A method for manufacturing a semiconductor device structure
By using a cyclic etching process to re-etch the conductive material and diffusion barrier layer, the problem of substrate thinning caused by re-etching in the manufacturing of buried word lines is solved, achieving higher integration density and voltage readout reliability.
Patent Information
- Application Number
- CN202010918074.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-09-03
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2040-09-03
AI Technical Summary
During the manufacturing process of embedded word lines, the etch-back process causes the interlayer dielectric layer on the substrate surface and the corresponding substrate to become thinner, which in turn exacerbates the short-channel effect.
A cyclic etching process is used to etch back the conductive material and diffusion barrier layer, so that the surface of the conductive material is lower than the surface of the semiconductor substrate. By precisely controlling the etching back thickness, the etching of the interlayer dielectric layer is reduced, thus avoiding the thinning of the semiconductor substrate.
It effectively reduces short-channel effects and improves the integration density of semiconductor devices and the reliability of voltage readout operations.
Smart Images

Figure CN114141710B_ABST
Abstract
Description
Technical Field
[0001] This application relates to a method for manufacturing semiconductor devices, particularly a method for manufacturing transistors, and especially a method for manufacturing embedded word lines in transistors. Background Technology
[0002] As semiconductor memory devices (such as dynamic random access memory (DRAM)) become highly integrated, the area of a single cell on the semiconductor substrate gradually decreases, and the channel length contained in metal-oxide-semiconductor (MOS) transistors also gradually decreases. This reduction in channel length easily leads to short-channel effects. To maintain the high integration of semiconductor memory devices, measures need to be taken to limit short-channel effects.
[0003] Buried word lines (also known as buried gates) offer a new option for increasing the integration density of semiconductor devices. Buried word lines refer to word lines that are embedded within the semiconductor substrate, which can significantly reduce parasitic capacitance between word lines and bit lines, greatly improving the reliability of voltage readout operations in semiconductor devices.
[0004] During the manufacturing process of embedded word lines, the conductive material deposited in the word line grooves needs to be etched back to a certain extent. During the etch-back process, the interlayer dielectric layer on the substrate surface and the corresponding substrate area become thinner, thereby reducing the active area and exacerbating the short-channel effect. Summary of the Invention
[0005] The objective of this application is achieved through the following technical solution:
[0006] According to one or more embodiments, this application discloses a method for manufacturing a semiconductor structure, including:
[0007] A semiconductor substrate is provided, and word line grooves are formed on the semiconductor substrate;
[0008] A gate oxide layer and a diffusion barrier layer are deposited sequentially;
[0009] Filled with conductive material;
[0010] Surface planarization;
[0011] The conductive material and diffusion barrier layer are etched back using a cyclic etching process, so that the surface of the conductive material is lower than the surface of the semiconductor substrate.
[0012] Other features and advantages of this application will be set forth in the following description and will be apparent in part from the description, or some features and advantages may be inferred from the description or determined without question, or may be learned by practicing embodiments of this application. The objectives and other advantages of this application may be realized and obtained by means of the structures particularly pointed out in the written description, claims, and drawings. Attached Figure Description
[0013] Various other advantages and benefits will become apparent to those skilled in the art upon reading the following detailed description of preferred embodiments. The accompanying drawings are for illustrative purposes only and are not intended to limit the scope of this application. Furthermore, the same reference numerals denote the same parts throughout the drawings. In the drawings:
[0014] Figures 1-2 This is a schematic diagram of the embedded character line manufacturing method in the embodiments of this application;
[0015] Figure 3 This is a partial schematic diagram of the case where the etch-back process is not used. Detailed Implementation
[0016] The present application will now be described more fully with reference to the accompanying drawings, in which embodiments of the present application are shown. However, the present application is not limited to the embodiments set forth herein. Rather, these embodiments are provided to thoroughly and completely illustrate and fully convey the scope of the present application to those skilled in the art. In the drawings, the thickness of layers and regions may be exaggerated for clarity. The same numerals throughout the text identify the same elements. As used herein, the term “and / or” includes any and all combinations of one or more of the associated listed items.
[0017] The terminology used herein is for the purpose of detailed description of embodiments only and is not intended to limit the application. As used herein, unless explicitly stated otherwise, the singular forms “a,” “the,” and “the” also include the plural forms. It should also be understood that the term “comprising” as used in the specification indicates the presence of the stated feature, integral, step, operation, element, and / or component, but does not exclude the presence or addition of one or more other features, integrals, steps, operations, elements, components, and / or combinations thereof.
[0018] It should be understood that when an element, such as a layer, region, or substrate, is referred to as "on another element" or "extends to another element," it can be directly on the other element, directly extended to the other element, or there may be intermediate elements. Conversely, when an element is referred to as "directly on another element" or "directly extended to another element," there are no intermediate elements. It should also be understood that when an element is referred to as "connected" or "coupled" to another element, it can be directly connected or coupled to the other element, or there may be intermediate elements. Conversely, when an element is referred to as "directly connected" or "directly coupled" to another element, there are no intermediate elements.
[0019] It should be understood that although the terms first, second, etc., may be used herein to describe different elements, components, regions, layers, and / or parts, these elements, components, regions, layers, and / or parts are not limited by these terms. These terms are used only to distinguish one element, component, region, layer, or part from another element, component, region, layer, or part. Therefore, without departing from the spirit of this application, the first element, component, region, layer, or part discussed below may be referred to as the second element, component, region, layer, or part.
[0020] Furthermore, relative terms, such as “below” or “bottom” and “above” or “top”, are used here to describe the relationship between one element and another as shown in the accompanying drawings. It should be understood that relative terms include not only the orientations described in the drawings but also different orientations of the device. For example, if a device in the drawing is flipped, an element described as being below another element becomes above another element. Therefore, the exemplary term “below” includes both the “below” and “above” orientations depending on the specific orientation of the drawing. Similarly, if a device in the drawing is flipped, an element described as “below other elements” or “under other elements” is oriented above other elements. Therefore, the exemplary term “below” or “under…” includes both the above and below orientations.
[0021] Embodiments of this application are described herein with reference to illustrative cross-sectional views (and / or plan views) illustrating idealized embodiments. Similarly, deviations from the schematic shapes are expected due to factors such as manufacturing processes and / or tolerances. Therefore, the embodiments of this application are not to be construed as limitations on the specific shapes of the areas illustrated herein, but rather to include shape deviations caused, for example, by manufacturing processes. For instance, etched areas illustrated as or described as rectangular typically have circular or curved features. Thus, the areas illustrated are schematic in nature, and their shapes do not represent the precise shapes of the device areas nor limit the scope of this application.
[0022] Unless otherwise specified, all terms used herein (including technical and scientific terms) have the same meaning as commonly understood by one of ordinary skill in the art to which this application pertains. It should also be understood that terms, such as those defined in common dictionaries, should be interpreted as consistent with their meaning in relevant art literature and, unless expressly defined herein, not as idealized or overly formal. Those skilled in the art will understand that references to structural or functional components configured adjacent to another component may have overlapping or subordinate parts.
[0023] This application discloses a method for manufacturing a semiconductor structure, which can be applied to the manufacturing method of embedded word lines in semiconductor memory structures, but is not limited to the manufacturing of embedded word lines. The specific manufacturing method is as follows:
[0024] First, such as Figure 1 As shown, a substrate 100 can be provided, and an interlayer dielectric layer 101 can be formed on the surface of the substrate 100. Specifically, the substrate 100 can be made of commonly used semiconductor substrate materials such as silicon (Si), germanium (Ge), silicon germanium (SiGe), and silicon-on-insulator (SOI). The interlayer dielectric layer 101 can be an oxide, such as silicon oxide (SiO2).
[0025] Subsequently, an isolation structure can be formed in the substrate 100 to define a plurality of active regions 102 in the substrate 100. The isolation structure can be a shallow trench isolation (STI) or other common isolation structures. The process of forming the isolation structure can be, for example, etching the interlayer dielectric layer 101 and the substrate 100 to form an isolation trench, depositing an oxide layer 103 in the isolation trench, and then filling it with a silicon nitride layer 104.
[0026] Subsequently, word line grooves can be formed in the substrate 100. The word line grooves can be formed by first obtaining a planarization process (e.g., CMP) to achieve a flat surface; then, a hard mask material layer can be formed using chemical vapor deposition, physical vapor deposition, or other deposition methods; subsequently, a photoresist layer can be formed on the surface of the hard mask material layer using spin coating or other coating methods; then, the photoresist layer can be patterned using photolithography, and the hard mask material layer can be patterned based on the patterned photoresist layer; finally, the patterned hard mask material layer and the photoresist layer can be used together as a mask for etching to form the word line grooves.
[0027] Subsequently, a gate oxide layer 105 can be formed on the surface of the word line recess. As an example, the gate oxide layer 105 can be made of silicon oxide and can be formed on the surface of the word line recess using thermal oxidation or other deposition methods. Subsequently, a diffusion barrier layer 106 can be formed on the surface of the gate oxide layer 105. Specifically, the diffusion barrier layer 106 can be made of materials including, but not limited to, titanium nitride (TiN) or tantalum nitride (TaN). The diffusion barrier layer 106 is used to reduce or prevent diffusion between the word line and the substrate.
[0028] Subsequently, conductive material 107 can be deposited on the surface of diffusion barrier layer 106 to fill the space of word line grooves. Specifically, conductive material 107 can be selected from tungsten (W) or other commonly used word line conductive materials. Subsequently, a planarization process (e.g., CMP) can be used to treat the surface of conductive material 107 to obtain a flat surface.
[0029] Subsequently, as Figure 2 As shown, a cyclic etching process can be used to etch back the conductive material 107 so that the surface of the conductive material 107 is lower than the upper surface of the substrate 100 to form word lines; during the cyclic etching back process, the diffusion barrier layer 106 can also be etched back and removed at the same time, so that it has the same height as the etched conductive material 107.
[0030] Specifically, the cyclic etching process of this application may include the following steps:
[0031] First, a precursor adsorption process can be performed. In this embodiment, since the conductive material 107 to be etched is tungsten, a precursor gas containing fluorine-containing gases such as NF3 or SF6 and an inert gas such as N2, He, or Ar can be supplied to the etching chamber to adsorb a portion of the precursor onto the surface of the conductive material. In this embodiment, the processing time of the precursor adsorption process can be less than 10 seconds.
[0032] Subsequently, a post-adsorption purging process can be performed. In this embodiment, after the adsorption process, purging gas can be supplied through a pump valve at a predetermined opening degree, and then the purging gas can be extracted through the pump valve. When extracting the purging gas, the pump valve can be set to a fully open state to extract the precursor gas as fully as possible out of the etching chamber along with the purging gas. In this embodiment, the purging gas can be Ar gas. In this embodiment, the processing time of the post-adsorption purging process can be 3-10 seconds.
[0033] Subsequently, an activation process can be performed. In this embodiment, the activation process may involve supplying an inert gas such as He, Ne, Ar, Kr, or Xe to the etching chamber, and applying a low-bias radio frequency power pulse to generate an inert gas plasma, thereby activating the adsorbed precursor and triggering a chemical reaction to achieve the etching back of the conductive material. In this embodiment, the activation process can be completed in less than 10 seconds.
[0034] Subsequently, a post-activation purging process can be performed. In this embodiment, after the activation process, purge gas can be supplied through a pump valve at a predetermined opening degree, and then the purge gas can be extracted through the pump valve. When extracting the purge gas, the pump valve can be set to a fully open state to ensure that the activation etching reaction products of the polymer precursor adsorbate are extracted out of the etching chamber with the purge gas as fully as possible. In this embodiment, the purge gas can be Ar gas. In this embodiment, the processing time of the post-adsorption purging process can be 3-10 seconds.
[0035] The above completes one cycle of etching in this embodiment. The above only describes one cycle of the process. In actual process manufacturing, the above process can usually be repeated more than one cycle. Specifically, the number of cycles of the above cyclic etching process is set according to the required height of the conductive material to be etched back, that is, to etch back the conductive material so that the height of the conductive material can be lower than the surface height of the semiconductor substrate. The cyclic etching process described in this application allows for precise control of the etching thickness and high selectivity of the dielectric material in each etching cycle. This minimizes etching of the surface of the interlayer dielectric layer 101 between adjacent word line recesses while the conductive tungsten material is being etched back, thus preventing thinning of the semiconductor substrate 100 beneath the interlayer dielectric layer 101. Conversely, without the cyclic etching process described in this application, and instead employing conventional, continuous, one-time etching back of the conductive tungsten material, undesirable etching of the upper portion of the interlayer dielectric layer 101 between adjacent word line recesses is unavoidable during the etch back of the conductive tungsten material, resulting in significant material loss. Figure 3 As indicated by the arrow on the right, this leads to a reduction in the semiconductor substrate 100 below it, which in turn results in a reduction in the active region 102, causing adverse effects such as short-channel effect.
[0036] After the cyclic etching process is used for re-etching, an insulating protective material can be filled on the surface of the conductive material 107 in the word line groove to completely cover the word line conductive material 107, preventing the sidewalls of the word line from being exposed, thereby preventing the word line from being electrically connected to the subsequently formed bit line contact portion and memory node contact portion. The insulating protective material can be silicon oxide or silicon nitride.
[0037] In addition to the above-described embodiments, the manufacturing method of using a cyclic etching process to etch back conductive materials in this application is also applicable to other forms of word line manufacturing methods, in order to solve the problem of undesirable etching of the interlayer dielectric layer and semiconductor substrate that is prone to occur during the etch-back process of tungsten and other word line conductive materials, thereby solving technical problems such as active area reduction and short channel effect.
[0038] The above description does not provide detailed explanations of the technical aspects of each layer's patterning, etching, etc. However, those skilled in the art should understand that various technical means can be used to form layers and regions of the desired shape. Furthermore, to form the same structure, those skilled in the art can also design methods that are not entirely identical to those described above. Additionally, although various embodiments have been described above, this does not mean that the measures in the various embodiments cannot be used advantageously in combination.
[0039] The embodiments of this disclosure have been described above. However, these embodiments are for illustrative purposes only and are not intended to limit the scope of this disclosure. The scope of this disclosure is defined by the appended claims and their equivalents. Various substitutions and modifications can be made by those skilled in the art without departing from the scope of this disclosure, and all such substitutions and modifications should fall within the scope of this disclosure.
Claims
1. A method for manufacturing a semiconductor structure, comprising: A semiconductor substrate is provided, and word line grooves are formed on the semiconductor substrate; A gate oxide layer and a diffusion barrier layer are deposited sequentially; Filled with conductive material; Surface planarization; The conductive material and diffusion barrier layer are etched back using a cyclic etching process, so that the surface of the conductive material is lower than the surface of the semiconductor substrate; The cyclic etching process includes a precursor adsorption step; Post-adsorption purging process; activation process; The activation and purging process, and the above process are repeated more than once; In the precursor adsorption process, a precursor gas containing fluorine gas and a first inert gas are supplied to the etching chamber, thereby adsorbing a portion of the precursor on the surface of the conductive material. In the activation process, a second inert gas is supplied to the etching chamber, and a low-bias power radio frequency pulse is applied to generate inert gas plasma, which activates the adsorbed precursor and then a chemical reaction occurs to achieve the re-etching of the conductive material.
2. The manufacturing method according to claim 1, characterized in that: The fluorine-containing gas contains NF3 or SF6, and the first inert gas contains N2, Ar or He.
3. The manufacturing method according to claim 1, characterized in that: The post-adsorption purging process and / or post-activation purging process include, Supply purge gas Ar; With the pump valve fully open, extract the purging gas for 3-10 seconds.
4. The manufacturing method according to claim 1, characterized in that: The second inert gas contains Ar, He, Ne, Kr, and Xe.
5. The manufacturing method according to any one of claims 1-4, characterized in that: The conductive material is tungsten.
6. The manufacturing method according to any one of claims 1-4, characterized in that: Before forming word line grooves on the semiconductor substrate, an interlayer dielectric layer is also formed on the semiconductor substrate.
7. The manufacturing method according to any one of claims 1-4, characterized in that: It also includes filling the conductive material with insulating protective material after etching back the conductive material to completely cover the conductive material.
Citation Information
Patent Citations
Transistor structure, memory unit array and preparation method thereof
CN108110005A