A laser welding butt joint seam misalignment automatic adjustment device and method
By using laser line structured light scanning and industrial camera image acquisition, and adjusting cylinder pressure in real time, the problem of controlling the misalignment of thin-walled parts in laser welding is solved, achieving efficient and high-precision automatic adjustment, and improving welding quality and efficiency.
Patent Information
- Application Number
- CN202111340955.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-11-12
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2041-11-12
AI Technical Summary
When processing thin-walled parts using existing laser welding methods, especially when splicing complex three-dimensional curved surfaces, it is difficult to ensure that the misalignment at the joint is less than 0.1mm. This results in a step difference after welding, which affects the appearance quality and mechanical properties of the weld.
The method employs laser line structured light scanning to assemble the seams. The scanning images are acquired by an industrial camera to determine the seam status, and the pressure of the clamping cylinder is adjusted in real time to achieve automatic adjustment of the misalignment. The pressure is controlled by the cylinder and proportional valve to ensure that the misalignment is within 0.1mm.
It enables high-precision splicing of thin-walled parts by laser welding, completely replacing manual adjustment and improving production efficiency and splicing accuracy.
Smart Images

Figure CN113996931B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of automatic control technology, and in particular to a device and method for automatically adjusting the misalignment of a laser welding butt joint. Background Art
[0002] At present, laser welding technology has been widely used in the fields of aviation, aerospace, automobiles, etc. in recent years due to its high energy density, small welding deformation, easy integration, automation, flexibility, high precision and high efficiency welding, etc., especially in the thin-walled parts of aviation and aerospace with high quality requirements.
[0003] Since the laser welding technology has a very small beam divergence angle and a small spot diameter after beam focusing, it is very demanding on the welding assembly gap and misalignment, and generally requires the weld gap to be less than 0.1mm and the misalignment to be less than 0.1mm. Especially in the parts with high quality requirements such as aviation and aerospace, the requirements for the assembly state of parts before welding are more stringent.
[0004] However, when laser welding thin-walled parts, especially when joining complex three-dimensional curved surfaces, it is difficult to ensure that the misalignment is less than 0.1 mm. Misalignment occurs locally after assembly and step difference occurs after welding, which seriously affects the appearance quality and mechanical properties of the weld. Therefore, there is an urgent need for an automatic adjustment device for the misalignment of welding assembly to achieve online detection and control of the misalignment. Summary of the invention
[0005] (1) Technical issues to be solved
[0006] The embodiment of the present invention provides an automatic adjustment device and method for the misalignment of a laser welding butt joint, which solves the technical problem that the misalignment amount of the butt joint is difficult to ensure when laser welding thin-walled parts, and a step difference is generated after welding, which seriously affects the appearance quality and mechanical properties of the weld.
[0007] (2) Technical solution
[0008] In the first aspect, an embodiment of the present invention proposes an automatic adjustment device for the misalignment of a laser welding butt joint, the device comprising: a pressure block, a cylinder and a proportional valve, the pressure block being arranged on the skin on both sides of the joint and connected to the output shaft of the cylinder, the proportional valve being connected to the cylinder for adjusting the pressure of the cylinder; an industrial camera and a laser line structure light source, the industrial camera and the laser line structure light source being both connected to a welding robot for capturing images of the joint; an industrial computer, the industrial computer being connected to the proportional valve and the industrial camera signal.
[0009] Furthermore, the device further comprises a pressure beam, which is arranged in parallel on both sides of the joint, and a plurality of cylinders are evenly connected to the pressure beam, and the positions of the cylinders connected to the pressure beams on both sides correspond to each other.
[0010] Furthermore, the device also includes a sensor, which is arranged at the connection position between the pressing block and the output shaft of the cylinder and is connected to the industrial computer signal.
[0011] In a second aspect, the present invention further provides a method for automatically adjusting the misalignment of a laser welding butt joint, the method comprising:
[0012] Step S1, obtaining image information including the seam at the position where the laser line structure light source is irradiated collected by an industrial camera, wherein the industrial camera and the laser line structure light source are installed on a welding robot at a certain angle, and the industrial camera moves along the seam direction according to a pre-programmed program to collect image information including the seam at the position where the laser line structure light source is irradiated;
[0013] Step S2, obtaining the spatial coordinates of the welding head of the welding robot to determine the cylinder corresponding to the coordinates and the proportional valve corresponding to the cylinder;
[0014] Step S3, obtaining the misalignment amount of the seam according to the image information, when the misalignment amount is less than a preset threshold, no adjustment is made; when the misalignment amount is greater than the preset threshold, further determining whether the left side is higher or the right side is higher, if the left side of the seam is higher, increasing the left cylinder pressure or reducing the right cylinder pressure, if the right side of the seam is higher, increasing the right cylinder pressure or reducing the left cylinder pressure;
[0015] Step S4, after the adjustment is completed, detection is performed again, and the above steps are repeated until the misalignment amount is less than a preset threshold.
[0016] Furthermore, the image acquisition speed of the industrial camera in step S1 is 30 frames per second.
[0017] Furthermore, the threshold value preset in step S3 is 0.1 mm.
[0018] In summary, this method uses laser line structured light to scan the joint seam, collects the scanned image through an industrial camera, determines the joint state, and adjusts the pressure of the clamping cylinder in real time according to the judgment result to achieve automatic adjustment of the joint misalignment. The present invention can completely replace manual adjustment, greatly improving production efficiency and joint accuracy. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments of the present invention are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0020] Figure 1It is a front view of an automatic adjustment device for misalignment of a laser welding butt joint according to an embodiment of the present invention.
[0021] Figure 2 It is a side view of an automatic adjustment device for misalignment of a laser welding butt joint according to an embodiment of the present invention.
[0022] Figure 3 The present invention is a schematic diagram of a pressing block of a device for automatically adjusting misalignment of a laser welding butt joint according to an embodiment of the present invention.
[0023] Figure 4 The present invention is a flowchart of a method for automatically adjusting misalignment of a laser welding butt joint according to an embodiment of the present invention.
[0024] In the figure:
[0025] 1-fetal membrane; 2-first skin; 3-pressure block; 4-sensor; 5-cylinder; 6-pressure beam; 7-welding robot; 8-second skin DETAILED DESCRIPTION
[0026] The following is a further detailed description of the embodiments of the present invention in conjunction with the accompanying drawings and examples. The detailed description of the following embodiments and the accompanying drawings are used to exemplarily illustrate the principles of the present invention, but cannot be used to limit the scope of the present invention, that is, the present invention is not limited to the described embodiments, and covers any modification, replacement and improvement of parts, components and connection modes without departing from the spirit of the present invention.
[0027] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application can be combined with each other. The present application will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.
[0028] The embodiment of the present invention provides a device for automatically adjusting the misalignment of a laser butt joint seam. Figure 1 to Figure 3 As shown, the device comprises:
[0029] A pressure block 3, a cylinder 5 and a proportional valve (not shown in the figure), wherein the pressure block 3 is arranged on the first skin 2 (second skin 8) on both sides of the seam and is connected to the output shaft of the cylinder 5. During operation, the first skin 2 and the second skin 8 are placed on the fetal membrane 1 of the welding tool. The proportional valve is connected to the cylinder 5 and is used to adjust the pressure of the cylinder 5; an industrial camera (not shown in the figure) and a laser line structure light source (not shown in the figure), wherein the industrial camera and the laser line structure light source are both connected to the welding robot 7 (usually arranged on the welding head of the welding robot 7) and are used to collect the image of the seam; an industrial computer (not shown in the figure), wherein the industrial computer is connected to the proportional valve and the industrial camera signal. In one aspect of the embodiment of the present invention, the automatic adjustment device for the misalignment of the laser butt joint seam further comprises: a pressure beam 6, wherein the pressure beam 6 is arranged in parallel on both sides of the seam, and a plurality of the cylinders 5 are evenly connected to the pressure beam 6, and the positions of the cylinders 5 connected to the pressure beams 6 on both sides correspond to each other.
[0030] It should be noted that: the cylinder 5 is SMC RHCB32-50; the proportional valve is SMC ITV3010-01; the pressure block is a self-made part made of brass, see Figure 3 shown.
[0031] In one aspect of the embodiments of the present invention, the laser butt joint seam misalignment automatic adjustment device further includes: a sensor 4, which is arranged at the connection position between the pressing block 3 and the output shaft of the cylinder 5 and is connected to the industrial computer signal.
[0032] It should be noted that the device of the present invention uses laser line structured light to scan the joint seam, collects the scanned image through an industrial camera, determines the state of the joint, and adjusts the pressure of the clamping cylinder in real time according to the judgment result to achieve automatic adjustment of the misalignment of the joint seam. The present invention can completely replace manual adjustment, greatly improving production efficiency and joint accuracy.
[0033] The embodiment of the present invention also provides a method for automatically adjusting the misalignment of a laser butt joint seam. Figure 4 As shown, including:
[0034] Step S1, obtaining image information including the seam at the position where the laser line structure light source is irradiated collected by an industrial camera, wherein the industrial camera and the laser line structure light source are installed on a welding robot at a certain angle, and the industrial camera moves along the seam direction according to a pre-programmed program to collect image information including the seam at the position where the laser line structure light source is irradiated;
[0035] Step S2, obtaining the spatial coordinates of the welding head of the welding robot to determine the cylinder corresponding to the coordinates and the proportional valve corresponding to the cylinder;
[0036] Step S3, obtaining the misalignment amount of the seam according to the image information, when the misalignment amount is less than a preset threshold, no adjustment is made; when the misalignment amount is greater than the preset threshold, further determining whether the left side is higher or the right side is higher, if the left side of the seam is higher, increasing the left cylinder pressure or reducing the right cylinder pressure, if the right side of the seam is higher, increasing the right cylinder pressure or reducing the left cylinder pressure;
[0037] Step S4, after the adjustment is completed, detection is performed again, and the above steps are repeated until the misalignment amount is less than a preset threshold.
[0038] In one aspect of the embodiment of the present invention, the image acquisition speed of the industrial camera in step S1 is 30 frames per second.
[0039] In one aspect of the embodiment of the present invention, the threshold value preset in step S3 is 0.1 mm.
[0040] In the present invention, the butt joint is pressed on both sides, and the misalignment of the butt joint is ensured by adjusting the pressing pressure on both sides. In the present invention, multiple cylinders are used to press the parts on both sides of the parts, and the cylinder air pressure is adjusted by a proportional valve to achieve the purpose of automatically adjusting the pressing force.
[0041] The industrial camera and laser line structure light source are installed on the welding robot at an angle suitable for the work, ensuring that the industrial camera can capture the area illuminated by the line structure light. The industrial camera moves along the seam direction according to the pre-programmed program and captures the image information including the seam illuminated by the laser line structure light at a speed of 30 frames per second. At the same time, the spatial coordinates of the robot are obtained to determine the corresponding adjustment of the cylinder.
[0042] After obtaining the seam misalignment, if the seam misalignment is less than 0.1mm, the splicing is qualified, the system does not make any adjustments, and the robot continues to detect forward; if the seam misalignment is greater than 0.1mm, the system further determines whether the left side or the right side is higher; if the left side of the seam is higher, the left cylinder pressure is increased or the right cylinder pressure is reduced; if the right side of the seam is higher, the right cylinder pressure is increased or the left cylinder pressure is reduced; after the adjustment is completed, the test is carried out again until the test result is qualified.
[0043] The present invention adopts laser line structured light scanning to connect the joint seams, collects the scanning image through the industrial camera, judges the joint state, and adjusts the pressure of the clamping cylinder in real time according to the judgment result, so as to realize automatic adjustment of the misalignment of the joint seams, which can completely replace manual adjustment and greatly improve the production efficiency and joint accuracy.
[0044] It should be clear that the various embodiments in this specification are described in a progressive manner, and the same or similar parts between the various embodiments can be referred to each other, and each embodiment focuses on the differences from other embodiments. The present invention is not limited to the specific steps and structures described above and shown in the figures. In addition, for the sake of brevity, a detailed description of known methods and technologies is omitted here.
[0045] The above is only an embodiment of the present application and is not limited to the present application. For those skilled in the art, the present application may have various changes and variations without departing from the scope of the present invention. Any modification, equivalent substitution, improvement, etc. made within the spirit and principle of the present application should be included in the scope of the claims of the present application.
Claims
1. A method for automatically adjusting the misalignment of a laser welding butt joint, characterized in that: A laser welding butt joint seam misalignment automatic adjustment device is used, and the laser welding butt joint seam misalignment automatic adjustment device comprises: A pressure block, a cylinder and a proportional valve, wherein the pressure block is arranged on the skin on both sides of the joint and is connected to the output shaft of the cylinder, and the proportional valve is connected to the cylinder to adjust the pressure of the cylinder; An industrial camera and a laser line structure light source, both of which are connected to the welding robot and used to collect images of the seams; An industrial computer, the industrial computer is connected to the proportional valve and the industrial camera signal; The device also includes a pressure beam, which is arranged in parallel on both sides of the joint, and a plurality of cylinders are evenly connected to the pressure beam, and the positions of the cylinders connected to the pressure beams on both sides correspond to each other; The device also includes a sensor, which is arranged at the connection position between the pressing block and the output shaft of the cylinder and is connected to the industrial computer signal; The method for automatically adjusting the misalignment of a laser welding butt joint seam comprises: Step S1, obtaining image information including the seam at the position where the laser line structure light source is irradiated collected by an industrial camera, wherein the industrial camera and the laser line structure light source are installed on a welding robot at a certain angle, and the industrial camera moves along the seam direction according to a pre-programmed program to collect image information including the seam at the position where the laser line structure light source is irradiated; Step S2, obtaining the spatial coordinates of the welding head of the welding robot to determine the cylinder corresponding to the coordinates and the proportional valve corresponding to the cylinder; Step S3, obtaining the misalignment amount of the seam according to the image information, when the misalignment amount is less than a preset threshold, no adjustment is made; when the misalignment amount is greater than the preset threshold, further determining whether the left side is higher or the right side is higher, if the left side of the seam is higher, increasing the left cylinder pressure or reducing the right cylinder pressure, if the right side of the seam is higher, increasing the right cylinder pressure or reducing the left cylinder pressure; Step S4, after the adjustment is completed, detection is performed again, and the above steps are repeated until the misalignment amount is less than a preset threshold.
2. The method for automatically adjusting the misalignment of laser welding butt joints according to claim 1 is characterized in that: The image acquisition speed of the industrial camera in step S1 is 30 frames per second.
3. The method for automatically adjusting the misalignment of laser welding butt joints according to claim 1 is characterized in that: The threshold value preset in step S3 is 0.1 mm.