A punching process for reducing deformation of high-precision parts
By dividing the punching process into multiple steps to form the head and symmetrical tearing plate of the component pins, and finally punching through to form the component pins, the problems of blade breakage and deformation in the traditional punching process are solved, and high-precision parts are realized. Blanking, extending mold life and ensuring component flatness.
Patent Information
- Application Number
- CN202210064410.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-01-20
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2042-01-20
AI Technical Summary
In the traditional component pin punching process, the cantilever of the punching edge is too long, causing the blade to break, and the two-step punching process can easily cause the component pins to deform, affecting the sheet metal pressing area and mold life.
The punching process is divided into multiple steps. First, the heads of the component pins are formed, and then the symmetrical first and second tearing plates are formed. Finally, the component pins are punched through, and the bevel and angle of the tearing plate punching mechanism are used. The R-angle design prevents tearing and ensures the strength and smoothness of the punching edge.
It effectively avoids the breakage of the punching blade and the force deformation of the component pins, prolongs the life of the mold parts, and obtains flat component pins.
Smart Images

Figure CN114393092B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of molds, and in particular to a punching process for reducing deformation of high-precision parts. Background Art
[0002] Blanking is a stamping process that uses a die to separate sheet materials, including blanking, punching, notching, cutting, trimming, etc. It can be used to make parts or prepare blanks for bending, drawing, forming and other processes. For example, blanking can be used to punch sheet materials to form component pins.
[0003] The traditional component pin punching process is usually divided into two types, such as Figure 1 As shown, one process is the integral punching process of the component pin 10. In this process, during punching, the punching edge cantilever 20 is too long and the width is usually less than 1 mm. The punching edge is weak due to the punching force around it, making the punching edge easy to break, thereby increasing the cost of later mold repair.
[0004] In order to solve the above problems, Figure 2 As shown, the prior art discloses another process, which is to divide the original punching process into two steps, first punching one side 101 of the component pin 10, and then punching the other side 102 of the component pin 10, which can effectively avoid the problem of too long blade cantilever. However, the defect of this process is that single-sided punching is easy to affect the component sheet, resulting in insufficient sheet pressing area, resulting in deformation of the component pin during the next punching step. Summary of the invention
[0005] The present invention aims to solve at least one of the technical problems in the above-mentioned technology to a certain extent. To this end, the purpose of the present invention is to propose a punching process for reducing deformation of high-precision parts, which divides the punching process into multiple steps, effectively avoids the problem of the punching blade being damaged due to the long cantilever of the punching blade, effectively prevents the problem of component pins being deformed by force, and obtains flat component pins under the premise of ensuring the service life of the mold.
[0006] To achieve the above object, an embodiment of the present invention provides a punching process for reducing deformation of high-precision parts, comprising the following steps:
[0007] Step S1, placing the sheet material in a mold;
[0008] Step S2, the mold initially punches through the sheet material to form the head of the component pin;
[0009] Step S3, the mold punches the sheet material without punching through it to form a first tear plate and a second tear plate symmetrical to the first tear plate;
[0010] Step S4: the mold punches through the first tear plate, the second tear plate and the plate material to form component pins.
[0011] According to a punching process for reducing deformation of high-precision parts according to an embodiment of the present invention, when punching a sheet of material, the sheet of material is first placed in a mold; then the mold initially punches through the sheet of material to form the head of the component pin. Since the head of the component pin is relatively short, the cantilever of the punching blade is short, and the problem of damage to the punching blade will not occur; then the mold punches through the sheet of material without punching through to form a first tear plate and a second tear plate. Since the first tear plate is symmetrical with the second tear plate, the problem of component pins being deformed by force will not occur during punching. Finally, the mold punches through the first tear plate, the second tear plate and the sheet of material to form component pins, thereby obtaining flat component pins.
[0012] In addition, the punching process for reducing deformation of high-precision parts proposed in the above embodiment of the present invention may also have the following additional technical features:
[0013] Furthermore, the mold includes a head punching mechanism for punching through the sheet material to form the head of the component pin, a tear plate punching mechanism for punching the sheet material without punching through to form the first tear plate and the second tear plate, and a waste punching mechanism for punching through the first tear plate, the second tear plate and the sheet material to form the component pin.
[0014] Furthermore, the tearing plate blanking mechanism includes a tearing plate punch and a tearing plate die opposite to the tearing plate punch. The end of the tearing plate punch close to the tearing plate die includes an inner side and an outer side opposite to the inner side, and a slope formed between the outer side and the inner side.
[0015] Further, the distance between the inner side and the tear plate concave die is smaller than the distance between the outer side and the tear plate concave die.
[0016] Furthermore, the angle formed by the inclined plane and the horizontal plane is 0.5 degrees to 2 degrees.
[0017] Furthermore, the angle formed by the inclined plane and the horizontal plane is 1 degree.
[0018] Furthermore, an R corner is provided on the outside to prevent the sheet from tearing.
[0019] Furthermore, a blanking gap is set between the tearing plate punch and the tearing plate concave die.
[0020] Furthermore, the tear plate blanking mechanism also includes a tear plate inner limit block for limiting the punching height, a tear plate die pad and a floating push rod. The tear plate inner limit block is arranged in the tear plate die, the tear plate die pad is connected to one side of the tear plate die, and the floating push rod can pass through the tear plate die pad and push out the sheet material.
[0021] Furthermore, the inner limit block of the tear plate includes an inclined surface parallel to the inclined surface and a curved surface opposite to the R angle. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 It is a structural schematic diagram of the punching process in the prior art;
[0023] Figure 2 for Figure 1 Schematic diagram of the structure of the middle punching punch;
[0024] Figure 3 It is a structural schematic diagram of another blanking process in the prior art;
[0025] Figure 4 A flowchart of a blanking process for reducing deformation of high-precision parts according to an embodiment of the present invention;
[0026] Figure 5 A schematic diagram of the structure of a punching process for reducing deformation of high-precision parts according to an embodiment of the present invention;
[0027] Figure 6 is a schematic structural diagram of a first stamping punch according to an embodiment of the present invention;
[0028] Figure 7 A schematic diagram of the structure of a second stamping punch and a third stamping punch according to an embodiment of the present invention;
[0029] Figure 8 A schematic structural diagram of a plate tearing and blanking mechanism according to an embodiment of the present invention;
[0030] Fig. 9 An exploded view of a plate tearing and blanking mechanism according to an embodiment of the present invention;
[0031] Fig.10 Schematic diagram of the structure of a sheet material after being punched by a sheet tearing and blanking mechanism according to an embodiment of the present invention.
[0032] Description of symbols
[0033] Sheet 1;
[0034] Die 2, tearing plate blanking mechanism 21, tearing plate punch 211, inner side 2111, outer side 2112, inclined surface 2113, R angle 2114, tearing plate die 212, tearing plate inner limit block 213, inclined surface 2131, curved surface 2132, tearing plate die pad 214, floating ejector 215, elastic member 216, first stamping punch 22, body 221, first stamping arm 222, second stamping arm 223, stamping gap 224, second stamping punch 23, third stamping punch 24;
[0035] Component pin 3, head 31, first tear plate 32, second tear plate 33. DETAILED DESCRIPTION
[0036] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present invention, and should not be construed as limiting the present invention.
[0037] like Figures 3 to 10 As shown, a punching process for reducing deformation of high-precision parts according to an embodiment of the present invention comprises the following steps:
[0038] Step S1, placing the sheet material 1 in the mold 2; Step S2, the mold 2 initially punches through the sheet material 1 to form the head 31 of the component pin 3; Step S3, the mold 2 punches through the sheet material 1 without punching through to form a first tear plate 32 and a second tear plate 33 symmetrical to the first tear plate 32; Step S4, the mold 2 punches through the first tear plate 32, the second tear plate 33 and the sheet material 1 to form the component pin 3.
[0039] When punching the sheet material 1, the sheet material 1 is first placed in the mold 2; then the mold 2 initially punches through the sheet material 1 to form the head 31 of the component pin 3. Since the head 31 of the component pin 3 is relatively short, the cantilever of the punching blade is short, and the problem of the punching blade being damaged will not occur; then the mold 2 punches through the sheet material 1 without punching through to form the first tear plate 32 and the second tear plate 33. Since the first tear plate 32 is symmetrical to the second tear plate 33, the problem of the component pin 3 being deformed by force will not occur during punching. Finally, the mold 2 punches through the first tear plate 32, the second tear plate 33 and the sheet material 1 to form the component pin 3, thereby obtaining a flat component pin 3.
[0040] Optionally, the mold 2 includes a head punching mechanism for punching the sheet material 1 to form the head 31 of the component pin 3, a tear plate punching mechanism 21 for punching the sheet material 1 without punching through to form a first tear plate 32 and a second tear plate 33, and a waste punching mechanism for punching the first tear plate 32, the second tear plate 33 and the sheet material 1 to form the component pin 3.
[0041] Among them, the head punching mechanism is to punch through the sheet material 1 to form the head 31 of the component pin 3, which includes a first punching punch 22, the first punching punch 22 includes a body 221, a first punching arm 222 and a second punching arm 223, a punching gap 224 is formed between the first punching arm 222 and the second punching arm 223, the length of the first punching arm 222 and the second punching arm 223 is relatively short, and the problem of the punching edge breaking can be effectively avoided during punching. The waste punching mechanism includes a second punching punch 23 and a third punching punch 24, the second punching punch 23 and the third punching punch 24 are independent of each other, and the second punching punch 23 and the third punching punch 24 are symmetrical to each other to prevent the component pin 3 from being deformed by force during punching. Since the second punching punch 23 and the third punching punch 24 are independent of each other, the problem of the punching edge breaking will not occur.
[0042] In this example, the tearing plate blanking mechanism 21 includes a tearing plate punch 211 and a tearing plate die 212 opposite to the tearing plate punch 211, and the end of the tearing plate punch 211 close to the tearing plate die 212 includes an inner side 2111 and an outer side 2112 opposite to the inner side 2111, and an inclined surface 2113 is formed between the outer side 2112 and the inner side 2111. Among them, the distance between the inner side 2111 and the tearing plate die 212 is smaller than the distance between the outer side 2112 and the tearing plate die 212. The angle formed by the inclined surface 2113 and the horizontal plane is 0.5 degrees to 2 degrees. As a preferred embodiment, the angle formed by the inclined surface 2113 and the horizontal plane is 1 degree.
[0043] After testing, it was found that when the angle formed by the inclined surface 2113 and the horizontal plane is 0.5 to 2 degrees, when the tearing punch 211 is punching, the force on the sheet 1 is distributed in a step-like manner, so that the punching effect is better. During punching, the punching depth of the inner sheet 2111 is greater than the punching depth of the outer sheet 2112, which prevents tearing during punching.
[0044] In some examples, an R angle 2114 is provided on the outer side 2112 to prevent the sheet material 1 from tearing, wherein the size of the R angle 2114 is preferably 0.3m, so that during stamping, this part of the material will not tear but bend, thereby ensuring the connection strength between the first tear plate 32 and the sheet material 1, and ensuring the connection strength between the second tear plate 33 and the sheet material 1.
[0045] As an example, a shearing gap is set between the tear plate punch 211 and the tear plate die 212. The shearing gap is preferably less than 0.03 mm, such as 0.03 mm. The smaller the shearing gap, the smaller the shearing collapse angle, but the inserts are severely worn. Therefore, a reasonable shearing gap can ensure both the quality of the components and the life of the inserts of the mold 2.
[0046] In this example, the tearing plate blanking mechanism 21 also includes a tearing plate inner limit block 213 for limiting the punching height, a tearing plate die pad 214 and a floating push rod 215. The tearing plate inner limit block 213 is set in the tearing plate die 212, and the tearing plate die pad 214 is connected to one side of the tearing plate die 212. The floating push rod 215 can pass through the tearing plate die pad 214 and push out the sheet 1. When the tearing plate blanking mechanism 21 punches, the R angle 2114 of the outer side 2112 corresponds to the position of the sheet 1 and shows a bending trend without tearing off, and cooperates with the inclined surface 2113 to achieve stepped punching. The tearing plate inner limit block 213 limits the punching height to prevent punching through. After the punching is completed, the floating push rod 215 of the tearing plate die pad 214 is pushed out to avoid deformation of the sheet 1 caused by uneven stripping. Among them, the floating push rod 215 is connected to an elastic member 216, such as a compression spring, and the floating push rod 215 can be pushed out by connecting the compression spring.
[0047] In this example, the tear plate inner limit block 213 includes an inclined surface 2131 parallel to the inclined surface 2113 and a curved surface 2132 opposite to the R angle 2114. In this way, when the tear plate punch 211 is punched, it can effectively cooperate with the tear plate inner limit block 213, so that the thickness of the first tear plate 32 and the second tear plate 33 are consistent, and the R angle 2114 and the curved surface 2132 prevent the sheet material 1 from tearing, ensuring that the sheet material 1 is bent.
[0048] The above embodiments and drawings do not limit the product form and style of the present invention. Any appropriate changes or modifications made thereto by ordinary technicians in the relevant technical field should be deemed to be within the patent scope of the present invention.
Claims
1. A punching process for reducing deformation of high-precision parts, characterized in that: The following steps are involved: Step S1, placing the sheet material in a mold; Step S2, the mold initially punches through the sheet material to form the head of the component pin; Step S3, the mold punches the sheet material without punching through it to form a first tear plate and a second tear plate symmetrical to the first tear plate; Step S4, the mold punches through the first tear plate, the second tear plate and the sheet material to form component pins; The die includes a head punching mechanism for punching through a sheet material to form a head of a component pin, a tear plate punching mechanism for punching the sheet material without punching through to form a first tear plate and a second tear plate, and a waste punching mechanism for punching through the first tear plate, the second tear plate and the sheet material to form a component pin; The tearing plate blanking mechanism includes a tearing plate punch and a tearing plate die opposite to the tearing plate punch. The end of the tearing plate punch close to the tearing plate die includes an inner side and an outer side opposite to the inner side, and an inclined surface is formed between the outer side and the inner side; the distance between the inner side and the tearing plate die is smaller than the distance between the outer side and the tearing plate die; the angle formed by the inclined surface and the horizontal plane is 0.5 to 2 degrees; an R angle is set on the outer side to prevent the sheet from tearing.
2. The punching process for reducing deformation of high-precision parts according to claim 1, characterized in that: The angle formed by the inclined plane and the horizontal plane is 1 degree.
3. The punching process for reducing deformation of high-precision parts according to claim 1, characterized in that: A blanking gap is set between the tearing plate punch and the tearing plate concave die.
4. The punching process for reducing deformation of high-precision parts according to claim 3, characterized in that: The tear plate blanking mechanism also includes a tear plate inner limit block for limiting the punching height, a tear plate die pad and a floating push rod. The tear plate inner limit block is arranged in the tear plate die, the tear plate die pad is connected to one side of the tear plate die, and the floating push rod can pass through the tear plate die pad and push out the sheet material.
5. The punching process for reducing deformation of high-precision parts according to claim 4, characterized in that: The inner limit block of the tear plate comprises an inclined surface parallel to the inclined surface and a curved surface opposite to the R angle.
Citation Information
Patent Citations
Precise progressive die multistep blanking method for controlling deformation of slender cantilever part
CN101879547A
Smooth and clean fine blanking mould
CN103143612A
Hardware strip double-surface no-burr blanking process and no-burr blanking mold
CN106424296A
Stamping die for spot-faced hole terminal pin
CN112808859A
Blanking mould without blanking trimming
CN201157864Y