Semiconductor package and method of manufacturing the same
By using interlayer perforations, stacking structures of dielectric films and backside films, and laser processes to expose perforations in semiconductor packaging, and combining solder paste to form grooves at the interface between the dielectric film and the backside film, the packaging problem is solved It eliminates the warpage problem and improves the stability and reliability of the package.
Patent Information
- Application Number
- CN202010093038.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-10-17
- Filing Date
- 2020-02-14
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2040-08-17
AI Technical Summary
In semiconductor packaging, the warpage problem is difficult to effectively solve, affecting the stability and reliability of the package.
A stacked structure of interlayer perforations, dielectric film and backside film is used, and the perforations are exposed through a laser process, and a groove is formed at the interface between the dielectric film and the backside film in combination with solder paste to reduce warpage.
Through the difference in thermal expansion coefficient and Young's modulus of materials, the warpage of the packaging structure can be alleviated or reduced, and the stability and reliability of the packaging can be improved.
Smart Images

Figure CN112687634B_ABST
Abstract
Description
Technical Field
[0001] Embodiments of the present disclosure relate to a semiconductor package and a method for manufacturing the same. Background Art
[0002] Semiconductor wafers and semiconductor dies may be processed at the wafer level and packaged with other semiconductor devices or dies, and controlling warpage is an important issue for wafer level packaging. Summary of the invention
[0003] A semiconductor package according to an embodiment of the present disclosure includes: a semiconductor die, which is laterally encapsulated by a molding compound; an interlayer through-hole, which is arranged next to the semiconductor die and penetrates the molding compound; a stack of a dielectric film and a backside film, which is arranged on the back side of the semiconductor die and on the molding compound and has an opening exposing the interlayer through-hole; and a solder paste portion, which is arranged on the interlayer through-hole within the opening and has a groove within the opening located at the interface between the dielectric film and the backside film.
[0004] A semiconductor package according to an embodiment of the present disclosure includes: a semiconductor die, which is laterally surrounded by a molding compound; an interlayer through-hole, which is arranged next to the semiconductor die and penetrates the molding compound; a dielectric film, which is arranged on the back side of the semiconductor die and on the molding compound; a backside film, which is arranged on the dielectric film and on the back side of the semiconductor die and on the molding compound, wherein at least one of the thermal expansion coefficient and the Young's modulus of the backside film is greater than at least one of the thermal expansion coefficient and the Young's modulus of the dielectric film; and a solder paste portion, which is arranged on the interlayer through-hole and in an opening that penetrates the dielectric film and the backside film, wherein a groove is located in the sidewall of the opening at the interface between the backside film and the dielectric film.
[0005] A method for manufacturing a semiconductor package according to an embodiment of the present disclosure includes: providing a molding structure having a die and interlayer perforations; forming a redistribution layer on a first side of the molding structure and on the die and the interlayer perforations, wherein the die and the interlayer perforations are electrically connected to the redistribution layer; forming a dielectric layer, wherein the dielectric layer is disposed on a second side of the molding structure, and the first side and the second side are opposite sides of the molding structure; forming a backside film; performing a laser process to form openings in the backside film and the dielectric layer to expose the interlayer perforations; and partially disposing solder paste in the openings and on the exposed interlayer perforations. BRIEF DESCRIPTION OF THE DRAWINGS
[0006] The various aspects of the present disclosure will be best understood by reading the following detailed description in conjunction with the accompanying drawings. It should be noted that, in accordance with standard practice in the industry, the various features are not drawn to scale. In fact, the size of the various features may be arbitrarily increased or reduced for clarity of discussion.
[0007] Figure 1A to Figure 1G are schematic cross-sectional views of various stages in a method of manufacturing a semiconductor package according to some exemplary embodiments of the present disclosure.
[0008] Figure 1F' and Figure 1G' is a schematic enlarged cross-sectional view of an opening of a semiconductor package according to some exemplary embodiments of the present disclosure.
[0009] Figure 2 is a schematic cross-sectional view illustrating a semiconductor package according to some exemplary embodiments of the present disclosure.
[0010] FIG. 3A to FIG. 3F are schematic cross-sectional views of various stages in a method of manufacturing a semiconductor package according to some exemplary embodiments of the present disclosure.
[0011] Figure 4 is a schematic enlarged partial cross-sectional view showing a connection portion of a semiconductor package structure according to some exemplary embodiments of the present disclosure.
[0012] [Explanation of Symbols]
[0013] 10, 30: Semiconductor packaging
[0014] 20: Bottom package
[0015] 40: Top package
[0016] 100, 300: packaging structure
[0017] 102, 302: Carrier
[0018] 103, 303: Peeling layer
[0019] 104, 235, 304: Dielectric layer
[0020] 104S, 200S: Sidewall
[0021] 106, 306: Die bonding film
[0022] 110, 310: interlayer perforation (TIV)
[0023] 110a, 310a: Top
[0024] 120, 320: tube core
[0025] 120a, 320a: Active surface
[0026] 121, 123: substrate
[0027] 122: Pad
[0028] 124: Passivation layer
[0029] 126: Conductive column
[0030] 130, 330, 430: Molding compounds
[0031] 130a: Top surface
[0032] 170, 370: Rewiring layer
[0033] 171: First dielectric material layer / dielectric material layer
[0034] 172: First metallization layer / metallization layer
[0035] 173: Second dielectric material layer / dielectric material layer
[0036] 174: Second metallization layer / metallization layer
[0037] 175: third dielectric material layer / dielectric material layer
[0038] 176: Third metallization layer / metallization layer
[0039] 177: Top dielectric material layer / dielectric material layer
[0040] 178: Top metallization layer / metallization layer
[0041] 178A: Contact pad
[0042] 178B: Joint
[0043] 190, 290, 390: Conductive elements
[0044] 192, 392: Passive components
[0045] 200, 240, 340, BF: posterior membrane
[0046] 201, 341: Opening
[0047] 210, 260, 360, SP: Solder paste part
[0048] 220: Semiconductor die
[0049] 250: Backside redistribution layer
[0050] 270: Front RDL
[0051] 292: Components
[0052] 420: Stacked Die
[0053] 450: Connectors
[0054] 460, UF: bottom filler
[0055] d1: size
[0056] d2: Depth of depression
[0057] DF: Dielectric Film
[0058] G: Gap
[0059] O1: Opening
[0060] RS: Groove
[0061] TP: Carrier Tape DETAILED DESCRIPTION
[0062] The following disclosure provides many different embodiments or examples for implementing the different features of the provided subject matter. Specific examples of components and arrangements are set forth below to simplify the present disclosure. Of course, these are merely examples and are not intended to be limiting. For example, the following description in which a first feature is formed on or on a second feature may include an embodiment in which the first feature and the second feature are formed to be in direct contact, and may also include an embodiment in which an additional feature may be formed between the first feature and the second feature so that the first feature and the second feature may not be in direct contact. In addition, the present disclosure may reuse reference numbers and / or letters in various examples. This repetition is for the purpose of simplicity and clarity, rather than indicating the relationship between the various embodiments and / or configurations discussed by itself.
[0063] Additionally, for ease of description, spatially relative terms such as "beneath," "below," "lower," "above," "upper," etc. may be used herein to describe the relationship of one element or feature illustrated in a figure to another (other) element or feature. The spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations), and the spatially relative descriptors used herein may be interpreted accordingly.
[0064] In addition, for ease of description, terms such as "first", "second", "third", "fourth", etc. may be used herein to describe similar elements or features or different elements or features shown in the figures, and may be used interchangeably depending on the order of presentation or the context of description.
[0065] Other features and processes may also be included. For example, a test structure may be included to help perform verification testing on a three-dimensional (3D) package or a three-dimensional integrated circuit (3DIC) device. The test structure may include, for example, a test pad formed in a redistribution layer (RDL) or on a substrate so that the 3D package or 3DIC can be tested, probes and / or probe cards can be used, etc. Verification testing can be performed on intermediate structures and final structures. In addition, the structures and methods disclosed herein can be used in combination with a test method that includes intermediate verification of a known good die to improve yield and reduce costs.
[0066] Figure 1A to Figure 1G Schematic cross-sectional views of various stages in a method for manufacturing a semiconductor package according to some exemplary embodiments of the present disclosure. In some embodiments, one or more dies are shown to represent multiple dies of a wafer, and one or more packages are shown to represent multiple semiconductor packages obtained after the semiconductor manufacturing method.
[0067] Reference Figure 1A In some embodiments, a carrier 102 having a release layer 103 and a dielectric layer 104 formed thereon is provided. For example, the release layer 103 is disposed between the carrier 102 and the dielectric layer 104. In some embodiments, the carrier 102 is a glass substrate, and the release layer 103 includes a light-to-heat conversion (LTHC) release layer formed on the glass substrate. In some embodiments, the dielectric layer 104 includes a buffer layer, and the material of the buffer layer includes polyimide (PI), polybenzoxazole (PBO), benzocyclobutene (BCB), or any other suitable polymer-based dielectric material.
[0068] Reference Figure 1AIn some embodiments, a through interlayer via (TIV) 110 is formed on the dielectric layer 104 above the carrier 102. In some embodiments, the TIV 110 is an integrated fan-out (InFO) via. In some embodiments, the TIV 110 can be formed by: forming a mask pattern (not shown) on the dielectric layer 104, the mask pattern having an opening exposing the dielectric layer 104 on the carrier 102; forming a metal material filling the opening by electroplating or deposition to form the TIV; and then removing the mask pattern. In some embodiments, the TIV 110 can be arranged next to and / or around the location of the tube core. In alternative embodiments, the TIV is optional and the formation of the TIV can be omitted.
[0069] Reference Figure 1B , providing one or more dies 120 and placing the one or more dies 120 on the carrier 102. Figure 1B In the embodiment, only one die is shown as an exemplary die of the package structure, but it should be understood that more than one die or different types of dies may be included in the package structure. In some embodiments, a die attach film 106 is provided between the dielectric layer 104 and the die 120 to better bond the die 120 to the dielectric layer 104 of the carrier 102. In an exemplary embodiment, as shown in FIG. Figure 1B As shown in , the die 120 may include one or more types of chips selected from the following: application-specific integrated circuit (ASIC) chips, analog chips, sensor chips, wireless and radio frequency chips, voltage regulator chips, or memory chips. In some embodiments, the die and chip can be used interchangeably.
[0070] In some embodiments, Figure 1BIn the embodiment, the die 120 is provided with a contact or pad 122, a passivation layer 124 and a conductive column 126, the contact or pad 122 is located on the substrate 121 of the die 120, the passivation layer 124 is formed on the substrate 121 and has an opening exposing the pad 122, and the conductive column 126 is located in the opening and connected to the pad 122. In some embodiments, the pad 122 is an aluminum pad, a copper pad or other suitable metal pad. In some embodiments, the material of the passivation layer 124 includes silicon nitride, silicon oxynitride, a polymer material or a dielectric material. In some embodiments, the conductive column 126 is a copper column or a copper alloy column. In one embodiment, the die 120 is provided and attached to the carrier 102 so that the active surface 120a of the die 120 faces upward. In some embodiments, the TIV 110 is arranged around the periphery of the die 120. However, depending on product design, some of the TIVs 110 may be arranged at locations other than the periphery of the die 120. In some embodiments, a plurality of dies 120 are stacked side by side on the carrier 102, and the number of dies arranged side by side or stacked on top of another die may be adjusted or modified according to product design, but is not limited by the exemplary embodiments.
[0071] Reference Figure 1B In some embodiments, the die 120 and the TIV 110 located on the carrier 102 are molded and encapsulated in a molding compound 130. In one embodiment, the molding compound 130 fills the space between the die 120 and the TIV 110 and covers the die 120 and the TIV 110 on the dielectric layer 104 at least laterally. In one embodiment, the material of the molding compound 130 includes an epoxy resin, a phenolic resin, or a silicone-containing resin. In some embodiments, the material of the molding compound 130 includes filler particles. In some embodiments, the molding compound 130 is overmolded, and then the molding compound 130 is planarized to expose the top 110a of the TIV 110 and the active surface 120a of the die 120. In some embodiments, the overmolded molding compound 130 and the TIV 110 are polished until the conductive pillars 126 of the die 120 are exposed. In one embodiment, after planarization, the top 110a of the TIV 110, the top surface 130a of the molding compound 130, and the active surface 120a of the die 120 become substantially flat and flush with each other. In some embodiments, the molding compound 130 and / or the TIV 110 are planarized by a grinding process or a chemical mechanical polishing (CMP) process.
[0072] Reference Figure 1CIn some embodiments, a redistribution layer 170 is formed on the molded structure having the mold compound 130, the TIV 110, and the die 120. In some embodiments, the redistribution layer 170 is electrically connected to the TIV 110 and the die 120. Forming the redistribution layer 170 includes sequentially forming alternating more than one dielectric material layer and more than one metallization layer.
[0073] Reference Figure 1C In some embodiments, a redistribution layer 170 is formed on the mold compound 130, on the TIV 110, and on the die 120 by sequentially forming a first dielectric material layer 171, a first metallization layer 172, a second dielectric material layer 173, a second metallization layer 174, a third dielectric material layer 175, and a third metallization layer 176. In some embodiments, forming the redistribution layer 170 further includes: forming a top dielectric material layer 177 having an opening, the opening exposing some portions of the third metallization layer 176; forming another metal layer (not shown) on the top dielectric material layer 177 filling the opening; and then patterning the metal layer to form a top metallization layer 178. In some embodiments, the first metallization layer 172 is electrically connected to the die 120 through the conductive pillars 126, and is electrically connected to the TIV 110.
[0074] In some embodiments, the materials of dielectric material layers 171, 173, 175, 177 may be the same or different. In some embodiments, the materials of dielectric material layers 171, 173, 175, 177 include one or more polymer dielectric materials, such as polyimide, benzocyclobutene (BCB), polybenzoxazole (PBO) or any other suitable polymer dielectric material. In some embodiments, the materials of metallization layers 172, 174, 176, 178 may be the same or different, and the materials of metallization layers 172, 174, 176, 178 may be selected from copper, nickel, aluminum, tungsten or a combination thereof. In some embodiments, metallization layers 172, 174, 176 may include routing traces or fan-out traces. In some embodiments, metallization layer 178 may include contact pads 178A and bonding portions 178B for receiving bumps or other components. In some embodiments, the bonding portion or the contact pad may further include an adhesion layer, a seed layer, and / or an under-ball metallurgy (UBM) pattern formed on the surface of the bonding portion or the pad for enhancing adhesion, as desired.
[0075] Reference Figure 1D, a conductive element 190 is disposed on the contact pad 178A of the redistribution layer 170. In some embodiments, the conductive element 190 can be disposed and fixed to the contact pad 178A by performing a ball placement process and then a reflow process. In some embodiments, the conductive element 190 is, for example, a controlled collapse chip connection (C4) bump or micro bump. Figure 1D As shown in FIG. 1 , some of the conductive elements 190 are electrically connected to the die 120 through the redistribution layer 170, and some of the conductive elements 190 are electrically connected to the TIV 110 through the redistribution layer 170. In some embodiments, a passive component 192 (e.g., a capacitor, an inductor, or a resistor) is connected to the bonding portion 178B of the redistribution layer 170 by a solder flux. In some embodiments, the passive component 192 may include an integrated passive device (IPD).
[0076] Reference Figure 1D and Figure 1E In some embodiments, the package structure 100 is turned upside down (flipped) and transferred to the carrier tape TP, and then the carrier 102 and the peeling layer 103 are removed together. Figure 1E In the embodiment of the present invention, a backside film 200 is formed on the dielectric layer 104 and on the molding compound 130 and the tube core 120. In some embodiments, the backside film 200 is laminated on the dielectric layer 104, and then cured to cure the backside film 200. In some embodiments, the backside film 200 is formed by coating or printing. In one embodiment, the backside film 200 has a thickness ranging from 20 microns to 100 microns. In some embodiments, the material of the backside film 200 may be a polymeric material, including a resin material mixed with a filler or a resin material with glass fiber. For example, the resin material includes epoxy resin, phenolic resin or silicone resin. In some embodiments, the polymeric material of the backside film 200 may include epoxy resin and a filler with a small particle size, and the filler with a small particle size may be a silica filler or an aluminum oxide filler with a particle size less than 0.5 microns. The material of the backside film 200 may be selected to make the backside film 200 transparent (transparent to visible light). As a result, the subsequent drilling process can achieve better alignment, and the pre-solder formed later can obtain better coverage on the TIV.
[0077] The backside film 200 has a relatively high coefficient of thermal expansion (CTE) and / or a relatively high Young's modulus, so that the backside film 200 can alleviate or reduce warpage of the package structure through the manufacturing process (especially during heat treatment).
[0078] In some embodiments, the coefficient of thermal expansion (CTE) of the backside film 200 is greater than the coefficient of thermal expansion of the underlying material layer. In some embodiments, the backside film 200 has a CTE in the range of 10ppm / °C to 200ppm / °C, while the underlying dielectric layer 104 has a CTE in the range of 5ppm / °C to 100ppm / °C. In some embodiments, the Young's modulus of the backside film 200 is higher than the Young's modulus of the underlying material layer. In some embodiments, the backside film 200 has a Young's modulus greater than 5GPa, while the underlying dielectric layer 104 has a Young's modulus less than 10GPa. In some embodiments, the CTE of the backside film 200 is greater than the CTE of the underlying material layer and the Young's modulus of the backside film 200 is higher than the Young's modulus of the underlying material layer. In certain embodiments, the backside film 200 has a CTE ranging from 10 ppm / °C to 200 ppm / °C and a Young's modulus greater than 5 GPa, while the underlying dielectric layer 104 has a CTE ranging from 5 ppm / °C to 100 ppm / °C and a Young's modulus less than 10 GPa.
[0079] exist Figure 1F In the embodiment of the present invention, the backside film 200 is partially removed by performing a laser process that forms an opening 201. For example, the laser process includes a laser drilling process. In some embodiments, the laser process removes portions of the backside film 200 and portions of the underlying dielectric layer 104 to form the opening 201 that exposes the underlying TIV 110. In some embodiments, since the backside film 200 is transparent, the alignment of the position of the opening 201 toward the underlying TIV 110 can be easier and more accurate. In principle, the position of the opening 201 is aligned and overlapped with the position of the TIV 110 in the vertical direction (in the thickness direction). In some embodiments, after the laser process is performed, the formed opening 201 has an oblique profile.
[0080] Additionally, if the backside film 200 is transparent, the laser marking or laser ablation process may be skipped and the risk of damaging the die may be avoided as the markings on the backside of the die 120 are clearly visible from above the backside film 200 .
[0081] Figure 1F' yes Figure 1F Schematic enlarged cross-sectional view of the opening 201 of the semiconductor package in FIG. Figure 1F' As shown in , since the opening 201 is formed by performing a laser process (e.g., a laser drilling process), the backside film 200 has an inclined sidewall 200S in the opening 201, and the dielectric layer 104 also has an inclined sidewall 104S in the opening 201. In some embodiments, according to the cross-sectional view, the inclined sidewall 104S and the inclined sidewall 200S are formed to have different steepness. In one embodiment, the steepness of the inclined sidewall 104S is less than the steepness of the inclined sidewall 200S. In some embodiments, due to the difference in thermal properties (and / or mechanical properties) between the dielectric layer 104 and the backside film 200, a recess is formed at the interface between the dielectric layer 104 and the backside film 200 after the laser process. In one embodiment, a recess RS is formed between the inclined sidewall 104S and the inclined sidewall 200S. From a top view, if the opening 201 is formed as a circular or elliptical opening, the groove RS is formed as a ring-shaped or arc-shaped groove (gap). In some embodiments, when the opening 201 is formed to have a size d1 (i.e., the maximum size of the opening) of about 200 micrometers to 300 micrometers, the groove RS is formed to have a recess depth d2 (measured from the most recessed portion of the dielectric layer 104 in the opening to the most protruding portion) of about 0.5 micrometers to 5 micrometers.
[0082] exist Figure 1G In some embodiments, the solder paste portion 210 is filled into the opening 201 and is directly disposed on the TIV 110 exposed by the opening 201 by applying the solder paste. In some embodiments, the opening 201 is not completely filled with the solder paste portion 210, so that the top of the solder paste portion filled in the opening 201 is lower than the top surface of the backside film 200. For example, the material of the solder paste may include a mixture of pre-alloyed solder powder and flux. In some embodiments, the solder paste may be formed by printing, coating, or dispensing.
[0083] Figure 1G' yes Figure 1G Schematic enlarged cross-sectional view of the opening 201 of the semiconductor package in FIG. Figure 1G'As shown in , the solder paste portion 210 does not fill the opening 201 and does not fill the recess RS in the opening 201. For example, the amount of the solder paste portion 210 provided into the opening 201 is well controlled so that the opening 201 is not completely filled or is only half filled. In some embodiments, due to the viscosity of the solder paste, the solder paste portion 210 filled into the opening 201 does not contact the inclined sidewall 200S of the backside film 200 and may partially contact the inclined sidewall 104S of the dielectric layer 104 in the opening 201. That is, the recess RS is not filled by the solder paste portion 210 provided into the opening 201, and the recess RS is retained. In some embodiments, the solder paste portion 210 filled into the opening 201 is in direct contact with the top surface of the TIV 110. As shown in FIG. Figure 1G' As shown in FIG. 2 , there is an empty space or gap G between the solder paste portion 210 inside the opening 201 , the dielectric layer 104 , and the backside film 200 .
[0084] Return to reference Figure 1G In some embodiments, a dicing process is then performed to cut the entire package structure 100 (at least through the backside film 200, the dielectric layer 104, the mold compound 130, and the redistribution layer 170) into individual and separate semiconductor packages 10. In one embodiment, the dicing process is a wafer dicing process including mechanical sawing or laser cutting. In some embodiments, a marking process may be performed as needed to produce a mark on the backside film 200 above the die 120.
[0085] FIG. 3A to FIG. 3F are schematic cross-sectional views of various stages in a method of manufacturing a semiconductor package according to some exemplary embodiments of the present disclosure.
[0086] Reference Figure 3A In some embodiments, a carrier 302 having a release layer 303 formed thereon is provided. In some embodiments, a backside film 340 is formed on the release layer 303. In some embodiments, the carrier 302 is a glass substrate, and the release layer 303 includes a light-to-heat conversion (LTHC) release layer formed on the glass substrate. In some embodiments, the material and formation of the backside film 340 are similar to the material and formation of the backside film 200 described in the previous embodiments.
[0087] Reference Figure 3BIn some embodiments, a dielectric layer 304 is formed on the backside film 340 and a through-interlayer via (TIV) 310 is formed on the dielectric layer 304 over the carrier 302. In some embodiments, the TIV 310 is an integrated fan-out (InFO) via. As described above, the materials and formation of the dielectric layer 304 and the TIV 310 are similar to the materials and formation of the dielectric layer 104 and the TIV 110. In alternative embodiments, the TIV is optional and the formation of the TIV may be omitted.
[0088] Reference Figure 3B , a die 320 having a substrate 321 is provided (only one die is shown as an exemplary die) and the die 320 is bonded to the dielectric layer 304 by providing a die attach film 306 between the die 320 and the dielectric layer 304. It should be understood that more than one die or different types of dies may be included in the package structure. In addition, the die 320 may include one or more types of chips selected from the following: application-specific integrated circuit (ASIC) chips, analog chips, sensor chips, wireless and radio frequency chips, voltage regulator chips, or memory chips. Figure 3B In the embodiment, a die 320 is provided and bonded to a carrier 302 such that an active surface 320a of the die 320 faces upward. Depending on product design, some of the TIVs 310 may be arranged around the periphery of the die 320 or at a position other than the periphery of the die 320.
[0089] Reference Figure 3B , in some embodiments, the die 320 and the TIV 310 are molded and encapsulated in a molding compound 330. In one embodiment, the molding compound 330 surrounds the die 320 and the TIV 310 at least laterally and fills the space between the die 320 and the TIV 310. In one embodiment, the material and formation of the molding compound 330 are similar to the material and formation of the molding compound 130. In some embodiments, after planarization, the top 310a of the TIV 310 and the active surface 320a of the die 320 are exposed from the molding compound 330.
[0090] Reference Figure 3C In some embodiments, a redistribution layer 370 is formed on the mold compound 330, on the TIV 310, and on the die 320. In some embodiments, the redistribution layer 370 is electrically connected to the TIV 310 and the die 320. Forming the redistribution layer 370 includes sequentially forming more than one dielectric material layer and more than one metallization layer alternately, and the material and formation of the redistribution layer 370 are similar to the material and formation of the redistribution layer 170.
[0091] Reference Figure 3C, the conductive element 390 and the passive component 392 are disposed and bonded to the redistribution layer 370. In some embodiments, the conductive element 390 is, for example, a C4 bump or a micro bump. Figure 3C As shown in , some of the conductive elements 390 are electrically connected to the die 320 through the redistribution layer 370 , and some of the conductive elements 390 are electrically connected to the TIV 310 through the redistribution layer 370 .
[0092] Reference Figure 3C and Figure 3D In some embodiments, the package structure 300 is flipped over and transferred to the carrier tape TP, and then the carrier 302 and the peeling layer 303 are removed together. Figure 3D In the embodiment, the backside film 340 formed on the dielectric layer 304 is exposed. In some embodiments, the backside film 340 may be transparent (transparent to visible light).
[0093] exist Figure 3E In the embodiment, a laser process is performed to form an opening 341 in the backside film 340. In some embodiments, the laser process includes a laser drilling process. In some embodiments, the laser drilling process removes portions of the backside film 340 and portions of the underlying dielectric layer 304 to form the opening 341 exposing the underlying TIV 310. During the laser drilling process, the backside film 340 and the dielectric layer 304, which are made of different materials, are drilled into different profiles to form the opening 341. The profile of the opening 341 may be similar to Figure 1F' , wherein a groove is formed between the backside film 340 and the dielectric layer 304 .
[0094] In some embodiments, since the backside film 340 is transparent, the alignment of the opening 341 toward the underlying TIV 310 is more accurate. In principle, the position of the opening 341 is vertically aligned (in the thickness direction) with and overlaps the position of the TIV 310. In some embodiments, after the laser process, the formed opening 341 has an inclined sidewall having an oblique profile.
[0095] exist Figure 3FIn some embodiments, the solder paste portion 360 is provided into the opening 341 and is directly disposed on the TIV 310 exposed by the opening 341. In some embodiments, the opening 341 is not completely filled with the solder paste portion 360. In an embodiment, the amount of the solder paste portion 360 provided into the opening 341 is well controlled so that the solder paste portion 360 filled into the opening 341 does not contact the inclined sidewall of the opening 341, and the groove is retained. As previously described, there is an empty space or gap between the solder paste portion 360 inside the opening 341, the dielectric layer 304, and the backside film 340.
[0096] Return to reference Figure 3F In some embodiments, a dicing process is then performed to cut the entire package structure 300 (at least through the backside film 340, the dielectric layer 304, the mold compound 330, and the redistribution layer 370) into individual and separate semiconductor packages 30. In some embodiments, a marking process may be performed as needed to produce a mark on the backside film 340 above the die 320.
[0097] Additionally, since backside film 340 is transparent, the markings on the back side of die 320 can be clearly seen from above the other side of backside film 340, which can reduce or minimize the laser marking or laser ablation process and avoid the risk of the die being damaged during the laser process.
[0098] Since the backside film 340 has a relatively high coefficient of thermal expansion (CTE) and / or a relatively high Young's modulus, the backside film 340 may mitigate or reduce warpage of the package structure through the manufacturing process, especially during thermal treatment.
[0099] In some embodiments, the previously obtained semiconductor package 10 or 30 may be used as a final product. In alternative embodiments, the semiconductor package 10 or 30 may further include an additional die or sub-package unit disposed on the die, and another redistribution layer may be formed to electrically connect the additional die or sub-package unit. The structure and / or process of the present disclosure are not limited by the exemplary embodiments.
[0100] Figure 2 is a schematic cross-sectional view showing a semiconductor package according to some exemplary embodiments of the present disclosure. Figure 2 In the embodiment, the bottom package 20 is similar to Figure 1A to Figure 1G or FIG. 3A to FIG. 3FThe package structure 10 or 30 is formed after the process described in , except that an additional backside redistribution layer (RDL) 250 is formed between the semiconductor die 220 and the stack of the dielectric layer 235 and the backside film 240. The bottom package 20 also includes a frontside RDL 270 formed on the semiconductor die 220 and a conductive element 290 and a component 292 mounted on the frontside RDL 270. The top package 40 having the stacked die 420 encapsulated by the molding compound 430 and the connector 450 is connected to the bottom package 20 through the connector 450, and the connector 450 is combined with the solder paste portion 260 disposed in the opening O1 of the stack of the dielectric layer 235 and the backside film 240. In some embodiments, the top package 40 can be picked up and placed on the bottom package 20, and the connector 450 is combined with the solder paste portion 260 in the corresponding opening by a reflow process. Afterwards, in some embodiments, an underfill 460 is formed between the top package 40 and the bottom package 20 and fills the gap between the top package 40 and the bottom package 20. In addition, the underfill 460 fills the empty space or gap between the connector 450, the solder paste portion 260, and the sidewall of the opening O1. It should be understood that Figure 2 The semiconductor package structure shown in is merely an exemplary structure, and the formation of the backside RDL may be optional.
[0101] Figure 4 is a schematic enlarged partial cross-sectional view showing a connection portion of a semiconductor package structure according to some exemplary embodiments of the present disclosure. Figure 4 As shown in FIG. 1 , inside the opening defined by the dielectric film DF and the backside film BF, the underfill UF fills the groove RS between the dielectric film DF and the backside film BF, and the underfill UF fills the empty space or gap between the solder paste portion SP, the dielectric film DF, and the backside film BF. In some embodiments, the size of the opening is smaller than the size of the TIV so that the TIV is not completely exposed. The solder paste portion SP formed on the exposed TIV is directly on the TIV (at Figure 4 However, the extension span of the solder paste portion SP is limited by the dielectric film DF located on the TIV.
[0102] According to the above exemplary embodiments, the configuration of stacked layers or package subunits can be formed in an integrated fan-out (InFO) wafer-level packaging structure or a fan-in wafer-level packaging structure in a suitable manner. The dielectric layer and the backside film laminated on the dielectric layer can be formed of different materials and have different thermal properties and mechanical properties, such as different thermal conductivity, Young's modulus and / or glass transition point. In some embodiments, since at least one of the CTE and Young's modulus of the backside film is higher than at least one or both of the CTE and Young's modulus of the underlying dielectric layer, the warpage of the package structure is significantly improved. Due to the difference in materials and their properties, a groove is formed between the dielectric layer and the backside film after the laser drilling process.
[0103] According to some embodiments, a semiconductor package includes a semiconductor die, a through-interlayer via (TIV), a stack of a dielectric film and a backside film, and a solder paste portion. The semiconductor die is encapsulated laterally by a molding compound. The TIV is disposed beside the semiconductor die and the TIV penetrates the molding compound. The stack of the dielectric film and the backside film is disposed on the back side of the semiconductor die and on the molding compound. The stack includes an opening exposing the TIV. The solder paste portion is disposed on the TIV in the opening. A groove is provided at an interface between the dielectric film and the backside film in the opening.
[0104] In some embodiments, a first redistribution layer is disposed on an active surface of the semiconductor die. In some embodiments, a second redistribution layer is disposed on the back side of the semiconductor die. In some embodiments, a top package has one or more chips and connectors, wherein the top package is disposed on the stack so that the connectors are partially bonded to the solder paste portion; and a bottom fill is disposed between the top package and the stack. In some embodiments, the bottom fill fills the groove. In some embodiments, the opening penetrating the stack has an inclined sidewall. In some embodiments, the solder paste portion partially fills the opening without filling the groove and does not contact the inclined sidewall of the opening. The dielectric film and the backside film are different materials, and the dielectric film is located between the interlayer perforation and the backside film.
[0105] According to some embodiments, a semiconductor package includes a semiconductor die, a through-interlayer via (TIV), a dielectric film, a backside film, and a solder paste portion. The semiconductor die is surrounded laterally by a molding compound. The TIV is disposed beside the semiconductor die and penetrates the molding compound. The dielectric film is disposed on the backside of the semiconductor die and on the molding compound. The backside film is disposed on the dielectric film and on the backside of the semiconductor die and on the molding compound. At least one of a coefficient of thermal expansion (CTE) and a Young's modulus of the backside film is greater than at least one of a coefficient of thermal expansion (CTE) and a Young's modulus of the dielectric film. The solder paste portion is disposed on the TIV and is located within an opening of the dielectric film and the backside film. A groove is located in a sidewall of the opening at an interface between the backside film and the dielectric film.
[0106] In some embodiments, the material of the backside film includes filler particles and the particle size of the filler particles is less than 0.5 microns. In some embodiments, the backside film is transparent to invisible light. In some embodiments, a redistribution layer is disposed on the active surface of the semiconductor die. In some embodiments, a top package has one or more chips and connectors, wherein the top package is disposed on the backside film so that the connector is combined with the solder paste portion; and an underfill is disposed between the top package and the backside film and between the solder paste portion, the dielectric film, and the backside film. In some embodiments, the underfill fills the groove at the interface between the dielectric film and the backside film in the opening.
[0107] According to some embodiments, a method for manufacturing a semiconductor package is provided. A molded structure having a die and a TIV is provided. A redistribution layer is formed on a first side of the molded structure and on the die and the TIV. The die and the TIV are electrically connected to the redistribution layer. A dielectric layer is formed, and the dielectric layer is disposed on a second side of the molded structure, and the first side and the second side are opposite sides of the molded structure. A backside film is formed. A laser process is performed to form an opening in the backside film and the dielectric layer to expose the TIV. A solder paste portion is provided into the opening and on the exposed TIV.
[0108] In some embodiments, performing the laser process includes: performing a laser drilling process of drilling through the backside film and the dielectric layer until the interlayer perforations are exposed. In some embodiments, performing the laser drilling process includes: forming a groove in the opening at the interface between the backside film and the dielectric layer during drilling through the backside film and the dielectric layer. In some embodiments, the dielectric layer is formed before forming the redistribution layer, and the backside film is formed on the dielectric layer after forming the redistribution layer. In some embodiments, the backside film is formed before forming the dielectric layer, and the dielectric layer is formed on the backside film before forming the redistribution layer.
[0109] The features of several embodiments are summarized above so that those skilled in the art can better understand the various aspects of the present disclosure. Those skilled in the art will understand that they can easily use the present disclosure as a basis for designing or modifying other processes and structures to implement the same purposes and / or achieve the same advantages as the embodiments described herein. Those skilled in the art will also recognize that these equivalent constructions do not depart from the spirit and scope of the present disclosure, and that they can make various changes, substitutions and modifications to them without departing from the spirit and scope of the present disclosure.
Claims
1. A semiconductor package, include: a semiconductor die laterally encapsulated by a molding compound; an interlayer via disposed beside the semiconductor die and penetrating through the molding compound; a stack of a dielectric film and a backside film disposed on the backside of the semiconductor die and on the molding compound and having an opening exposing the interlayer through-hole; a top package disposed on the stack; A bottom filler, disposed between the top package and the stack; as well as a solder paste portion disposed on the interlayer through-hole within the opening, A groove is provided in the opening at the interface between the dielectric film and the backside film, and the bottom filling glue fills the groove. 2 . The semiconductor package of claim 1 , further comprising a first redistribution layer disposed on an active surface of the semiconductor die. 3 . The semiconductor package of claim 2 , further comprising a second redistribution layer disposed on the backside of the semiconductor die. 4 . The semiconductor package of claim 2 , wherein the top package having one or more chips and connectors is disposed on the stack such that the connectors are partially bonded to the solder paste. 5 . The semiconductor package of claim 4 , further comprising a second redistribution layer disposed on the backside of the semiconductor die. The semiconductor package according to claim 4 , wherein the underfill fills up spaces between the connectors. 7 . The semiconductor package of claim 1 , wherein the opening penetrating through the stack has an inclined sidewall. 8 . The semiconductor package according to claim 7 , wherein the solder paste portion partially fills the opening without filling up the groove and without contacting the inclined sidewall of the opening. 9 . The semiconductor package according to claim 1 , wherein the dielectric film and the backside film are different materials, and the dielectric film is located between the interlayer through-hole and the backside film.
10. A semiconductor package, include: a semiconductor die laterally surrounded by a molding compound; an interlayer via disposed beside the semiconductor die and penetrating through the molding compound; a dielectric film disposed on the back side of the semiconductor die and on the molding compound; a backside film disposed on the dielectric film and on the backside of the semiconductor die and on the molding compound, wherein at least one of a coefficient of thermal expansion and a Young's modulus of the backside film is greater than at least one of a coefficient of thermal expansion and a Young's modulus of the dielectric film, and a material of the backside film comprises filler particles and a particle size of the filler particles is less than 0.5 micrometers; and A solder paste portion is disposed on the interlayer through-hole and within an opening penetrating through the dielectric film and the backside film, wherein a groove is located in a sidewall of the opening at an interface between the backside film and the dielectric film. The semiconductor package according to claim 10 , wherein a material of the backside film comprises a polymer material. 12 . The semiconductor package according to claim 11 , wherein the backside film is transparent to invisible light.
13. The semiconductor package of claim 10, further comprising a redistribution layer disposed on an active surface of the semiconductor die.
14. The semiconductor package according to claim 13, further comprising: include: a top package having one or more chips and connectors, wherein the top package is disposed on the backside film such that the connectors are partially bonded to the solder paste; as well as An underfill is disposed between the top package and the backside film and between the solder paste portion, the dielectric film, and the backside film. 15 . The semiconductor package of claim 14 , wherein the underfill fills up the groove within the opening at the interface between the dielectric film and the backside film.
16. A method for manufacturing a semiconductor package, include: Providing a molded structure having a tube core and interlayer through holes; forming a redistribution layer on the first side of the mold structure and on the die and the interlayer vias, wherein the die and the interlayer vias are electrically connected to the redistribution layer; forming a dielectric layer, wherein the dielectric layer is disposed on a second side of the mold structure, and the first side and the second side are opposite sides of the mold structure; forming a backside film on the dielectric layer; performing a laser process of forming openings in the backside film and the dielectric layer to expose the interlayer through-holes and form grooves at the interface between the backside film and the dielectric layer; disposing a solder paste portion in the opening and on the exposed interlayer through-hole; providing a top package with a connector and connecting the connector to the solder paste portion; as well as An underfill is formed between the top package, the backside film and the dielectric layer to fill the groove.
17. The method according to claim 16, wherein the laser process is performed include: A laser drilling process is performed to drill through the backside film and the dielectric layer until the interlayer through-hole is exposed. 18 . The method of claim 16 , wherein the dielectric layer is formed before forming the redistribution layer, and the backside film is formed on the dielectric layer after forming the redistribution layer.
19. The method of claim 16, wherein the backside film is formed before forming the dielectric layer, and the dielectric layer is formed on the backside film before forming the redistribution layer.
Citation Information
Patent Citations
Package structure and fabrication method thereof
CN104576593A
Semiconductor Package Structure And Method For Forming The Same
CN106560918A
Chip package
CN107958891A
Package substrate and fabrication method thereof
TW201025533A
Method of manufacturing thin-film electronic device
US20070026581A1