MEMS common cavity and separate membrane SOC chip and preparation method thereof

By bonding the acceleration chip on the MEMS microphone chip to form a MEMS common cavity membrane SOC chip, the problem of large volume of multi-chip combination products is solved, the simultaneous collection of audio and inertial signals is achieved, and the space utilization rate and production advantages are improved. .

CN114105084BActive Publication Date: 2024-10-25GOERTEK MICROELECTRONICS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111346521.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-11-15
Publication Date
2024-10-25
Estimated Expiration
2041-11-15

AI Technical Summary

Technical Problem

The overall volume of existing multi-chip combination products is relatively large and cannot meet customers' space requirements.

Method used

By performing a bonding process on the MEMS microphone chip to fix the acceleration chip, a MEMS common-cavity membrane SOC chip is formed. The corresponding position design of the diaphragm and the mass block is used to achieve simultaneous acquisition of audio signals and inertial signals, reducing the overall chip volume.

Benefits of technology

It significantly improves space utilization and reduces the overall size of the chip, while ensuring the sensitivity of signal acquisition and the low cost, consistency, and high reliability of production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114105084B_ABST
    Figure CN114105084B_ABST
Patent Text Reader

Abstract

The present invention provides a MEMS common cavity and split membrane SOC chip and a preparation method thereof, wherein the MEMS common cavity and split membrane SOC chip comprises a first chip component and a second chip component; the second chip component is fixed on the top of the first chip component by a bonding process, and the functional part of the second chip component corresponds to the functional part of the first chip component. The MEMS common cavity and split membrane SOC chip and the preparation method thereof provided by the present invention can effectively reduce the overall volume of existing multi-chip combination products and improve the integration.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of electronic devices, and more specifically, to a MEMS common cavity and divided membrane SOC chip and a preparation method thereof. Background Art

[0002] With the rapid prosperity of the consumer market, the market size of MEMS (Micro-Electro-Mechanical System) sensors has been greatly improved, and there has been a trend of miniaturization, intelligence and integration of consumer electronics. This trend requires the redesign of device layout in various links including the whole machine, substrate, packaging, chip, etc. to upgrade the product stacking method.

[0003] With the development requirements of multifunctional, entertainment and commercial terminal consumer products, the types of sensors carried by them are increasing, which makes the effective space of consumer products with relatively narrow space even more cramped. Therefore, multi-chip combination solutions have become the main means to improve space utilization. At present, the main multi-chip combination method is SIP (System in Package) packaging technology. However, since the SIP packaging solution mainly uses multiple chips to stack through packaging, the overall volume of the formed product is still large and often cannot meet customer needs.

[0004] Based on the above technical problems, a method is urgently needed to further reduce the overall volume of multi-chip combination products. Summary of the invention

[0005] In view of the above problems, an object of the present invention is to provide a MEMS common cavity and divided membrane SOC chip which can effectively reduce the overall volume of a multi-chip combination product.

[0006] The present invention provides a MEMS common cavity and split-film SOC chip, comprising a first chip assembly and a second chip assembly; wherein:

[0007] The second chip assembly is fixed on the top of the first chip assembly through a bonding process, and the functional part of the second chip assembly corresponds to the functional part of the first chip assembly.

[0008] In addition, a preferred solution is that the first chip component is a microphone chip, the second chip component is an acceleration chip; and,

[0009] The diaphragm of the microphone chip corresponds to the upper and lower positions of the mass block of the acceleration chip.

[0010] In addition, a preferred solution is that the microphone chip includes a first substrate, the diaphragm is fixed on the top of the first substrate, a back plate is fixed above the diaphragm, and the acceleration chip is fixed on the top of the back plate by a bonding process.

[0011] A vibration cavity is formed between the vibration membrane and the back plate.

[0012] In addition, a preferred solution is that the acceleration chip includes a second substrate fixed on the top of the back plate, a cantilever beam is connected to the second substrate, the mass block is connected to an end of the cantilever beam away from the second substrate, and a resistance strain gauge is arranged at an end of the cantilever beam away from the mass block.

[0013] In addition, a preferred solution is that the diaphragm and the back plate are respectively led out from both sides of the microphone chip through a first PAD lead, and the resistance strain gauge is led out from one side of the acceleration chip through a second PAD lead.

[0014] In addition, a preferred solution is that an external through cavity corresponding to the upper and lower positions of the diaphragm is opened on the first substrate, and a through cavity corresponding to the upper and lower positions of the mass block is opened on the second substrate; and,

[0015] The diaphragm is provided with a first through hole at both ends respectively connected with the external through cavity and the vibration cavity, and the back plate is provided with a second through hole at both ends respectively connected with the conduction cavity and the vibration cavity.

[0016] On the other hand, the present invention also provides a method for preparing a MEMS common cavity and divided membrane SOC chip, comprising:

[0017] respectively manufacturing the first chip assembly and the second chip assembly;

[0018] Making a first PAD lead for the first chip assembly and a second PAD lead for the second chip assembly;

[0019] The second chip assembly is fixed on the top of the first chip assembly through a bonding process.

[0020] In addition, a preferred solution is that the first chip is a microphone chip, the second chip is an acceleration chip; and,

[0021] The process of making the microphone chip includes:

[0022] Manufacturing a first substrate, and manufacturing a diaphragm on the first substrate;

[0023] Producing an insulating dielectric layer on the diaphragm;

[0024] A back plate is fabricated on the insulating dielectric layer; and

[0025] The process of manufacturing the acceleration chip includes:

[0026] Manufacturing a second substrate, and manufacturing a cantilever beam on the second substrate;

[0027] A mass block is connected to one end of the cantilever beam away from the second substrate; wherein a resistance strain gauge is arranged at one end of the cantilever beam away from the mass block.

[0028] In addition, a preferred solution is that the method for preparing a MEMS common cavity and split film SOC chip comprises the following steps:

[0029] The diaphragm and the back plate are respectively led out from two sides of the microphone chip through the first PAD leads; and,

[0030] The process of making the second PAD lead for the second chip assembly includes:

[0031] The resistance strain gauge is led out from one side of the acceleration chip through a second PAD lead.

[0032] In addition, a preferred solution is that the method for preparing the MEMS common cavity and divided membrane SOC chip further comprises:

[0033] An external through cavity corresponding to the upper and lower positions of the diaphragm is formed on the first substrate, and a conducting cavity corresponding to the upper and lower positions of the mass block is formed on the second substrate; and

[0034] In the process of fixing the acceleration chip on the top of the microphone chip through a bonding process: the diaphragm of the microphone chip is made to correspond to the upper and lower positions of the mass block of the acceleration chip.

[0035] Compared with the prior art, the MEMS common cavity and separate membrane SOC chip according to the present invention has the following beneficial effects:

[0036] The MEMS common cavity and split membrane SOC chip provided by the present invention designs two functionally related chips into a MEMS common cavity and split membrane SOC chip through a bonding process, which can save space to the maximum extent and improve space utilization. Specifically, the present invention uses a MEMS microphone chip to collect audio signals through a special structural design, and then designs a MEMS acceleration chip on the upper surface of the microphone chip through a bonding process. Through this design, it is possible to effectively realize the simultaneous collection of audio signals and inertial signals on a single chip volume, significantly improving the space utilization of the entire chip.

[0037] In the present invention, it is fully considered that the performance of the microphone sensor with back-input sound is better than that of the front-input sound with the same principle. Therefore, the bottom microphone in this solution adopts the back-input sound mode, and the upper acceleration chip is designed as a mass block structure with a hollow design around it, which can effectively reduce the audio transmission barrier and ensure the signal acquisition and sensitivity of the microphone. The MEMS acceleration sensor chip design adopts the piezoresistive principle, combined with the conditioning end Wheatstone bridge circuit, which can convert acceleration into analog signals. The overall design structure is simple, and the difficulty of the acceleration chip manufacturing process is reduced as a whole. While reducing the overall size of the chip, it ensures that the SOC chip in the present invention has the production advantages of low cost, consistency, and high reliability.

[0038] In order to achieve the above and related purposes, one or more aspects of the present invention include features that will be described in detail later and are particularly pointed out in the claims. The following description and the accompanying drawings describe some exemplary aspects of the present invention in detail. However, these aspects indicate only some of the various ways in which the principles of the present invention can be used. In addition, the present invention is intended to include all of these aspects and their equivalents. BRIEF DESCRIPTION OF THE DRAWINGS

[0039] By referring to the following description and claims in conjunction with the accompanying drawings, and with a more comprehensive understanding of the present invention, other objects and results of the present invention will become more apparent and easier to understand. In the accompanying drawings:

[0040] Figure 1 It is a front view of a MEMS common cavity and separate membrane SOC chip according to an embodiment of the present invention;

[0041] Figure 2 is a structural diagram of a microphone chip after preliminary processing according to an embodiment of the present invention;

[0042] Figure 3 is a structural diagram of a microphone chip according to an embodiment of the present invention when manufacturing a first PAD lead;

[0043] Figure 4 A structural diagram of an acceleration chip when manufacturing a second PAD lead according to an embodiment of the present invention;

[0044] Figure 5 It is a structural diagram of a MEMS common cavity and divided membrane SOC chip during a bonding process according to an embodiment of the present invention.

[0045] Figure numerals: microphone chip 1, first substrate 11, diaphragm 12, insulating dielectric layer 13, back plate 14, first PAD lead 15, bonding glue 17, vibration cavity 18, acceleration sensor 2, second substrate 21, mass block 22, second PAD lead 23, resistance strain gauge 24.

[0046] The same reference numerals throughout the drawings indicate similar or corresponding features or functions. DETAILED DESCRIPTION

[0047] In the following description, for the purpose of illustration, in order to provide a comprehensive understanding of one or more embodiments, many specific details are set forth. However, it is apparent that these embodiments may also be implemented without these specific details. In other examples, for ease of describing one or more embodiments, known structures and devices are shown in the form of block diagrams.

[0048] In the description of the present invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inside", "outside" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific position, be constructed and operated in a specific position, and therefore cannot be understood as limiting the present invention; the terms "first", "second", and "third" are only used for descriptive purposes, and cannot be understood as indicating or implying relative importance; in addition, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be an indirect connection through an intermediate medium, or it can be a connection between the two elements. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0049] Before introducing the MEMS shared cavity and split membrane SOC chip provided by the present invention in detail, it should be noted that SOC (System on Chip) means an integrated circuit with a dedicated purpose, which contains all the contents of a complete system and embedded software. At the same time, it is a technology that is used to realize the entire process from determining the system function to software / hardware division and completing the design. The MEMS shared cavity and split membrane SOC chip provided by the present invention is designed based on the system on chip technology.

[0050] The results of the MEMS common cavity and divided membrane SOC chip provided by the present invention and the process of its preparation method are described in detail below with reference to the accompanying drawings.

[0051] Figure 1 It is a front view of a MEMS common cavity and divided membrane SOC chip according to an embodiment of the present invention.

[0052] Depend on Figure 1It can be seen that the MEMS common cavity and split membrane SOC chip provided by the present invention comprises at least a first chip component and a second chip component; wherein the functions of the first chip component and the second chip component need to be mutually related to achieve functional linkage between the two.

[0053] Specifically, in order to reduce the integration level of the first chip component and the second chip component and effectively improve the space utilization rate of the device, the second chip component needs to be fixed on the top of the first chip component through a bonding process, and the functional parts of the second chip component correspond to the functional parts of the first chip component to achieve functional linkage between the two.

[0054] It should be noted that the bonding process refers to the method of tightly bonding silicon wafers to silicon wafers, silicon wafers to glass or other materials through chemical and physical effects. The silicon wafer bonding process is often combined with surface silicon processing and bulk silicon processing, and is used in the processing technology of MEMS. Common silicon wafer bonding technologies include gold-silicon eutectic bonding, silicon / glass electrostatic bonding, silicon / silicon direct bonding, and glass solder sintering.

[0055] It should be noted that, in the actual design process, the first chip assembly and the second chip assembly can both be chips of any function in the field of microelectronics, as long as the functional linkage between the first functional chip and the second functional chip is satisfied, and a third chip assembly with a linkage function can also be fixed on top of the second chip assembly (and so on). In a specific embodiment of the present invention, the first chip assembly can be a microphone chip 1, and the second chip assembly can be an acceleration chip; and after the acceleration chip is bonded and fixed on the top of the microphone chip 1, the functional part of the microphone chip 1 (mainly the diaphragm 12) and the functional part of the acceleration chip (mainly the mass block 22) just correspond to each other in upper and lower positions.

[0056] More specifically, the microphone chip 1 includes a first substrate 11 (usually a silicon substrate), the diaphragm 12 needs to be fixed on the top of the first substrate 11, a back plate 14 is fixed above the diaphragm 12, and the acceleration chip is fixed on the top of the back plate 14 by a bonding process (it can be fixed by bonding with bonding glue 17); and a vibration cavity 18 is formed between the diaphragm 12 and the back plate 14.

[0057] During actual use, the diaphragm 12 of the microphone chip 1 vibrates in the vibration cavity 18 , so that the distance between the diaphragm 12 and the back plate 14 changes, thereby realizing the sound transmission function of the microphone chip 1 .

[0058] Furthermore, the acceleration chip includes a second substrate 21 (usually a silicon substrate) fixed on the top of the back plate 14, a cantilever beam is connected to the second substrate 21, a mass block 22 is connected to one end of the cantilever beam away from the second substrate 21, and a resistance strain gauge 24 is provided at one end of the cantilever beam away from the mass block 22. In actual use, when the entire MEMS common cavity and divided membrane SOC chip moves and generates acceleration and then stops, the resistance strain gauge 24 on the cantilever beam will bend, and as the resistance strain gauge 24 bends, its resistance value will change, thereby realizing the measurement of the acceleration of the entire MEMS common cavity and divided membrane SOC chip.

[0059] It should be noted that, since the electrical functional components of the microphone chip 1 are the diaphragm 12 and the back plate 14, and the functional component of the acceleration chip is the resistance strain gauge 24, and the acceleration chip is fixed on the top of the back plate 14, in order to realize the electrical connection between the diaphragm 12 and the back plate 14 and external devices respectively without increasing the overall volume of the entire MEMS common cavity divided membrane SOC chip, the diaphragm 12 and the back plate 14 can be respectively led out from both sides of the microphone chip 1 through the first PAD (pad) lead, and then connected to the external devices.

[0060] In addition, since the resistance strain gauge 24 is arranged on the cantilever beam on the top of the second substrate 21, in order to realize the electrical connection between the resistance strain gauge 24 and the external device without increasing the overall volume of the entire MEMS common cavity divided membrane SOC chip, the resistance strain gauge 24 can be led out from one side of the acceleration chip through the second PAD lead 23 and then connected to the external device.

[0061] It should be noted that, in order to ensure the sound transmission effect of the microphone chip 1, an external through cavity corresponding to the upper and lower positions of the diaphragm 12 can be opened at one end of the first substrate 11 away from the diaphragm 12, and a conduction cavity corresponding to the upper and lower positions of the mass block 22 can be opened on the second substrate 21; and a first through hole whose two ends are respectively connected to the external through cavity and the vibration cavity 18 is opened on the diaphragm 12, and a second through hole whose two ends are respectively connected to the conduction cavity and the vibration cavity 18 is opened on the back plate 14. Through this design, the external through cavity, the first channel, the vibration cavity 18, the second channel and the conduction cavity can form an air passage together, thereby ensuring the sound transmission effect of the microphone chip 1. Of course, through this design, the conduction cavity can not only balance the air pressure at various positions of the SOC chip of the entire MEMS common cavity and membrane, but also provide a vibration space for the acceleration sensor 2 (provided by the conduction cavity), thereby significantly improving the measurement accuracy of the acceleration sensor 2.

[0062] On the other hand, the present invention also provides a method for preparing a MEMS common cavity and divided membrane SOC chip, and: Figure 2shows the structure of the microphone chip 1 after preliminary processing according to an embodiment of the present invention, Figure 3 FIG. 4 shows the structure of the microphone chip 1 when manufacturing the first PAD lead 15 according to an embodiment of the present invention. Figure 4 FIG. 4 shows the structure of the acceleration chip according to an embodiment of the present invention when manufacturing the second PAD lead 23. Figure 5 The structure of the MEMS common cavity and split film SOC chip during the bonding process according to an embodiment of the present invention is shown. Figures 1 to 5 As shown in the figure, the method for preparing a MEMS common cavity and divided membrane SOC chip provided by the invention comprises:

[0063] respectively manufacturing a first chip assembly and a second chip assembly;

[0064] Making a first PAD lead 15 for the first chip assembly and a second PAD lead 23 for the second chip assembly;

[0065] The second chip assembly is fixed on top of the first chip assembly by a bonding process to form a Figure 1 The structure of the MEMS common cavity and divided membrane SOC chip is shown.

[0066] Specifically, the first chip may be a microphone chip 1, and the second chip may be an acceleration chip; and the process of manufacturing the microphone chip 1 includes:

[0067] Manufacturing a first substrate 11, and manufacturing a diaphragm 12 on the first substrate 11;

[0068] An insulating dielectric layer 13 is formed on the diaphragm 12;

[0069] A back plate 14 is manufactured on the insulating dielectric layer 13 .

[0070] In addition, the process of making an accelerometer chip includes:

[0071] Manufacturing a second substrate 21, and manufacturing a cantilever beam on the second substrate 21;

[0072] The end of the cantilever beam away from the second substrate 21 is connected to the mass block 22 ; wherein, a resistance strain gauge 24 is arranged at the end of the cantilever beam away from the mass block 22 .

[0073] In addition, a preferred solution is that the method for preparing a MEMS common cavity and split film SOC chip comprises the following steps:

[0074] The diaphragm 12 and the back plate 14 are led out from two sides of the microphone chip 1 through two first PAD leads 15 respectively, so as to be connected to other external electrical components.

[0075] Furthermore, the process of making the second PAD lead 23 for the second chip assembly includes:

[0076] The resistance strain gauge 24 is led out from one side of the acceleration chip through the second PAD lead 23 for connecting to other external electrical components.

[0077] In addition, a preferred solution is that the method for preparing a MEMS common cavity and divided membrane SOC chip further includes:

[0078] An external through cavity corresponding to the upper and lower positions of the diaphragm 12 is opened on the first substrate 11, and a through cavity corresponding to the upper and lower positions of the mass block 22 is opened on the second substrate 21; and

[0079] In the process of fixing the acceleration chip on the top of the microphone chip 1 through the bonding process, the diaphragm 12 of the microphone chip 1 and the mass block 22 of the acceleration chip are made to correspond to each other in the upper and lower positions.

[0080] It should be noted that, through this design, the external through cavity, the first channel, the vibration cavity 18, the second channel and the conduction cavity can form an air passage together, thereby ensuring the sound transmission effect of the microphone chip 1. Of course, through this design, the conduction cavity can not only balance the air pressure at each position of the entire MEMS common cavity and membrane SOC chip, but also provide a vibration space for the acceleration sensor 2 (provided by the conduction cavity), thereby significantly improving the measurement accuracy of the acceleration sensor 2.

[0081] As above Figures 1 to 5 The MEMS common cavity and divided membrane SOC chip according to the present invention is described by way of example. However, those skilled in the art should understand that various improvements can be made to the MEMS common cavity and divided membrane SOC chip proposed by the present invention without departing from the content of the present invention. Therefore, the protection scope of the present invention should be determined by the content of the attached claims.

Claims

1. A MEMS common cavity and separate membrane SOC chip, characterized in that: It comprises a first chip assembly and a second chip assembly; wherein, The second chip assembly is fixed on the top of the first chip assembly by a bonding process, and the functional part of the second chip assembly corresponds to the functional part of the first chip assembly; wherein, When the first chip component is a microphone chip and the second chip component is an acceleration chip, the microphone chip adopts a back-input sound method, the diaphragm of the microphone chip corresponds to the upper and lower positions of the mass block on the acceleration chip, the mass block is arranged on a side of the acceleration chip away from the diaphragm, and the surroundings of the mass block are hollowed out; wherein, The microphone chip includes a first substrate, the diaphragm is fixed on the top of the first substrate, a back plate is fixed above the diaphragm, the acceleration chip is fixed on the top of the back plate by a bonding process, and a vibration cavity is formed between the diaphragm and the back plate; the acceleration chip includes a second substrate fixed on the top of the back plate, a cantilever beam is connected to the second substrate, the mass block is connected to one end of the cantilever beam away from the second substrate, and a resistance strain gauge is arranged at one end of the cantilever beam away from the mass block.

2. The MEMS common cavity and divided membrane SOC chip as claimed in claim 1, characterized in that: The diaphragm and the back plate are respectively led out from two sides of the microphone chip through a first PAD lead, and the resistance strain gauge is led out from one side of the acceleration chip through a second PAD lead.

3. The MEMS common cavity and divided membrane SOC chip as claimed in claim 2, characterized in that: An external through cavity corresponding to the upper and lower positions of the diaphragm is opened on the first substrate, and a conducting cavity corresponding to the upper and lower positions of the mass block is opened on the second substrate; and The diaphragm is provided with a first through hole at both ends respectively connected to the external through cavity and the vibration cavity, and the back plate is provided with a second through hole at both ends respectively connected to the conduction cavity and the vibration cavity.

4. A method for preparing a MEMS common cavity and divided membrane SOC chip as claimed in any one of claims 1 to 3, characterized in that: include: respectively manufacturing the first chip assembly and the second chip assembly; Making a first PAD lead for the first chip assembly and a second PAD lead for the second chip assembly; The second chip assembly is fixed on the top of the first chip assembly through a bonding process.

5. The method for preparing a MEMS common cavity and divided membrane SOC chip according to claim 4, characterized in that: The process of making the microphone chip includes: Manufacturing a first substrate, and manufacturing a diaphragm on the first substrate; Producing an insulating dielectric layer on the diaphragm; A back plate is fabricated on the insulating dielectric layer; and The process of manufacturing the acceleration chip includes: Manufacturing a second substrate, and manufacturing a cantilever beam on the second substrate; A mass block is connected to one end of the cantilever beam away from the second substrate; wherein a resistance strain gauge is arranged at one end of the cantilever beam away from the mass block.

6. The method for preparing a MEMS common cavity and divided membrane SOC chip according to claim 5, characterized in that: The process of making the first PAD lead for the first chip component includes: The diaphragm and the back plate are respectively led out from two sides of the microphone chip through the first PAD leads; and, The process of making the second PAD lead for the second chip assembly includes: The resistance strain gauge is led out from one side of the acceleration chip through a second PAD lead.

7. The method for preparing a MEMS common cavity and divided membrane SOC chip according to claim 5 or 6, characterized in that: Also includes: An external through cavity corresponding to the upper and lower positions of the diaphragm is formed on the first substrate, and a conducting cavity corresponding to the upper and lower positions of the mass block is formed on the second substrate; and, In the process of fixing the acceleration chip on the top of the microphone chip through a bonding process: the diaphragm of the microphone chip is made to correspond to the upper and lower positions of the mass block of the acceleration chip.