A compound, its application and organic electroluminescent device using the same

By using new compounds as electron blocking layer materials in OLED devices and using 2-naphthyltriarylamine system with 2-naphthylamine as the core to increase the triplet energy level, the efficiency and life problems of OLED products are solved, and low starting voltage is achieved. and high luminous efficiency, suitable for mass production.

CN113511978BActive Publication Date: 2024-10-15BEIJING DINGCAI TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010272589.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-04-09
Publication Date
2024-10-15
Estimated Expiration
2040-04-09

AI Technical Summary

Technical Problem

Existing OLED materials and device structures cannot fully solve the problems of efficiency, lifespan and cost of OLED products.

Method used

Provide a new type of compound and its application in OLED devices. As an electron blocking layer material, a 2-naphthyl triarylamine system with 2-naphthylamine as the core is used. By introducing an aryl group substitution on the naphthalene ring, the third line is improved. state energy levels, improving luminous efficiency and extending device life.

Benefits of technology

It achieves low starting voltage, high luminous efficiency and better service life, meets the requirements of high-performance materials, and the preparation process is simple and easy to implement, suitable for mass production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113511978B_ABST
    Figure CN113511978B_ABST
Patent Text Reader

Abstract

The present invention relates to a novel organic compound having the following structure (1): #imgabs0#L 1 , L 2 Each independently represents a single bond, a substituted or unsubstituted C6-C 30 arylene, substituted or unsubstituted C3~C 30 One of the heteroarylene groups; Ar 1 ,Ar 2 ,Ar 3 Each independently represents a substituted or unsubstituted C6 to C 30 aryl, substituted or unsubstituted C3~C 30 One of the heteroaryl groups; R 1 , R 2 are independently selected from hydrogen, substituted or unsubstituted C1-C 20 Alkyl, substituted or unsubstituted C1~C 20 Alkoxy, substituted or unsubstituted C3~C 20 cycloalkyl, substituted or unsubstituted C1~C6 ether, substituted or unsubstituted C6~C 30 aryl, substituted or unsubstituted C3~C 30 The compound of the present invention exhibits excellent device performance and stability when used as an electron blocking layer material in an OLED device. The present invention also protects an organic electroluminescent device using the compound of the general formula.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of organic electroluminescence, in particular to an organic compound and an organic electroluminescence device containing the same. Background Art

[0002] In recent years, optoelectronic devices based on organic materials have become increasingly popular. The inherent flexibility of organic materials makes them very suitable for manufacturing on flexible substrates. Beautiful and cool optoelectronic products can be designed and produced according to demand, gaining unparalleled advantages over inorganic materials. Examples of such organic optoelectronic devices include organic light-emitting diodes (OLEDs), organic field-effect transistors, organic photovoltaic cells, organic sensors, etc. Among them, OLED has developed particularly rapidly and has achieved commercial success in the field of information display. OLED can provide highly saturated red, green, and blue colors. Full-color display devices made of OLEDs do not require additional backlight sources and have the advantages of brilliant colors, lightness, thinness, and softness.

[0003] The core of OLED devices is a thin film structure containing a variety of organic functional materials. Common functionalized organic materials include: hole injection materials, hole transport materials, hole blocking materials, electron injection materials, electron transport materials, electron blocking materials, luminescent host materials and luminescent guest (dyes), etc. When power is turned on, electrons and holes are injected and transported to the luminescent area respectively and recombine there, thereby generating excitons and emitting light.

[0004] People have developed a variety of organic materials, combined with various unique device structures, which can improve carrier mobility, regulate carrier balance, break through electroluminescence efficiency, and delay device attenuation. For quantum mechanical reasons, common fluorescent luminescent bodies mainly use singlet excitons generated when electrons and voids combine to emit light, and are still widely used in various OLED products. Some metal complexes, such as iridium complexes, can use triplet excitons and singlet excitons to emit light at the same time, and are called phosphorescent luminescent bodies. Their energy conversion efficiency can be increased by up to four times that of traditional fluorescent luminescent bodies. Thermally excited delayed fluorescence (TADF) technology promotes the transformation of triplet excitons to singlet excitons. Without the use of metal complexes, triplet excitons can still be effectively utilized to achieve higher luminescence efficiency. Thermally excited sensitized fluorescence (TASF) technology uses materials with TADF properties to sensitize luminescent bodies through energy transfer, which can also achieve higher luminescence efficiency.

[0005] As OLED products gradually enter the market, people have higher and higher requirements for the performance of such products. The currently used OLED materials and device structures cannot completely solve the problems of OLED product efficiency, life span, cost and other aspects. Summary of the invention

[0006] In order to solve the above technical problems, the present invention provides a novel compound, and also provides an application method of the compound in an OLED device and an organic electroluminescent device using the compound.

[0007] The present application provides a novel compound having a structure shown in the following formula (1):

[0008]

[0009] Among them, L 1 , L 2 Each independently represents a single bond, a substituted or unsubstituted C6-C 30 arylene, substituted or unsubstituted C3~C 30 One of the heteroarylene groups;

[0010] Ar 1 ,Ar 2 ,Ar 3 Each independently represents a substituted or unsubstituted C6 to C 30 Aryl, substituted or unsubstituted C3~C 30 One of the heteroaryl groups;

[0011] R 1 , R 2 Each independently represents a single substituent to the maximum permissible substituent, and each independently selected from hydrogen, substituted or unsubstituted C1-C 20 Alkyl, substituted or unsubstituted C1~C 20 Alkoxy, substituted or unsubstituted C3~C 20 cycloalkyl, substituted or unsubstituted C1~C6 ether, substituted or unsubstituted C6~C 30 Aryl, substituted or unsubstituted C3~C 30 One of the heteroaryl groups; preferably, R 1 , R 2 They are independently connected to the mother core by single bonds.

[0012] When the above groups have substituents, the substituents are selected from halogen, C1-C 20 Chain alkyl, C3~C 20 cycloalkyl, C1-C6 alkoxy, C1-C6 thioalkoxy, C6-C 30 A monocyclic aromatic group or a condensed aromatic group, a C3~C 30 One or a combination of at least two of a monocyclic heteroaryl group or a condensed-ring heteroaryl group.

[0013] It should be noted that, in the present invention, the maximum permissible substituents refer to the maximum number of substituents under the premise that the substituted groups meet the bonding requirements.

[0014] In this manual, C a ~C b The expression "a" represents that the number of carbon atoms in the group is a to b. Unless otherwise specified, the number of carbon atoms generally does not include the number of carbon atoms in the substituent.

[0015] In this specification, the expression of a ring structure crossed by “—” indicates that the connection site is any position on the ring structure that can form a bond; “*” represents the access position of a group.

[0016] The atomic names described in the present invention include their corresponding isotopes. For example, hydrogen (H) includes 1 H (hydrogen or H), 2 H (deuterium or D), etc.; Carbon (C) includes 12 C. 13 C, etc.

[0017] In this specification, substituted or unsubstituted C6 to C 30 The aryl group is preferably C6-C 20 Aryl, more preferably phenyl, biphenyl, terphenyl, naphthyl, anthracenyl, phenanthrenyl, indenyl, fluorenyl and its derivatives, fluoranthenyl, triphenylene, pyrenyl, peryl, A group consisting of a tetraphenyl group and a naphthyl group. Specifically preferably, the biphenyl group is selected from 2-biphenyl, 3-biphenyl and 4-biphenyl; the terphenyl group includes p-terphenyl-4-yl, p-terphenyl-3-yl, p-terphenyl-2-yl, m-terphenyl-4-yl, m-terphenyl-3-yl and m-terphenyl-2-yl; preferably the naphthyl group includes 1-naphthyl and 2-naphthyl; preferably the anthracenyl group is selected from 1-anthracenyl, 2-anthracenyl and 9-anthracenyl; preferably the fluorenyl group is selected from 1-fluorenyl, 2-fluorenyl, 3-fluorenyl, 4-fluorenyl and 9-fluorenyl; preferably the fluorenyl derivative is selected from 9,9'-dimethylfluorene, 9,9'-spirobifluorene and benzofluorene; preferably the pyrenyl group is selected from 1-pyrenyl, 2-pyrenyl and 4-pyrenyl; preferably the tetraphenyl group is selected from 1-tetraphenyl, 2-tetraphenyl and 9-tetraphenyl.

[0018] The heteroatom in the present invention generally refers to an atom or an atom group selected from N, O, S, P, Si and Se, preferably selected from N, O and S.

[0019] In this specification, substituted or unsubstituted C3 to C 30 The heteroaryl group is preferably C4 to C 20The heteroaryl group is more preferably a nitrogen-containing heteroaryl group, an oxygen-containing heteroaryl group, a sulfur-containing heteroaryl group, and the like. Preferred examples include: furyl, thienyl, pyrrolyl, benzofuranyl, benzothienyl, isobenzofuranyl, indolyl, dibenzofuranyl, dibenzothienyl, carbazolyl and derivatives thereof, wherein the carbazolyl derivative is preferably 9-phenylcarbazole, 9-naphthylcarbazole, benzocarbazole, dibenzocarbazole, or indolecarbazole.

[0020] In this specification, the above C1 to C 20 The alkyl group is preferably C1 to C 10 The chain alkyl group is preferably a C1-C6 chain alkyl group, and further preferably a methyl group, an ethyl group, an n-propyl group, an isopropyl group, an n-butyl group, an n-hexyl group, an n-octyl group, an isobutyl group, a tert-butyl group, a cyclopentyl group or a cyclohexyl group.

[0021] In this manual, C3 to C 20 Cycloalkyl includes monocyclic alkyl and polycyclic alkyl, preferably C1-C 10 Monocyclic alkyl and C3~C 10 The polycyclic alkyl group is preferably cyclopropyl, cyclobutyl, cyclopentyl or cyclohexyl.

[0022] More preferably, the compound of the general formula of the present invention is selected from one of the following formulas (2-1), (2-2) or (2-3):

[0023]

[0024] More preferred is formula (2-1).

[0025] Still more preferably, in the above formula (1), (2-1), (2-2) or (2-3), Ar 1 ,Ar 2 ,Ar 3 Each independently represents a substituted or unsubstituted C6 to C 20 Aryl, substituted or unsubstituted C4~C 20 The heteroaryl group.

[0026] More preferably, in the above formula (1), (2-1), (2-2) or (2-3), R 1 , R 2 Each independently selected from substituted or unsubstituted C1 to C 10 Alkyl, substituted or unsubstituted C3~C 10 cycloalkyl, substituted or unsubstituted C3~C6 ether, substituted or unsubstituted C6~C 20 Aryl, substituted or unsubstituted C4~C 20 Any one of the heteroaryl groups.

[0027] More preferably, the above Ar1 ,Ar 2 ,Ar 3 Each is independently selected from one of the following substituted or unsubstituted groups: phenyl, biphenyl, terphenyl, naphthyl, phenanthryl, anthracenyl, dibenzofuranyl, dibenzothiophenyl, carbazolyl, 9,9-dimethylfluorenyl, 9,9-diphenylfluorenyl, spirofluorene, triphenylene, fluoranthene, benzo-9,9-dimethylfluorenyl, benzospirofluorene;

[0028] When the above groups have substituents, the substituents are selected from halogen, C1-C 20 Chain alkyl, C3~C 20 cycloalkyl, C1-C6 alkoxy, C1-C6 thioalkoxy, C6-C 30 A monocyclic aromatic group or a condensed aromatic group, a C3~C 30 One or a combination of at least two of a monocyclic heteroaryl group or a condensed-ring heteroaryl group;

[0029] Preferably, Ar 1 ,Ar 2 ,Ar 3 Each is independently selected from one of the following groups:

[0030]

[0031] The expression of a ring structure crossed by “—” indicates that the connection site is any position on the ring structure that can form a bond, and “*” represents the access position of the group.

[0032] More preferably, in the above formula (1), (2-1), (2-2) or (2-3), R 1 and R 2 At least one of them is hydrogen; more preferably, R 1 and R 2 At the same time, it is hydrogen.

[0033] More preferably, in the above formula (1), (2-1), (2-2) or (2-3), L 1 and L 2 More preferably, L 1 and L 2 It is also a single bond.

[0034] The preferred structures of the compounds involved in the present invention are shown in the following structures P1 to P324:

[0035]

[0036]

[0037]

[0038]

[0039]

[0040]

[0041]

[0042]

[0043]

[0044]

[0045]

[0046]

[0047]

[0048]

[0049]

[0050]

[0051]

[0052]

[0053]

[0054]

[0055]

[0056]

[0057]

[0058]

[0059]

[0060]

[0061]

[0062] As another aspect of the present invention, there is also provided an application of the compound as described above in an organic electroluminescent device, in particular, preferably used as an electron blocking layer material in an organic electroluminescent device.

[0063] In addition, the compounds of the present invention can be applied to electron blocking layers in organic electronic devices, such as organic electroluminescent devices, lighting elements, organic thin film transistors, organic field effect transistors, organic thin film solar cells, information tags, electronic artificial skin sheets, large area sensors such as sheet-type scanners, electronic paper, and organic EL panels.

[0064] As another aspect of the present invention, an organic electroluminescent device is provided, comprising a first electrode, a second electrode and one or more organic layers inserted between the first electrode and the second electrode, wherein the organic layer contains a compound of the general formula (1) as described above, or contains a compound having a structure shown in P1 to P324 as described above.

[0065] In one embodiment, the organic layer includes a hole transport layer and / or an electron blocking layer, and the compound of the present application is disposed in the electron blocking layer.

[0066] In addition, the above-mentioned multi-layer organic functional material layer may also include a hole transport layer, a hole injection layer, an electron blocking layer, a light-emitting layer, a hole blocking layer, an electron injection layer, and an electron transport layer which are sequentially arranged away from the anode.

[0067] The present invention further discloses a display screen or a display panel, wherein the organic electroluminescent device as described above is adopted in the display screen or the display panel; preferably, the display screen or the display panel is an OLED display.

[0068] The present invention also discloses an electronic device, wherein the electronic device has a display screen or a display panel, and the display screen or the display panel adopts the organic electroluminescent device as described above.

[0069] The OLED device prepared by using the compound of the present invention as the electron blocking layer material has a low starting voltage, high luminous efficiency and a better service life, and can meet the requirements of current panel manufacturing companies for high-performance materials.

[0070] The specific reason why the above-mentioned compound of the present invention has excellent performance as an electron blocking layer material in an organic electroluminescent device is still unclear, but it is speculated that the reasons may be as follows:

[0071] 1. In the structural design of the compound of the present invention, a 2-naphthyl triarylamine system with 2-naphthylamine as the main nucleus is adopted. The introduction of an aryl substitution at the 1-position of the naphthalene ring can improve the triplet energy level of the entire molecule to a certain extent. When the compound of the present invention is used in an organic electroluminescent device, it will help to improve the luminous efficiency of the device;

[0072] 2. The introduction of a group at the 1-position of the naphthalene ring in the parent core structure, especially at the di-ortho position in the sub-formula, may not only enhance the triplet energy level, but also further protect the central nitrogen atom. When the compound of the present invention is used in an organic electroluminescent device, it will help to extend the service life of the device.

[0073] In addition, the preparation process of the compound of the present invention is simple and easy, the raw materials are easily available, and it is suitable for mass production and expansion. DETAILED DESCRIPTION

[0074] The specific preparation method of the above-mentioned novel compound of the present invention will be described in detail below by taking a plurality of synthesis examples as examples, but the preparation method of the present invention is not limited to these synthesis examples.

[0075] However, it should be noted that obtaining the compound is not limited to the synthesis method and raw materials used in the present invention, and those skilled in the art may also select other methods or routes to obtain the novel compound proposed in the present invention. The compounds for which the synthesis method is not mentioned in the present invention are raw materials obtained from commercial channels, or are prepared by themselves according to known methods using these raw materials.

[0076] The solvents and reagents used in the following synthesis examples of the present invention, such as aryl bromide, 2-bromo-9,9'-dimethylfluorene, 2-bromodibenzofuran, 2-bromodibenzothiophene, 4-bromobiphenyl, [1,1'-bis(diphenylphosphino)ferrocene] palladium dichloride, tris(dibenzylideneacetone)dipalladium, toluene, petroleum ether, n-hexane, dichloromethane, acetone, sodium sulfate, ethyl acetate, ethanol, tri-tert-butylphosphine, potassium / sodium tert-butyl alcohol and other chemical reagents, can be purchased or customized from the domestic chemical product market, such as purchased from Sinopharm Group Reagent Company, Sigma-Aldrich Company, and J&K Reagent Company, and intermediate M is customized by Zhengzhou Haikuo, J&K and other companies. In addition, those skilled in the art can also synthesize by known methods.

[0077] The analysis and detection of the intermediates and compounds in the synthesis examples were performed using an ABSCIEX mass spectrometer (4000QTRAP).

[0078] The synthesis method of the compound of the present invention is briefly described below.

[0079] Synthesis Example

[0080] Representative synthetic routes:

[0081]

[0082] Based on the synthetic routes and ideas of the above compounds, those skilled in the art can obtain 1 ,Ar 2 The compound represented by formula (1).

[0083] Synthesis Example 1: Synthesis of Compound P1

[0084]

[0085] In a 1000mL single-mouth bottle, add 15g (50mmol) M1, 16g (100mmol) bromobenzene, 0.9g (1mmol) tris (dibenzylideneacetone) dipalladium (i.e. Pd2 (dba) 3), 0.5mL tri-tert-butylphosphine ((t-Bu) 3P), 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen three times, and heat the reaction to 110°C for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain light yellow powder P1.

[0086] Theoretical M / Z value: 447; measured M / Z value using ZAB-HS mass spectrometer (manufactured by Micromass, UK): 448.

[0087] Synthesis Example 2: Synthesis of Compound P12

[0088]

[0089] In a 1000mL single-mouth bottle, add 15g (50mmol) M1, 12g (50mmol) 4-bromobiphenyl, 0.9g (1mmol) tris (dibenzylideneacetone) dipalladium (i.e. Pd2 (dba) 3), 0.5g IPr.HCl, 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen 3 times, and heat the reaction to 90°C for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain a light yellow powder M1-1.

[0090] In a 1000mL single-mouth bottle, add 22.5g (50mmol) M1-1, 10.3g (50mmol) 2-bromonaphthalene, 0.9g (1mmol) tri(dibenzylideneacetone)dipalladium (i.e. Pd2(dba)3), 0.5mL tri-tert-butylphosphine ((t-Bu)3P), 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen three times, and heat the reaction to 110°C for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain light yellow powder P12.

[0091] Theoretical M / Z value: 573; measured M / Z value using ZAB-HS mass spectrometer (manufactured by Micromass, UK): 574.

[0092] Synthesis Example 3: Synthesis of Compound P18

[0093]

[0094] In a 1000mL single-mouth bottle, add 15g (50mmol) M1, 23.2g (100mmol) 4-bromobiphenyl, 0.9g (1mmol) tri(dibenzylideneacetone) dipalladium (i.e. Pd2(dba)3), 0.5mL tri-tert-butylphosphine ((t-Bu)3P), 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen three times, and heat the reaction to 110℃ for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain light yellow powder P18.

[0095] Theoretical M / Z value: 599; measured M / Z value using ZAB-HS mass spectrometer (manufactured by Micromass, UK): 600.

[0096] Synthesis Example 4: Synthesis of Compound P31

[0097]

[0098] In a 1000mL single-mouth bottle, add 15g (50mmol) M1, 12g (50mmol) 4-bromobiphenyl, 0.9g (1mmol) tris (dibenzylideneacetone) dipalladium (i.e. Pd2 (dba) 3), 0.5g IPr.HCl, 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen 3 times, and heat the reaction to 90°C for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain a light yellow powder M1-1.

[0099] In a 1000mL single-mouth bottle, add 22.5g (50mmol) M1-1, 13.5g (50mmol) 3-bromo-9,9-dimethylfluorene, 0.9g (1mmol) tri(dibenzylideneacetone)dipalladium (i.e. Pd2(dba)3), 0.5mL tri-tert-butylphosphine ((t-Bu)3P), 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen three times, and heat the reaction to 110℃ for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain light yellow powder P31.

[0100] Theoretical M / Z value: 639; measured M / Z value using ZAB-HS mass spectrometer (manufactured by Micromass, UK): 640.

[0101] Synthesis Example 5: Synthesis of Compound P33

[0102]

[0103] In a 1000mL single-mouth bottle, add 15g (50mmol) M1, 7.8g (50mmol) 4-bromobenzene, 0.9g (1mmol) tris (dibenzylideneacetone) dipalladium (i.e. Pd2 (dba) 3), 0.5g IPr.HCl, 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen 3 times, and heat the reaction to 90°C for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain a light yellow powder M1-2.

[0104] In a 1000mL single-mouth bottle, add 18.5g (50mmol) M1-2, 12.3g (50mmol) 2-bromo-dibenzofuran, 0.9g (1mmol) tri(dibenzylideneacetone)dipalladium (i.e. Pd2(dba)3), 0.5mL tri-tert-butylphosphine ((t-Bu)3P), 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen three times, and heat the reaction to 110°C for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain light yellow powder P33.

[0105] Theoretical M / Z value: 537; measured M / Z value using ZAB-HS mass spectrometer (manufactured by Micromass, UK): 538.

[0106] Synthesis Example 6: Synthesis of Compound P96

[0107]

[0108] In a 1000mL single-mouth bottle, add 15g (50mmol) M2, 12g (50mmol) 4-bromobiphenyl, 0.9g (1mmol) tris (dibenzylideneacetone) dipalladium (i.e. Pd2 (dba) 3), 0.5g IPr.HCl, 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), evacuate and replace with nitrogen 3 times, and heat the reaction to 90°C for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain a light yellow powder M2-1.

[0109] In a 1000mL single-mouth bottle, add 22.5g (50mmol) M2-1, 10.3g (50mmol) 2-bromonaphthalene, 0.9g (1mmol) tri(dibenzylideneacetone)dipalladium (i.e. Pd2(dba)3), 0.5mL tri-tert-butylphosphine ((t-Bu)3P), 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen three times, and heat the reaction to 110°C for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain light yellow powder P96.

[0110] Theoretical M / Z value: 573; measured M / Z value using ZAB-HS mass spectrometer (manufactured by Micromass, UK): 574.

[0111] Synthesis Example 7: Synthesis of Compound P115

[0112]

[0113] In a 1000mL single-mouth bottle, add 15g (50mmol) M2, 12g (50mmol) 4-bromobiphenyl, 0.9g (1mmol) tris (dibenzylideneacetone) dipalladium (i.e. Pd2 (dba) 3), 0.5g IPr.HCl, 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), evacuate and replace with nitrogen 3 times, and heat the reaction to 90°C for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain a light yellow powder M2-1.

[0114] In a 1000mL single-mouth bottle, add 22.5g (50mmol) M2-1, 13.6g (50mmol) 2-bromo-9,9-dimethylfluorene, 0.9g (1mmol) tri(dibenzylideneacetone)dipalladium (i.e. Pd2(dba)3), 0.5mL tri-tert-butylphosphine ((t-Bu)3P), 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen three times, and heat the reaction to 110℃ for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain light yellow powder P115.

[0115] Theoretical M / Z value: 639; measured M / Z value using ZAB-HS mass spectrometer (manufactured by Micromass, UK): 640.

[0116] Synthesis Example 8: Synthesis of Compound P186

[0117]

[0118] In a 1000mL single-mouth bottle, add 15g (50mmol) M3, 23.2g (100mmol) 4-bromo-biphenyl, 0.9g (1mmol) tri(dibenzylideneacetone) dipalladium (i.e. Pd2(dba)3), 0.5mL tri-tert-butylphosphine ((t-Bu)3P), 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen 3 times, and heat the reaction to 110℃ for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain light yellow powder P186.

[0119] Theoretical M / Z value: 599; measured M / Z value using ZAB-HS mass spectrometer (manufactured by Micromass, UK): 600.

[0120] Synthesis Example 9: Synthesis of Compound P199

[0121]

[0122] In a 1000mL single-mouth bottle, add 15g (50mmol) M3, 10.3g (50mmol) 4-bromobiphenyl, 0.9g (1mmol) tris (dibenzylideneacetone) dipalladium (i.e. Pd2 (dba) 3), 0.5g IPr.HCl, 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), evacuate and replace with nitrogen 3 times, heat the reaction to 90°C for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain a light yellow powder M3-1.

[0123] In a 1000mL single-mouth bottle, add 22.3g (50mmol) M3-1, 13.6g (50mmol) 3-bromo-9,8-dimethylfluorene, 0.9g (1mmol) tri(dibenzylideneacetone)dipalladium (i.e. Pd2(dba)3), 0.5mL tri-tert-butylphosphine ((t-Bu)3P), 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen three times, and heat the reaction to 110℃ for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain light yellow powder P199.

[0124] Theoretical M / Z value: 639; measured M / Z value using ZAB-HS mass spectrometer (manufactured by Micromass, UK): 640.

[0125] Synthesis Example 10: Synthesis of Compound P258

[0126]

[0127] In a 1000mL single-mouth bottle, add 17.4g (50mmol) M4, 23.2g (100mmol) 4-bromobiphenyl, 0.9g (1mmol) tris (dibenzylideneacetone) dipalladium (i.e. Pd2 (dba) 3), 0.5mL tri-tert-butylphosphine ((t-Bu) 3P), 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen 3 times, and heat the reaction to 110°C for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain light yellow powder P258.

[0128] Theoretical M / Z value: 649; measured M / Z value using ZAB-HS mass spectrometer (manufactured by Micromass, UK): 650.

[0129] Synthesis Example 11: Synthesis of Compound P302

[0130]

[0131] In a 1000mL single-mouth bottle, add 17.2g (50mmol) M5, 13.6g (50mmol) 3-bromo-9,9-dimethylfluorene, 0.9g (1mmol) tris (dibenzylideneacetone) dipalladium (i.e. Pd2 (dba) 3), 0.5g IPr.HCl, 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen 3 times, and heat the reaction to 90°C for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain a light yellow powder M5-1.

[0132] In a 1000mL single-mouth bottle, add 27g (50mmol) M5-1, 15.4g (50mmol) 2,4-diphenylbromobenzene, 0.9g (1mmol) tris (dibenzylideneacetone) dipalladium (i.e. Pd2 (dba) 3), 0.5mL tri-tert-butylphosphine ((t-Bu) 3P), 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen 3 times, and heat the reaction to 110℃ for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain light yellow powder P302.

[0133] Theoretical M / Z value: 765; measured M / Z value using ZAB-HS mass spectrometer (manufactured by Micromass, UK): 766.

[0134] Synthesis Example 12: Synthesis of Compound P306

[0135]

[0136] In a 1000mL single-mouth bottle, add 19g (50mmol) M6, 12.3g (50mmol) 3-bromo-dibenzofuran, 0.9g (1mmol) tris (dibenzylideneacetone) dipalladium (i.e. Pd2 (dba) 3), 0.5g IPr.HCl, 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen 3 times, and heat the reaction to 90°C for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain a light yellow powder M6-1.

[0137] In a 1000mL single-mouth bottle, add 26g (50mmol) M6-1, 15.4g (50mmol) 2,4-diphenylbromobenzene, 0.9g (1mmol) tris (dibenzylideneacetone) dipalladium (i.e. Pd2 (dba) 3), 0.5mL tri-tert-butylphosphine ((t-Bu) 3P), 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen 3 times, and heat the reaction to 110°C for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain light yellow powder P306.

[0138] Theoretical M / Z value: 779; measured M / Z value using ZAB-HS mass spectrometer (manufactured by Micromass, UK): 780.

[0139] Synthesis Example 13: Synthesis of Compound P307

[0140]

[0141] In a 1000mL single-mouth bottle, add 18.5g (50mmol) M7, 12g (50mmol) 4-bromobiphenyl, 0.9g (1mmol) tris (dibenzylideneacetone) dipalladium (i.e. Pd2 (dba) 3), 0.5g IPr.HCl, 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen 3 times, and heat the reaction to 90°C for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain a light yellow powder M7-1.

[0142] In a 1000mL single-mouth bottle, add 26g (50mmol) M7-1, 13.6g (50mmol) 2-bromo-9,9-dimethylfluorene, 0.9g (1mmol) tri(dibenzylideneacetone)dipalladium (i.e. Pd2(dba)3), 0.5mL tri-tert-butylphosphine ((t-Bu)3P), 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen 3 times, and heat the reaction to 110℃ for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain light yellow powder P307.

[0143] Theoretical M / Z value: 715; measured M / Z value using ZAB-HS mass spectrometer (manufactured by Micromass, UK): 716.

[0144] Synthesis Example 14: Synthesis of Compound 315

[0145]

[0146] In a 1000mL single-mouth bottle, add 15g (50mmol) M2, 15.4g (50mmol) 4-bromoterphenyl) biphenyl, 0.9g (1mmol) tris (dibenzylideneacetone) palladium (i.e. Pd2 (dba) 3), 0.5g IPr.HCl, 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen 3 times, and heat the reaction to 90°C for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain a light yellow powder M2-2.

[0147] In a 1000mL single-mouth bottle, add 26g (50mmol) M2-2, 13.6g (50mmol) 2-bromo-9,9-dimethylfluorene, 0.9g (1mmol) tri(dibenzylideneacetone)dipalladium (i.e. Pd2(dba)3), 0.5mL tri-tert-butylphosphine ((t-Bu)3P), 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen three times, and heat the reaction to 110℃ for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain light yellow powder P315.

[0148] Theoretical M / Z value: 715; measured M / Z value using ZAB-HS mass spectrometer (manufactured by Micromass, UK): 716.

[0149] Synthesis Example 15: Synthesis of Compound P319

[0150]

[0151] In a 1000mL single-mouth bottle, add 15g (50mmol) M1, 16.5g (50mmol) 4-bromo-4'-cyclohexylbiphenyl, 0.9g (1mmol) tris (dibenzylideneacetone) dipalladium (i.e. Pd2(dba)3), 0.5g IPr.HCl, 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen 3 times, and heat the reaction to 90°C for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain a light yellow powder M1-3.

[0152] In a 1000mL single-mouth bottle, add 26.5g (50mmol) M1-3, 13.5g (50mmol) 3-bromo-9,9-dimethylfluorene, 0.9g (1mmol) tri(dibenzylideneacetone)dipalladium (i.e. Pd2(dba)3), 0.5mL tri-tert-butylphosphine ((t-Bu)3P), 500mL toluene, 14.4g (150mmol) sodium tert-butoxide (NaOBu-t), vacuum and replace nitrogen three times, and heat the reaction to 110℃ for 5h. After the reaction is complete, stop the reaction. Cool to room temperature, separate the reaction solution, concentrate the organic phase, add methanol and stir for 1h, and filter to obtain light yellow powder P319.

[0153] Theoretical M / Z value: 721; measured M / Z value using ZAB-HS mass spectrometer (manufactured by Micromass, UK): 722.

[0154] Based on the same inventive concept, an embodiment of the present invention further provides an organic electronic light-emitting device comprising the compound prepared in the above synthesis embodiment. OLED is used as an organic electronic light-emitting device as an example of a device for illustration below, but it should be understood that the following detailed description is not a limitation of the present invention, and those skilled in the art can extend the following detailed description to other organic electronic light-emitting devices.

[0155] Next, the organic electroluminescent device is described in detail.

[0156] The organic electroluminescent device includes a first electrode, a second electrode, and an organic material layer between the electrodes. The organic material layer can be divided into multiple regions. For example, the organic material layer can include a hole transport region, a light emitting layer, and an electron transport region.

[0157] In a specific embodiment, a substrate may be used below the first electrode or above the second electrode. The substrate is a glass or polymer material with excellent mechanical strength, thermal stability, water resistance, and transparency. In addition, a thin film transistor (TFT) may also be provided on the substrate used as a display.

[0158] The first electrode can be formed by sputtering or depositing the material used as the first electrode on the substrate. When the first electrode is used as an anode, an oxide transparent conductive material such as indium tin oxide (ITO), indium zinc oxide (IZO), tin dioxide (SnO2), zinc oxide (ZnO) and any combination thereof can be used. When the first electrode is used as a cathode, a metal or alloy such as magnesium (Mg), silver (Ag), aluminum (Al), aluminum-lithium (Al-Li), calcium (Ca), magnesium-indium (Mg-In), magnesium-silver (Mg-Ag) and any combination thereof can be used.

[0159] The organic material layer can be formed on the electrode by vacuum thermal evaporation, spin coating, printing, etc. The compound used as the organic material layer can be organic small molecules, organic macromolecules and polymers, and combinations thereof.

[0160] The hole transport region is located between the anode and the light-emitting layer. The hole transport region can be a hole transport layer (HTL) of a single-layer structure, including a single-layer hole transport layer containing only one compound and a single-layer hole transport layer containing multiple compounds. The hole transport region can also be a multi-layer structure including at least one layer of a hole injection layer (HIL), a hole transport layer (HTL), and an electron blocking layer (EBL).

[0161] When the hole transport layer in the hole transport zone can have and be selected from, but not limited to, phthalocyanine derivatives such as CuPc, conductive polymers or polymers containing conductive dopants such as polyphenylene ethylene, polyaniline / dodecylbenzenesulfonic acid (Pani / DBSA), poly(3,4-ethylenedioxythiophene) / poly(4-styrenesulfonate) (PEDOT / PSS), polyaniline / camphorsulfonic acid (Pani / CSA), polyaniline / poly(4-styrenesulfonate) (Pani / PSS), aromatic amine derivatives such as the compounds shown in HT-1 to HT-34 below; or any combination thereof. When the hole transport layer in the hole transport zone is selected from, but not limited to, phthalocyanine derivatives such as CuPc, conductive polymers or polymers containing conductive dopants such as polyphenylene ethylene, polyaniline / dodecylbenzenesulfonic acid (Pani / DBSA), poly(3,4-ethylenedioxythiophene) / poly(4-styrenesulfonate) (PEDOT / PSS), polyaniline / camphorsulfonic acid (Pani / CSA), polyaniline / poly(4-styrenesulfonate) (Pani / PSS), aromatic amine derivatives such as the compounds shown in HT-1 to HT-34 below, or any combination thereof; the electron blocking layer in the hole transport zone is selected from one of the compounds described above or any combination thereof.

[0162]

[0163]

[0164] The materials of the hole transport region and the hole injection region can be selected from, but not limited to, the compounds described in the present invention and the above compounds; or any combination thereof. Among them, the hole injection layer can be a single compound material or a combination of multiple compounds. For example, the hole injection layer can use one or more of the compounds in the present invention described above, or one or more of the compounds in the following HI-1-HI-3; or one or more of the compounds can be doped with one or more of the compounds in the following HI-1-HI-3.

[0165]

[0166] The light-emitting layer includes a light-emitting dye (i.e., dopant) that can emit different wavelength spectra, and may also include a host material (Host). The light-emitting layer can be a monochrome light-emitting layer that emits a single color such as red, green, and blue. A plurality of monochrome light-emitting layers of different colors can be arranged in a plane according to a pixel pattern, or they can be stacked together to form a color light-emitting layer. When light-emitting layers of different colors are stacked together, they can be separated from each other or connected to each other. The light-emitting layer can also be a single color light-emitting layer that can simultaneously emit different colors such as red, green, and blue.

[0167] According to different technologies, the light-emitting layer material can be made of different materials such as fluorescent electroluminescent materials, phosphorescent electroluminescent materials, and thermally activated delayed fluorescent materials. In an OLED device, a single light-emitting technology can be used, or a combination of multiple different light-emitting technologies can be used. These different light-emitting materials classified by technology can emit light of the same color or different colors.

[0168] In one aspect of the present invention, the light-emitting layer adopts phosphorescent electroluminescence technology, and the main material of the light-emitting layer is selected from, but not limited to, one or more combinations of GPH-1 to GPH-80.

[0169]

[0170]

[0171]

[0172]

[0173] In one aspect of the present invention, the light-emitting layer adopts phosphorescent electroluminescence technology. The phosphorescent dopant of the light-emitting layer can be selected from, but not limited to, one or more combinations of GPD-1 to GPD-47 listed below.

[0174]

[0175]

[0176]

[0177] Where D is deuterium.

[0178] In one aspect of the present invention, the light-emitting layer adopts phosphorescent electroluminescence technology. The phosphorescent dopant of the light-emitting layer can be selected from, but not limited to, one or more combinations of RPD-1 to RPD-28 listed below.

[0179]

[0180]

[0181] In one aspect of the present invention, the light-emitting layer adopts phosphorescent electroluminescence technology. The phosphorescent dopant of the light-emitting layer can be selected from, but not limited to, one or more combinations of YPD-1 to YPD-11 listed below.

[0182]

[0183] The OLED organic material layer may further include an electron transport region between the light emitting layer and the cathode. The electron transport region may be a single-layer electron transport layer (ETL), including a single-layer electron transport layer containing only one compound and a single-layer electron transport layer containing multiple compounds. The electron transport region may also be a multilayer structure including at least one layer of an electron injection layer (EIL), an electron transport layer (ETL), and a hole blocking layer (HBL).

[0184] In one aspect of the present invention, the electron transport layer material can be selected from, but not limited to, one or more combinations of ET-1 to ET-57 listed below.

[0185]

[0186]

[0187]

[0188] The device may also include an electron injection layer located between the electron transport layer and the cathode. The electron injection layer material includes but is not limited to one or more combinations of the following: LiQ, LiF, NaCl, CsF, Li2O, Cs2CO3, BaO, Na, Li and Ca.

[0189] The technical scheme of the present invention is further illustrated by specific examples below. Those skilled in the art should understand that the examples are only to help understand the present invention and should not be regarded as specific limitations of the present invention.

[0190] Device Example 1

[0191] The preparation process of the organic electroluminescent device in this embodiment is as follows:

[0192] The glass plate coated with the ITO transparent conductive layer (as the anode) was ultrasonically treated in a commercial cleaning agent, rinsed in deionized water, ultrasonically degreased in a mixed solvent of acetone:ethanol, baked in a clean environment until the water was completely removed, cleaned with ultraviolet light and ozone, and bombarded with a low-energy cation beam;

[0193] Place the glass substrate with the anode in a vacuum chamber and evacuate the chamber to a vacuum of less than 1×10 -5 Pa, vacuum evaporating HI-3 on the above anode layer as a hole injection layer, the evaporation rate is 0.1nm / s, and the evaporation film thickness is 10nm;

[0194] HT-4 was vacuum-deposited on the hole injection layer as the hole transport layer of the device, with a deposition rate of 0.1 nm / s and a total deposition film thickness of 80 nm.

[0195] Compound P1 synthesized in Synthesis Example 1 was vacuum-deposited on the hole transport layer as the electron blocking layer material of the device. The deposition rate was 0.1 nm / s and the total deposition film thickness was 80 nm.

[0196] The light-emitting layer of the device is vacuum-evaporated on the electron blocking layer. The light-emitting layer includes a main material and a dye material. The evaporation rate of the main material GPH-59 is adjusted to 0.1nm / s by a multi-source co-evaporation method. The evaporation rate of the dye RPD-8 is set to 3% of the main material. The total film thickness of the evaporation is 30nm.

[0197] The electron transport layer materials ET-46 and ET-57 of the device are vacuum-deposited on the light-emitting layer, with a mass ratio of 1:1, a deposition rate of 0.1 nm / s, and a total deposition film thickness of 30 nm;

[0198] LiF with a thickness of 0.5 nm was vacuum-evaporated on the electron transport layer (ETL) as an electron injection layer, and an Al layer with a thickness of 150 nm was used as the cathode of the device.

[0199] Example 2-15

[0200] The manufacturing process of Examples 2-15 is the same as that of Example 1, except that the electron blocking layer material compound P1 is replaced by the compounds shown in Table 1.

[0201] Comparative Examples 1-4

[0202] The preparation process of Comparative Examples 1-4 is the same as that of Example 1, except that the electron blocking layer material compound P1 is replaced by compounds R-1 to R-4, respectively. The structures of the compounds used in the comparative examples are as follows:

[0203]

[0204] The organic electroluminescent device prepared by the above process was subjected to the following performance tests:

[0205] At the same brightness, a digital source meter (Keithley 2400) and a brightness meter (ST-86LA brightness meter, Beijing Normal University Optoelectronic Instrument Factory) and a brightness meter were used to measure the driving voltage and current efficiency of the organic electroluminescent devices prepared in Examples 1-15 and Comparative Examples 1-4. Specifically, the voltage was increased at a rate of 0.1 V per second, and the brightness of the organic electroluminescent device was measured when it reached 3000 cd / m 2 The voltage at this time is the driving voltage, and the current density at this time is measured at the same time; the ratio of brightness to current density is the current efficiency. The test results are shown in Table 1.

[0206] Table 1:

[0207]

[0208]

[0209] It can be seen from the data in Table 1 that when the compound of the present invention is used as an electron blocking layer material of an organic electroluminescent device, the brightness of the device reaches 3000 cd / m 2 When the driving voltage is as low as 4.3V or less, the current efficiency is as high as 16.8cd / A or more, which can effectively reduce the driving voltage and improve the current efficiency. It is an electron blocking layer material with good performance.

[0210] The only difference between the compound R-1 of comparative example 1 and the compound P18 of example 3 is that the structural formula of the compound R-1 is a 2-biphenyl substituted at the 6-position of the naphthalene ring, and the structural formula of P18 is a 2-biphenyl substituted at the 1-position of the naphthalene ring. When the compound R-1 is used as an electron blocking material for an organic electroluminescent device, the driving voltage of the device is 6.7V and the current efficiency is 8.5cd / A, which are worse than those of example 3, which may be attributed to the better hole transport performance and relatively higher triplet energy level of the compound P18 of the present invention.

[0211] The only difference between the compound R-2 of Comparative Example 2 and the compound P115 of Example 7 is that the structural formula of the compound R-2 is a 3-biphenyl substituted at the 6-position of the naphthalene ring, and the structural formula of P115 is a 3-biphenyl substituted at the 1-position of the naphthalene ring. When the compound is used as an electron blocking material for an organic electroluminescent device, the driving voltage of the device is 6.3V and the current efficiency is 9.4cd / A, which are worse than those of Example 7, which may be attributed to the better hole transport performance and relatively higher triplet energy level of the compound P115 of the present invention.

[0212] The difference between the compound R-3 of comparative example 3 and the compound P33 of example 5 is that the structural formula of the compound R-3 is that the 1-position of the naphthalene ring is substituted with 10-(9-phenyl)-naphthyl, and the structural formula of P33 is that the 2-position biphenyl is substituted with the 1-position of the naphthalene ring. When the compound is used as an electron blocking material of an organic electroluminescent device, the driving voltage of the device is 5.8V and the current efficiency is 11.2cd / A, which are worse than those of example 5, which may be attributed to the better hole transport performance of the compound P33 of the present invention.

[0213] The compound R-4 of comparative example 4 is compared with the compound P31 in example 4, and the difference is that the 1-naphthyl substitution is in the 1-position of the naphthalene ring of the structural formula of the compound R-4, and the structural formula of the compound P31 is in the 1-position of the naphthalene ring. When the compound is used as an electron blocking material of an organic electroluminescent device, the driving voltage of the device is 3.1V and the current efficiency is 19.3cd / A. Compared with P31, R-4 has better hole transport performance due to the 1-naphthyl substitution at the 1-position of the naphthalene ring, and thus has a lower driving voltage, but P31 has a relatively higher triplet state and spatial stacking structure, and thus exhibits better current efficiency.

[0214] It can be seen from this that in the compounds provided by the present invention, the substitution position of the 1-position of the naphthylamine is an important factor that enables the compound to bring about excellent performance when applied to organic electroluminescent devices.

[0215] The present invention uses the above-mentioned embodiments to illustrate the compounds of the present invention and their application in OLED devices, but the present invention is not limited to the above-mentioned embodiments, that is, it does not mean that the present invention must rely on the above-mentioned embodiments to be implemented. Those skilled in the art should understand that any improvement of the present invention, equivalent replacement of various raw materials of the product of the present invention, addition of auxiliary components, selection of specific methods, etc., all fall within the protection scope and disclosure scope of the present invention.

Claims

1. A compound of the general formula, as shown in the following formula (1): in, L 1 , L 2 Each independently represents a single bond, a substituted or unsubstituted C6-C 30 arylene, substituted or unsubstituted C3~C 30 One of the heteroarylene groups; Ar 1 ,Ar 2 Each independently represents a substituted or unsubstituted C6 to C 30 Aryl, substituted or unsubstituted C3~C 30 One of the heteroaryl groups; Ar 3 Selected from one of the following groups: Among them, the expression of the ring structure crossed by "—" indicates that the connection site is at any position on the ring structure that can form a bond, and "*" represents the access position of the group; R 1 , R 2 Each independently represents a single substituent to the maximum permissible substituent, each independently selected from hydrogen, substituted or unsubstituted C1-C 20 Alkyl, substituted or unsubstituted C1~C 20 substituted or unsubstituted C1-C6 ether group, substituted or unsubstituted C6-C 30 Aryl, substituted or unsubstituted C3~C 30 One of the heteroaryl groups; R 1 , R 2 They are independently connected to the parent nucleus by single bonds; When the above groups have substituents, the substituents are selected from halogen, C1-C 20 chain alkyl, C1-C6 alkoxy, C1-C6 thioalkoxy, C6-C 30 A monocyclic aromatic group or a condensed aromatic group, a C3~C 30 One or a combination of at least two of a monocyclic heteroaryl group or a condensed-ring heteroaryl group.

2. The compound of the general formula according to claim 1, as shown in one of the following formulas (2-1), (2-2) or (2-3): in, Ar 1 ,Ar 2 ,Ar 3 , R 1 , R 2 , L 1 and L 2 The definition of is the same as in the general formula (1).

3. The compound of the general formula according to claim 1, as shown in the following formula (2-1):

4. A compound of the general formula according to any one of claims 1 to 3, wherein Ar 1 ,Ar 2 Each is independently selected from one of the following substituted or unsubstituted groups: phenyl, biphenyl, terphenyl, naphthyl, phenanthryl, anthracenyl, dibenzofuranyl, dibenzothiophenyl, carbazolyl, 9,9-dimethylfluorenyl, 9,9-diphenylfluorenyl, spirofluorene, triphenylene, fluoranthene, benzo-9,9-dimethylfluorenyl, benzospirofluorene; When the above groups have substituents, the substituents are selected from halogen, C1-C 20 chain alkyl, C1-C6 alkoxy, C1-C6 thioalkoxy, C6-C 30 A monocyclic aromatic group or a condensed aromatic group, a C3~C 30 One or a combination of at least two of a monocyclic heteroaryl group or a condensed-ring heteroaryl group.

5. A compound of the general formula according to any one of claims 1 to 3, wherein R 1 and R 2 At least one of them is hydrogen.

6. A compound of the general formula according to any one of claims 1 to 3, wherein R 1 and R 2 At the same time, it is hydrogen.

7. A compound of the general formula according to any one of claims 1 to 3, wherein L 1 and L 2 At least one of them is a single bond.

8. According to any one of the general formula compounds described in claim 1-3, L 1 and L 2 It is also a single bond.

9. The compound of the general formula according to claim 1 is selected from the following specific structural compounds:

10. Use of the compound of the general formula according to claim 1 or 2 as an electron blocking layer material in an organic electroluminescent device.

11. An organic electroluminescent device, comprising a first electrode, a second electrode and one or more organic layers inserted between the first electrode and the second electrode, characterized in that: The organic layer comprises at least one compound according to any one of claims 1 to 9.

12. An organic electroluminescent device according to claim 11, wherein the organic layer comprises a hole transport layer and / or an electron blocking layer, characterized in that: The electron blocking layer comprises at least one compound according to any one of claims 1 to 9.