Welding process of IGBT power module terminals and bare copper substrate

By designing IGBT power module terminals with a specific structure, using arc-shaped welding parts and diamond-shaped groove structures, combined with ultrasonic welding technology, the problem of insufficient bonding strength between the IGBT power module terminals and the bare copper substrate welding surface is solved, and the welding quality and stability.

CN112271142BActive Publication Date: 2024-10-01ANHUI REDPOWER MICROELECTRONICS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011174712.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-10-28
Publication Date
2024-10-01
Estimated Expiration
2040-10-28

AI Technical Summary

Technical Problem

During the ultrasonic welding process of IGBT power module terminals and bare copper substrates, there are problems such as insufficient welding surface roughness, insufficient welding bonding strength, and the risk of solder joints falling off.

Method used

The IGBT power module terminal adopts a specific structure, including the first and second connecting parts and the welding part. The welding part is arc-shaped, the terminal front and the welding surface are arc surfaces, multiple diamond-shaped grooves are provided, and the welding surface and bare copper When welding the substrate, the bonding head applies ultrasonic energy and downward pressure, and the welding part is bent inward by 80-90° to reduce the pulling force and increase the contact area.

Benefits of technology

During the ultrasonic welding process, the pulling force on the welding surface is reduced, the welding bonding strength is enhanced, the welding quality is improved, and the risk of solder joints falling off is reduced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112271142B_ABST
    Figure CN112271142B_ABST
Patent Text Reader

Abstract

The present invention discloses a welding process for an IGBT power module terminal and a bare copper substrate, comprising the steps of: S1, placing the terminal above the bare copper substrate, and contacting the terminal welding surface with the bare copper substrate welding surface; S2, a bonding welding head applies ultrasonic energy to the terminal and the bare copper substrate to weld the terminal to the bare copper substrate. The terminal comprises a first connecting portion, a second connecting portion and a welding portion, the first connecting portion has a first back side, the second connecting portion has a second back side, the first back side is connected to the second back side, and the angle between the first back side and the second back side is 80-90°, the width of the welding portion is 1.5-2 times the width of the second connecting portion, and the welding portion is welded to the bare copper substrate. The welding process for the GBT power module terminal and the bare copper substrate of the present invention makes the welding stress point of the terminal bend inward by 80-90°, which can reduce the pulling force on the welding surface during ultrasonic welding.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of semiconductor products, and in particular, relates to a welding process for an IGBT power module terminal and a bare copper substrate. Background Art

[0002] During the manufacturing process of IGBT power modules, in traditional ultrasonic terminal bonding, the bonding welder uses ultrasonic cold pressure welding to press the copper terminals onto the bare copper surface of the DBC substrate. The roughness of the terminal welding surface is increased during ultrasonic vibration to complete the welding of the welding surface and the bare copper substrate.

[0003] The prior art has the following disadvantages:

[0004] 1. The terminal is a stamped part. In view of the processing technology characteristics of stamped parts, the welding stress points on the terminal will generate pulling force on the welding surface during ultrasonic welding, which is not conducive to the combination of the welding surface and the bare copper substrate, and there is a risk of the solder joint falling off during long-term use;

[0005] 2. During ultrasonic welding, the roughness of the front surface of the terminal and the welding surface is insufficient, and longer vibration friction is required to enhance the bonding between the welding surfaces;

[0006] 3. The front of the terminal and the welding surface are relatively flat, and the welding bonding time of the welding surface is long; and if the welding surface is warped, the bonding strength between the surfaces will be insufficient. Summary of the invention

[0007] The present invention aims to solve at least one of the technical problems existing in the prior art. To this end, the present invention provides a welding process for an IGBT power module terminal and a bare copper substrate, the purpose of which is to reduce the pulling force on the welding surface during ultrasonic welding.

[0008] In order to achieve the above object, the technical solution adopted by the present invention is: a welding process of a GBT power module terminal and a bare copper substrate, comprising the steps of:

[0009] S1. Place the terminal on top of the bare copper substrate, and make the terminal welding surface contact with the welding surface of the bare copper substrate;

[0010] S2, the bonding welding head applies ultrasonic energy to the terminal and the bare copper substrate to weld the terminal to the bare copper substrate;

[0011] In which, in step S1, the terminal includes a first connecting part, a second connecting part connected to the first connecting part, and a welding part connected to the second connecting part, the first connecting part has a first back side, the second connecting part has a second back side, the first back side is connected to the second back side, and the angle between the first back side and the second back side is 80-90°, the width of the welding part is 1.5-2 times the width of the second connecting part, and the welding part is welded to the bare copper substrate.

[0012] The second connection portion is fixedly connected to the welding portion at a middle portion in a width direction of the welding portion, and the first connection portion and the second connection portion have the same width.

[0013] The welding portion is an arc-shaped structure, and the welding portion has a terminal front face for contacting the bonding welding head and a terminal welding surface for contacting the welding surface of the bare copper substrate. The terminal front face and the terminal welding surface are both arc surfaces, and the axes of the terminal front face and the terminal welding surface are parallel to the welding surface of the bare copper substrate.

[0014] In the step S2, the bonding head applies downward pressure to the welding portion of the terminal to flatten the welding portion.

[0015] A plurality of first grooves are arranged on the front surface of the terminal.

[0016] All the first grooves on the front side of the terminal are distributed in an n*m matrix.

[0017] The first groove is a diamond-shaped groove.

[0018] A plurality of second grooves are arranged on the terminal welding surface.

[0019] All the second grooves on the terminal welding surface are distributed in an n*m matrix.

[0020] The second groove is a diamond-shaped groove.

[0021] The welding process of the GBT power module terminal and the bare copper substrate of the present invention makes the welding stress point of the terminal bend inward by 80-90 degrees, which can reduce the pulling force on the welding surface during ultrasonic welding; at the same time, the welding contact area is increased, the bonding strength of the welding surface is enhanced, and the product quality is improved. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] This specification includes the following drawings, which show the following contents:

[0023] Figure 1 It is a schematic diagram of the welding status of the IGBT power module terminal and the bare copper substrate;

[0024] Figure 2 It is a top view of the IGBT power module terminals;

[0025] The markings in the figure are: 1. Welding force point; 2. Bonding weld head; 3. Terminal front side; 4. Terminal welding side; 5. Bare copper substrate back side; 6. Welding side of bare copper substrate; 7. Ceramic substrate; 8. First connection part; 9. Second connection part; 10. Welding part; 11. First front side; 12. First back side; 13. Second front side; 14. Second back side. DETAILED DESCRIPTION

[0026] The specific implementation methods of the present invention are further explained in detail below by describing the embodiments with reference to the accompanying drawings, with the aim of helping those skilled in the art to have a more complete, accurate and in-depth understanding of the concept and technical solution of the present invention and facilitating its implementation.

[0027] It should be noted that, in the following embodiments, the “first” and “second” mentioned do not represent an absolute distinction in structure and / or function, nor do they represent a sequential order of execution, but are merely for the convenience of description.

[0028] like Figure 1 and Figure 2 As shown, the present invention provides a welding process for a GBT power module terminal and a bare copper substrate, comprising the following steps:

[0029] S1, placing the terminal on top of the bare copper substrate, and bringing the terminal welding surface 4 into contact with the welding surface 6 of the bare copper substrate;

[0030] S2. The bonding welding head 2 applies ultrasonic energy to the terminal and the bare copper substrate to weld the terminal to the bare copper substrate.

[0031] Specifically, if Figure 1 and Figure 2 As shown, in the above step S1, the terminal used includes a first connecting part 8, a second connecting part 9 connected to the first connecting part 8, and a welding part 10 connected to the second connecting part 9 and welded to the bare copper substrate, the first connecting part 8 has a first front side 11 and a first back side 12, the second connecting part 9 has a second front side 13 and a second back side 14, the first back side 12 is connected to the second back side 14 and the angle between the first back side 12 and the second back side 14 is 80-90°, the width of the welding part 10 is 1.5-2 times the width of the second connecting part 9, and the bare copper substrate is a DBC substrate.

[0032] like Figure 1 and Figure 2As shown, the first connection part 8 has a certain length, width and thickness, and the length direction, width direction and thickness direction of the first connection part 8 are mutually perpendicular, and the first front face 11 and the first back face 12 of the first connection part 8 are planes perpendicular to the thickness direction of the first connection part 8 and parallel to the length direction and width direction of the first connection part 8. The second connection part 9 has a certain length, width and thickness, and the length direction, width direction and thickness direction of the second connection part 9 are mutually perpendicular, and the second front face 13 and the second back face 14 of the second connection part 9 are planes perpendicular to the thickness direction of the second connection part 9 and parallel to the length direction and width direction of the second connection part 9. The width direction of the first connection part 8 is parallel to the width direction of the second connection part 9, one end of the first connection part 8 in the length direction is fixedly connected to one end of the second connection part 9 in the length direction, and the other end of the second connection part 9 in the length direction is fixedly connected to the welding part 10. The first front face 11 and the first back face 12 are two opposite surfaces of the first connection part 8, and the distance between the first front face 11 and the bare copper substrate is greater than the distance between the first back face 12 and the bare copper substrate. The second front side 13 and the second back side 14 are two opposite surfaces of the second connecting portion 9 . During ultrasonic welding, the distance between the second front side 13 and the bonding horn 2 is smaller than the distance between the second back side 14 and the bonding horn 2 .

[0033] like Figure 1 and Figure 2 As shown, the second connection part 9 is fixedly connected to the welding part 10 at the middle part in the width direction of the welding part 10, the width of the welding part 10 is greater than the width of the first connection part 8 and the second connection part 9, the widths of the first connection part 8 and the second connection part 9 are the same, and the two ends of the first connection part 8 and the second connection part 9 in the width direction are aligned respectively.

[0034] As a preferred example, Figure 1 and Figure 2 As shown, the welding portion 10 is an arc-shaped structure, and the welding portion 10 has a terminal front face 3 for contacting the bonding welding head 2 and a terminal welding surface 4 for contacting the welding surface 6 of the bare copper substrate. The terminal front face 3 and the terminal welding surface 4 are both arc surfaces, and the axes of the terminal front face 3 and the terminal welding surface 4 are parallel to the welding surface 6 of the bare copper substrate. The distance between the terminal front face 3 and the bare copper substrate is greater than the distance between the terminal welding surface 4 and the bare copper substrate, and the axis of the terminal front face 3 is located above the terminal front face 3, and the axis of the terminal welding surface 4 is also located above the terminal front face 3.

[0035] like Figure 1 and Figure 2As shown, the terminal front face 3 and the terminal welding surface 4 are two opposite surfaces of the welding portion 10, and the curvature of the terminal front face 3 and the terminal welding surface 4 is less than 180 degrees. One end of the first back face 12 is directly connected to one end of the second back face 14, and the other end of the second back face 14 is connected to one end of the terminal welding surface 4. The angle between the length direction of the first back face 12 (that is, the length direction of the first connecting portion 8) and the second back face 14 (that is, the length direction of the second connecting portion 9) is 80-90°. The connection between the first back face 12 and the second back face 14 forms a welding stress point, and the welding stress point is bent inward by 80-90°, which can reduce the pulling force on the welding surface during ultrasonic welding. One end of the first front face 11 is connected to one end of the second front face 13, and the two are connected by a circular arc transition, and the other end of the second front face 13 is connected to one end of the terminal front face 3.

[0036] As a preferred example, Figure 1 and Figure 2 As shown, a plurality of first grooves are arranged on the front face 3 of the terminal, and all the first grooves on the front face 3 of the terminal are distributed in an n*m matrix. A plurality of second grooves are arranged on the terminal welding surface 4, and all the second grooves on the terminal welding surface 4 are distributed in an n*m matrix. Therefore, the front face 3 of the terminal and the terminal welding surface 4 adopt a concave structure design, and by setting the first groove and the second groove, in the above step S2, during ultrasonic welding, the terminal welding surface 4 and the bare copper substrate can be combined more quickly, and the two welding surfaces can be gradually completely welded.

[0037] As a preferred example, Figure 1 and Figure 2 As shown, the first groove and the second groove are both diamond-shaped grooves.

[0038] Preferably, the terminal front surface 3 and the terminal welding surface 4 need to be roughened. In the above step S2, the roughness of the terminal welding surface 4 is increased, thereby enhancing the friction between the ultrasonic vibration surfaces and shortening the ultrasonic welding time.

[0039] In the above step S2, the bonding head 2 applies downward pressure to the welding portion 10 of the terminal to flatten the welding portion 10, and finally makes the terminal front surface 3 and the terminal welding surface 4 become a plane parallel to the welding surface 6 of the bare copper substrate.

[0040] The present invention is described above by way of example in conjunction with the accompanying drawings. Obviously, the specific implementation of the present invention is not limited to the above-mentioned methods. As long as various non-substantial improvements are made using the method concept and technical solution of the present invention; or the above concept and technical solution of the present invention are directly applied to other occasions without improvement, they are all within the protection scope of the present invention.

Claims

1. The welding process of IGBT power module terminal and bare copper substrate is characterized in that: Includes steps: S1. Place the terminal on top of the bare copper substrate, and make the terminal welding surface contact with the welding surface of the bare copper substrate; S2, the bonding welding head applies ultrasonic energy to the terminal and the bare copper substrate to weld the terminal to the bare copper substrate; Wherein, in the step S1, the terminal includes a first connecting portion, a second connecting portion connected to the first connecting portion, and a welding portion connected to the second connecting portion, the first connecting portion has a first back side, the second connecting portion has a second back side, the first back side is connected to the second back side, and the angle between the first back side and the second back side is 80-90°, the width of the welding portion is 1.5-2 times the width of the second connecting portion, and the welding portion is welded to the bare copper substrate; The welding portion is an arc-shaped structure, and the welding portion has a terminal front face for contacting with the bonding welding head and a terminal welding surface for contacting with the welding surface of the bare copper substrate, the terminal front face and the terminal welding surface are both arc surfaces, and the axes of the terminal front face and the terminal welding surface are parallel to the welding surface of the bare copper substrate; The distance between the front face of the terminal and the bare copper substrate is greater than the distance between the welding surface of the terminal and the bare copper substrate, the axis of the front face of the terminal is located above the front face of the terminal, and the axis of the welding surface of the terminal is also located above the front face of the terminal; A plurality of first grooves are arranged on the front surface of the terminal, and a plurality of second grooves are arranged on the welding surface of the terminal, all the first grooves on the front surface of the terminal are distributed in an n*m matrix, and all the second grooves on the welding surface of the terminal are distributed in an n*m matrix; In the step S2, the bonding head applies downward pressure to the welding portion of the terminal to flatten the welding portion, and finally makes the front surface of the terminal and the welding surface of the terminal become a plane parallel to the welding surface of the bare copper substrate.

2. The welding process of the IGBT power module terminal and the bare copper substrate according to claim 1, characterized in that: The second connection portion is fixedly connected to the welding portion at a middle portion in a width direction of the welding portion, and the first connection portion and the second connection portion have the same width.

3. The welding process of the IGBT power module terminal and the bare copper substrate according to claim 1, characterized in that: The arc of the terminal front surface and the terminal welding surface is less than 180 degrees.

4. The welding process of the IGBT power module terminal and the bare copper substrate according to claim 1, characterized in that: The front surface of the terminal and the welding surface of the terminal need to be subjected to surface roughening treatment. In the step S2, the roughness of the welding surface of the terminal is increased.

5. The welding process of the IGBT power module terminal and the bare copper substrate according to claim 1, characterized in that: The first groove is a diamond-shaped groove.

6. The welding process of the IGBT power module terminal and the bare copper substrate according to claim 1, characterized in that: The second groove is a diamond-shaped groove.