Semiconductor packaging and its manufacturing process
By arranging the die on the semiconductor interposer layer so that the gap extension direction is not parallel to the crystallization orientation, and stress transmission is reduced, the problem of warping and cracking of the packaging structure in the heating process is solved, and the reliability and yield of the packaging are improved.
Patent Information
- Application Number
- CN202010142769.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-10-17
- Filing Date
- 2020-03-04
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2040-09-15
AI Technical Summary
In advanced packaging processes, semiconductor packaging structures are prone to warping due to mismatch in the thermal expansion coefficient during the heating process, resulting in cracking of the interposer layer, affecting the reliability and yield of the packaging.
By arranging the first die and the second die on the semiconductor interposer layer, the gap extension direction is not parallel to the crystalline orientation of the interposer layer, stress transmission is reduced, warping and cracking risks are reduced, and covering tubes are formed on the interposer layer The molded compound of the core is used to enhance structural strength.
It effectively improves the strength of the packaging structure, reduces the possibility of interposer cracking, and enhances the reliability and productivity of the packaging.
Smart Images

Figure CN112687552B_ABST
Abstract
Description
Technical Field
[0001] Embodiments of the present invention relate to semiconductor packaging and manufacturing processes thereof. Background Art
[0002] In advanced packaging processes, semiconductor packaging can integrate multiple chips onto an interposer with perforations through a chip-to-wafer bonding process, and the assemblies can be mounted onto a substrate. The improvement in the structural strength and integrity of the package enables better reliability and high yield. Summary of the invention
[0003] According to some embodiments of the present disclosure, a manufacturing process is provided. An interposer having a crystal structure is provided. After a first die is disposed on the interposer, a second die is disposed on the interposer. The second die is positioned to be spaced apart from the first die by a gap and to define a gap extension direction of the gap. The gap extension direction is not parallel to a crystallographic orientation of the crystal structure of the interposer. The first die and the second die are bonded to the interposer. A molding compound covering the first die and the second die is formed on the interposer. The molding compound and the interposer are cut into packages.
[0004] According to some alternative embodiments of the present disclosure, a packaging process includes the following steps. A wafer interposer having a crystal structure is provided and a crystal orientation of the crystal structure is determined. A first die is disposed on the wafer interposer and one side of each first die is oriented to be parallel to a first direction. The first direction is oriented to have an angle θ between the crystal orientation and the first direction, and the angle θ is greater than zero and less than 90 degrees. A second die is disposed on the wafer interposer and one side of each second die is oriented to be parallel to the first direction. The second die is disposed next to the first die and is spaced apart from the first die by a gap, and the gap extends in the first direction. The first die and the second die are bonded to the wafer interposer. A molding compound covering the first die and the second die is formed on the wafer interposer. The molding compound and the wafer interposer are cut into packages.
[0005] According to some embodiments of the present disclosure, a packaging structure is described. The packaging structure includes a semiconductor interposer, a first die and a second die, and a conductive connector. The semiconductor interposer has a crystal structure and has a first surface and a second surface opposite to the first surface. The semiconductor interposer includes a through hole (204) extending from the first surface to the second surface. The first die is disposed on the first surface of the semiconductor interposer and is electrically connected to the through hole. The second die is disposed on the first surface of the semiconductor interposer, disposed beside the first die, and is electrically connected to the through hole. The first die and the second die are separated by a gap between the first die and the second die, and the mutually facing sides of the first die and the second die define a gap extension direction of the gap. The gap extension direction is not parallel to the crystallographic orientation of the crystal structure of the semiconductor interposer. The conductive connector is disposed on the second surface of the semiconductor interposer and is electrically connected to the through hole. BRIEF DESCRIPTION OF THE DRAWINGS
[0006] The various aspects of the present disclosure will be best understood by reading the following detailed description in conjunction with the accompanying drawings. It should be noted that, in accordance with standard practice in the industry, the various features are not drawn to scale. In fact, the size of the various features may be arbitrarily increased or reduced for clarity of discussion.
[0007] Figure 1 , Figure 2A and Figures 3 to 6 are schematic cross-sectional views of various stages in a method for manufacturing a package structure according to some exemplary embodiments of the present disclosure.
[0008] Figure 2B is a schematic diagram showing the location of dies on an interposer according to some embodiments of the present disclosure.
[0009] Fig. 7A and Figure 7B The crystallographic orientation of the (100) wafer is shown.
[0010] Fig. 8A is a schematic cross-sectional view showing a package and a circuit substrate according to an embodiment of the present disclosure.
[0011] Figure 8B is a schematic diagram showing the location of a die on an interposer according to an embodiment of the present disclosure. DETAILED DESCRIPTION
[0012] The following disclosure provides many different embodiments or examples for implementing the different features of the provided subject matter. Specific examples of components and arrangements are set forth below to simplify the present disclosure. Of course, these are merely examples and are not intended to be limiting. For example, in the following description, forming a first feature on or on a second feature may include an embodiment in which the first feature and the second feature are formed to be in direct contact, and may also include an embodiment in which an additional feature may be formed between the first feature and the second feature so that the first feature and the second feature may not be in direct contact. In addition, the present disclosure may reuse reference numbers and / or letters in various examples. This repetition is for the purpose of simplicity and clarity, rather than indicating the relationship between the various embodiments and / or configurations discussed by itself.
[0013] Additionally, for ease of description, spatially relative terms such as "below," "beneath," "lower," "above," "upper," etc. may be used herein to describe the relationship of one element or feature to another (other) element or feature as illustrated in the figures. The spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations), and the spatially relative descriptors used herein should be interpreted accordingly.
[0014] Other features and processes may also be included. For example, a test structure may be included to help perform verification testing on a three-dimensional (3D) package or a three-dimensional integrated circuit (3DIC) device. The test structure may include, for example, a test pad formed in a redistribution layer or on a substrate so that the 3D package or 3DIC can be tested, probes and / or probe cards can be used, etc. Verification testing can be performed on intermediate structures as well as final structures. In addition, the structures and methods disclosed herein can be used in conjunction with a test method that includes intermediate verification of a known good die to improve yield and reduce costs.
[0015] For the embodiments provided herein, the techniques may be discussed in a specific context, i.e., arranging the die or chip in a specific orientation relative to the crystallographic orientation of the underlying crystalline semiconductor wafer interposer. By arranging and designing the layout of the die so that the stress location is not parallel to the crystallographic orientation of the underlying interposer and the smaller or minimal stress is transmitted along the crystallographic orientation, the possible cracking of the underlying crystalline semiconductor wafer interposer due to the warping of the package structure during the heating process may be avoided or reduced. This enables a more reliable package structure by reducing the possibility of cracking of the interposer. The relative orientation of the die to the underlying crystalline semiconductor wafer interposer may mitigate or alleviate the effects of warping caused by a mismatch in the coefficient of thermal expansion (CTE).
[0016] The packaging process may include forming a multi-chip package structure using a Chip-on-Wafer-on-Substrate (CoWoS) packaging process. Other embodiments may also include other processes (including wafer-level packaging processes or package-on-package assembly processes). The embodiments discussed herein are intended to provide examples of how the disclosed subject matter can be made or used, and a person of ordinary skill in the art will readily understand that modifications may be made while remaining within the intended scope of the different embodiments. The same reference numbers and characters in the following figures refer to the same components. Although method embodiments may be discussed as being performed in a particular order, other method embodiments may be performed in any logical order.
[0017] Figures 1 to 6 Schematic diagrams of various stages in a method for manufacturing a package structure according to some exemplary embodiments of the present disclosure.
[0018] exist Figure 1 In the embodiment, an interposer 200 is provided. In some embodiments, the interposer 200 includes a semiconductor substrate 202 and a through hole 204. Figure 1In the figure, the entire interposer 200 is not shown, but only a portion of the interposer 200 including one or more package units PKU is shown, and the number of perforations in the interposer is not limited to the exemplary examples shown in the figure. In some embodiments, a rewiring structure 210 is formed on the substrate 202 and above the perforations 204. In some embodiments, the substrate 202 may include a bulk semiconductor material substrate, a silicon on insulator (SOI) substrate, or a multilayer semiconductor material substrate. The semiconductor material of the semiconductor substrate 202 may be silicon, germanium, silicon germanium, silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, indium antimonide, GaAsP, AlInAs, AlGaAs, GaInAs, GaInP, GaInAsP, or a combination thereof. In some embodiments, the substrate 202 may be doped or undoped. In some embodiments, the substrate 202 may be doped with a P-type dopant (e.g., boron (B), aluminum (Al), or gallium (Ga)) or doped with an N-type dopant (e.g., phosphorus (P), arsenic (As), or antimony (Sb)). In some embodiments, interposer 200 includes a bulk semiconductor wafer having a crystal structure. In one embodiment, interposer 200 may be a bulk silicon wafer having a crystal structure (eg, a cubic crystal structure).
[0019] In some embodiments, a through hole 204 is formed in the substrate 202 to penetrate through the substrate 202. In some embodiments, as Figure 1 As shown in , the through-hole 204 is a substrate through-hole. In some embodiments, when the substrate 202 includes a silicon substrate, the through-hole 204 is a silicon through-hole. In some other embodiments, the through-hole 204 may extend into the substrate 202 without penetrating through the substrate 202, and at a later stage, the substrate 202 may be thinned from the back side to expose the end of the through-hole 204. Figure 1In this stage, the interposer 200 has been thinned and the ends of the through-holes 204 are exposed. Although not shown in the figure, it should be understood that a carrier or glass carrier may be provided under the interposer 200 for support purposes. In some embodiments, the through-holes 204 may be formed by forming a hole or recess in the substrate 202 and then filling the recess with a conductive material. In some embodiments, the recess may be formed by, for example, etching, milling, laser drilling, etc. In some embodiments, the conductive material may be formed by an electro-chemical plating process, chemical vapor deposition (CVD), atomic layer deposition (ALD), or physical vapor deposition (PVD), and the conductive material may include copper, tungsten, aluminum, silver, gold, or a combination thereof.
[0020] Wafers are grown from crystals with a regular crystal structure. Crystal planes and directions are described by Miller Indices (e.g., (100), (111), (110), etc.). In a symmetrical crystal lattice, certain directions are equivalent to each other, and groups of equivalent directions or planes are called families. For example, in a cubic crystal system, directions
[100] ,
[010] , and
[001] belong to a family. <100> The crystal orientation of a wafer is specified in two ways: the orientation of the plane of the wafer surface and the location of the wafer primary flat (the longest straight side of the wafer's circumference). For commonly used wafers (p-type and n-type (100) and (111) wafers), the primary flat is aligned with the
[110] direction. Alternatively, for larger wafer sizes, notches are used during fabrication to mark the orientation of the wafer instead of the primary flat. For example, a (100) silicon wafer can be oriented by cutting along the {100} plane using a notch pointing in the
[011] direction.
[0021] In some embodiments, the bulk silicon wafer is a silicon wafer having a crystal structure, and the crystal orientation of the surface of the crystalline silicon wafer may be (100) or (111). In one embodiment, the bulk silicon wafer is a (100) wafer having the top surface of the wafer oriented on the (100) crystal plane and having a major plane aligned with the
[110] direction. Fig. 7A The crystal orientation of (100) silicon wafer is described in Figure 7BThe chip is shown in <110> The directions in the direction and the natural X-axis and Y-axis. For a (100) silicon wafer, the direction of the X-axis is the
[110] direction, the direction of the Y-axis is the [-110] direction, and the direction orthogonal to the top surface of (100) is the
[100] direction, which can be regarded as the natural Z-axis of the XYZ coordinate system.
[0022] In some embodiments, an interposer 200 having a crystal structure is provided, and then a crystal orientation of the crystal structure of the interposer 200 is determined. In one embodiment, the interposer 200 may be oriented based on a main plane of a wafer, and a crystal orientation (e.g., an X-axis and a Y-axis) of the crystal structure of the interposer 200 is determined.
[0023] In some embodiments, the redistribution structure 210 formed on the substrate 202 includes metal patterns 206a, 206b, 206c and dielectric layers 208a, 208b, 208c that are alternately stacked. In some embodiments, the metal pattern 206a may include a conductive portion connected to the through-hole 204, and the metal pattern 206c may include a conductive portion used as a bump pad and / or under bump metallurgy (UBM). In some embodiments, the material of the dielectric layers 208a, 208b, 208c may include a polymer material (including polyimide (PI), polybenzoxazole (PBO), benzocyclobutene (BCB) or any other suitable polymer-based dielectric material. In some embodiments, the dielectric layers 208a, 208b, 208c may be formed by lamination, coating, chemical vapor deposition (CVD), etc. In some embodiments, the formation of the metallization patterns 206a, 206b, 206c may include patterning the dielectric layer using photolithography and one or more etching processes and filling the metal material into the openings of the patterned dielectric layer. Any excess conductive material on the dielectric layer may be removed, for example, using a chemical mechanical polishing process. In some embodiments, the material of the metallization patterns 206a, 206b, 206c includes copper, aluminum, tungsten, silver, titanium, and combinations thereof.
[0024] In certain embodiments, the interposer 200 may also include active or passive components, such as transistor, capacitor, resistor, or diode passive components formed in the substrate 202 .
[0025] Reference Figure 2A and Figure 2B, a first die 12 and a second die 14 are provided and mounted on the interposer 200. Only one first die and one second die are shown in the figure as illustrative examples, but the number of first dies and second dies is not limited to the examples shown in this article. In some embodiments, the first die 12 and the second die 14 are individual semiconductor dies singulated from a wafer. In some embodiments, each first die 12 contains the same circuit (e.g., device and metallization pattern), or each first die 12 is the same type of die. In some embodiments, each second die 14 contains the same circuit, or each second die 14 is the same type of die. In some embodiments, the first die 12 and the second die 14 have different circuits or are different types of dies. In alternative embodiments, the first die 12 and the second die 14 may have the same circuit.
[0026] From the perspective of the package unit PKU defined between scribe lanes (SL), the first die 12 and the second die 14 are arranged on the top surface 200a of the interposer 200 within the span of the package unit PKU, and the first die 12 and the second die 14 are arranged side by side and spaced apart from each other. The layout design of the die or the position design of the die arrangement is intended to orient the die in a specific manner relative to the crystallographic orientation of the underlying interposer.
[0027] In some embodiments, Figure 2B As shown in , the first die 12 is a rectangular die having two opposite sides 12X and two other opposite sides connecting the two opposite sides 12X. In addition, the second die 14 may be a rectangular die. In one embodiment, two second dies 14 are arranged next to one first die 12 in each package unit PKU. In one embodiment, each second die 14 is spaced apart from the first die 12 by a gap of a pitch SP. In one embodiment, the pitch SP may be in a range of 40 microns to 100 microns. Referring to Figure 2B , when the first die 12 is placed on the interposer 200, the position of the first die 12 is appropriately selected so that one side 12X of the first die 12 is aligned with the direction X1 (substantially parallel to (within manufacturing tolerances) the direction X1), and then the second die 14 is oriented so that the side of the second die 14 is aligned substantially parallel to (within manufacturing tolerances) the side 12X of the first die 12 and substantially parallel to (within manufacturing tolerances) the direction X1. Figure 2BFrom the perspective of the embodiment of the present invention, each second die 14 is arranged to be substantially parallel (within manufacturing deviations) and beside the side 12X of the first die 12. Since the two second dies 14 are arranged to be spaced apart from the first die 12 by a gap (e.g., having the same pitch SP) and the two second dies 14 are arranged along the direction X1, the direction X1 is also the gap extension direction. That is, the second dies 14 are positioned so that the sides of the second dies 14 are aligned to be substantially parallel to the side 12X of the first die 12 (within manufacturing deviations), and by the arrangement of the mutually facing sides of the first die 12 and the second die 14, the gap extension direction X1 (gap extension direction X1) is defined as a direction parallel to the mutually facing sides of the first die 12 and the second die 14. In some embodiments, the gap or pitch SP between the first die 12 and the second die 14 is the shortest distance between the two mutually facing sides of the first die 12 and the second die 14, and the gap extension direction X1 is substantially perpendicular to the direction of the pitch SP. When warping occurs in the package structure, the gap between the dies is the location of maximum stress, and the stress can be transmitted along the longitudinal extension direction of the gap. FIG. 7A to FIG. 7B A silicon (100) wafer having a crystal orientation (e.g., X, Y, Z axis) as shown in FIG. , and the first die 12 and the second die 14 are arranged in a manner that the extension direction X1 of the gap is not parallel to the natural axis X of the interposer 200. By mismatching the stress position with the lattice orientation of the underlying wafer interposer, the stress transfer direction is not parallel to the lattice orientation, thereby avoiding stress transfer to the interposer and causing cracking. That is, there is an angle θ between the gap extension direction X1 (defined by the mutually facing sides of the first die and the second die) and the crystal orientation X of the interposer 200 (i.e., the natural axis X of the wafer of the interposer 200), and the angle θ is greater than zero and less than 180 degrees. In some embodiments, the angle θ is in the range of about 60 degrees to about 120 degrees. In some embodiments, the angle θ is in the range of 75 degrees to about 105 degrees. In some embodiments, the angle θ is in the range of 85 degrees to about 95 degrees. In one embodiment, the angle θ is about 90 degrees, and the direction X1 is in the [-1-10] direction. When the angle θ is about 90 degrees, the transmitted stress is minimized and a better anti-stress effect is achieved.
[0028] In some embodiments, the first die 12 has a surface area greater than the surface area of the second die 14. In addition, in some embodiments, the first die 12 and the second die 14 may have different sizes, thereby including different surface areas and / or different thicknesses. In some embodiments, the first die 12 may be a logic die, including a central processing unit (CPU) die, a graphics processing unit (GPU) die, a system-on-a-chip (SoC) die, a microcontroller, etc. In some embodiments, the first die 12 is a power management die, such as a power management integrated circuit (PMIC) die. In some embodiments, the second die 14 may be a memory die, including a dynamic random access memory (DRAM) die, a static random access memory (SRAM) die, or a high bandwidth memory (HBM) die. In some embodiments, the first die 12 includes a connection element 122 formed on an active surface of the body of the first die 12. In some embodiments, the connection element 122 may also include a pillar structure. In some embodiments, the second die 14 includes a connection element 142 formed on an active surface of the second die 14. In other embodiments, the connection element 142 may also include a pillar structure. In some embodiments, the active die is a stack of one or more dies (e.g., a logic die stack or a memory die stack). In these embodiments, the material, quantity and / or size may not be limited to the description provided in the embodiments.
[0029] exist Figure 2A to Figure 2B In the embodiment, the first die 12 and the second die 14 are attached to the top surface 200a of the interposer 200 by flip-chip bonding, for example, through the connecting elements 122 and 142. In some embodiments, the connecting elements 122 and 142 are bonded to certain conductive portions of the metal pattern 206c by performing a reflow process, thereby electrically and physically connecting the dies 12 and 14 to the interposer 200. In some embodiments, the connecting elements 122 and 142 may be micro-bumps, such as micro-bumps having copper metal pillars. The connecting elements 122 and 142 electrically connect the first die 12 and the second die 14 to the through-holes 204 of the interposer 200 through the metal patterns 206a, 206b, and 206c.
[0030] In some embodiments, a reflow process is performed as part of the bonding process to bond the first die 12 and the second die 14 to the redistribution structure 210 and to the interposer 200. In one embodiment, the connecting elements 122, 142 are microbumps, and the reflow temperature is in the range of 210 degrees Celsius to 250 degrees Celsius, or about 240 degrees Celsius.
[0031] In some embodiments, the strength of the interposer is improved by arranging the first die and the second die in a specific manner so that the gap between the first die and the second die extends in a direction not parallel to the crystallographic orientation of the semiconductor wafer of the interposer. Thus, the strength of the interposer is enhanced, especially at the gap between the dies that are prone to warping during high-temperature heat treatment (e.g., reflow process), and cracking of the interposer that may be caused by the warping can be significantly reduced or minimized.
[0032] In some embodiments, the bonding between the dies 12, 14 and the interposer 200 may be solder bonding. In some embodiments, the bonding between the dies 12, 14 and the interposer 200 may be direct metal-to-metal bonding, such as copper-to-copper bonding. In some embodiments, an underfill material 150 may be disposed between the gaps between the dies 12, 14 and the interposer 200 and surround the connection elements 122 of the die 12 and the connection elements 142 of the die 14.
[0033] exist Figure 3 In the embodiment, an encapsulant 240 is formed on the interposer 200 to cover the first die 12 and the second die 14, the bottom fill material 150, and the connecting elements 122 and 142. In some embodiments, the encapsulant 240 may be a molding compound. In some embodiments, the encapsulant 240 includes an epoxy resin and may be formed by over-molding, compression molding, or transfer molding. In one embodiment, a curing process may be performed to cure the encapsulant 240. In some embodiments, the first die 12 and the second die 14 and the connecting elements 122 and 142 are encapsulated by the encapsulant 240. In some embodiments, a planarization process (including grinding or polishing) may be performed to partially remove the encapsulant 240, thereby exposing the backside surface 12S of the first die 12 and the backside surface 14S of the second die 14. In some embodiments, the backside surface 12S of the first die 12 and the backside surface 14S of the second die 14 are flush with the top surface 240 a of the encapsulant 240 .
[0034] exist Figure 4 In Figure 3 The structure is shown flipped or turned upside down and placed on a carrier C such that the carrier C directly contacts the backside surfaces 12S and 14S of the first and second dies 12 and 14 and the top surface 240 a of the encapsulant 240 .
[0035] exist Figure 4 In the embodiment, a redistribution structure 220 is formed on the other surface 200b of the interposer 200. In some embodiments, the redistribution structure 220 electrically connects the through-hole 204 and the redistribution structures 210 and 220 are electrically connected through the through-hole 204. In some embodiments, the redistribution structure 220 includes at least one dielectric layer 214 and a metallization pattern 216 located in the dielectric layer 214. In some embodiments, the metallization pattern 216 may include pads, vias, and / or traces to interconnect the through-hole 204 and further connect the through-hole 204 to one or more conductive elements and / or external devices. Although in Figure 4 One dielectric layer is shown in the figure, however, it should be understood that more than one dielectric layer may be included in the rewiring structure. In some embodiments, the material of the dielectric layer 214 may include a polymer material (including polyimide (PI), polybenzoxazole (PBO), benzocyclobutene (BCB) or any other suitable polymer-based dielectric material). In some embodiments, the dielectric layer 214 may be formed by lamination, coating, CVD, etc. In some embodiments, the formation of the metallization pattern 216 may include: patterning the dielectric layer using photolithography and one or more etching processes; and filling the metal material into the opening; and polishing the excess conductive material on the dielectric layer using a chemical mechanical polishing process. In some embodiments, the material of the metallization pattern 216 includes copper, aluminum, tungsten, silver, titanium, and combinations thereof.
[0036] exist Figure 5In the embodiment of the present invention, a conductive connector 250 is formed on the metallization pattern 216 of the rewiring structure 220. In some embodiments, an under bump pad 230 is formed on the metallization pattern 216, and a conductive connector 250 is formed on the under bump pad 230. In some embodiments, the under bump pad 230 includes an under bump metal (UBM). The conductive connector 250 is electrically coupled to the perforation 204 through the metallization pattern 216 of the rewiring structure 220. In some embodiments, the conductive connector 250 is located on the top surface 220a of the rewiring structure 220. In some embodiments, the conductive connector 250 includes a lead-free solder ball, a solder ball, a ball grid array (BGA) ball, a gold bump, a controlled collapse chip connection (C4) bump, or a micro bump containing a copper pillar. In some embodiments, the conductive connector 250 may include a conductive material, such as solder, copper, aluminum, gold, nickel, silver, palladium, tin, or a combination thereof. In some embodiments, the conductive connector 250 is formed by forming a solder paste on the redistribution structure 300 by, for example, evaporation, electroplating, printing, or solder transfer, and then reflowing the solder paste into a desired bump shape. In some embodiments, the conductive connector 250 is placed on the redistribution structure 300 by ball placement, etc. In other embodiments, the conductive connector 250 is formed by forming a solder-free metal pillar (e.g., a copper pillar) by sputtering, printing, electroless plating or electroplating, or CVD, and then forming a lead-free cap layer by plating the metal pillar.
[0037] The conductive connector 250 can be used to bond to an external device or additional electrical components. In some embodiments, the conductive connector 250 is used to bond to a circuit substrate, a semiconductor substrate, or a packaging substrate.
[0038] exist Figure 5 In the embodiment, after forming the conductive connection member 250, a singulation process is performed to cut along the cutting lanes SL ( Figure 4 As shown in FIG. 5 , the wafer form structure is cut into a plurality of individual packages 50. In some embodiments, as shown in FIG. Figure 5 As shown in FIG. 1 , each package 50 includes at least one first die 12, more than one second die 14, an encapsulation body 240 surrounding the first die 12 and the second die 14, connecting elements 122, 142, a portion of the interposer 200 (including the through-hole 204), and a redistribution structure 210, 220 (in the embodiment of FIG. 1 ) including a metal pattern and a metallization pattern 216. Figure 5In the embodiment, the cut redistribution structure is also referred to as a redistribution structure) and the conductive connection member 250 disposed on the top surface 220a of the redistribution structure 220. In some embodiments, the singulation process may include a blade sawing process or a wafer dicing process.
[0039] After the singulation process, the package 50 may be separated from the carrier C and transferred to the tape film TP. In a subsequent process, the package 50 may be turned over and further mounted on a circuit substrate or a package substrate.
[0040] exist Figure 6 In the embodiment of the present invention, a circuit substrate 300 having a mounting portion 302 thereon is provided. In some embodiments, the circuit substrate 300 may include a build-up substrate, a laminate substrate, a circuit board (e.g., a printed circuit board (PCB)), etc. In some embodiments, the mounting portion 302 may include a pre-solder formed on a pad of the circuit substrate. In addition, the circuit substrate 300 may also include electrical contacts or other electrical components embedded in the circuit substrate 300.
[0041] exist Figure 6 In the embodiment of the present invention, the package 50 is placed on the circuit substrate 300 and the package 50 is bonded to the circuit substrate 300 by performing a reflow process. In some embodiments, the package 50 is picked up and placed on the top surface of the circuit substrate 300, and the conductive connector 250 on the bottom surface of the package 50 is aligned with and disposed on the mounting portion 302 of the circuit substrate 300. The reflow process is performed as a part of the bonding process of the package 50 and the circuit substrate 300 to bond the conductive connector 250 to the mounting portion 302. In some embodiments, the reflow process includes performing a heat treatment to transform the conductive connector 250 into a molten state or a semi-molten state so as to be integrated and bonded with the mounting portion 302 of the circuit substrate 300. The reflow temperature of the conductive connector 250 needs to be higher than the melting point of the conductive connector 250. In one embodiment, the conductive connector 250 is a C4 bump, and the reflow temperature is in the range of 210 degrees Celsius to 250 degrees Celsius. In one embodiment, the conductive connection member 250 is a solder ball or a lead-free solder ball, and the reflow temperature is in the range of 200 degrees Celsius to 260 degrees Celsius.
[0042] In some embodiments, the package 50 has a first die 12 bonded to the interposer 200 and a second die 14 located around the first die 12. Figure 2A and Figure 2B As shown in , by arranging the first die 12 and the second die 14 in a specific manner to ensure that the gap extension direction X1 between the first die 12 and the second die 14 is not parallel to the crystallographic orientation of the semiconductor wafer of the interposer, the strength of the interposer structure can be improved. Under thermal shock during the reflow process, even due to CTE mismatch, the warping of the package 50 (and the dies 12, 14) can become less as the strength of the interposer is improved, and the interposer structure can experience less or no cracking.
[0043] By adjusting the arrangement or alignment of the semiconductor die on the semiconductor interposer, the structural strength of the package structure can be improved. Since the gap extension direction defined by the spaced-apart die is pre-arranged to be non-parallel to the crystallographic orientation of the crystal structure of the interposer, the strength of the crystalline interposer is improved by 20% compared to the arrangement of the die with the gap extension direction parallel to the crystallographic orientation of the underlying interposer. Therefore, the problem of interposer cracking during reflow can be significantly reduced. Therefore, the reliability of the package is greatly enhanced and the production yield is greatly increased.
[0044] Fig. 8A is a schematic cross-sectional view showing a package and a circuit substrate according to an embodiment of the present disclosure. Figure 8B is a schematic top view showing the arrangement of dies on an interposer in a package according to an embodiment of the present disclosure.
[0045] exist Fig. 8A In the embodiment, the package 50A is bonded to the circuit substrate 300 through the conductive connector 250. In some embodiments, the package 50A is a CoWoS package having a first die 12A of a larger size and a plurality of second dies 14A arranged around the first die 12A, and the circuit substrate 300 further includes a conductive ball 80 for external connection. In this embodiment, four second dies 14A are arranged next to and around one first die 12A in the package 50A, and two groups of two second dies 14A are arranged in parallel and respectively arranged next to two opposite sides 12X of the first die 12A, as shown in FIG. Figure 8B . In some embodiments, the first die 12A may be a logic die, including a central processing unit (CPU) die, a graphics processing unit (GPU) die, a system chip (SoC) die, a microcontroller, etc. In some embodiments, the first die 12A is a power management die, such as a power management integrated circuit (PMIC) die. In some embodiments, the second die 14A may be a memory die, including a dynamic random access memory (DRAM) die, a static random access memory (SRAM) die, or a high bandwidth memory (HBM) die.
[0046] In one embodiment, the second die 14A is separated from the first die 12A by a gap or spacing SP, and there is a gap extension direction X1 defined by the mutually facing sides of the first die 12A and the second die 14A. In one embodiment, the interposer 200 may have a crystalline structure having a crystal orientation X, such as Figure 8B As shown in , there is an angle θ between the gap extension direction X1 (defined by the mutually facing sides of the first tube core and the second tube core) and the crystallographic orientation X of the interposer 200, and the angle θ is greater than zero and less than 180 degrees. In some embodiments, the angle θ is in the range of about 60 degrees to about 120 degrees. In some embodiments, the angle θ is in the range of 75 degrees to about 105 degrees. In some embodiments, the angle θ is in the range of 85 degrees to about 95 degrees. In one embodiment, the angle θ is about 90 degrees.
[0047] In an embodiment, through displacement of the dies, the gaps between the dies are designed to have an extension direction that is not parallel to the crystallographic orientation of the underlying crystal structure of the interposer. In certain embodiments, the strength of the interposer of the package is improved and the structural reliability of the package is enhanced.
[0048] According to some embodiments of the present disclosure, a manufacturing process is provided. An interposer having a crystal structure is provided. After a first die is disposed on the interposer, a second die is disposed on the interposer. The second die is positioned to be spaced apart from the first die by a gap and to define a gap extension direction of the gap. The gap extension direction is not parallel to a crystallographic orientation of the crystal structure of the interposer. The first die and the second die are bonded to the interposer. A molding compound covering the first die and the second die is formed on the interposer. The molding compound and the interposer are cut into packages.
[0049] According to some embodiments of the present disclosure, bonding the first die and the second die to the interposer includes performing a reflow process. According to some embodiments of the present disclosure, the first die and the second die are bonded to the interposer by microbumps, and the reflow process is performed at a reflow temperature in the range of about 210 degrees Celsius to about 250 degrees Celsius. According to some embodiments of the present disclosure, the manufacturing process also includes: forming a conductive connector on the cut interposer of the package, wherein the cut interposer includes a through hole and the conductive connector is electrically connected to the through hole. According to some embodiments of the present disclosure, the manufacturing process also includes: providing a circuit substrate and bonding the conductive connector of the package to the circuit substrate by performing a reflow process. According to some embodiments of the present disclosure, wherein the conductive connector is a controlled collapse chip connection bump, and the reflow process is performed at a reflow temperature in the range of about 210 degrees Celsius to about 250 degrees Celsius. According to some embodiments of the present disclosure, the manufacturing process also includes: forming a rewiring structure on the interposer before forming the conductive connector. According to some embodiments of the present disclosure, the first die includes at least one logic die, and the second die includes at least one memory die. According to some embodiments of the present disclosure, the manufacturing process further includes: before the first die is arranged and the second die is arranged, a rewiring structure is formed on the interposer. According to some alternative embodiments of the present disclosure, a packaging process includes the following steps. A wafer interposer having a crystal structure is provided and a crystal orientation of the crystal structure is determined. First dies are arranged on the wafer interposer and one side of each first die is oriented to be parallel to a first direction. The first direction is oriented to have an angle θ between the crystal orientation and the first direction, and the angle θ is greater than zero and less than 90 degrees. Second dies are arranged on the wafer interposer and one side of each second die is oriented to be parallel to the first direction. The second die is arranged beside the first die and is spaced apart from the first die by a gap, and the gap extends in the first direction. The first die and the second die are bonded to the wafer interposer. A molding compound covering the first die and the second die is formed on the wafer interposer. The molding compound and the wafer interposer are cut into packages.
[0050] According to some embodiments of the present disclosure, the wafer interposer includes a silicon wafer having a cubic crystal structure.
[0051] According to some embodiments of the present disclosure, the angle θ is in a range of about 60 degrees to about 120 degrees. According to some embodiments of the present disclosure, the angle θ is in a range of about 85 degrees to about 95 degrees. According to some embodiments of the present disclosure, bonding the first die and the second die to the wafer interposer includes performing a reflow process. According to some embodiments of the present disclosure, the first die and the second die are bonded to the wafer interposer via microbumps, and the reflow process is performed at a reflow temperature in a range of about 210 degrees Celsius to about 250 degrees Celsius.
[0052] According to some embodiments of the present disclosure, a packaging structure is described. The packaging structure includes a semiconductor interposer, a first die and a second die, and a conductive connector. The semiconductor interposer has a crystal structure and has a first surface and a second surface opposite to the first surface. The semiconductor interposer includes a through hole (204) extending from the first surface to the second surface. The first die is disposed on the first surface of the semiconductor interposer and is electrically connected to the through hole. The second die is disposed on the first surface of the semiconductor interposer, disposed beside the first die, and is electrically connected to the through hole. The first die and the second die are separated by a gap between the first die and the second die, and the mutually facing sides of the first die and the second die define a gap extension direction of the gap. The gap extension direction is not parallel to the crystallographic orientation of the crystal structure of the semiconductor interposer. The conductive connector is disposed on the second surface of the semiconductor interposer and is electrically connected to the through hole.
[0053] According to some embodiments of the present disclosure, the first die includes at least one logic die, and the second die includes at least one memory die. According to some embodiments of the present disclosure, the package structure further includes a rewiring structure disposed on the first surface of the semiconductor interposer, and the first die and the second die are electrically connected to the through-hole through the rewiring structure. According to some embodiments of the present disclosure, the package structure further includes a rewiring structure disposed on the second surface of the semiconductor interposer, and the conductive connector is electrically connected to the through-hole through the rewiring structure. According to some embodiments of the present disclosure, there is an angle θ between the first direction and the crystallographic orientation, and the angle θ is in the range of about 85 degrees to about 95 degrees.
[0054] The features of several embodiments are summarized above so that those skilled in the art can better understand the various aspects of the present disclosure. Those skilled in the art will understand that they can easily use the present disclosure as a basis for designing or modifying other processes and structures to implement the same purposes and / or achieve the same advantages as the embodiments described herein. Those skilled in the art will also recognize that these equivalent constructions do not depart from the spirit and scope of the present disclosure, and that they can make various changes, substitutions and modifications to them without departing from the spirit and scope of the present disclosure.
[0055] [Explanation of Symbols]
[0056] 12: First die / die
[0057] 12A: First die
[0058] 12S, 14S: Dorsal surface
[0059] 12X: Side
[0060] 14: Second die / die
[0061] 14A: Second die
[0062] 50, 50A: Package
[0063] 80: Conductive ball
[0064] 122, 142: Connecting elements
[0065] 150, 260: bottom filling material
[0066] 200: Intermediary layer
[0067] 200a, 220a, 240a: top surface
[0068] 202: Semiconductor substrate / substrate
[0069] 200b: Surface
[0070] 204: Perforation
[0071] 206a, 206b, 206c: Metal pattern / metallized pattern
[0072] 208a, 208b, 208c, 214: dielectric layer
[0073] 210, 220: Rewiring structure
[0074] 216: Metallized pattern
[0075] 230: Pad under bump
[0076] 240: Encapsulation
[0077] 250: Conductive connector
[0078] 300: Rewiring structure / circuit substrate
[0079] 302: Installation part
[0080] (100): Chip
[0081]
[001] ,
[010] ,
[011] ,
[100] ,
[110] , [-110], [-1-10]: Direction
[0082] {100}: plane
[0083] C: Carrier
[0084] PKU: Packaging Unit
[0085] SL: Cutting Lane
[0086] SP: Spacing
[0087] TP: Tape Film
[0088] X: axis / natural axis / crystallographic orientation
[0089] X1, Y1: direction
[0090] Y: Axis
[0091] θ: angle.
Claims
1. A process for manufacturing a semiconductor package, comprising: providing an interposer having a crystalline structure; disposing a first die on the interposer; disposing a second die on the interposer and positioning the second die to be spaced apart from the first die by a gap and defining a gap extension direction perpendicular to a shortest distance of the gap, wherein the gap extension direction is not parallel to a crystallographic orientation of the crystal structure of the interposer; bonding the first die and the second die to the interposer; forming a molding compound over the interposer covering the first die and the second die; as well as The molding compound and the interposer are cut through to form a package. 2 . The process for manufacturing a semiconductor package according to claim 1 , wherein bonding the first die and the second die to the interposer comprises performing a reflow process.
3. The process for manufacturing a semiconductor package according to claim 2, wherein: The first die and the second die are bonded to the interposer by micro bumps, and the reflow process is performed at a reflow temperature ranging from 210 degrees Celsius to 250 degrees Celsius.
4. The process for manufacturing a semiconductor package according to claim 1, further comprising: Conductive connectors are formed on the cut interposer of the package, wherein the cut interposer includes a through hole and the conductive connector is electrically connected to the through hole.
5. The process for manufacturing a semiconductor package according to claim 4, wherein: Also includes: A circuit substrate is provided and the conductive connectors of the package are bonded to the circuit substrate by performing a reflow process. 6 . The process for manufacturing a semiconductor package according to claim 5 , wherein the conductive connection is a controlled collapse chip connection bump, and the reflow process is performed at a reflow temperature ranging from 210 degrees Celsius to 250 degrees Celsius.
7. The process for manufacturing a semiconductor package according to claim 4, further comprising: Before forming the conductive connection, a redistribution structure is formed on the interposer.
8. The process for manufacturing a semiconductor package according to claim 1, wherein: The first die includes at least one logic die and the second die includes at least one memory die.
9. The process for manufacturing a semiconductor package according to claim 1, wherein: Also includes: Before disposing the first tube core and disposing the second tube core, a redistribution structure is formed on the interposer.
10. A packaging process, comprising: providing a wafer interposer having a crystalline structure; Bonding a first die and a second die on the wafer interposer and separating the first die and the second die from each other by a gap between a side of the first die and a side of the second die, the side of the first die and the side of the second die being substantially parallel to a first direction, wherein the first direction is oriented to have an angle θ between a crystallographic orientation of the crystal structure of the wafer interposer and the first direction, and the angle θ is greater than zero and less than 180 degrees; forming a molding compound over the wafer interposer covering the first die and the second die; as well as The molding compound and the wafer interposer are cut through to form a package. The packaging process according to claim 10 , wherein the wafer interposer comprises a silicon wafer having a cubic crystal structure. 12 . The packaging process according to claim 10 , wherein the angle θ is in a range of 60 degrees to 120 degrees. 13 . The packaging process of claim 10 , wherein bonding the first die and the second die to the wafer interposer comprises performing a reflow process. The packaging process according to claim 10 , wherein the angle θ is in a range of 85 degrees to 95 degrees.
15. The packaging process of claim 13, wherein the first die and the second die are bonded to the wafer interposer by micro bumps, and the reflow process is performed at a reflow temperature ranging from 210 degrees Celsius to 250 degrees Celsius.
16. A packaging structure, comprising: A semiconductor interposer having a crystalline structure, wherein the semiconductor interposer has a first surface and a second surface opposite to the first surface, and the semiconductor interposer includes a through hole extending from the first surface to the second surface; A first tube die and a second tube die are respectively disposed on the first surface of the semiconductor interposer and electrically connected to the through-hole; wherein the first die and the second die are spaced apart from each other by a gap between a side of the first die and a side of the second die, the side of the first die and the side of the second die being substantially parallel to a first direction, and the first direction being non-parallel to a crystallographic orientation of the crystal structure of the semiconductor interposer; as well as A conductive connection member is disposed on the second surface of the semiconductor interposer and is electrically connected to the through hole.
17. The packaging structure according to claim 16, wherein: The first die includes at least one logic die and the second die includes at least one memory die.
18. The package structure according to claim 16, wherein: The invention also includes a redistribution structure disposed on the first surface of the semiconductor interposer, and the first die and the second die are electrically connected to the through-hole through the redistribution structure.
19. The package structure according to claim 16, wherein: The method further includes a redistribution structure disposed on the second surface of the semiconductor interposer, and the conductive connection element is electrically connected to the through-hole through the redistribution structure.
20. The package structure according to claim 16, wherein: An angle θ exists between the first direction and the crystal orientation, and the angle θ is in a range of 85 degrees to 95 degrees.