Ferroelectric memory devices

By using ferroelectric films and plate crystals with a fluorite crystal structure in ferroelectric memory devices, combined with appropriate electrode materials, the problem of insufficient electrical properties of existing ferroelectric memory devices is solved, and excellent signal storage is achieved and erasure performance.

CN112243535BActive Publication Date: 2024-10-29SONY GROUP CORP
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN201980035926.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-04-23
Publication Date
2024-10-29
Estimated Expiration
2039-04-23

AI Technical Summary

Technical Problem

Existing ferroelectric memory devices have insufficient electrical properties to meet excellent storage requirements.

Method used

A ferroelectric memory device using a ferroelectric film with a fluorite crystal structure. The ferroelectric film contains plate-shaped crystallites with a length greater than the thickness, a thickness of more than 1 nm and less than 30 nm, and a length-to-thickness ratio of more than 2 and less than 100. Control the shape of crystallites and electrode materials to improve the stability of the polarization state.

Benefits of technology

The excellent electrical characteristics of the ferroelectric memory device are achieved, and the polarization state can be stably maintained for a long time, thereby improving the signal storage and erasing performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112243535B_ABST
    Figure CN112243535B_ABST
Patent Text Reader

Abstract

A ferroelectric storage device comprises a ferroelectric film and a pair of electrodes, wherein the ferroelectric film: (A) has a fluorite crystal structure, (B) contains plate-like crystals whose length (nm) is greater than its thickness (nm), (C) has a thickness of greater than 1nm and less than 30nm, and (D) has a ratio of length to thickness of greater than 2 and less than 100; the pair of electrodes are connected to the ferroelectric film.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present technology relates to a ferroelectric memory device including a ferroelectric film having a fluorite-type crystal structure. Background Art

[0002] In the field of memory devices, development of memory devices using ferroelectric films (ferroelectric memory devices) is in progress. This is because ferroelectric films have spontaneous polarization whose polarization direction can be reversed, and thus they are expected to be applied to various memory devices that utilize the reversal of the polarization direction.

[0003] Specifically, a ferroelectric field effect transistor using a ferroelectric film as a gate insulating film (hafnium oxide film) has been proposed (for example, see non-patent document 1). In this ferroelectric field effect transistor, the voltage threshold (threshold voltage) changes according to the polarization direction of the spontaneous polarization of the ferroelectric film. Therefore, it is possible to alternately switch between a state in which the drain current is high (on state) and a state in which the drain current is low (off state) by fixing the gate voltage.

[0004] Prior art literature

[0005] Non-patent literature

[0006] Non-patent document 1: “Ferroelectricity in HfO2 enables nonvolatile data storage in 28nm HKMG”, J. Muller et al., 2012 Symposium on VLSI Technology Digest of Technical Papers, pages 25 and 26. Summary of the invention

[0007] Although various proposals have been made regarding ferroelectric memory devices, the electrical characteristics of the ferroelectric memory devices are still insufficient, and thus there is room for improvement.

[0008] Therefore, it is desirable to provide a ferroelectric memory device capable of obtaining excellent electrical characteristics.

[0009] A ferroelectric memory device of one embodiment of the present technology comprises a ferroelectric film and a pair of electrodes, wherein the ferroelectric film: (A) has a fluorite crystal structure, (B) contains plate-like crystals whose length (nm) is greater than its thickness (nm), (C) has a thickness of greater than 1nm and less than 30nm, and (D) has a ratio of length to thickness of greater than 2 and less than 100, and the pair of electrodes are connected to the ferroelectric film.

[0010] Here, "crystal" refers to a microcrystal that can be regarded as a single crystal having the same composition. It should be noted that the detailed definition and determination method of plate-like crystals will be described later.

[0011] The "thickness" of the plate-like crystal refers to the dimension in the film-forming direction of the ferroelectric film when the ferroelectric film is formed using a film-forming method, and the "length" of the plate-like crystal refers to the dimension in the direction intersecting with the above-mentioned thickness. More specifically, the thickness is the dimension in the direction in which a voltage (electric field) is applied to the ferroelectric memory device, and the length is the dimension in the direction intersecting with the above-mentioned voltage application direction.

[0012] According to a ferroelectric memory device of one embodiment of the present technology, a ferroelectric film having a fluorite-type crystal structure includes plate-like crystallites whose shapes (thickness and ratio of length to thickness) satisfy the above conditions, thereby achieving excellent electrical characteristics.

[0013] It should be noted that the effects described here are not necessarily limited thereto, and may be any effects described in this technology. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 This is a plan view schematically showing the configuration of a ferroelectric memory device according to one embodiment of the present technology.

[0015] Figure 2 It is a perspective view schematically showing the structure (shape) of a crystal.

[0016] Figure 3 It is a cross-sectional view schematically showing the structure of a ferroelectric film (polycrystalline film).

[0017] Figure 4 It is a cross-sectional view schematically showing the structure of a ferroelectric film (crystal grain).

[0018] Figure 5 It is a plan view schematically showing the structure (crystal phase) of a crystallite.

[0019] Figure 6 It is a plan view for explaining a method of forming a ferroelectric film.

[0020] Figure 7 It is a plan view for explaining another method of forming a ferroelectric film.

[0021] Figure 8 This is a cross-sectional view showing the structure of a ferroelectric capacitor as an application example of a ferroelectric memory device.

[0022] Fig. 9 It is a cross-sectional view showing the structure of a ferroelectric field effect transistor as an application example of the ferroelectric memory device.

[0023] Fig.10 This is a cross-sectional view showing the structure of a ferroelectric tunnel junction memory as an application example of a ferroelectric memory device.

[0024] Fig.11 It is a graph showing the polarization-electric field characteristics of the ferroelectric capacitor of the present invention (Experimental Example 1-4).

[0025] Fig.12 It is a graph showing the polarization-electric field characteristics of the ferroelectric capacitor of the comparative example (Experimental Example 1-1).

[0026] Fig.13 Graph showing the change over time of the drain current of the ferroelectric field effect transistor. DETAILED DESCRIPTION

[0027] Hereinafter, an embodiment of the present technology will be described in detail with reference to the accompanying drawings. It should be noted that the description order is as follows.

[0028] 1. Ferroelectric memory devices

[0029] 1-1. Overall composition

[0030] 1-2. Detailed structure of ferroelectric film

[0031] 1-3. Work

[0032] 1-4. Manufacturing method

[0033] 1-5. Actions and effects

[0034] 2. Application examples of ferroelectric memory devices

[0035] 2-1. Ferroelectric capacitor

[0036] 2-2. Ferroelectric Field Effect Transistor

[0037] 2-3. Ferroelectric Tunnel Junction Memory

[0038] 2-4. Others

[0039] <1. Ferroelectric Memory Device>

[0040] First, a ferroelectric memory device according to an embodiment of the present technology will be described.

[0041] The ferroelectric memory device uses a ferroelectric film 10 (see Figure 1 A device that stores signals by changing (reversing) the polarization state (polarization direction of spontaneous polarization) of a ferroelectric memory device can be used as a variety of memory devices. Specific application examples of ferroelectric memory devices will be described later.

[0042] <1-1. Overall composition>

[0043] Figure 1 The planar structure of a ferroelectric memory device is schematically shown. Figure 1As shown in FIG. 1 , the ferroelectric memory device comprises a ferroelectric film 10, an upper electrode 20 and a lower electrode 30. Figure 1 In FIG. 1 , the ferroelectric film 10 is subjected to a shadowing process.

[0044] [Ferroelectric film]

[0045] As described above, the ferroelectric film 10 is a main part of the ferroelectric memory device, and its polarization state can be changed so that a signal can be stored. The ferroelectric film 10 has a fluorite crystal structure and is a so-called fluorite ferroelectric thin film. In addition, the ferroelectric film 10 includes plate-like crystals as crystals forming the crystal structure. It should be noted that the detailed structure of the ferroelectric film 10 (including the definition of plate-like crystals, etc.) will be described later.

[0046] The ferroelectric film 10 contains any one or more of the ferroelectric materials. Specifically, the ferroelectric materials are, for example, zirconium oxide (ZrO2), hafnium oxide (HfO2) and cerium oxide (CeO2). Among them, the ferroelectric material can be, for example, a solid solution of two or more of the above-mentioned series of materials. The solid solution contains, for example, a zirconium-hafnium compound represented by the following formula (1). This is because sufficient ferroelectricity can be obtained in the ferroelectric film 10, and plate-like crystals are easily formed in the formation process of the ferroelectric film 10.

[0047] Hf x Zr 1-x O2……(1)

[0048] Among them, x satisfies 0 <x<1。

[0049] The zirconium-hafnium compound is not particularly limited as long as it is a compound represented by formula (1). Specifically, the zirconium-hafnium compound is, for example, Hf 0.5 Zr 0.5 O2 and Hf 0.25 Zr 0.75 O2, etc.

[0050] Among them, the ferroelectric material is preferably zirconium oxide, a zirconium-hafnium compound, or the like, and more preferably zirconium oxide, or the like, because the ferroelectricity of the ferroelectric film 10 can be further improved.

[0051] [Upper electrode and lower electrode]

[0052] The upper electrode 20 and the lower electrode 30 are a pair of electrodes for applying a voltage to the ferroelectric film 10. The upper electrode 20 and the lower electrode 30 are separated from each other and are both connected to the ferroelectric film 10.

[0053] The upper electrode 20 and the lower electrode 30 each include any one or more of the conductive materials. Specifically, the conductive materials are, for example, silicon (Si), platinum (Pt), ruthenium (Ru), metal oxides and metal nitrides. Metal oxides are, for example, indium oxide (In2O3), gallium oxide (Ga2O3), zinc oxide (ZnO), tin oxide (SnO), indium tin oxide (ITO) and indium zinc oxide (IZO). Metal nitrides are, for example, titanium nitride (TiN) and tantalum nitride (TaN). Among them, the conductive material can be, for example, a solid solution of two or more of the above-mentioned series of materials. This is because voltage can be stably applied to the ferroelectric film 10.

[0054] It should be noted that, as long as the upper electrode 20 and the lower electrode 30 are separated from each other and connected to the ferroelectric film 10, there is no particular limitation on the connection positions of the upper electrode 20 and the lower electrode 30 relative to the ferroelectric film 10. Therefore, the connection positions of the upper electrode 20 and the lower electrode 30 can be arbitrarily set according to conditions such as the purpose of the ferroelectric memory device.

[0055] In detail, for example, in Figure 1 The following situation is shown in the figure: the ferroelectric film 10 is arranged between the upper electrode 20 and the lower electrode 30, so that the upper electrode 20 and the lower electrode 30 are opposite to each other across the ferroelectric film 10. That is, for example, in the case where the ferroelectric film 10 has two surfaces facing opposite sides to each other, the upper electrode 20 is arranged on one of the two surfaces (for example, the upper surface), and the lower electrode 30 is arranged on the other surface (for example, the lower surface). However, the setting positions of the upper electrode 20 and the lower electrode 30 relative to the ferroelectric film 10 can be changed arbitrarily. In the following, the upper surface and the lower surface of the ferroelectric film 10 mentioned above will be referred to at any time.

[0056] Specifically, for example, the ferroelectric film 10 is disposed between the upper electrode 20 and the lower electrode 30, but the upper electrode 20 and the lower electrode 30 may not be opposite to each other via the ferroelectric film 10. That is, for example, the upper electrode 20 is disposed on the upper surface of the ferroelectric film 10, and the lower electrode 30 is disposed on the lower surface of the ferroelectric film 10, but the upper electrode 20 and the lower electrode 30 may not be opposite to each other. In this case, the position of the upper electrode 20 and the position of the lower electrode 30 are offset from each other in the direction along the upper surface (or lower surface) of the ferroelectric film 10.

[0057] Alternatively, for example, both the upper electrode 20 and the lower electrode 30 may be disposed on the upper surface (or lower surface) of the ferroelectric film 10 .

[0058] <1-2. Detailed Structure of Ferroelectric Film>

[0059] Next, the basic composition and definition of plate-like crystals will be described, and then the shape and crystal phase of the plate-like crystals will be described, and a method for determining the shape of the crystals will be described.

[0060] [Basic composition of plate-like crystals]

[0061] Figure 2 The three-dimensional structure of the crystal 1C is schematically shown in order to explain the structure (shape) of the crystal 1C. Figure 3 and Figure 4 The cross-sectional structure of the ferroelectric film 10 is schematically shown. Specifically, Figure 3 The cross-sectional structure of the polycrystalline film 1 is shown in FIG. Figure 4 2 shows the cross-sectional structure of the crystal grain 1G.

[0062] As described above, the ferroelectric film 10 includes plate-like crystallites. As described above, the "crystallites" refer to crystallites that can be regarded as single crystals having the same composition.

[0063] Specifically, if Figure 1 As shown, the crystallite 1C has a plate-like shape with a thickness T (nm) and a length L (nm), and thus the length L is greater than the thickness T.

[0064] Here, as described above, "thickness T" refers to the dimension in the film-forming direction of the ferroelectric film 10 when the ferroelectric film 10 is formed using the film-forming method, and as described above, "length L" refers to the dimension in the direction intersecting with the film-forming direction of the above-mentioned ferroelectric film 10. It should be noted that the details of the film-forming method will be described later. More specifically, as described later, the thickness T is the dimension in the direction of applying a voltage (electric field) to the ferroelectric memory device, and the length L is the dimension in the direction intersecting with the above-mentioned voltage application direction.

[0065] The direction for specifying the length L is not particularly limited as long as it intersects with the thickness T, and thus may be any direction. Figure 2 , for example, the thickness T is a dimension in the up-down direction, and the length L is a dimension in the left-right direction.

[0066] It should be noted that in Figure 2 , for example, shows a case where the crystallite 1C is in a flat plate shape. In this case, the crystallite 1C has a flat surface, and therefore the length L is specified along the flat surface. However, the crystallite 1C is not limited to a flat plate shape, and may be a twisted plate shape, that is, a curved plate shape. In this case, the crystallite 1C has a curved surface, and therefore the length L is specified along the curved surface.

[0067] As described above, if the crystallite 1C is in a flat plate shape, the thickness T is in principle a dimension in the direction in which the voltage is applied to the ferroelectric memory device. However, in the case where the crystallite 1C is in a curved plate shape, strictly speaking, the thickness T is sometimes a dimension in a direction slightly deviated from the direction in which the voltage is applied to the ferroelectric memory device.

[0068] The reason why the shape of the crystallite 1C forming the ferroelectric film 10 is plate-like, that is, the length L is greater than the thickness T, is that it is easier to maintain the polarization state (polarization direction of spontaneous polarization) of the ferroelectric film 10 than when the length L is equal to the thickness T. As a result, it is easier to maintain the signal recorded in the ferroelectric memory device without being erased. It should be noted that the crystallite 1C whose length L is equal to the thickness T is a so-called spherical crystallite 1C.

[0069] [Definition of plate-like crystals]

[0070] When the ferroelectric material is formed into a film by using a film forming method to form the ferroelectric film 10, for example, Figure 3 As shown, a polycrystalline film 1 (thickness T) is formed. The amount of the ferroelectric material formed (thickness T) is not particularly limited, and is, for example, about 10 nm.

[0071] The polycrystalline film 1 includes a plurality of crystal grains 1G, which are so-called crystal blocks. The plurality of crystal grains 1G are adjacent to each other, and gaps 1S (depressions) are formed at the boundaries between the adjacent crystal grains 1G. When the polycrystalline film 1 is observed using an electron microscope, a concave-convex structure having a plurality of gaps 1S is observed, so each crystal grain 1G can be identified based on the gaps 1S. That is, one crystal grain 1G can be visually distinguished from other crystal grains 1G by the gaps 1S. It should be noted that the type of electron microscope is not particularly limited, and may be, for example, a transmission electron microscope (TEM).

[0072] In the case where the ferroelectric film 10 is a polycrystalline film 1 and the polycrystalline film 1 includes a plurality of crystal grains 1G, for example, Figure 3 As shown, each crystal grain 1G may be a crystallite 1C. That is, since each crystal grain 1G is a single crystal, the crystal grain 1G itself may be a crystallite 1C.

[0073] However, only a part of the plurality of crystal grains 1G may be crystallites 1C. In this case, for example, as described later, the remaining crystal grains 1G of the plurality of crystal grains 1G include a plurality of crystallites 1C (see Figure 4 ).

[0074] In addition, when the ferroelectric film 10 is a polycrystalline film 1 and the polycrystalline film 1 includes a plurality of crystal grains 1G, for example, Figure 4As shown, one crystal grain 1G may include a plurality of crystallites 1C. This is because, for example, any one or two or more of low-angle grain boundaries, stacking defects, and twin crystals are formed in one crystal grain 1G.

[0075] [Shape of plate-like crystallites]

[0076] In the plate-like crystallite 1C, as described above, the length L is greater than the thickness T. The thickness T is greater than 1 nm and less than 30 nm, and the ratio L / T of the length L to the thickness T is greater than 2 and less than 100. This is because, in the ferroelectric film 10 having a fluorite-type crystal structure, the shape of the plate-like crystallite 1C becomes appropriate, so it is easy to maintain the polarization state (polarization direction of spontaneous polarization) of the ferroelectric film 10 without changing. Therefore, when a signal is stored in the ferroelectric memory device, it is easy to maintain the signal without being erased.

[0077] Among them, the ratio L / T is more preferably not less than 5 and not more than 50. This is because it is easier to maintain the polarization state of the ferroelectric film 10, and thus it is easier to maintain the signal stored in the ferroelectric memory device.

[0078] It should be noted that in Figure 2 to Figure 4 , respectively, the following cases are shown: the shape of the crystallite 1C observed from the direction intersecting with the thickness T (the front side of the paper surface), more specifically, the shape (projected shape) formed by the outer edge (contour) of the crystallite 1C projected in the direction intersecting with the thickness T is a substantially rectangular shape. However, the projected shape of the crystallite 1C is not particularly limited as long as the above conditions are satisfied with respect to the thickness T and the ratio L / T.

[0079] Specifically, the projected shape of the crystal 1C may be, for example, a substantially elliptical shape or a polygonal shape, or may be other shapes other than these. Other shapes are not particularly limited, for example, a container-like shape described later (see Figure 7 ). In the case where the thickness T varies depending on the position, the thickness T is set to the maximum thickness, and in the case where the length L varies depending on the position, the length L is set to the maximum length.

[0080] [Crystal phase of plate crystallites]

[0081] Figure 5 The planar structure (crystal phase) of the crystallite 1C is schematically shown. In the ferroelectric film 10 (polycrystalline film 1) having a fluorite type crystal structure, for example, Figure 5 As shown, each crystallite 1C forming the polycrystalline film 1 includes a plurality of crystal phases 1P.

[0082] Specifically, the crystallite 1C includes, for example, three crystal phases 1P. The crystal phase 1P marked with "m" is a monoclinic crystal phase. The crystal phase 1P marked with "t" is a tetragonal crystal phase. The crystal phase 1P marked with "o" is an orthorhombic crystal phase.

[0083] Among the three crystal phases 1P (monoclinic phase, tetragonal phase, and orthorhombic phase), the orthorhombic phase is the most likely to show ferroelectricity. Therefore, the crystal phase of the crystallite 1C preferably includes the orthorhombic phase. This is because sufficient ferroelectricity can be obtained in the ferroelectric film 10.

[0084] [Method for determining plate-like crystals]

[0085] Here, a method of determining the existence range of the crystallite 1C and a method of determining the shape of the crystallite 1C are described.

[0086] (Method for determining the range of existence of crystallites)

[0087] When determining the existence range of the crystallite 1C, for example, after forming the ferroelectric material into a film using a film forming method to form the ferroelectric film 10 (polycrystalline film 1), the ferroelectric film 10 is observed using an electron microscope as described above. In this way, the contrast in each crystallite 1C varies due to the difference in crystal structure (orientation direction of the crystal), so the existence range of each crystallite 1C can be determined based on the difference in the contrast. That is, the area with almost uniform contrast is the existence range of one crystallite 1C.

[0088] In this case, it is preferred to focus on the above-mentioned concavo-convex structure having a plurality of gaps 1S. This is because the gap 1S is a mark for determining the boundary between a plurality of grains 1G, and therefore based on the existence of the gap 1S, the adjacent grains 1G can be visually distinguished. In this way, when the existence range of the grain 1G is determined based on the existence of the gap 1S, the existence range of the crystallite 1C can also be determined by focusing on the uniformity of the contrast inside the grain 1G. Specifically, when the contrast of the grain 1G is almost uniform, the grain 1G does not contain a plurality of crystallites 1C, and therefore the grain 1G itself is a crystallite 1C. On the other hand, when the contrast of the grain 1G is uneven, more specifically, when a plurality of regions with mutually different contrasts are observed inside the grain 1G, the grain 1G contains a plurality of crystallites 1C. In this case, each region with mutually different contrasts is a crystallite 1C.

[0089] It should be noted that when the ferroelectric film 10 includes two or more different ferroelectric materials, an interface is sometimes formed between a crystal phase of a single crystal formed by a certain ferroelectric material and a crystal layer of a single crystal formed by another ferroelectric material in the polycrystalline film 1. In this case, the crystal phase of a single crystal formed by any one ferroelectric material is a crystallite 1C.

[0090] (Method for determining crystallite shape)

[0091] When determining the shape of the crystallite 1C, for example, after determining the existence range of the crystallite 1C according to the above steps, the shape of the crystallite 1C is confirmed. In this case, for example, the shape of the crystallite 1C can be visually confirmed. Or, for example, after measuring the length L and thickness T of the crystallite 1C, the size relationship between the length L and the thickness T can be studied.

[0092] Thus, if the length L is greater than the thickness T, it can be determined that the crystallite 1C having the length L and the thickness T is plate-shaped. On the other hand, when the length L is equal to the thickness T, it can be determined that the crystallite 1C having the length L and the thickness T is not plate-shaped. In the former case in particular, based on the length L and the thickness T, it can be determined whether the thickness T and the ratio L / T satisfy the above conditions, respectively.

[0093] <1-3. Work>

[0094] In the ferroelectric memory device, a voltage is applied between the upper electrode 20 and the lower electrode 30. In this case, as described above, the polarization state (polarization direction of spontaneous polarization) of the ferroelectric film 10 changes (reverses) according to the application of the voltage. Thus, a signal is stored in the ferroelectric memory device, and the signal stored in the ferroelectric memory device is erased.

[0095] <1-4. Manufacturing method>

[0096] Figure 6 and Figure 7 They are shown corresponding to Figure 1 ’s planar structure is used to illustrate the method of forming the ferroelectric film 10.

[0097] Here, a method for forming the ferroelectric film 10, which is a main part of the ferroelectric memory device, in the method for manufacturing the ferroelectric memory device will be described. The ferroelectric film 10 is formed to include the plate-like crystals 1C according to the steps described below.

[0098] [Method 1 for forming ferroelectric film]

[0099] When the ferroelectric film 10 is formed, for example, Figure 6As shown, a film forming method is used to form a ferroelectric material on the surface of a substrate 40. The substrate 40 described here is a support body when the ferroelectric film 10 is formed, and has, for example, a flat surface.

[0100] In this case, by controlling the type of film forming method, the speed during film forming (film forming speed), the material of the substrate 40, the temperature of the substrate 40, etc., the ferroelectric film 10 can be formed in a manner including the plate-like crystals 1C.

[0101] Specifically, the film forming method is, for example, any one or two or more of a sputtering method, an atomic layer deposition method, a chemical vapor deposition method, and a coating method.

[0102] From the viewpoint of controlling the shape of the crystal 1C (the relationship between the length L and the thickness T) to be plate-like, the material of the substrate 40 is a material having good compatibility with the ferroelectric material. Specifically, the material forming the substrate 40 is, for example, any one or more of silicon, germanium, platinum, ruthenium, gold, silver, copper, aluminum, iridium, titanium, tantalum, indium, zinc, tin, gallium, carbon, molybdenum, and tungsten. In addition, the material forming the substrate 40 may be, for example, any one or more of compounds such as oxides, nitrides, sulfides, and selenides of the above-mentioned series of materials.

[0103] The base 40 may be, for example, a rigid substrate, or a flexible film or foil.

[0104] Compared with a fast film forming speed, a slow film forming speed is preferred. This is because the slower the film forming speed, the more the shape of the crystallite 1C tends to be plate-like. In detail, the faster the film forming speed, the smaller the length L becomes relative to the thickness T, and the slower the film forming speed, the larger the length L becomes relative to the thickness T.

[0105] The temperature of the substrate 40 is preferably high rather than low. This is because the higher the temperature of the substrate 40, the more the shape of the crystallite 1 tends to be plate-like. In detail, the lower the temperature of the substrate 40, the smaller the length L becomes relative to the thickness T, and the higher the temperature of the substrate 40, the larger the length L becomes relative to the thickness T.

[0106] [Method 2 for forming ferroelectric film]

[0107] It should be noted that when forming the ferroelectric film 10, the projection shape of the ferroelectric film 10 can be arbitrarily changed. Figure 7 As shown, by using the substrate 50 having the recess 50U, the ferroelectric material can be formed into a film inside the recess 50U. The details of the film forming method, the film forming speed, the material of the substrate 50, and the temperature of the substrate 50 are as described above.

[0108] In this case, inside the recess 50U, the ferroelectric material is formed into a film in a manner that covers the bottom surface and the inner wall surface, respectively, thereby forming a ferroelectric film 10 whose projected shape is a container shape. The ferroelectric film 10 includes, for example: a bottom 10B that covers the bottom surface; and a wall portion 10W that covers the inner wall surface and surrounds the bottom 10B from all sides. When the bottom 10B and the wall portion 10W are formed, a grain boundary is formed between the bottom 10B and the wall portion 10W. In this way, the ferroelectric material is formed into a film in a manner that includes plate-like crystals 1C, respectively, at the bottom 10B and the wall portion 10W.

[0109] <1-5. Actions and Effects>

[0110] According to the ferroelectric memory device, the ferroelectric film 10 having a fluorite crystal structure includes plate-like crystallites 1C, and the shape (thickness T and ratio L / T) of the plate-like crystallites 1C satisfies the above-mentioned conditions (T=1 nm or more and 30 nm or less, and L / T=2 or more and less than 100). In this case, as described above, compared with the case where the length L is equal to the thickness T (spherical crystallites 1C), the polarization state (polarization direction of spontaneous polarization) of the ferroelectric film 10 is easily maintained without changing. Therefore, it is easy to maintain the signal stored in the ferroelectric memory device without being erased, so that excellent electrical characteristics can be obtained.

[0111] In particular, when the ratio L / T is 5 or more and 50 or less, the polarization state of the ferroelectric film 10 is more easily maintained, and a higher effect can be obtained.

[0112] In addition, if the ferroelectric film 10 contains zirconium oxide or the like, sufficient ferroelectricity can be obtained in the ferroelectric film 10, and the plate-like crystals 1C can be easily formed in the formation step of the ferroelectric film 10, so that a better effect can be obtained.

[0113] In addition, if the crystal phase 1P of the ferroelectric film 10 includes an orthorhombic phase, sufficient ferroelectricity can be obtained in the ferroelectric film 10, so that a higher effect can be obtained.

[0114] In addition, if the upper electrode 20 and the lower electrode 30 are respectively made of silicon, metal oxide, metal nitride, etc., a voltage can be stably applied to the ferroelectric film 10, so that a better effect can be obtained.

[0115] <2. Application Examples of Ferroelectric Memory Devices>

[0116] Next, application examples of the ferroelectric memory device described above will be described. Components of the ferroelectric memory device described above will be referred to as needed in the following.

[0117] As described above, the application examples of the ferroelectric memory device are not particularly limited as long as the device can store or erase a signal by utilizing the change in the polarization state of the ferroelectric film 10. Here, three specific application examples of the ferroelectric memory device are described.

[0118] <2-1. Ferroelectric capacitor>

[0119] Figure 8 FIG. 4 shows a cross-sectional structure of a ferroelectric capacitor. Figure 8 As shown, the ferroelectric capacitor includes an insulating film 110, an upper electrode 120, and a lower electrode 130. The insulating film 110, the upper electrode 120, and the lower electrode 130 correspond to the ferroelectric film 10, the upper electrode 20, and the lower electrode 30, respectively.

[0120] The insulating film 110 has the same structure as the ferroelectric film 10. That is, the insulating film 110 includes a ferroelectric material such as zirconium oxide. In addition, the insulating film 110 includes plate-like crystals 1C, and the shape (thickness T and ratio L / T) of the plate-like crystals 1C satisfies the above-mentioned conditions.

[0121] The upper electrode 120 and the lower electrode 130 have the same configurations as the upper electrode 20 and the lower electrode 30, respectively. The material forming the upper electrode 120 and the material forming the lower electrode 130 may be the same as or different from each other.

[0122] When the material forming the upper electrode 120 and the material forming the lower electrode 130 are the same, the material forming the upper electrode 120 and the material forming the lower electrode 130 are, for example, platinum and indium tin oxide, respectively. On the other hand, when the material forming the upper electrode 120 and the material forming the lower electrode 130 are different from each other, the material forming the upper electrode 120 is, for example, titanium nitride, and the material forming the lower electrode 130 is, for example, indium tin oxide.

[0123] In the ferroelectric capacitor, when a voltage is applied between the upper electrode 120 and the lower electrode 130, the polarization direction and polarization amount of the insulating film 110 change according to the applied direction and applied amount of the voltage. Therefore, by using the change in the polarization state of the insulating film 110, a signal is stored between the upper electrode 120 and the lower electrode 130, and the signal is erased.

[0124] <2-2. Ferroelectric Field Effect Transistor>

[0125] Fig. 9 The cross-sectional structure of a ferroelectric field effect transistor (FeFET) is shown. Fig. 9As shown, the ferroelectric field effect transistor includes a substrate 210, an isolation insulating film 220, a source electrode 230 and a drain electrode 240, a semiconductor film 250, a gate insulating film 260 and a gate electrode 270. The gate insulating film 260 corresponds to the ferroelectric film 10. The gate electrode 270 corresponds to the upper electrode 20. The source electrode 230 and the drain electrode 240 correspond to the lower electrode 30.

[0126] The source electrode 230 and the drain electrode 240 are formed on the substrate 210 via the isolation insulating film 220 and are separated from each other. The semiconductor film 250 is formed on the isolation insulating film 220, the source electrode 230, and the drain electrode 240 in a manner that one end is connected to the source electrode 230 and the other end is connected to the drain electrode 240. The gate electrode 270 is formed on the semiconductor film 250 via the gate insulating film 260. It should be noted that the gate insulating film 260 is formed not only on the semiconductor film 250, but also around the semiconductor film 250.

[0127] The substrate 210 includes, for example, silicon. The substrate 210 may be, for example, a rigid substrate, or a flexible film or foil. The isolation insulating film 220 includes, for example, an insulating material such as silicon oxide. The semiconductor film 250 includes, for example, a semiconductor material such as indium oxide.

[0128] The gate insulating film 260 has the same structure as the ferroelectric film 10. That is, the gate insulating film 260 includes a ferroelectric material such as zirconium oxide. In addition, the gate insulating film 260 includes a plate-like crystallite 1C, and the shape (thickness T and ratio L / T) of the plate-like crystallite 1C satisfies the above conditions.

[0129] The source electrode 230, the drain electrode 240, and the gate electrode 270 each have the same structure as the upper electrode 20 and the lower electrode 30. The material forming the source electrode 230 and the material forming the gate electrode 270 may be the same or different from each other, and the material forming the drain electrode 240 and the material forming the gate electrode 270 may be the same or different from each other. The point that the materials forming the source electrode 230 and the materials forming the drain electrode 240 may be the same or different from each other also applies to the materials forming the source electrode 230 and the drain electrode 240.

[0130] When the material forming the source electrode 230 and the material forming the drain electrode 240 are the same as each other and the material forming the source electrode 230 and the material forming the drain electrode 240 are respectively different from the material forming the gate electrode 270, the material forming the source electrode 230 and the material forming the drain electrode 240 are respectively, for example, titanium nitride, etc., and the material forming the gate electrode 270 is, for example, indium tin oxide, etc.

[0131] In this ferroelectric field effect transistor, when a voltage (gate voltage) is applied between the source electrode 230 and the gate electrode 270, the polarization state (polarization direction of spontaneous polarization) of the gate insulating film 260 changes. As a result, the threshold voltage changes according to the change in the polarization state of the gate insulating film 260, and the current (drain current) flowing from the source electrode 230 to the drain electrode 240 changes.

[0132] Specifically, for example, if the semiconductor film 250 includes an N-type semiconductor material, when the threshold voltage changes in the negative direction, the drain current increases when the gate voltage = 0, and when the threshold voltage changes in the positive direction, the drain current decreases when the gate voltage = 0. Thus, in the ferroelectric field effect transistor, a state in which the drain current is high (on state) and a state in which the drain current is low (off state) are alternately switched.

[0133] Therefore, by utilizing the change in the polarization state of the gate insulating film 260 , the on state and the off state can be alternately switched, so that a signal is stored between the source electrode 230 and the drain electrode 240 and the gate electrode 270 , and the signal is erased.

[0134] <2-3. Ferroelectric Tunnel Junction Memory>

[0135] Fig.10 The cross-sectional structure of a ferroelectric tunnel junction memory (FTJ) is shown. Fig.10 As shown, the ferroelectric tunnel junction memory includes a tunnel insulating film 310, an upper electrode (positive electrode) 320, and a lower electrode (negative electrode) 330. The tunnel insulating film 310, the upper electrode 320, and the lower electrode 330 correspond to the ferroelectric film 10, the upper electrode 20, and the lower electrode 30, respectively.

[0136] The tunnel insulating film 310 has the same structure as the ferroelectric film 10. That is, the tunnel insulating film 310 includes a ferroelectric material such as zirconium oxide. In addition, the tunnel insulating film 310 includes a plate-like crystallite 1C, and the shape (thickness T and ratio L / T) of the plate-like crystallite 1C satisfies the above-mentioned conditions.

[0137] The tunnel insulating film 310 functions as a tunnel barrier for controlling whether current flows between the positive electrode 320 and the negative electrode 330. Therefore, the thickness of the tunnel insulating film 310 is preferably thin enough to allow the so-called tunnel effect to be observed. Specifically, the thickness of the tunnel insulating film 310 is not particularly limited, and is, for example, not less than 1 nm and not more than 5 nm.

[0138] The upper electrode 320 and the lower electrode 330 have the same structure as the upper electrode 20 and the lower electrode 30, respectively. The material forming the upper electrode 320 and the material forming the lower electrode 330 may be the same as or different from each other. It should be noted that the material forming the upper electrode 320 and the material forming the lower electrode 330 may be, for example, a semiconductor material.

[0139] For example, when the upper electrode 320 and the lower electrode 330 are formed of different materials, the upper electrode 320 is formed of titanium nitride, and the lower electrode 330 is formed of indium tin oxide.

[0140] In the ferroelectric tunnel junction memory, when a voltage is applied between the upper electrode 320 and the lower electrode 330, the polarization state (polarization direction of spontaneous polarization) of the tunnel insulating film 310 changes according to the application of the voltage, thereby changing the resistance of the tunnel insulating film 310. Therefore, by utilizing the change in the polarization state of the tunnel insulating film 310, a signal is stored between the positive electrode 320 and the negative electrode 330, and the signal is erased.

[0141] <2-4. Others>

[0142] Of course, the application examples of the ferroelectric memory device are not limited to the above three application examples (ferroelectric capacitor, ferroelectric field effect transistor and ferroelectric tunnel junction memory). Other application examples are not particularly limited, such as ferroelectric diodes.

[0143] [Example]

[0144] Next, embodiments of the present technology will be described. It should be noted that the description order is as follows.

[0145] 1. Ferroelectric capacitor

[0146] 2. Ferroelectric Field Effect Transistor

[0147] 3. Ferroelectric tunnel junction memory

[0148] 4. Summary

[0149] <1. Ferroelectric capacitors>

[0150] (Examples 1-1 to 1-10)

[0151] First, manufacture Figure 8 The performance of the ferroelectric capacitor was evaluated after

[0152] [Manufacturing of ferroelectric capacitors]

[0153] A ferroelectric capacitor was fabricated, comprising an insulating film 110 (ferroelectric material = zirconium oxide, thickness = 10 nm), an upper electrode 120 (conductive material = indium tin oxide, diameter = 100 μm), and a lower electrode 130 (conductive material = indium tin oxide, diameter > 100 μm).

[0154] When forming the insulating film 110, a ferroelectric material (zirconium oxide) is deposited on the surface of the lower electrode 130 by using a sputtering method, and the insulating film 110 is formed on the lower electrode 130. Then, a conductive material (indium tin oxide) is deposited on the surface of the insulating film 110 by using a sputtering method, and the upper electrode 120 is formed on the insulating film 110.

[0155] It should be noted that when the insulating film 110 is formed, the shape (thickness T (nm), length L (nm) and ratio L / T) of the crystallite 1C contained in the insulating film 110 is changed by changing the film formation speed of the ferroelectric material. The relationship between the film formation speed of the ferroelectric material and the shape of the crystallite 1C is as described above, and the details about the thickness T, length L and ratio L / T are shown in Table 1.

[0156] [Performance Evaluation of Ferroelectric Capacitors]

[0157] As the performance of ferroelectric capacitors, polarization characteristics and retention characteristics were studied.

[0158] (Polarization characteristics)

[0159] When studying the polarization characteristics, a voltage (electric field) was applied to the ferroelectric capacitor (insulating film 110) and the polarization amount of the ferroelectric capacitor was measured, and the result was Fig.11 and Fig.12 Results shown.

[0160] Fig.11 and Fig.12 The polarization-electric field characteristics of the ferroelectric capacitor are shown (horizontal axis: electric field E (MV / cm), vertical axis: polarization P (μC / cm 2 )). It should be noted that Fig.11 In the figure, the measurement results of Experimental Examples 1 to 4 are shown, taking the case where the shape of crystal 1C is plate-shaped as a representative example. Fig.12 , the measurement results of Experimental Example 1-1 in which the shape of the crystallite 1C is spherical are shown. It should be noted that, Fig.11 and Fig.12 The electric field E when the polarization P is zero (coercive electric field Ec, -Ec) and the polarization P when the electric field E is zero (residual polarization Pr, -Pr) are shown respectively.

[0161] (Maintaining characteristics)

[0162] When studying the retention characteristics, 2Pr (μC / cm 2 ) and the ratio P2 / P1.

[0163] When calculating 2Pr, we use Fig.11 and Fig.12 After the remnant polarization Pr is determined, the remnant polarization Pr is doubled.

[0164] When calculating the ratio P2 / P1, first, based on Fig.11 and Fig.12 The coercive electric field Ec was determined. Then, an electric field was applied to the ferroelectric capacitor (insulating film 110) to cause spontaneous polarization of the insulating film 110. Then, an electric field was applied in the opposite direction to the direction of spontaneous polarization, and the residual polarization P1 (μC / cm 2 ), and after 10 5 The residual polarization after seconds P2 (μC / cm 2 ). In this case, an electric field equivalent to about four times the coercive electric field Ec (=6 MV / cm) is applied, and the application time is 1 msec. Finally, the ratio P2 / P1 of the residual polarization P2 to the residual polarization P1 is calculated. The closer the value of the ratio P2 / P1 is to 1, the less likely the residual polarization is to decrease over time, thereby showing excellent retention characteristics.

[0165]

Table 1

[0166]

[0167] [Investigation]

[0168] The performance of the ferroelectric capacitor showed the following tendency.

[0169] First, regarding the polarization characteristics, such as Fig.11 and Fig.12 As shown in Table 1, in the case of using plate-like crystals 1C (Experimental Example 1-4), compared with the case of using spherical crystals 1C (Experimental Example 1-1), almost equal coercive electric field Ec was obtained, and almost equal residual polarization Pr was obtained. Therefore, as shown in Table 1, in the former case, almost equal 2Pr was obtained as in the latter case.

[0170] However, when the plate-like crystals 1C are used, the polarization P changes rapidly near the coercive electric field Ec, unlike the case of using the spherical crystals 1C. Therefore, in the former case, the change amount of the polarization P near the electric field E=0 MV / cm is smaller than that in the latter case.

[0171] Therefore, when the plate-like crystals 1C having an appropriate shape are used, the polarization state of the insulating film 110 is less susceptible to external disturbances, and it is therefore considered that the polarization state of the insulating film 110 can be stably maintained for a long period of time.

[0172] In addition, regarding the retention characteristics, as shown in Table 1, when a plate-like crystal 1C is used (Experimental Examples 1-2 to 1-10), the ratio P2 / P1 changes according to the shape of the plate-like crystal 1C. Specifically, when the shape of the plate-like crystal 1C satisfies appropriate conditions (T=1 nm or more and 30 nm or less, and L / T=2 or more and less than 100) (Experimental Examples 1-2 to 1-6, 1-8, 1-9), the ratio P2 / P1 increases significantly compared to the case where spherical crystals 1C are used (Experimental Example 1-1). Therefore, the polarization state of the insulating film 110 can be stably maintained for a long time. It should be noted that when the shape of the plate-like crystal 1C does not satisfy appropriate conditions (Experimental Examples 1-7, 1-10), the ferroelectric capacitor does not work at all.

[0173] In particular, when the plate-like crystals 1C having an appropriate shape were used, if the ratio L / T was 5 or more and 50 or less (Experimental Examples 1-3 to 1-5), the ratio P2 / P1 was further increased.

[0174] <2. Ferroelectric Field Effect Transistor>

[0175] (Examples 2-1 to 2-10)

[0176] Next, make Fig. 9 After the ferroelectric field effect transistor shown, the performance of the ferroelectric field effect transistor was evaluated.

[0177] [Fabrication of ferroelectric field effect transistor]

[0178] A ferroelectric field effect transistor (channel width = 1 μm, gate length = 1 μm) was manufactured, which includes a substrate 210 (silicon, thickness = 380 μm), an isolation insulating film 220 (insulating material = silicon oxide, thickness = 0.5 μm), a source electrode 230 (conductive material = titanium nitride, thickness = 0.02 μm), a drain electrode 240 (conductive material = titanium nitride, thickness = 0.02 μm), a semiconductor film 250 (N-type semiconductor material = indium oxide, thickness = 30 nm), a gate insulating film 260 (ferroelectric material = zirconium oxide, thickness = 0.008 μm), and a gate electrode 270 (conductive material = indium tin oxide, thickness = 0.1 μm).

[0179] When the gate insulating film 260 is formed, as shown in Table 2, the shape (thickness T (nm), length L (nm) and ratio L / T) of the crystal 1C contained in the gate insulating film 260 is changed according to the same steps as when the above-mentioned ferroelectric capacitor (insulating film 110) is formed.

[0180] [Performance Evaluation of Ferroelectric Field Effect Transistors]

[0181] As the performance of ferroelectric field effect transistors, voltage change characteristics and retention characteristics were studied.

[0182] (Voltage variation characteristics)

[0183] When studying the voltage change characteristics, in the ferroelectric field effect transistor, the absolute value of the change in threshold voltage Vt when the gate voltage Vg (=6V) was applied (application time = 1msec) and when the gate voltage Vg (=-6V) was applied (application time = 1msec) was measured (voltage change ΔVt (V)).

[0184] (Maintaining characteristics)

[0185] When the retention characteristics were examined, after a gate voltage Vg (=6 V) was applied to the ferroelectric field effect transistor (application time=1 msec), the drain current Id when the gate voltage Vg=0 V was measured over time. Fig.13 The time-dependent change of the drain current Id is shown (horizontal axis: time T (seconds), and vertical axis: drain current Id (μA)). Fig.13 In the figure, the measurement results (○) of Experimental Example 2-4 (ratio L / T=10) are shown, taking the case where the shape of crystal 1C is plate-like as a representative example, and the measurement results (□) of Experimental Example 2-1 (ratio L / T=1) where the shape of crystal 1C is spherical are shown.

[0186] In addition, when the drain current Id is measured over time, the drain current Id1 (μA) after 10 seconds is measured and the drain current Id2 (μA) after 10 seconds is measured. 5 The ratio Id2 / Id1 is calculated from the measurement result of the drain current Id2 (μA) after 10 seconds. The larger the ratio Id2 / Id1 is, the less likely the drain current Id is to decrease with the passage of time, and the better the retention characteristics are.

[0187]

Table 2

[0188]

[0189] [Investigation]

[0190] As described below, the performance of the ferroelectric field effect transistor has been confirmed to have the same tendency as the performance of the ferroelectric capacitor described above.

[0191] First, regarding the voltage change characteristics, as shown in Table 2, when the plate-like crystals 1C having an appropriate shape are used (Experimental Examples 2-2 to 2-6, 2-8, and 2-9), almost the same voltage change ΔVt is obtained compared to the case where the spherical crystals 1C are used (Experimental Example 2-1). It should be noted that even when the plate-like crystals 1C are used, when the shape does not meet the appropriate conditions (Experimental Examples 2-7 and 2-10), the voltage change ΔVt is significantly reduced.

[0192] Therefore, when a plate-like crystal 1C having an appropriate shape is used, since the threshold voltage Vt sufficiently changes according to the reversal of the polarization direction of the spontaneous polarization of the gate insulating film 260, it can be considered that the ferroelectric field effect transistor can function as a ferroelectric memory device.

[0193] In addition, regarding the retention characteristics, as shown in Table 2, when plate-like crystals 1C having an appropriate shape are used (Experimental Examples 2-2 to 2-6, 2-8, and 2-9), the ratio Id2 / Id1 increases significantly compared to the case where spherical crystals 1C are used (Experimental Example 2-1). Therefore, the drain current Id is difficult to decrease over time, so the polarization state of the gate insulating film 260 can be stably maintained for a long time. It should be noted that when plate-like crystals 1C that do not have an appropriate shape are used (Experimental Examples 2-7 and 2-10), the ratio Id2 / Id1 decreases significantly, or the ferroelectric field effect transistor does not work at all.

[0194] More specifically, if Fig.13 As shown, when spherical crystals 1C are used (Experimental Example 2-1), the drain current Id decreases sharply with the passage of time. In contrast, when plate-like crystals 1C with an appropriate shape are used (Experimental Example 2-4), the drain current Id hardly decreases with the passage of time.

[0195] In particular, when the plate-like crystals 1C having an appropriate shape were used, when the ratio L / T was 5 or more and 50 or less (Experimental Examples 2-3 to 2-5), the ratio Id2 / Id1 was further increased.

[0196] <3. Ferroelectric Tunnel Junction Memory>

[0197] (Examples 3-1 to 3-10)

[0198] Next, make Fig.10 After the ferroelectric tunnel junction memory is shown, the performance of the ferroelectric tunnel junction memory is evaluated.

[0199] [Ferroelectric Tunnel Junction Memory]

[0200] A ferroelectric tunnel junction memory was manufactured, which has a tunnel insulating film 310 (ferroelectric material = zirconium oxide, thickness = 3nm), a positive electrode 320 (conductive material = titanium nitride, diameter = 100μm) and a negative electrode 330 (conductive material = indium tin oxide, diameter>100μm).

[0201] When the tunnel insulating film 310 is formed, as shown in Table 3, the shape (thickness T (nm), length L (nm) and ratio L / T) of the crystal 1C contained in the tunnel insulating film 310 is changed according to the same steps as when the above-mentioned ferroelectric capacitor (insulating film 110) is formed.

[0202] [Performance evaluation of ferroelectric tunnel junction memory]

[0203] As the performance of ferroelectric tunnel junction memory, the impedance change characteristics and retention characteristics were studied.

[0204] (Impedance change characteristics)

[0205] When studying the impedance change characteristics, first, after polarizing the tunnel insulating film 310 by applying a voltage (=-2.5V) to the ferroelectric tunnel junction memory (application time = 1 msec), the resistance RH of the ferroelectric tunnel junction memory (tunnel insulating film 310) on the high impedance side was measured by applying a voltage (=-0.2V) to the ferroelectric tunnel junction memory (application time = 1 msec). Then, after reversing the polarization direction of the spontaneous polarization of the tunnel insulating film 310 by applying a voltage (=2.5V) to the ferroelectric tunnel junction memory (application time = 1 msec), the resistance RL of the ferroelectric tunnel junction memory (tunnel insulating film 310) on the low impedance side was measured by applying a voltage (=-0.2V) to the ferroelectric tunnel junction memory (application time = 1 msec). Finally, the ratio RH / RL was calculated based on the measurement results of the resistance RH on the high impedance side and the measurement results of the resistance RL on the low impedance side.

[0206] (Maintaining characteristics)

[0207] When studying the retention characteristics, after applying a voltage (=-2.5V) to the ferroelectric tunnel junction memory (positive electrode 320) (application time = 1msec), the resistance R of the ferroelectric tunnel junction memory (tunnel insulating film 310) was measured. In this case, the current when the voltage (=-0.2V) was applied to the positive electrode 320 was measured, and the resistance R based on the current was obtained. Thus, based on the measurement result of the resistance R1 after 10 seconds and the resistance R1 after 10 seconds, the resistance R1 after 10 seconds was obtained. 5 The resistance R2 after 1 second is measured and the ratio R2 / R1 is calculated. The larger the ratio R2 / R1 is, the less likely the resistance R is to decrease with time, and the better the retention characteristics are.

[0208]

Table 3

[0209]

[0210] [Investigation]

[0211] As described below, the performance of the ferroelectric tunnel junction memory has been confirmed to have the same tendency as the performance of the ferroelectric capacitor described above.

[0212] First, regarding the impedance change characteristics, as shown in Table 3, when plate-like crystals 1C with an appropriate shape are used (Experimental Examples 3-2 to 3-6, 3-9, and 3-10), the ratio RH / RL increases significantly compared to the case where spherical crystals 1C are used (Experimental Example 3-1) and the case where plate-like crystals 1C with an inappropriate shape are used (Experimental Examples 3-7 and 3-8).

[0213] Therefore, when the plate-like crystal 1C having an appropriate shape is used, the resistance R changes sufficiently according to the reversal of the polarization direction of the spontaneous polarization of the tunnel insulating film 310, so it can be considered that the ferroelectric tunnel junction memory can function as a ferroelectric memory device. In particular, as described above, the ratio RH / RL becomes large enough, so the ferroelectric tunnel junction memory can be used as a synapse of the neural network.

[0214] In addition, regarding the retention characteristics, as shown in Table 3, when plate-like crystals 1C having an appropriate shape are used (Experimental Examples 3-2 to 3-6, 3-9, and 3-10), the ratio R2 / R1 increases significantly compared to the case where spherical crystals 1C are used (Experiment 3-1) and the case where plate-like crystals 1C having an inappropriate shape are used (Experimental Example 3-7). Therefore, the resistance R is difficult to decrease over time, so the polarization state of the tunnel insulating film 310 can be stably maintained for a long time. It should be noted that when plate-like crystals 1C having an inappropriate shape are used (Experimental Example 3-8), the ferroelectric field effect transistor does not work at all.

[0215] In particular, when the plate-like crystals 1C having an appropriate shape were used, if the ratio L / T was 5 or more and 50 or less (Experimental Examples 3-3 to 3-5), the ratio R2 / R1 was further increased.

[0216] <4. Conclusion>

[0217] From the results shown in Tables 1 to 3, it can be seen that in a ferroelectric memory device having a ferroelectric film having a fluorite-type crystal structure, when the ferroelectric film includes plate-like crystals and the shape of the plate-like crystals (thickness T and ratio L / T) satisfies appropriate conditions, the retention characteristics are improved. Therefore, excellent electrical characteristics are obtained in the ferroelectric memory device.

[0218] The present technology has been described above with reference to one embodiment and an example, but the present technology is not limited to the methods described in the embodiment and the example, and various modifications can be made. In addition, the effects described in this specification are only examples and are not limited thereto, so other effects can be obtained.

[0219] It should be noted that the present technology can also be configured as follows.

[0220] (1) A ferroelectric memory device comprising a ferroelectric film and a pair of electrodes.

[0221] The ferroelectric film: (A) has a fluorite crystal structure, (B) includes plate-like crystallites whose length (nm) is greater than the thickness (nm), (C) the thickness is greater than 1 nm and less than 30 nm, and (D) the ratio of the length to the thickness is greater than 2 and less than 100; and

[0222] The pair of electrodes is connected to the ferroelectric film.

[0223] (2) A ferroelectric memory device according to (1) above, wherein:

[0224] A ratio of the length to the thickness is 5 or more and 50 or less.

[0225] (3) The ferroelectric memory device according to (1) or (2) above, wherein:

[0226] The ferroelectric film includes at least one of zirconium oxide, hafnium oxide, cerium oxide, and solid solutions of two or more thereof.

[0227] The solid solution contains a zirconium-hafnium compound represented by the following formula (1),

[0228] Hf x Zr 1-x O2……(1)

[0229] Among them, x satisfies 0 <x<1。

[0230] (4) The ferroelectric memory device according to any one of (1) to (3) above, wherein:

[0231] The crystal phase of the ferroelectric film includes an orthorhombic phase.

[0232] (5) The ferroelectric memory device according to any one of (1) to (4) above, wherein:

[0233] Each of the pair of electrodes comprises at least one of silicon, platinum, ruthenium, metal oxides and metal nitrides,

[0234] The metal oxide comprises at least one of indium oxide, gallium oxide, zinc oxide, tin oxide, indium tin oxide, indium zinc oxide and solid solutions of two or more thereof,

[0235] The metal nitride includes at least one of titanium nitride and tantalum nitride.

[0236] (6) The ferroelectric memory device according to any one of (1) to (5) above, wherein:

[0237] The ferroelectric memory device is any one of a ferroelectric capacitor, a ferroelectric field effect transistor and a ferroelectric tunnel junction memory.

[0238] This application is based upon and claims the benefit of priority from Japanese Patent Application No. 2018-108634, filed with the Japan Patent Office on June 6, 2018, the entire contents of which are incorporated herein by reference.

[0239] Those skilled in the art may conceive of various modifications, combinations, sub-combinations and changes depending on design requirements and other factors, but it should be understood that these modifications, combinations, sub-combinations and changes are included in the spirit and scope of the appended claims and their equivalents.

Claims

1. A ferroelectric memory device comprising a ferroelectric film and a pair of electrodes, The ferroelectric film: (A) has a fluorite crystal structure, (B) includes plate-like crystallites whose length is greater than their thickness, (C) the thickness is greater than or equal to 1 nm and less than or equal to 30 nm, and (D) the ratio of the length to the thickness is greater than or equal to 2 and less than 100, The pair of electrodes is connected to the ferroelectric film, The thickness is a dimension in a direction in which a voltage is applied to the ferroelectric memory device, and the length is a dimension in a direction intersecting with the voltage application direction. The ferroelectric film includes at least one of zirconium oxide, hafnium oxide, cerium oxide, and solid solutions of two or more thereof. The solid solution contains a zirconium-hafnium compound represented by the following formula (1): Hf x Zr 1-x O2……(1), x satisfies 0<x<1.

2. The ferroelectric memory device according to claim 1, wherein: A ratio of the length to the thickness is 5 or more and 50 or less.

3. The ferroelectric memory device according to claim 1, wherein: The crystal phase of the ferroelectric film includes an orthorhombic phase.

4. The ferroelectric memory device according to claim 1, wherein: Each of the pair of electrodes comprises at least one of silicon, platinum, ruthenium, metal oxides and metal nitrides, The metal oxide comprises at least one of indium oxide, gallium oxide, zinc oxide, tin oxide, indium tin oxide, indium zinc oxide and solid solutions of two or more thereof, The metal nitride includes at least one of titanium nitride and tantalum nitride.

5. The ferroelectric memory device according to claim 1, wherein: The ferroelectric memory device is any one of a ferroelectric capacitor, a ferroelectric field effect transistor and a ferroelectric tunnel junction memory.

Citation Information

Patent Citations

  • Aerosol method for producing chemical mechanical planarization (CMP) polishing pad

    JP2018108634A

  • Ferroelectric memory

    JP2000022091A

  • Metal oxide structure having network structure

    JP2000096236A