A method for establishing constitutive model of geotechnical materials

By conducting uniaxial compression tests and pore compaction characteristics analysis in geotechnical materials, combined with the macroscopic strain probability density function modified by the yield point, a more accurate constitutive model of geotechnical materials was established, which solved the problem of existing models in the compaction stage. The problem of insufficient description ability improves the accuracy of theoretical modeling and engineering analysis in the field of geotechnical engineering.

CN114357564BActive Publication Date: 2024-10-01CENT SOUTH UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111462318.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-12-02
Publication Date
2024-10-01
Estimated Expiration
2041-12-02

AI Technical Summary

Technical Problem

The simplified assumptions of existing geomaterial constitutive models in the compaction stage limit their quantitative description capabilities, especially for porous rocks, resulting in low accuracy and large errors in model description results, which cannot effectively reflect the nonlinear deformation characteristics of rocks. .

Method used

The compaction point and yield point are determined through uniaxial compression tests, and a constitutive model under multi-level loading is established based on the compaction characteristics of pores. The complete constitutive structure of geotechnical materials is constructed through the macroscopic strain probability density function modified by the yield point. Model.

Benefits of technology

This method improves the accuracy of describing the compression deformation behavior of geotechnical materials. It is especially suitable for theoretical modeling and engineering stability analysis in the field of geotechnical engineering. It reduces the experience and subjectivity of the model and improves the accuracy of the results.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114357564B_ABST
    Figure CN114357564B_ABST
Patent Text Reader

Abstract

The present invention discloses a method for establishing a constitutive model of geotechnical materials, including performing a uniaxial compression test, determining a compaction point and a yield point based on an axial stress difference; calculating the axial strain of a rock matrix and the axial strain of pores based on the compaction characteristics of pores, and establishing a constitutive model before the yield point after multi-stage loading; establishing a constitutive model after the yield point through a probability density function of macroscopic strain corrected based on the yield point; and completing the establishment of a constitutive model of geotechnical materials by combining the constitutive model before the yield point and the constitutive model after the yield point. The present invention utilizes an analysis of the compaction stage of rock, and uses the yield point to correct the probability density function of the existing strain, which is in good agreement with the test results, ensuring the accuracy of the description of the rock compression deformation behavior, and is particularly suitable for theoretical modeling and engineering stability analysis in the field of geotechnical engineering.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of geotechnical engineering, and in particular relates to a method for establishing a constitutive model of geotechnical materials. Background Art

[0002] The constitutive model is one of the important tools for evaluating the mechanical properties and deformation properties of geotechnical materials. It has important guiding significance for the reasonable design and accurate evaluation of the stability and reliability of rock structures. The constitutive model is referred to as the SDC model. The existing constitutive models can be roughly divided into two categories: linear models and nonlinear models, such as Figure 1 is a schematic diagram of the existing constitutive model; Figure 1 a is the elastic-brittle model, Figure 1 b is a trilinear model, Figure 1 c is a four-linear model, Figure 1 d is a five-linear model, Figure 1 e is the Duncan model, Figure 1 f is the Mazars model, Figure 1 g is the Loland model, Figure 1 h is the statistical damage. Among them, the linear models include the elastic-brittle damage model, the trilinear model, the quadrilinear model (i.e., the bilinear strain softening-residual ideal plasticity model) and the pentalinear model; the nonlinear constitutive models include the Duncan model, the Loland model, the Mazars model and the SCD model. These models all make simplified assumptions about the compaction stage of the axial stress-strain, which limits these models to qualitative analysis but not quantitative description of the complete axial stress-strain curve. The nonlinear characteristics of the compaction stage can be attributed to the deformation of the original microcracks. For dense rocks such as granite, diabase, and marble, there are fewer original microcracks and smaller nonlinear deformations. The simplified assumption of ignoring the compaction stage is basically consistent with the experimental observations of dense rocks. However, this assumption is not applicable to porous rocks such as carbonaceous shale, sandy slate, and clastic sandstone, because their axial stress-strain curves have obvious compaction stages and show obvious nonlinear characteristics. Since the compaction stage is the key stage of rock deformation, the compaction stage should be considered when establishing the constitutive model.

[0003] Generally speaking, the stress-strain curve of geomaterials under compression can be divided into four stages: compaction stage, elastic stage, plastic yield stage and post-peak stage, such as Figure 2 This is a schematic diagram of the axial stress-strain of a typical compression test. Figure 2 The strains at the compaction point a and the yield point b are ε cc and ε y By identifying three specific stress thresholds (crack closure stress σ cc , yield stress σ y and peak stress σ p), the range of four stages can be determined: (1) crack closure stress represents the complete closure of the original microcracks and the beginning of elastic deformation; (2) yield stress appears at the end of the elastic stage, and the rock begins to deform nonlinearly; (3) peak stress is the maximum stress of the entire constitutive curve. It is worth noting that in the triaxial compression test, the axial stress σ i refers to the deviatoric stress σ 1 -σ 3 , while in the uniaxial compression test, σ i The maximum principal stress σ 1 .

[0004] At present, some representative studies on the constitutive model of geotechnical materials considering the compaction stage are as follows:

[0005] Cao,et al.[K.Cao,L.Ma,Y.Wu,A.Spearing,N.Khan,and Y.Xie,"Thedetermination of a damage model for mudstone under uniaxial loading in acidicconditions,"Geofluids,vol.2020,pp.1-12,10 / 08 2020.]phenomenologically simplified the constitutive relation in the compaction stage to a quadratic function based on crack closure stress. Liu,et al.[HHLiu,J.Rutqvist,andJ.G.Berryman,"On the relationship between stress and elastic strain forporous and fractured rock,"Int J Rock Mech Min Sci,vol.46,no.2,pp.289-296,2009.]developed a dual-strain Hooke model to simulate the stress-strain relationship of rock. Cao, et al. [WG Cao, H. Zhao, X. Li, and YJ Zhang, "Statistical damage model with strain softening and hardening for rocks under the influence of voids and volume changes," (in English), Can. Geotech. J., Article vol. 47, no. 8, pp. 857-871, Aug 2010.] abstracted the rock material into two parts: pores and rock matrix (including damaged parts and undamaged parts), and modified the classic Lemaitre damage model, assuming that the damaged part can also bear the load. This improves the calculation accuracy of the overall deformation of the rock to a certain extent.Peng,et al.[J.Peng,G.Rong,CBZhou,and K.Peng,"A study of crack closure effect of rocks and its quantitative model,"(in Chinese),Rock And SoilMechanics, Article vol.37,no.1,pp.126-132,Jan 2016],[J.Peng,G.Rong,M.Cai,andC.B. Zhou,"A model for characterizing crack closure effect of rocks,"EngGeol,vol.189,pp.48-57,2015 / 04 / 30 / 2015.]Based on the compression test results of North African gabbro and Carrara marble, an empirical constitutive model for the rock compaction stage was proposed.

[0006] However, the above studies have not yet identified a universally recognized model with clear physical and mathematical meanings. Each method is highly empirical and subjective, and the model description results have low accuracy, large errors, and large deviations from actual results. Summary of the invention

[0007] The object of the present invention is to provide a method for establishing a constitutive model of geotechnical materials, which takes into account the pore compaction characteristics and establishes a more efficient and accurate constitutive model of geotechnical materials.

[0008] The method for establishing the constitutive model of geotechnical materials provided by the present invention comprises the following steps:

[0009] S1. Perform uniaxial compression test to determine the compaction point and yield point based on the axial stress difference;

[0010] S2. Based on the compaction characteristics of pores, the axial strain of the rock matrix and the axial strain of the pores are calculated, and the constitutive model before the yield point after multi-level loading is established;

[0011] S3. Establish the constitutive model after the yield point through the probability density function of the macroscopic strain corrected based on the yield point;

[0012] S4. Combine the constitutive model before the yield point and the constitutive model after the yield point to complete the establishment of the constitutive model of geotechnical materials.

[0013] The step S1 includes performing a uniaxial compression test on a rock sample, establishing an axial strain-axial stress curve of the rock sample based on the test data; drawing a reference straight line based on the elastic modulus; drawing a stress difference-strain curve, including calculating the axial stress difference between each test data point on the axial stress-strain curve and the reference straight line; one end of the horizontal end of the obtained stress difference-strain curve is the compaction point, and the other end is the yield point.

[0014] The step S1 includes performing a uniaxial compression test on the rock sample, establishing an axial strain-axial stress curve of the rock sample based on the test data, and drawing a reference straight line based on the elastic modulus E, the formula of the reference straight line is σ i *=Eε i , where σ i * is the reference stress, ε i Represents strain; draws stress difference-strain curve, including calculating each test data point (ε i ,σ i ) and the reference straight line σ i *=Eε i The axial stress difference (σ i *-σ i );σ i Represents stress; one end of the horizontal end of the obtained stress difference-strain curve is the compression point a, and the other end is the yield point b.

[0015] The step S2 comprises the following steps:

[0016] A1. Establish an initial model of columnar rock units;

[0017] A2. Calculate the axial strain of the rock matrix and the axial strain of the pores based on the compaction characteristics of the pores;

[0018] A3. Substitute the deformation under axial stress into the columnar rock model to obtain the basic constitutive model of the rock;

[0019] A4. Substitute the axial strain of the rock matrix and the axial strain of the pores obtained in step A2 into the basic constitutive model of the rock in step A3 to obtain the final constitutive model of the rock before the yield point.

[0020] The step A1 comprises taking a representative columnar rock unit along the axial stress direction, setting the axial length of the columnar rock unit to L, and the rock matrix length to L. m , the pore length is L v , γ is the proportion of pores in the columnar rock unit; the step A2 includes obtaining the axial strain ε of the rock matrix after loading m :

[0021]

[0022] Among them, E m represents the elastic modulus of the rock matrix; μ m represents the Poisson's ratio of the rock matrix; σ 1 represents the maximum principal stress; σ 2 represents the intermediate principal stress; σ 3 represents the minimum principal stress; and the length of the pore after compression is The axial strain ε of the pore is v for:

[0023]

[0024] Among them, L v is the pore length;

[0025] Stress σ i In the compression test, multi-stage loading is used, and the stress increment of the i-th stage is tends to infinitesimal; the axial strain of the pore ε v is the strain Δε under each level of stress increment v,i sum:

[0026]

[0027] Among them, E v i represents the stress increment at level i The corresponding pore deformation modulus; the length of the pore after compression is derived

[0028]

[0029] Among them, L v is the pore length; E v i represents the stress increment at level i The corresponding pore deformation modulus; thus the axial strain ε of the compressed pore is obtained v :

[0030]

[0031] Among them, σ 1 represents the maximum principal stress; E v is the elastic modulus of the pore.

[0032] The step A3 includes setting the deformation of the rock matrix to be ΔL m , the deformation of the pore is ΔL v , calculate and obtain the axial strain ε of the rock matrix m Deformation of rock matrix ΔLm The relationship between the axial strain ε of the pore v The deformation of the pore ΔL v Relationship:

[0033]

[0034] Where L is the axial length of the columnar rock unit; ΔL m is the rock matrix deformation; ΔL v is the pore deformation; γ is the proportion of pores in the columnar rock unit; suppose the macroscopic deformation of the columnar rock unit under axial stress ΔL = ΔL m +ΔL v , and obtain the basic constitutive model of rock:

[0035]

[0036] Where ε is the macroscopic strain, L is the axial length of the columnar rock unit; ΔL m is the rock matrix deformation; ΔL v is the pore deformation; γ is the proportion of pores in columnar rock units.

[0037] The step A4 comprises converting the axial strain ε of the rock matrix obtained in step A2 into m and the axial strain ε of the pore v Substitute the basic constitutive model of rock in step A3 to obtain the final constitutive model of rock before the yield point:

[0038]

[0039] Where E represents the elastic modulus of the rock material; μ represents the Poisson's ratio of the rock material before the yield point; γ is the proportion of pores in the columnar rock unit; E v is the elastic modulus of the pore; σ 1 represents the maximum principal stress; σ 2 represents the intermediate principal stress; σ 3 represents the minimum principal stress;

[0040] Calculate the elastic modulus E of the pore v and the proportion of pores in the columnar rock unit, γ, including: For the stress-strain curve under uniaxial compression, at the yield point b(ε y ,σ y ) where the derivative of the axial stress-strain curve is equal to the elastic modulus E of the rock material before the yield point:

[0041]

[0042] Where E represents the elastic modulus of rock material; (ε y ,σy ) is the stress-strain coordinate of the yield point b; γ is the proportion of pores in the columnar rock unit; E v is the elastic modulus of the pore; σ 1 represents the maximum principal stress; ε represents the macroscopic strain;

[0043] Solving for this yields: Assume the reference equation The horizontal coordinate of the intersection of the reference equation is the elastic modulus E of the pore v .

[0044] The step S3 comprises the following steps:

[0045] B1. Calculate the improved damage model:

[0046] B2. Using the modified Weibull distribution, calculate the probability density function of macroscopic strain;

[0047] B3. Calculate the damage variable through the probability density function of macroscopic strain, and substitute the damage variable into the improved damage model of step B1 to obtain the constitutive model after the yield point.

[0048] The step B1 includes that the axial stress is borne by the rock matrix and the damaged rock matrix:

[0049] σ i A=E(ε-ε cc )A * +σ r (AA * )

[0050] Among them, σ i represents stress; σ r represents the stress that damages the rock matrix; A is the area of ​​axial stress action; ε represents the macroscopic strain; E represents the elastic modulus of the rock material; ε cc represents the strain at the compaction point a; A* represents the distribution area of ​​the undamaged rock matrix;

[0051] Set the damage variable D to: D = (AA*) / A, then simplify the formula to

[0052] σ i =E(ε-ε cc )(1-D)+σ r D

[0053] Among them, σ i represents stress; σ r represents the stress that damages the rock matrix; ε represents the macroscopic strain; E represents the elastic modulus of the rock material; ε cc represents the strain at the compaction point a; combined with the crack closure stress σ cc, and the improved damage model is obtained:

[0054] σ i -σ cc =E(ε-ε cc )(1-D)+(σ r -σ cc )D

[0055] Among them, σ i represents stress; σ r represents the stress that damages the rock matrix; ε represents the macroscopic strain; E represents the elastic modulus of the rock material; ε cc represents the strain at the compaction point a; σ cc is the crack closure stress; D is the damage variable.

[0056] The step B2 comprises setting the yield point b(ε y ,σ y ) is taken as the starting point of rock damage; therefore, the yield stress σ y Modified Weibull distribution:

[0057]

[0058] Where ω(ε) represents the probability density function of the macroscopic strain ε; M is the model shape parameter; ε 0 is the model scale parameter; (ε y ,σ y ) is the stress-strain coordinate of the yield point b;

[0059] The step B3 includes integrating the probability density function ω(ε) of the macro strain ε to obtain the damage variable D:

[0060]

[0061] Where ω(ε) represents the probability density function of the macroscopic strain ε; M is the model shape parameter; ε 0 is the model scale parameter; (ε y ,σ y ) is the stress-strain coordinate of the yield point b;

[0062] Substitute the damage variable D into the improved damage model in step B1 to obtain the yield point b(ε y ,σ y ) after:

[0063]

[0064] Among them, σ i represents stress; ε represents macroscopic strain; σ rrepresents the stress that damages the rock matrix; E represents the elastic modulus of the rock material; ε cc represents the strain at the compaction point a; σ cc is the crack closure stress; (ε y ,σ y ) is the stress-strain coordinate of the yield point b; M is the model shape parameter; ε 0 is the model scale parameter; fitting model shape parameter and model scale parameter ε 0 ,include:

[0065] The yield point b(ε y ,σ y ) is substituted into the yield point b(ε y ,σ y ) after:

[0066] σ y =E(ε y -ε cc )+σ cc

[0067] Where E represents the elastic modulus of rock material; ε cc represents the strain at the compaction point a; σ cc is the crack closure stress; (ε y ,σ y ) is the stress-strain coordinate of the yield point b; mathematical operations are used to obtain the model shape parameter M and model scale parameter ε 0 Relationship:

[0068]

[0069] Think of both sides as new variables X, Y, and Z:

[0070]

[0071] Then the yield point b(ε y ,σ y ) can be simplified as follows:

[0072] Y=MX+Z

[0073] The yield point b(ε y ,σ y ) after the constitutive model, the slope and intercept of the fitting line are the parameters M and -Mlnε respectively. 0 , and obtain M and -Mlnε through linear regression 0 , and obtain the model shape parameter M and model scale parameter ε 0 The value of .

[0074] The method for establishing the constitutive model of geotechnical materials provided by the present invention utilizes the analysis of the rock compaction stage and adopts the yield point to correct the probability density function of the existing strain, thereby ensuring the accuracy of the description of the rock compression deformation behavior, and is particularly suitable for theoretical modeling and engineering stability analysis in the field of geotechnical engineering. BRIEF DESCRIPTION OF THE DRAWINGS

[0075] Figure 1 It is a schematic diagram of the existing constitutive model;

[0076] Figure 2 Schematic diagram of axial stress-strain in a typical compression test.

[0077] Figure 3 It is a schematic diagram of the process of the present invention.

[0078] Figure 4 It is a schematic diagram of the positions of the compaction point and the yield point of the method of the present invention.

[0079] Figure 5 The figure is a schematic diagram of the structure of the columnar rock unit of the method of the present invention.

[0080] Figure 6 Schematic diagram of the intersection of the reference equations of the method of the present invention.

[0081] Figure 7 Schematic diagram of the damaged rock matrix portion of the method of the present invention.

[0082] Figure 8 Schematic diagram of comparison between the existing theoretical constitutive model and the test results of an embodiment of the present invention.

[0083] Fig. 9 Schematic diagram of the uniaxial compression stress-strain curve of the A1 sample according to an embodiment of the present invention.

[0084] Fig.10 Schematic diagram of determining relevant parameters of the A1 sample according to an embodiment of the present invention.

[0085] Fig.11 Schematic diagram of the intersection of reference equations according to an embodiment of the present invention.

[0086] Fig.12 Schematic diagram of model parameter fitting according to an embodiment of the present invention.

[0087] Fig.13 It is a schematic diagram comparing the embodiment of the present invention with the test results. DETAILED DESCRIPTION

[0088] like Figure 3 The flowchart of the method of the present invention is as follows: The method for establishing the constitutive model of geotechnical materials provided by the present invention comprises the following steps:

[0089] S1. Perform uniaxial compression test to determine the compaction point and yield point based on the axial stress difference;

[0090] S2. Based on the compaction characteristics of pores, the axial strain of the rock matrix and the axial strain of the pores are calculated, and the constitutive model before the yield point after multi-level loading is established;

[0091] S3. Establish the constitutive model after the yield point through the probability density function of the macroscopic strain corrected based on the yield point;

[0092] S4. Combine the constitutive model before the yield point and the constitutive model after the yield point to complete the establishment of the constitutive model of geotechnical materials.

[0093] like Figure 4 The schematic diagram of the compaction point and yield point position of the method of the present invention. The step S1 includes performing a uniaxial compression test on the rock sample, establishing an axial strain-axial stress curve of the rock sample based on the test data; drawing a reference straight line based on the elastic modulus E, and the formula of the reference straight line is σ i *=Eε i , where σ i * is the reference stress, ε i Represent strain; draw stress difference-strain curve, including calculating each test data point (ε i ,σ i ) and the reference straight line σ i *=Eε i The axial stress difference (σ i *-σ i );σ i Represents stress; one end of the horizontal end of the obtained stress difference-strain curve is the compression point a, and the other end is the yield point b.

[0094] The step S2 comprises the following steps:

[0095] like Figure 5 A1. Establish an initial model of the columnar rock unit; for ease of analysis, the rock matrix is ​​regarded as a composite geological material composed of pores and rock matrix; Figure 3 As shown in the figure, a representative columnar rock unit is taken along the axial stress direction, and the axial length of the columnar rock unit is set to L, and the rock matrix length is L m , the pore length is L v , γ is the proportion of pores in columnar rock units, so:

[0096]

[0097] A2. Based on the compaction characteristics of pores, calculate the axial strain of the rock matrix and the axial strain of the pores: Since the rock matrix deforms linearly after loading and can return to its original state before the yield point after unloading, the axial strain ε of the rock matrix after loading is obtained according to the generalized Hooke's law. m :

[0098]

[0099] Among them, E m represents the elastic modulus of the rock matrix; μ m represents the Poisson's ratio of the rock matrix; σ 1 represents the maximum principal stress; σ 2 represents the intermediate principal stress; σ 3 represents the minimum principal stress; in conventional triaxial compression tests, σ 2 =σ 3 ; When the deformation reaches the elastic stage, the pores are almost closed, so there is no need to consider the influence of the pores, and the deformation at this stage can be approximated to the deformation of the bedrock matrix. m and μ m It can be approximately replaced by the elastic modulus E of the rock material before the yield point and the Poisson's ratio μ of the rock material before the yield point.

[0100] Starting from the definition of strain itself, we can accurately describe the deformation of the pore after compression: Assume that the length of the pore after compression is The axial strain ε of the pore is v for:

[0101]

[0102] Among them, L v is the pore length;

[0103] Assuming stress σ i In the compression test, it is considered as multi-stage loading, and the stress increment of the i-th stage is tends to infinitesimal; then the axial strain ε of the pore v can be converted into the stress σ i function; ignoring the influence of lateral stress, the axial strain ε of the pore v is the strain Δε under each level of stress increment v,i sum:

[0104]

[0105] Among them, E v i represents the stress increment at level i The corresponding pore deformation modulus; then the equation is obtained:

[0106]

[0107] Solve to get the length of the pore after compression

[0108]

[0109] Among them, L v is the pore length; E v i represents the stress increment at level i The corresponding pore deformation modulus; thus the axial strain ε of the compressed pore is obtained v

[0110]

[0111] Among them, E v i represents the stress increment at level i The corresponding pore deformation modulus;

[0112] If each level of stress increment The corresponding pore deformation modulus E v i remain unchanged, Simplified to Among them, E v is the elastic modulus of the pore.

[0113] A3. Substitute the deformation under axial stress into the columnar rock model to obtain the macroscopic strain of the columnar rock unit under axial stress: Assume that the deformation of the rock matrix is ​​ΔL m , the deformation of the pore is ΔL v , calculate and obtain the axial strain ε of the rock matrix m Deformation of rock matrix ΔL m The relationship between the axial strain ε of the pore v The deformation of the pore ΔL v Relationship:

[0114]

[0115] Where L is the axial length of the columnar rock unit; ΔL m is the rock matrix deformation; ΔL v is the pore deformation; γ is the proportion of pores in the columnar rock unit; suppose the macroscopic deformation of the columnar rock unit under axial stress ΔL = ΔL m +ΔL v , the macroscopic strain ε of the columnar rock unit under axial stress is obtained, that is, the basic constitutive model of rock:

[0116]

[0117] Where L is the axial length of the columnar rock unit; ΔL m is the rock matrix deformation; ΔL v is the pore deformation; γ is the proportion of pores in the columnar rock unit; in the prior art, the macroscopic strain ε is ε = ε m +ε v ,This method adds the influence of the proportion of pores in the columnar rock unit on the columnar rock unit, and the prediction is more accurate and closer to the actual deformation of the rock material.

[0118] A4. Substitute the axial strain ε of the rock matrix obtained in step A2 into m and the axial strain ε of the pore v Substitute the basic constitutive model of rock in step A3 to obtain the final constitutive model of rock before the yield point:

[0119]

[0120] Where E represents the elastic modulus of the rock material; μ represents the Poisson's ratio of the rock material before the yield point; γ is the proportion of pores in the columnar rock unit; E v is the elastic modulus of the pore; σ 1 represents the maximum principal stress; σ 2 represents the intermediate principal stress; σ 3 represents the minimum principal stress;

[0121] Among them, the elastic modulus of the pore E v The solution method for the ratio of pores in columnar rock units is as follows: Figure 2 The strain at the yield point b is shown as ε y ; For the stress-strain curve under uniaxial compression, at the yield point b(ε y ,σ y ) exists a special boundary condition, that is, the derivative of the axial stress-strain curve is equal to the elastic modulus E of the rock material before the yield point:

[0122]

[0123] Where E represents the elastic modulus of rock material; (ε y ,σ y ) is the stress-strain coordinate of the yield point b; γ is the proportion of pores in the columnar rock unit; E v is the elastic modulus of the pore; σ 1 represents the maximum principal stress; ε represents the macroscopic strain;

[0124] Solving for this yields: like Figure 6The reference equation intersection diagram of the method of the present invention is shown in FIG. The horizontal coordinate of the intersection of the reference equation is the elastic modulus E of the pore v .

[0125] like Figure 7 FIG. 1 is a schematic diagram of the damaged rock matrix of the method of the present invention. Since the rock deformation enters the plastic yield stage after the yield point, the rock matrix is ​​not damaged in the elastic stage, but is damaged after the yield point. Considering that in the triaxial compression test, Figure 2 As shown, the rock sample in the post-peak stage still has bearing capacity under the influence of friction and confining pressure. The step S3 comprises the following steps:

[0126] B1. Calculate the improved damage model: Figure 7 As shown in Figure 2, the axial stress is shared by the rock matrix and the damaged rock matrix:

[0127] σ i A=E(ε-ε cc )A * +σ r (AA * )

[0128] Among them, σ i represents stress; σ r represents the stress that damages the rock matrix; A is the area where the axial stress acts; ε represents the macroscopic strain; E represents the elastic modulus of the rock material; Figure 2 As shown cc represents the strain at the compaction point a; A* represents the distribution area of ​​the undamaged rock matrix;

[0129] Set the damage variable D to: D = (AA*) / A, then simplify the formula to

[0130] σ i =E(ε-ε cc )(1-D)+σ r D

[0131] Among them, σ i represents stress; σ r represents the stress that damages the rock matrix; ε represents the macroscopic strain; E represents the elastic modulus of the rock material; ε cc represents the strain at the compaction point a; combined with the crack closure stress σ cc , we can get the improved damage model:

[0132] σ i -σ cc =E(ε-ε cc )(1-D)+(σ r -σ cc )D

[0133] Among them, σ i represents stress; σ r represents the stress that damages the rock matrix; ε represents the macroscopic strain; E represents the elastic modulus of the rock material; ε cc represents the strain at the compaction point a; σ cc is the crack closure stress; D represents the damage variable;

[0134] B2. The probability density function of the macroscopic strain ε is calculated using the modified Weibull distribution. According to the damage statistics theory, the damage variable D is solved using the probability density function. The statistical constitutive model based on the Weibull distribution in the prior art is suitable for the damage variable D of rock materials, namely:

[0135]

[0136] Where M is the model shape parameter; ε 0 is the model scale parameter. Figure 8 The figure is a schematic diagram comparing the existing theoretical constitutive model and the test results of the embodiment of the present invention. However, the theoretical constitutive model established according to the prior art has a large deviation from the experimental results in the pre-peak stage. The reason is that the prior art ignores the compaction stage and considers the damage starting point to be (0,0), that is, the rock material will be damaged as soon as the macroscopic compression deformation occurs, which conflicts with the fact that the rock sample can restore the stress-strain curve after unloading in the elastic stage.

[0137] Therefore, since the stress σ at the yield point y is the stress threshold of rock plastic yield deformation, and the yield point b(ε y ,σ y ) is taken as the starting point of rock damage; therefore, the yield point stress σ y Modified Weibull distribution:

[0138]

[0139] Where ω(ε) represents the probability density function of the macroscopic strain ε; M is the model shape parameter; ε 0 is the model scale parameter; (ε y ,σ y ) is the stress-strain coordinate of the yield point b;

[0140] B3. Calculate the damage variable D through the probability density function of the macro strain ε, including integrating the probability density function ω(ε) of the macro strain ε to obtain the damage variable D:

[0141]

[0142] Where ω(ε) represents the probability density function of the macroscopic strain ε; M is the model shape parameter; ε 0 is the model scale parameter; (ε y ,σ y ) is the stress-strain coordinate of the yield point b;

[0143] Substitute the damage variable D into the improved damage model in step B1 to obtain the yield point b(ε y ,σ y ) after:

[0144]

[0145] Among them, σ i represents stress; ε represents macroscopic strain; σ r represents the stress that damages the rock matrix; E represents the elastic modulus of the rock material; ε cc represents the strain at the compaction point a; σ cc is the crack closure stress; M is the model shape parameter; ε 0 is the model scale parameter; (ε y ,σ y ) is the stress-strain coordinate of the yield point b.

[0146] Since this method uses the yield point b(ε y ,σ y ) as the dividing point to establish the constitutive model respectively. Therefore, it is necessary to prove whether the constitutive model before the yield point and the constitutive model after the yield point can be connected at the dividing point. In step A4, the coordinates of the yield point have been substituted into the constitutive model before the yield point. Therefore, it is only necessary to prove that the yield point b(ε y ,σ y ) conforms to the constitutive model after the yield point, and the yield point b(ε y ,σ y ) is substituted into the yield point b(ε y ,σ y ) after:

[0147] σ y =E(ε y -ε cc )+σ cc

[0148] Where E represents the elastic modulus of rock material; ε cc represents the strain at the compaction point a; σ cc is the crack closure stress; (ε y ,σ y ) is the stress-strain coordinate of the yield point b; Figure 2As shown, in the elastic stage, the increment of axial stress is linearly related to the increment of axial strain, and the stress-strain ratio is the elastic modulus E, that is: σ i -σ cc =E(ε-ε cc ), due to the yield point b(ε y ,σ y ) is the end point of the elastic stage, and we can get σ y -σ cc =E(ε y -ε cc ), therefore, the yield point b(ε y ,σ y ) is substituted into the yield point b(ε y ,σ y ) after the constitutive model, that is, σ y =E(ε y -ε cc )+σ cc Therefore, the yield point b(ε y ,σ y ) is consistent with the constitutive model after the yield point.

[0149] Fitting model shape parameter M and model scale parameter ε 0 , the yield point b(ε y ,σ y ) is substituted into the yield point b(ε y ,σ y ) after the constitutive model: σ y =E(ε y -ε cc )+σ cc Rewritten as:

[0150]

[0151] Divide both sides by E(ε-ε cc )-(σ r -σ cc ):

[0152]

[0153] Take the logarithm of both sides:

[0154]

[0155] Take the logarithm of both sides again:

[0156]

[0157] Think of both sides as new variables X, Y, and Z:

[0158]

[0159] Then the yield point b(ε y ,σ y ) can be simplified as follows:

[0160] Y=MX+Z

[0161] Then the yield point b(ε y ,σ y ) after the constitutive model, the slope and intercept of the fitting line are the parameters M and -Mlnε respectively. 0 Therefore, linear regression gives M and -Mlnε 0 The model shape parameters M and ε can be further obtained 0 is the model scale parameter ε 0 The value of .

[0162] like Fig. 9 Schematic diagram of the uniaxial compression stress-strain curve of the A1 sample of the embodiment of the present invention. In this embodiment, the stress-strain data of the red sandstone A1 sample under uniaxial compression of Bai, et al. [Y.Bai, RL Shan, Y.Ju, YX Wu, PF Sun, and ZE Wang, "Study on the mechanical properties and damage constitutive model of frozen weaklycemented red sandstone," Cold Reg Sci Technol, vol.171, p.102980, 2020 / 03 / 01 / 2020.] are used to verify the new model.

[0163] like Fig.10 Schematic diagram of determining relevant parameters of sample A1 according to an embodiment of the present invention. First, the compaction point a and the yield point b are determined according to the method of step S1. From the elastic modulus E = 1.302 GPa, the residual strength σ r =7.083MPa. The reference line σ=1302·ε can be determined from the elastic modulus. The stress difference between the reference line and the axial stress-strain curve is calculated and plotted on Fig.10 In. From Fig.10 The two endpoints of the horizontal segment can be directly determined: the compression point a and the yield point b, from which σ can be determined cc =4.254Mpa, ε cc =0.01058,σ y =12.61MPa, ε y =0.017; Fig.11Schematic diagram of the intersection of reference equations in an embodiment of the present invention. Calculate E v =1.936MPa,γ=0.0074.

[0164] The model expression before obtaining the yield point is:

[0165]

[0166] like Fig.12 The following is a schematic diagram of model parameter fitting in an embodiment of the present invention. The fitting results show that M = 2.147, ε 0 =0.0067. Therefore, the model expression after the yield point can be obtained:

[0167]

[0168] The model expressions before and after the yield point are obtained. Fig.12 It is a schematic diagram comparing the embodiment of the present invention with the test results. Fig.13 The comparison results show that the model curve is in good agreement with the experimental results.

Claims

1. A method for establishing a constitutive model of geotechnical materials, characterized in that The steps include: S1. Perform uniaxial compression test to determine the compaction point and yield point based on the axial stress difference; S2. Based on the compaction characteristics of the pores, the axial strain of the rock matrix and the axial strain of the pores are calculated, and a constitutive model before the yield point after multi-level loading is established; including the following steps: A1. Establish an initial model of columnar rock units; A2. Calculate the axial strain of the rock matrix and the axial strain of the pores based on the compaction characteristics of the pores; A3. Substitute the deformation under axial stress into the columnar rock model to obtain the basic constitutive model of the rock; A4. Substitute the axial strain of the rock matrix and the axial strain of the pores obtained in step A2 into the basic constitutive model of the rock in step A3 to obtain the final constitutive model of the rock before the yield point; S3. Establishing a constitutive model after the yield point by using a probability density function of macroscopic strain corrected based on the yield point; comprising the following steps: B1. Calculate the improved damage model: B2. Using the modified Weibull distribution, calculate the probability density function of macroscopic strain; B3. Calculate the damage variable through the probability density function of the macroscopic strain, and substitute the damage variable into the improved damage model of step B1 to obtain the constitutive model after the yield point; S4. Combine the constitutive model before the yield point and the constitutive model after the yield point to complete the establishment of the constitutive model of geotechnical materials.

2. The method for establishing a constitutive model of geotechnical materials according to claim 1, characterized in that The step S1 includes performing a uniaxial compression test on the rock sample, establishing an axial strain-axial stress curve of the rock sample based on the test data, and drawing a reference straight line based on the elastic modulus; Drawing a stress difference-strain curve, including calculating the axial stress difference between each test data point on the axial stress-strain curve and the reference straight line; One end of the horizontal end of the obtained stress difference-strain curve is the compression point, and the other end is the yield point.

3. The method for establishing a constitutive model of geotechnical materials according to claim 2, characterized in that The step S1 includes performing a uniaxial compression test on the rock sample, establishing an axial strain-axial stress curve of the rock sample based on the test data, and drawing a reference straight line based on the elastic modulus E, the formula of the reference straight line is σ i *=Eε i , where σ i * is the reference stress, ε i Represents strain; draws stress difference-strain curve, including calculating each test data point (ε i ,σ i ) and the reference straight line σ i *=Eε i The axial stress difference (σ i *-σ i );σ i Represents stress; one end of the horizontal end of the obtained stress difference-strain curve is the compression point a, and the other end is the yield point b.

4. The method for establishing a constitutive model of geotechnical materials according to claim 3, characterized in that The step A1 comprises taking a representative columnar rock unit along the axial stress direction, setting the axial length of the columnar rock unit to L, and the rock matrix length to L. m , the pore length is L v , γ is the proportion of pores in the columnar rock unit; the step A2 includes obtaining the axial strain ε of the rock matrix after loading m : Among them, E m represents the elastic modulus of the rock matrix; μ m represents the Poisson's ratio of the rock matrix; σ1 represents the maximum principal stress; σ2 represents the intermediate principal stress; σ3 represents the minimum principal stress; and the length of the pore after compression is The axial strain ε of the pore is v for: Among them, L v is the pore length; Stress σ i In the compression test, it is considered as multi-stage loading, and the stress increment of the i-th stage is tends to infinitesimal; the axial strain of the pore ε v is the strain Δε under each level of stress increment v,i sum: Among them, E v i represents the stress increment at level i The corresponding pore deformation modulus; the length of the pore after compression is derived Among them, L v is the pore length; E v i represents the stress increment at level i The corresponding pore deformation modulus; thus the axial strain ε of the compressed pore is obtained v : Where, σ1 represents the maximum principal stress; E v is the elastic modulus of the pore.

5. The method for establishing a constitutive model of geotechnical materials according to claim 4, characterized in that The step A3 includes setting the deformation of the rock matrix to be ΔL m , the deformation of the pore is ΔL v , calculate and obtain the axial strain ε of the rock matrix m Deformation of rock matrix ΔL m The relationship between the axial strain ε of the pore v The deformation of the pore ΔL v Relationship: Where L is the axial length of the columnar rock unit; ΔL m is the rock matrix deformation; ΔL v is the pore deformation; γ is the proportion of pores in the columnar rock unit; suppose the macroscopic deformation of the columnar rock unit under axial stress ΔL = ΔL m +ΔL v , and obtain the basic constitutive model of rock: Where ε is the macroscopic strain, L is the axial length of the columnar rock unit; ΔL m is the rock matrix deformation; ΔL v is the pore deformation; γ is the proportion of pores in columnar rock units.

6. The method for establishing a constitutive model of geotechnical materials according to claim 5, characterized in that The step A4 comprises converting the axial strain ε of the rock matrix obtained in step A2 into m and the axial strain ε of the pore v Substitute the basic constitutive model of rock in step A3 to obtain the final constitutive model of rock before the yield point: Where E represents the elastic modulus of the rock material; μ represents the Poisson's ratio of the rock material before the yield point; γ is the proportion of pores in the columnar rock unit; E v is the elastic modulus of the pore; σ1 represents the maximum principal stress; σ2 represents the intermediate principal stress; σ3 represents the minimum principal stress; Calculate the elastic modulus E of the pore v and the proportion of pores in the columnar rock unit, γ, including: For the stress-strain curve under uniaxial compression, at the yield point b(ε y ,σ y ) where the derivative of the axial stress-strain curve is equal to the elastic modulus E of the rock material before the yield point: Where E represents the elastic modulus of rock material; (ε y ,σ y ) is the stress-strain coordinate of the yield point b; γ is the proportion of pores in the columnar rock unit; E v is the elastic modulus of the pore; σ1 represents the maximum principal stress; ε represents the macroscopic strain; Solving for this yields: Assume the reference equation The horizontal coordinate of the intersection of the reference equation is the elastic modulus E of the pore v .

7. The method for establishing a constitutive model of geotechnical materials according to claim 6, characterized in that The step B1 includes that the axial stress is borne by the rock matrix and the damaged rock matrix: s i A=E(e-e cc )A * +s r (AA * ) Among them, σ i represents stress; σ r represents the stress that damages the rock matrix; A is the area of ​​axial stress action; ε represents the macroscopic strain; E represents the elastic modulus of the rock material; ε cc represents the strain at the compaction point a; A* represents the distribution area of ​​the undamaged rock matrix; Set the damage variable D to: D = (AA*) / A, then simplify the formula to s i =E(e-e cc )(1-D)+σ r D Among them, σ i represents stress; σ r represents the stress that damages the rock matrix; ε represents the macroscopic strain; E represents the elastic modulus of the rock material; ε cc represents the strain at the compaction point a; combined with the crack closure stress ε cc , and the improved damage model is obtained: s i -s cc =E(e-e cc )(1-D)+(σ r -s cc )D Among them, σ i represents stress; σ r represents the stress that damages the rock matrix; ε represents the macroscopic strain; E represents the elastic modulus of the rock material; ε cc represents the strain at the compaction point a; σ cc is the crack closure stress; D is the damage variable.

8. The method for establishing a constitutive model of geotechnical materials according to claim 7, characterized in that The step B2 comprises setting the yield point b(ε y ,σ y ) is taken as the starting point of rock damage; therefore, the yield point stress σ y Modified Weibull distribution: Where ω(ε) represents the probability density function of the macroscopic strain ε; M is the model shape parameter; ε0 is the model scale parameter; (ε y ,σ y ) is the stress-strain coordinate of the yield point b; The step B3 includes integrating the probability density function ω(ε) of the macro strain ε to obtain the damage variable D: Where ω(ε) represents the probability density function of the macroscopic strain ε; M is the model shape parameter; ε0 is the model scale parameter; (ε y ,σ y ) is the stress-strain coordinate of the yield point b; Substitute the damage variable D into the improved damage model in step B1 to obtain the yield point b(ε y ,σ y ) after: Among them, σ i represents stress; ε represents macroscopic strain; σ r represents the strain of the damaged rock matrix; E represents the elastic modulus of the rock material; ε cc represents the strain at the compaction point a; σ cc is the crack closure stress; (ε y ,σ y ) is the stress-strain coordinate of the yield point b; M is the model shape parameter; ε0 is the model scale parameter; the fitting model shape parameter M and the model scale parameter ε0 include: The yield point b(ε y ,σ y ) is substituted into the yield point b(ε y ,σ y ) after: s y =E(e y -e cc )+s cc Where E represents the elastic modulus of rock material; ε cc represents the strain at the compaction point a; σ cc is the crack closure stress; (ε y ,σ y ) is the stress-strain coordinate of the yield point b; mathematical operations are used to obtain the relationship between the model shape parameter M and the model scale parameter ε0: Think of both sides as new variables X, Y, and Z: Then the yield point b(ε y ,σ y ) after which the constitutive model can be simplified as: Y=MX+Z The yield point b(ε y ,σ y ), the slope and intercept of the fitting line are M and -Mlnε0 respectively, and M and -Mlnε0 are obtained by linear regression, and the values ​​of the model shape parameter M and the model scale parameter ε0 are obtained.