Electrostatic adsorption process

By controlling the sequence of DC voltage and RF power and process gas flow in semiconductor device manufacturing, combined with the design of the base surface of the multi-layer pillar structure, the problem of substrate damage during adsorption and desorption is solved and the stability and yield of production are improved. .

CN113748227BActive Publication Date: 2024-10-29APPLIED MATERIALS INC
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202080030601.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-04-14
Publication Date
2024-10-29
Estimated Expiration
2040-04-14

AI Technical Summary

Technical Problem

In semiconductor device manufacturing, as chip design complexity and circuit density increase, the adsorption and desorption process of the substrate on the electrostatic chuck can easily lead to substrate damage and photolithography defocus, affecting production yield.

Method used

By controlling the application sequence of DC voltage and RF power and the flow of process gases in the process chamber, the stability of the substrate during adsorption and processing is ensured, and damage caused by accidental movement and thermal expansion is prevented. The base surface design of the multi-layer column structure is adopted to Improve heat transfer uniformity.

Benefits of technology

It effectively reduces damage to the backside of the substrate, improves photolithography defocus rate and production yield, extends the service life of the process chamber, and improves deposition uniformity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113748227B_ABST
    Figure CN113748227B_ABST
Patent Text Reader

Abstract

One or more embodiments described herein generally relate to methods for attaching a substrate to an electrostatic chuck used in a semiconductor processing system and deattaching a substrate from the electrostatic chuck. Generally, in the embodiments described herein, the method includes: (1) applying a first voltage from a direct current (DC) power source to an electrode disposed in a susceptor; (2) directing a process gas into a process chamber; (3) applying power from a radio frequency (RF) power source to a showerhead; (4) performing a process on the substrate; (5) stopping applying the RF power; (6) removing the process gas from the process chamber; and (7) stopping applying the DC power.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] One or more embodiments described herein relate generally to semiconductor processing systems, and more particularly, to methods for absorbing a substrate into and desorbing a substrate from an electrostatic chuck used in a semiconductor processing system. Background Art

[0002] Electrostatic suction (ESC) pedestals (commonly referred to as electrostatic chucks) are used in semiconductor device manufacturing to firmly hold a substrate in a processing position within a processing space of a process chamber using an electrostatic suction force. The suction force varies with the potential between a DC voltage supplied to a suction electrode embedded in a dielectric material of the pedestal and a substrate disposed on a surface of the dielectric material.

[0003] In the manufacture of semiconductor devices, integrated circuits have evolved into complex devices that can include millions of transistors, capacitors, and resistors on a single chip. The evolution of chip design continues to require greater circuit density, which will result in increased substrate curvature in multi-stacked structures. Flattening the substrate to the base surface facilitates fixing the substrate during the plasma process and ensures that the correct radio frequency (RF) is coupled to the ground to extend the service life of the chamber and uniform film deposition. As the distance between the substrate and the adsorption electrode increases, the loss of adsorption force becomes a danger. In this way, a higher electrostatic adsorption voltage is required to clamp the substrate to the base surface. The higher electrostatic adsorption voltage may cause DC plasma discharges adjacent to the substrate. The DC plasma discharge may damage the substrate during processing.

[0004] In addition, the development of chip design has led to modified pedestal surface designs that include multiple points where the substrate contacts the pedestal surface, commonly referred to as posts. However, although the posts are expected to provide repeatable contact to minimize particle defects on the back side of the substrate, the substrate can often become damaged or cracked during conventional processing due to the modified structure of the pedestal surface. When the position of the substrate is not properly controlled, the posts may cause damage at a higher rate to increase the electrostatic adsorption voltage. Damage on the back side of the substrate at the posts causes lithographic defocusing and significantly affects production yield.

[0005] Accordingly, there is a need for a method of adsorbing and desorbing a substrate onto an electrostatic chuck to reduce lithography defocus and yield loss by eliminating backside damage. Summary of the invention

[0006] One or more embodiments described herein generally relate to methods for absorbing a substrate into and desorbing a substrate from an electrostatic chuck used in a semiconductor processing system.

[0007] In one embodiment, a method for processing a substrate in a process chamber includes: applying a direct current to an electrode disposed in a susceptor, the substrate being disposed on the susceptor in the process chamber; flowing one or more process gases into the process chamber after applying the direct current to the electrode; applying radio frequency (RF) power to a showerhead in the process chamber after flowing one or more process gases into the process chamber; processing the substrate after applying the RF power; stopping the application of the RF power after processing the substrate; removing the one or more process gases from the process chamber after stopping the application of the RF power; and stopping the application of the DC power after removing the one or more process gases.

[0008] In another embodiment, a method for processing a substrate includes: (a) positioning the substrate on a surface of a pedestal, wherein the pedestal is at a first spacing from a showerhead; (b) applying a DC voltage at a first DC voltage level to an electrode disposed within the pedestal; (c) flowing one or more process gases into the process chamber through the showerhead; (d) applying RF power at a first RF power level to the showerhead within the process chamber; (e) increasing the DC voltage and the RF power to a second DC voltage level and a second RF power level before, during, or both before and during processing of the substrate; (f) reducing the DC voltage and the RF power to a third DC voltage level and a third RF power level after processing the substrate; (g) moving the pedestal within the process chamber to a second spacing from the showerhead; (h) ceasing the application of RF power to the showerhead; (i) removing the one or more process gases from the process chamber; and (j) ceasing the application of the DC voltage to the electrode.

[0009] In yet another embodiment, a method for processing a substrate includes: positioning the substrate on a surface of a pedestal, wherein the pedestal is at a first spacing from a showerhead in a process chamber; applying a DC voltage to an electrode disposed in the pedestal at a first DC voltage; flowing a first process gas into the process chamber through the showerhead after applying the DC voltage at the first DC voltage level; applying RF power to the showerhead in the process chamber at a first radio frequency (RF) power level; moving the pedestal to a second spacing from the showerhead, wherein the second spacing is closer to the showerhead than the first spacing; flowing a second process gas mixture into the process chamber through the showerhead; before, during, or both before and during execution of a process on the substrate, increasing the DC voltage and the RF power to a second DC voltage level and a second RF power level; reducing the DC voltage and the RF power to a third DC voltage level and a third RF power level after performing the process on the substrate; flowing the first process gas into the process chamber through the nozzle while removing the second process gas mixture from the process chamber after performing the process on the substrate; moving the susceptor in the process chamber to a third interval from the nozzle; stopping the application of the RF power; removing the first process gas from the process chamber after stopping the application of the RF power; and stopping the application of the DC power after removing the first process gas from the process chamber. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] In order that the manner in which the above-mentioned features of the present disclosure may be understood in detail, a more particular description of the present disclosure may be given (briefly summarized above) by reference to embodiments, some of which are illustrated in the accompanying drawings. It should be noted, however, that the drawings illustrate only typical embodiments of the present disclosure and are therefore not to be considered limiting of its scope, as the present disclosure may admit to other equally effective embodiments.

[0011] Figure 1 is a schematic cross-sectional view of a process chamber according to at least one embodiment described herein;

[0012] Figure 2A According to at least one embodiment described herein Figure 1 A top plan view of a patterned surface of a base;

[0013] Figure 2B According to at least one embodiment described herein Figure 2A a cross-sectional view of a base; and

[0014] FIG. 3A to FIG. 3B Methods 300A and 300B are depicted according to embodiments described herein.

[0015] Figure 4 is a graph showing the relationships of process parameters at operations within the methods disclosed herein. DETAILED DESCRIPTION

[0016] In the following description, many specific details are set forth to provide a more thorough understanding of the embodiments of the present disclosure. However, it will be apparent to those skilled in the art that one or more embodiments of the present disclosure may be practiced without one or more of the specific details. In other examples, well-known features are not described to avoid confusing one or more embodiments of the present disclosure.

[0017] One or more embodiments described herein generally relate to methods for adsorbing a substrate to an electrostatic chuck used in a semiconductor processing system and desorbing a substrate from an electrostatic chuck. In the embodiments described herein, a susceptor in a process chamber has a modified susceptor surface, including multiple points at which the substrate contacts the susceptor surface, commonly referred to as pillars. In a conventional method for adsorbing a substrate to a modified susceptor surface, a first process gas is introduced into a process chamber. Then, RF power is generated from a radio frequency (RF) power source to generate an RF plasma in the process chamber. Thereafter, a DC voltage is generated from a direct current (DC) power source to an electrode disposed in the susceptor to apply a DC electrostatic adsorption bias to adsorb the substrate to the susceptor surface by an electrostatic adsorption force. After adsorbing the substrate, a process is performed on the substrate in the process chamber. After the process, the DC electrostatic adsorption is turned off, and then the RF power is turned off. Once the DC electrostatic adsorption and the RF power are turned off, the gas flow into the process chamber is stopped.

[0018] However, the above conventional method causes a high degree of movement of the substrate when the gas is introduced without the adsorption force, which may cause the substrate to crack. In addition, in the conventional method, backside damage may occur when the substrate is subjected to a force that causes the substrate to move relative to the posts on the susceptor surface. The force may be due to movement or due to thermal expansion. In the case of thermal expansion, when the substrate expands or contracts relative to the susceptor surface, the difference between the temperature of the substrate and the susceptor surface at the posts may cause local damage.

[0019] In a method for adsorbing a substrate to a modified susceptor surface as described in an embodiment of the present invention, first, a DC voltage is generated from a direct current (DC) power source to an electrode disposed in the susceptor, and the substrate is adsorbed to the susceptor surface by an electrostatic adsorption force. After the substrate is adsorbed using the electrostatic adsorption force, a first process gas can be introduced into the process chamber. After the first process gas is introduced, RF power is generated from an RF power source to generate an RF plasma in the process chamber. Applying an adsorption force before generating an RF plasma advantageously controls the position of the substrate, preventing the substrate from being broken or damaged by accidental movement of the substrate on the susceptor surface during the introduction of the first process gas. In addition, applying an adsorption force first can reduce lithography defocusing by eliminating backside damage, thereby improving yield.

[0020] After applying RF power to generate RF plasma, a process is performed on the substrate. The process may be a deposition process, an etching process, a thermal process, or another process. After performing the process on the substrate, the RF power is turned off. After the RF power is turned off, the first process gas stops flowing into the process chamber. After stopping the gas flow, the electrostatic adsorption force is turned off before removing the substrate from the process chamber.

[0021] In general, in the embodiments described herein, the method generally applies the following sequence: (1) applying a first voltage from a direct current (DC) power source to an electrode disposed within a susceptor; (2) introducing a process gas into a process chamber; (3) applying a second voltage from an RF power source; (4) performing a deposition (or other) process on a substrate; (5) ceasing to apply the second voltage from the RF power source; (6) removing the process gas from the process chamber; and (7) ceasing to apply DC power from the DC power source.

[0022] Figure 1 1 is a schematic cross-sectional view of a process chamber 100 according to one embodiment described herein. The process chamber 100 is a plasma enhanced chemical vapor deposition (PECVD) process, but it is contemplated that other process chambers may benefit from the aspects described herein. An exemplary process chamber that may benefit from the embodiments described herein is a PECVD-enabled chamber available from Applied Materials, Inc. of Santa Clara, California. It is contemplated that other similarly equipped process chambers, including process chambers from other manufacturers, may also benefit from the embodiments described herein.

[0023] The process chamber 100 includes a chamber body 102, a susceptor 104 disposed inside the chamber body 102, and a lid assembly 106 coupled to the chamber body 102 and enclosing the susceptor 104 in a processing region 120. The lid assembly 106 includes a gas distributor 112. A substrate 107 is provided to the processing region 120 via an opening 126 (such as a slit valve) formed in the chamber body 102.

[0024] An insulator 110 (being a dielectric material, such as a ceramic or a metal oxide, such as aluminum oxide and / or aluminum nitride) separates a gas distributor 112 from the chamber body 102. The gas distributor 112 includes an opening 118 for allowing process gas to enter the processing region 120. The process gas is supplied to the process chamber 100 through a conduit 114, and the process gas enters a gas mixing region 116 before flowing through the opening 118. An exhaust port 152 is formed in the chamber body 102 at a location below the susceptor 104. The exhaust port 152 may be connected to a vacuum pump (not shown) to remove unreacted substances and byproducts from the process chamber 100.

[0025] The gas distributor 112 is coupled to a power source 141, such as an RF generator. The power source 141 supplies continuous and / or pulsed RF power to the gas distributor 112. During operation, the power source 141 is turned on to supply electrical power to the gas distributor 112 to facilitate forming a plasma in the processing region 120.

[0026] The pedestal 104 is formed of a ceramic material, such as a metal oxide or nitride or oxide / nitride mixture, such as aluminum, aluminum oxide, aluminum nitride, or an aluminum oxide / aluminum nitride mixture. The pedestal 104 is supported by a shaft 143. The pedestal 104 is electrically grounded. An electrode 128 is embedded in the pedestal 104. The electrode 128 may be a plate, a perforated plate, a mesh, a wire mesh, or any other distributed arrangement. The electrode 128 is coupled to an electrical power source 132 via a connection 130. The electrical power source 132 supplies power to the electrode 128. In some embodiments, the electrode 128 facilitates electrostatic adsorption of the substrate 107, so that the pedestal 104 acts as an electrostatic chuck. When the electrode 128 acts as an electrostatic chuck, the electrical power source 132 can be used to control the properties of the plasma formed in the processing region 120, or to facilitate the generation of plasma within the processing region 120. The pedestal 104 includes a patterned surface 142 for supporting the substrate 107. The pedestal 104 also includes a pocket 140. The pocket 140 may alternatively be an edge ring. The substrate 107 and the pocket 140 are concentrically disposed on a surface 142 of the base 104 .

[0027] The power source 141, the base 104, and the electric power source 132 may all be connected to a controller 150. The controller 150 controls the application of power to each of the power source 141, the base 104, and the electric power source 132. The controller 150 may increase or decrease the power supplied to each of the power source 141, the base 104, and the electric power source 132. The controller 150 may integrate the use of the power source 141, the base 104, and the electric power source 132 so that the power supply to each of the power source 141, the base 104, and the electric power source 132 is coordinated. In some embodiments, each of the power source 141, the base 104, and the electric power source 132 may be connected to a separate controller 150. In embodiments where each of the power source 141, the base 104, and the electric power source 132 is connected to a different controller, each of the controllers 150 may communicate with each other via a wired connection or a wireless connection.

[0028] Figure 2A is an embodiment having a patterned surface 142 Figure 1 A top plan view of the base 104 is shown. Figure 2A The base 104 shown in FIG. 1 includes a peripheral ledge 202 surrounded by a pocket 140. The patterned surface 142 includes two separate regions, such as a central region 200 surrounded by a peripheral region 205. The patterned surface 142 includes a plurality of posts 210 having an upper surface 215 defining a substrate receiving surface 220. The posts 210 in the central region 200 may have a different height than the posts 210 in the peripheral region 205. The upper surface 215 of each of the plurality of posts 210 is substantially coplanar. Figure 2B The relative heights of the pillars 210 within the central region 200 and the peripheral region 205 are shown in more detail in FIG.

[0029] Each of the plurality of pillars 210 is shown as a rectangle in plan view, but the pillars 210 may be circular, oval, hexagonal, or other shapes in plan view. In some embodiments that may be combined with other embodiments, the central region 200 has a surface area that is smaller than the surface area of ​​the peripheral region 205. For example, if the diameter of the patterned surface 142 is about 12 inches, the surface area of ​​the peripheral region 205 is about 113 square inches, and the surface area of ​​the central region 200 is about 11 square inches. In some embodiments that may be combined with other embodiments, the surface area of ​​the peripheral region 205 is about 900% greater than the surface area of ​​the central region 200. The upper surface 215 of each of the plurality of pillars 210 includes a surface roughness (average surface roughness or Ra) of about 20 micro-inches to about 60 micro-inches, such as about 30 micro-inches to about 50 micro-inches or about 35 micro-inches to about 45 micro-inches. In some embodiments, the upper surface 215 of each of the plurality of pillars 210 includes a surface roughness of about 40 micro-inches. The patterned surface 142 also includes lift pin holes 212. Lift pin holes 212 are located within the perimeter region of the patterning surface 142 and are spaced between the posts 210. The lift pin holes 212 are used with corresponding lift pins (not shown) to lower and raise the substrate during transfer to / from the process chamber 100.

[0030] Figure 2B yes Figure 2A A cross-sectional view of the base 104. Figure 2B As shown in , the plurality of posts 210 include a plurality of first posts 225A in the peripheral region 205 and a plurality of second posts 225B in the central region 200. The height 230 of each of the plurality of first posts 225A is greater than the height 235 of the plurality of second posts 225B. The height 230 and the height 235 are measured from the upper surface or the base surface 232 of the base 104. In some embodiments, the height 230 of each of the plurality of first posts 225A is about 0.002 inches to about 0.0024 inches, such as about 0.0022 inches. In some embodiments that can be combined with other embodiments, the height 235 of each of the plurality of second posts 225B is about 0.0005 inches to about 0.0007 inches, such as about 0.0006 inches. Although only two different heights (i.e., height 230 and height 235) of the posts 210 are shown, the patterned surface 142 may include other multiple posts at heights different from the height 230 and the height 235.

[0031] The difference in height 230 and 235, and / or the difference in surface area of ​​central region 200 and peripheral region 205 changes the heat transfer rate between susceptor 104 and the susceptor thereon. The modified heat transfer rate modifies the temperature profile of the substrate. In some embodiments, the difference in height 230 and 235 and / or the difference in surface area of ​​central region 200 and peripheral region 205 improves the temperature uniformity in the substrate, which improves the deposition uniformity on the substrate. In some embodiments, making the height 235 of each of the plurality of second pillars 225B less than the height 230 of each of the plurality of first pillars 225A increases the temperature in the center of the substrate. Increasing the temperature at the center of the substrate can improve the temperature uniformity of the entire substrate, which improves the deposition uniformity on the substrate.

[0032] The heights 230 and 235 of the pillars 210 make the base surface 232 of the base 104 a multi-level structure. For example, the base surface 232 of the central region 200 defines an elevated surface 240 compared to the base surface 232 of the peripheral region 205, which is referred to as a recessed surface 245. Figure 2B The raised surface 240 and the recessed surface 245 of the base 104 shown in FIG. 1 define a profile, such as an inverted or reversed U-shaped profile 250 .

[0033] Figure 3A A method 300A according to embodiments described herein is depicted. In operation 302, a substrate 107 is positioned on a susceptor 104 in a process chamber 100. During positioning of the substrate 107 on the susceptor 104, the susceptor 104 is in a substrate receiving position and the substrate 107 is in a pre-processing position. When the susceptor 104 is in the substrate receiving position, the susceptor is at a distance of about 3500 mils to about 5000 mils from a gas distributor, such as about 3750 mils to about 4750 mils, such as about 4000 mils to about 4500 mils. While the substrate 107 is positioned on the susceptor 104, the process chamber 100 is purged using a first process gas. Purging the process chamber 100 removes unwanted gases and contaminants from the process space and fills the process chamber with a first process gas having a high threshold ionization energy. The first process gas is introduced at a rate of about 1000 sccm to about 3000 sccm, such as about 1500 sccm to about 2500 sccm. The introduction of the first process gas is gradually reduced and then stopped at the end of operation 302 and after the substrate 107 is positioned on the susceptor 104 .

[0034] In operation 304, the electrical power source 132 is turned on after operation 302. In operation 304, the process chamber 100 is filled with a first process gas, such as helium from operation 302. The electrical power source 132 is a DC power source, which applies a DC voltage to the electrode 128 in the pedestal 104 and adsorbs the substrate 107 to the patterned surface 142. The DC voltage may be a first DC voltage level of about 300 volts to about 1000 volts, such as about 300 volts to about 600 volts, such as about 300 volts to about 500 volts, such as about 350 volts to about 450 volts, such as about 400 volts. Adsorbing the substrate 107 provides the advantage of controlling the position of the substrate 107 before subsequent operations in the method, and helps prevent the substrate 107 from moving. The stability of the substrate 107 prevents backside damage that may occur when the substrate 107 moves because the movement causes forces between the pillars 210 on the patterned surface 142 and the substrate 107. The DC voltage disclosed herein mitigates undesirable electrostatic discharge of the first process gas within the process chamber and further introduced in operation 306 , particularly when used in combination with other disclosed process parameters, such as gas composition, internal chamber pressure, and substrate spacing.

[0035] In operation 306, one or more first process gases flow into the process chamber 100 via the gas distributor 112. Operation 306 is performed after operation 304. The first process gas may include helium or other similar process gases. Using helium provides the advantage of having a higher thermal conductivity, which helps to flatten local temperature variations on the patterned surface 142, which can help prevent backside damage through uniform thermal expansion. It is expected that other process gases can be used instead of helium as the first process gas. The first process gas has a high threshold energy to eliminate ionization during substrate adsorption. Helium provides a high bias breakdown medium for DC discharge, which improves stability when the susceptor 104 is spaced farther from the gas distributor 112. When compared under process conditions similar to those described herein, helium exhibits a much higher bias breakdown voltage than gases such as argon. When comparing the amount of defects on the substrate when using helium, it is found that the amount of defects on the substrate can be reduced by between 90% and 95% compared to using argon as the first process gas.

[0036] The first gas is introduced at a rate of about 1 sccm to about 10,000 sccm, such as about 1 sccm to about 4,000 sccm, such as about 1,000 sccm to about 3,000 sccm, such as about 2,000 sccm. In some embodiments, the flow rate of the process gas entering the process chamber 100 during operation 306 may be ramped up from an initial flow rate of about 0 sccm to a final flow rate described in one of the above ranges. The ramping up of the process gas further minimizes movement of the substrate.

[0037] During operation 306, the pressure within the chamber is increased to a pressure of about 5 Torr to about 15 Torr, such as about 6 Torr to about 12 Torr, such as about 7 Torr to about 10 Torr. The pressure within the chamber is maintained at that pressure during substrate processing.

[0038] In operation 308, the electrical power source 141 is turned on. Operation 308 is performed after operation 306. The electrical power source 141 may be an RF generator that applies RF power to the gas distributor 112. The RF power may be a first RF power level and in the range of about 100 Watts to about 6000 Watts, such as about 150 Watts to about 3000 Watts, such as about 200 to about 2000 Watts, such as about 250 and about 500 Watts, such as about 350 Watts.

[0039] In operation 314, when performing substrate processing on substrate 107, the DC voltage and RF power are both increased to a second DC voltage level and a second RF power level. Substrate processing may include a deposition process or a treatment process. In some embodiments, substrate 107 is subjected to an oxidation process. Figure 3B ) and operation 312( Figure 3B ), the DC voltage and RF power may be increased after operation 310 or operation 312. In embodiments where operation 310 and operation 312 are not used, the DC voltage and RF power may be increased after operation 308. The second DC voltage level is about 800 volts to about 1100 volts, such as about 900 volts to about 1050 volts, such as 950 volts to about 1000 volts. In some embodiments, the second DC voltage level may be about 980 volts. The RF power is increased to a second RF power level. The second RF power level is about 1000 watts to about 4000 watts, such as about 2000 watts to about 3000 watts, such as about 2250 watts to about 2750 watts. In some embodiments, the second RF power level may be about 2450 watts. Substrate processing is performed during or after the DC voltage and RF power are increased to the second DC voltage level and the second RF power level. In some embodiments, substrate processing is performed both during and after the DC voltage and RF power are increased to the second DC voltage level and the second RF power level.

[0040] In operation 316, the DC voltage and the RF power are both reduced to a third DC voltage level and a third RF power level. In operation 314, the reduction in DC voltage and RF power is accompanied by the cessation of the substrate processing performed on the substrate 107. In some embodiments that can be combined with other embodiments, the DC voltage and RF power are reduced after the substrate processing is performed so that the third DC voltage level and the third RF power level are at the same DC voltage and RF power level as the first DC voltage level and the first RF power level of operation 314. The third DC voltage level is about 300 volts to about 1000 volts, such as about 300 volts to about 600 volts, such as about 300 volts to about 500 volts, such as about 350 volts to about 450 volts, such as about 400 volts. The third RF power level is about 100 watts to about 6000 watts, such as about 150 watts to about 3000 watts, such as about 200 to about 2000 watts, such as about 250 and about 500 watts, such as about 350 watts. In these embodiments, at this stage of the method 300, the amount of RF power supplied is higher than in conventional methods, which provides a more stable transition from the higher RF power used when performing substrate processing. This facilitates improved temperature stability to prevent backside damage.

[0041] In operation 322, the power source 141 is turned off, so that the application of RF power to the gas distributor 112 is stopped. By turning off the RF power, the generation of plasma within the process chamber 100 may be stopped.

[0042] In operation 324, the flow of the first gas into the process chamber is stopped. In operation 324, the first gas may be removed from the process chamber 100. The first gas is removed from the process chamber 100 while DC power is still supplied to the electrode 128 within the susceptor 104. By stopping the flow of the first gas while supplying DC power to the electrode 128, movement of the substrate 107 caused by exhaust of the process chamber 100 is minimized. The pressure within the process chamber 100 may be substantially reduced to a pressure close to vacuum during operation 324. Operation 324 is performed after operation 322. Also during the removal of the first gas from the process chamber 100, the pressure within the process chamber 100 is reduced. The pressure within the process chamber 100 is reduced to a predetermined pressure, such as less than about 5 Torr, such as less than about 3 Torr, such as less than about 2 Torr, such as less than about 1 Torr.

[0043] In operation 326, the power source 132 is turned off after operation 324. When the power source 132 is turned off, the application of the DC voltage stops, and the adsorption of the substrate 107 on the patterned surface stops. Once the adsorption of the substrate 107 stops, the substrate 107 can be removed from the patterned surface 142.

[0044] Figure 3B A method 300B is depicted according to embodiments described herein. Figure 3B Method 300B is similar to Figure 3A 300A, but may include several additional process operations, such as operation 303, operation 310, operation 312, operation 318, and operation 320 as described herein.

[0045] In optional operation 303 ( Figure 3B ), the susceptor 104 is moved from the substrate receiving position to a first spacing from the gas distributor. The first spacing is about 200 mils to about 3000 mils from the gas distributor 112, such as about 200 mils to about 1000 mils, such as about 450 mils to about 750 mils. In some embodiments, the susceptor 104 is spaced about 550 mils from the gas distributor 112, although other positions are possible. The selected spacing facilitates the adsorption of the substrate without accidentally generating plasma.

[0046] In optional operation 310 ( Figure 3B ), the susceptor 104 is moved within the process chamber 100 to be positioned closer to the gas distributor 112. As previously described, operation 310 is performed between operations 308 and 310. In this embodiment, the susceptor 104 is moved to a second spacing. The second spacing is between about 200 mils and about 400 mils from the gas distributor 112, such as about 250 mils to about 350 mils, such as about 300 mils from the gas distributor 112.

[0047] Operation 312 is performed after or simultaneously with operation 310. In optional operation 312 ( Figure 3B ), a second process gas mixture flows into the process chamber 100 via the gas distributor 112, while the first process gas is stopped from flowing into the process chamber 100. In some embodiments, the first process gas may be removed from the process chamber 100 during the above operation. The second process gas mixture includes one or more carrier gases and process / deposition gases, such as a mixture of argon and propylene. Other carrier gases and process / deposition gases may also be used, such as nitrogen, ethylene, oxygen, tungsten hexafluoride, diborane, tungsten, pentacarbonyl 1-methylbutyl isonitrile, silane, or nitrous oxide. The second gas mixture flows into the process chamber 100 at a rate of about 1 sccm to about 10,000 sccm (such as about 1 sccm to about 4,000 sccm, such as about 1,000 sccm to about 4,000 sccm, such as about 2,500 sccm).

[0048] In some exemplary embodiments, which may be combined with other embodiments, the ramp-up of the second gas mixture flowing into the process chamber 100 is about 10 sccm / s to 1000 sccm / s. In some embodiments, the flow rate of the first gas entering the process chamber 100 is reduced by the same rate as the flow rate of the second gas mixture flow is increased. This enables the pressure within the process chamber 100 to remain constant during the transition from the first gas to the second gas mixture flow.

[0049] In embodiments where the second gas mixture is a mixture of argon and propane, the ratio of argon gas to propane gas flowing into the process chamber 100 may be between about 3:1 and about 10:1, such as between about 4:1 and about 8:1, such as between about 5:1 and about 7:1. In embodiments where other precursor gases are used, similar ratios of inert gas to reactive gas may be used.

[0050] In some embodiments, which may be combined with other embodiments, operation 310 and operation 312 may be performed simultaneously such that the second gas mixture is introduced while the susceptor 104 is moved to a new position.

[0051] Operation 318 is performed after operation 316 and before operation 320. In operation 318, the first gas mixture flows into the process chamber 100 via the gas distributor 112, while the second gas mixture is removed from the process chamber 100. At the end of operation 318, the flow rates of the first gas mixture and the second gas mixture are the same as the flow rates used in operation 306. In some embodiments, the flow rate of the second gas mixture in the process chamber 100 may be about 0 sccm or close to about 0 sccm at the end of operation 318. At the end of operation 318, the first gas may be flowed at a rate of about 1 sccm to about 10,000 sccm, such as about 1 sccm to about 4,000 sccm, such as about 1,000 sccm to about 3,000 sccm, such as about 2,000 sccm.

[0052] In optional operation 320, the pedestal 104 is moved within the process chamber 100 to a third spacing that is farther from the gas distributor 112 than the second spacing. In some embodiments, the third spacing between the pedestal 104 and the gas distributor 112 is about 450 mils to about 750 mils, such as about 500 mils to about 700 mils, such as about 550 mils to about 650 mils, such as about 600 mils from the gas distributor 112. Operation 320 may be performed after or simultaneously with operation 318. Moving the pedestal 104 to the third spacing increases the breakdown potential required to generate a DC plasma arc. By moving the pedestal 104 to the third spacing that is greater than the second spacing before operation 320, plasma generation within the process chamber 100 is stopped or reduced and application of RF power is stopped before operation 322.

[0053] In method 300A and method 300B, operations 302, 304, 306, 308, 310, 312, 314, 316, 318, 320, 322, 324, 326 are described as being performed sequentially. In alternative embodiments, several operations of method 300A and method 300B may be performed simultaneously. In some embodiments, operation 310 and operation 312 are performed simultaneously. In some exemplary embodiments, operation 322 and operation 324 are performed simultaneously.

[0054] After the RF power is turned off, the DC clamping voltage supplied by the power source 132 is turned off, so that the position of the substrate 107 on the patterned surface 142 can be controlled throughout operations 302, 304, 306, 308, 310, 312, 314, 316, 318, 310, 322, and 324. Position control helps stabilize the temperature of the substrate 107 relative to the patterned surface 142, thereby helping to prevent backside damage caused by the displacement of the substrate 107 during processing. In addition, after the RF power is turned off, the DC clamping voltage remains elevated at the DC clamping voltage described in operation 316, which is sufficient to hold the substrate 107 in position without discharging the plasma. Another benefit of the method described herein is the time it takes to complete the process. One aspect of obtaining and maintaining thermal equilibrium is time. Since the clamping voltage is applied throughout operations 304, 306, 308, 310, 312, 314, 316, 318, 320, 322, and 322, position control is improved. Improved position control allows the substrate 107 to be attracted and acted upon by the heater for a longer period of time. The extended time allows the substrate 107 to relax around the posts 210 and prevents backside damage.

[0055] For operations 304 to 326, it is beneficial to control the position of the substrate 107 on the patterned surface 142. Previous attempts to adsorb the substrate 107 before moving the substrate 107 to the second interval resulted in a DC-based electrostatic discharge of the first gas. The electrostatic discharge of the first gas can cause hardware damage and substrate defects. The method proposed herein prevents the electrostatic discharge of the first gas and allows the substrate 107 to be adsorbed earlier in the method.

[0056] Figure 4 4 is a graph 400 showing process parameter relationships for operations within the methods disclosed herein. Graph 400 shows process conditions for a spacing 402 between the susceptor 104 and the gas distributor 112, a pressure 404 within the process chamber 100, a flow rate of a first process gas 406, a flow rate of a carrier gas 408, a flow rate of a second process / deposition gas 410, an applied DC clamping voltage 412, and an applied RF power 414 during different times within performing the methods described herein. Graph 400 shows process parameters for one embodiment of operations 302, 304, 306, 308, 310, 312, 314, 316, 318, 310, 322, 324, and 326. However, other process configurations are contemplated.

[0057] Graph 400 is only one exemplary embodiment of how the processing parameters and the relationship of each processing parameter may be used. In other embodiments, each parameter may follow a different path over time. In some embodiments, the slope of each parameter may be greater or less than the slope of the parameters disclosed herein. In some embodiments, operations 302, 304, 306, 308, 310, 312, 314, 316, 318, 310, 322, 324, and 326 may be slightly rearranged, and some operations not disclosed in graph 400 may be performed simultaneously.

[0058] The combination of spacing, pressure, process gas, and adsorption voltage used in the methods described herein allows for adsorption of substrates during the introduction and movement of the substrates. One or more combinations of these factors mitigate against accidental plasma formation and electrostatic discharge adjacent to the substrate. Since accidental plasma formation and electrostatic discharge lead to hardware damage and substrate defects, the methods herein provide improved processing over conventional methods. In the aspects disclosed herein, the spacing, pressure, gas composition, and / or adsorption voltage are controlled to prevent the process gas from arcing and accidentally forming a plasma.

[0059] While the foregoing is directed to embodiments of the present invention, other and further embodiments of the invention may be devised without departing from the basic scope thereof, and the scope of the invention is determined by the claims that follow.

Claims

1. A method for processing a substrate in a process chamber, comprising: applying a direct current to an electrode disposed in a susceptor, the substrate being disposed on the susceptor in the process chamber; flowing one or more first process gases including helium into the process chamber after applying the direct current to the electrode; After flowing the one or more first process gases into the process chamber through a showerhead within the process chamber, applying radio frequency (RF) power to the showerhead at a first RF power level; flowing one or more second process gases into the process chamber while removing the one or more first process gases from the process chamber; applying a plasma generated from at least one of the one or more first process gases and the one or more second process gases to the substrate after applying the RF power at the first RF power level; at least one of before or during applying the plasma to the substrate, increasing the RF power to a second RF power level; after increasing the RF power to the second RF power level, flowing the one or more first process gases into the process chamber while removing the one or more second process gases from the process chamber; after applying the plasma to the substrate, stopping the applying of the RF power; removing the one or more first process gases from the process chamber after said ceasing said applying of RF power; as well as After removing the one or more first process gases after the stopping of the applying of RF power, the applying of the direct current is stopped.

2. The method of claim 1, wherein applying the direct current to the electrode further comprises: A DC voltage of 300 volts to 500 volts is applied, and applying the RF power to the showerhead further includes applying a power of 100 watts to 6000 watts. 3 . The method of claim 2 , wherein during the processing of the substrate, a pressure within the process chamber is 5 to 15 Torr, and a spacing between the showerhead and the pedestal is 450 mils to 750 mils.

4. A method for processing a substrate, comprising the following operations in sequence: (a) positioning the substrate on a surface of a susceptor in a process chamber, wherein the susceptor is at a first spacing from a showerhead; (b) applying a DC voltage at a first DC voltage level to an electrode disposed in the base to adsorb the substrate; (c) flowing one or more first process gases including helium into the process chamber; (d) applying RF power to the showerhead in the process chamber at a first RF power level; (e) flowing one or more second process gases into the process chamber while removing the one or more first process gases from the process chamber; (f) at least one of increasing the DC voltage and the RF power to a second DC voltage level and a second RF power level before or during applying a plasma generated by at least one of the one or more first process gases and the one or more second process gases to the substrate; (g) after applying the plasma to the substrate, reducing the DC voltage and the RF power to a third DC voltage level and a third RF power level; (h) flowing the one or more first process gases into the process chamber while removing the one or more second process gases from the process chamber; (i) moving the susceptor in the process chamber to a second distance from the showerhead; (j) stopping the application of the RF power to the showerhead; (k) removing the one or more first process gases from the process chamber; as well as (1) Stopping the application of the DC voltage to the electrodes.

5. The method of claim 4, wherein the first interval is 450 mils to 750 mils.

6. The method of claim 4, wherein the second interval is 200 mils to 400 mils.

7. The method of claim 4, wherein the first DC voltage level is 300 volts to 500 volts.

8. The method of claim 4, wherein the first RF power level is 100 Watts to 6000 Watts.

9. The method of claim 4, wherein the second DC voltage level is 800 volts to 1100 volts.

10. The method of claim 4, wherein the second RF power level is 1000 Watts to 4000 Watts.

11. The method of claim 4, wherein a pressure within the process chamber during the substrate processing is 5 Torr to 15 Torr.

12. The method of claim 4, wherein the third DC voltage level is 300 volts to 500 volts.

13. A method for processing a substrate, comprising: positioning the substrate on a surface of a susceptor, wherein the susceptor is spaced a first distance from a showerhead within a process chamber; applying a DC voltage to an electrode disposed in the base at a first DC voltage; flowing a first process gas including helium into the process chamber through the showerhead after applying the DC voltage at a first DC voltage level; applying radio frequency (RF) power to the showerhead within the process chamber at a first RF power level; moving the base to a second interval from the nozzle, wherein the second interval is closer to the nozzle than the first interval; flowing a second process gas mixture including at least one of tungsten hexafluoride, diborane, tungsten, or pentacarbonyl 1-methylbutyl isonitrile into the process chamber through the showerhead while removing the first process gas from the process chamber; at least one of before or during applying a plasma generated by at least one of the first process gas and the second process gas mixture to the substrate, increasing the DC voltage and the RF power to a second DC voltage level and a second RF power level; reducing the DC voltage and the RF power to a third DC voltage level and a third RF power level after applying the plasma to the substrate; after applying the plasma to the substrate, flowing the first process gas into the process chamber through the showerhead while removing the second process gas mixture from the process chamber; Moving the susceptor in the process chamber to a third distance from the showerhead; stopping said applying of said RF power; removing the first process gas from the process chamber after stopping the applying of the RF power; as well as After stopping the applying of the RF power, after removing the first process gas from the process chamber, stopping the applying of the DC voltage.

14. The method of claim 13, wherein the pedestal is spaced between 450 and 750 mils from the showerhead at the first spacing.

15. The method of claim 14, wherein the first DC voltage level is 300 volts to 500 volts.

16. The method of claim 13, wherein after flowing the first process gas into the process chamber, a pressure within the process chamber during the substrate processing is between 5 Torr and 15 Torr.

17. The method of claim 15, wherein the second DC voltage level is 800 volts to 1100 volts and the second process gas mixture further comprises argon, propylene, or both argon and propylene.

Citation Information

Patent Citations

  • Plasma processing method and apparatus

    US20100025372A1

  • Method and apparatus for ESC charge control for wafer clamping

    US20160027620A1

  • Method for improved sputter etch processing

    US6057244A