RRAM, integrated chip and forming method thereof
By using a top electrode and a conductive barrier layer containing metal elements and non-metal elements in the RRAM unit to block the diffusion of non-metal elements, the problem of small difference in the RRAM unit switching window and parasitic resistance is solved, and the manufacturing yield and reliability are improved.
Patent Information
- Application Number
- CN202010592590.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-06-24
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2040-06-24
AI Technical Summary
The difference in the switching window between the high resistance state (HRS) and the low resistance state (LRS) of existing RRAM cells is reduced, resulting in reduced manufacturing yield and reliability, and nitrogen in the top electrode may diffuse into the active metal layer Undesirable switching layers are formed, increasing parasitic resistance.
A top electrode including metal elements and non-metal elements is used. The top electrode barrier layer blocks or slows down the diffusion of non-metal elements (such as nitrogen) to the active metal layer. The top electrode is configured with a conductive barrier layer to reduce the oxygen reactivity of the top electrode. , and form the top electrode barrier layer and top electrode through the PVD process to ensure that non-metallic elements do not diffuse into the active metal layer.
Expand the switching window of RRAM cells, improve manufacturing yield and reliability, and reduce parasitic resistance, thereby optimizing the operating parameters of RRAM cells.
Smart Images

Figure CN112151673B_ABST
Abstract
Description
Technical Field
[0001] Embodiments of the present invention relate to RRAM, integrated chips, and methods of forming the same. Background Art
[0002] Many modern electronic devices include nonvolatile memory. Nonvolatile memory is electronic memory that is able to store data in the absence of power. Some promising candidates for the next generation of nonvolatile memory include resistive random access memory (RRAM). RRAM has a relatively simple structure and is compatible with complementary metal oxide semiconductor (CMOS) logic manufacturing processes. Summary of the invention
[0003] Some embodiments of the present invention provide a resistive random access memory (RRAM) cell, comprising: a bottom electrode; a switching layer located above the bottom electrode; an active metal layer located above the switching layer; a top electrode located above the active metal layer, wherein the top electrode comprises a metal element and a non-metal element, and wherein the top electrode has a lower reactivity to oxygen than the active metal layer; and a blocking layer located between the top electrode and the active metal layer, wherein the blocking layer is conductive and is configured to block diffusion of the non-metal element from the top electrode to the active metal layer.
[0004] Other embodiments of the present invention provide an integrated chip, comprising: a substrate; and a storage unit located above the substrate and comprising: a bottom electrode; and a solid electrolyte layer located above the bottom electrode; a metal layer located above the solid electrolyte layer and configured to be electrochemically dissolved in the solid electrolyte layer; a top electrode located above the metal layer and comprising a metal nitride; and a barrier layer located between the top electrode and the metal layer and directly contacting the top electrode and the metal layer, wherein the barrier layer comprises titanium, tantalum or tungsten, and wherein the barrier layer does not contain nitrogen along the bottom of the barrier layer.
[0005] Still other embodiments of the present invention provide a method for forming an integrated chip, comprising: depositing a bottom electrode layer electrically coupled to the conductive line above the conductive line; depositing a dielectric layer above the bottom electrode layer; depositing a metal layer above the dielectric layer; depositing a conductive barrier layer above the metal layer; depositing a top electrode layer above the conductive barrier layer, wherein the top electrode layer includes a metallic element and a non-metallic element, wherein the deposition of the top electrode layer exposes the conductive barrier layer to a gas containing the non-metallic element, and wherein the conductive barrier layer prevents the non-metallic element from diffusing from the gas to the metal layer; patterning the bottom electrode layer and the top electrode layer, the dielectric layer, the conductive barrier layer, and the metal layer to form a storage unit. BRIEF DESCRIPTION OF THE DRAWINGS
[0006] When read in conjunction with the accompanying drawings, various aspects of the present invention can be best understood from the following detailed description. It should be noted that, in accordance with standard practice in the industry, the various components are not drawn to scale. In fact, for clarity of discussion, the size of the various components may be arbitrarily increased or reduced.
[0007] Figure 1 Cross-sectional views of some embodiments of a resistive random access memory (RRAM) cell including a top electrode barrier layer are shown.
[0008] Figure 2 Shown in Figure 1 FIG. 1 is a graph illustrating some embodiments of an RRAM cell, illustrating atomic percentage as a function of position of various materials.
[0009] Figure 3 Shows Figure 1 Cross-sectional views of some alternative embodiments of an RRAM cell, wherein the top electrode barrier layer is a multi-layer film.
[0010] FIG. 4A to FIG. 4G Shows Figure 1 1 and 2 , wherein the RRAM cell is located in an interconnect structure of an integrated circuit chip.
[0011] Figure 5A and Figure 5B A cross-sectional view of some embodiments of an integrated circuit chip is shown in which an RRAM cell is integrated with a separate one-transistor-one-resistor (1T1R) cell and includes a separate top electrode barrier layer.
[0012] Figure 6 Shows Figure 5A and Figure 5B A top view of some embodiments of an integrated circuit chip.
[0013] Figures 7 to 15 A series of cross-sectional views of some embodiments of methods for forming a RRAM cell integrated with a 1T1R cell and including a top electrode barrier layer are shown.
[0014] Fig.16 Shows Figures 7 to 15 A block diagram of some embodiments of the method.
[0015] Figures 17 to 21 Shows Figures 7 to 15 A series of cross-sectional views of some optional embodiments of the method, wherein the top electrode barrier layer has a U-shaped profile.
[0016] Fig. 22 Shows Figures 17 to 21 A block diagram of some embodiments of the method. DETAILED DESCRIPTION
[0017] The following disclosure provides many different embodiments or examples for realizing different features of the present invention. Specific examples of components and arrangements are described below to simplify the present invention. Of course, these are merely examples and are not intended to limit the present invention. For example, in the following description, forming a first component above or on a second component may include an embodiment in which the first component and the second component are directly in contact with each other, and may also include an embodiment in which an additional component may be formed between the first component and the second component so that the first component and the second component may not be in direct contact. In addition, the present invention may repeat reference numerals and / or characters in various embodiments. This repetition is for the purpose of simplicity and clarity, and does not itself indicate the relationship between the various embodiments and / or configurations discussed.
[0018] Furthermore, for ease of description, spatially relative terms such as "below," "beneath," "lower," "above," "upper," etc. may be used herein to describe the relationship of one element or component to another (or additional) elements or components as shown in the figures. The spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations) and the spatially relative descriptors used herein should be interpreted accordingly.
[0019] In some embodiments, a resistive random access memory (RRAM) cell includes a bottom electrode, a switching layer located above the bottom electrode, an active metal layer located above the switching layer, and a top electrode layer located above the active metal layer. During operation of the RRAM cell, the RRAM cell is alternately set to a low resistance state (LRS) and reset to a high resistance state (HRS). In order to set the RRAM cell, a setting voltage with a positive polarity is applied from the top electrode to the bottom electrode. The setting voltage causes oxidation of the active metal layer and forms metal cations. In addition, the electric field from the setting voltage causes the metal cations to migrate toward the bottom electrode and be reduced to metal filaments in the switching layer. Forming the metal filaments changes the switching layer and thereby the RRAM cell to LRS. In order to reset the RRAM cell, a reset voltage with a negative polarity is applied from the top electrode to the bottom electrode. The reset voltage reverses the process of forming the metal filament and thereby dissolving the metal filament. Dissolving the metal filament changes the switching layer and thereby changes the RRAM cell to HRS.
[0020] In some embodiments, the top electrode is or includes a metal nitride. It is cheaper to use a metal nitride for the top electrode than platinum, ruthenium or some other precious metals. However, the nitrogen used during the formation of the top electrode and / or the nitrogen in the top electrode may diffuse into the active metal layer and form an undesirable switching layer between the top electrode and the active metal layer. The undesirable switching layer changes between HRS and LRS in the same manner as the above-mentioned switching layer, except that the metal wire of the undesirable switching layer extends from the top electrode to the active metal layer, and the polarity for switching between HRS and LRS is opposite. Due to the opposite polarity, when the switching layer is in LRS, the undesirable switching layer is in HRS, and vice versa. This has the effect of increasing the overall resistance of the RRAM cell, especially when it is in LRS. Due to the increase in resistance, the operating parameters of the RRAM cell may be out of range and / or the switching window of the RRAM cell (i.e., the difference between the resistance of the RRAM cell in LRS and HRS) may be reduced. This in turn may reduce the manufacturing yield and / or reliability of the RRAM cell.
[0021] Various embodiments of the present application are directed to an RRAM cell including a top electrode barrier layer. In some embodiments, the RRAM cell includes a bottom electrode, a switching layer located above the bottom electrode, an active metal layer located above the switching layer, a top electrode barrier layer located above the active metal layer, and a top electrode located above the top electrode barrier layer. The top electrode and the bottom electrode are both less reactive to oxygen than the active metal layer, and each contains a metal element. In addition, the top electrode includes nitrogen or some other suitable non-metallic element. The top electrode barrier layer is conductive and is configured to block or otherwise reduce the diffusion of non-metallic elements from the top electrode to the active metal layer.
[0022] In at least one embodiment where the top electrode is or includes a metal nitride and the non-metallic element is nitrogen, the top electrode barrier layer is arranged between the top electrode and the active metal layer to reduce the parasitic resistance at the top electrode. For example, in the absence of a top electrode barrier layer, nitrogen may diffuse into the active metal layer and produce an undesirable switching layer. The undesirable switching layer may become HRS, and the switching layer may become LRS, and vice versa, whereby the undesirable switching layer may cause parasitic resistance. By reducing the parasitic resistance at the top electrode, the switching window of the RRAM cell can be expanded, the reliability of the RRAM cell can be improved, and the manufacturing yield can be higher. In some embodiments, when in LRS, the top electrode barrier layer reduces the parasitic resistance of the RRAM cell from about 15 kilo-ohms to about 30 ohms. However, other suitable resistance values are also possible.
[0023] refer to Figure 1, a cross-sectional view 100 of some embodiments of a RRAM cell 102 including a top electrode barrier layer 104 is provided. As described above, the top electrode barrier layer 104 blocks or otherwise reduces the diffusion of nitrogen or some other suitable non-metallic element in the top electrode 106 to reduce the parasitic resistance at the top electrode 106. The RRAM cell 102 can be integrated with other devices in an integrated circuit (IC) chip, for example, and / or can be a cation RRAM cell or some other suitable type of RRAM cell, for example. Note that a cation RRAM cell is sometimes referred to as a programmable metallization cell (PMC) or a conductive bridge random access memory (CBRAM) cell.
[0024] The bottom electrode 108, the switching layer 110, and the active metal layer 112 are stacked with the top electrode barrier layer 104 and the top electrode 106 to define the RRAM cell 102. The switching layer 110 is located on the bottom electrode 108, the active metal layer 112 is located on the switching layer 110, the top electrode barrier layer 104 is located on the active metal layer 112, and the top electrode 106 is located on the top electrode barrier layer 104. During the operation of the RRAM cell 102, the metal filament 114 is repeatedly formed and dissolved in the switching layer 110 to change the RRAM cell 102 between RRS and HRS. When the metal filament 114 is formed, a set voltage with a positive polarity is applied from the top electrode 106 to the bottom electrode 108. The set voltage causes oxidation of the active metal layer 112 and forms metal cations. In addition, the electric field from the set voltage causes the metal cations to migrate to the switching layer 110 and be reduced to the metal filament 114. When dissolving the metal wire 114, a reset voltage with negative polarity is applied from the top electrode 106 to the bottom electrode 108. The reset voltage oxidizes the metal wire 114 and forms metal cations. In addition, the electric field from the reset voltage causes the metal cations to migrate to the active metal layer 112 and be reduced to the active metal layer 112.
[0025] The top electrode 106 and the bottom electrode 108 and the active metal layer 112 are conductive. However, compared with the top electrode 106 and the bottom electrode 108, the active metal layer 112 is electrochemically active. Therefore, the top electrode 106 and the bottom electrode 108 have lower oxygen reactivity than the active metal layer 112, and rely on more energy for oxidation than the active metal layer 112. For example, the top electrode 106 and the bottom electrode 108 can rely on 5 or more electron volts (eV) to oxidize, while the active metal layer 112 can rely on 3 or less eV to oxidize. However, other eV values are also possible. The top electrode 106 and / or the bottom electrode 108 can be, for example, or include titanium nitride, tantalum nitride, tungsten nitride, some other suitable metal nitrides, some other suitable materials, or any combination of the foregoing. The active metal layer 112 can be, for example, or include aluminum, copper, silver, nickel, some other suitable metals, or any combination of the foregoing.
[0026] The top electrode 106 includes a metal element and a non-metal element. In some but not all embodiments, the top electrode 106 is composed of a metal element and a non-metal element or is substantially composed of a metal element and a non-metal element. The non-metal element reduces the position where oxygen may be bonded to the metal element, and thus reduces the oxygen reactivity. Therefore, platinum, ruthenium and other expensive noble metals may not be used to form the top electrode 106. In some embodiments, the ratio of the atoms of the metal element to the atoms of the non-metal element is between about 1:1 and 1:1.1, so that the position where oxygen can be bonded to the metal element is saturated or substantially saturated. In some embodiments, the atomic percentage of the metal element is about 50% and / or the atomic percentage of the non-metal element is about 50%. The metal element may be, for example, titanium, tungsten, tantalum or other suitable elements, and / or the non-metal element may be, for example, nitrogen or other suitable elements.
[0027] Although the non-metallic element reduces oxygen reactivity and allows the top electrode 106 to be formed at a lower cost, the non-metallic element may generate parasitic resistance if the top electrode barrier layer 104 is not used. The top electrode barrier layer 104 blocks or slows the diffusion of the non-metallic element into the active metal layer 112, and can be exposed to the non-metallic element, for example, by the gas used to form the top electrode 106 and / or by the top electrode 106. In at least one embodiment in which the non-metallic element is nitrogen and the active metal layer 112 is aluminum, if nitrogen is allowed to diffuse into the active metal 112, the nitrogen will generate an undesirable switching layer between the active metal layer 112 and the top electrode 106. The undesirable switching layer will become HRS, while the switching layer 110 will become LRS, and vice versa, whereby the undesirable switching layer will cause parasitic resistance. Because the undesirable switching layer will be in HRS when the switching layer 110 is in LRS, the parasitic resistance will be more significant when the switching layer 110 and therefore the RRAM cell 102 is in LRS. Therefore, the top electrode barrier layer 104 can reduce the parasitic resistance by preventing or slowing down the diffusion of non-metallic elements into the active metal layer 112. By reducing the parasitic resistance, the switching window of the RRAM cell 102 can be expanded, the reliability of the RRAM cell 102 can be improved, and the manufacturing yield of the RRAM cell 102 can be higher.
[0028] In some embodiments, the bottom electrode 108 is or includes ruthenium, platinum, some other suitable noble metal, or any combination of the foregoing. In some embodiments, the bottom electrode 108 includes a metal element and a non-metal element. In some but not all embodiments, the bottom electrode 108 is composed of a metal element and a non-metal element or is substantially composed of a metal element and a non-metal element. The non-metal element of the bottom electrode 108 can reduce the position where oxygen can be bonded to the metal element to reduce the oxygen reactivity and manufacturing cost of the bottom electrode 108. In some embodiments, the bottom electrode 108 has the same material composition as the top electrode 106. In some embodiments, the metal element of the bottom electrode 108 is the same as the metal element of the top electrode 106 and / or the non-metal element of the bottom electrode 108 is the same as the non-metal element of the top electrode 106.
[0029] The metal element of the top electrode 106 and / or the metal element of the bottom electrode 108 may be, for example, or include titanium, tantalum, tungsten, or some other suitable metal. The non-metal element of the top electrode 106 and / or the non-metal element of the bottom electrode 108 may be, for example, nitrogen or other suitable elements. In some embodiments, the metal element of the top electrode 106 has a greater reactivity with oxygen than the active metal layer 112, but the non-metal element of the top electrode 106 reduces the oxygen reactivity of the top electrode 106 to less than the oxygen reactivity of the active metal layer 112.
[0030] In some embodiments, the top electrode 106 and the bottom electrode 108 have a single electrode thickness Te of about 150-250 angstroms, about 150-200 angstroms, about 200-250 angstroms, or about 200 angstroms. However, other thicknesses are also possible. In some embodiments, the active metal thickness T of the active metal layer 112 is about 150-250 angstroms, about 150-200 angstroms, about 200-250 angstroms, or about 200 angstroms. am The active metal layer 112 may be about 10-500 angstroms, about 10-255 angstroms, about 255-500 angstroms, or about 400 angstroms. However, other thicknesses are also possible. If the active metal layer 112 is too thin (e.g., less than about 10 angstroms or some other suitable value), the active metal layer 112 may not be able to fully supply the active metal to the switching layer 110. If the active metal layer 112 is too thick (e.g., greater than about 500 angstroms or some other suitable value), the voltage drop on the active metal layer 112 may be very high, and thus the reliability may be poor. Additionally or alternatively, if the active metal layer 112 is too thick (e.g., greater than about 500 angstroms or some other suitable value), the active metal layer 112 may make integration with existing processes more difficult.
[0031] The switching layer 110 is a solid electrolyte for metal cations produced by oxidation of the active metal layer 112. For example, where the active metal layer 112 is or includes aluminum, the switching layer 110 may be a solid electrolyte for aluminum cations. In some embodiments, the switching layer 110 is or includes silicon oxide (e.g., SiO 2), hafnium oxide (e.g., HfO 2 ), silicon nitride (e.g., SiN x ), aluminum oxide (e.g., Al 2 O 3 ), zirconium oxide (e.g., ZrO 2 ), some other suitable dielectric, or any combination thereof. In addition, in some embodiments, the switching layer 110 is or includes germanium sulfide (e.g., GeS), germanium selenium (e.g., GeSe), germanium tellurium (e.g., GeTe), a metal oxide, amorphous silicon, some other suitable electrolyte, or any combination thereof.
[0032] The top electrode barrier layer 104 is conductive and, as described above, is configured to block or slow down the diffusion of the non-metallic element of the top electrode 106 to the active metal layer 112. In some embodiments, the top electrode barrier layer 104 is or includes titanium, tantalum, tungsten, some other suitable barrier material, or any combination of the foregoing. In some embodiments, the top electrode barrier layer 104 has an amorphous structure to eliminate grain boundaries and increase the complexity of the diffusion path of the non-metallic element of the top electrode 106. Optionally, in some embodiments, the top electrode barrier layer 104 has a nanocrystalline structure, and the metal grains of the top electrode barrier layer 104 are equiaxed grains rather than columnar grains to increase the complexity of the diffusion path of the non-metallic element of the top electrode 106. By increasing the path complexity of the non-metallic element of the top electrode 106, the diffusion of the non-metallic element through the top electrode barrier layer 104 is slowed down or otherwise stopped.
[0033] In some embodiments, the top electrode barrier layer 104 is or includes a metal element of the top electrode 106 and / or a metal element of the bottom electrode 108. In some but not all embodiments, the top electrode barrier layer 104 consists of or consists essentially of a single metal element, such as, for example, a metal element of the top electrode 106, a metal element of the bottom electrode 108, or some other suitable metal element. In some embodiments, the combined resistance of the top electrode barrier layer 104 and the top electrode 106 from the top surface of the top electrode 106 to the bottom surface of the top electrode barrier layer 104 is about 30 ohms, less than about 1000 ohms, about 10-100 ohms, or some other suitable value.
[0034] In some embodiments, the top electrode barrier layer 104 has a barrier thickness T of about 50-100 angstroms, about 50-75 angstroms, about 75-100 angstroms, or about 50 angstroms. b. However, other thicknesses are possible. If the top electrode barrier layer 104 is too thin (e.g., less than about 50 angstroms or some other suitable value), the top electrode barrier layer 104 may not block or otherwise slow the migration of non-metallic elements of the top electrode 106 through the top electrode barrier layer 104, and may thereby fail to reduce the parasitic resistance at the top electrode 106. On the other hand, if the top electrode barrier layer 104 is too thick (e.g., greater than about 100 angstroms or some other suitable value), the top electrode barrier layer 104 may introduce too much resistance to the RRAM cell 102 and cause the operating parameters of the RRAM cell 102 to be out of specification. Additionally or alternatively, if the top electrode barrier layer 104 is too thick (e.g., greater than about 100 angstroms or some other suitable value), the top electrode barrier layer 104 may make integration with existing manufacturing processes more difficult. In some embodiments, the barrier thickness T b The electrode thickness T of the top electrode 106 e The ratio of is about 1:2-4 or some other suitable ratio. In some embodiments, the barrier thickness T b and the electrode thickness T of the top electrode 106 e The sum of is less than about 250 angstroms, about 200-300 angstroms, or some other suitable value.
[0035] Reference Figure 2 , provides a description of Figure 1 A graph 200 of atomic percentage as a function of position of various materials for some embodiments of the RRAM cell 102. The position corresponds to the vertical distance from the top surface of the top electrode 106 and can be, for example, along Figure 1 . As shown, the top electrode 106 is mainly composed of titanium and nitrogen, that is, the active metal layer 112 is mainly composed of aluminum, and the top electrode barrier layer 104 is mainly composed of titanium. In addition, when transitioning from the top electrode 106 to the top electrode barrier layer 104, the atomic percentage of nitrogen drops to about zero. Therefore, along the bottom of the top electrode barrier layer 104, the top electrode barrier layer 104 has no or substantially no nitrogen. Although specific elements and atomic percentage ratios are shown by the curve graph 200, it should be understood that in alternative embodiments, other elements and / or atomic percentage ratios are also possible.
[0036] refer to Figure 3 , provides Figure 1 300 of some optional embodiments of the RRAM cell 102, wherein the top electrode barrier layer 104 is a multi-layer film. The top electrode barrier layer 104 includes a first top electrode barrier layer 104a, and also includes a second top electrode barrier layer 104b located above the first top electrode barrier layer 104a. The first top electrode barrier layer 104a and the second top electrode barrier layer 104b are both similar to the reference Figure 1The top electrode barrier layers 104 described are the same, but each is or includes a different material. For example, the first top electrode barrier layer 104a can be or include tantalum, and the second top electrode barrier layer 104b can be or include titanium, or vice versa. However, other materials are also possible.
[0037] In some embodiments, the first top electrode barrier layer 104a and the second top electrode barrier layer 104b have a nanocrystalline structure. In such an embodiment, because the first top electrode barrier layer 104a and the second top electrode barrier layer 104b are different materials, the metal grains of the first top electrode barrier layer 104a are not aligned with the metal grains of the second top electrode barrier layer 104b. In this way, the complexity of the diffusion path of the non-metallic element of the top electrode 106 is increased. By increasing the complexity of the diffusion path, the diffusion of the non-metallic element through the top electrode barrier layer 104 is slowed down or otherwise stopped.
[0038] although Figure 3 The RRAM cell 102 is shown as having two separate top electrode barrier layers 104a, 104b, but in alternative embodiments, more separate top electrode barrier layers may be used. For example, a third top electrode barrier layer may be vertically located between the second top electrode barrier layer 104b and the top electrode 106 and directly contact the second top electrode barrier layer 104b and the top electrode 106. In this example, the third top electrode barrier layer may be a different material from the first top electrode barrier layer 104a and the second top electrode barrier layer 104b or may be or include, for example, the same material as the first top electrode barrier layer 104a. As another example, the first top electrode barrier layer 104a and the second top electrode barrier layer 104b may be repeated alternately, so that the RRAM cell 102 alternates multiple times between the material of the first top electrode barrier layer 104a and the material of the second top electrode barrier layer 104b from the top electrode 106 to the active metal layer 112. In this example, the first top electrode barrier layer 104a may be repeated 2, 3, 4 or more times with the second top electrode barrier layer 104b.
[0039] refer to Figure 4A , provides Figure 1 400A is a cross-sectional view of some embodiments of an RRAM cell 102, wherein the RRAM cell 102 is located in an interconnect structure 402 of an integrated circuit chip, and the bottom electrode 108 of the RRAM cell 102 has a T-shaped profile. The RRAM cell 102 is located below a top electrode line 404t and a top electrode via 406t, and is further located above a bottom electrode line 404b.
[0040] The top electrode via 406t extends from the top electrode line 404t downward to the top electrode 106. In some embodiments (as shown), the top electrode via 406t extends through a hard mask 408 on top of the top electrode 106. In alternative embodiments, the hard mask 408 is omitted. The hard mask 408 can be or include, for example, silicon nitride and / or some other suitable dielectric. The top electrode line 404t, the bottom electrode line 404b, and the top electrode via 406t can be or include, for example, copper, aluminum copper, some other suitable metal, or any combination of the foregoing.
[0041] The bottom electrode 108 protrudes downward to the bottom electrode line 404b, thereby defining a bottom electrode through hole 410 that electrically couples the bottom electrode 108 to the bottom electrode line 404b. The bottom electrode 108 includes a bottom electrode body 108b and a bottom electrode pad 108l that covers the lower side of the bottom electrode body 108b. In some embodiments, the bottom electrode pad 108l is an adhesion layer to enhance the deposition of the layer forming the bottom electrode body 108b. In addition, in some embodiments, the bottom electrode pad 108l is a diffusion barrier layer to prevent the material of the bottom electrode line 404b from diffusing to the bottom electrode body 108b. The bottom electrode pad 108l can be or include, for example, tantalum nitride and / or some other suitable conductive barrier material. The bottom electrode body 108b can be or include, for example, titanium nitride and / or some other suitable conductive material.
[0042] In an alternative embodiment, the bottom electrode pad 1081 is omitted. In such an alternative embodiment, the bottom electrode 108 can be a single conductive material throughout the bottom electrode 108. For example, the bottom electrode 108 can be or include tantalum nitride, titanium nitride, some other suitable conductive material, or any combination of the foregoing. When the bottom electrode 108 is formed using chemical mechanical polishing (CMP) or some other suitable planarization, forming the bottom electrode 108 from a single conductive material improves the flatness along the top surface of the bottom electrode 108 because the bottom electrode 108 has a single hardness throughout, and thus a single removal rate throughout. This in turn improves the uniformity of the electric field across the RRAM cell 102.
[0043] The dielectric structure surrounds the RRAM cell 102 and the top electrode line 404t, the top electrode via 406t, and the bottom electrode line 404b. The dielectric structure includes a hard mask 408 along the top surface of the top electrode 106, and also includes a sidewall spacer structure 412 located on the sidewalls of the RRAM cell 102. The sidewall spacer structure 412 includes a pair of segments located on opposite sides of the RRAM cell 102, respectively, and can be or include, for example, silicon nitride and / or some other suitable dielectric. Optionally, the dielectric structure includes a plurality of intermetal dielectric (IMD) layers 414, a via dielectric layer 416, an etch stop layer 418, and an IMD liner 420.
[0044] IMD layers 414 surround bottom electrode line 404b and top electrode line 404t, respectively. IMD layers 414 may be or include, for example, ultra-low-k dielectric and / or some other suitable dielectric. Via dielectric layers 416, etch stop layers 418, and IMD pads 420 are stacked between IMD layers 414.
[0045] The through-hole dielectric layer 416 surrounds the bottom electrode through hole 410 and is located between the RRAM cell 102 and the lower electrode line 404b. In some embodiments, the through-hole dielectric layer 416 is a multilayer film, which includes a lower through-hole dielectric layer 416a and an upper through-hole dielectric layer 416b located above the lower through-hole dielectric layer 416a. The lower through-hole dielectric layer 416a and the upper through-hole dielectric layer 416b are different materials and can be, for example, or include silicon carbide and silicon-rich oxide, respectively. However, other materials are also possible. In an optional embodiment, the through-hole dielectric layer 416 is a single layer.
[0046] The etch stop layer 418 covers the through-hole dielectric layer 416 and wraps around the top of the RRAM cell 102. In addition, the IMD liner 420 covers and lines the etch stop layer 418 to separate the etch stop layer 418 from an adjacent one of the IMD layers 414. The IMD liner 420 can be or include, for example, tetraethyl orthosilicate (TEOS) oxide and / or some other suitable dielectric. The etch stop layer 418 can be or include, for example, silicon carbide and / or some other suitable dielectric.
[0047] refer to Figure 4B , provides Figure 4A 400B of some alternative embodiments of the RRAM cell 102, wherein the top edge of the sidewall spacer structure 412 is flush with the top electrode barrier layer 104. Therefore, the etch stop layer 418 contacts the sidewall of the top electrode barrier layer 104. In alternative embodiments, the top edge of the sidewall spacer structure 412 is flush with the top electrode 106.
[0048] refer to Figure 4C , provides Figure 4A 400C of some alternative embodiments of the RRAM cell 102, wherein the sidewall spacer structure 412 is located above the switching layer 110. In addition, the sidewall spacer structure 412 lines the sidewalls of the active metal layer 112, the top electrode barrier layer 104, and the top electrode 106, respectively, but does not line the sidewalls of the switching layer 110 and the bottom electrode 108, respectively.
[0049] refer to Figure 4D , provides Figure 4A400D of some optional embodiments of the RRAM cell 102, wherein the sidewall spacer structure 412 is replaced by a first sidewall spacer structure 412a and a second sidewall spacer structure 412b. The first sidewall spacer structure 412a is located above the top electrode barrier layer 104 and lines the sidewalls of the top electrode 106 and the hard mask 408, respectively. Therefore, the sidewalls of the top electrode 106 and the hard mask 408 are offset from the sidewalls of the top electrode barrier layer 104, respectively. The second sidewall spacer structure 412b lines the sidewalls of the first sidewall spacer structure 412a, the top electrode barrier layer 104, the active metal layer 112, the switching layer 110, and the bottom electrode 108, respectively. In an optional embodiment, the second sidewall spacer structure 412b is formed in a manner similar to that of the first sidewall spacer structure 412a. Figure 4C The sidewall spacer structures 412 are located above the switching layer 110 in the same manner. The first sidewall spacer structure 412a and / or the second sidewall spacer structure 412b may be or include, for example, silicon nitride and / or some other suitable dielectric.
[0050] refer to Figure 4E , provides Figure 4A 400E of some alternative embodiments of the RRAM cell 102, wherein the top of the RRAM cell 102 is recessed at the bottom electrode via 410. In addition, the RRAM cell 102 does not have a bottom electrode pad 1081 (see Figure 4A ), and the top corners of the through-hole dielectric layer 416 at the bottom electrode through-hole 410 are rounded or otherwise curved. In an alternative embodiment, the RRAM cell 102 further includes Figure 4A The top angles of the bottom electrode pad 1081 and / or the through-hole dielectric layer 416 are shown as follows: Figure 4A shown.
[0051] refer to Figure 4F , provides Figure 4A 400F of some alternative embodiments of the RRAM cell 102, wherein the bottom electrode via 410 is omitted. In addition, the top electrode 106 and the bottom electrode 108, the top electrode barrier layer 104, the switching layer 110 and the active metal layer 112 have a U-shaped profile, and the bottom electrode via 410 is omitted. Figure 4A The omitted components are the sidewall spacer structure 412, the hard mask 408, the etch stop layer 418, and the IMD liner 420. As described below, the RRAM cell 102 can be formed by a single lithography / etching process, thereby reducing costs.
[0052] refer to Figure 4G , provides Figure 4A 400G of some optional embodiments of the RRAM cell 102, wherein the top electrode 106, the top electrode barrier layer 104 and the active metal layer 112 have a U-shaped profile and the top electrode 106, the top electrode barrier layer 104 and the active metal layer 112 are omitted. Figure 4AThese omitted components are the sidewall spacer structure 412, the hard mask 408, the etch stop layer 418, and the IMD liner 420.
[0053] Although using Figure 1 An embodiment of the RRAM cell 102 is shown in FIG. 4A to FIG. 4G , but can optionally use Figure 3 In other words, FIG. 4A to FIG. 4G The top electrode barrier layer 104 may be a reference Figure 3 The multilayer film shown and described. Although the sidewalls of the bottom electrode 108 and the switching layer 110 are shown Figure 4B , Figure 4D and Figure 4E , but the sidewall spacer structure 412 may alternatively be as Figure 4C shown as being located above the bottom electrode 108 and the switching layer 110. Although Figure 4F and Figure 4G The etch stop layer 418 and the IMD liner 420 are shown without, but may optionally be present. Figure 4F and Figure 4G The various layers constituting the RRAM cell 102 are shown to have a U-shaped profile, but the various layers may alternatively have a V-shaped profile or some other suitable profile.
[0054] Reference Figure 5A , a cross-sectional view 500A of some embodiments of a RRAM cell 102 is provided, wherein the RRAM cell 102 includes a separate top electrode barrier layer 104 and is integrated with a separate one-transistor-one-resistor (1T1R) cell 502 in an integrated circuit chip. Figure 5A Each of the RRAM cells 102 is Figure 4A The RRAM cell 102 is shown and described. The 1T1R cell 502 includes a separate drain region 504 and a separate drain-side conductive path 506 .
[0055] The drain regions 504 are doped regions of the substrate 508 and each have a doping type opposite to that of an adjacent region of the substrate 508. In addition, the drain regions 504 are electrically isolated from each other by trench isolation structures 510 and partially define access transistors 512 (partially shown) for respectively selecting the RRAM cells 102. The trench isolation structures 510 extend to the top of the substrate 508 and include silicon oxide and / or some other suitable dielectric material. The trench isolation structures 510 may be, for example, shallow trench isolation (STI) structures or some other suitable trench isolation structures. The substrate 508 may be, for example, a bulk silicon substrate, a silicon-on-insulator (SOI) substrate, or some other suitable semiconductor substrate.
[0056] The drain side conductive path 506 electrically couples the drain region 504 to the RRAM cell 102. In addition, the drain side conductive path 506 is defined by the interconnect structure 402, which includes a plurality of lines 404 and a plurality of vias 406. The plurality of lines 404 include a top electrode line 404t and a bottom electrode line 404b. In some embodiments, the top electrode line 404t corresponds to a bit line BL shared by other RRAM cells (not shown). The plurality of vias 406 include a top electrode via 406t. The level of the via 406 closest to the substrate 508 is located in the interlayer dielectric (ILD) layer 514, while the remaining levels of the via 406 and the line 404 are located in the IMD layer 414. The line 404 and the via 406 can be or include, for example, copper, aluminum, aluminum copper, some other suitable conductive material, or any combination of the foregoing.
[0057] The peripheral region 516 to one side of the 1T1R cell 502 accommodates a peripheral device 518 (only partially shown). The peripheral device 518 can be, for example, a metal oxide semiconductor field effect transistor (MOSFET) or some other suitable semiconductor device. The peripheral device 518 includes a pair of source / drain regions 520 (only one is shown) located in the substrate 508, and also includes a gate structure (not shown) located between the source / drain regions 520. The source / drain regions 520 are doped regions of the substrate 508, and each has a doping type opposite to that of the adjacent regions of the substrate 508.
[0058] refer to Figure 5B , provides Figure 5A A cross-sectional view 500B of some embodiments of an integrated circuit chip, taken along a plane perpendicular to Figure 5A The 1T1R cell 502 includes a separate RRAM cell 102 , a separate drain-side conductive path 506 , a separate access transistor 512 , and a separate source-side conductive path 522 . Figure 5B Each of the RRAM cells 102 is Figure 4A The RRAM cell 102 is shown and described.
[0059] The access transistor 512 is located on the substrate 508, between the substrate 508 and the interconnect structure 402. In addition, the access transistors 512 are electrically isolated from each other by the trench isolation structure 510. The access transistor 512 includes a separate drain region 504, a separate source region 524, a separate gate dielectric layer 526, and a separate gate electrode 528. The gate electrode 528 is respectively located above the gate dielectric layer 526, and in some embodiments, defines a word line WL. The drain region 504 and the source region 524 are doped regions of the substrate 508, and each has a doping type opposite to the adjacent region of the substrate 508. The drain region 504 is respectively adjacent to the drain side of the gate electrode 528, and the source region 524 is respectively adjacent to the source side of the gate electrode 528. The access transistor 512 can be, for example, a MOSFET or other suitable semiconductor device.
[0060] Drain side conductive path 506 electrically couples drain region 504 to RRAM cell 102 , and source side conductive path 522 electrically couples source region 524 to source line SL. Drain side conductive path 506 and source side conductive path 522 are defined by multiple lines 404 and multiple vias 406 in interconnect structure 402 .
[0061] Although the figure uses Figure 4A The RRAM cell embodiment shows Figure 5A and Figure 5B , but can optionally use Figure 1 , Figure 3 and FIG. 4B to FIG. 4G Any one of the RRAM cell embodiments. For example, Figure 5A and Figure 5B Each of the RRAM cells 102 may be Figure 4F As shown in .
[0062] refer to Figure 6 , provides Figure 5A and Figure 5B FIG. 6 is a top view of some embodiments of an integrated circuit chip. Figure 5A A cross-sectional view 500A and Figure 5B The cross-sectional view 500B can be taken, for example, along lines B and C or other suitable positions. The integrated circuit chip includes a plurality of RRAM cells 102 in a plurality of rows and columns, thereby defining an RRAM array 602. The RRAM cells 102 can be, for example, Figure 1 , Figure 3 , FIG. 4A to FIG. 4G , Figure 5A and Figure 5BThe peripheral device 518 surrounds the RRAM array 602 at the peripheral area 516 of the integrated circuit chip. The peripheral device 518 can be, for example, or include a transistor and / or other suitable semiconductor device. In addition, the peripheral device 518 can, for example, implement a read / write circuit and / or other suitable circuit for operating the RRAM cell 102.
[0063] Reference Figures 7 to 15 , a series of cross-sectional views 700-1500 of some embodiments of a method for forming an RRAM cell are provided, wherein the RRAM cell includes a separate top electrode barrier layer and is integrated with a 1T1R cell in an integrated circuit chip. The cross-sectional views 700-1500 may be, for example, along Figure 6 In addition, the cross-sectional views 700-1500 may correspond to, for example, Figure 5A , and thus can be, for example, as shown and described Figure 5A and Figure 5B integrated circuit chip.
[0064] like Figure 7 As shown in the cross-sectional view 700 of FIG. 5 , the trench isolation structures 510 are formed to extend to the top of the substrate 508. The trench isolation structures 510 respectively surround and define the areas of the substrate 508 where the 1T1R cells 502 will be formed. In addition, the trench isolation structures 510 surround and define the peripheral area 516 of the integrated circuit chip.
[0065] Also through Figure 7 As shown in the cross-sectional view 700 of , a plurality of semiconductor devices are formed on a substrate 508. The plurality of semiconductor devices include separate access transistors 512 respectively located at the 1T1R cells 502 to be formed. In addition, the plurality of semiconductor devices include a peripheral device 518 located at a peripheral region 516 of the integrated circuit chip. The access transistor 512 includes a separate drain region 504 and a separate source region (not shown) located in the substrate 508. In addition, the access transistor 512 includes a separate gate structure (not shown). The gate structure has separate drain sides respectively adjacent to the drain regions 504, and also has separate source sides respectively adjacent to the source regions. The peripheral device 518 includes a pair of source / drain regions 520 (only one is shown) located in the substrate 508, and also includes a gate structure (not shown) located between and adjacent to the source / drain regions 520.
[0066] Also through Figure 7As shown in the cross-sectional view 700 of , the interconnect structure 402 is partially formed above the semiconductor device (e.g., the access transistor 512 and the peripheral device 518) and electrically coupled to the semiconductor device. The interconnect structure 402 includes a dielectric structure, and also includes a plurality of lines 404 and a plurality of through holes 406 stacked in the dielectric structure. The dielectric structure includes an ILD layer 514 and a plurality of IMD layers 414 located above the ILD layer 514. The plurality of lines 404 include a plurality of bottom electrode lines 404b along the top surface of the interconnect structure 402. The bottom electrode lines 404b are separate and are respectively located at the 1T1R unit 502 to be formed. In addition, the bottom electrode lines 404b are electrically coupled to the drain region 504 of the access transistor 512 through the following lines and through holes.
[0067] like Figure 8 As shown in the cross-sectional view 800 of , a through-hole dielectric layer 416 is deposited or otherwise formed on the interconnect structure 402. Note that for the sake of drawing compactness, the lower portion of the interconnect structure 402 is omitted here and in subsequent figures. In some embodiments, the through-hole dielectric layer 416 is a multilayer film, which includes a lower through-hole dielectric layer 416a and an upper through-hole dielectric layer 416b located above the lower through-hole dielectric layer 416a. The lower through-hole dielectric layer 416a and the upper through-hole dielectric layer 416b are different materials and can be, for example, or include silicon carbide and silicon-rich oxide, respectively. However, other materials are also possible. In an optional embodiment, the through-hole dielectric layer 416 is a single layer.
[0068] Also through Figure 8 As shown in the cross-sectional view 800 of , the through-hole dielectric layer 416 is patterned to form separate through-hole openings 802 respectively located at the 1T1R cells 502 to be formed. The through-hole openings 802 extend through the through-hole dielectric layer 416 and expose the bottom electrode lines 404b respectively. The patterning can be implemented, for example, by a photolithography / etching process or some other suitable patterning process.
[0069] like Fig. 9 As shown in the cross-sectional view 900 of FIG. 8 , a bottom electrode layer 902 and a bottom electrode pad 1081 are formed. In an alternative embodiment, the bottom electrode pad 1081 is omitted. The bottom electrode layer 902 and the bottom electrode pad 1081 fill the through hole opening 802 (see FIG. 8 ). Figure 8), and define a separate and respectively located bottom electrode through hole 410 in the through hole opening 802. The bottom electrode layer 902 covers the interconnect structure 402, and the bottom electrode pad 1081 separates the bottom electrode layer 902 from the through hole dielectric layer 416 and the bottom electrode line 404b. The bottom electrode layer 902 has low reactivity to oxygen and is or includes titanium nitride and / or some other suitable material. Such a low reactivity material can be, for example, a material above 5eV depending on reaction with oxygen. The bottom electrode pad 1081 can be, for example, or include tantalum nitride and / or some other suitable material.
[0070] Also through Fig. 9 As shown in the cross-sectional view 900 of FIG. 1 , a switching layer 904 is deposited above the bottom electrode layer 902. The switching layer 904 is a solid electrolyte for metal cations, which is formed by an active metal layer (not shown; see FIG. 1 ). Fig.10 ) is produced by oxidation. In some embodiments, the switching layer 904 is or includes silicon nitride and / or some other suitable electrolyte.
[0071] like Fig.10 As shown in the cross-sectional view 1000 of FIG. 1 , an active metal layer 1002, a top electrode barrier layer 1004, and a top electrode layer 1006 are deposited above the switching layer 904. The top electrode barrier layer 1004 is located above the active metal layer 1002, and the top electrode layer 1006 is located above the top electrode barrier layer 1004. The active metal layer 1002, the top electrode barrier layer 1004, and the top electrode layer 1006 can be deposited, for example, by physical vapor deposition (PVD), chemical vapor deposition (CVD), some other suitable deposition process, or any combination of the foregoing.
[0072] The active metal layer 1002 is electrochemically active and has a higher reactivity to oxygen relative to the top electrode layer 1006. In some embodiments, the active metal layer 1002 also has a higher reactivity to oxygen relative to the top electrode barrier layer 1004. For example, when the active metal layer 1002 is or includes aluminum and the top electrode barrier layer 1004 is or includes tungsten, the active metal layer 1002 can have a higher reactivity to oxygen relative to the top electrode barrier layer 1004. In an optional embodiment, the active metal layer 1002 has a lower reactivity to oxygen relative to the top electrode barrier layer 1004. For example, when the active metal layer 1002 is or includes aluminum and the top electrode barrier layer 1004 is or includes titanium, the active metal layer 1002 can have a lower reactivity to oxygen relative to the top electrode barrier layer 1004. In addition, the active metal layer 1002 allows the active metal layer 1002 to be electrochemically dissolved into the switching layer 904 and conducted through the switching layer 904. In some embodiments, active metal layer 1002 is or includes aluminum and / or some other suitable material.
[0073] The top electrode layer 1006 has a lower reactivity to oxygen than the active metal layer 1002 and the top electrode barrier layer 1004. In addition, the top electrode layer 1006 prevents oxygen from reaching the active metal layer 1002 and the top electrode barrier layer 1004 during subsequent processing. If oxygen were to reach such layers, an oxide may be formed on the active metal layer 1002 and / or the top electrode barrier layer 1004, thereby increasing the resistance of the RRAM cell to be formed. Such an increase may in turn cause the operating parameters of the RRAM cell to be out of range and / or may reduce the manufacturing yield. In some embodiments, the top electrode layer 1006 is or includes titanium nitride, tantalum nitride, tungsten nitride, some other suitable material, or any combination of the foregoing.
[0074] The top electrode layer 1006 includes metal elements and non-metal elements. In some but not all embodiments, the top electrode layer 1006 is composed of metal elements and non-metal elements or is basically composed of metal elements and non-metal elements. Non-metal elements reduce the position where oxygen may be combined with metal elements, and thus reduce oxygen reactivity. Therefore, the top electrode layer 1006 can be formed without using platinum, ruthenium and other expensive noble metals. In some embodiments, the ratio of atoms of metal elements to atoms of non-metal elements is between about 1:1 and 1:1.1, so that oxygen can be combined with the position of metal elements. In some embodiments, the atomic percentage of metal elements is about 50% and / or the atomic percentage of non-metal elements is about 50%. Metal elements can be, for example, titanium, tungsten, tantalum or other suitable elements, and / or non-metal elements can be, for example, nitrogen or some other suitable elements.
[0075] Although the non-metallic element reduces oxygen reactivity and allows the top electrode layer 1006 to be formed at a lower cost, the non-metallic element may cause parasitic resistance if the top electrode barrier layer 1004 is not used. In at least one embodiment in which the non-metallic element is nitrogen and the active metal layer 1002 is aluminum, if the top electrode barrier layer 1004 is not used, the nitrogen will diffuse into the active metal layer 1002. For example, the nitrogen may be derived from nitrogen gas used to form the top electrode layer 1006 and / or from the top electrode layer 1006 itself. The nitrogen diffused into the active metal layer 1002 will in turn form an undesirable switching layer between the active metal layer 1002 and the top electrode layer 1006, and thus increase the parasitic resistance. The top electrode barrier layer 1004 blocks or slows down the diffusion of the non-metallic element into the active metal layer 1002 to prevent the formation of an undesirable switching layer, and thereby reduce the parasitic resistance. By reducing the parasitic resistance, the switching window of the formed RRAM cell can be expanded, the reliability can be improved, and the manufacturing yield can be higher.
[0076] In some embodiments, the top electrode layer 1006 has an electrode thickness T of about 150-250 angstroms, about 150-200 angstroms, about 200-250 angstroms, or about 200 angstroms. e In some embodiments, the active metal layer 1002 has an active metal thickness T of about 10-500 angstroms, about 10-255 angstroms, about 255-500 angstroms, or about 400 angstroms. am However, other thicknesses are possible.
[0077] The top electrode barrier layer 1004 is conductive and, as described above, is configured to prevent or otherwise slow down the diffusion of non-metallic elements of the top electrode layer 1006 into the active metal layer 1002. The top electrode barrier layer 1004 is or includes the metal element of the top electrode layer 1006. In some but not all embodiments, the top electrode barrier layer 1004 is composed of or substantially composed of a single metal element. In some embodiments, the top electrode barrier layer 1004 has an amorphous structure to eliminate grain boundaries and increase the complexity of the diffusion path of the non-metallic elements of the top electrode layer 1006. Optionally, in some embodiments, the electrode barrier layer 1004 has a nanocrystalline structure, and the metal grains of the top electrode barrier layer 1004 are equiaxed grains rather than columnar grains to increase the complexity of the diffusion path of the non-metallic elements of the top electrode layer 1006. By increasing the complexity of the diffusion path, the diffusion of the non-metallic elements through the top electrode barrier layer 1004 is slowed down or otherwise stopped. In some embodiments, the top electrode barrier layer 1004 is or includes titanium, tantalum, tungsten, some other suitable material, or any combination of the foregoing. In some embodiments, the resistance from the top surface of the top electrode layer 1006 to the bottom surface of the top electrode barrier layer 1004 is about 30 ohms, less than about 1000 ohms, about 10-100 ohms, or some other suitable value.
[0078] In some embodiments, the top electrode barrier layer 1004 has a barrier thickness T of about 50-100 angstroms, about 50-75 angstroms, about 75-100 angstroms, or about 50 angstroms. b. However, other thicknesses are possible. If the top electrode barrier layer 1004 is too thin (e.g., less than about 50 angstroms or some other suitable value), the top electrode barrier layer 1004 may not block or otherwise slow down the migration of non-metallic elements of the top electrode layer 1006 through the top electrode barrier layer 1004. On the other hand, if the top electrode barrier layer 1004 is too thick (e.g., greater than about 100 angstroms or some other suitable value), the top electrode barrier layer 1004 may introduce excessive resistance in the RRAM cell to be formed, and thereby may cause the operating parameters of the RRAM cell to exceed specifications. Additionally or alternatively, if the top electrode barrier layer 1004 is too thick (e.g., greater than about 100 angstroms or some other suitable value), the top electrode barrier layer 1004 may make integration with existing manufacturing processes more difficult. In some embodiments, the barrier thickness T b The electrode thickness T of the top electrode layer 1006 e The ratio of is about 1:2-4 or some other suitable ratio. In some embodiments, the barrier thickness T of the top electrode layer 1006 is about 1:2-4 or some other suitable ratio. b and electrode thickness T e The sum of is less than about 250 angstroms, about 200-300 angstroms, or some other suitable value.
[0079] As described above, for example, the active metal layer 1002, the top electrode barrier layer 1004, and the top electrode layer 1006 may be deposited by PVD, CVD, some other suitable deposition process, or any combination of the above. In embodiments where the top electrode layer 1006 is or includes a metal nitride, nitrogen may be used to form the top electrode layer 1006. In the absence of the top electrode barrier layer 1004 covering the active metal layer 1002, the nitrogen may directly impinge on the active metal layer 1002 and diffuse into the active metal layer 1002. As described above, this would produce an undesirable switching layer that introduces parasitic resistance to the RRAM cell to be formed. Thus, the top electrode barrier layer 1004 protects the active metal layer 112 from ambient gases (e.g., nitrogen) that may diffuse into the active metal layer 112 and produce an undesirable switching layer.
[0080] In some embodiments, the top electrode barrier layer 1004 and the top electrode layer 1006 are formed together in the same PVD processing chamber 1008 by a PVD process. Therefore, the semiconductor structure on which the top electrode barrier layer 1004 and the top electrode layer 1006 are formed remains in the PVD processing chamber 1008, and in some embodiments, remains stationary from the beginning of the PVD process to the end of the PVD process. This prevents the formation of oxide on the top electrode barrier layer 1004 between the formation of the top electrode barrier layer 1004 and the top electrode layer 1006. The PVD process includes a first PVD step to form the top electrode barrier layer 1004, and further includes a second PVD step to form the top electrode layer 1006 located above the top electrode barrier layer 1004.
[0081] The first PVD step may, for example, include performing PVD deposition using the PVD target for about 1-10 seconds (e.g., about 3 seconds or some other suitable value) while flowing argon gas, rather than nitrogen gas, into the PVD process chamber 1008. The second PVD step may, for example, include performing PVD deposition using the PVD target for about 5-15 seconds (e.g., about 10 seconds or some other suitable value) while flowing both argon gas and nitrogen gas into the PVD process chamber 1008. Thus, nitrogen gas does not flow into the PVD process chamber 1008 when the top electrode barrier layer 1004 is formed, and then nitrogen gas is added to the PVD process chamber 1008 when the top electrode layer 1006 is formed. The flow rate for argon gas during the first PVD step may, for example, be about 300 standard cubic centimeters per minute (SCCM), about 250-350 SCCM, or some other suitable flow rate. The flow rate for argon during the second PVD step is less than the flow rate for argon during the first PVD step, and can be, for example, about 200 SCCM, about 150-250 SCCM, or some other suitable flow rate. During the second PVD step, the flow rate for nitrogen can be, for example, about 80 standard SCCM, about 50-150 SCCM, or some other suitable flow rate. During the first and / or second PVD step, the temperature in the PVD treatment chamber 1008 can be, for example, about 25 degrees Celsius, about 20-30 degrees Celsius, or some other suitable temperature. The PVD target can be, for example, or include titanium, tungsten, tantalum, or some other suitable material.
[0082] In some embodiments, the active metal layer 1002 is formed in situ with the top electrode barrier layer 1004 and the top electrode layer 1006. This prevents oxide from forming on the active metal layer 1002 and the top electrode barrier layer 1004 between the formation of the active metal layer 1002 and the top electrode layer 1006. The in situ formation may be located, for example, in a PVD processing chamber 1008 and / or a multi-chamber processing tool.
[0083] In some embodiments where in-situ formation is confined to a multi-chamber processing tool, Fig. 9The structure of FIG. 100 is loaded into a multi-chamber processing tool, and then the active metal layer 1002, the top electrode barrier layer 1004, and the top electrode layer 1006 are deposited within the multi-chamber processing tool. In these embodiments, the structure is not removed from the multi-chamber process until the deposition of the top electrode layer 1006 is completed. The multi-chamber processing tool may, for example, have a PVD processing chamber 1008 for depositing the top electrode barrier layer 1004 and the top electrode layer 1006, and may further have another PVD processing chamber for depositing the active metal layer 1002. In some embodiments where the in-situ formation is confined to the PVD processing chamber 1008, the active metal layer 1002 is deposited. Fig. 9 The structure of FIG. 1004 is loaded into a PVD processing chamber 1008, and then an active metal layer 1002, a top electrode barrier layer 1004, and a top electrode layer 1006 are deposited within the PVD processing chamber 1008. In these embodiments, the structure is not removed from the PVD processing chamber 1008 until after the deposition of the top electrode layer 1006 is completed. In at least some of these embodiments, the PVD processing chamber 1008 can accommodate multiple PVD targets and / or allow the PVD target to be changed without disrupting the atmosphere within the PVD processing chamber 1008.
[0084] like Fig.11 As shown in the cross-sectional view 1100 of FIG. 100 , hard masks 408 are formed separately and are respectively formed at the 1T1R cells 502 to be formed. As described below, the hard masks 408 have a pattern of an RRAM cell for the 1T1R cells 502. For example, the hard masks 408 may be formed by depositing a hard mask layer over the top electrode layer 1006 and then patterning the hard mask layer into the hard mask 408. For example, patterning may be performed by a photolithography / etching process or some other suitable patterning process.
[0085] like Fig.12 As shown in the cross-sectional view 1200 of FIG. 1 , the top electrode layer 1006 (see FIG. 1 ) is formed by using a hard mask 408 located at an appropriate position. Fig.11 ), top electrode barrier layer 1004 (see Fig.11 ), active metal layer 1002 (see Fig.11 ), switching layer 904 (see Fig.11 ) and bottom electrode layer 902 (see Fig.11 ) is etched. The etching transfers the pattern of the hard mask 408 to the underlying layers to form separate RRAM cells 102 respectively located at the 1T1R cells 502. The RRAM cells 102 include separate top electrodes 106, separate top electrode barrier layers 104, separate active metal layers 112, separate switching layers 110, and separate bottom electrodes 108. The separate bottom electrodes 108 include a bottom electrode pad 108l and a bottom electrode body 108b.
[0086] By arranging a separate top electrode barrier layer 104 between a separate top electrode 106 and a separate active metal layer 112, parasitic resistance can be reduced. For example, assume that the active metal layer 112 of the RRAM cell 102 is or includes aluminum, and the top electrode 106 of the RRAM cell 102 is or includes a metal nitride. In this example, the top electrode barrier layer 104 of the RRAM cell 102 prevents nitrogen of the top electrode 106 and / or nitrogen gas used during the formation of the top electrode 106 from diffusing into the active metal layer 112 and forming an undesirable switching layer between the active metal layer 112 and the top electrode 106. Such an undesirable switching layer will introduce a parasitic resistance that increases the overall resistance of the RRAM cell 102. This in turn may cause the operating parameters of the RRAM cell 102 to be out of range and may reduce the manufacturing yield. Therefore, since the top electrode barrier layer 104 stops the formation of the undesirable switching layer, the parasitic resistance is reduced and the manufacturing yield can be high.
[0087] like Fig.13 As shown in the cross-sectional view 1300 of FIG. 1 , a sidewall spacer structure 412 is formed on the sidewalls of the RRAM cell 102. In addition, an etch stop layer 418, an IMD liner 420, and an additional IMD layer 414 are deposited over the RRAM cell 102 and the sidewall spacer structure 412. The IMD liner 420 is located on the etch stop layer 418, and the additional IMD layer 414 is located on the IMD liner 420.
[0088] like Fig.14 As shown in the cross-sectional view 1400 of FIG. 1 , a plurality of additional lines 404 and a plurality of additional vias 406 are formed above the RRAM cell 102 and recessed into the additional IMD layer 414 above the RRAM cell 102. The plurality of additional lines 404 include top electrode lines 404t respectively located above the RRAM cell 102, and the plurality of additional vias 406 include top electrode vias 406t extending from the top electrode lines 404t to the RRAM cell 102.
[0089] like Fig.15 As shown in the cross-sectional view 1500 of FIG. 1 , separate metal wires 114 are formed and are respectively located in the switching layer 110. The formation may, for example, include applying a formation voltage to each RRAM cell 102. For example, the bottom electrode 108 of the RRAM cell 102 may be grounded when the top electrode 106 is biased. However, other processes for forming the metal wires 114 are also possible.
[0090] Although Figures 7 to 15 The reference method is described, but it should be understood that Figures 7 to 15 The structures shown are not limited to the method but can exist independently of the method. Figures 7 to 15Although described as a series of steps, it should be understood that in other embodiments, the order of the steps may be changed. Figures 7 to 15 Although shown and described as a specific set of steps, in other embodiments, some of the steps shown and / or described may be omitted. In addition, in other embodiments, steps not shown and / or described may be included. Figures 7 to 15 use Figure 5A The method is shown in the embodiment of the RRAM cell 102, but can be used Figure 1 , Figure 3 and FIG. 4A to FIG. 4E Alternative embodiments of the method may be implemented using any one or combination of embodiments of the RRAM cell 102 .
[0091] In some embodiments, to implement the Figure 4C In an embodiment of the RRAM cell 102, Fig.12 The etching stops at the switching layer 904. This forms a separate top electrode 106, a separate top electrode barrier layer 104, and a separate active metal layer 112, each of which is shown in FIG. Figure 4C Then, as Fig.13 The sidewall spacer structure 412 is formed as described above. In addition, additional etching is selectively performed on the switching layer 904 and the bottom electrode layer 902 using the hard mask 408 and the sidewall spacer structure 412 as masks. Fig.13 The formation of the sidewall spacer structure 412 at Fig.13 The additional etching forms a separate switching layer 110 and a separate bottom electrode 108, each of which is performed between the deposition of the etch stop layer 418 at Figure 4C After the additional etching, the method is Fig.13 Deposition of the etch stop layer 418 at is performed as described above.
[0092] In some embodiments, to implement the Figure 4D In an embodiment of the RRAM cell 102, Fig.12 The etching at stops at the top electrode barrier layer 1004. This forms a separate top electrode 106, each electrode instance at Figure 4D Then, a first sidewall spacer structure 412a is formed on the sidewalls of the hard mask 408 and the top electrode 106, an example of which is shown in FIG. Figure 4D In addition, using the hard mask 408 and the first sidewall spacer structure 412a as a mask, additional etching is selectively performed on the top electrode barrier layer 1004, the active metal layer 1002, the switching layer 904 and the bottom electrode layer 902. Fig.13Additional etching is performed between the formation of the sidewall spacer structure 412 in the embodiment. The additional etching forms a separate top electrode barrier layer 104, a separate active metal layer 112, a separate switching layer 110, and a separate bottom electrode 108, each of which is shown in FIG. Figure 4D After the additional etching, the method is Fig.13 The formation of the sidewall spacer structure 412 is performed as described above. In these embodiments, the sidewall spacer structure 412 may be formed as described above. Fig.13 The sidewall spacer structure 412 formed at the bottom is more appropriately referred to as a second sidewall spacer structure 412b, an example of which is shown in FIG. Figure 4D Shown in.
[0093] refer to Fig.16 , provides Figures 7 to 15 Block diagram 1600 of some embodiments of the method.
[0094] In 1602, an interconnect structure is partially formed over a substrate, wherein the interconnect structure includes a bottom electrode line. See, e.g. Figure 7 .
[0095] At 1604, a through-hole dielectric layer is formed over the interconnect structure. See, e.g. Figure 8 .
[0096] At 1606, a bottom electrode via is formed extending through the via dielectric layer to the bottom electrode line. See e.g. Figure 8 and Fig. 9 .
[0097] At 1608, a memory film is formed on the via dielectric layer and the bottom electrode via, wherein the memory film includes a switching layer, an active metal layer located above the switching layer, a top electrode barrier layer located above the active metal layer, and a top electrode layer located above the top electrode barrier layer, and wherein the top electrode barrier layer blocks material of the top electrode layer from diffusing into the active metal layer. See, e.g. Fig. 9 and Fig.10 .
[0098] At 1610, the memory film is patterned to form a memory cell located above and electrically coupled to the bottom electrode via. See, e.g. Fig.11 and Fig.12 .
[0099] In 1612, the interconnect structure around the memory cell is completed. See e.g. Fig.13 and Fig.14 .
[0100] At 1614, a forming voltage is applied across the memory cell to form a metal filament in the switching layer. See e.g. Fig.15 .
[0101] Although Fig.16The block diagram 1600 is shown and described as a series of steps or events here, but it should be understood that the order of these steps or events is not to be interpreted as limiting. For example, some steps can occur in different orders and / or occur simultaneously with other steps or events other than those shown and / or described here. In addition, it may not be necessary for all the steps shown to implement one or more aspects or embodiments described here, and one or more steps described here can be implemented in one or more separate steps and / or stages.
[0102] refer to Figures 17 to 21 , provides Figures 7 to 15 A series of cross-sectional views 1700-2100 of some optional embodiments of the method of Figure 4F The method is implemented in accordance with an embodiment of the RRAM cell 102 in FIG. Figures 7 to 15 Like the cross-sectional views 700-1500 in FIG. 1 , the cross-sectional views 1700-2100 may be, for example, along Figure 6 The interception may be made at line B in or at some other suitable location.
[0103] like Fig.17 As shown in the cross-sectional view 1700 of , the interconnect structure 402 is partially formed. The interconnect structure 402 includes a dielectric structure, a plurality of lines 404 and a plurality of through holes (not shown). The dielectric structure includes a plurality of IMD layers 414, and also includes a through-hole dielectric layer 416 located between the IMD layers 414. In some embodiments, the through-hole dielectric layer 416 is a multilayer film including a lower through-hole dielectric layer 416a and an upper through-hole dielectric layer 416b located above the lower through-hole dielectric layer 416a. In an optional embodiment, the through-hole dielectric layer 416 is a single layer. In addition, the lines 404 and the through holes are alternately stacked in the dielectric structure to define a conductive path. The interconnect structure 402 can be, for example, as described in reference Figure 7 Note that for drawing compactness, only the upper portion of interconnect structure 402 is shown. The remainder of interconnect structure 402 may be, for example, Figure 7 Note also that, although not shown, interconnect structure 402 is located above and electrically coupled to the substrate and semiconductor device. The substrate and / or semiconductor device may be, for example, Figure 7 As shown, and / or may be, for example, as referenced Figure 7 Describe the formation.
[0104] like Fig.18 As shown in the cross-sectional view 1800 of FIG. 1 , the through-hole dielectric layer 416 and the IMD layer 414 on top of the through-hole dielectric layer 416 are patterned to form separate memory cell openings 1802 respectively located at the 1T1R cells 502 to be formed. The patterning may be implemented, for example, by a photolithography / etching process or some other suitable patterning process.
[0105] like Fig.19 As shown in cross-sectional view 1900, the deposition lining the memory cell opening 1802 (see Fig.18 ) of the bottom electrode layer 902, the switching layer 904, the active metal layer 1002, the top electrode barrier layer 1004 and the top electrode layer 1006. The bottom electrode layer 902, the switching layer 904, the active metal layer 1002, the top electrode barrier layer 1004 and the top electrode layer 1006 can be, for example, reference Fig. 9 and Fig.10 described, and can be referred to for example as Fig. 9 and Fig.10 For example, the top electrode barrier layer 1004 and the top electrode layer 1006 may be deposited together by a PVD process, as shown in the example of FIG. Fig.10 For example, in a common processing chamber (e.g. Fig.10 The active metal layer 1002, the top electrode barrier layer 1004 and the top electrode layer 1006 are deposited in situ in a PVD processing chamber 1008) and / or in a common multi-chamber processing tool.
[0106] like Fig. 20 As shown in the cross-sectional view 2000, the bottom electrode layer 902 (see Fig.19 ), switching layer 904 (see Fig.19 ), active metal layer 1002 (see Fig.19 ), top electrode barrier layer 1004 (see Fig.19 ) and the top electrode layer 1006 (see Fig.19 ) Planarization is performed to form individual RRAM cells 102 located separately at 1T1R cells 502. Cell 102 includes individual top electrodes 106, individual top electrode barrier layers 104, individual active metal layers 112, individual switching layers 110, and individual bottom electrodes 108. Planarization may be or include CMP or some other suitable planarization, for example.
[0107] Because the flattening will come from Fig.18 The patterned pattern at the RRAM cell 102 is transferred to each layer of the RRAM cell 102, so the RRAM cell 102 can be formed by a single lithography / etching process. Figures 7 to 15 The multiple lithography / etching processes of the RRAM cell 102 (for example, respectively Figure 8 and Fig.11 By reducing the number of photolithography / etching processes, the cost is reduced.
[0108] like Fig.21As shown in the cross-sectional view 2100 of FIG. 2 , an additional IMD layer 414 is deposited above the RRAM cell 102. In addition, a plurality of additional lines 404 and a plurality of additional vias 406 are formed above the RRAM cell 102, recessed into the additional IMD layer 414 above the RRAM cell 102. The plurality of additional lines 404 and the plurality of additional vias 406 may be, for example, as described in reference Fig.13 and Fig.14 Describe the formation.
[0109] Also through Fig.21 The cross-sectional view 2100 of FIG. 2 shows that separate metal wires 114 are formed and are located in the switching layer 110. For example, the formation can be as described in reference Fig.15 Implementation of the description.
[0110] Although Figures 17 to 21 The reference method is described, but it should be understood that Figures 17 to 21 The structures shown are not limited to the method but can exist independently of the method. Figures 17 to 21 Although described as a series of steps, it should be understood that in other embodiments, the order of the steps may be changed. Figures 17 to 21 Although shown and described as a specific set of steps, in other embodiments, some of the steps shown and / or described may be omitted. In addition, in other embodiments, steps not shown and / or described may be included. Figures 17 to 21 use Figure 4F The method is shown in the embodiment of the RRAM cell 102, but can be used Figure 1 , Figure 3 and Figure 4G An alternative embodiment of the method is implemented using an embodiment of the RRAM cell 102 .
[0111] In some embodiments, to implement the Figure 4G In the method of an embodiment of the RRAM cell 102, the Fig.17 The deposition of the through-hole dielectric layer 416 in the substrate and the deposition of the IMD layer 414 on top of the through-hole dielectric layer 416 are performed between Figure 8 and Fig. 9 In addition, Fig.17 The bottom electrode layer 902 and the switching layer 904 are patterned between the deposition of the through-hole dielectric layer 416 and the deposition of the IMD layer 414 on top of the through-hole dielectric layer 416. The patterning forms a separate bottom electrode 108 and a separate switching layer 110, an example of which is shown in FIG. Fig.12 and can be implemented, for example, by a photolithography / etching process or some other suitable patterning process. Fig.17 After depositing the IMD layer 414 on top of the through-hole dielectric layer 416, the top of the IMD layer 414 is patterned. Fig.18 The patterning of the IMD layer 414 in the embodiment is performed as described above. However, instead of exposing the bottom electrode line 404b Fig.18 The patterning in the embodiment of the present invention exposes the individual switching layers 110 .
[0112] refer to Fig. 22 , provides Figures 17 to 21 Block diagram 2200 of some embodiments of the method.
[0113] In 2202, an interconnect structure is partially formed over a substrate, wherein the interconnect structure includes a bottom electrode line. See, e.g. Fig.17 .
[0114] In 2204, a through-hole dielectric layer and an IMD layer are stacked and formed over the interconnect structure. See, e.g. Fig.17 .
[0115] In 2206, the through-hole dielectric layer and the IMD layer are patterned to form a memory cell opening located above and exposing the bottom electrode line. See, e.g. Fig.18 .
[0116] In 2208, a memory film is deposited on the IMD layer and fills the memory cell opening, wherein the memory film includes a switching layer, an active metal layer located above the switching layer, a top electrode barrier layer located above the active metal layer, and a top electrode layer located above the top electrode barrier layer, and wherein the top electrode barrier layer blocks the material of the top electrode layer from diffusing into the active metal layer. See, e.g. Fig.19 .
[0117] In 2210, the memory film is planarized until the top surface of the memory film is substantially flush with the top surface of the IMD layer. Fig. 20 .
[0118] In 2212, the interconnect structure around the memory cell is completed. See e.g. Fig.21 .
[0119] At 2214, a forming voltage is applied to the memory cell to form a metal filament in the switching layer. See e.g. Fig.21 .
[0120] Although Fig. 22The block diagram 2200 is shown and described as a series of steps or events here, but it should be understood that the order of these steps or events is not to be interpreted as limiting. For example, some steps can occur in different orders and / or occur simultaneously with other steps or events other than those shown and / or described here. In addition, it may not be necessary for all the steps shown to implement one or more aspects or embodiments described here, and one or more steps described here can be implemented in one or more separate steps and / or stages.
[0121] In some embodiments, the present disclosure provides an RRAM cell, which includes: a bottom electrode; a switching layer located above the bottom electrode; an active metal layer located above the switching layer; a top electrode located above the active metal layer, wherein the top electrode includes a metal element and a non-metal element, and wherein the top electrode has a lower reactivity to oxygen than the active metal layer; and a barrier layer located between the top electrode and the active metal layer, wherein the barrier layer is conductive and configured to block the diffusion of the non-metal element from the top electrode to the active metal layer. In some embodiments, the barrier layer consists essentially of a metal element. In some embodiments, the non-metal element is nitrogen. In some embodiments, the top electrode includes titanium nitride, tantalum nitride, or tungsten nitride, the active metal layer includes aluminum, and the barrier layer consists essentially of titanium, tantalum, or tungsten. In some embodiments, the thickness of the barrier layer is between about 50-100 angstroms. In some embodiments, the ratio of atoms of the metal element in the top electrode to atoms of the non-metal element in the top electrode is about 1:1 to about 1:1.1. In some embodiments, the barrier layer has a higher reactivity to oxygen than the active metal layer. In some embodiments, the barrier layer has a lower reactivity to oxygen than the active metal layer. In some embodiments, the active metal layer includes a majority element, wherein the RRAM cell further includes a conductive filament in the switching layer, and wherein the conductive filament consists essentially of the majority element.
[0122] In some embodiments, the present disclosure provides an integrated chip, comprising: a substrate; and a memory cell located above the substrate, and the memory cell comprises: a bottom electrode; and a solid electrolyte layer located above the bottom electrode; a metal layer located above the solid electrolyte layer and configured to be electrochemically dissolved in the solid electrolyte layer; a top electrode located above the metal layer and comprising a metal nitride; and a barrier layer located between the top electrode and the metal layer and directly contacting the top electrode and the metal layer, wherein the barrier layer comprises titanium, tantalum or tungsten, and wherein the barrier layer is substantially free of nitrogen along the bottom of the barrier layer. In some embodiments, the barrier layer has a U-shaped profile. In some embodiments, the width of the barrier layer is less than the width of the metal layer. In some embodiments, the integrated chip further comprises: a line located below the bottom electrode; and a through-hole dielectric layer located between the line and the memory cell, wherein the bottom electrode has a T-shaped profile, which is located above the through-hole dielectric layer and protrudes through the through-hole dielectric layer to the line. In some embodiments, the atomic percentage of the metal element in the top electrode is about 50%, wherein the atomic percentage of nitrogen in the top electrode is about 50%.
[0123] In some embodiments, the present disclosure provides a method, the method comprising: depositing a bottom electrode layer electrically coupled to the wire over the wire; depositing a dielectric layer over the bottom electrode layer; depositing a metal layer over the dielectric layer; depositing a conductive barrier layer over the metal layer; depositing a top electrode layer over the conductive barrier layer, wherein the top electrode layer includes a metal element and a non-metal element, wherein the deposition of the top electrode layer exposes the conductive barrier layer to a gas containing the non-metal element, and wherein the conductive barrier layer prevents the non-metal element from diffusing from the gas to the metal layer; patterning the bottom electrode layer and the top electrode layer, the dielectric layer, the conductive barrier layer, and the metal layer to form a memory cell. In some embodiments, the top electrode layer, the conductive barrier layer, and the metal layer are deposited in situ in the same multi-chamber processing tool. In some embodiments, the conductive barrier layer and the top electrode layer are deposited together by PVD using a common metal target and a common processing chamber. In some embodiments, during the deposition of the conductive barrier layer, there is no gas in the common processing chamber, and the gas is subsequently added to the common processing chamber during the deposition of the top electrode layer. In some embodiments, the method further comprises applying a forming voltage to the memory cell, wherein the application causes metal cations to migrate from the metal layer to the dielectric layer, and further causes metal wires to be formed from the metal cations in the dielectric layer. In some embodiments, the method further comprises: depositing a second dielectric layer covering the conductive line; and patterning the second dielectric layer to form an opening located above the conductive line and exposing the conductive line, wherein the bottom electrode layer and the top electrode layer, the dielectric layer, the conductive barrier layer, and the metal layer are deposited to cover the second dielectric layer and line the opening, wherein the patterning of the bottom electrode layer and the top electrode layer, the dielectric layer, the conductive barrier layer, and the metal layer comprises planarizing the bottom electrode layer and the top electrode layer and the conductive barrier layer.
[0124] The features of several embodiments are summarized above so that those skilled in the art can better understand aspects of the present invention. Those skilled in the art should understand that they can easily use the present invention as a basis to design or modify other processes and structures for implementing the same purpose and / or achieving the same advantages as the embodiments introduced herein. Those skilled in the art should also appreciate that this equivalent construction does not deviate from the spirit and scope of the present invention, and that they can make multiple changes, substitutions and changes herein without departing from the spirit and scope of the present invention.
Claims
1. A resistive random access memory (RRAM) cell, comprising: bottom electrode; a switching layer, located above the bottom electrode; an active metal layer, located above the switching layer; a top electrode located above the active metal layer, wherein the top electrode comprises a metal element and a non-metal element, and wherein the top electrode has a lower reactivity to oxygen than the active metal layer; and A barrier layer is located between the top electrode and the active metal layer, wherein the barrier layer is conductive and is configured to block diffusion of the non-metallic element from the top electrode to the active metal layer, the width of the barrier layer is greater than the width of the top electrode, and the barrier layer directly contacts the active metal layer and the top electrode.
2. The resistive random access memory cell according to claim 1, wherein: The barrier layer consists of the metal element.
3. The RRAM cell according to claim 1, wherein: The non-metallic element is nitrogen.
4. The RRAM cell according to claim 1, wherein: The top electrode includes titanium nitride, tantalum nitride, or tungsten nitride, the active metal layer includes aluminum, and the barrier layer is composed of titanium, tantalum, or tungsten.
5. The RRAM cell according to claim 1, wherein: The thickness of the barrier layer is between 50 and 100 angstroms.
6. The RRAM cell according to claim 1, wherein: A ratio of atoms of the metal element in the top electrode to atoms of the non-metal element in the top electrode is 1:1 to 1:1.
1.
7. The RRAM cell according to claim 1, wherein: The barrier layer has a higher reactivity with oxygen than the active metal layer.
8. The RRAM cell according to claim 1, wherein: The barrier layer is less reactive with oxygen than the active metal layer.
9. The RRAM cell according to claim 1, wherein: The active metal layer includes aluminum, copper, silver, and nickel, and wherein the resistance random access memory cell further includes: A conductive filament is located in the switching layer, wherein the conductive filament includes the same element as the active metal layer.
10. An integrated chip, comprising: substrate; as well as A memory cell is located above the substrate and includes: a bottom electrode; and a solid electrolyte layer, located above the bottom electrode; a metal layer located above the solid electrolyte layer and configured to electrochemically dissolve in the solid electrolyte layer; a top electrode located above the metal layer and comprising a metal nitride; and A barrier layer is located between the top electrode and the metal layer and directly contacts the top electrode and the metal layer, wherein the barrier layer comprises titanium, tantalum or tungsten, and wherein the barrier layer does not contain nitrogen along the bottom of the barrier layer, the width of the barrier layer is smaller than the width of the metal layer, the barrier layer has a pair of side walls located on both sides, the metal layer has a pair of side walls located on both sides, the pair of side walls of the barrier layer are located between the pair of side walls of the metal layer and are laterally offset relative to the pair of side walls of the metal layer.
11. The integrated chip according to claim 10, wherein: The barrier layer has a U-shaped profile.
12. The integrated chip according to claim 10, wherein: The top electrode reacts with oxygen with more energy than the metal layer.
13. The integrated chip according to claim 10, further comprising: A line located below the bottom electrode; as well as A through-hole dielectric layer is located between the line and the memory cell, wherein the bottom electrode has a T-shaped profile, the T-shaped profile is located on the through-hole dielectric layer and protrudes through the through-hole dielectric layer to the line.
14. The integrated chip according to claim 10, wherein: The atomic percentage of the metal element in the top electrode is 50%, and wherein the atomic percentage of nitrogen in the top electrode is 50%.
15. A method for forming an integrated chip, comprising: depositing a bottom electrode layer over the conductive line electrically coupled to the conductive line; depositing a dielectric layer over the bottom electrode layer; depositing a metal layer over the dielectric layer; depositing a conductive barrier layer over the metal layer; depositing a top electrode layer over the conductive barrier layer, wherein the top electrode layer comprises a metal element and a non-metal element, wherein deposition of the top electrode layer exposes the conductive barrier layer to a gas comprising the non-metal element, and wherein the conductive barrier layer prevents diffusion of the non-metal element from the gas to the metal layer; patterning the bottom electrode layer and the top electrode layer, the dielectric layer, the conductive barrier layer and the metal layer to form a memory cell; depositing a second dielectric layer covering the conductive line; and The second dielectric layer is patterned to form an opening located above the conductive line and exposing the conductive line, wherein the bottom electrode layer and the top electrode layer, the dielectric layer, the conductive barrier layer and the metal layer are deposited to cover the second dielectric layer and line the opening, and wherein the patterning of the bottom electrode layer and the top electrode layer, the dielectric layer, the conductive barrier layer and the metal layer includes planarizing the bottom electrode layer and the top electrode layer and the conductive barrier layer.
16. The method according to claim 15, wherein: The top electrode layer, the conductive barrier layer, and the metal layer are deposited in-situ in the same multi-chamber processing tool.
17. The method according to claim 15, wherein: The conductive barrier layer and the top electrode layer are deposited together by physical vapor deposition (PVD) using a common metal target and a common processing chamber.
18. The method according to claim 17, wherein: The gas is absent from the common process chamber during deposition of the conductive barrier layer and is subsequently added to the common process chamber during deposition of the top electrode layer.
19. The method according to claim 15, wherein: A forming voltage is applied to the memory cell, wherein the application causes metal cations to migrate from the metal layer to the dielectric layer and further causes metal filaments to be formed in the dielectric layer from the metal cations.
20. The method according to claim 15, wherein: The conductive barrier layer has a barrier thickness of 50-100 angstroms.
Citation Information
Patent Citations
Nonvolatile memory device
US20140008603A1
Bilayered Oxide Structures for ReRAM Cells
US20140175360A1
Top electrode for device structures in interconnect
US20160380193A1