Atomic layer processing chamber for 3D conformal processing
By using atomic layer processing and peak annealing technology, material layers of semiconductor substrates are formed or processed under low thermal balance conditions, solving the conformal deposition problem of 3D structures and achieving efficient material layer formation or etching effects.
Patent Information
- Application Number
- CN202111142728.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2015-03-20
- Filing Date
- 2016-02-25
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2036-02-25
AI Technical Summary
Existing technologies struggle to form or process material layers for three-dimensional (3D) semiconductor structures while minimizing thermal expenditure, especially when high-temperature thermal processes are not applicable, and plasma or light-generated processes are not suitable for 3D conformal deposition.
Atomic layer technology is used to form or process material layers by delivering substances to the substrate surface and performing adsorption and reaction at different temperatures, combined with peak annealing. This includes adsorbing substances at low temperatures and rapidly heating them at high temperatures to achieve reaction or diffusion.
It enables the formation of high-quality conformal layers or conformal etching of substrate surfaces under low thermal expansion and contraction conditions, and is suitable for 3D structures in modern semiconductor manufacturing.
Smart Images

Figure CN113981414B_ABST
Abstract
Description
[0001] This application is a divisional application of the invention patent application with application date of February 25, 2016, application number 201680016568.X, and invention name “Atomic layer processing chamber for 3D conformal processing”. Technical Field
[0002] Embodiments described herein relate to semiconductor manufacturing processes. More particularly, methods for forming or processing material layers on semiconductor substrates are disclosed. Background Art
[0003] Semiconductor component geometries have been reduced significantly in size over the decades since their introduction. Modern semiconductor manufacturing equipment routinely produces devices with 45nm, 32nm, and 28nm feature sizes, and new equipment is being developed and implemented to produce devices with sizes less than 12nm. In addition, chip architectures are at a turning point from two-dimensional (2D) to three-dimensional (3D) structures to accommodate devices with better performance and lower power consumption. Therefore, conformal deposition of materials that form these devices is becoming increasingly important.
[0004] Conformal deposition of materials that form 3D structures can be performed at high temperatures. However, reduced heat budgets and tighter critical dimension requirements make high temperature thermal processes unsuitable for advanced device nodes. Pre-breaking of reactant bonds can be performed using plasma or light under reduced heat budgets. However, processes based on plasma or light generation of ions or radicals are generally not 3D conformal due to the presence of a plasma sheath and low pressure (typically less than about 5 Torr) to maintain the plasma.
[0005] Therefore, there is a need in the art for improved methods for forming or processing material layers. Summary of the invention
[0006] Embodiments described herein relate to methods for forming or processing a material layer on a semiconductor substrate. In one embodiment, the method includes delivering a substance to a surface of a substrate. The substrate is at a first temperature, and the substance is adsorbed on the surface of the substrate. The method further includes heating the surface of the substrate to a second temperature, and at the second temperature, the substance reacts with the surface of the substrate. The method further includes repeating the delivering and heating process.
[0007] In another embodiment, a method includes delivering a substance to a surface of a substrate. The substrate is at a first temperature and the substance is adsorbed on the surface of the substrate. The method further includes heating the surface of the substrate to a second temperature, and at the second temperature, the substance diffuses into the surface of the substrate. The method further includes repeating the delivering and heating process.
[0008] In another embodiment, the method includes placing a substrate in a processing chamber and delivering a first substance to a surface of the substrate. The substrate is at a first temperature and the first substance is adsorbed on the surface of the substrate. The method further includes removing excess first substance that is not adsorbed on the surface of the substrate and heating the surface of the substrate to a second temperature. At the second temperature, the first substance reacts with the surface of the substrate. The method further includes repeating the delivering and heating process. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] The manner in which the above-described detailed features of the disclosure briefly summarized above can be understood in detail, as well as a more specific description of the disclosure, can be obtained by reference to the embodiments, some of which are illustrated in the accompanying drawings. However, it should be noted that the drawings illustrate only typical embodiments of the disclosure and thus these drawings should not be considered as limiting the scope of the invention, as the disclosure may admit to other equally effective embodiments.
[0010] Figure 1 Illustrate a processing sequence according to various embodiments.
[0011] FIG. 2A to FIG. 2C A process sequence according to one embodiment is illustrated.
[0012] FIG. 3A to FIG. 3C A process sequence according to another embodiment is illustrated.
[0013] FIG. 4A to FIG. 4C A process sequence according to another embodiment is illustrated.
[0014] Figure 5 is a schematic cross-sectional view of a processing chamber according to one embodiment.
[0015] Figure 6 is a schematic cross-sectional view of a processing chamber according to another embodiment.
[0016] Figure 7 is a schematic cross-sectional top view of a processing chamber according to another embodiment.
[0017] To facilitate understanding, identical reference numerals have been used, where possible, to designate identical elements that are common to the figures. It is contemplated that elements disclosed in one embodiment may be beneficially utilized in other embodiments without specific description. DETAILED DESCRIPTION
[0018] Embodiments described herein relate to methods for forming or processing a material layer on a semiconductor substrate. In one embodiment, a method for performing an atomic layer process includes delivering a substance to a surface of a substrate at a first temperature, and then spike annealing the surface of the substrate to a second temperature to induce a reaction between the substance and molecules on the surface of the substrate. The second temperature is higher than the first temperature. By repeating the delivery and spike annealing process, a conformal layer is formed on the surface of the substrate or a conformal etching process is performed on the surface of the substrate.
[0019] Figure 1 A processing sequence 100 is illustrated according to various embodiments. The processing sequence 100 can be an atomic layer process performed on a surface of a substrate. The processing sequence 100 starts at block 102. At block 102, a substance is delivered to a surface of a substrate. The substrate can be any suitable substrate, such as a silicon substrate, and the surface of the substrate can include silicon molecules. In some embodiments, a dielectric layer, such as an oxide layer, can be formed on the substrate, and the surface of the substrate can include oxide molecules. The surface of the substrate can include multiple features. The substrate can be placed inside a processing chamber. In one embodiment, the processing chamber includes one processing station. In another embodiment, the processing chamber includes two processing stations. In other embodiments, the processing chamber includes more than two processing stations. The delivery of a substance to the surface of the substrate can be performed at one processing station in a processing chamber having two or more processing stations.
[0020] The substance may be any suitable substance, such as one or more gases or free radicals. Free radicals may be formed at a remote end and subsequently transported to the surface of the substrate. Alternatively, free radicals may be formed by exciting a gas introduced into a processing chamber. The plasma source used to excite the gas in the processing chamber may be any suitable plasma source, such as a capacitively coupled plasma source, an inductively coupled plasma source, or a microwave plasma source. The substance may be introduced to the surface of the substrate while the substrate is heated or cooled to a first temperature. At the first temperature, the substance does not react with molecules on the surface of the substrate. Instead, the substance is adsorbed on the surface of the substrate until the substance saturates the surface. The first temperature of the substrate is high enough to cause the substance to be adsorbed on the surface of the substrate and low enough to avoid reaction between the substance and the molecules on the surface of the substrate. Saturation of the substance at the surface of the substrate is a self-limiting process because there is no reaction between the substance and the molecules on the surface of the substrate caused by the first temperature.
[0021] At block 104, a spike annealing process is performed on the substrate. The spike annealing process can quickly increase the temperature of the surface of the substrate to the second temperature without substantially increasing the temperature of the remainder of the substrate. The spike annealing process can be performed on the substrate in the same processing chamber. In one embodiment, the processing chamber includes two processing stations, at one processing station, the delivery of the substance to the surface of the substrate is performed, and the substrate is transferred to another processing station where the spike annealing process is performed. A purge process can be performed after the delivery of the substance to the surface of the substrate and before the spike annealing process to remove excess substance that is not adsorbed on the surface of the substrate.
[0022] The dwell time or the time during which the substrate is heated by, for example, a laser or flash lamp, can be short, such as about 1 microsecond. Since the dwell time is short and the temperature of the substrate body is not substantially increased, rapid dissipation of heat through the substrate body during the cooling period is ensured. The cooling period from the second temperature back to the starting temperature at the substrate surface is also short, such as from about 10 microseconds to 100 microseconds.
[0023] When the surface of the substrate is rapidly heated to a second temperature (such as above 1000 degrees Celsius), the substance adsorbed on the saturated surface of the substrate becomes reactive with molecules on the surface of the substrate. The second temperature may range from about 1000 degrees Celsius to about 1300 degrees Celsius. In one embodiment, the substance is diffused into the surface of the substrate. In another embodiment, the substance conformally detaches from a portion of the surface of the substrate by forming a product with the portion of the surface of the substrate. In yet another embodiment, a second substance is introduced into the processing chamber, and at the second temperature, the second substance reacts with the substance on the surface of the substrate to form a conformal layer on the surface of the substrate.
[0024] Next, at block 106, the processes described at blocks 102 and 104 are repeated. As a result of the repeated processes described at blocks 102 and 104, a conformal layer may be formed on the surface of the substrate, or the conformal layer may diffuse into the surface of the substrate. Alternatively, repeating the processes described at blocks 102 and 104 may conformally remove a portion of the surface.
[0025] FIG. 2A to FIG. 2C 1 illustrates a processing sequence 100 according to one embodiment. Figure 2A As shown, a surface 204 of a substrate (not shown) may include features 202. Figure 2AAs shown, feature 202 is made of silicon dioxide. However, the material of feature 202 may not be limited to silicon dioxide. In some embodiments, feature 202 is made of silicon. A substrate having a surface 204 is placed on a substrate support in a processing chamber. In some embodiments, a substrate having a surface 204 is placed on a substrate support at a first processing station in the processing chamber. Surface 204 may have been cleaned by a cleaning process to remove any contaminants from surface 204. The cleaning process may be any suitable cleaning process, such as a cleaning process using a halogen-based cleaning gas or free radicals (such as a chlorine- or fluorine-based gas or free radical). The substrate may be brought to a first temperature by a temperature control device formed in the substrate support. The first temperature may vary based on the type of substance and the material of surface 204. The first temperature is low enough so that there is no reaction between the substance and surface 204.
[0026] like Figure 2B As shown, substance 206 is introduced into a processing chamber or a processing station of a processing chamber. Substance 206 adsorbs on surface 204 until substance 206 saturates surface 204. Again, substance 206 may be any suitable substance, such as one or more gases or free radicals. In one embodiment, substance 206 is a nitrogen-containing free radical, such as an NH* free radical. In another embodiment, substance 206 is a boron-containing substance, such as a boron-containing gas or a boron-containing free radical. Boron-containing free radicals may be B*, BH x * or any suitable boron-containing radical.
[0027] In one embodiment, the substance 206 is formed by introducing a boron-containing gas into a processing region of a processing chamber, the processing chamber including a substrate having a surface 204 disposed in the processing chamber. The boron-containing gas may be any suitable boron-containing gas, such as B2H6. The boron-containing gas may be activated by a plasma source, such as a capacitively coupled plasma source, an inductively coupled plasma source, or a microwave plasma source, to form a plasma containing the substance 206. The substance 206 may be a boron-containing radical, such as B* or BH x *, where x can be 1, 2, or 3. In another embodiment, the species 206 is formed by flowing a boron-containing gas to a remote plasma source coupled to a processing chamber including a substrate having a surface 204 disposed therein. The boron-containing gas can be any suitable boron-containing gas (such as B2H6). The boron-containing gas can be activated by the remote plasma source to form a plasma containing the species 206. The species 206 can be a boron-containing radical, such as B* or BH x *, where x can be 1, 2, or 3. A substance 206 is flowed into a processing region of a processing chamber.
[0028] Then, if Figure 2CAs shown, the temperature of the surface 204 is rapidly increased to a second temperature, and the substance 206 becomes reactive with the molecules of the surface 204. In one embodiment, the substance 206 is diffused into the feature 202. The temperature of the surface 204 of the substrate may be rapidly increased by the spike annealing process. The spike annealing process may be performed in the same processing chamber. In some embodiments, the substrate is transferred to a second processing station within the processing chamber, and the spike annealing process is performed at the second processing station. As a repeat Figure 2B and Figure 2C As a result of the described process, portion 208 of feature 202 is modified, such as nitrided.
[0029] FIG. 3A to FIG. 3C A processing sequence 100 according to another embodiment is shown. Figure 3A As shown, a surface 304 of a substrate (not shown) may include features 302. Figure 3A As shown, feature 302 is made of silicon. However, the material of feature 302 may not be limited to silicon. A substrate having a surface 304 is placed on a substrate support in a processing chamber. In some embodiments, the substrate having a surface 304 is placed on a substrate support at a first processing station in the processing chamber. The substrate may be brought to a first temperature by a temperature control device formed in the substrate support. The first temperature may vary based on the type of substance and the material of the surface 304. The first temperature is low enough so that there is no reaction between the substance and the surface 304.
[0030] like Figure 3B As shown, a substance 306 is introduced into a processing chamber or a processing station of a processing chamber. The substance 306 is adsorbed on the surface 304 until the substance 306 saturates the surface 304. Again, the substance can be any suitable reactive substance, such as one or more gases or free radicals. In one embodiment, the substance 306 is Br* or other halogen free radicals.
[0031] Then, if Figure 3C As shown, the temperature of the surface 304 is rapidly increased to a second temperature, and the substance 306 becomes reactive with the molecules of the surface 304. In one embodiment, the substance 306 and the silicon molecules of the surface 304 form a product 308, such as SiBr x , and remove product 308 from surface 304. The temperature of surface 304 of the substrate may be rapidly increased by the spike annealing process. The spike annealing process may be performed in the same processing chamber. In some embodiments, the substrate is transferred to a second processing station within the processing chamber, and the spike annealing process is performed at the second processing station. Figure 3B and Figure 3C As a result of the described process, a conformal etching process may be performed on the surface 304 and a portion of the feature 302 may be removed having a substantially uniform thickness.
[0032] FIG. 4A to FIG. 4C A processing sequence 100 according to another embodiment is shown. Figure 4A As shown, a surface 304 of a substrate (not shown) may include features 302. Figure 4A As shown, feature 302 is made of silicon. However, the material of feature 302 may not be limited to silicon. A substrate having a surface 304 is placed on a substrate support within a processing chamber. In some embodiments, the substrate having a surface 304 is placed on a substrate support at a first processing station in the processing chamber. The substrate may be brought to a first temperature by a temperature control device formed in the substrate support. The first temperature may vary based on the type of substance and the material of surface 304. The first temperature is low enough so that there is no reaction between the substance and surface 304.
[0033] like Figure 4B As shown, substance 406 is introduced into the processing chamber or into a processing station of the processing chamber. Substance 406 adsorbs on surface 304 until substance 406 saturates surface 304. Again, substance 406 may be any suitable substance, such as one or more gases or free radicals. In one embodiment, substance 406 is a nitrogen-containing free radical or gas, such as NH* free radical or ammonia gas.
[0034] Then, if Figure 4C As shown, the temperature of the surface 304 is rapidly increased to a second temperature, and a second substance 408 is introduced into the processing chamber or a second processing station of the processing chamber. The second substance 408 may be trimethylsilane. At the second temperature, the substance 406 becomes reactive with the second substance 408. In one embodiment, the substance 406 and the second substance 408 form a product, such as SiCN, on the surface 304. The temperature of the surface 304 of the substrate may be rapidly increased by a spike annealing process so that the surface 304 reaches the second temperature. The spike annealing process may be performed in the same processing chamber. In some embodiments, the substrate is moved to a second processing station within the processing chamber, and the spike annealing process is performed at the second processing station. As a repeat Figure 4B and Figure 4C As a result of the process described in , a conformal layer may be formed on surface 304. The conformal layer may be SiCN.
[0035] Figure 55 is a schematic cross-sectional view of a processing chamber 500 according to one embodiment. The processing sequence 100 may be performed in the processing chamber 500. The processing chamber 500 includes a bottom 502, a sidewall 504, and a top 506 to define a processing region 507. A substrate support 508 may be disposed in the processing region 507, and a substrate 512 may be disposed on the substrate support 508. A temperature control element 510 (such as a heating element or a cooling channel) may be formed in the substrate support 508 for controlling the temperature of the substrate 512. A flash heat source 514 may be disposed above the substrate support 508 for performing a spike annealing process. The flash heat source 514 may include a plurality of lasers or flash lamps. A substance injection port 516 may be formed in the sidewall 504, and a substance source 518 may be connected to the substance injection port 516. The sequence of delivering substances to the substrate surface and spike annealing described above may be performed in the processing chamber 500. The processing chamber 500 may include a purge gas injection port (not shown) connected to a purge gas source (not shown) for purging the processing region 507 .
[0036] Figure 6 6 is a schematic cross-sectional view of a processing chamber 600 according to one embodiment. The processing sequence 100 may be performed in the processing chamber 600. The processing chamber 600 includes a bottom 602, a sidewall 604, and a top 606. A partition 608 may be disposed in the processing chamber 600 and may form two processing stations 610, 611. The partition 608 may be a physical partition or an air curtain. The first processing station 610 may include a substrate support 612 and a temperature control element 614 embedded in the substrate support 612. The temperature control element 614 may be connected to the substrate support 612. Figure 5 The temperature control element 510 described above is the same. A substance injection port 622 may be formed in the side wall at the first processing station 610, and a substance source 624 may be coupled to the substance injection port 622. The first processing station 610 may further include a purge gas injection port (not shown) connected to a purge gas source (not shown) for purging the processing station 610.
[0037] The second processing station 611 may include a substrate support 618 for supporting the substrate 616. The substrate support 618 may include a temperature control element (not shown) that is the same as the temperature control element 614. A flash heat source 620 may be disposed above the substrate support 618. The flash heat source 620 may be connected to the substrate support 618. Figure 5 The flash heat source 514 described above is the same. The second processing station 611 can further include a substance injection port 626, and a substance source 628 can be coupled to the substance injection port 626. The substance source 628 and the substance injection port 626 can be used to deliver a second substance to the surface of the substrate 616. The substrate 616 can be moved to the first processing station 610 and the second processing station 611 to perform the processing sequence 100 on the substrate.
[0038] Figure 7 7 is a schematic cross-sectional top view of a processing chamber 700 according to one embodiment. The processing chamber 700 may include a plurality of processing stations 702, 704, 706, 708, 710, 712 (six are shown, but not limited to six). Each processing station 702, 704, 706, 708, 710, 712 includes a substrate holder 714 for supporting a substrate (not shown). The substrate holder 714 may be formed on a substrate support 716. The substrate support 716 may include a temperature control element (not shown) for controlling the temperature of a substrate disposed on the substrate holder 714. The plurality of processing stations 702, 704, 706, 708, 710, 712 may be separated by a partition 718, which may be a physical partition or an air curtain. Some of the plurality of processing stations may be capable of performing a delivery of a substance to a surface of the substrate at a first temperature, while the remaining processing stations may be capable of performing a spike annealing process. In one embodiment, delivery of species to the substrate surface is performed at processing stations 702, 706, 710. After the species saturates the surface of the substrate, the substrate support 716 is rotated to place the substrate at the processing station 704, 708, 712 where the spike anneal process may be performed. The substrate support 716 may be rotated to place the substrate at the selected processing station to perform the processing sequence 100.
[0039] While the foregoing is directed to embodiments, other and further embodiments may be devised without departing from the basic scope of the invention, and the scope of the invention is determined by the claims that follow.
Claims
1. A processing chamber, comprising: bottom; Side wall; a top portion, wherein the bottom portion, the sidewalls, and the top portion define a processing area; an injection port formed in the side wall and leading to the processing area; a substrate support disposed in the processing region; a temperature control element disposed in the substrate support; a flash heat source disposed above the substrate support, wherein the flash heat source comprises a plurality of lasers; as well as a radical gas source coupled to the injection port, wherein The temperature control element is configured to control the substrate supported on the substrate support to a first temperature that is sufficiently low so that there is no reaction between the surface of the substrate and substances delivered from the radical gas source through the injection port to the processing region, and The flash heat source is configured to perform a spike annealing process that raises the surface of the substrate to a second temperature higher than the first temperature to form a conformal layer on the surface of the substrate.
2. The processing chamber of claim 1, wherein the temperature control element comprises a heating element.
3. The processing chamber of claim 1, further comprising a purge gas source. 4 . The processing chamber of claim 1 , further comprising a partition disposed in the processing area.
5. The processing chamber of claim 4, wherein the partition forms two processing stations.
6. The processing chamber of claim 4, wherein the partition comprises a physical partition or an air curtain.
7. A processing chamber comprising: bottom; Side wall; a top portion, wherein the bottom portion, the sidewalls, and the top portion define a processing area; an injection port formed in the side wall and leading to the processing area; a substrate support disposed in the processing region; a temperature control element disposed in the substrate support; a flash heat source disposed above the substrate support, wherein the flash heat source comprises a plurality of lamps; as well as a radical gas source coupled to the injection port, wherein The temperature control element is configured to control the substrate supported on the substrate support to a first temperature that is sufficiently low so that there is no reaction between the surface of the substrate and substances delivered from the radical gas source through the injection port to the processing region, and The flash heat source is configured to perform a spike annealing process that raises the surface of the substrate to a second temperature higher than the first temperature to form a conformal layer on the surface of the substrate.
8. The processing chamber of claim 7, wherein the temperature control element comprises a heating element.
9. The processing chamber of claim 7, further comprising a purge gas source.
10. The processing chamber of claim 7, further comprising a partition disposed in the processing area.
11. The processing chamber of claim 10, wherein the partition forms two processing stations.
12. The processing chamber of claim 10, wherein the partition comprises a physical partition or an air curtain.