions are made here.

[0101] This embodiment also provides a gallium nitride Schottky diode, see Fig.15 The GaN Schottky diode comprises a conical GaN layer protrusion 102, a GaN layer 103 and a defect isolation structure 107. The GaN layer 103 covers the conical GaN layer protrusion 102, the doping concentration of the conical GaN layer protrusion 102 is greater than that of the GaN layer, and the conical GaN layer protrusion 102 and the GaN layer 103 form a defect closure area A; the GaN layer 103 covers the defect isolation structure 107, the vertical projection of the defect closure area A is completely located in the defect isolation structure 107, and the defect isolation structure 107 and the conical GaN layer protrusion 102 are arranged alternately.

[0102] Specifically, the GaN Schottky diode in this embodiment can be prepared by the above-mentioned preparation process, but is not limited thereto. The formation method, material and structure of the GaN Schottky diode will not be described in detail here.

[0103] As an example, it also includes a Schottky anode metal layer 111 in contact with the gallium nitride layer 103 , a metal substrate 109 in contact with the conical gallium nitride layer protrusion 102 , and a cathode metal layer 110 in contact with the metal substrate 109 .

[0104] Specifically, a bonding metal layer 108 is further provided between the conical gallium nitride layer protrusion 102 and the metal substrate 109 , and an isolation layer 112 is further provided in the Schottky anode metal layer 111 .

[0105] As an example, the range of the cone bottom width D of the cone-shaped GaN layer protrusion 112 includes 1 μm to 5 μm, and the range of the height H of the cone-shaped GaN layer protrusion 112 includes 1 μm to 5 μm.

[0106] Specifically, the cone bottom width D of the cone-shaped GaN layer protrusion 102 may include 2 μm, 3 μm, 4 μm, etc., and the height H of the cone-shaped GaN layer protrusion 102 may include 2 μm, 3 μm, 4 μm, etc.

[0107] As an example, the width d of the defect isolation structure 107 ranges from 0.2 μm to 2 μm, and the height h of the defect isolation structure 107 ranges from 0.1 μm to 1.5 μm; the defect isolation structure 107 includes a tapered defect isolation structure.

[0108] Specifically, the width d of the defect isolation structure 107 may include 0.2μm, 0.4μm, 0.5μm, 0.6μm, 0.8μm, 1μm, 1.5μm, etc., and the height h of the defect isolation structure 107 may include 0.2μm, 0.4μm, 0.5μm, 0.6μm, 0.8μm, 1μm, 1.2μm, etc.

[0109] The gallium nitride Schottky diode in this embodiment is tested by XRD, and the 002RC FWHM of the gallium nitride crystal is less than 80sec, and the 102RC FWHM is less than 100sec; through the dislocation concentration technology and the dislocation passivation technology, as well as the current conduction technology, the gallium nitride Schottky diode with a vertical structure is manufactured and can withstand large current and high voltage.

[0110] Embodiment 2

[0111] See also Figure 17 to Figure 27 This embodiment also provides another method for preparing a gallium nitride Schottky diode, which is different from the first embodiment mainly in that: in this embodiment, a composite pattern substrate 201 with different morphologies is used to form spaced conical gallium nitride layer protrusions 202, and no temporary supporting substrate is required to prepare the Schottky anode metal layer 211 and the cathode metal layer 210, as follows:

[0112] See also Fig.17 First, the composite pattern substrate 201 is provided. The composite pattern substrate 201 includes a growth substrate 2011, a dielectric layer protrusion 2012 and a buffer layer 2013.

[0113] In this embodiment, the dielectric layer protrusion 2012 is located on the surface of the buffer layer 2013, but it is not limited thereto. The material and morphology of the growth substrate 2011, buffer layer 2013 and dielectric layer protrusion 2012 can be found in the first embodiment and will not be described in detail here.

[0114] Next, see Fig.18 , the conical GaN layer protrusions 202 are formed on the composite pattern substrate 201 by MOCVD, and the cone tops of the conical GaN layer protrusions 202 are away from the composite pattern substrate 201. In this embodiment, the conical GaN layer protrusions 102 are arranged at intervals, but are not limited to this. Please refer to the first embodiment, which will not be described here.

[0115] Next, see Fig.19 and Fig. 20 A gallium nitride layer 203 is formed on the conical gallium nitride layer protrusion 202 by MOCVD method. The doping concentration of the conical gallium nitride layer protrusion 202 is greater than that of the gallium nitride layer 203. The conical gallium nitride layer protrusion 202 and the gallium nitride layer 203 form the defect closing area A'. The function of the defect closing area A' can be found in Example 1 and will not be described in detail here.

[0116] See also Figure 21 to Figure 27 In this embodiment, before forming the cavity 205, a Schottky anode metal layer 211 in contact with the gallium nitride layer 203 and a metal substrate 209 in contact with the Schottky anode metal layer 211 are sequentially formed on the surface of the gallium nitride layer 203 away from the composite pattern substrate 201, and a cathode metal layer 210 is formed on the surface of the exposed conical gallium nitride layer protrusion 202.

[0117] For details, see Fig.21 The Schottky anode metal layer 211 and the isolation layer 212 are first formed on the surface of the gallium nitride layer 203, and then refer to Fig. 22 A bonding metal layer 208 is formed and a metal substrate 209 is formed through the bonding metal layer 208 , so that subsequent processes are performed with the metal substrate 209 as a support.

[0118] Next, see Fig.23 , a first etching solution is used to remove the dielectric layer protrusion 2012 to form the cavity 205, wherein the first etching solution includes an HF solution or a BOE solution that reacts with the dielectric layer protrusion 2012, and the type, action time, temperature, etc. of the first etching solution can be set as needed, and no excessive restrictions are imposed here.

[0119] Next, see Fig.24 and Fig.25Based on the cavity 205, the buffer layer 2013 is removed by a second etching solution to peel off the growth substrate 2011, and a groove 206 is formed in the defect closing area A' by the second etching solution. The second etching solution is a KOH solution, a NaOH solution, or a mixed solution of H2SO4 and H2PO4. The formation process of the groove 206 is not described here, and can refer to the first embodiment.

[0120] Next, see Fig.26 , an insulating layer is deposited to fill the groove 206 to form a defect isolation structure 207 , and the vertical projection of the defect closing area A′ is completely located within the defect isolation structure 207 .

[0121] Specifically, the defect isolation structure 207 includes a SiO2 layer, a SiON x Layer or SiN x Since the vertical projection of the defect closing region A' is completely located within the defect isolation structure 207, the carrier transmission path can be completely cut off in the vertical direction through the defect isolation structure 207, thereby effectively avoiding leakage current and improving the withstand voltage characteristics. Wherein, the defect isolation structure 207 includes a conical defect isolation structure.

[0122] Next, see Fig. 27 , planarization is performed to expose the GaN layer protrusion 202 and the defect isolation structure 207 , and a cathode metal layer 210 is formed on the surface of the exposed conical GaN layer protrusion 202 .

[0123] The preparation of the gallium nitride Schottky diode described above is not limited to this, and the sequence can be changed according to specific preparation requirements. For the material, structure, etc., please refer to Example 1, and no excessive restrictions are made here.

[0124] This embodiment also provides a gallium nitride Schottky diode, see Fig. 27 The GaN Schottky diode comprises a conical GaN layer protrusion 202, a GaN layer 203 and a defect isolation structure 207. The GaN layer 203 covers the conical GaN layer protrusion 202, the doping concentration of the conical GaN layer protrusion 202 is greater than that of the GaN layer 203, and the conical GaN layer protrusion 202 and the GaN layer 203 form a defect closure area A'; the GaN layer 203 covers the defect isolation structure 207, the vertical projection of the defect closure area A' is completely located in the defect isolation structure 207, and the defect isolation structure 207 and the conical GaN layer protrusion 202 are arranged alternately.

[0125] Specifically, the gallium nitride Schottky diode in this embodiment can be prepared by the above-mentioned preparation process, but is not limited thereto. The formation method, material and structure of the gallium nitride Schottky diode are not described in detail here.

[0126] As an example, it also includes a Schottky anode metal layer 211 in contact with the gallium nitride layer 203 , a metal substrate 209 in contact with the Schottky anode metal layer 211 , and a cathode metal layer 210 in contact with the conical gallium nitride layer protrusion 202 .

[0127] Specifically, a bonding metal layer 208 is further provided between the Schottky anode metal layer 211 and the metal substrate 209 , and an isolation layer 212 is further provided in the Schottky anode metal layer 212 .

[0128] As an example, the cone bottom width D' of the conical gallium nitride layer protrusion 202 ranges from 1 μm to 5 μm, and the height H' of the conical gallium nitride layer protrusion 202 ranges from 1 μm to 5 μm; for example, the cone bottom width D' of the conical gallium nitride layer protrusion 202 may include 2 μm, 3 μm, 4 μm, etc., and the height H' of the conical gallium nitride layer protrusion 202 may include 2 μm, 3 μm, 4 μm, etc.

[0129] As an example, the width d' of the defect isolation structure 207 ranges from 0.2 μm to 2 μm, and the height h' of the defect isolation structure 207 ranges from 0.1 μm to 1.5 μm; the defect isolation structure 207 includes a tapered defect isolation structure. For example, the width d of the defect isolation structure 207 may include 0.2 μm, 0.4 μm, 0.5 μm, 0.6 μm, 0.8 μm, 1 μm, 1.5 μm, etc., and the height h of the defect isolation structure 207 may include 0.2 μm, 0.4 μm, 0.5 μm, 0.6 μm, 0.8 μm, 1 μm, 1.2 μm, etc.

[0130] The gallium nitride Schottky diode in this embodiment is tested by XRD, and the 002RC FWHM of the gallium nitride crystal is less than 80sec, and the 102RC FWHM is less than 100sec; through the dislocation concentration technology and the dislocation passivation technology, as well as the current conduction technology, the gallium nitride Schottky diode with a vertical structure is manufactured and can withstand large current and high voltage.

[0131] In summary, the gallium nitride Schottky diode and the preparation method thereof of the present invention form a conical gallium nitride layer protrusion on a composite pattern substrate by MOCVD method to obtain a conical gallium nitride layer protrusion with high doping, high carrier concentration and high crystal quality, and then form a gallium nitride layer on the conical gallium nitride layer protrusion by MOCVD method, and because the conical gallium nitride layer protrusion has a conical morphology, the conical gallium nitride layer protrusion and the gallium nitride layer can form a defective closure area, so that the defects are concentrated; in the process of stripping the growth substrate by using an etching solution, the etching solution can form a groove in the defect closure area, and by filling the insulating layer, a defective closure area can be formed. The isolation structure passivates the defects, and the vertical projection of the defect closing area is completely located within the defect isolation structure, so that the carrier transmission path can be cut off vertically by the defect isolation structure; further, since the conical gallium nitride layer protrusion has a conical morphology, the carriers can be gathered to the cone top of the conical gallium nitride layer protrusion like a funnel for transmission, so that the current is guided and the carriers can be avoided from passing through the defect closing area with more defects in the edge area; the gallium nitride Schottky diode of the present invention and the preparation method thereof can obtain a gallium nitride Schottky diode with high withstand voltage characteristics and good anti-leakage characteristics, thereby improving the device performance.

[0132] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A method for preparing a gallium nitride Schottky diode, characterized in that: The following steps are involved: Providing a composite pattern substrate, the composite pattern substrate comprising a growth substrate, a dielectric layer protrusion and a buffer layer, wherein gap grooves are provided between adjacent dielectric layer protrusions, and the width of the gap grooves is 0.5 μm to 2 μm, and the depth of the gap grooves is 0.5 μm to 1 μm; Using MOCVD method, forming a conical gallium nitride layer protrusion on the composite pattern substrate, wherein the cone top of the conical gallium nitride layer protrusion is away from the composite pattern substrate; A gallium nitride layer is formed on the conical gallium nitride layer protrusion by using MOCVD method, wherein the doping concentration of the conical gallium nitride layer protrusion is greater than that of the gallium nitride layer, and the conical gallium nitride layer protrusion and the gallium nitride layer form a defective closure area, and the growth of the gallium nitride layer also adopts MOCVD method to epitaxially grow from the surface of the conical gallium nitride layer protrusion to the outside to form the gallium nitride layer with a conical morphology, and when the gallium nitride layer is epitaxially grown, the gallium nitride layer also forms a defect aggregation area between adjacent gallium nitride layers; Using a first etching solution to remove the protrusions of the dielectric layer to form a cavity; Using a second etching solution to remove the buffer layer to peel off the growth substrate, and forming a groove in the defect closing area by the second etching solution; Depositing an insulating layer to fill the groove to form a defect isolation structure, wherein the vertical projection of the defect closing area is completely located within the defect isolation structure; Performing planarization to reveal the protrusions and defect isolation structure of the gallium nitride layer; Among them, before forming the said cavity, it also includes the steps of forming a temporary supporting substrate on the surface of the said gallium nitride layer away from the said composite pattern substrate, and forming a metal substrate on the exposed surface of the said conical gallium nitride layer protrusion, and then removing the said temporary supporting substrate, and respectively forming a Schottky anode metal layer in contact with the said gallium nitride layer and a cathode metal layer in contact with the said metal substrate; or before forming the said cavity, it also includes the steps of sequentially forming a Schottky anode metal layer in contact with the said gallium nitride layer and a metal substrate in contact with the said Schottky anode metal layer on the surface of the said gallium nitride layer away from the said composite pattern substrate, and forming a cathode metal layer on the exposed surface of the said conical gallium nitride layer protrusion.

2. The method for preparing a gallium nitride Schottky diode according to claim 1, characterized in that: The conical GaN layer protrusions are arranged at intervals or in contact with each other.

3. The method for preparing a gallium nitride Schottky diode according to claim 1, characterized in that: The dielectric layer protrusion includes SiO2 layer, SiON x Layer or SiN x The buffer layer includes an AlN layer, an Al x Ga 1-x The defect isolation structure includes a SiO2 layer, a SiON x Layer or SiN x The first etching solution is HF solution or BOE solution, and the second etching solution is KOH solution, NaOH solution or a mixed solution of H2SO4 and H2PO4.