An ultrasonic laminated transducer for detecting viscoelastic solids
By designing an ultrasonic stacked transducer including a piezoelectric wafer stack structure, and using matching layers and backing materials to optimize sound energy conversion, the problem of sound energy attenuation in viscoelastic solid detection is solved and higher detection is achieved. resolution and detection effects.
Patent Information
- Application Number
- CN202111036790.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-09-06
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2041-09-06
AI Technical Summary
Due to the large attenuation of sound energy when detecting viscoelastic solids, existing ultrasonic transducers cannot meet normal detection needs and cannot be directly used for flaw detection of industrial components.
An ultrasonic laminated transducer including a shell, insulating material, backing, piezoelectric wafer, matching layer, conductive copper sheet, ground wire and cable joint is designed. It adopts a stack structure of four 4MHz piezoelectric wafers. Optimize sound energy conversion and propagation through matching layers and backing materials to improve the incident efficiency of sound energy.
It effectively improves the detection resolution of ultrasonic waves in viscoelastic solids, overcomes the attenuation characteristics of sound energy, achieves better detection results, and can be used in industrial flaw detection.
Smart Images

Figure CN113686972B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of viscoelastic solid detection equipment, and in particular relates to an ultrasonic laminated transducer for detecting viscoelastic solids. Background Art
[0002] A transducer is a device that converts electrical energy into acoustic energy. Common ultrasonic transducers convert electrical energy into ultrasonic waves for underwater communications. According to relevant literature at home and abroad, the current piezoelectric chip stacking technology is mainly used in underwater acoustic transducers. Since there are significant differences in structure between underwater acoustic transducers and industrial component flaw detection transducers, underwater acoustic transducers are not directly used for flaw detection of industrial components. No relevant applications were found in ultrasonic flaw detection transducers. When underwater transducers are used to detect viscoelastic solids, due to the large attenuation of acoustic energy, their performance indicators are greatly reduced and cannot meet normal needs.
[0003] For plane simple harmonic waves in infinite viscoelastic media, the solution can be obtained according to the correspondence principle of simple harmonic wave problems. That is, as long as the elastic material constant is replaced by the viscoelastic material complex function in the elastic solution, the solution of the wave equation of the viscoelastic solid can be obtained, where the longitudinal wave solution is:
[0004]
[0005] The shear wave solution is:
[0006]
[0007] or
[0008]
[0009] From the above formula, we can see that the viscoelastic solution and the elastic solution are the same in form, except that λ and μ are replaced by λ. * (iω) and μ * (iω), but it has a significant impact on the characteristics of wave propagation, mainly manifested as follows:
[0010] 1) Assume that the viscoelastic longitudinal wave and transverse wave velocities are c Lv 、c Tv ,but
[0011]
[0012] Because λ * (iω) and μ * (iω) are all functions of ω, so c Lv 、c Tv They are all functions of the angular frequency ω. Therefore, when waves propagate in viscoelastic media, dispersion (chromatic dispersion, diffusion) will occur.
[0013] 2) In an ideal elastic medium, plane waves do not attenuate, but in a viscoelastic medium, plane waves attenuate as the propagation distance increases. If the attenuation coefficients of the longitudinal and transverse waves are denoted by α L , α T , then
[0014]
[0015] Here, Re represents the real part of the complex number, and Im represents the imaginary part of the complex number.
[0016] From the above research results, it can be seen that compared with elastic solids, when ultrasonic waves propagate in viscoelastic solids, they cause greater energy attenuation due to dispersion and viscoelastic properties, which brings great challenges to the ultrasonic detection of viscoelastic solids. If you want to obtain the same detection resolution as elastic solids, you need to develop high-energy ultrasonic transducers. Summary of the invention
[0017] The object of the present invention is to provide an ultrasonic laminated transducer for detecting viscoelastic solids, which has good detection effect and is suitable for flaw detection and material property characterization of viscoelastic solids.
[0018] To achieve the above-mentioned purpose, the solution of the present invention is: an ultrasonic stacked transducer for detecting viscoelastic solids, comprising a shell, an insulating material, a backing, a piezoelectric chip, a matching layer, a conductive copper sheet, a ground wire, a signal line and a cable connector, the shell being provided with an inner cavity, a matching layer being provided at the bottom of the inner cavity, a chip group being provided above the matching layer, the chip group being composed of a stack of four 4MHz piezoelectric chips, a conductive copper sheet being sandwiched between two adjacent piezoelectric chips, surfaces of two adjacent piezoelectric chips with the same polarity facing each other, and the piezoelectric chip being a circular solid structure; the backing being provided above the chip group, the inner cavity above the backing being filled with insulating material, the cable connector being provided outside the shell, and the cable connector being connected to both ends of the electrode of the chip group through the signal line and the ground wire respectively.
[0019] Preferably, the piezoelectric chip is made of PT material.
[0020] Preferably, the conductive copper sheet and the piezoelectric chip are bonded by epoxy resin.
[0021] After adopting the above scheme, the beneficial effect of the present invention is that the present invention fills the gap in the field of ultrasonic transducers for viscoelastic solid detection. For viscoelastic solid materials with a large attenuation amplitude, the present invention not only overcomes this characteristic, but also has a better detection effect. The high gain can better compensate for the high attenuation characteristics of ultrasonic waves when propagating in viscoelastic solids, and can effectively improve the resolution of ultrasonic detection of viscoelastic solids, so that the transducer of the present invention can be fully competent in industrial flaw detection. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 It is a schematic diagram of the structure of the transducer of the present invention;
[0023] Figure 2 is the amplitude-frequency relationship of the viscoelastic material of the present invention (wherein the actual line represents the viscoelastic material and the dotted line represents the elastic material);
[0024] Figure 3 It is a schematic structural diagram of a piezoelectric chip group composed of four identical piezoelectric chips of the present invention, which are connected in parallel in a circuit;
[0025] Figure 4 is an electromechanical equivalent circuit diagram of a single piezoelectric chip of the present invention;
[0026] Figure 5 is an electromechanical equivalent circuit diagram of the stacked piezoelectric wafer of the present invention;
[0027] Figure 6 It is a schematic diagram of the resonant frequency graphical method of the present invention;
[0028] Figure 7 It is a schematic diagram of a simulation model of a transducer of the present invention;
[0029] Figure 8 It is a schematic diagram of the sound field energy of a conventional transducer;
[0030] Fig. 9 Schematic diagram of the sound field energy of the transducer of the present invention;
[0031] Fig.10 It is the time domain waveform of a conventional transducer;
[0032] Fig.11 It is the time domain waveform diagram of the transducer of the present invention.
[0033] Description of labels:
[0034] Shell 1, insulating material 2, backing 3, piezoelectric chip 4, matching layer 5, conductive copper sheet 6, ground wire 7, signal wire 8, cable connector 9, viscoelastic solid 10. DETAILED DESCRIPTION
[0035] The present invention is described in detail below with reference to the accompanying drawings and specific embodiments.
[0036] The present invention provides an ultrasonic laminated transducer for detecting viscoelastic solids, such as Figure 1As shown, it includes a shell 1, an insulating material 2, a backing 3, a piezoelectric chip 4, a matching layer 5, a conductive copper sheet 6, a ground wire 7, a signal line 8 and a cable connector 9. The shell 1 is used to protect the internal components of the transducer. The shell 1 is provided with an inner cavity, a matching layer 5 is provided at the bottom of the inner cavity, and a chip group is provided above the matching layer 5. The chip group is composed of four 4MHz piezoelectric chips 4 stacked together. The piezoelectric chip 4 mainly realizes the conversion between electrical energy and acoustic energy. The matching layer 5 is used to alleviate the difference in acoustic impedance between the piezoelectric chip 4 and the object to be detected, so that the acoustic energy generated by the piezoelectric chip 4 can be incident on the object to be detected as much as possible. The matching layer is also called the acoustic membrane. Its thickness is generally d = 1 / 4λ. In this way, the half-wave loss and path difference in the reflection process make the reflected waves of the two interfaces in front and behind the acoustic membrane have opposite phases and cancel each other out, and the accumulated superposition effect of the residual waves in the acoustic membrane makes the transmitted wave stronger. In addition, there is a requirement for the acoustic impedance z of the acoustic membrane. After the acoustic membrane is added between the two media, the total transmittance is t = 2*z / (z1+z)*2*z2 / (z+z2). To maximize the total transmittance, z2 = z1*z2 should be satisfied. The raw material formula of the matching layer needs to be developed according to the acoustic impedance value of the object to be detected, so that the acoustic energy can be incident on the object to be detected to the maximum extent.
[0037] The conductive copper sheet 6 is sandwiched between two adjacent piezoelectric chips 4. The surfaces of the two adjacent piezoelectric chips 4 with the same polarity are opposite to each other. The conductive copper sheet 6 is used to realize the parallel connection of the electrodes between the piezoelectric chips 4. The piezoelectric chip 4 is a circular solid structure, which is different from the piezoelectric chip of the underwater acoustic transducer which is annular or curved. The backing 3 is arranged above the chip group. The backing 3 is used to control the vibration degree of the piezoelectric chip 4 on the one hand, and to absorb the acoustic energy on the back of the piezoelectric chip 4 on the other hand. In order to reduce the specific gravity of the reflected wave, the acoustic impedance of the backing is required to be close to the acoustic impedance of the stacked piezoelectric chips. The proportions of tungsten powder, epoxy resin, curing agent, adhesive, etc. in the backing material are different, and the acoustic impedance of the obtained backing material is very different. Epoxy resin and tungsten powder are configured with epoxy tungsten powder in a mass ratio of 1:6. After adjustment, a hot air blower is used to heat and remove bubbles.
[0038] The inner cavity above the backing 3 is filled with insulating material 2, and the insulating material 2 plays an insulating role between the components below the backing and the shell 1. The cable connector 9 is arranged outside the shell 1, and the cable connector 9 is respectively connected to the two ends of the electrode of the chip group through the signal line 8 and the ground line 7. The ground line 7, the signal line 8 and the cable connector 9 realize the transmission of ultrasonic signals. During the operation of the ultrasonic transducer, on the one hand, an excitation pulse is generated by the transmitting / receiving circuit, which is transmitted to the piezoelectric chip group through the signal line 8 and the ground line 7 through the cable connector 9, and the piezoelectric chip group is driven to vibrate to generate ultrasonic waves, thereby realizing the conversion of electrical energy into acoustic energy; on the other hand, when the ultrasonic wave propagates in the detected object, it will be reflected, and the ultrasonic transducer receives the reflected sound wave and converts it into a pulse signal, which is then transmitted to the transmitting / receiving circuit through the signal line 8 and the ground line 7 through the cable connector 9 to form an ultrasonic echo signal, and the material characteristics of the detected object and whether the internal structure has damaged parts are judged according to the echo signal.
[0039] The present invention designs an ultrasonic laminated transducer according to the above structure, which is also called an industrial flaw detection laminated transducer, an ultrasonic laminated piezoelectric transducer, etc. For viscoelastic solid materials, there is a relationship between the echo amplitude of the ultrasonic wave and the frequency of the transducer. Figure 2 The linear relationship shown. Figure 2 It can be seen that for elastic materials (dashed line in the figure), as the transducer frequency increases, the amplitude of the ultrasonic echo signal decreases linearly at a certain proportion. For viscoelastic materials (solid line in the figure), as the transducer frequency increases, the amplitude of the ultrasonic echo signal decays rapidly. When the frequency is 3MHz, the amplitude of the ultrasonic echo signal almost decays to 0. Therefore, for the detection of viscoelastic materials, the frequency of the ultrasonic transducer should be as low as possible to ensure the amplitude of the ultrasonic echo signal. Therefore, 1MHz is selected as the resonant frequency of the laminated transducer in this case.
[0040] The natural resonant frequency of a single piezoelectric chip mainly depends on the thickness of the piezoelectric chip 4 and the propagation speed of ultrasonic waves in the chip material. In order to obtain a higher acoustic-to-electric conversion efficiency, the piezoelectric chip 4 must work in a resonant state. According to the standing wave theory, the chip thickness is half of the wavelength, that is:
[0041]
[0042] Where, t is the thickness of the wafer, in mm; λ L --The wavelength of the longitudinal wave in the chip, in mm; c L --The velocity of the longitudinal wave in the chip, in m / s; f 0 --The natural frequency of the chip, in Hz.
[0043] Since the radial vibration energy of PT material is small and the vibration energy in the thickness direction is large, it is beneficial for industrial flaw detection. Therefore, the flaw detection stacked transducer uses a piezoelectric chip 4 made of PT material, and its longitudinal wave sound velocity is 4350m / s. When designing the structure of the stacked transducer, four 4MHz chips are stacked in parallel, and a 0.2mm thick copper sheet is placed between the stacked chips. This ensures good electrical conductivity and facilitates the welding of electrode leads. When the natural frequency is 4MHz, according to formula (1), the chip thickness is 0.54375mm. While ensuring high emission energy, the frequency of the stacked transducer reaches 1MHz. The stacked structure of piezoelectric chips 4 is shown in Figure 3 As shown, during the stacking process, the surfaces of the piezoelectric chips 4 with the same polarity face each other, and a conductive copper sheet 6 is placed in the middle and bonded with an adhesive. In order to obtain a better sound transmission effect, the adhesive is made of epoxy resin.
[0044] Whether the actual resonance frequency of the stacked four piezoelectric chips 4 reaches the ideal resonance frequency of 1MHz is verified by calculation below. It is more convenient to use cylindrical coordinates for the thickness vibration of the thin disc (i.e., the piezoelectric chip 4). The electrodes are plated on two circular surfaces perpendicular to the z-axis, and the polarization direction is the z-axis. The corresponding relationship between the basic coordinates of the piezoelectric chip 4 and the cylindrical coordinates is:
[0045]
[0046] Since the piezoelectric chip 4 is a thin sheet (i.e., the thickness of the chip is much smaller than the wavelength within the operating frequency range), the upper and lower electrode surfaces are free, and the shear stress T zr 、T zθ 、T zz and the axial displacement component ξ z is zero, that is:
[0047]
[0048] The chip is subjected to axisymmetric vibration. The geometric shape, constraint and external force of the primitive are symmetrical about the z-axis. Then all stress components, strain components and displacement components are also symmetrical about the z-axis. At this time, each component is only a function of r and z and has nothing to do with θ. Then:
[0049]
[0050] The equation of motion is simplified to
[0051]
[0052] The relationship between strain and displacement is simplified to
[0053]
[0054] Since the electric field is applied on the z-axis, ignoring the boundary effect of the electric field, only E 3 ≠0, the piezoelectric equation is simplified to
[0055]
[0056] Solve T r and T θ get
[0057]
[0058] In the formula is Young's modulus under constant electric field, is the Poisson coefficient under constant electric field.
[0059] The mechanical vibration equation is
[0060]
[0061] Where F is the circumferential force, ρ is the density, is the wave propagation speed, S = 2πat, k = ω / v is the wave number, ω = 2πf is the angular frequency, f is the resonance frequency, J 0 (ka) is a zero-order first-class Bessel function, J 1 (ka) is a first-order first-type Bessel function, is the circular vibration speed, is the electromechanical conversion coefficient, and V is the voltage applied to the chip.
[0062] The circuit state equation is
[0063]
[0064] In the formula is the two-dimensional cut-off capacitance.
[0065] The electromechanical equivalent diagram of a single piezoelectric chip 4 can be obtained from the mechanical vibration equation and the circuit state equation, as shown in Figure 4 shown.
[0066] If the piezoelectric chip 4 is in free vibration, that is, F = 0, the resonance frequency equation can be obtained as follows:
[0067] J 0 (ka)=(1-σ)J 1 (ka)
[0068] From this, the admittance equation of a single piezoelectric chip 4 can be derived as
[0069]
[0070] For a piezoelectric chip group consisting of p identical piezoelectric chips 4, they are connected in parallel in circuit and in series in mechanics. From the circuit theory, it is to cascade p identical four-terminal networks. According to the cascade theory in the circuit, the electromechanical equivalent circuit diagram of the stacked piezoelectric chips 4 can be obtained, as shown in Figure 5 shown.
[0071] The stacked transducer is formed by stacking piezoelectric chips 4 to form a cylindrical radiation surface, and each piezoelectric chip 4 is connected in parallel. Therefore, the admittance of the stacked transducer is the superposition of the admittances of each piezoelectric chip 4. Since the material properties and dimensions of each piezoelectric circular chip are the same, the admittance equation of four piezoelectric chips 4 stacked can be derived based on the admittance equation of a single piezoelectric chip 4:
[0072]
[0073] According to the definition of resonant frequency, when Y→∞, the transducer enters the resonant state, and the vibration frequency at this time is the resonant frequency of the transducer. From the admittance equation of the stack transducer, it can be seen that to meet the condition of Y→∞, it is only necessary to transcend the equation kaJ 0 (ka)=(1-σ)J 1 The value of (ka) is the resonant frequency of the stacked transducer with four piezoelectric chips 4. The radius a of the piezoelectric chip 4 is 12 mm, and the flexibility constant of the piezoelectric chip 4 is Density ρ=7500kg / m 3 , to obtain The resonant frequency of the stacked transducer can be calculated by graphical method, such as Figure 6 shown.
[0074] From the figure, it can be concluded that the resonant frequency of the transducer formed by stacking four 4MHz piezoelectric chips 4 is 1MHz, which is consistent with the actual measured value of 1.03MHz, with a relative error of 0.3%.
[0075] The gain effect of the present invention is:
[0076] The circular laminated transducer is an axisymmetric structure, so a simplified structural model can be used, that is, taking a quarter of the transducer structure. This not only ensures the accuracy requirements but also reduces the simulation calculation time. Figure 7 As shown, it is mainly composed of a viscoelastic solid 10, a piezoelectric chip 4 (PT) and a conductive copper sheet 6. The radius of the sector-shaped area formed by the viscoelastic solid 10 is 36 mm; the radius of the piezoelectric chip 4 is 12 mm, the thickness is 0.5 mm, and the frequency is 4 MHz; the radius of the conductive copper sheet 6 is 12 mm, and the thickness is 0.2 mm. The parameters of the materials used in the simulation process are shown in the following table.
[0077] Material <![CDATA[Density (kg / m 3 )]]> Longitudinal wave speed (m / s) Poisson's ratio Viscoelastic materials 1500 2000 0.5 PT Materials 7750 4350 0.34 Copper Sheet 8600 4700 0.37
[0078] During the simulation, under the condition of comprehensive consideration of accuracy and calculation speed, one wavelength is divided into 10 units. Symmetric boundary conditions are added in the x direction, the polarization directions of adjacent piezoelectric chips 4 are opposite, the upper surface of the piezoelectric chip 4 is loaded with Volt=1, and the lower surface is grounded. The simulation results of the conventional single-chip chip transducer are shown in Figure 2. Figure 8 As shown, the simulation results of the four-chip stacked transducer of the present invention are as follows Fig. 9 As shown in the figure, it can be seen that the acoustic field energy distribution of the laminated transducer is more concentrated than that of the conventional transducer, and the gain is 25dB higher. Therefore, the high gain of the laminated transducer can better compensate for the high attenuation characteristics of ultrasonic waves when propagating in viscoelastic solids, and to a certain extent, it can effectively improve the resolution of ultrasonic detection of viscoelastic solids.
[0079] The time domain waveform of a conventional monolithic chip transducer is as follows: Fig.10 As shown, the time domain waveform of the four-chip stacked transducer of the present invention is as follows Fig.11 As shown. During the experiment, the sample to be tested was 35mm thick industrial rubber, and the penetration method was used to obtain a better waveform amplitude. It can be seen from the experimental results that for industrial rubber of the same thickness, the gain of the conventional transducer is 35.6dB, and the gain of the stacked transducer is 20.4dB. That is, the gain of the stacked transducer is 15.2dB higher than that of the single-chip transducer, which is 25dB lower than the simulation result. The main reason is that in order to reduce the amount of calculation during the simulation, some edge effects and losses are ignored. Therefore, the 1MHz four-stack transducer proposed in the present invention can ensure the defect resolution of the viscoelastic solid ultrasonic detection method.
[0080] Compared with the underwater acoustic transducer, the transducer in this case has the following four different characteristics:
[0081] (1) The upper part of the piezoelectric chip stack. The industrial flaw detection transducer is a backing material, which is used to control the vibration of the chip on the one hand and absorb the acoustic energy on the back of the chip on the other hand; the underwater acoustic transducer is a rubber sheet and a metal cover plate, which are used to protect the piezoelectric chip and prevent the reverse propagation of acoustic energy.
[0082] (2) Piezoelectric chip stacking. The chip shape of the industrial flaw detection stacked transducer is circular, which is determined by the thickness vibration mode. The chip shape of other transducers is annular, which is determined by the radial vibration mode.
[0083] (3) The lower part of the piezoelectric chip stack. The industrial flaw detection transducer is a matching layer, and its acoustic impedance is generally the product of the acoustic impedance of the piezoelectric chip stack and the acoustic impedance of the object being tested, so that as much acoustic energy as possible is incident on the object being tested; the underwater acoustic transducer is a rubber sheet and a metal cover plate, which are used to protect the piezoelectric chip and adjust the sound field radiation angle.
[0084] (4) Application scenarios. The 1MHz laminated ultrasonic transducer proposed in the present invention is mainly used for flaw detection and material property characterization of viscoelastic solids. The hydroacoustic transducer is mainly used for underwater communications in the ocean.
[0085] The above description is only a preferred embodiment of the present invention and is not a limitation on the design of this case. Any equivalent changes made based on the design key of this case shall fall within the protection scope of this case.
Claims
1. An ultrasonic laminated transducer for detecting viscoelastic solids, characterized in that: The invention comprises a shell, an insulating material, a backing, a piezoelectric chip, a matching layer, a conductive copper sheet, a ground wire, a signal wire and a cable connector. The shell is provided with an inner cavity, a matching layer is arranged at the bottom of the inner cavity, a chip group is arranged above the matching layer, the chip group is composed of four 4MHz piezoelectric chips stacked, the piezoelectric chip is made of PT material, the longitudinal wave sound velocity is 4350m / s, the radius of the piezoelectric chip is 12mm, a conductive copper sheet is sandwiched between two adjacent piezoelectric chips, the surfaces of the two adjacent piezoelectric chips with the same polarity are opposite, the piezoelectric chip is a circular solid structure, and the frequency of the stacked transducer reaches 1MHz while ensuring high emission energy; the backing is arranged above the chip group, in the backing material, epoxy resin and tungsten powder are configured in a mass ratio of 1:6, so that the acoustic impedance of the backing and the stacked piezoelectric chips is close; the inner cavity above the backing is filled with insulating material, the cable connector is arranged outside the shell, and the cable connector is connected to the two ends of the electrode of the chip group through the signal line and the ground line respectively.
2. An ultrasonic laminated transducer for detecting viscoelastic solids as claimed in claim 1, characterized in that: The conductive copper sheet and the piezoelectric chip are bonded together by epoxy resin.
Citation Information
Patent Citations
Stacked piezoelectric smart aggregate for health monitoring of concrete structure
CN106770653A
Nondestructive detection method of composite insulator
CN107478728A
Embedded type ultrasonic sensor arranged in cement concrete structure
CN108332846A
Piezoelectric intelligent aggregates with adjustable resonant frequency
CN108802197A
Ultrasonic imaging method for polymer bonded explosive surface crack detection and device
CN109781865A