Three-dimensional flash memory and its manufacturing method
By forming specific stacked layers and pillar structures in three-dimensional NAND flash memory, the problem of insufficient development of NAND flash memory is solved, high process qualification rate and fast operation speed are achieved, and the performance of the memory is improved.
Patent Information
- Application Number
- CN201911020352.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-10-18
- Filing Date
- 2019-10-25
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2040-04-30
AI Technical Summary
In the existing technology, NAND flash memory has been less developed, and its application in multi-dimensional flash memory cell arrays has not been fully utilized, resulting in a lag in its development in the memory field.
Using the manufacturing method of three-dimensional flash memory, by forming a stacked structure and a pillar structure, including alternating insulating layers, sacrificial layers, channel layers and conductor layers, using the combination of gate dielectric layers and conductor layers to achieve high process qualification efficiency and fast operating speed.
It achieves a simple process, high process qualification rate and fast operation speed of three-dimensional flash memory. By defining the position of the conductor layer and selecting the memory unit, the performance of the memory is improved.
Smart Images

Figure CN112687697B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a three-dimensional flash memory and a manufacturing method thereof, and in particular to a three-dimensional and type flash memory and a manufacturing method thereof. Background Art
[0002] Non-volatile memory (eg, flash memory) has become a widely used memory in personal computers and other electronic devices because it has the advantage that the stored data will not disappear after power failure.
[0003] The flash memories commonly used in the industry at present include NOR flash memories and NAND flash memories, but AND flash memories are less used. Since AND flash memories can also be used in multi-dimensional flash memory cell arrays, they have the same high density and area utilization as NAND flash memories. Therefore, the development of AND flash memories has become a current trend. Summary of the invention
[0004] The invention provides a method for manufacturing a three-dimensional flash memory, which has the advantages of simple process, high process qualification rate and the like.
[0005] The manufacturing method of the three-dimensional flash memory of the present invention includes the following steps. First, a stacked structure is formed on a substrate. The stacked structure includes a first insulating layer and a first sacrificial layer that are alternately stacked. Then, a first column structure that penetrates the stacked structure and has a rectangular outline is formed. The first column structure includes a second insulating layer and a second sacrificial layer, and the second insulating layer surrounds the second sacrificial layer. After that, a second column structure that penetrates the stacked structure and has an elliptical outline is formed. The second column structure includes a channel layer and an insulating column, and the channel layer surrounds the insulating column. The second sacrificial layer is located on both sides of the channel layer and contacts the channel layer, and the second sacrificial layer faces the long axis section of the second column structure. Next, the first sacrificial layer is removed to form a lateral opening. The lateral opening exposes a portion of the second insulating layer and a portion of the channel layer. Then, a gate dielectric layer is formed in the lateral opening. The gate dielectric layer surrounds the exposed second insulating layer and the channel layer. Then, a gate layer is filled in the lateral opening. Finally, the second sacrificial layer is replaced by a conductor layer.
[0006] The invention provides a three-dimensional flash memory with a fast operating speed.
[0007] The three-dimensional flash memory of the present invention includes a stacked structure and a column structure. The stacked structure is located on a substrate and includes a first insulating layer and a gate layer alternately arranged. A gate dielectric layer is arranged between the first insulating layer and the gate layer. The column structure runs through the stacked structure and includes an insulating column, a channel layer, a conductor layer and a second insulating layer. The insulating column has an elliptical profile. The channel layer surrounds the insulating column. The conductor layer is located on both sides of the channel layer and contacts the channel layer, and the conductor layer faces the long axis section of the insulating column. The second insulating layer surrounds the side wall of the conductor layer that is not in contact with the channel layer. Among them, the gate dielectric layer surrounds the side wall of the column structure exposed by the first insulating layer.
[0008] Based on the above, the present invention can define the position of the subsequent conductor layer by forming the first column structure and the second column structure in sequence, so that the conductor layer can be formed by a simple process with a high process yield. In addition, in the three-dimensional and type flash memory of the present invention, each column structure has an independent conductor layer, so that the storage unit (the intersection of the gate layer and the column structure) can be arbitrarily selected by selecting a certain layer of gate layer and a certain layer of conductor layer, so that the three-dimensional and type flash memory of the present invention has a fast operating speed.
[0009] In order to make the above features and advantages of the present invention more clearly understood, embodiments are given below and described in detail with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] Figures 1A to 1L FIG. 4 is a schematic diagram of a method for manufacturing a three-dimensional flash memory according to an embodiment of the present invention.
[0011] Figure 2 yes Fig. 1I Schematic side view of .
[0012] Figure 3 FIG. 4 is a schematic diagram of a three-dimensional flash memory according to another embodiment of the present invention.
[0013]
Explanation of symbols
[0014] 10, 20: 3D Flash Memory
[0015] 100: Substrate
[0016] 101, 101a, 101b: laminated structure
[0017] 102: First insulation layer
[0018] 104: First sacrificial layer
[0019] 106: First Opening
[0020] 108, 108a, 108b: second insulating layer
[0021] 110, 110a, 110b: second sacrificial layer
[0022] 112: Second opening
[0023] 114: Channel layer
[0024] 116: Insulation column
[0025] 118: Channel
[0026] 120: Side opening
[0027] 122: Gate dielectric layer
[0028] 124: Gate layer
[0029] 126, 126a, 126b: conductor layer
[0030] 128: The third insulation layer
[0031] 130: First contact
[0032] 132: Second contact
[0033] 134: Source line connection line
[0034] 136: Bit line connection line
[0035] D1: First direction
[0036] D2: Second direction
[0037] P: Column structure
[0038] P1: First column structure
[0039] P1': The remaining first column structure
[0040] P2: Second column structure
[0041] R1: Unit area
[0042] R2: Peripheral area DETAILED DESCRIPTION
[0043] In order to make the objectives, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with specific embodiments and with reference to the accompanying drawings.
[0044] Figures 1A to 1L FIG. 4 is a schematic diagram of a method for manufacturing a three-dimensional flash memory according to an embodiment of the present invention. Figure 2 yes Fig. 1I Schematic side view of .
[0045] Please refer to Figure 1A, forming a stacked structure 101 on a substrate 100. The substrate 100 may be, for example, a semiconductor substrate, for example, the substrate 100 may be a silicon substrate. In some embodiments, a doped region (for example, an N+ doped region or an N-type well region) may be formed in the substrate 100 according to design requirements. In other embodiments, a buried oxide layer (not shown) may be further formed on the substrate 100. In this embodiment, the substrate 100 may be defined into a cell region and a peripheral region due to subsequent processes.
[0046] The stacked structure 101 includes a plurality of first insulating layers 102 and a plurality of first sacrificial layers 104 that are alternately stacked. The material of the first insulating layer 102 is, for example, a dielectric material. For example, the material of the first insulating layer 102 may be silicon oxide. The material of the first sacrificial layer 104 is different from the material of the first insulating layer 102 and has a sufficient etching selectivity with the first insulating layer 102. In some embodiments, the material of the first sacrificial layer 104 may be silicon nitride. The first insulating layer 102 and the first sacrificial layer 104 are formed, for example, by performing multiple chemical vapor deposition processes. It should be noted here that the number of layers of the first insulating layer 102 and the first sacrificial layer 104 in the stacked structure 101 is not necessarily determined in increments of 1:1. Figure 1A The embodiment shown is limited to that described above. Specifically, the number of layers of the first insulating layer 102 and the first sacrificial layer 104 may be at least greater than 16, respectively. For example, the number of layers of the first insulating layer 102 and the first sacrificial layer 104 may be 56, 64, or 96. However, the present invention is not limited thereto. The number of layers of the first insulating layer 102 and the first sacrificial layer 104 in the stacked structure 101 may depend on the design and density of the desired three-dimensional flash memory.
[0047] Please refer to Figure 1B , forming a first opening 106 penetrating the stacked structure 101. The first opening 106, for example, has a rectangular outline, that is, the outline from the top to the bottom of the first opening 106 is rectangular. It should be noted here that the rectangular may mean that at least one corner of the rectangle is rounded rather than square, but the present invention is not limited to this, that is, the first opening 106 may also have a rectangular outline. The side of the first opening 106, for example, exposes part of the first insulating layer 102 and the first sacrificial layer 104, and the bottom of the first opening 106, for example, exposes part of the substrate 100. The first opening 106 penetrating the stacked structure 101 may be formed, for example, by performing the following steps. First, a mask layer (not shown) is formed on the stacked structure 101. The mask layer, for example, has an opening with a rectangular outline. Thereafter, the mask layer is used to perform an etching process on the stacked structure 101 to form the first opening 106 in the stacked structure 101. In the present embodiment, the first opening 106 may have a substantially vertical sidewall, and based on this, the first opening 106 is also referred to as a first vertical channel (VC) opening.
[0048] Please refer to Figure 1C , forming a second insulating layer 108 on the sidewall of the first opening 106. The second insulating layer 108 may be, for example, a conformal layer. Specifically, the second insulating layer 108 may conform to the shape of the first opening 106 and cover the first insulating layer 102 and the first sacrificial layer 104 on the sidewall of the first opening 106, and expose a portion of the substrate 100 on the bottom surface of the first opening 106. In other words, the second insulating layer 108 and the first opening 106 have similar shapes and contours. The second insulating layer 108 may, for example, have a material similar to that of the first insulating layer 102. For example, the material of the second insulating layer 108 may be silicon oxide.
[0049] Please continue to refer to Figure 1C , fill the second sacrificial layer 110 in the first opening 106. In the case where the second insulating layer 108 is conformal to the first opening 106, the second sacrificial layer 110 also has, for example, a rectangular outline. In the present embodiment, the second sacrificial layer 110 fills the first opening 106. The second sacrificial layer 110 may, for example, have a material similar to that of the first sacrificial layer 104. For example, the material of the second insulating layer 108 may be silicon nitride. In the present embodiment, the second insulating layer 108 and the second sacrificial layer 110 form a first pillar structure P1, and the second insulating layer 108 surrounds the sidewall of the second sacrificial layer 110.
[0050] Please refer to Figure 1D, forming a second opening 112 that penetrates the stacked structure 101. The second opening 112 has, for example, an elliptical profile, that is, the profile from the top to the bottom of the second opening 112 is elliptical. In the present embodiment, the second opening 112 partially overlaps with the first opening 106, and the extension direction of the long axis of the second opening 112 is orthogonal to the extension direction of the length of the first opening 106. In detail, the second opening 112 formed will not only remove part of the first insulating layer 102 and the first sacrificial layer 104, but also remove part of the first column structure P1. In detail, in the present embodiment, part of the second insulating layer 108 and the second sacrificial layer 110 are removed to form two second insulating layers 108a, 108b and two second sacrificial layers 110a, 110b, respectively, which are the remaining first column structure P1'. Based on this, the side surface of the second opening 112 may be, for example, an exposed portion of the first insulating layer 102, the first sacrificial layer 104, the second insulating layer 108a, 108b, and the two second sacrificial layers 110a, 110b. In addition, the bottom surface of the second opening 112 may be, for example, an exposed portion of the substrate 100. The second opening 112 that penetrates the stacked structure 101 may be formed by, for example, performing the following steps. First, a mask layer (not shown) is formed on the stacked structure 101. The mask layer may have, for example, an opening with an elliptical profile. Thereafter, the stacked structure 101 is etched using the mask layer to form the second opening 112 in the stacked structure 101. In the present embodiment, the second opening 112 may have substantially vertical sidewalls, and based on this, the second opening 112 is also referred to as a second vertical channel (VC) opening.
[0051] Afterwards, please refer to Figure 1E , forming a channel layer 114 on the sidewall of the second opening 112. The channel layer 114 may be, for example, a conformal layer. In detail, the channel layer 114 may conform to the shape of the second opening 112 and cover the first insulating layer 102, the first sacrificial layer 104, the second insulating layer 108a, 108b and the two second sacrificial layers 110a, 110b on the sidewall of the second opening 112, and expose a portion of the substrate 100 on the bottom surface of the second opening 112. In other words, the channel layer 114 and the second opening 112 have similar shapes and contours. The material of the channel layer 114 may be, for example, a semiconductor material. For example, the material of the channel layer 114 may be polysilicon or doped polysilicon. The doped polysilicon may be doped by in-situ doping or ion implantation. The channel layer 114 may be used as a bit line, for example.
[0052] Please continue to refer to Figure 1E, fill the insulating pillar 116 in the second opening 112. In the case where the channel layer 114 is conformal to the second opening 112, the insulating pillar 116 also has an elliptical profile, for example. In the present embodiment, the insulating pillar 116 fills the second opening 112. The insulating pillar 116 may, for example, have a material similar to that of the first insulating layer 102 and the second insulating layer 108. For example, the material of the insulating pillar 116 may be silicon oxide. In the present embodiment, the channel layer 114 and the insulating pillar 116 constitute the second pillar structure P2, and the channel layer 114 surrounds the sidewall of the insulating pillar 116.
[0053] Next, please refer to Figure 1F , after forming the second column structure P2, patterning the stacked structure 101 to form a stepped structure. It is previously explained that after forming the second column structure P2, the unit region R1 and the peripheral region R2 can be defined. In detail, the unit region R1 is formed with the remaining first column structure P1' and the second column structure P2, and the remaining area is the peripheral region R2, and the stepped structure is formed in the peripheral region R2. The formation of the stepped structure is a continuous patterning process of the portion of the stacked structure 101 where the first column structure P1 and the second column structure P2 are not formed. From another perspective, the distance that the first insulating layer 102 and the first sacrificial layer 104 protrude from the unit region R1 decreases as they gradually move away from the substrate 100. Afterwards, a planarization process ( Figure 1F In other words, the step structure is filled with an insulating layer ( Figure 1F (not shown) to form a surface with planarization.
[0054] Afterwards, please refer to Figure 1G , forming a channel 118 penetrating the stacked structure 101. In the present embodiment, the channel 118 is formed along the formation direction of the step structure to divide the stacked structure 101 into a pair of stacked structures 101a and 101b. The channel 118, for example, exposes the first insulating layer 102 and the first sacrificial layer 104 on the side walls of the pair of stacked structures 101a and 101b facing each other. The formation of the channel 118 penetrating the stacked structure 101 may, for example, be performed by performing the following steps. First, a mask layer (not shown) is formed on the stacked structure 101. Thereafter, an etching process is performed on the stacked structure 101 using the mask layer to form the channel 118 in the stacked structure 101. In some embodiments, a portion of the substrate 100 is also removed simultaneously after the channel is formed.
[0055] Next, please refer to Figure 1H , removing the first sacrificial layer 104 exposed by the lateral opening 120 to form the lateral opening 120. The lateral opening 120, for example, exposes a portion of the second insulating layer 108a, 108b and the channel layer 114. Figure 2. The method of removing the first sacrificial layer 104 exposed by the lateral opening 120 is, for example, dry etching or wet etching, wherein the etchant used in the dry etching is, for example, NF3, H2, HBr, O2, N2, He or a combination thereof, and the etchant used in the wet etching is, for example, phosphoric acid (H3PO4) solution. In the present embodiment, the wet etching method is used to remove the first sacrificial layer 104 exposed by the lateral opening 120.
[0056] Afterwards, please also refer to Fig. 1I as well as Figure 2 , forming a gate dielectric layer 122 in the lateral opening 120. The gate dielectric layer 122 may be, for example, a conformal layer. Specifically, the gate dielectric layer 122 may conform to the shape of the lateral opening 120 and cover the second insulating layers 108a, 108b and the channel layer 114 exposed through the lateral opening 120. Figure 2 As shown. In addition, the gate dielectric layer 122 needs to have good step coverage to obtain good film thickness uniformity. The material of the gate dielectric layer 122 may be, for example, oxide, nitride or a combination thereof. In some embodiments, the gate dielectric layer 122 includes an oxide-nitride-oxide (ONO) composite layer. For example, the gate dielectric layer 122 may include a composite layer consisting of a silicon oxide layer, a silicon nitride layer and a silicon oxide layer. In other embodiments, the gate dielectric layer 122 may include an oxide-nitride-oxide-nitride-oxide (ONONO) composite layer. For example, the gate dielectric layer 122 may include a composite layer consisting of a silicon oxide layer, a silicon nitride layer, a silicon oxide layer, a silicon nitride layer and a silicon oxide layer. In addition, in some embodiments, the gate dielectric layer 122 may be further formed on the side walls of the first insulating layer 102 facing each other in a pair of stacked structures 101a, 101b.
[0057] Afterwards, please refer to Figure 1J , a gate layer 124 is filled in the lateral opening 120. The material of the gate layer 124 may be, for example, polysilicon, amorphous silicon, tungsten (W), cobalt (Co), aluminum (Al), tungsten silicide (WSi x ) or cobalt silicide (CoSi x). The method of forming the gate layer 124 may be, for example, chemical vapor deposition. In the present embodiment, the gate layer 124 may be used as a word line. In some embodiments, before filling the gate layer 124 in the lateral opening 120, a buffer layer (not shown) and a barrier layer (not shown) may be sequentially formed in the lateral opening 120. The material of the buffer layer may be, for example, a high dielectric constant material having a dielectric constant greater than 7. For example, the material of the buffer layer may be aluminum oxide (Al2O3), hafnium oxide (HfO2), lanthanum oxide (La2O5), transition metal oxide, lanthanide oxide or a combination thereof. The method of forming the buffer layer may be, for example, chemical vapor deposition or atomic layer deposition. The material of the barrier layer may be, for example, titanium (Ti), titanium nitride (TiN), tantalum (Ta), tantalum nitride (TaN) or a combination thereof. The method of forming the barrier layer may be, for example, chemical vapor deposition.
[0058] Please refer to Figure 1K , the second sacrificial layers 110a and 110b are replaced by the conductor layer 126, for example, by the following steps. First, the second sacrificial layers 110a and 110b are removed by dry etching or wet etching to form a third opening (not shown). Then, the conductor layer 126 is filled in the third opening. The material of the conductor layer 126 may be, for example, polysilicon, doped polysilicon or other conductive metal materials. In the present embodiment, the conductor layer 126 may be used as a source layer or a drain layer. For example, the conductor layer 126 replacing the second sacrificial layer 110a is used as a source layer, and the conductor layer 126 replacing the second sacrificial layer 110b is used as a drain layer, but the present invention is not limited thereto. The cross-sectional area of the conductor layer 126 replacing the second sacrificial layer 110a and the conductor layer 126 replacing the second sacrificial layer 110b may be the same or different, and the present invention is not particularly limited thereto. The method for forming the source layer / drain layer of the present embodiment uses the conductor layer 126 to replace the first formed second sacrificial layers 110a and 110b, which is a self-alignment process, and therefore has the effects of simple process and high process yield. In addition, the formed source layer / drain layer has substantially the same distance from the gate layer 124 because the second insulating layers 108a and 108b conforming to the source layer / drain layer are respectively disposed on the periphery thereof, so that the three-dimensional and type flash memory 10 of the present embodiment can operate stably.
[0059] In addition, before the second sacrificial layers 110a and 110b are replaced by the conductive layer 126, the third insulating layer 128 may be first filled in the trench 118. The third insulating layer 128, for example, covers the gate dielectric layer 122 and the gate layer 124 on the facing sidewalls of the pair of stacked structures 101a and 101b.
[0060] Finally, please refer to Figure 1L, forming a first contact 130 electrically connected to the conductor layer 126 located in the unit region R1 and a second contact 132 electrically connected to the gate layer 124 (which is a step structure) located in the peripheral region R2. For example, a first contact 130 is correspondingly disposed on each conductor layer 126, and a second contact 132 is correspondingly disposed on each step gate layer 124. Next, a source line connection line 134 and a bit line connection line 136 are formed. The source line connection line 134, for example, electrically connects the conductor layers 126 as source layers in a pair of stacked structures 101a and 101b through the first contact 130, and the bit line connection line 136, for example, also electrically connects the conductor layers 126 as drain layers in a pair of stacked structures 101a and 101b through the first contact 130. The material of the source line connection line 134 and the bit line connection line 136 can be, for example, a metal material.
[0061] At this point, the manufacturing of the three-dimensional flash memory 10 of the present invention is completed.
[0062] Although the manufacturing method of the 3D 3D flash memory 10 of the present embodiment is described by taking the above method as an example, the manufacturing method of the 3D 3D flash memory 10 of the present invention is not limited thereto.
[0063] Please continue to refer to Figure 1L , Figure 1L A schematic diagram of a three-dimensional and type flash memory according to an embodiment of the present invention is depicted. The three-dimensional and type flash memory 10 according to the embodiment of the present invention includes a substrate 100, a stacked structure 101 and a pillar structure P, wherein the pillar structure P penetrates the stacked structure 101. The substrate 100, for example, has a cell region R1 and a peripheral region R2, wherein the pillar structure P is located in the cell region, and a step structure is formed in the peripheral region R2. The stacked structure 101 is located on the substrate 100 and, for example, includes a pair of stacked structures 101a and 101b. A third insulating layer 128 may be provided between the pair of stacked structures 101a and 101b, for example. In one embodiment, the stacked structure 101 includes first insulating layers 102 and gate layers 124 that are alternately provided. The first insulating layer 102 and the gate layer 124 may form a step structure, for example, in the peripheral region R2 with the portion protruding from the cell region R1. In this embodiment, a gate dielectric layer 122 is provided between the first insulating layer 102 and the gate layer 124. It should be noted here that the gate dielectric layer 122 is not only disposed between the first insulating layer 102 and the gate layer 124. In detail, the gate dielectric layer 122 can be further disposed on the sidewalls of the first insulating layer 102 in a pair of stacked structures 101a and 101b that face each other. In addition, the gate dielectric layer 122 can be further disposed on the sidewalls of the column structure P exposed by the first insulating layer 102, that is, the gate dielectric layer 122 surrounds the sidewalls of the column structure P exposed by the first insulating layer 102.
[0064] In one embodiment, the column structure P includes an insulating column 116, a channel layer 114, a conductor layer 126, and second insulating layers 108a and 108b. The insulating column 116, for example, has an elliptical profile, that is, the profile from the top to the bottom of the insulating column 116 is elliptical. The channel layer 114 surrounds the insulating column 116 and conforms to the insulating column 116. The conductor layer 126 is located on both sides of the channel layer 114 and contacts the channel layer 114. In other words, the conductor layer 126 may include two conductor layers 126a and 126b, each located on opposite sides of the channel layer 114, and each may serve as a source and a drain. In this embodiment, the conductor layer 126 faces the long axis section of the insulating column 116. The second insulating layers 108a and 108b, for example, each surround the sidewall of the conductor layer 126 that is not in contact with the channel layer 114.
[0065] The three-dimensional AND type flash memory 10 of the embodiment of the present invention may further include a first contact 130, a second contact 132, a source line connection line 134, and a bit line connection line 136. The first contact 130 is, for example, located on the cell region R1 and electrically connected to the conductor layer 126, and the second contact 132 is, for example, located on the peripheral region R2 and electrically connected to the gate layer 124. The source line connection line 134, for example, electrically connects the conductor layers 126 as source layers in a pair of stacked structures 101a and 101b through the first contact 130, and the bit line connection line 136, for example, also electrically connects the conductor layers 126 as drain layers in a pair of stacked structures 101a and 101b through the first contact 130.
[0066] In the present embodiment, there are multiple pillar structures P and they are separated from each other. The pillar structures P are, for example, arranged in sequence along the first direction D1 and arranged alternately in the second direction D2, wherein the second direction D2 is orthogonal to the first direction D1. Since the multiple pillar structures P are separated from each other, each pillar structure P has an independent source and drain (conductor layer 126), therefore, a storage unit (the intersection of the gate layer 124 and the pillar structure P) can be arbitrarily selected by selecting a certain layer of gate layer 124 and a certain layer of conductor layer 126, so that the three-dimensional and type flash memory 10 of the present embodiment has a fast operating speed.
[0067] Figure 3 FIG. 1 is a schematic diagram of a three-dimensional flash memory according to another embodiment of the present invention. It should be noted that: Figure 3 The implementation examples are used Figure 1L The component numbers and partial contents of the embodiments are the same or similar numbers are used to represent the same or similar components, and the description of the same technical contents is omitted. For the description of the omitted parts, please refer to the description and effects of the above embodiments, and the following embodiments will not be repeated. Figure 3 For at least a portion of the description of the embodiments that is not omitted, please refer to the subsequent content.
[0068] The difference between the three-dimensional AND type flash memory 20 of the present embodiment and the three-dimensional AND type flash memory 10 of the above-mentioned embodiment is that the plurality of pillar structures P are not arranged in the first direction D1, and each pillar structure P includes a plurality of insulating pillars 116, a plurality of channel layers 114, a plurality of conductor layers 126, and a plurality of second insulating layers 108a, 108b. In detail, since a pillar structure P has a plurality of insulating pillars 116 and a plurality of channel layers 114, most of the conductor layers 126 will contact two adjacent channel layers 114 in the first direction D1, so that it has a profile similar to the shape of a candied haws. In addition, the plurality of pillar structures P are separated from each other in the second direction D2, and each pillar structure P has a plurality of sharable source and drain electrodes (conductor layers 126), so that a storage unit (the intersection of the gate layer 124 and the pillar structure P) can be arbitrarily selected by selecting a certain layer of gate layer 124 and two certain conductor layers 126, so that the three-dimensional AND type flash memory 20 of the present embodiment has a fast operating speed. In addition, since the source and the drain (conductive layer 126 ) of each pillar structure P can be shared by adjacent memory cells, the size of the 3D flash memory 20 can be further reduced.
[0069] In summary, in the above embodiment, by sequentially forming the first pillar structure and the second pillar structure, the position where the source layer / drain layer is to be formed can be defined, so that the source layer / drain layer can be formed by a simple process with a high process yield, and the formed source layer / drain layer has substantially the same distance as the gate layer due to the conformal second insulating layer, so that the three-dimensional AND type flash memory of the present invention can be stably operated. In addition, in the three-dimensional AND type flash memory of the present invention, each pillar structure has an independent conductor layer, so that the storage unit (the intersection of the gate layer and the pillar structure) can be arbitrarily selected by selecting a certain layer of the gate layer and a certain layer of the conductor layer, so that the three-dimensional AND type flash memory of the present invention has a fast operating speed.
[0070] The specific embodiments described above further illustrate the objectives, technical solutions and beneficial effects of the present invention in detail. It should be understood that the above description is only a specific embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A method for manufacturing a three-dimensional flash memory, comprising: forming a stacked structure on a substrate, wherein the stacked structure comprises a first insulating layer and a first sacrificial layer that are alternately stacked; Forming a first column structure penetrating the stacked structure and having a rectangular outline, wherein the first column structure includes a second insulating layer and a second sacrificial layer, and the second insulating layer surrounds the second sacrificial layer, and the rectangular outline means that at least one corner of the rectangle is rounded instead of square; forming a second column structure penetrating the stacked structure and having an elliptical profile, wherein the second column structure comprises a channel layer and an insulating column, the channel layer surrounds the insulating column, and the second sacrificial layer is located on both sides of the channel layer and contacts the channel layer, wherein the second sacrificial layer faces a long axis section of the second column structure; removing the first sacrificial layer to form a lateral opening, wherein the lateral opening exposes a portion of the second insulating layer and a portion of the channel layer; forming a gate dielectric layer in the lateral opening, wherein the gate dielectric layer surrounds the exposed second insulating layer and the channel layer; Filling a gate layer into the lateral opening; as well as The second sacrificial layer is replaced with a conductive layer.
2. The method for manufacturing a three-dimensional flash memory according to claim 1, wherein the step of forming the first pillar structure comprises: forming a first opening penetrating the stacked structure, wherein the first opening has a rectangular-like outline; forming the second insulating layer on the sidewalls of the first opening; as well as The second sacrificial layer is filled in the first opening.
3. The method for manufacturing a three-dimensional flash memory according to claim 1 , wherein the step of forming the second pillar structure comprises: forming a second opening penetrating the stacked structure, wherein the second opening has an elliptical profile, and the second insulating layer and the second sacrificial layer are partially removed; forming the channel layer on the sidewall of the second opening; as well as Fill the insulating column into the second opening.
4. The method for manufacturing a three-dimensional flash memory according to claim 1 , wherein the step of removing the first sacrificial layer to form the lateral opening comprises: forming a channel penetrating the stacked structure, wherein the channel exposes the first sacrificial layer; as well as The first sacrificial layer is laterally etched. 5 . The method for manufacturing a three-dimensional flash memory according to claim 4 , wherein after the gate layer is filled in the lateral opening, a third insulating layer is filled in the channel.
6. A three-dimensional flash memory, comprising: A stacked structure, located on a substrate and comprising first insulating layers and gate layers alternately arranged, wherein a gate dielectric layer is arranged between the first insulating layers and the gate layers; as well as The column structure runs through the stacked structure and includes: an insulating column having an oval profile; a channel layer surrounding the insulating column; a conductor layer, located on both sides of the channel layer and in contact with the channel layer, wherein the conductor layer faces the long axis section of the insulating column; and a second insulating layer surrounding the sidewall of the conductor layer not in contact with the channel layer, The gate dielectric layer surrounds the sidewalls of the pillar structure exposed by the first insulating layer. 7 . The three-dimensional flash memory according to claim 6 , comprising a pair of the stacked structures, wherein a third insulating layer is disposed between the pair of stacked structures. 8 . The three-dimensional flash memory according to claim 7 , wherein the gate dielectric layer is disposed on the sidewalls of the first insulating layer facing each other in the pair of stacked structures. 9 . The three-dimensional flash memory according to claim 6 , wherein the column structure is multiple, and the column structures are arranged in sequence in a first direction and staggered in a second direction orthogonal to the first direction.
10. The three-dimensional flash memory according to claim 6, wherein the column structure is multiple, each column structure comprises multiple insulating columns, multiple channel layers, multiple conductor layers and multiple second insulating layers, wherein: In a first direction, one conductor layer is formed between two adjacent channel layers among the plurality of channel layers, and the plurality of column structures are separated from each other in a second direction orthogonal to the first direction.