Method for producing oil-repellent treated mechanical parts
By locally depositing an oil-proof base film on mechanical parts, the immersion bath and concentration reduction problems of the immersion method in the existing technology are solved, precise oil-proof effects and aesthetics are achieved, and the operating performance and production efficiency of the parts are improved.
Patent Information
- Application Number
- CN202080069279.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-10-02
- Filing Date
- 2020-10-01
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2040-10-01
AI Technical Summary
In the existing technology, when manufacturing mechanical parts, the oil-proof base film deposited by the immersion method has problems such as immersing a large number of parts in the bath, reducing the concentration, high technical risks, low volatility of environmentally friendly solvents, and aesthetic problems. Moreover, the deposition is inaccurate and difficult to localize and save. contact area.
The collimated or localized beam of the oil-proof base film material is deposited on the substrate in the form of projection. Combined with AJP technology, through atomization, projection, and curing steps, heat treatment, photo-cross-linking, chemical cross-linking and other methods are used to achieve precise Protects against oil-based film deposition and localization.
It achieves precise deposition of oil-proof base film on mechanical parts, restricts lubricants to target areas, ensures perfect operation of parts, improves oil-proof effect and aesthetics, and reduces production costs and technical risks.
Smart Images

Figure CN114631065B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for manufacturing a mechanical component treated to be oil-proof.
[0002] The invention also relates to a mechanical part treated to be oil-repellent obtained according to this manufacturing method. The mechanical part comprises a substrate on which is deposited a layer of an oil-repellent base film, such as a watch part, typically a bridge, anchor, wheel, balance or axle. Background Art
[0003] In the field of mechanical parts in frictional contact and in relative displacement, such as in the field of watchmaking, the correct functioning of the mechanical parts depends in particular on their lubrication. The main function of the lubricants used is to separate the contacting surfaces in relative displacement while reducing energy dissipation and wear.
[0004] The lubricants used are mainly divided into two categories: fluid lubricants and lubricants using a lubricating action called solid lubrication of the mechanism. Solid lubricants usually have a layered structure and are less used in the watchmaking field than fluid lubricants because they themselves generate debris. Therefore, the disadvantage of such solid lubricants is that they cause mechanical wear over a more or less long period of time. However, this unpredictable wear is very detrimental to the reliability of the watch movement.
[0005] Fluid lubricants are usually in the form of more or less viscous greases or oils. They have the advantage that they are easier and faster to apply than solid lubricants. In addition, the amount of lubricant used is also more easily controllable. The physical properties of oil (viscosity, wettability, etc.) allow lubrication of multiple functional areas of a mechanism, regardless of the complexity of the mechanism. The energy generated by heating is mainly consumed by the oil. Usually, the oil film is formed again even after rupture, and the amount used is small. The fluid must remain confined to the functional area as much as possible, but the fluid naturally tends to spread. The durability of the lubricant therefore depends on the degree of its retention in the operating area: however, any watchmaker has observed that a drop of lubricant spreads quickly on a clean component. If this property proves to be beneficial, because all the sensitive areas of the mechanism are effectively covered, it may also prove to be detrimental to the correct operation of the component. In fact, the loss of oil in critical areas (usually the contact areas and relative displacement areas (functional areas) of the components), aggravated by the potential degradation of critical areas under severe operating conditions, can lead to irreversible damage. Furthermore, the lubricant may get into undesired locations and cause sticking problems (or more generally, aesthetic problems).
[0006] The spreading of a fluid lubricant, whether in the form of oil or grease, therefore presents a major problem for the operation of a timepiece mechanism. In the case of grease, in fact, a delamination phenomenon is very often observed between soap and base oil. The base oil will therefore be able to displace onto the surface of the component and away from the functional area, which leads to the above-mentioned problems for a fluid lubricant in the form of oil. In general, a fluid lubricant remains in place when its surface tension is higher than the surface tension of the carrier on which it is deposited. If the surface tension of the lubricant is too low, the oil will spread and will not remain in place.
[0007] To overcome this problem, watchmakers deposit a coating called an oleophobic film on their components. This oleophobic film, which usually comes in the form of an invisible layer of oleophobic molecules, is a product that reduces the apparent surface tension of the carrier. It should be noted that the surface tension given by the oleophobic film is of the order of 20 to 30 mN / m, while the surface tension of watch oil is usually 35 mN / m. This difference of 5 to 15 mN / m gives a water drop shape with an angle of attachment that is acceptable to watchmakers. It is usually of the order of 25 to 60. This allows the lubricant to be kept in the desired area. Larger angles would lead to undesirable displacements (for example, the lubricant ball rolling on the surface, like water on the new Gore-Tex TM as above).
[0008] This oil-repellent film can be deposited in many ways, but the main known methods for this purpose consist of immersing the mechanical part to be treated with oil-repellent in a solution consisting of a solvent and a certain amount of molecules that will be deposited on the surface of the part to change its surface tension. The solvent is then evaporated in a next step, leaving only the deposited molecular layer. The oil-repellent film thus covers the entire surface of the part. At the first moments of operation and in the friction zone, the oil-repellent film is removed due to wear, leaving a surface that can be wetted by the lubricant. Some critical mechanisms (such as the escapement) can be operated for the shortest duration to allow this wear of the oil-repellent film to occur. Once this operation is completed, a new lubrication is performed. The lubricant will then wet the surface that has been worn exactly at the friction point.
[0009] However, one of the main disadvantages of this deposition method by immersion is related to the fact that a large number of parts need to be immersed in a bath in which the concentration of the "active" molecules decreases, which makes it mandatory to monitor the process regularly and leads to possible technical risks (i.e. too low a concentration) and therefore too low an oil-repellent effect. In addition, the oil-repellent treatment solvents based on fluorinated compounds implemented by this method often violate existing standards, especially those aimed at combating greenhouse gas emissions. Finally, this method provides, in particular, too high a concentration of "active" molecules or more environmentally friendly but less volatile solvents, which may cause stains during the oil-repellent treatment operation. However, they can be located far away from the functional area and therefore do not require oil-repellent treatment.
[0010] Furthermore, this method may lead to aesthetic problems of the part due to poor solvent evaporation and / or lack of concentration in the oil-repellent base film. More generally, this deposition method by bulk immersion is relatively imprecise, as it is not localized and does not conserve contact area. Summary of the invention
[0011] The object of the present invention is therefore to provide a method for producing oil-repellent treated mechanical components which allows local deposition of an oil-repellent based film on the component in order to define precisely limited areas of lubricant in a simple and inexpensive manner.
[0012] To this end, the invention relates to a method for producing an oil-repellent treated mechanical component, the method comprising the features mentioned in the independent claim 1 .
[0013] Particular embodiments of the method are defined in dependent claims 2 to 17 .
[0014] Thanks to the step of depositing at least one collimated or localized beam of material containing the oil-proof base film product on the substrate in the form of a projection, the method according to the invention allows the oil-proof base film to be deposited very accurately on the component (in terms of the volume and position of the deposited fluid). It can therefore be understood that, unlike the methods of the prior art, a fine oil-proof base film cordon is deposited locally on the component, which allows the lubricant to be confined to the area defined by the deposited cordon. The surface thus defined is then perfectly wetted by the lubricant, ensuring the perfect operation of the component as long as the defined area corresponds to at least one target functional area. It should be noted that in the context of the present invention, the deposited oil-proof base film product can be an oil-proof base film product that causes the retention (accroche) or repulsion (répulsion) of the lubricant by a physical effect, a chemical effect or a combination of these two effects.
[0015] Advantageously, the deposition step comprises an atomization phase for atomizing an ink containing an oil-repellent base film product in the form of a solution or a particle suspension, and a projection phase for projecting the atomized ink onto the substrate of the component; and the treatment step for treating the second material comprises a curing phase for curing the second material. This method corresponds to the method known as AJP (for "Aerosol Jet Printing" in English). It should be noted that, in an alternative, some inks do not require a curing step, for example by crosslinking in the strict sense. A brief exposure to air is sufficient for the solvent to evaporate and for the resin to crosslink "completely on its own". This method offers a very wide variety in the choice of possible materials for depositing the oil-repellent base film product and allows very precise deposition, in particular deposition at the micrometric level on flat but also flexible and / or three-dimensional components.
[0016] According to a particular technical feature of the invention, the curing stage comprises a heat treatment comprising at least an annealing step and / or a localized sintering step and / or a vacuum step. This allows the solidification process to be accelerated. In the case of an oil-proof base film product comprising an active ingredient in solid and powder form, this heat treatment further allows the material to be melted to ensure cohesion between the granules.
[0017] According to another particular technical feature of the invention, the localized sintering step is obtained by irradiating said second material with the aid of a laser.
[0018] According to another particular technical feature of the invention, the curing stage comprises polymerization by photocrosslinking and / or by chemical crosslinking.
[0019] According to another particular technical feature of the invention, the polymerization stage by photocrosslinking is obtained by projecting ultraviolet rays at a predetermined wavelength onto the material comprising the oil-repellent base film product.
[0020] According to another particular technical feature of the present invention, the treatment step for treating the second material comprises at least one of the following stages:
[0021] - stages for modifying the chemical structure of the materials comprising the oil-repellent film product, in particular ion implantation stages;
[0022] - a stage for modifying the crystal structure of the material comprising the oil-repellent base film product, in particular a localized laser heat treatment stage; and / or
[0023] - Stages for modifying the roughness of materials comprising oil-repellent based film products, in particular laser treatment stages.
[0024] According to one embodiment of the invention, the deposition of the oil-repellent film product is carried out in the form of projecting a localized band of material comprising the oil-repellent film product on the substrate, said band being a continuous or discontinuous band.
[0025] Advantageously, the width of the localised strip of material is at least 10 μm, preferably at least 15 μm.
[0026] According to another embodiment of the present invention, the deposition of the oil-proof base film product is carried out in the form of projecting two collimated or localized beams of liquid materials onto a substrate, at least one of the liquid materials containing the oil-proof base film product, and the two liquid materials projected by the beams are selected so as to cause solidification when in contact with each other.
[0027] According to a first variant embodiment of the invention, during the deposition step, at least one collimated or localized beam of material containing the oil-proof base film product is projected onto the substrate by means of at least one fixed projection nozzle, the projection nozzle or each projection nozzle being configured to project a collimated or localized beam of material substantially vertically from top to bottom; the orientation and / or position of the substrate in space is changed during the deposition step. This structure enables vertical projection of material from top to bottom, improving the accuracy of the deposition of the oil-proof base film product, which allows to ensure that the deposition is carried out at the desired precise position on the component.
[0028] According to a second variant embodiment of the invention, during the deposition step, at least one collimated or localized beam of material containing the oil-proof base film product is projected onto the substrate, for example by means of at least one projection nozzle mounted movably relative to the substrate on a multi-axis robot; the substrate remains stationary during the deposition step.
[0029] According to a particular technical feature of the present invention, the second material consists of a single component, in particular a polymer, more particularly an epoxy resin, which is usually a photosetting polymer or a thermosetting polymer.
[0030] Optionally, the second material comprises a plurality of components, each component being generally in liquid or solid form.
[0031] According to the specific technical characteristics of the present invention, each of these ingredients is selected from the group including the following ingredients: surfactant ingredients; solvents; ingredients with physical, chemical or mechanical repellency functions; ingredients with aesthetic functions; ingredients with functions intended to promote crosslinking; or combinations thereof.
[0032] Advantageously, the substrate comprises a surface comprising said oil-proof base film product, said surface comprising:
[0033] - the outer part of a base which constrains the base in all directions, i.e. the outer face of the base, or
[0034] - a part of the outer portion, i.e. a part of the outer surface of the base body.
[0035] To this end, the invention also relates to an oil-repellent treated mechanical component obtained by the above-mentioned manufacturing method and comprising the features mentioned in the dependent claim 17 .
[0036] A special form of the oil-repellent treated machine component is defined in dependent claim 18 .
[0037] According to a particular technical feature of the present invention, the timepiece component is an oil-proof treated mechanical component. BRIEF DESCRIPTION OF THE DRAWINGS
[0038] The objects, advantages and features of the method for manufacturing an oil-repellent treated mechanical component according to the invention will become more apparent in the following description based on at least one non-limiting embodiment illustrated by the accompanying drawings, in which:
[0039] - Figure 1 is a flow chart showing the steps of a method for manufacturing a mechanical component treated with oil repellent according to the present invention;
[0040] - Figure 2 According to the first embodiment of the present invention, Figure 1 A schematic diagram of a system of the method;
[0041] - Figure 3 According to the second embodiment of the present invention Figure 2 similar views to those of the view; and
[0042] - Figure 4 is through Figure 1 Perspective view of a mechanical component treated with oil repellent obtained by the method. DETAILED DESCRIPTION
[0043] Figure 1 The method for manufacturing a mechanical component 2 treated with oil repellent according to the present invention is shown. Figures 2 to 4 The oil-repellent treated mechanical part 2 shown in FIG. 4 comprises a substrate 4. The substrate 4 is a carrier on which the oil-repellent base film product 6 will be deposited. The carrier capable of receiving the oil-repellent base film product comprises a surface of the substrate 4, which is referred to as an oil-repellent treated surface. It can be a surface comprising:
[0044] - the outer part of a base body which constrains the base body in all directions, i.e. the entire outer surface of the base body, or
[0045] - a portion of the outer portion, i.e. a portion of the entire outer surface of the base body.
[0046] It will therefore be understood that the surface is intended to receive or contain the oil-repellent based film product 6 which is intended to reduce the surface tension of the surface, thereby reducing the surface tension of the carrier and thereby the surface tension of the substrate.
[0047] The oil-proofed mechanical part 2 can be a watch part, such as a splint, an anchor, a wheel, a balance wheel or an axle. The part 2 can also be a part of an object that uses mechanical elements or micromechanical elements that are relatively displaced and whose contact points are lubricated by a fluid lubricant that can move and thus change the friction function. Of course, the method for manufacturing such an oil-proofed mechanical part 2 according to the invention can be applied to all applications using oil-proof base films.
[0048] Back to Figure 1 , the method comprises an initial step 10 of depositing an oil-proof base film product 6 on a substrate 4. The substrate 4 is composed of a first material, while the oil-proof base film product 6 is composed of a second material different from the first material. For example, the first material may include metal, ceramic, ruby, sapphire, plastic, diamond, quartz, glass, silicon carbide, amorphous material (metallic glass) or a combination thereof. The second material may be composed of a single component, such as a polymer. The polymer is typically a photocurable or thermosetting polymer, such as an epoxy resin. Optionally, the second material comprises a plurality of components. Each component is, for example, in liquid or solid form. These components may be specifically selected so that their functions are complementary, so as to, for example, promote cross-linking, promote the positioning of the material, provide a function dedicated to lubricant repellency, provide an aesthetic function (such as a function related to color or texture), provide roughness to the deposited material, or transfer one or more useful components to the final function. Therefore, these components may be selected from the group comprising the following components: a surfactant component; a solvent; a component having a physical, chemical or mechanical repellency function; a component having an aesthetic function; or a component having a function intended to promote cross-linking. The component selected as a solvent can facilitate the transfer of one or more other useful components to the final function. For example, by imparting color to the lubricant, the component selected to provide visible coloration to the oil-proof base film product 6 can allow for visual convenience for the operator to operate.
[0049] The method comprises a subsequent treatment step 11 for treating the second material constituting the oil-repellent based film product 6 in order to ensure the cohesion of these components on the substrate 4 of the component 2. These components may be components of the second material.
[0050] The deposition step 10 is performed in such a way that at least one collimated or localized beam 12, 12A, 12B of the material comprising the oil-repellent based film product 6 is projected onto the substrate 4. Figure 2In the first embodiment of the invention shown, deposition is performed in the following manner: a single beam 12 containing an oil-proof base film product 6 is projected onto a substrate 4. For example, the beam 12 is configured to project a continuous and localized band 14 of material containing an oil-proof base film product 6 onto the substrate 4. The width of the continuous band 14 is typically at least 10 μm, preferably at least 15 μm. It should be noted that the maximum width of the band depends on the geometry of the component and the desired aesthetics. In extreme cases, it is therefore possible to completely cover the component except for a separate functional area. In a variant not shown, the beam 12 is configured to project a discontinuous and localized band of material containing an oil-proof base film product onto the substrate 4, for example in the form of a discontinuous series of patterns (such as dots or lines).
[0051] Note that if it is desired that the band be closed, then the band must be closed. As an example, the beam 12 is configured to project a closed band of material containing an oil-proof base film product onto the substrate 4, on which a travel path is described, and the lubricant will move in a controlled manner. This allows the lubricant to be deposited in an easily accessible area, from which the lubricant moves to a less accessible target functional area.
[0052] According to the second embodiment of the present invention, Figure 3 As shown, deposition is performed in the following manner: two collimated or localized beams 12A, 12B of liquid materials are projected onto the substrate 4. At least one of the liquid materials contains an oil-proof base film product 6. Figure 3 In a particular embodiment, only the liquid material projected by the first nozzle 16A contains the oil-proof base film product 6. The two liquid materials projected by the beams 12A, 12B are selected so as to cause solidification when they come into contact with each other. This is the two-component adhesive Araldite TM The principle of the polymer is that it consists of epoxy resin and polymerizing agent 1,4,7,10-tetraazadecane. When these two components come into contact, polyepoxide is formed.
[0053] Preferably, if Figure 2 and Figure 3 As shown in the two embodiments of the present invention, at least one collimated or localized beam 12, 12A, 12B of material containing the oil-proof base film product 6 is projected onto the substrate 4 by means of at least one fixed projection nozzle 16, 16A, 16B. For this purpose, a system 18 is used, which, in addition to one or more nozzles 16, 16A, 16B, also includes control means 20 for controlling the jets projected by said nozzles. The mechanical part 2 on which the oil-proof base film product 6 is deposited is arranged below the nozzle or each nozzle 16, 16A, 16B, vertically below said nozzle. Figure 2 In the first embodiment shown, the system 18 includes a single fixed projection nozzle 16. Figure 3In the second embodiment shown, the system 18 includes two fixed projection nozzles 16A, 16B, each nozzle 16A, 16B projects one of the collimated or localized beams 12A, 12B of the liquid material. In both cases, the fixed projection nozzle or each fixed projection nozzle 16, 16A, 16B is configured to project the corresponding material beams 12, 12A, 12B substantially vertically from top to bottom. During the deposition step 10, the orientation and / or position of the mechanical part 2 in space, and therefore the orientation and / or position of the substrate 4 on which the oil-proof base film product 6 is deposited in space are changed. For this purpose, for example, the system 18 includes a multi-axis positioning device 22 for multi-axis positioning of the part 2, which is connected to the control device 20. This allows the orientation and / or position of the mechanical part 2 in space to be accurately adjusted via the control device 20. This configuration improves the accuracy of the deposition of the oil-proof base film product 6, which allows to ensure that the deposition is implemented at the desired precise position on the mechanical part 2.
[0054] In a variant not shown, a multi-axis positioning device 22 is used to give mobility in space to the or each projection nozzle. The mechanical part 2 and therefore the substrate 4 on which the oil-proof base film product 6 is deposited are then kept immobile during the deposition step 10 by any known means. For example, the positioning device is a multi-axis robot that allows the orientation and / or position of the or each nozzle in space to be changed according to the three dimensions of space, and then the or each nozzle is moved around the part 2.
[0055] Preferably, and although this is not limiting in the context of the present invention, the deposition step 10 comprises an atomization phase 24 for atomizing an ink containing an oil-proof base film product 6 in the form of a solution or a particle suspension, and a projection phase 26 for projecting the atomized ink onto the substrate 4 of the component 2. In this case, the or each projection nozzle 16, 16A, 16B is connected to an atomization chamber, which is not shown in the figure for the sake of clarity. Then, the atomization phase 24 takes place in the atomization chamber, and the projection phase 26 is performed by one or more nozzles 16, 16A, 16B, which are controlled by the control device 20 if necessary. These particles are generally micron, submicron or nanoparticles, which have an active function of the type of active function described in detail above. Of course, other variant embodiments of the deposition step 10 are possible without departing from the scope of the present invention. It should be noted that the deposition step described here is based on the AJP (abbreviation for "Aerosol Jet Printing", "Aerosol Jet Printing") technology. However, the material may also be deposited by other techniques such as digital printing, droplet jetting that forms a band close together, etc. Therefore, it should be understood that the deposition step is not limited to the AJP technique.
[0056] When the deposition step 10 comprises an atomization phase 24 for atomizing the ink and a projection phase 26 for projecting the atomized ink onto the substrate 4, the treatment step 11 preferably comprises a curing phase 28 for curing the second material, when the ink requires it. "Curing" refers to the process of direct or indirect bonding of the particles to obtain their cohesion. It should be noted that some inks do not require a curing step, for example by crosslinking in the strict sense. A brief exposure to air is sufficient to allow the solvent to evaporate and the resin to crosslink "completely by itself".
[0057] For example, the curing stage 28 includes a heat treatment of the second material, which includes at least an annealing step and / or a localized sintering step and / or a vacuum step. This is especially true when the second material consists of a thermosetting polymer. It should be noted that the annealing step can also be referred to as a heating step, for example, for heating the second material based on the application of microwave energy. This heat treatment allows the solidification process to be accelerated. Localized sintering is performed, for example, by irradiating the second material with the aid of a laser (e.g., an infrared laser). Typically, in the case where the particles are suspended in a volatile solvent, before the strict heat treatment, this natural curing stage can further include a natural drying step.
[0058] Alternatively, the curing stage 28 may include artificial curing obtained via polymerization by photocrosslinking and / or by chemical crosslinking. This is particularly true when the second material consists of a photocurable polymer. Polymerization by photocrosslinking is usually obtained by projecting ultraviolet rays at a predetermined wavelength onto the material comprising the oil-proof base film product 6.
[0059] Further alternatively, and more generally, the processing step 11 for processing the second material comprises at least one of the following stages:
[0060] - a stage for modifying the chemical structure of the material comprising the oil-repellent film product 6 , in particular an ion implantation stage;
[0061] - a stage for modifying the crystal structure of the material comprising the oil-repellent based film product 6, in particular a localized laser heat treatment stage; and / or
[0062] - a stage for modifying the roughness of the material comprising the oil-repellent based film product 6, in particular a laser treatment stage.
Claims
1. A method for manufacturing a mechanical component (2), the mechanical component comprising a substrate (4) made of a first material, the substrate being able to comprise an oil-proof base film product (6), the oil-proof base film product (6) reducing the surface tension of the substrate, the method comprising at least include: - a step (10) of depositing the oil-proof film product (6) composed of a second material on the substrate (4), the deposition being carried out in the form of projecting at least one collimated or localized beam (12; 12A, 12B) of the material containing the oil-proof film product (6) onto the substrate (4), the deposition step comprising: projecting two collimated or localized beams (12A, 12B) of liquid materials onto the substrate (4) by means of two fixed projection nozzles, at least one of the liquid materials comprising the oil-proof base film product (6), the two liquid materials projected by the beams (12A, 12B) being selected so as to cause solidification when in contact with each other; the orientation and / or position of the substrate (4) in space being changed during the deposition step (10); or projecting at least one collimated or localized beam (12; 12A, 12B) of material comprising the oil-proof base film product (6) onto the substrate (4) by means of at least one fixed projection nozzle (16; 16A, 16B), wherein each projection nozzle (16; 16A, 16B) is configured to project a collimated or localized beam (12; 12A, 12B) of material vertically from top to bottom, the orientation and / or position of the substrate (4) in space being changed during the deposition step (10); and - a step (11) of treating the second material so as to ensure the cohesion of the several components on the substrate (4), said step (11) comprising a curing phase (28) of curing the second material, said curing phase comprising a localized sintering step or a polymerization by photocrosslinking and / or by chemical crosslinking, said localized sintering step being obtained by irradiating the second material with the aid of a laser; The deposition of the oil-proof film product (6) is carried out in the form of projecting a localized band (14) of the material containing the oil-proof film product (6) onto the substrate (4), the band (14) being a continuous or discontinuous band.
2. The manufacturing method according to claim 1, It is characterized in that The deposition step (10) comprises a phase (24) of atomizing ink containing the oil-proof base film product (6) in the form of a solution or a particle suspension, and a phase (26) of projecting the atomized ink onto the substrate (4) of the component (2); and the step (11) of treating the second material comprises the curing phase (28) of curing the second material.
3. The manufacturing method according to claim 1 or 2, It is characterized in that The solidification phase (28) comprises a thermal treatment including the localized sintering step.
4. The manufacturing method according to claim 1 or 2, It is characterized in that The polymerization stage by photo-crosslinking is obtained by projecting ultraviolet rays at a predetermined wavelength onto the material comprising the oil-proof base film product (6).
5. The manufacturing method according to claim 1 or 2, It is characterized in that The step (11) of treating the second material comprises at least one of the following stages: - a stage for modifying the chemical structure of said material comprising said oil-repellent based film product (6); - a stage for modifying the crystal structure of the material comprising the oil-repellent based film product (6); - a stage for varying the roughness of said material comprising said oil-repellent based film product (6).
6. The manufacturing method according to claim 1, It is characterized in that The localized band (14) of material has a width of at least 10 μm.
7. The manufacturing method according to claim 1 or 2, It is characterized in that During the deposition step (10), at least one collimated or localized beam (12; 12A, 12B) of material comprising the oil-proof base film product (6) is projected onto the substrate (4) by means of at least one projection nozzle mounted movably relative to the substrate (4); the substrate (4) remains stationary during the deposition step (10).
8. The manufacturing method according to claim 1 or 2, It is characterized in that The second material consists of a single component.
9. The manufacturing method according to claim 1 or 2, It is characterized in that The second material includes a plurality of components.
10. The manufacturing method according to claim 9, It is characterized in that Each of the ingredients is in liquid or solid form.
11. The manufacturing method according to claim 9, It is characterized in that Each of the ingredients is selected from the group consisting of: a surfactant ingredient; a solvent; an ingredient having a physical, chemical or mechanical repelling function; an ingredient having an aesthetic function; an ingredient having a function intended to promote cross-linking; or a combination thereof.
12. The manufacturing method according to claim 1 or 2, It is characterized in that The substrate includes a so-called oil-repellent treated surface, the surface comprising the oil-repellent base film product, the surface comprising: - an outer part of the base body which limits the base body in all directions, ie the entire outer face of the base body, or - a part of the outer portion, ie a part of the entire outer surface of the basic body.
13. The manufacturing method according to claim 5, It is characterized in that The step (11) of treating the second material comprises at least one of the following stages: -Ion implantation stage; - Localized laser heat treatment stage; -Laser processing stage.
14. The manufacturing method according to claim 8, It is characterized in that The second material consists of a polymer.
15. The manufacturing method according to claim 8, It is characterized in that The second material consists of epoxy resin.
16. The manufacturing method according to claim 6, It is characterized in that The width of said localised band (14) of material is at least 15 μm.
17. The manufacturing method according to claim 7, It is characterized in that During the deposition step (10), at least one collimated or localized beam (12; 12A, 12B) of material comprising the oil-proof base film product (6) is projected onto the substrate (4) by means of at least one projection nozzle mounted movably relative to the substrate (4) on a multi-axis robot.
18. An oil-proof treated mechanical component (2) obtained by the manufacturing method according to any one of claims 1 to 17.
19. The machine component (2) according to claim 18, It is characterized in that The mechanical component (2) treated with oil repellent is a watch component.