Power semiconductor devices

By arranging a recess at the connection between the conductor and the insulating substrate, the strain of the solder is reduced, which solves the problem of fatigue damage of the connecting material in the power semiconductor device due to repeated heating, improves the reliability of the device and suppresses the increase in thermal resistance.

CN113039636BActive Publication Date: 2024-10-29HITACHI AUTOMOTIVE SYST LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN201980074479.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-11-05
Publication Date
2024-10-29
Estimated Expiration
2039-11-05

AI Technical Summary

Technical Problem

In power semiconductor devices, the connecting material undergoes large strains due to repeated heating, which may cause fatigue damage and affect the reliability of the device.

Method used

A recess is provided at the connection between the conductor and the insulating substrate so that the thickness of the connection material is thicker at the periphery than at other parts, thereby reducing the strain of the solder, reducing the possibility of fatigue damage, and reducing thermal resistance by optimizing the shape and position of the recess.

Benefits of technology

It effectively reduces the strain of the solder, improves the reliability of the power semiconductor device, prevents fatigue damage, and avoids an increase in thermal resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113039636B_ABST
    Figure CN113039636B_ABST
Patent Text Reader

Abstract

The power semiconductor device of the present invention includes: an insulating substrate, a first conductor layer is arranged on one surface of the insulating substrate; a first conductor, the first conductor is connected to the first conductor layer via a first connecting material; and a semiconductor element, the semiconductor element is connected to the first conductor via the first connecting material, when viewed from a right angle to the electrode surface of the semiconductor element, the first conductor has a peripheral portion formed to be larger than the semiconductor element, and a first recess is formed in the peripheral portion for making the thickness of the first connecting material thicker than other portions.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a power semiconductor device, and in particular to a power semiconductor device used in a power conversion device for controlling a motor for driving a vehicle, but can also be applied to power conversion devices for railways, elevators, industrial equipment, aircraft, etc. Background Art

[0002] In power conversion devices for hybrid vehicles and electric vehicles, a power semiconductor device with a high operating voltage is desired for the purpose of shortening the charging time. In a power semiconductor device with a high operating voltage, an insulating component such as a ceramic substrate with a high insulation withstand voltage needs to be used as an insulating component. As a power semiconductor device using a ceramic substrate as an insulating material, for example, Patent Document 1 is disclosed.

[0003] On the other hand, there is a demand for miniaturization and cooling performance of power conversion devices. For example, as shown in Patent Document 2, a power semiconductor device of a double-side direct cooling system is disclosed.

[0004] Prior art literature

[0005] Patent Literature

[0006] Patent Document 1: Japanese Patent Laid-Open No. 10-189845

[0007] Patent Document 2: Japanese Patent Application Publication No. 2012-257369 Summary of the invention

[0008] Technical problem to be solved by the invention

[0009] In a power semiconductor device that uses a connecting material such as solder to connect a conductor plate to an insulating substrate such as ceramic, when the power semiconductor element repeatedly generates heat (the power semiconductor device is repeatedly operated and stopped), there is a concern that fatigue damage may occur due to repeated application of large strain to the connecting material.

[0010] In particular, the connection material connecting the conductor plate and the insulating substrate has a large temperature rise and a large area, so the strain of the connection material increases, which may cause fatigue failure.

[0011] An object of the present invention is to provide a power semiconductor device with high reliability.

[0012] Technical solutions adopted to solve technical problems

[0013] In order to solve the above-mentioned problem, the power semiconductor device according to the present invention includes: an insulating substrate, a first conductor layer is arranged on one surface of the insulating substrate; a first conductor, the first conductor is connected to the first conductor layer via a first connecting material; and a semiconductor element, the semiconductor element is connected to the first conductor via a second connecting material. Moreover, when viewed from a right angle direction of an electrode surface of the semiconductor element, the first conductor has a peripheral portion formed larger than the semiconductor element, and the peripheral portion is formed with a first recessed portion for making the thickness of the first connecting material thicker than other portions.

[0014] Effects of the Invention

[0015] According to the present invention, a highly reliable power semiconductor device can be realized. Technical problems, structures, and effects other than the above will become more apparent from the following description of the embodiments. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 It is a cross-sectional view of the power semiconductor device according to the first embodiment of the present invention.

[0017] Figure 2 This is a diagram showing the comparison results of solder strain.

[0018] Figure 3 It is a cross-sectional view of the power semiconductor device according to the first embodiment of the present invention.

[0019] Figure 4 It is a cross-sectional view of a power semiconductor device according to a second embodiment of the present invention.

[0020] Figure 5 It is a cross-sectional view of a power semiconductor device according to a third embodiment of the present invention.

[0021] Figure 6 It is a cross-sectional view of a power semiconductor device according to a fourth embodiment of the present invention.

[0022] Figure 7 It is a cross-sectional view of a power semiconductor device according to a fifth embodiment of the present invention.

[0023] Figure 8 It is a cross-sectional view of a power semiconductor device according to a sixth embodiment of the present invention.

[0024] Fig. 9 It is a cross-sectional view of a power semiconductor device according to a seventh embodiment of the present invention.

[0025] Fig.10 It is a cross-sectional view of a power semiconductor device according to another embodiment of the present invention.

[0026] Fig.11This is an external view of a power semiconductor device according to Embodiment 1 of the present invention.

[0027] Fig.12 It is a developed perspective view of the power semiconductor device according to the first embodiment of the present invention.

[0028] Fig.13 This is a front view of the power semiconductor device according to the first embodiment of the present invention.

[0029] Fig.14 It is a front view of a power semiconductor device according to a seventh embodiment of the present invention.

[0030] FIG. 15( a ) is a diagram showing a manufacturing process of a power semiconductor device according to an embodiment of the present invention.

[0031] FIG. 15( b ) is a diagram showing a manufacturing process of the power semiconductor device according to the embodiment of the present invention.

[0032] FIG. 15( c ) is a diagram showing a manufacturing process of the power semiconductor device according to the embodiment of the present invention.

[0033] FIG. 15( d ) is a diagram showing a manufacturing process of the power semiconductor device according to the embodiment of the present invention.

[0034] FIG. 16( a ) is a graph showing the ratio of the concave portion width / the concave portion depth.

[0035] FIG. 16( b ) is a graph showing the relationship between the ratio of the recess width / the recess depth and the solder strain.

[0036] Fig.17 It is a cross-sectional view of a power semiconductor device according to a fifth embodiment of the present invention.

[0037] Fig.18 It is a cross-sectional view of a power semiconductor device according to an eighth embodiment of the present invention. DETAILED DESCRIPTION

[0038] [Implementation Method 1]

[0039] Fig.13 It is a front view of the power semiconductor device according to the present embodiment. Fig.12 It is a developed perspective view of the power semiconductor device according to the first embodiment of the present invention. Figure 1 It is a cross-sectional view of the power semiconductor device according to the first embodiment of the present invention. Figure 1 express Fig.12 A portion of the cross section at AA' in FIG.

[0040] Below, refer to Figure 1An embodiment of a power semiconductor device according to the present invention is described below. Figure 1 As shown, in the power semiconductor device of this embodiment, the power semiconductor element 1 is sandwiched by the first conductor 3 and the second conductor 4 arranged opposite to the electrode surface of each electrode. The power semiconductor element 1 and the first conductor 3 and the second conductor 4 are respectively connected by the connecting material 2. The first conductor 3 and the second conductor 4 are formed of, for example, copper, copper alloy or aluminum, aluminum alloy, etc., and the connecting material 2 is formed of solder, sintered material, etc. In addition, Figure 1 , the first conductor 3 is shown as being formed by a single member, but it may also be formed by joining a plurality of members. The insulating substrate 5 is composed of an insulating member 5a, a first conductor layer 5b, and a second conductor layer 5c. The first conductor layer 5b is arranged on one surface of the insulating member 5a, and the second conductor layer 5c is arranged on the other surface. The surface of the first conductor 3 opposite to the surface connected to the power semiconductor element 1 is connected to the first conductor layer 5b via a connecting material 6. The second conductor layer 5c is connected to the heat dissipation member 8 via a connecting material 7. Heat dissipation fins 9 are formed on the surface of the heat dissipation member 8.

[0041] Similarly, the surface of the second conductor 4 opposite to the surface connected to the power semiconductor element 1 is connected to the first conductor layer 5b via the connecting material 6. In the insulating substrate 5, the first conductor layer 5b is arranged on one surface of the insulating member 5a, and the second conductor layer 5c is arranged on the other surface. The second conductor layer 5c is connected to the heat dissipation member 8 via the connecting material 7. Heat dissipation fins 9 are formed on the surface of the heat dissipation member 8. The insulating member 5a conducts the heat generated from the power semiconductor element 1 to the heat dissipation member 8, and it is preferable to use a material with high thermal conductivity and high insulation withstand voltage. For example, ceramics such as aluminum oxide (aluminum oxide), aluminum nitride, silicon nitride, etc. can be used. The connecting material 6 and the connecting material 7 are formed of solder, sintered materials, etc. The heat dissipation member 8 and the heat dissipation fins 9 are formed of a conductive member, such as Cu, Cu alloy, Cu-C, Cu-CuO and other composite materials or Al, Al alloy, AlSiC, Al-C and other composite materials. As Fig.12 As shown, the terminal 14 is connected to the first conductor layer 5b. Fig.11 FIG. 1 is an external view of a power semiconductor device according to Embodiment 1 of the present invention. Fig.11 As shown, the portion other than the heat dissipation surface 8 a where the heat dissipation fins of the heat dissipation member 8 are formed and a portion of the terminal 14 is sealed with a sealing resin 10 .

[0042] With the above structure, the heat generated by the power semiconductor element 1 can be thermally conducted to the insulating substrate 5 via the first conductor 3 and the second conductor 4, and the heat can be effectively dissipated to the outside via the heat dissipation member 8. In addition, since ceramics with high insulation withstand voltage are used as the insulating substrate 5, a power semiconductor device with high operating voltage can be realized. However, in a power semiconductor device in which the insulating substrate 5 such as ceramics is connected to the first conductor 3 and the second conductor 4 using a connecting material 6 such as solder, when the power semiconductor element 1 repeatedly generates heat (when the power semiconductor device is repeatedly operated and stopped), large strain is repeatedly applied to the connecting material 6, so there is a concern that fatigue damage may occur.

[0043] exist Figure 1 In the power semiconductor device shown, there are three kinds of bonding interfaces such as solder. They are the connection material 2 on the upper and lower surfaces of the chip, the connection material 6 connecting the first conductor and the second conductor with the insulating substrate 5, and the connection material 7 connecting the insulating substrate 5 with the heat dissipation component 8. In the process of repeated operation and stop of the power semiconductor device, the connection material 6 has the largest strain and is the main cause of fatigue life. The reason is that although the temperature rise of the connection material 2 is large when the power semiconductor device is in operation, the strain is small due to the small contact area. In addition, although the contact area of ​​the connection material 7 is large, it is arranged near the heat dissipation component 8, so the temperature rise is small and the strain is small. On the other hand, since the temperature rise of the connection material 6 is also large and the connection area is also large, the strain becomes larger and the possibility of fatigue damage becomes higher. Therefore, in this embodiment, recesses 3a and 4a are provided on the peripheral portions of the surfaces of the first conductor 3 and the second conductor 4 that are soldered to the insulating substrate 5.

[0044] Figure 2 This is a diagram showing the results of comparing the strain of the connection material 6 when the power semiconductor element 1 is heated when the connection material 6 is made of solder in the case where there are recesses 3a and 4a and in the case where there are no recesses 3a and 4a. In the temperature distribution when the active region of the power semiconductor device is heated, the stress when the temperature distribution occurs is evaluated using the equivalent plastic strain that dominates the fatigue damage of the solder. The maximum value of the strain near the end of the second conductor 4 of the connection material 6 is used for comparison. As a result, as shown in FIG. Figure 2As shown, it was confirmed that when the strain of the solder of the structure without the recess was set to 1, the strain of the solder could be reduced to 0.61 in the case of the recess. This is because the thickness of the connecting material (solder thickness) at the end of the connecting material 6 is increased by providing the recess, so it is considered that the solder strain is reduced. Therefore, in the peripheral portion of the first conductor 3, the connecting material 6 is formed thicker than other portions, so that the strain of the solder can be reduced. Therefore, in this embodiment, since the strain of the solder connecting material 6 that generates heat when the power semiconductor element 1 is repeatedly heated (power cycle) can be reduced, a power semiconductor device that prevents fatigue damage and has high reliability is provided.

[0045] Here, the thermal conductivity of the solder is greater than that of the first conductor 3 and the second conductor 4. Therefore, when the thickness of the connection material 6 composed of the solder increases, the thermal resistance increases and the heat dissipation decreases. Therefore, by providing a recessed portion at a position of the first conductor 3 and the second conductor 4 away from the power semiconductor element 1, the thermal conductivity will not be deteriorated when the chip is heated, and the solder thickness of the connection material 6 can be increased only at the ends of the first conductor 3 and the second conductor 4 where the strain becomes high, thereby reducing the strain. Since the thickness of the solder outside the recessed portion is relatively thinner than the surrounding area, the increase in thermal resistance can be suppressed, fatigue damage of the solder can be prevented, and a power semiconductor device with high reliability can be realized.

[0046] In addition, it is preferable to consider the diffusion of the heat of the chip from the end of the power semiconductor element 1 when providing the recessed portion 4 a . Figure 3 is a cross-sectional view of a power semiconductor device according to Embodiment 1 of the present invention. Figure 3 As shown, the angle between the line from the intersection of the second conductor 4 and the end of the connecting material 2 toward the outside on the surface of the second conductor 4 and the line 4b connecting the intersection of the second conductor 4 and the end of the connecting material 2 and the intersection 4d of the second conductor 4 and the bonding surface 4c of the insulating substrate 5 is set to 45 degrees. At this time, it is preferable to set the position of the recess 4a to the outside of the intersection 4d. That is, when viewed from the right angle direction of the electrode surface of the semiconductor element 1, the recess 4a is formed between the virtual line and the outer periphery of the first conductor 3, wherein the virtual line is composed of a collection of points separated from the end of the semiconductor element 1 by a distance equivalent to the thickness of the first conductor 3. As a result, the deterioration of thermal resistance can be suppressed, and thus a power semiconductor device with higher reliability can be provided.

[0047] As described above, by deepening the recess depth, the solder thickness can be increased, and the strain of the solder can be reduced. At this time, it is preferred that the recess width is set to more than twice the recess depth. Figure 16 (b) is a diagram showing the relationship between the ratio of recess width / recess depth and solder strain. The solder strain during power cycling of a structure in which the ratio of recess width to recess depth is changed was evaluated. Each value represents the solder strain value after normalizing the solder strain in the case of recess width / recess depth = 1 as 1. As shown in Figure 16 (b), in an area where the value of recess width / recess depth is less than 2, the strain of the solder increases as the value of recess width / recess depth decreases. Generally speaking, the strain of the solder is reduced by increasing the thickness of the solder, but if the recess depth is only deepened, the effect cannot be fully obtained. In order to fully obtain the effect of reducing solder strain by forming a recess, it is preferred to form the value of recess width / recess depth to be greater than 2. Therefore, when the shapes of the recesses 3a and 4a are viewed from a direction perpendicular to the electrode surface of the semiconductor element 1, in the recesses 3a and 4a, when the length in the width direction parallel to the electrode surface of the semiconductor element 1 is defined as W and the length in the depth direction is defined as D, W / D is formed to be greater than 2.

[0048] Here, in Figure 6 In the case of the power semiconductor device structure with single-side cooling shown in the embodiment, when the chip is heated, warping deformation occurs in the direction of reducing the strain of the solder of the connection material 6. On the other hand, in the power semiconductor device with double-side cooling structure shown in the present embodiment, deformation increases the strain of the solder of the connection material 6. Therefore, the solder strain when the chip is heated becomes larger in the double-side cooling structure shown in the present embodiment. Therefore, the solder strain reduction effect of the recessed portion 4a provided in the second conductor 4 becomes larger.

[0049] In addition, in this embodiment, the case where the connection material is solder is shown, but other connection materials such as sintered materials may also be used.

[0050] [Implementation Method 2]

[0051] Figure 4 2 is a cross-sectional view showing a power semiconductor device according to a second embodiment of the present invention. When manufacturing a power semiconductor device, warping occurs due to a difference in thermal conductivity between the insulating substrate 5 and the heat dissipation member 8. Due to this warping, strain may be generated in the connection material 7, and the connection material 7 may be damaged. In this embodiment, Figure 4As shown, a recess 8d is provided on the surface 8b of the heat dissipation member 8 on which the insulating substrate 5 is mounted. Thus, by increasing the thickness of the connection material (solder thickness) at the end of the connection material 7, strain can be reduced and damage to the connection material 7 can be prevented. The position where the recess 8d is provided can be provided outside the intersection 8e, wherein the intersection 8e is the intersection of a perpendicular line from the end of the second conductor 4 to the heat dissipation material 8 and the insulating substrate mounting surface 8b of the heat dissipation member. In addition, the position where the recess 8d is provided can be provided outside the intersection 8c, wherein the intersection 8c is the intersection of a line 4b at 45 degrees to the end of the power semiconductor element 1 and the insulating substrate mounting surface 8b of the heat dissipation member. With such a structure, a power semiconductor device with high reliability that suppresses deterioration of thermal resistance can be provided.

[0052] [Implementation method 3]

[0053] In the first embodiment, one semiconductor element 1 is provided on the first conductor 3, but a plurality of semiconductor elements 1 may be provided on the first conductor 3. This can reduce the length in the width direction compared to a semiconductor device in which one semiconductor element is arranged, and can provide a more compact power semiconductor device.

[0054] Figure 5 FIG. 2 is a cross-sectional view showing a power semiconductor device according to the present embodiment. Figure 5 As shown in the figure, in this embodiment, the first conductor 3 and the third conductor 11 are welded separately so as to be adjacent to each other on the same surface of the insulating substrate 5. Similarly, the second conductor 4 and the fourth conductor 12 are welded to the first conductor 4. In such a power semiconductor device, the connecting material 6 and the connecting material 13 of the adjacent conductors may overflow and cause bridging. In particular, in the case of a double-sided cooling module, when forming the sealing resin 10, since it is pressurized from both sides at a high temperature, the connecting material 6 and the connecting material 13 are likely to overflow and bridge.

[0055] Therefore, in this embodiment, recesses 3a, 4a, 11a, and 12a are provided on the outer periphery of the connection surface of the first conductor 3, the second conductor 4, the third conductor 11, and the fourth conductor 12 with the insulating substrate 5. Thus, the solder pressed out from the center to the outside flows into each recess, so that overflow of the solder can be prevented. Therefore, the connection material 6 and the connection material 13 of the adjacent conductors can be prevented from overflowing and bridging, and reliability and assembly performance can be improved.

[0056] [Implementation Method 4]

[0057] exist Figure 1In the first embodiment shown, an example of a power semiconductor device with a double-sided cooling structure is shown, that is, a first conductor 3 and a second conductor 4 are connected to the front and back surfaces of a power semiconductor element 1 through a connecting material 2, and an insulating substrate 5 and a heat dissipation member 8 are further connected to the outer sides thereof through connecting materials 6 and 7, respectively. Figure 6 As shown, a power semiconductor device with a single-sided cooling structure may also be used. The power semiconductor element 1 is connected to the second conductor 4 via the connecting material 2. In addition, the power semiconductor element 1 is connected to the first conductor layer 5b of the insulating substrate 5 via the connecting material 6, and the second conductor layer 5c of the insulating substrate 5 is connected to the heat dissipation member 8. Here, in the case of such a structure, since the difference in thermal expansion coefficient between the first conductor 3 and the insulating substrate 5 becomes large, even in a power semiconductor device with a single-sided cooling structure, there is a problem that the strain of the connecting material 6 becomes large.

[0058] Therefore, the recessed portion 4a is provided at the peripheral portion of the surface of the second conductor 4 to be soldered to the insulating substrate 5. As a result, the thickness of the connection material 6 is thicker at the peripheral portion of the second conductor 4 than at other portions, so that the strain of the solder can be reduced. In addition, since the thickness of the solder outside the recessed portion 4a is relatively thinner than that of the peripheral portion, the thermal resistance is not increased, fatigue damage of the solder can be prevented, and a highly reliable power semiconductor device can be realized.

[0059] [Implementation method 5]

[0060] Figure 7 FIG. 1 is a cross-sectional view showing a power semiconductor device according to a fifth embodiment of the present invention. Figure 1 In the first embodiment shown in the figure, the shape of the recessed portion 3a and the recessed portion 4a provided at the peripheral portion of the surface of the first conductor 3 and the second conductor 4 to be welded to the insulating substrate 5 is shown as a step-shaped example. However, when the shape of the recessed portion 3a and the recessed portion 4a is a step-shaped shape, there is a possibility that the connection material 6 cannot be buried in the corner of the step and a gap is generated. Therefore, in this embodiment, Figure 7 As shown, the shape of the recess is formed into a conical shape like the recess 3e and the recess 4e. That is, when viewed from a right angle to the electrode surface of the semiconductor element 1, the depth of the recess 3e and the recess 4e is formed so that the side away from the semiconductor element 1 is larger than the side close to the semiconductor element 1.

[0061] By making the recessed portion 3e and the recessed portion 4e tapered, the thickness of the solder becomes thinner on the inner side which affects the heat conduction, so the influence on the thermal resistance is smaller than that of making the recessed portion into a step shape. In addition, the tapered shape is easier to process than the step shape. In addition, it is possible to prevent the generation of a gap between the first conductor 3 and the connecting material 6 and the decrease in the adhesion of the solder.

[0062] In addition, you can Fig.17As shown in the figure, when the shapes of the recess 3e and the recess 4e are viewed from the right angle direction of the electrode surface of the semiconductor element 1, in the recess 3e and the recess 4e, when the length in the width direction parallel to the electrode surface of the semiconductor element 1 is defined as W and the length in the depth direction is defined as D, W / D is formed to be greater than 2. As a result, the thickness of the solder of the connecting material 6 is thicker than other parts in the peripheral part of the first conductor 3 and the second conductor 4, so the effect of reducing the strain of the solder can be expected. In addition, since the thickness of the solder outside the recess is relatively thin compared with the peripheral part, the thermal resistance will not be increased, and fatigue damage of the solder can be prevented. In addition, it is possible to prevent the generation of gaps between the first conductor 3 and the connecting material 6, and a power semiconductor device with high reliability can be realized.

[0063] [Implementation Method 6]

[0064] Figure 8 FIG. 1 is a cross-sectional view showing a power semiconductor device according to a fifth embodiment of the present invention. Figure 1 In the first embodiment shown in FIG. 1 , the recessed portion 3a and the recessed portion 4a provided at the peripheral portion of the surface of the first conductor 3 and the second conductor 4 to be welded to the insulating substrate 5 are in a stepped shape and are provided at the outermost periphery of the first conductor 3 and the second conductor 4. In this embodiment, as shown in FIG. Figure 8 As shown, a wall 3f and a wall 4f are provided at the outermost periphery of the first conductor 3 and the second conductor 4. In this case, the thickness of the solder of the connecting material 6 is thicker than other parts at the periphery of the first conductor and the second conductor, so that the strain of the solder can be reduced. In addition, since the thickness of the solder outside the recessed portion 3a and the recessed portion 4a is relatively thinner than the periphery, the thermal resistance is not increased, fatigue damage of the solder can be prevented, and a power semiconductor device with high reliability can be realized. In addition, the wall 3f and the wall 4f can also be configured so that a part is in contact with at least a part of the first conductor layer 5b. As a result, the diffusion of the solder near the wall 3f and the wall 4f can be prevented, and the overflow of the solder can be prevented.

[0065] [Implementation method 7]

[0066] Fig. 9 1 is a cross-sectional view showing a power semiconductor device according to a sixth embodiment of the present invention. Figure 1 In the embodiment shown, the power semiconductor element 1 is connected to the first conductor 3 and the second conductor 4 through a connecting material 2. However, Fig. 9As shown, the present embodiment can also be applied to a power semiconductor device in which multiple chips are driven in parallel. Specifically, two or more power semiconductor elements 1 are connected to a first conductor 3 and a second conductor 4 via a connecting material 2. As a result, the lateral width can be reduced, thereby enabling miniaturization of the power semiconductor device. In the present embodiment, a recess 4a is provided at the peripheral portion of the surface of the second conductor 4 that is soldered to the insulating substrate 5. As a result, at the peripheral portion of the second conductor 4, the thickness of the connecting material 6 is thicker than other portions, thereby enabling the strain of the solder to be reduced. In addition, since the thickness of the solder outside the recess is relatively thin compared to the periphery, the thermal resistance will not be increased, fatigue damage of the solder can be prevented, and a power semiconductor device with high reliability can be achieved.

[0067] As in the present embodiment, when a plurality of power semiconductor elements 1 are connected to the first conductor 3 and the second conductor 4, the surface area of ​​the connection material 6 becomes larger than when the number of power semiconductor elements 1 is singular. Therefore, since the strain of the connection material 6 at the peripheral portion of the first conductor 3 and the second conductor 4 becomes larger, the effect of reducing the solder strain by providing the recesses 3a and 4a can be further expected. In addition, by providing a plurality of power semiconductor elements 1, the heat source can be dispersed and the thermal resistance can be reduced. Even when the recesses 3a and 4a provided at the peripheral portion of the first conductor 3 and the second conductor 4 are formed at a position close to the end of the chip, only the outermost chip is affected by the thermal resistance. Therefore, compared with the case where there is only one power semiconductor element 1, the increase in thermal resistance caused by providing the recesses can be suppressed.

[0068] [Embodiment 8]

[0069] use Fig.18 Embodiment 8 of the present invention will be described. Fig.18 is a cross-sectional view of a power semiconductor device according to an eighth embodiment of the present invention. Fig.18 As shown, in this embodiment, the heat dissipation fins 9 may be directly provided on the second conductor layer 5c. In this case, the heat dissipation fins 9 are joined to the second conductor layer 5c by arc welding or the like. This enables miniaturization and a reduction in the number of components.

[0070] [Implementation Method 9]

[0071] use Figure 1 15 and 15 illustrate a method for manufacturing a power semiconductor device according to an embodiment of the present invention. Figures 15(a) to 15(d) It is a diagram showing a manufacturing process of a power semiconductor device according to one embodiment of the present invention.

[0072] First, as shown in Fig. 15(a), recesses 3a and 4a are provided in the first conductor 3 and the second conductor 4. The recesses 3a and 4a are formed by, for example, extraction. Fig.14 FIG. 2 is a front view of a power semiconductor device according to an embodiment of the present invention. Fig.14 As shown, by providing the recessed portion 3a and the recessed portion 4a along the extraction direction, the recessed portion can be formed by extraction, thereby improving the manufacturability.

[0073] 16(b), the semiconductor element 1 is connected to the first conductor 3 and the second conductor 4 via the connection material 2. The first conductor 3 and the second conductor 4 are formed of, for example, copper, copper alloy, aluminum, aluminum alloy, etc. The connection material 2 is formed of solder or sintered material, etc.

[0074] Next, as shown in FIG. 15( c ), the first conductor 3 and the second conductor 4 are connected to the first conductor layer 5 b of the insulating substrate 5 via the connecting material 6. In the insulating substrate 5, the first conductor layer 5 b is arranged on one surface of the insulating member 5 a, and the second conductor layer 5 c is arranged on the other surface. In addition, both surfaces of the insulating substrate 5 can be connected to the first conductor 3 and the second conductor 4 at the same time. In this way, symmetry can be maintained, and warping deformation during assembly can be suppressed.

[0075] Next, as shown in FIG15( d ), the heat dissipation member 8 is connected to the insulating substrate 5 via the connection material 7 . At this time, the heat dissipation members 8 on both sides may be connected simultaneously. This can suppress warping deformation during assembly. Heat dissipation fins 9 are formed on the surface of the heat dissipation member 8 .

[0076] Finally, if Figure 1 As shown, the portion other than the heat dissipation surface 8 a of the heat dissipation fins forming the heat dissipation member 8 is sealed with a sealing resin 10 .

[0077] In the above embodiment, the shape of the heat dissipation fins 9 of the heat dissipation member 8 is set to be a pin fin, but it can also be other shapes, such as straight fins and corrugated fins. In addition, in the above embodiment, the sealing resin 10 includes the heat dissipation member 8 and seals the heat dissipation surface 8a, but it can also be as shown in the cross-sectional view of the power semiconductor device of another embodiment of the present invention. Fig.10 As shown in FIG. 1 , the resin is sealed to the insulating substrate 5. In this case, if the second conductor layer 5c of the insulating substrate 5 is connected to the heat dissipation member 8, the same effect can be obtained. In addition, if the thickness of the connecting material 6 is increased too much, the adhesion of the resin will deteriorate during the resin sealing, which may cause the resin to peel off. Therefore, it is configured to include a sealing member, which seals the insulating substrate 5, the first conductor 3 and the semiconductor element 1, and the depth of the recessed parts 3a and 4a is formed to be smaller than the length of the side surface of the first conductor 3 along the depth direction. In this way, the deterioration of the adhesion of the resin can be prevented.

[0078] In addition, in the above-mentioned embodiment, an on-vehicle power semiconductor device mounted on an electric vehicle or a hybrid vehicle is used as an example for explanation, but the present invention can be similarly applied as long as the conductor is connected to the power semiconductor element 1 through a connecting material, and then connected to the insulating substrate and has a heat dissipation portion (surface) on a surface different from the surface to which the conductor is joined.

[0079] The present invention is not limited to the above-described embodiment, and various modifications and applications are possible within the scope of the gist of the present invention.

[0080] Description of symbols

[0081] 1Power semiconductor components

[0082] 2. Connecting materials

[0083] 3First conductor

[0084] 3a concave part

[0085] 3f wall

[0086] 4 Second conductor

[0087] 4a concave part

[0088] 4b 45 degree line

[0089] 4c The bonding surface of the second conductor and the insulating substrate 5

[0090] 4d intersection

[0091] 4e recess

[0092] 4f wall

[0093] 5Insulation substrate

[0094] 5a Insulation components

[0095] 5b First conductor layer

[0096] 5c Second conductor layer

[0097] 6. Connecting materials

[0098] 7. Connecting Materials

[0099] 8. Heat dissipation components

[0100] 8a heat dissipation surface

[0101] 9 cooling fins

[0102] 10 Sealing resin

[0103] 11Third conductor

[0104] 11a recess

[0105] 12Fourth conductor

[0106] 12a recess

[0107] 13. Connecting materials

[0108] 14 terminals.

Claims

1. A power semiconductor device, It is characterized in that include: a first insulating substrate, a first conductor layer being disposed on one surface of the first insulating substrate; Semiconductor components; as well as a first conductor having a peripheral portion and a narrow portion, wherein the peripheral portion is connected to the first conductor layer via a first connecting material, and the narrow portion is connected to the semiconductor element via a second connecting material, When viewed from a right angle to the electrode surface of the semiconductor element, The narrow portion of the first conductor is narrower than the peripheral portion of the first conductor, The peripheral portion of the first conductor is larger than the semiconductor element, A first recessed portion is formed in the peripheral portion to make the first connection material thicker than other portions.

2. The power semiconductor device according to claim 1, It is characterized in that include: a second conductor connected to a surface of the semiconductor element opposite to the surface to which the first conductor is connected via a fourth connecting material; as well as a second insulating substrate, a third conductor layer being disposed on one surface of the second insulating substrate; The second conductor is connected to the third conductor layer via a fifth connecting material, When viewed from a right angle to the electrode surface of the semiconductor element, The second conductor has a peripheral portion formed larger than the semiconductor element, A second recessed portion is formed in the peripheral portion to make the fifth connecting material thicker than other portions.

3. The power semiconductor device according to claim 1 or 2, It is characterized in that When viewed from a right angle to the electrode surface of the semiconductor element, The depth of the first recess is greater on a side farther from the semiconductor element than on a side closer to the semiconductor element.

4. The power semiconductor device according to claim 1 or 2, It is characterized in that When viewed from a right angle to the electrode surface of the semiconductor element, In the first recessed portion, when W is defined as a length in a width direction parallel to the electrode surface and D is defined as a length in a depth direction, W / D is equal to or greater than 2.

5. The power semiconductor device according to claim 1 or 2, It is characterized in that The first conductor has a protrusion forming a side portion of the recessed portion on a side close to the outer periphery of the first connecting material. The protrusion is in contact with the first connection material.

6. The power semiconductor device according to claim 5, It is characterized in that The protrusion is in contact with the first conductor layer.

7. The power semiconductor device according to claim 1 or 2, It is characterized in that When viewed from a right angle to the electrode surface of the semiconductor element, The first recessed portion is formed between a virtual line and an outer periphery of the first conductor, the virtual line being composed of a set of points separated from an end portion of the semiconductor element by a distance corresponding to a thickness of the first conductor.

8. The power semiconductor device according to claim 1 or 2, It is characterized in that A second conductor layer is disposed on the other surface of the insulating substrate. The power semiconductor device includes a heat dissipation portion connected to the second conductor layer via a third connection material.

9. The power semiconductor device according to claim 8, It is characterized in that When viewed from the arrangement direction of the first conductor layer and the second conductor layer, The heat dissipation portion has a second peripheral portion formed larger than the first conductor, A third recessed portion is formed in the second peripheral portion so as to make the third connection material thicker than other portions.

10. The power semiconductor device according to claim 1 or 2, It is characterized in that A second conductor layer is disposed on the other surface of the insulating substrate. The second conductor layer includes fins for heat dissipation.

11. The power semiconductor device according to claim 1 or 2, It is characterized in that The peripheral portion is composed of a first side having the first recess formed thereon and a second side having no recess formed thereon, The semiconductor element is arranged so that a distance from the semiconductor element to the first side is smaller than a distance from the semiconductor element to the second side.

12. The power semiconductor device according to claim 1 or 2, It is characterized in that comprising a sealing member that seals the insulating substrate, the first conductor, and the semiconductor element, The depth of the first recess is smaller than the length of the side surface of the first conductor along the depth direction.

13. The power semiconductor device according to claim 1 or 2, It is characterized in that The first conductor includes two or more of the semiconductor elements.

Citation Information

Patent Citations

  • Heat sink for semiconductor device

    JP1998189845A

  • Power module and electric power conversion apparatus using the same

    JP2012257369A

  • Double-sided cooling power module and method for manufacturing the same

    US20160126157A1

  • Semiconductor module and inverter device

    US20160197028A1