Systems for flip chip laser bonding

Through the pressure and infrared measurement and control technology of the laser bonding system, the problem of poor solder bump contact caused by bending or warping of the semiconductor wafer is solved, efficient flip-chip laser bonding is achieved, and bonding quality and production efficiency are improved.

CN113748492BActive Publication Date: 2024-10-29PROTEC CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN201980095881.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-06-05
Publication Date
2024-10-29
Estimated Expiration
2039-06-05

AI Technical Summary

Technical Problem

Flip-chip semiconductor wafers bend or warp due to thinning and temperature changes during the installation process, resulting in poor solder bump contact and affecting the quality of the bonding process.

Method used

Using a laser bonding system, through the cooperation of a pressure mask and an infrared camera, the laser beam and infrared transmitting part (made of BaF2 or ZnSe and other materials) are used to pressurize and temperature measure and control the semiconductor wafer to ensure the solder bumps Proper contact and even heating.

Benefits of technology

It effectively prevents poor contact of solder bumps, ensures that bent or warped semiconductor wafers are successfully bonded to the substrate under pressure, and improves bonding quality and production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113748492B_ABST
    Figure CN113748492B_ABST
Patent Text Reader

Abstract

The present invention relates to a flip chip laser bonding system and a flip chip laser bonding system, and more particularly to a flip chip laser bonding system for bonding a semiconductor chip in a flip chip form to a substrate using a laser beam. The flip chip laser bonding system of the present invention has the following effects: by bonding a semiconductor chip to a substrate by laser in a pressurized state, a semiconductor chip that is bent or may be bent can be bonded to a substrate without poor contact of solder bumps.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a flip chip laser bonding system, and more particularly to a flip chip laser bonding system for bonding a semiconductor wafer in a flip chip form to a substrate using a laser beam. Background Art

[0002] As electronic products become smaller, flip-chip semiconductor chips that do not use wire bonding are widely used. The flip-chip semiconductor chip is mounted on a substrate in the following manner: a plurality of electrodes in the form of solder bumps are formed on the lower surface of the semiconductor chip and bonded to positions corresponding to the solder bumps formed on the substrate.

[0003] As described above, there are roughly two methods for mounting a semiconductor chip on a substrate in a flip chip manner: a reflow method and a laser bonding method. The reflow method is a method in which a semiconductor chip is bonded to a substrate by reflowing at high temperature while a semiconductor chip coated with flux on solder bumps is arranged on a substrate. Similar to the reflow method, the laser bonding method is a method in which a laser beam is irradiated on a semiconductor chip while a semiconductor chip coated with flux on solder bumps is arranged on a substrate to transfer energy, thereby instantly melting the solder bumps and then solidifying the semiconductor chip while bonding the semiconductor chip to the substrate.

[0004] Recently, there is a trend that the thickness of the semiconductor wafers used in flip-chip form has become thinner to less than tens of microns. As mentioned above, when the semiconductor wafer is thin, there are many cases where the semiconductor wafer is slightly bent or warped due to the internal stress of the semiconductor wafer itself. As mentioned above, when the semiconductor wafer is deformed, there will be a situation where the solder bumps of the semiconductor wafer are bonded to the corresponding solder bumps of the substrate in a non-contact state. This situation leads to a defect in the semiconductor wafer bonding process. In addition, when the temperature of the semiconductor wafer and the substrate rises to bond the semiconductor wafer to the substrate, the semiconductor wafer or the substrate may be partially bent or warped due to the difference in the thermal expansion coefficient of the material inside the material. This phenomenon also leads to a defect in the semiconductor wafer bonding process. Summary of the invention

[0005] Problems to be solved by the invention

[0006] The present invention is proposed to solve the above-mentioned problems, and its purpose is to provide a flip-chip laser bonding system, which can prevent poor contact of solder bumps and effectively bond a bent or warped semiconductor chip or a semiconductor chip that may be bent or warped due to temperature rise to a substrate.

[0007] Means of solving problems

[0008] The flip-chip laser bonding system of the present invention for achieving the above-mentioned purpose is characterized in that it includes: a supply unit for supplying a substrate, wherein the substrate is in a state where a plurality of semiconductor chips are arranged to be bonded to the upper surface of the substrate; a fixing unit for receiving the substrate from the supply unit and fixing the lower surface of the substrate; a laser unit including a laser head for irradiating a laser beam to the substrate fixed to the fixing unit to bond the semiconductor chip to the substrate, and a laser transfer unit for transferring the laser head; a mask including a transmission unit, wherein the transmission unit transmits the laser beam irradiated from the laser head of the laser unit and transmits infrared rays including a region band having a wavelength of more than 3 microns and less than 9 microns; and a mask for placing A placing unit for placing the mask on the upper side of the fixing unit; a pressurizing unit for lifting or lowering either the mask placing unit or the fixing unit relative to the other so that the transparent portion of the mask can pressurize the plurality of semiconductor wafers on the substrate fixed to the fixing unit; a discharging unit for receiving and discharging the substrate from the fixing unit; an infrared camera for photographing the semiconductor wafer irradiated with a laser beam by the laser head of the laser unit; and a control unit for controlling the operation of the supply unit, the fixing unit, and the discharging unit, and controlling the operation of the laser head of the laser unit using the value measured in the infrared camera.

[0009] The flip-chip laser bonding system of the present invention for achieving the above-mentioned purpose is characterized by comprising: a supply unit for supplying a substrate, wherein the substrate is in a state where a plurality of semiconductor chips are arranged to be bonded to the upper surface of the substrate; a fixing unit for receiving the substrate from the supply unit and fixing the lower surface of the substrate; a laser unit comprising a laser head for irradiating a laser beam to the substrate fixed to the fixing unit to bond the semiconductor chip to the substrate, and a laser transfer unit for transferring the laser head; a mask comprising a transmission part, wherein the transmission part transmits the laser beam irradiated from the laser head of the laser unit, and the transmission part is formed by any one of BaF2 and ZnSe; a mask placement unit, The mask is placed on the upper side of the fixing unit; a pressurizing unit is used to raise and lower either the mask placing unit or the fixing unit relative to the other so that the transparent portion of the mask can pressurize the plurality of semiconductor wafers on the substrate fixed to the fixing unit; a discharge unit is used to receive and discharge the substrate from the fixing unit; an infrared camera is used to photograph the semiconductor wafer irradiated with the laser beam by the laser head of the laser unit; and a control unit is used to control the operation of the supply unit, the fixing unit, and the discharge unit, and to control the operation of the laser head of the laser unit using the value measured in the infrared camera.

[0010] Effects of the Invention

[0011] The flip chip laser bonding system of the present invention has the effect that a semiconductor wafer that is bent or may be bent can be bonded to a substrate without poor contact of solder bumps by laser bonding the semiconductor wafer to the substrate in a pressurized state. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 is a perspective view of a flip chip laser bonding system according to an embodiment of the present invention.

[0013] Figure 2 yes Figure 1 Front view of the flip chip laser bonding system shown.

[0014] Figure 3 It is for Figure 1 A top view of a portion of a flip chip laser bonding system is shown.

[0015] Figure 4 yes Figure 1 A plan view of a mask used in a flip chip laser bonding system is shown.

[0016] Figure 5 yes Figure 4 A cross-sectional view of the mask taken along line VV is shown. DETAILED DESCRIPTION

[0017] Hereinafter, the flip chip laser bonding system of the present invention will be described in detail with reference to the accompanying drawings.

[0018] Figure 1 is a three-dimensional diagram of a flip chip laser bonding system according to an embodiment of the present invention. Figure 2 yes Figure 1 Front view of the flip chip laser bonding system shown.

[0019] The flip chip laser bonding system of this embodiment is a device that uses a laser beam to bond a semiconductor chip to a substrate in a flip chip form. Solder bumps are formed on either or both of the substrate and the semiconductor chip, so the energy transmitted by the laser beam is used to melt the solder bumps instantly and then solidify, while bonding the semiconductor chip to the substrate.

[0020] Reference Figure 1 and Figure 2 The flip chip laser bonding system according to the present embodiment includes a supply unit 110 , a fixing unit 120 , a laser unit 200 and a discharge unit 130 .

[0021] The supply unit 110 is a structure for supplying a substrate for laser bonding to the fixing unit 120. The substrate is supplied in a state where a plurality of semiconductor wafers are arranged. Usually, flux is applied to the substrate and semiconductor wafers are arranged thereon. The semiconductor wafer is temporarily attached to the substrate due to the viscosity or adhesiveness of the flux. Unless a large vibration or external force is applied, the semiconductor wafer arranged on one substrate does not shake due to the flux and maintains its position relative to the substrate.

[0022] As described above, the supply unit 110 sequentially supplies a plurality of substrates with semiconductor wafers temporarily attached thereto to the fixing unit 120. In the present embodiment, the supply unit 110 supplies the substrates to the fixing unit 120 using belts supporting both sides of the substrates.

[0023] The fixing unit 120 also uses belts supporting both sides of the substrate to transfer the substrate received from the supply unit 110 to the working position. The fixing unit 120 fixes the substrate by adsorbing the lower surface of the substrate.

[0024] The laser unit 200 is disposed on the upper side of the fixing unit 120. The laser unit 200 includes a laser head 210 and a laser transfer unit 220. The laser head 210 irradiates a laser beam to the substrate fixed to the fixing unit 120 and transmits energy. The laser transfer unit 220 transfers the laser head 210 in the vertical direction and the horizontal direction. The control unit 500 operates the laser unit 200 so that the laser head 210 sequentially moves along the upper side of the semiconductor wafer of the substrate fixed to the fixing unit 120 while irradiating the laser beam.

[0025] A mask 400 is arranged on the upper side of the fixing unit 120 for fixing the substrate. The mask 400 is supported by the mask placement unit 300. The mask 400 includes a transmissive portion 440 through which laser light can pass. The laser beam irradiated from the laser head 210 is transmitted to the semiconductor wafer on the lower side through the transmissive portion 440 of the mask 400. In the flip chip laser bonding system according to the present embodiment, the transmissive portion 440 is formed of BaF2. Unlike quartz, which only transmits visible light and infrared rays in the short wavelength region, BaF2 is a transparent material that also transmits infrared rays in the longer wavelength region. Quartz is a material that transmits light with a wavelength of 0.18 microns to 3.5 microns, while BaF2 also transmits light with a wavelength of 0.15 microns to 12 microns. The specific structure of the mask 400 will be described below.

[0026] The pressurizing unit 350 is configured to raise or lower one of the mask placement unit 300 and the fixing unit 120 relative to the other so as to pressurize the semiconductor wafer attached to the substrate through the transparent portion 440 of the mask 400. In this embodiment, the pressurizing unit 350 raises or lowers the substrate. Figure 2The pressurizing unit 350 raises and lowers the structure that adsorbs the lower surface of the substrate in the fixing unit 120. When the pressurizing unit 350 lifts the substrate with the mask 400 placed in the mask placement unit 300, the weight of the transparent portion 440 of the mask 400 is placed on the semiconductor wafer to pressurize the semiconductor wafer at the same time.

[0027] The discharge unit 130 receives and discharges the substrate after laser bonding of the semiconductor wafer from the fixing unit 120. Similar to the supply unit 110 and the fixing unit 120, the discharge unit 130 receives and transfers the substrate from the fixing unit 120 using belts supporting both sides of the substrate and discharges the substrate to an unloader.

[0028] The control unit 500 controls the operation of the main components of the present invention including the supply unit 110 , the fixing unit 120 , the laser unit 200 , the discharge unit 130 and the like.

[0029] The inspection camera 230 is disposed on the upper side of the fixing unit 120. In this embodiment, the inspection camera 230 is provided on the laser unit 200 and moves together with the laser head 210 through the laser transfer unit 220. The inspection camera 230 photographs the substrate or the mask 400 disposed on the lower side so that the control unit 500 can grasp the position of the semiconductor wafer or determine whether the mask 400 is contaminated.

[0030] The inspection light 610 is arranged at the lower side of the inspection camera 230. In the case of the present embodiment, the inspection light 610 is provided in the mask replacement unit 600 described later. The inspection light 610 is arranged at the lower side of the path for transferring the mask 400. The inspection light 610 irradiates light from the lower side of the mask 400. The light generated from the inspection light 610 is transmitted to the inspection camera 230 on the upper side through the transparent portion 440 of the mask 400. With the illumination of the inspection light 610, the inspection camera 230 can more effectively photograph the transparent portion 440 of the mask 400. The control unit 500, which receives the image photographed in the inspection camera 230, inspects whether the transparent portion 440 of the mask 400 is contaminated, and based on this, inspects the necessity of replacing the mask 400.

[0031] Reference Figure 3, an infrared camera 240 is provided on the upper side of the fixing unit 120. The infrared camera 240 photographs the semiconductor wafer fixed to the substrate of the fixing unit 120. In the process of melting the solder bump by irradiating the laser beam, the temperature of the semiconductor wafer also rises. Generally, the temperature of the semiconductor wafer varies between 50°C and 500°C. According to the Wien displacement law, the wavelength of infrared rays emitted from the semiconductor wafer varying between 50°C and 500°C is about 3 microns or more and 9 microns or less. In the case where the mask 400 is arranged on the upper side of the substrate, the semiconductor wafer is photographed through the transparent portion 440 of the mask 400. As described above, the transparent portion 440 of the mask 400 of the present embodiment contains BaF2, so that light with a wavelength of 0.15 microns to 12 microns is transmitted. That is, the transparent portion 440 not only transmits all the laser light generated by the laser head 210, but also transmits all infrared rays with a wavelength of from 3 microns to 9 microns. Therefore, the semiconductor wafer disposed on the lower side of the transmission part 440 can be irradiated with a laser beam to be heated, and the infrared camera 240 can simultaneously photograph the semiconductor wafer through the transmission part 440. That is, the infrared camera 240 can accurately measure the temperature of the semiconductor wafer that varies between 50°C and 500°C through the transmission part 440. Since the temperature at which the semiconductor wafer is actually heated is often between 200°C and 400°C, even if the transmission part 440 that allows the laser beam to pass through and also allows the infrared rays in this temperature range to pass through is used, the semiconductor wafer can be heated by the laser and the temperature can be confirmed at the same time. In this case, the wavelength of the infrared rays corresponding to 200°C to 400°C corresponds to approximately 4 microns to 6 microns. As described above, since BaF2 allows the laser beam to pass through and also allows the infrared rays in the same wavelength range to pass through, it can be used as the material of the transmission part 440.

[0032] The control unit 500 can grasp the temperature of different regions of the semiconductor wafer using the values ​​captured by the infrared camera 240. The control unit 500 controls the operation of the laser head 210 of the laser unit 200 using the values ​​measured by the infrared camera 240.

[0033] The mask replacement unit 600 is a structure for accommodating a plurality of masks 400, and is a structure for replacing the mask 400 placed on the mask placement unit 300 as needed. The control unit 500 transmits a mask 400 replacement command to the mask replacement unit 600 as needed, so that the mask replacement unit 600 replaces the mask 400 placed on the mask placement unit 300 with a new mask 400. As described above, the inspection lamp 610 is provided in the mask replacement unit 600, and therefore, the mask 400, which is the object of replacement, is inspected to see whether it is contaminated by being arranged on the upper side of the inspection lamp 610. If the control unit 500 checks the image captured by the inspection camera 230 and determines that it is not contaminated, the mask 400 is transferred to the mask placement unit 300 again. When the control unit 500 determines that the mask 400 is contaminated, the contaminated mask 400 is stored in the mask replacement unit 600 and a new mask 400 is taken out and transferred to the mask placement unit 300 .

[0034] Below, refer to Figure 4 and Figure 5 , the structure of the mask 400 is described.

[0035] The mask 400 used in this embodiment includes a mask body 410 , a plurality of through holes 420 , and a through portion 440 .

[0036] The mask body 410 is formed in a flat plate shape. The mask body 410 is made into a shape corresponding to the shape of the substrate, and is made into a size similar to the substrate in consideration of the size of the substrate.

[0037] The mask body 410 is formed with a plurality of through holes 420. The through holes 420 are formed at positions corresponding to the positions of the semiconductor wafer of the substrate to be arranged on the lower side of the mask 400. The through holes 420 are made to have a size and shape similar to that of the semiconductor wafer. In the case of this embodiment, the mask body 410 including the through holes 420 formed slightly larger than the size of the semiconductor wafer is used.

[0038] The stopper ribs 430 are formed in each through hole 420 so as to protrude inward. Figure 4 As shown, the stopper rib 430 is formed into a shape corresponding to the through hole 420. The shape of the stopper rib 430 can be Figure 4 Various shapes other than those shown.

[0039] Reference Figure 5, the transparent portion 440 is respectively inserted into each of the transparent holes 420. At this time, the lower portion of the transparent portion 440 is formed in a manner of hanging on the stop rib 430. The lower surface of the transparent portion 440 is formed in a planar shape. When the transparent portion 440 presses the semiconductor wafers on each substrate through the operation of the pressurizing unit 350, the semiconductor wafers are uniformly pressurized in a planar manner through the transparent portion 440 formed flat on the lower surface. The transparent portion 440 includes a transparent material that is transparent to the laser beam. As described above, in the case of this embodiment, the transparent portion 440 is formed of BaF2. The mask body 410 is formed of an opaque material that is not transparent to the laser beam. The mask body 410 plays the following role: preventing the laser beam from passing through areas other than the transparent portion 440.

[0040] In the present embodiment, a weight groove 441 is formed in a concave manner on the upper surface of the transparent portion 440. A weight 442 is disposed in each of the weight grooves 441. The weight 442 serves to further increase the force applied to the semiconductor wafer by the transparent portion 440.

[0041] Hereinafter, the operation of the flip chip laser bonding system according to the present embodiment configured as described above will be described.

[0042] First, a substrate with semiconductor wafers disposed thereon is prepared. As described above, the substrate with semiconductor wafers disposed thereon, with flux applied to solder bumps formed on the lower surface of the semiconductor wafers, is sequentially supplied from the supply unit 110 by temporarily bonding the semiconductor wafers to the substrates.

[0043] The supply unit 110 supplies the substrate to the fixing unit 120. The fixing unit 120 transfers and receives the substrate and fixes it by adsorbing the lower surface.

[0044] In this state, the laser transfer unit 220 of the laser unit 200 moves the inspection camera 230 over the substrate and simultaneously photographs the semiconductor wafer on the substrate. The control unit 500 uses the image transmitted and received from the inspection camera 230 to grasp the position of each semiconductor wafer.

[0045] Next, the mask replacing unit 600 transfers the mask 400 to the upper side of the fixing unit 120. The mask placing unit 300 transfers and receives the mask 400 and places it on the upper side of the substrate.

[0046] In this state, the pressurizing unit 350 raises the substrate fixed to the fixing unit 120 .

[0047] If the substrate is raised by the pressurizing unit 350, the semiconductor wafer of the substrate is brought into contact with the lower surface of the transparent portion 440 of each mask 400. If the pressurizing unit 350 further raises the substrate, each semiconductor wafer lifts the transparent portion 440 relative to the mask body 410. As described above, since the transparent portion 440 is in a state of being hung on the stopper rib 430 of the mask body 410, if the semiconductor wafer is further raised, the transparent portion 440 is lifted upward through the semiconductor wafer. That is, when the mask body 410 is stationary, only the transparent portion 440 is raised. As a result, the load of the transparent portion 440 is transmitted to each semiconductor wafer, and the upper surface of the semiconductor wafer is evenly pressurized. At this time, as described above, if a weight 442 is arranged in the weight groove 441 of the transparent portion 440, the magnitude of the force pressurizing the semiconductor wafer is increased according to the weight of the weight 442.

[0048] In this state, the control unit 500 operates the laser unit 200 to sequentially bond the semiconductor wafers of the substrate. If the laser transfer unit 220 sequentially arranges the laser head 210 on each semiconductor wafer and the laser head 210 irradiates the laser beam, the semiconductor wafer is bonded to the substrate. The laser beam is transmitted through the transparent part 440 and the body of the semiconductor wafer to the solder bump, causing the temperature to rise and the solder bump to be bonded to the pad of the substrate.

[0049] The laser beam instantly raises the temperature of the solder bump, so it has the advantage of not making the temperature of the semiconductor chip itself higher than the required temperature. Therefore, the laser beam completes the solder bump bonding operation in a short time, so it has the advantage of not heating the semiconductor chip to a high temperature for a long time. At this time, even if the semiconductor chip is warped or thermally deformed, the transparent portion 440 of the mask 400 presses the upper surface of the semiconductor chip, so it has the advantage of preventing the semiconductor chip from warping or bending. As described above, if the semiconductor chip is prevented from bending, defects caused by a part of the solder bump of the semiconductor chip not being bonded to the substrate can be prevented.

[0050] As described above, the laser beam can only pass through the transparent portion 440 of the mask 400 and cannot pass through the mask body 410, so the laser beam irradiated from the laser head 210 is only transmitted to the semiconductor wafer. As described above, the mask 400 including the transparent portion 440 and the mask body 410 has the following effect: by using the mask 400 including the transparent portion 440 and the mask body 410, it is possible to prevent the laser beam from being irradiated to the substrate portion to which the energy of the laser beam does not need to be transmitted.

[0051] In addition, multiple semiconductor wafers can be bonded to the substrate at the same time. If the laser head 210 is operated to widen the irradiation area of ​​the laser beam, the laser beam can be irradiated to more than two semiconductor wafers at the same time. Since the laser beam cannot pass through the mask body 410 of the mask 400, even if the laser beam is irradiated to a wide area, the energy of the laser beam can be transmitted only to the semiconductor wafers to be bonded. By bonding multiple semiconductor wafers to the substrate at the same time in this way, the productivity of the process can be improved as a whole. Depending on the situation, the laser beam can be irradiated to the entire mask 400 to bond the entire semiconductor wafer to the substrate at the same time.

[0052] On the other hand, the area where the weight groove 441 and the weight hammer 442 are arranged in the transparent part 440 is formed in the area where the solder bumps of the semiconductor wafer are not formed. In the case of this embodiment, there is no solder bump in the central part of the semiconductor wafer and there is only a solder bump in the edge part of the semiconductor wafer. Therefore, as shown in the figure, the weight groove 441 and the weight hammer 442 are arranged in the central part of the transparent part 440.

[0053] The substrates bonded after the above-mentioned process are transferred from the fixing unit 120 to the discharge unit 130. The discharge unit 130 receives the corresponding substrate and transfers it to the unloader.

[0054] If the number of times the mask 400 is used exceeds a fixed number of times, the control unit 500 activates the mask replacement unit 600 to perform a contamination check or replace the mask.

[0055] For example, after the mask 400 is used twenty times, the control unit 500 transfers the mask 400 from the mask placement unit 300 to the upper side of the inspection lamp 610 through the mask replacement unit 600. In this state, the control unit 500 turns on the inspection lamp 610 and photographs the mask 400 through the inspection camera 230. If the transparent portion 440 is found to be contaminated and dust particles are found in the photographed image of the mask 400, the control unit 500 activates the mask replacement unit 600 to replace the mask 400. The mask replacement unit 600 replaces the contaminated mask 400 and transfers and places the new mask 400 to the mask placement unit 300. If the inspection result of the control unit 500 determines that the mask 400 is not contaminated, the mask 400 that was on the upper side of the inspection lamp 610 is transferred to the mask placement unit 300 again for reuse.

[0056] On the other hand, the flip-chip laser bonding system according to the present embodiment can measure the temperature change of the semiconductor wafer in real time in a state where the transparent portion 440 of the mask 400 presses the upper surface of the semiconductor wafer. Previously, the transparent portion was formed using quartz, which is a representative transparent material. When the temperature is measured through quartz using an infrared camera, it is impossible to measure the temperature range below 500°C. As described above, the reason is that quartz cannot transmit infrared rays with a wavelength of 3.5 microns or more. According to the flip-chip laser bonding system of the present embodiment, the transparent portion 440 is formed of BaF2. BaF2 can transmit light with a wavelength of 0.15 microns to 12 microns. That is, the transparent portion 440 can transmit all infrared rays emitted from a substance with a temperature between 50°C and 500°C. Therefore, even in a state where the transparent portion 440 presses the upper surface of the semiconductor wafer, the infrared camera 240 can accurately measure the temperature of the semiconductor wafer through the transparent portion 440. Therefore, the semiconductor wafer can be heated by irradiating a laser beam through the transparent portion 440, and the temperature of the semiconductor wafer can be measured by the infrared camera 240 at the same time.

[0057] The control unit 500 can use the infrared camera 240 to measure the temperature of the semiconductor wafer in real time and control the operation of the laser head 210 based on the temperature. During the period when the laser beam is irradiated on the semiconductor wafer, the infrared camera 240 measures the temperature of the semiconductor wafer through the transparent portion 440 of the mask 400. In the process of melting the solder bump due to the irradiation of the laser beam, the temperature of the semiconductor wafer adjacent to the solder bump also rises. That is, the infrared camera 240 indirectly measures the temperature of the solder bump through the temperature of the semiconductor wafer. The control unit 500 receives the temperature information of the semiconductor wafer measured by the infrared camera 240 to control the operation of the laser head 210 in real time. It is preferable to uniformly irradiate the laser beam to the plurality of solder bumps between the semiconductor wafer and the substrate. That is, it is preferable that the temperature of the solder bump rises uniformly. The infrared camera 240 measures the temperature of the surface of the semiconductor wafer. The control unit 500 controls the operation of the laser head 210 so that the laser beam is irradiated with a higher intensity to the portion of the semiconductor wafer with a low surface temperature. As described above, the control unit 500 can control the laser head 210 so that all solder bumps are raised at a uniform temperature. This means that all solder bumps are irradiated with a laser beam uniformly. In the case of the present invention, the transparent unit 440 that can transmit a wide range of infrared rays can be used, and the infrared camera 240 can be used to confirm in real time whether the upper surface of the semiconductor wafer is uniformly heated. Finally, the present invention can be controlled in a manner that the intensity of the laser beam is uniformly maintained according to the position.

[0058] As mentioned above, although the present invention has been described by taking the preferred examples, the scope of the present invention is not limited to the above-described and illustrated embodiments.

[0059] For example, the above text describes the case where the transparent portion 440 of the mask 400 is formed of BaF2, but other transparent materials can also be used to form the transparent portion of the mask. As described above, during the laser beam irradiation process, the temperature of the semiconductor chip varies between 50°C and 500°C. At this time, the wavelength of the infrared light irradiated from the semiconductor chip is approximately 3 microns or more and 9 microns or less. Therefore, the transparent portion can be formed using various materials that allow infrared light with a wavelength of 3 microns or more and 9 microns to pass through. For example, the transparent portion can also be formed using a material such as ZnSe. ZnSe allows infrared light with a wavelength of 0.6 microns to 16 microns to pass through. The transparent portion can also be formed using materials such as Ge and similar materials that allow infrared light with a wavelength of 2 microns to 16 microns to pass through.

[0060] In addition, depending on the situation, the mask may be formed by a transparent portion that transmits infrared rays with a wavelength of 4 micrometers or more and 6.5 micrometers or less. Such materials are, for example, CaF2 or MgF2.

[0061] In addition, an anti-reflection coating may be applied to the transmission portion for use. In the case where the transmission portion is formed of a material that allows infrared rays to be transmitted preferably in a manner consistent with the purpose of the present invention, the transmittance of the laser beam may also be relatively low depending on the material of the transmission portion. In this case, an anti-reflection coating may also be applied to the transmission portion to reduce the reflection of the laser beam. As described above, the transmission portion can be formed in a manner consistent with the purpose of the present invention, and by applying an anti-reflection coating to the transmission portion, the laser beam used to heat the semiconductor wafer and the infrared rays used to measure the temperature of the semiconductor wafer are preferably transmitted.

[0062] In addition, the above description has been given of a case where the pressurizing member raises the substrate, but the semiconductor wafer may also be pressurized by lowering the mask 400 by the pressurizing member.

[0063] In addition, the above description has been given of the case where the weight groove 441 is formed in the transparent portion 440 of the mask 400 and the weight 442 is arranged, but the mask 400 having a structure not including the weight groove 441 and the weight 442 may also be used. Depending on the situation, a mask including a transparent portion including only the weight groove and the weight may also be used.

[0064] In addition, the flip chip laser bonding system including the mask replacement unit 600 is described above as an example, but a flip chip laser bonding system not including the mask replacement unit 600 may be configured. In this case, the flip chip laser bonding system may be configured as follows: the mask 400 may be used continuously without checking whether it is contaminated, and the mask 400 may be replaced manually for use.

[0065] In addition, a flip chip laser bonding system that does not include the infrared camera 240 , the inspection lamp 610 , the inspection camera 230 , and the like may be configured.

Claims

1. A flip chip laser bonding system, comprising: a supply unit that supplies a substrate in a state where a plurality of semiconductor wafers are provided to be bonded to an upper surface of the substrate; a fixing unit, receiving the substrate from the supply unit and fixing the lower surface of the substrate; a laser unit including a laser head for irradiating the substrate fixed to the fixing unit with a laser beam to bond the semiconductor wafer to the substrate, and a laser transfer unit for transferring the laser head; a mask including a transmission portion that transmits the laser beam irradiated from the laser head of the laser unit and transmits infrared light including a wavelength band of 3 μm to 9 μm; A mask placement unit, which places the mask on the upper side of the fixing unit; a pressurizing unit that causes either the mask placement unit or the fixing unit to be raised or lowered relative to the other so that the transparent portion of the mask can pressurize the plurality of semiconductor wafers on the substrate fixed to the fixing unit; a discharging unit, receiving and discharging the substrate from the fixing unit; an infrared camera for photographing the semiconductor wafer irradiated with the laser beam by the laser head of the laser unit; and The control unit controls the operation of the supply unit, the fixing unit, and the discharge unit, and controls the operation of the laser head of the laser unit using the value measured by the infrared camera. 2 . The flip chip laser bonding system according to claim 1 , wherein the transmission portion of the mask transmits infrared light including a wavelength band of 4 μm to 6.5 μm.

3. A flip chip laser bonding system, comprising: a supply unit that supplies a substrate in a state where a plurality of semiconductor wafers are provided to be bonded to an upper surface of the substrate; a fixing unit, receiving the substrate from the supply unit and fixing the lower surface of the substrate; a laser unit including a laser head for irradiating the substrate fixed to the fixing unit with a laser beam to bond the semiconductor wafer to the substrate, and a laser transfer unit for transferring the laser head; a mask including a transmission portion that transmits the laser beam irradiated from the laser head of the laser unit, and the transmission portion is formed of any one of BaF2 and ZnSe; A mask placement unit, which places the mask on the upper side of the fixing unit; a pressurizing unit that causes either the mask placement unit or the fixing unit to be raised or lowered relative to the other so that the transparent portion of the mask can pressurize the plurality of semiconductor wafers on the substrate fixed to the fixing unit; a discharging unit, receiving and discharging the substrate from the fixing unit; an infrared camera for photographing the semiconductor wafer irradiated with the laser beam by the laser head of the laser unit; and The control unit controls the operation of the supply unit, the fixing unit, and the discharge unit, and controls the operation of the laser head of the laser unit using the value measured by the infrared camera.

4. The flip chip laser bonding system according to claim 3, wherein the infrared camera photographs the semiconductor wafer when the laser head of the laser unit irradiates the semiconductor wafer with the laser beam, The control unit receives the value measured by the infrared camera and adjusts the intensity of the laser beam radiated from the laser head of the laser unit. 5 . The flip chip laser bonding system according to claim 4 , further comprising a mask replacing unit configured to supply the mask to the mask placing unit or discharge the mask.

6. The flip chip laser bonding system according to claim 4, further comprising: an inspection light for irradiating light to the mask from the underside of the mask; as well as An inspection camera is used to photograph the mask or the substrate from above. The control unit determines whether the mask is contaminated by using the image of the mask captured by the inspection camera.

7. The flip chip laser bonding system according to claim 6, wherein the inspection light is disposed on the mask replacement unit, The inspection camera is provided in the laser unit and is transferred by the laser transfer unit.

8. The flip chip laser bonding system according to claim 4, wherein weight grooves are formed in a concave manner on the upper surfaces of the plurality of transmission portions of the mask, respectively. The mask further includes a weight placed in the weight slot of the transparent portion to increase the weight for pressurizing the plurality of semiconductor wafers disposed on the substrate. 9 . The flip chip laser bonding system according to claim 4 , wherein the transparent portion of the mask is coated with an anti-reflection coating.

Citation Information

Patent Citations

  • Apparatus and Method for Laser Bonding of Flip Chip

    CN109103116A

  • Bonding device

    JP2000040712A