A method for synthesizing FDCA via carbon dioxide oxidation and metal-catalyzed HMF

The method of carbon dioxide oxidation and metal-catalyzed HMF simplifies the synthesis process of FDCA, solves the tediousness and environmental protection issues of traditional methods, achieves efficient and economical FDCA production, and uses carbon dioxide to provide solutions to global warming.

CN114573531BActive Publication Date: 2024-10-18NANJING ADVANCED BIOLOGICAL MATERIALS & PROCESS EQUIP INST CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202210302509.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-03-25
Publication Date
2024-10-18
Estimated Expiration
2042-03-25

AI Technical Summary

Technical Problem

The traditional FDCA synthesis process is cumbersome, with complex steps, long reaction times, and the use of a large amount of strong oxidants, which is costly and unfriendly to the environment. The global warming problem requires an effective method to utilize carbon dioxide.

Method used

The method of synthesizing FDCA using carbon dioxide oxidation and metal-catalyzed HMF, reacts with CO2 through NHC coordination metal catalyst, first generates DFF, and then further reacts in an alkali solvent to generate FDCA, preferably Ru/IMes·HCl, Rh/IMes·HCl or Pd /IMes·HCl is used as a catalyst, and the reaction conditions include specific temperature, pressure and solvent system.

Benefits of technology

It simplifies the operation, reduces energy consumption, improves the reaction efficiency, is suitable for industrial production, solves the problems of complicated steps, long reaction time and excessive strong oxidants in the traditional method, and at the same time provides an environmentally friendly solution using carbon dioxide.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114573531B_ABST
    Figure CN114573531B_ABST
Patent Text Reader

Abstract

The present invention discloses a method for synthesizing FDCA by oxidation of carbon dioxide and metal-catalyzed HMF, comprising the following steps: (1) using HMF as a raw material, reacting under the conditions of NHC coordinated metal catalyst and CO2 to obtain DFE; (2) dissolving DFF, ligand NHC and alkali in a solvent, and reacting under a CO2 atmosphere to obtain a compound FDCA. Compared with the prior art, the method provided by the present invention is simple to operate, more economical, environmentally friendly, green and practical. At the same time, it can effectively solve the problems of complicated steps, long reaction time, excessive strong oxidant, low atomic efficiency, high cost, and environmental disadvantages in the traditional reaction process, and can improve the reaction efficiency, which is suitable for industrial production. #imgabs0#
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of FDCA synthesis, and particularly relates to a method for synthesizing FDCA through carbon dioxide oxidation and metal-catalyzed HMF. Background Art

[0002] Furandicarboxylic acid (FDCA) can be converted from biomass resources such as sugars. Since its structure is similar to terephthalic acid, it is regarded as an important biomass platform compound comparable to petrochemical products phthalic acid, terephthalic acid or isophthalic acid. At the same time, FDCA has better performance in terms of biosafety and degradability. In recent years, the preparation of FDCA and its derivative transformation have become a major research hotspot in the field of biochemical engineering. Polyester and polyamide materials using FDCA as raw materials can be used in fibers, films, packaging materials, engineering plastics and other fields. Due to the special non-planar structure of FDCA, the sealing performance of products made of this type of material is better. In addition, FDCA is also widely used in the fields of medicine, chemical industry and so on.

[0003] At present, the most extensive and in-depth research on the synthesis method of FDCA is to use hexose as raw material to generate 5-hydroxymethylfurfural (HMF) through dehydration and cyclization and then oxidize it. Domestic and foreign scholars have carried out a lot of research work on the preparation of HMF and achieved good research results. Common oxidants in the oxidation process of HMF include oxygen, air, H2O2, KMnO4, etc. Among them, the oxidation reaction involving gas has become the current mainstream research route due to its environmental protection and economic advantages.

[0004] Global warming is an increasingly serious problem, mainly caused by the emission of greenhouse gases such as carbon dioxide, methane, nitrous oxide, and chlorofluorocarbons. Since the combustion of oil, coal, and natural gas produces a large amount of CO2 with a significant greenhouse effect, CO2 is the main cause of global warming. Therefore, reducing the content of CO2 in the atmosphere has always been an urgent problem that needs to be solved worldwide. To overcome this problem, there are currently four methods: (1) reducing energy consumption by improving conversion efficiency; (2) replacing non-renewable resources that produce greenhouse gases such as CO2 with renewable energy such as solar energy and wind energy; (3) carbon dioxide capture / storage; and (4) carbon dioxide capture and utilization. Currently, the carbon dioxide capture / storage method may be the most effective method to reduce CO2 in the air. Among these methods, the carbon dioxide capture and utilization method is very promising both in terms of CO2 consumption and in the production of value-added chemicals, because CO2 is an abundant, cheap, non-toxic and non-flammable C1 building block in organic synthesis. Since CO2 has a stable structure and contains carbon with the highest oxidation state, it requires a lot of energy to convert CO2 into raw materials for industrial production. Summary of the invention

[0005] Purpose of the invention: In order to solve the problems existing in the prior art, the present invention provides a method for synthesizing FDCA by oxidation of carbon dioxide and metal-catalyzed HMF, so as to solve the problem of cumbersome process of traditional synthesis of FDCA and provide a new idea for solving global warming by using CO2.

[0006] Technical solution: In order to achieve the above-mentioned invention problem, the technical solution adopted by the present invention is as follows:

[0007] A method for synthesizing FDCA by oxidation of carbon dioxide and metal-catalyzed HMF, comprising the following steps:

[0008]

[0009] (1) Using HMF as raw material, reacting in the presence of NHC coordinated metal catalyst and CO2 to obtain DFF;

[0010] (2) DFF, ligand NHC and base are dissolved in a solvent and reacted under a CO2 atmosphere to obtain the compound FDCA.

[0011] The specific reaction process is as follows:

[0012]

[0013] As a preferred option:

[0014] In step (1), the NHC coordinated metal catalyst is selected from one of Ru / NHC, Rh / NHC, and Pd / NHC; the mass ratio of the metal catalyst to HMF is (0.05-0.15):1, more preferably (0.1-0.14):1, and most preferably 0.12:1.

[0015] Considering the influence of metal on the reaction, IMes·HCl is selected as NHC, and the NHC coordinated metal catalyst is Ru / IMes·HCl, Rh / IMes·HCl or Pd / IMes·HCl, preferably Rh / IMes·HCl; considering the influence of NHC structure on the metal catalyst, the NHC coordinated metal catalyst is Rh / IMes·HCl, Rh / IPr·HCl, Rh / SIMes·HCl, Rh / SIPr·HCl, preferably Rh / IPr·HCl.

[0016] In step (1), the method for preparing the NHC coordinated metal catalyst comprises the following steps:

[0017] The metal catalyst, NHC and alkali are dissolved in a solvent, heated under an inert atmosphere, stirred for reaction, and a solid is separated to obtain the NHC coordinated metal catalyst.

[0018] Further preferably, the metal catalyst is selected from one of Ru / C, Rh / C or Pd / C; the base is one of potassium tert-butoxide or sodium tert-butoxide, more preferably potassium tert-butoxide; the solvent is one of toluene and THF, more preferably toluene; the NHC is selected from any one of IMes·HCl, IPr·HCl, SIMes·HCl and SIPr·HCl, more preferably IMes·HCl and IPr·HCl.

[0019]

[0020] Further preferably, the molar ratio of the metal catalyst: NHC: base is 1:(1-3):(2-6), and more preferably the molar ratio of the metal catalyst: NHC: base is 1:2:4; the reaction temperature is 40-70°C, more preferably 50°C; after the reaction, the solid is washed with ethanol and acetone and then dried to obtain the NHC coordinated metal catalyst.

[0021] In step (1), the reaction pressure is 0.1MPa-4MPa, the reaction time is 4-18h, and the temperature is 130-150°C. More preferably, the reaction pressure is 3-4MPa, the reaction time is 2-4h, and the reaction temperature is 145-150°C.

[0022] In step (2), the NHC is selected from any one of IMes·HCl, IPr·HCl, SIMes·HCl and SIPr·HCl, more preferably IMes·HCl; the base is any one of potassium tert-butoxide, sodium tert-butoxide or DBU; and the solvent is any one of toluene, THF or acetonitrile.

[0023] In step (2), the molar ratio of the ligand NHC:base:DFF is (0.1-0.3):(0.15-0.6):1, more preferably (0.2-0.3):(0.3-0.6):1, and most preferably 0.25:0.5:1.

[0024] In step (2), the reaction temperature is 25±5°C, the reaction time is 1-3h, the reaction pressure is normal pressure, and the more preferred reaction time is 2h.

[0025] In step (1), the autoclave is cooled with an ice bath, and then the solid catalyst is separated from the liquid product by filtration.

[0026] After the reaction in step (2) is quenched with hydrochloric acid, all products are identified by liquid chromatography-mass spectrometry, preferably using a liquid chromatography (HPX-87H) column (Agilent, 300x7.8mm).

[0027] Beneficial effects: Compared with the prior art, the method provided by the present invention is simple to operate, more economical, environmentally friendly, green and practical. At the same time, it can effectively solve the problems of complicated steps, long reaction time, excessive strong oxidant, low atomic efficiency, high cost, unfavorable environmental protection, etc. in the traditional reaction process, and can improve the reaction efficiency, which is suitable for industrial production. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 This is the infrared spectrum of the metal catalyst Rh / IMes.

[0029] Figure 2 This is the FDCA liquid phase standard curve. DETAILED DESCRIPTION

[0030] The experimental methods described in the following examples are conventional methods unless otherwise specified; the reagents and materials described are commercially available unless otherwise specified.

[0031] Embodiment 1:

[0032] 205.82 mg (0.1 mmoL, 5 wt% Rh) Rh / C, 44.8 mg (0.4 mmoL) potassium tert-butoxide and 98.6 mg (0.2 mmoL) IPr·HCl were added to a flask containing toluene, stirred at 50°C overnight under N2 atmosphere, and then the solid and solution were taken out, centrifuged at 2500 rpm for 30 min, and the solid was washed with toluene, ethanol, and acetone and dried to obtain the Rh / IPr metal catalyst; 126.11 mg (1 mmoL) HMF and 15 mg Rh / IPr metal catalyst were added to the autoclave, and flushed with CO2 5 times to remove the air in the autoclave. The autoclave was heated for a period of time to stabilize to the required temperature of 150°C, and then CO2 was charged into the autoclave using a high-pressure liquid pump, and then compressed to 4 MPa, and the reaction was continued for 4 hours, and the contents of the autoclave were stirred with a magnetic stirring bar. After the reaction, the autoclave was cooled with an ice bath, and then the solid catalyst was separated from the liquid product by filtration to obtain 118 mg of DFF with a yield of 95%. 111.7 mg (0.9 mmoL) of DFF, 76.7 mg (0.225 mmoL) of IMes·HCl and 50.5 mg (0.45 mmoL) of potassium tert-butoxide were dissolved in THF, and reacted in a CO2 atmosphere at normal pressure and room temperature of 25°C for 2 h. After the reaction was completed, a hydrochloric acid solution (1N) was added to quench the reaction until the solution was neutral, and then all products were identified by liquid chromatography-mass spectrometry, and the yield of FDCA was 85% (the FDCA peak time was 17.157 min, the maximum absorption wavelength was 265.4 nm, and the peak area was 35885: m / z for C6H4O5(M+H) + 157.0132;

[0033] found157.0130).

[0034] The final yield of FDCA from the two-step reaction was 80.75%.

[0035] Embodiment 2:

[0036] 205.82 mg (0.1 mmoL, 5 wt% Rh) Rh / C, 44.8 mg (0.4 mmoL) potassium tert-butoxide and 68.2 mg (0.2 mmoL) IMes·HCl were added to a flask containing toluene, stirred at 50°C overnight under N2 atmosphere, and then the solid and solution were taken out, centrifuged at 2500 rpm for 30 min, and the solid was washed with toluene, ethanol, and acetone and dried to obtain the Rh / IMes metal catalyst; 126.11 mg (1 mmoL) HMF and 15 mg Rh / IMes metal catalyst were added to the autoclave, and flushed with CO2 5 times to remove the air in the autoclave. The autoclave was heated for a period of time to stabilize to the required temperature of 150°C, and then CO2 was charged into the autoclave using a high-pressure liquid pump, and then compressed to 4 MPa, and the reaction was continued for 4 hours, and the contents of the autoclave were stirred with a magnetic stirring bar. After the reaction, the autoclave was cooled with an ice bath, and then the solid catalyst was separated from the liquid product by filtration to obtain 96.8 mg DFF with a yield of 78%. 93.1 mg (0.75 mmoL) DFF, 63.9 mg (0.189 mmoL) IMes·HCl and 42 mg (0.375 mmoL) potassium tert-butoxide were dissolved in THF, and reacted in a CO2 atmosphere at normal pressure and room temperature of 25°C for 2 h. After the reaction was completed, a hydrochloric acid solution (1N) was added to quench the reaction until the solution was neutral, and then all products were identified by liquid chromatography-mass spectrometry, and the yield of FDCA was 84%.

[0037] The final yield of FDCA from the two-step reaction was 65.5%.

[0038] Embodiment 3:

[0039] 205.82 mg (0.1 mmoL, 5 wt% Rh) Rh / C, 44.8 mg (0.4 mmoL) potassium tert-butoxide and 78.5 mg (0.2 mmoL) SIPr·HCl were added to a flask containing toluene, stirred at 50°C overnight under N2 atmosphere, and then the solid and solution were taken out, centrifuged at 2500 rpm for 30 min, and the solid was washed with toluene, ethanol, and acetone and dried to obtain the Rh / SIPr metal catalyst; 126.11 mg (1 mmoL) HMF and 15 mg Rh / SIPr metal catalyst were added to the autoclave, and flushed with CO2 5 times to remove the air in the autoclave. The autoclave was heated for a period of time to stabilize to the required temperature of 150°C, and then CO2 was charged into the autoclave using a high-pressure liquid pump, and then compressed to 4 MPa, and the reaction was continued for 4 hours, and the contents of the autoclave were stirred with a magnetic stirring bar. After the reaction, the autoclave was cooled with an ice bath, and then the solid catalyst was separated from the liquid product by filtration to obtain 81.9 mg DFF with a yield of 66%. 74.5 mg (0.6 mmoL) DFF, 51.1 mg (0.15 mmoL) IMes·HCl and 33.6 mg (0.3 mmoL) potassium tert-butoxide were dissolved in THF, and reacted in a CO2 atmosphere at normal pressure and room temperature of 25°C for 2 h. After the reaction was completed, a hydrochloric acid solution (1 N) was added to quench the reaction until the solution was neutral, and then all products were identified by liquid chromatography-mass spectrometry, and the yield of FDCA was 85%.

[0040] The final yield of FDCA from the two-step reaction was 56.1%.

[0041] Embodiment 4:

[0042] 205.82 mg (0.1 mmoL, 5 wt% Rh) Rh / C, 44.8 mg (0.4 mmoL) potassium tert-butoxide and 68.6 mg (0.2 mmoL) SIMes·HCl were added to a flask containing toluene, stirred at 50°C overnight under N2 atmosphere, and then the solid and solution were taken out, centrifuged at 2500 rpm for 30 min, and the solid was washed with toluene, ethanol, and acetone and dried to obtain the Rh / SIMes metal catalyst; 126.11 mg (1 mmoL) HMF and 15 mg Rh / SIMes metal catalyst were added to the autoclave, and flushed with CO2 5 times to remove the air in the autoclave. The autoclave was heated for a period of time to stabilize to the required temperature of 150°C, and then CO2 was charged into the autoclave using a high-pressure liquid pump, and then compressed to 4 MPa, and the reaction was continued for 4 hours, and the contents of the autoclave were stirred with a magnetic stirring bar. After the reaction, the autoclave was cooled with an ice bath, and then the solid catalyst was separated from the liquid product by filtration to obtain 65.6 mg DFF with a yield of 52%. 62 mg (0.5 mmoL) DFF, 42.6 mg (0.125 mmoL) IMes·HCl and 28 mg (0.25 mmoL) potassium tert-butoxide were dissolved in THF, and reacted in a CO2 atmosphere at normal pressure and room temperature of 25°C for 2 h. After the reaction was completed, a hydrochloric acid solution (1 N) was added to quench the reaction until the solution was neutral, and then all products were identified by liquid chromatography-mass spectrometry, and the yield of FDCA was 86%.

[0043] The final yield of FDCA obtained by the two-step reaction was 43%.

[0044] Embodiment 5:

[0045] 205.82 mg (0.1 mmoL, 5 wt% Rh) Rh / C, 44.8 mg (0.4 mmoL) potassium tert-butoxide and 98.6 mg (0.2 mmoL) IPr·HCl were added to a flask containing toluene, stirred at 50°C overnight under N2 atmosphere, and then the solid and solution were taken out, centrifuged at 2500 rpm for 30 min, and the solid was washed with toluene, ethanol, and acetone and dried to obtain the Rh / IPr metal catalyst; 126.11 mg (1 mmoL) HMF and 15 mg Rh / IPr metal catalyst were added to the autoclave, and flushed with CO2 5 times to remove the air in the autoclave. The autoclave was heated for a period of time to stabilize to the required temperature of 150°C, and then CO2 was charged into the autoclave using a high-pressure liquid pump, and then compressed to 4 MPa, and the reaction was continued for 4 hours, and the contents of the autoclave were stirred with a magnetic stirring bar. After the reaction, the autoclave was cooled with an ice bath, and then the solid catalyst was separated from the liquid product by filtration to obtain 118 mg of DFF with a yield of 95%. 111.7 mg (0.9 mmoL) of DFF, 87.8 mg (0.225 mmoL) of IPr·HCl and 50.5 mg (0.45 mmoL) of potassium tert-butoxide were dissolved in THF, and reacted in a CO2 atmosphere at normal pressure and room temperature of 25°C for 2 h. After the reaction was completed, a hydrochloric acid solution (1 N) was added to quench the reaction until the solution was neutral, and then all products were identified by liquid chromatography-mass spectrometry, and the yield of FDCA was 80%.

[0046] The final yield of FDCA obtained by the two-step reaction was 76%.

[0047] Embodiment 6:

[0048] 205.82 mg (0.1 mmoL, 5 wt% Rh) Rh / C, 44.8 mg (0.4 mmoL) potassium tert-butoxide and 98.6 mg (0.2 mmoL) IPr·HCl were added to a flask containing toluene, stirred at 50°C overnight under N2 atmosphere, and then the solid and solution were taken out, centrifuged at 2500 rpm for 30 min, and the solid was washed with toluene, ethanol, and acetone and dried to obtain the Rh / IPr metal catalyst; 126.11 mg (1 mmoL) HMF and 15 mg Rh / IPr metal catalyst were added to the autoclave, and flushed with CO2 5 times to remove the air in the autoclave. The autoclave was heated for a period of time to stabilize to the required temperature of 150°C, and then CO2 was charged into the autoclave using a high-pressure liquid pump, and then compressed to 4 MPa, and the reaction was continued for 4 hours, and the contents of the autoclave were stirred with a magnetic stirring bar. After the reaction, the autoclave was cooled with an ice bath, and then the solid catalyst was separated from the liquid product by filtration to obtain 118 mg of DFF with a yield of 95%. 111.7 mg (0.9 mmoL) of DFF, 88.2 mg (0.225 mmoL) of SIPr·HCl and 50.5 mg (0.45 mmoL) of potassium tert-butoxide were dissolved in THF, and reacted in a CO2 atmosphere at normal pressure and room temperature of 25°C for 2 h. After the reaction was completed, a hydrochloric acid solution (1 N) was added to quench the reaction until the solution was neutral, and then all products were identified by liquid chromatography-mass spectrometry, and the yield of FDCA was 77%.

[0049] The final yield of FDCA from the two-step reaction was 73.2%.

[0050] Embodiment 7:

[0051] 205.82 mg (0.1 mmoL, 5 wt% Rh) Rh / C, 44.8 mg (0.4 mmoL) potassium tert-butoxide and 98.6 mg (0.2 mmoL) IPr·HCl were added to a flask containing toluene, stirred at 50°C overnight under N2 atmosphere, and then the solid and solution were taken out, centrifuged at 2500 rpm for 30 min, and the solid was washed with toluene, ethanol, and acetone and dried to obtain the Rh / IPr metal catalyst; 126.11 mg (1 mmoL) HMF and 15 mg Rh / IPr metal catalyst were added to the autoclave, and flushed with CO2 5 times to remove the air in the autoclave. The autoclave was heated for a period of time to stabilize to the required temperature of 150°C, and then CO2 was charged into the autoclave using a high-pressure liquid pump, and then compressed to 4 MPa, and the reaction was continued for 4 hours, and the contents of the autoclave were stirred with a magnetic stirring bar. After the reaction, the autoclave was cooled with an ice bath, and then the solid catalyst was separated from the liquid product by filtration to obtain 118 mg of DFF with a yield of 95%. 111.7 mg (0.9 mmoL) of DFF, 77 mg (0.225 mmoL) of SIMes·HCl and 50.5 mg (0.45 mmoL) of potassium tert-butoxide were dissolved in THF, and reacted in a CO2 atmosphere at normal pressure and room temperature of 25°C for 2 h. After the reaction was completed, a hydrochloric acid solution (1 N) was added to quench the reaction until the solution was neutral, and then all products were identified by liquid chromatography-mass spectrometry, and the yield of FDCA was 82%.

[0052] The final yield of FDCA from the two-step reaction was 77.9%.

[0053] Comparative Example 1:

[0054] 126.11 mg (1 mmoL) of HMF and 15 mg of Rh / C metal catalyst were added to the autoclave, and the air in the autoclave was removed by flushing with CO2 5 times. The autoclave was heated for a period of time to stabilize to the required temperature of 150°C, and then CO2 was charged into the autoclave using a high-pressure liquid pump, which was then compressed to 4 MPa. The reaction was continued for 4 h, and the contents of the autoclave were stirred with a magnetic stirring bar. After the reaction, the autoclave was cooled with an ice bath, and then the solid catalyst was separated from the liquid product by filtration to obtain 89.3 mg DFF with a yield of 72%. 74.4 mg (0.6 mmoL) DFF, 51 mg (0.15 mmoL) IMes·HCl and 33.6 mg (0.3 mmoL) potassium tert-butoxide were dissolved in THF, and reacted in a CO2 atmosphere at normal pressure and room temperature of 25°C for 2 h. After the reaction was completed, a hydrochloric acid solution (1 N) was added to quench the reaction until the solution was neutral, and then all products were identified by liquid chromatography-mass spectrometry, and the yield of FDCA was 86%.

[0055] The final yield of FDCA obtained by the two-step reaction was 61.9%.

[0056] The present invention provides a thought and method. There are many methods and ways to implement the technical solution. The above is only the preferred implementation of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the protection scope of the present invention. All components not specified in this embodiment can be implemented by existing technologies.

Claims

1. A method for synthesizing FDCA by oxidation of carbon dioxide and metal-catalyzed HMF, characterized in that: The following steps are involved: (1) Using HMF as a raw material, reacting under the conditions of an NHC coordinated metal catalyst and CO2 to obtain DFF; the preparation method of the NHC coordinated metal catalyst comprises the following steps: The metal catalyst, NHC and alkali are dissolved in a solvent, heated under an inert atmosphere, stirred for reaction, and a solid is separated to obtain the NHC coordinated metal catalyst; the metal catalyst is selected from Rh / C, and the NHC is selected from any one of IMes·HCl, IPr·HCl, SIMes·HCl and SIPr·HCl; (2) DFF, ligand NHC and base are dissolved in a solvent and reacted under a CO2 atmosphere to obtain the compound FDCA.

2. The method for synthesizing FDCA by oxidation of carbon dioxide and metal-catalyzed HMF according to claim 1, characterized in that: In step (1), the mass ratio of the NHC coordinated metal catalyst to HMF is (0.05-0.15):

1.

3. The method for synthesizing FDCA by oxidation of carbon dioxide and metal-catalyzed HMF according to claim 1, characterized in that: In step (1), the base is one of potassium tert-butoxide or sodium tert-butoxide; and the solvent is one of toluene and THF.

4. The method for synthesizing FDCA by oxidation of carbon dioxide and metal-catalyzed HMF according to claim 1, characterized in that: In step (1), in the preparation method of the NHC coordinated metal catalyst, the molar ratio of the metal catalyst: NHC: base is 1: (1-3): (2-6); the reaction temperature is 40-70° C.; after the reaction, the solid is washed with ethanol and acetone and then dried to obtain the NHC coordinated metal catalyst.

5. The method for synthesizing FDCA by oxidation of carbon dioxide and metal-catalyzed HMF according to claim 1, characterized in that: In step (1), HMF is used as a raw material and reacted under the conditions of NHC coordinated metal catalyst and CO2, wherein the reaction pressure is 0.1MPa-4MPa, the reaction time is 4-18h, and the temperature is 130-150°C.

6. The method for synthesizing FDCA by oxidation of carbon dioxide and metal-catalyzed HMF according to claim 1, characterized in that: In step (2), the NHC is selected from any one of IMes·HCl, IPr·HCl, SIMes·HCl and SIPr·HCl; the base is any one of potassium tert-butoxide, sodium tert-butoxide or DBU; and the solvent is any one of toluene, THF or acetonitrile.

7. The method for synthesizing FDCA by oxidation of carbon dioxide and metal-catalyzed HMF according to claim 1, characterized in that: In step (2), the molar ratio of the ligand NHC:base:DFF is (0.1-0.3):(0.15-0.6):

1.

8. The method for synthesizing FDCA by oxidation of carbon dioxide and metal-catalyzed HMF according to claim 1, characterized in that: In step (2), the reaction temperature is 25±5°C, the reaction time is 1-3h, and the reaction pressure is normal pressure.

Citation Information

Patent Citations

  • Preparation method for furan-2,5-dicarbaldehyde

    CN102731448A

  • A furan-2,5-dicarboxylic acid purge process

    CN109476623A