A process for continuous vacuum crystallization of potassium sorbate

By adopting a continuous vacuum crystallization process in the potassium sorbate preparation process, using liquid-liquid reaction and two-stage vacuum crystallizer, the problems of uneven reaction and solid waste are solved, product quality and production efficiency are improved, and dust-free production is achieved.

CN114230455BActive Publication Date: 2024-11-19NANTONG ACETIC ACID CHEM
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111635238.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-12-29
Publication Date
2024-11-19
Estimated Expiration
2041-12-29

AI Technical Summary

Technical Problem

In the existing potassium sorbate preparation process, there are problems such as uneven reactions, many by-products, many solid wastes and low product quality. In particular, the solid-liquid reaction ratio is difficult to control, resulting in relatively high by-products and residual impurities in the aqueous solution.

Method used

Using continuous vacuum crystallization technology, sorbic acid is dissolved in solvent and reacted with potassium hydroxide or potassium carbonate solution for liquid-liquid reaction. It is vacuum crystallized through two-stage continuous crystallizers, which avoids solid waste generation and impurities residues and reduces drying energy. Consumption.

Benefits of technology

The uniformity of the reaction system is achieved, the quality and production capacity of potassium sorbate is improved, solid waste generation is reduced, equipment costs are reduced, and dust-free production is achieved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114230455B_ABST
    Figure CN114230455B_ABST
Patent Text Reader

Abstract

This invention discloses a process for continuous vacuum crystallization of potassium sorbate, belonging to the chemical industry. The method includes the following steps: dissolving sorbic acid in a mixed solvent of organic solvent and water to obtain a sorbic acid solution, wherein the organic solvent includes one or both of ethanol and acetone; continuously pumping the obtained sorbic acid solution and a potassium hydroxide aqueous solution of a certain concentration into a neutralization reactor at a certain flow rate for continuous neutralization reaction; pumping the neutralized potassium sorbate solution after the neutralization reaction into a two-stage continuous crystallizer at a certain flow rate for continuous vacuum crystallization, wherein the solvent distilled off during crystallization is condensed and refluxed back into the crystallizer; finally, continuously separating the precipitated potassium sorbate crystals and drying them to obtain the finished potassium sorbate product. This invention uses sorbic acid dissolved in a solution for a liquid-liquid reaction with a potassium hydroxide solution, resulting in more uniform mixing and easier reaction control, improving product quality and drying efficiency, and achieving dust-free production.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a process for continuous vacuum crystallization of potassium sorbate, and belongs to the field of chemical industry. Background Art

[0002] Potassium sorbate appears as colorless to white flaky crystals or crystalline powder, with a molecular weight of 150.217, a melting point of 270°C, and a water solubility of 58.2g / 100mL (20°C). Potassium sorbate is an internationally recognized safe preservative, with an antiseptic effect 5 to 10 times that of sodium benzoate and 1 / 5 of its toxicity. Potassium sorbate is widely used in food, beverages, cosmetics, feed and other fields due to its low price, high safety and good antibacterial effect.

[0003] At present, the main method for preparing potassium sorbate in industrial production is: crude sorbic acid reacts with potassium carbonate to obtain a potassium sorbate solution, then activated carbon is added to remove the pigment in the potassium sorbate solution, and then the activated carbon is separated by filtration to obtain a potassium sorbate liquid, and the potassium sorbate liquid is dried by high-speed centrifugal spray to obtain a potassium sorbate powder, which is then granulated by a granulator to become columnar potassium sorbate particles, and then dried and sifted by a fluidized bed to obtain the product potassium sorbate.

[0004] Patent publication CN105198731A provides a method for preparing potassium sorbate, which comprises reacting sorbic acid solid with potassium hydroxide, decolorizing and filtering with activated carbon, then adding low carbon ester to the filtrate for cooling and crystallization, and drying to obtain a quicksand-like potassium sorbate product. This process provides a method for granulating potassium sorbate, but a solvent is added in the later crystallization process, and there are many impurities remaining in the potassium sorbate, and the quality is not high.

[0005] Patent publication CN106478411A provides a method for purifying potassium sorbate, which dissolves potassium sorbate in a solution, decolorizes it twice with a catalyst and block activated carbon, and then distills and crystallizes it to obtain a finished potassium sorbate product. The potassium sorbate decolorization process is complex and produces a large amount of solid waste.

[0006] Patent publication CN104086407A provides a method for preparing potassium sorbate, which includes adding solid sorbic acid and potassium carbonate into an aqueous solution for neutralization reaction, decolorizing with activated carbon, spray drying, and granulating to obtain a finished potassium sorbate product. The process uses a solid-liquid reaction, the reaction is uneven, and activated carbon decolorization produces solid waste.

[0007] The existing potassium sorbate preparation process is to conduct solid-liquid reaction between solid sorbic acid and potassium hydroxide solution, the reaction is uneven, activated carbon is used for decolorization in the later stage, a large amount of solid waste is generated, and impurities in the aqueous solution cannot be effectively removed by spray drying. Specifically, the existing process has the following disadvantages: 1) The potassium sorbate neutralization process is to conduct a neutralization reaction between solid sorbic acid and potassium hydroxide solution. The solid-liquid reaction ratio is difficult to control accurately. At the same time, the reaction is uneven, the local concentration is too high, and the by-products are relatively high; 2) After the reaction is completed, activated carbon is used for decolorization, which produces a large amount of solid waste; 3) The treated potassium sorbate solution is directly spray-dried, potassium sorbate has no crystalline form, and the impurities in the aqueous solution will remain in the potassium sorbate after drying, affecting the product quality. Summary of the invention

[0008] [Technical issues]

[0009] The current process for producing potassium sorbate using sorbic acid and potassium hydroxide / potassium carbonate has problems such as uneven reaction, many by-products, much solid waste, and low product quality.

[0010] [Technical solution]

[0011] In order to solve the problems of uneven neutralization reaction of potassium sorbate, many by-products, much solid waste, and low product quality. The present invention provides a process method for continuous vacuum crystallization of potassium sorbate, which uses continuous vacuum crystallization to make the preparation process of potassium sorbate continuous. Specifically, the present invention dissolves sorbic acid in a solvent and reacts with potassium hydroxide solution or potassium carbonate solution in a liquid-liquid manner to ensure the uniformity of the reaction system, and then uses a vacuum crystallizer for continuous crystallization to avoid the generation of crystal scale and solid waste in the crystallizer. The vacuum crystallizer does not require a heat exchange device, has a simple structure, and is relatively low in price. The potassium sorbate content in the wet product obtained by crystallization is high, the product quality is high, and the drying energy consumption is reduced.

[0012] The first object of the present invention is to provide a process for continuous vacuum crystallization of potassium sorbate, the process comprising the following steps:

[0013] (1) dissolving sorbic acid in a mixed solvent of an organic solvent and water to obtain a sorbic acid solution, wherein the organic solvent comprises one or both of ethanol and acetone;

[0014] (2) continuously pumping the sorbic acid solution obtained in step (1) and a certain concentration of potassium hydroxide or potassium carbonate aqueous solution into a neutralization reactor at a certain flow rate to carry out a continuous neutralization reaction;

[0015] (3) pumping the potassium sorbate neutralized solution after the neutralization reaction into a two-stage continuous crystallizer at a certain flow rate for continuous vacuum crystallization, wherein the solvent evaporated during the crystallization process is condensed and then refluxed into the crystallizer;

[0016] (4) After the potassium sorbate crystals precipitated in step (3) are continuously separated, they are dried to obtain a potassium sorbate product.

[0017] In one embodiment of the present invention, in step (1), the concentration of the organic solvent in the organic solvent-water mixed solvent is 10 to 90% (v / v).

[0018] In one embodiment of the present invention, in step (1), the concentration of the sorbic acid solution is 10 to 60 wt %.

[0019] In one embodiment of the present invention, in step (1), the dissolution process is continuously carried out at a certain temperature, and the temperature is 30-80°C.

[0020] In one embodiment of the present invention, in step (2), the reaction temperature is controlled at 40-80°C, the pH is maintained at 9-11 and the reaction residence time is 0.5-5h.

[0021] In one embodiment of the present invention, in step (2), the concentration of the potassium hydroxide or potassium carbonate aqueous solution is 5 to 15 wt %.

[0022] In one embodiment of the present invention, in step (2), the molar ratio of sorbic acid to potassium hydroxide or potassium carbonate is 1:0.9-1.3.

[0023] In one embodiment of the present invention, in step (2), the flow rate of the sorbic acid solution is 3-10 mL / min, and the flow rate of the potassium hydroxide aqueous solution or potassium carbonate solution is 4-8 mL / min.

[0024] In one embodiment of the present invention, in step (3), the operating parameters of the two-stage continuous crystallizer are: the system pressure of the first-stage vacuum crystallizer is -0.06 to -0.02 MPa, the crystallization temperature is controlled at 45 to 60°C, and the crystallization residence time is 0.5 to 3 hours; the system pressure of the second-stage vacuum crystallizer is -0.1 to -0.05 MPa, the crystallization temperature is controlled at 10-30°C, and the crystallization residence time is 0.5 to 5 hours.

[0025] In one embodiment of the present invention, in step (3), the crystallizer is any one of a kettle crystallizer or a tubular crystallizer.

[0026] In one embodiment of the present invention, in step (3), the certain flow rate is 7 to 18 mL / min.

[0027] In one embodiment of the present invention, step (4) also includes the following operations: recovering the solvent from the mother liquor accounting for 5-30% of the total mass of the mother liquor, incinerating the kettle liquid after the solvent is recovered, and returning the recovered solvent and the remaining mother liquor to the dissolution process of step (1) to dissolve sorbic acid.

[0028] In one embodiment of the present invention, the solvent recovery is preferably carried out under normal pressure.

[0029] In one embodiment of the present invention, the potassium sorbate crystals obtained in step (4) are in the form of regular particles, with a content of ≥99.8%, a transmittance of ≥98.5%, a proportion of less than 80 mesh and less than 1%, and a proportion of more than 30 mesh and less than 5%.

[0030] In one embodiment of the present invention, the method specifically comprises the following steps:

[0031] 1) firstly, sorbic acid and an aqueous solution containing a solvent of a certain concentration are continuously mixed and dissolved at a certain mass ratio at a certain temperature, wherein the solvent is one of ethanol or acetone, the concentration of the aqueous solution containing the solvent is in the range of 10-90% (v / v), the mixing temperature is controlled at 30-80° C., and the mass concentration of the dissolved sorbic acid is 10-60%;

[0032] 2) The solution containing sorbic acid and a certain concentration of potassium hydroxide aqueous solution are continuously injected into a neutralization reactor at a certain flow rate for continuous neutralization reaction, and the reaction temperature is controlled at 40-80° C., the pH is maintained at 9-11, and the reaction residence time is 0.5-5 h;

[0033] 3) The potassium sorbate neutralized solution obtained in step 2) is pumped into a two-stage continuous crystallizer at a certain flow rate for continuous vacuum crystallization, the system pressure of the first-stage vacuum crystallizer is -0.06 to -0.02 MPa, the crystallization temperature is controlled at 45 to 60° C., and the crystallization residence time is 0.5 to 3 h. The system pressure of the second-stage vacuum crystallizer is -0.1 to -0.05 MPa, the crystallization temperature is controlled at 10-30° C., and the crystallization residence time is 0.5 to 5 h. The crystallizer involved is a kettle crystallizer or a tubular crystallizer. The solvent evaporated during the crystallization process is condensed and then refluxed into the crystallizer to keep the concentration of the potassium sorbate neutralized solution in the crystallizer unchanged;

[0034] 4) After the precipitated potassium sorbate crystals are continuously separated, the damp potassium sorbate is dried to obtain a potassium sorbate product, and the mother liquor accounting for 5-30% of the total mass of the mother liquor is subjected to solvent recovery under normal pressure, the kettle liquid after the solvent is recovered is incinerated, and the recovered solvent and the remaining mother liquor are returned to the dissolution process to dissolve sorbic acid.

[0035] The present invention also provides application of the above-mentioned potassium sorbate continuous vacuum crystallization process method in the fields of food, beverage, cosmetics and feed.

[0036] Compared with the prior art, the present invention has the following advantages and effects:

[0037] 1) In the present invention, sorbic acid is dissolved in a solution to obtain a sorbic acid solution, and then a liquid-liquid reaction is carried out with a potassium hydroxide or potassium carbonate solution. Compared with the traditional solid-liquid reaction, the liquid-liquid reaction process of the present invention is easy to control, and the reactants are mixed more evenly;

[0038] 2) The present invention adopts a vacuum crystallizer for continuous crystallization, and does not need to use a heat exchanger for heat exchange, which reduces equipment cost and avoids the generation of crystal scale on the heat exchange surface. The crystallization process can separate impurities well, and the content of potassium sorbate in the wet product is increased, which greatly reduces the energy consumption of drying and the residence time of the material at high temperature, further improves the product quality and product drying capacity, and the proportion of crystallized products below 80 mesh is very small, realizing dust-free production;

[0039] 3) Solvent recovery is performed after the mother liquor is partially eliminated, so that impurities will not accumulate excessively in the reaction system, avoiding the use of activated carbon, reducing the generation of solid waste, and at the same time greatly reducing the cost of raw materials. BRIEF DESCRIPTION OF THE DRAWINGS

[0040] Figure 1 The present invention provides a schematic flow chart of a process method for continuous vacuum crystallization of potassium sorbate.

[0041] Figure 2 Example 1 Granular potassium sorbate obtained by vacuum crystallization. DETAILED DESCRIPTION

[0042] Transmittance test method: Weigh 5.0g (accurate to 0.01g) of potassium sorbate sample and dissolve it in 20mL of distilled water. Use distilled water as the reference solution and measure its transmittance at 430nm.

[0043] Particle size test method: Take 100g (accurate to 0.01g) of potassium sorbate sample and sieve it with sieves of different mesh sizes. The particle size ratio = mass at the particle size / total mass*100%.

[0044] Potassium sorbate content determination method: Weigh 0.2g of dry potassium sorbate, accurate to 0.0002g, and place it in a 250mL iodine volumetric flask containing 48mL glacial acetic acid and 2mL acetic anhydride, and warm it to make a solution. Cool it to room temperature, add 2 drops of crystal violet indicator solution, and titrate it with a perchloric acid standard titration solution (C = 0.1mol / L) until the solution changes from purple to blue-green. The required volume of the perchloric acid standard titration solution is V1.

[0045] At the same time as the determination, a blank test is performed on the actual solution with the same amount of the added sample according to the same steps as the determination. The required volume of the standard perchloric acid titration solution is V2.

[0046] The mass fraction of potassium sorbate (on a dry basis) W1 = (V1-V2) / 1000*0.1*150.2 / m*100%, where m is the mass of the sample.

[0047] The present invention is further described below in conjunction with examples, but the embodiments of the present invention are not limited thereto.

[0048] The present invention provides a process for continuous vacuum crystallization of potassium sorbate, the method comprising:

[0049] 1) continuously mixing and dissolving sorbic acid and an aqueous solution containing a solvent at a certain concentration in a certain mass ratio at a certain temperature, wherein the solvent is one of ethanol or acetone, the concentration of the aqueous solution containing the solvent is in the range of 10-90%, the mixing temperature is controlled at 30-80° C., and the mass concentration of the dissolved sorbic acid is 10-60%;

[0050] 2) The solution containing sorbic acid and a certain concentration of potassium hydroxide aqueous solution are continuously injected into a neutralization reactor at a certain flow rate for continuous neutralization reaction, and the reaction temperature is controlled at 40-80° C., the pH is maintained at 9-11, and the reaction residence time is 0.5-5 h;

[0051] 3) The potassium sorbate neutralized solution obtained in step 2) is pumped into a two-stage continuous crystallizer at a certain flow rate for continuous vacuum crystallization, the system pressure of the first-stage vacuum crystallizer is -0.06 to -0.02 MPa, the crystallization temperature is controlled at 45 to 60° C., and the crystallization residence time is 0.5 to 3 h. The system pressure of the second-stage vacuum crystallizer is -0.1 to -0.05 MPa, the crystallization temperature is controlled at 10-30° C., and the crystallization residence time is 0.5 to 5 h. The crystallizer involved is a kettle crystallizer or a tubular crystallizer. The solvent evaporated during the crystallization process is condensed and then refluxed into the crystallizer to keep the concentration of the potassium sorbate neutralized solution in the crystallizer unchanged;

[0052] 4) After the precipitated potassium sorbate crystals are continuously separated, the damp potassium sorbate is dried to obtain a potassium sorbate product, and the mother liquor accounting for 5-30% of the total mass of the mother liquor is subjected to solvent recovery under normal pressure, the kettle liquid after the solvent is recovered is incinerated, and the recovered solvent and the remaining mother liquor are returned to the dissolution process to dissolve sorbic acid.

[0053] The potassium sorbate crystals prepared according to the above method are in the form of regular particles, with a content of ≥99.8%, a transmittance of ≥98.5%, a proportion of less than 80 meshes <1%, and a proportion of more than 30 meshes <5%.

[0054] Example 1

[0055] 1) 100 g of sorbic acid and 250 g of an aqueous solution with a 40% alcohol concentration are continuously mixed and dissolved at 80° C., and the mass concentration of the sorbic acid after the dissolution is 28.6%;

[0056] 2) injecting a sorbic acid solution with a mass concentration of 28.6% and 600 g of an 8.4% potassium hydroxide aqueous solution into a neutralization reactor at flow rates of 3.7 mL / min and 6.3 mL / min, respectively, for continuous neutralization reaction, controlling the reaction temperature at 80° C., maintaining the pH at 10.5, and the reaction residence time for 2 h;

[0057] 3) The potassium sorbate neutralized solution obtained in step 2) is then injected into a two-stage continuous crystallizer at a flow rate of 10 mL / min for continuous vacuum crystallization, the system pressure of the first crystallizer is -0.04 MPa, the crystallization temperature is controlled at 52° C., the crystallization residence time is 2.5 h, the system pressure of the second crystallizer is controlled at -0.06 MPa, the crystallization temperature is controlled at 23° C., and the crystallization residence time is 2 h, wherein the crystallizers involved are all kettle crystallizers;

[0058] 4) After the potassium sorbate crystals precipitated in step 3) are continuously separated, the obtained damp potassium sorbate is dried to obtain a potassium sorbate product, and the mother liquor accounting for 28% of the total mass of the mother liquor is subjected to solvent recovery under normal pressure.

[0059] After testing, it was found that the finished potassium sorbate was in regular granular form, with a content of 99.81%, a transmittance of 98.5%, 0.3% below 80 mesh, and 4.6% above 30 mesh.

[0060] Example 2

[0061] 1) 100 g of sorbic acid and 250 g of an aqueous solution having an alcohol content of 90% are continuously mixed and dissolved at 50° C., and the mass concentration of the sorbic acid after the dissolution is 28.57%;

[0062] 2) 28.57% sorbic acid solution and 360 g 14% potassium hydroxide aqueous solution were continuously introduced into the neutralization reactor at flow rates of 5.5 mL / min and 5.5 mL / min, respectively, for continuous neutralization reaction, the reaction temperature was controlled at 60° C., the pH was maintained at 10.5, and the reaction residence time was 3 h;

[0063] 3) The potassium sorbate neutralized solution obtained in step 2) is then injected into a two-stage continuous crystallizer at a flow rate of 11 mL / min for continuous vacuum crystallization, the system pressure of the first-stage crystallizer is -0.02 MPa, the crystallization temperature is controlled at 45° C., the crystallization residence time is 3 h, the system pressure of the second-stage crystallizer is -0.09 MPa, the crystallization temperature is controlled at 19° C., and the crystallization residence time is 2.5 h, wherein the crystallizers involved are all kettle crystallizers;

[0064] 4) After the potassium sorbate crystals precipitated in step 3) are continuously separated, the obtained damp potassium sorbate is dried to obtain a potassium sorbate product, and the mother liquor accounting for 14% of the total mass of the mother liquor is subjected to solvent recovery under normal pressure.

[0065] After testing, it was found that the finished potassium sorbate was in regular granular form, with a content of 99.82%, a transmittance of 98.6%, 0.7% below 80 mesh, and 3% above 30 mesh.

[0066] Example 3

[0067] 1) 100 g of sorbic acid and 400 g of an aqueous solution of 40% acetone were continuously mixed and dissolved at 70° C., and the mass concentration of the sorbic acid after the dissolution was 20%;

[0068] 2) 20% sorbic acid solution and 500 g 10.1% potassium hydroxide aqueous solution were continuously introduced into the neutralization reactor at flow rates of 5 mL / min and 5 mL / min, respectively, for continuous neutralization reaction, the reaction temperature was controlled at 75° C., the pH was maintained at 10.5, and the reaction residence time was 3.5 h;

[0069] 3) The potassium sorbate neutralized solution obtained in step 2) is then injected into a two-stage continuous crystallizer at a flow rate of 10 mL / min for continuous vacuum crystallization, the system pressure of the first-stage crystallizer is -0.06 MPa, the crystallization temperature is controlled at 49° C., the crystallization residence time is 2 h, the system pressure of the second-stage crystallizer is -0.08 MPa, the crystallization temperature is controlled at 12° C., and the crystallization residence time is 3.5 h, wherein the crystallizers involved are all tubular crystallizers;

[0070] 4) After the potassium sorbate crystals precipitated in step 3) are continuously separated, the obtained damp potassium sorbate is dried to obtain a finished potassium sorbate product, and the mother liquor accounting for 23% of the total mass of the mother liquor is subjected to solvent recovery under normal pressure. After testing, it can be found that the finished potassium sorbate is in the form of regular particles, with a content of 98.83%, a transmittance of 98.7%, 4.7% above 30 mesh, 95.1% between 30 and 80 mesh, and 0.2% below 80 mesh.

[0071] Example 4

[0072] 1) 100 g of sorbic acid and 550 g of an aqueous solution of 60% acetone were continuously mixed and dissolved at 40° C., and the mass concentration of the sorbic acid after the dissolution was 15.38%;

[0073] 2) 15.38% sorbic acid solution and 700 g 7.2% potassium hydroxide aqueous solution were continuously introduced into the neutralization reactor at flow rates of 4.8 mL / min and 5.2 mL / min, respectively, for continuous neutralization reaction, the reaction temperature was controlled at 65° C., the pH was maintained at 10.5, and the reaction residence time was 5 h;

[0074] 3) The potassium sorbate neutralized solution obtained in step 2) is then injected into a two-stage continuous crystallizer at a flow rate of 10 mL / min for continuous vacuum crystallization, the system pressure of the first-stage crystallizer is -0.04 MPa, the crystallization temperature is controlled at 55° C., the crystallization residence time is 1 h, the system pressure of the second-stage crystallizer is -0.1 MPa, the crystallization temperature is controlled at 27° C., and the crystallization residence time is 2.5 h, wherein the crystallizers involved are all tubular crystallizers;

[0075] 4) After the potassium sorbate crystals precipitated in step 3) are continuously separated, the obtained damp potassium sorbate is dried to obtain a potassium sorbate product, and the mother liquor accounting for 27% of the total mass of the mother liquor is subjected to solvent recovery under normal pressure.

[0076] After testing, it was found that the finished potassium sorbate was in the form of regular particles, with a content of 99.87%, a transmittance of 98.8%, 0.3% below 80 mesh, and 2.6% above 30 mesh.

[0077] Comparative Example 1

[0078] 1) 10 g of sorbic acid and 1020 g of water were continuously mixed and dissolved at 80° C. The mass concentration of sorbic acid after the dissolution was 0.97%;

[0079] 2) 0.97% sorbic acid solution and 500 g 1% potassium hydroxide aqueous solution were continuously introduced into the neutralization reactor at flow rates of 6.6 mL / min and 3.3 mL / min, respectively, for continuous neutralization reaction, the reaction temperature was controlled at 75° C., the pH was maintained at 10.5, and the reaction residence time was 3 h;

[0080] (2) 3) The potassium sorbate neutralized solution obtained in step 2) is then pumped into a two-stage continuous crystallizer at a flow rate of 9.9 mL / min for continuous vacuum crystallization. The system pressure of the first-stage crystallizer is -0.02 MPa, the crystallization temperature is controlled at 45°C, and the crystallization residence time is 3 h. The system pressure of the second-stage crystallizer is -0.09 MPa, the crystallization temperature is controlled at 19°C, and the crystallization residence time is 2.5 h. The crystallizers involved are all kettle crystallizers; no potassium sorbate is precipitated.

[0081] Comparative Example 2

[0082] 1) 100 g of sorbic acid and 550 g of an aqueous solution of 60% acetone were continuously mixed and dissolved at 40° C., and the mass concentration of the sorbic acid after the dissolution was 15.38%;

[0083] 2) 15.38% sorbic acid solution and 700 g 7.2% potassium hydroxide aqueous solution were continuously introduced into the neutralization reactor at flow rates of 4.8 mL / min and 5.2 mL / min, respectively, for continuous neutralization reaction, the reaction temperature was controlled at 65° C., the pH was maintained at 10.5, and the reaction residence time was 5 h;

[0084] 3) The potassium sorbate neutralized solution obtained in step 2) is then injected into a two-stage continuous crystallizer at a flow rate of 9.9 mL / min for continuous vacuum crystallization, the system pressure of the first crystallizer is -0.04 MPa, the crystallization temperature is controlled at 55° C., the crystallization residence time is 1 h, the system pressure of the second crystallizer is -0.04 MPa, the crystallization temperature is controlled at 27° C., and the crystallization residence time is 2.5 h, wherein the crystallizers involved are all kettle crystallizers;

[0085] 4) After the potassium sorbate crystals precipitated in step 3) are continuously separated, the obtained damp potassium sorbate is dried to obtain a potassium sorbate product, and the mother liquor accounting for 27% of the total mass of the mother liquor is subjected to solvent recovery under normal pressure.

[0086] After testing, it was found that the finished potassium sorbate was in regular granular form, with a content of 98.5% and a transmittance of 96.3%. The proportion of particles above 30 mesh was 7.7%, the proportion of particles between 30 and 80 mesh was 86%, and the proportion of particles below 80 mesh was 6.3%.

[0087] Comparative Example 3

[0088] 1) 100 g of sorbic acid and 550 g of an aqueous solution of 60% acetone were continuously mixed and dissolved at 40° C., and the mass concentration of the sorbic acid after the dissolution was 15.38%;

[0089] 2) 15.38% sorbic acid solution and 700 g 7.2% potassium hydroxide aqueous solution were continuously introduced into the neutralization reactor at flow rates of 4.8 mL / min and 5.2 mL / min, respectively, for continuous neutralization reaction, the reaction temperature was controlled at 65° C., the pH was maintained at 10.5, and the reaction residence time was 5 h;

[0090] 3) The potassium sorbate neutralized solution obtained in step 2) is then injected into a two-stage continuous crystallizer at a flow rate of 10 mL / min for continuous vacuum crystallization, the system pressure of the first-stage crystallizer is -0.08 MPa, the crystallization temperature is controlled at 55° C., the crystallization residence time is 1 h, the system pressure of the second-stage crystallizer is -0.1 MPa, the crystallization temperature is controlled at 27° C., and the crystallization residence time is 0.5 h, wherein the crystallizers involved are all tubular crystallizers;

[0091] 4) After the potassium sorbate crystals precipitated in step 3) are continuously separated, the obtained damp potassium sorbate is dried to obtain a potassium sorbate product, and the mother liquor accounting for 27% of the total mass of the mother liquor is subjected to solvent recovery under normal pressure.

[0092] After testing, it was found that the finished potassium sorbate was in regular granular form, with a content of 96.21%, a transmittance of 88.6%, 7.4% of the particles above 30 mesh, 87.5% of the particles between 30 and 80 mesh, and 5.1% of the particles below 80 mesh.

[0093] Although the present invention has been disclosed as above in the form of a preferred embodiment, it is not intended to limit the present invention. Anyone familiar with this technology can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the scope of protection of the present invention should be based on the definition of the claims.

Claims

1. A process for continuous vacuum crystallization of potassium sorbate, characterized in that: The process comprises the following steps: (1) dissolving sorbic acid in a mixed solvent of an organic solvent and water to obtain a sorbic acid solution, wherein the concentration of the organic solvent is 10 to 90% (v / v), wherein the organic solvent comprises one or both of ethanol and acetone; (2) continuously pumping the sorbic acid solution obtained in step (1) and a certain concentration of potassium hydroxide or potassium carbonate aqueous solution into a neutralization reactor at a certain flow rate to carry out a continuous neutralization reaction; (3) The potassium sorbate neutralized solution after the neutralization reaction is pumped into a two-stage continuous crystallizer at a certain flow rate for continuous vacuum crystallization. The system pressure of the first-stage vacuum crystallizer is -0.06~-0.02 MPa, the crystallization temperature is controlled at 45~60°C, and the crystallization residence time is 0.5~3 h. The system pressure of the second-stage vacuum crystallizer is -0.1~-0.05 MPa, the crystallization temperature is controlled at 10~30°C, and the crystallization residence time is 0.5~5 h. The solvent evaporated during the crystallization process is condensed and then refluxed into the crystallizer; (4) The potassium sorbate crystals precipitated in step (3) are continuously separated and then dried to obtain a potassium sorbate product.

2. The process according to claim 1, characterized in that: In step (1), the concentration of the sorbic acid solution is 10-60 wt %.

3. The process according to claim 1, characterized in that: In step (1), the dissolution process is carried out continuously at a certain temperature, which is 30-80°C.

4. The process according to claim 1, characterized in that: In step (2), the reaction temperature is controlled at 40-80°C, the pH is maintained at 9-11, and the reaction residence time is 0.5-5 h.

5. The process according to claim 1, characterized in that: In step (2), the molar ratio of sorbic acid to potassium hydroxide or potassium carbonate is 1:0.9-1.

3.

6. The process according to claim 1, characterized in that: Step (4) also includes the following operations: recovering the solvent from the mother liquor accounting for 5 to 30% of the total mass of the mother liquor, incinerating the kettle liquid after the solvent is recovered, and returning the recovered solvent and the remaining mother liquor to the dissolution process of step (1) to dissolve the sorbic acid.

7. The process according to claim 1, characterized in that: The method specifically comprises the following steps: 1) First, sorbic acid and an aqueous solution containing a certain concentration of solvent are continuously mixed and dissolved at a certain mass ratio at a certain temperature, wherein the solvent is one of ethanol or acetone, the concentration range of the aqueous solution containing the solvent is 10-90% (v / v), the mixing temperature is controlled at 30-80°C, and the mass concentration of the dissolved sorbic acid is 10-60%; 2) The solution containing sorbic acid and a certain concentration of potassium hydroxide aqueous solution are continuously injected into the neutralization reactor at a certain flow rate for continuous neutralization reaction, and the reaction temperature is controlled at 40-80°C, the pH is maintained at 9-11, and the reaction residence time is 0.5-5 h; 3) The potassium sorbate neutralized solution obtained in step 2) is pumped into a two-stage continuous crystallizer at a certain flow rate for continuous vacuum crystallization, the system pressure of the first-stage vacuum crystallizer is -0.06~-0.02 MPa, the crystallization temperature is controlled at 45~60°C, and the crystallization residence time is 0.5~3 h. The system pressure of the second-stage vacuum crystallizer is -0.1~-0.05 MPa, the crystallization temperature is controlled at 10~30°C, and the crystallization residence time is 0.5~5 h. The crystallizer involved is a kettle crystallizer or a tubular crystallizer. The solvent evaporated during the crystallization process is condensed and then refluxed into the crystallizer to keep the concentration of the potassium sorbate neutralized solution in the crystallizer unchanged; 4) After the precipitated potassium sorbate crystals are continuously separated, the potassium sorbate product is dried to obtain the finished potassium sorbate product, and the mother liquor accounting for 5-30% of the total mass of the mother liquor is subjected to solvent recovery under normal pressure. The kettle liquid after the solvent is recovered is incinerated, and the recovered solvent and the remaining mother liquor are returned to the dissolution process to dissolve sorbic acid.