Defect classification and location based on Lamb wave pulse inversion and improved total focusing method

Through Lamb wave pulse inversion and improved full focus method, the second harmonic signal is extracted and combined with the improved full focus algorithm, the problem of low microcrack positioning accuracy in the existing technology is solved, and the microcracks and round holes in the plate are realized. Accurate classification and positioning improves detection accuracy and stability.

CN114705755BActive Publication Date: 2024-11-26NANJING TECH UNIV
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202210276424.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-03-21
Publication Date
2024-11-26
Estimated Expiration
2042-03-21

AI Technical Summary

Technical Problem

The existing in-plate damage imaging algorithm based on linear Lamb wave has low positioning accuracy for microcrack imaging, and it is impossible to achieve classified positioning of defects.

Method used

The Lamb wave pulse inversion and improved full focus method is adopted to extract the second harmonic signal, combine the improved full focus algorithm to realize the classification and positioning of microcracks and circular holes, and fuse the prediction results to improve detection accuracy.

Benefits of technology

The accuracy and accuracy of focusing imaging of different damages in the plate are improved, and effective classification and positioning of microcracks and round hole defects are realized. The method is stable for various operating and environmental conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114705755B_ABST
    Figure CN114705755B_ABST
Patent Text Reader

Abstract

The present invention realizes the classification and positioning of defects in the plate based on Lamb wave pulse inversion and improved full focusing method. The method includes the steps of extracting second harmonic by pulse inversion method, positioning microcracks by improved full focusing algorithm based on second harmonic, positioning circular holes by improved full focusing algorithm based on fundamental frequency, and fusion of defect prediction results. The method obtains the baseline signal and damage signal in the plate through the sensor array and pulse inversion method set on the plate, and then obtains the second harmonic signal; then, based on the traditional full focusing imaging algorithm, an improved full focusing imaging algorithm is proposed by using the speed difference of different echo signals, and the classification and positioning of microcracks and circular hole defects in different areas of the plate are realized. Finally, the two types of defect positioning results are fused to obtain the final defect classification and positioning result. The method of the present invention has high precision and accuracy in focusing imaging of different damages in the plate, and is stable under various operating and environmental conditions.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to defect classification and positioning based on Lamb wave pulse inversion and improved total focusing method, and belongs to the technical field of nondestructive testing. Background Art

[0002] Whether in the shipbuilding industry, aerospace, large pressure vessels, oil pipelines, bridge construction and other engineering fields, or in various utensils that can be seen everywhere in daily life, plate-like structural materials are widely used and are an important part of the prosperity and development of social economy. However, in the process of design, production and manufacturing of plate-like components, problems such as process and equipment will inevitably affect the uniformity of components, resulting in various defects such as delamination and cracks. In addition, in long-term engineering applications, due to the influence of various factors such as external force impact, high-pressure vibration, chemical corrosion, thermal fatigue, etc., it is very easy to cause changes in the structure, resulting in defects, cracks, through holes and other damages. These damages are located inside the structure, are highly concealed, and are very harmful. If they are not discovered and resolved in time, unexpected losses are likely to occur, and even serious engineering accidents may occur.

[0003] Regular and periodic damage inspection of plate-like components in use can timely discover and eliminate various minor hidden dangers, make comprehensive and effective protective measures as early as possible, and prevent and avoid accidents as much as possible. Structural health monitoring technology and non-destructive testing technology were born and developed in such an engineering background, and are the focus of research in the current field. In the field of non-destructive testing, ultrasound has the advantages of strong penetration, high sensitivity, no pollution and no harm to the human body. It is the most widely used. The ultrasonic detection method mainly uses body waves and guided waves to achieve detection. The ultrasonic wave propagating in the plate-like structure with a small thickness is called Lamb wave. Compared with traditional ultrasonic guided waves, Lamb waves have the characteristics of small propagation energy attenuation, long propagation distance, and can simultaneously detect the surface and internal health of the plate. Therefore, it is widely used in damage detection of plate structures and shell structures, and has great development and application potential.

[0004] Among the existing methods for locating and imaging damage in plates based on Lamb waves, most methods use the calculation of wave arrival time, wave arrival direction or probability imaging based on damage coefficient. These methods are based on the positioning and imaging algorithm of linear Lamb waves. When microcracks and linear damage coexist, it is often difficult to distinguish the type of damage. Moreover, since they are not sensitive to microcracks, microcracks are easily ignored in the imaging results. In the prior art, there is a method that uses pulse inversion to extract the second harmonic to achieve selective imaging of fatigue cracks. On this basis, the nonlinear effect of Lamb waves propagating through the microcrack area when microcracks and circular hole damage coexist can be used to distinguish and locate the two different types of damage, microcracks and circular holes in the plate. Compared with the traditional linear imaging algorithm, it can not only provide more accurate position predictions, but also effectively identify the types of damage in different regions. Summary of the invention

[0005] Technical problem to be solved by the invention

[0006] In order to solve the shortcomings of the existing plate damage imaging algorithm based on linear Lamb wave, such as low accuracy in microcrack imaging and positioning, and inability to classify and locate defects, the present invention realizes the classification and positioning of defects in the plate based on Lamb wave pulse inversion and improved full focusing method.

[0007] Technical Solution

[0008] In order to achieve the above object, the technical solution provided by the present invention is:

[0009] Defect classification and positioning based on Lamb wave pulse inversion and improved total focusing method, characterized by including the steps of extracting second harmonic by pulse inversion method, locating microcracks by improved total focusing algorithm based on second harmonic, locating circular holes by improved total focusing algorithm based on fundamental frequency, and fusing defect prediction results, wherein the second harmonic extraction by pulse inversion method includes the following steps:

[0010] Step 1, obtain the Lamb wave dispersion curve, select the appropriate mode as the excitation signal and modulate it;

[0011] Step 2, a group of linear sensor arrays are set on the upper surface at the designated position of the lossless plate, which are used as excitations and receive echo signals from the target area in turn, and a movable sensor is set on the lower surface to apply symmetrical excitation. When each sensor on the upper surface is used as an excitation sensor, the positive phase excitation and negative phase excitation signals described in step 1 are symmetrically emitted at the same position on the upper and lower surfaces of the plate at the excitation sensor, and all sensors in the sensor array are used as receiving sensors to obtain response signals, and obtain positive phase baseline signals and negative phase baseline signals;

[0012] Step 3, performing step 2 on the damaged board to obtain a positive phase damage signal and a negative phase damage signal;

[0013] Step 4: Subtract the positive phase damage signal obtained in step 3 from the positive phase baseline signal obtained in step 2 to obtain the positive phase damage scattering signal f s+ , subtract the inverse damage signal obtained in step 3 from the inverse baseline signal obtained in step 2 to obtain the inverse damage scattering signal f s- ;

[0014] Step 5: Superimpose the positive phase damage scattering signal obtained in step 4 with the negative phase damage scattering signal to obtain the second harmonic signal in the response signal, the method is:

[0015]

[0016] where f s+ is the positive phase damage scattering signal, f s- is the anti-phase damage scattering signal, f p is the second harmonic signal;

[0017] The improved total focusing algorithm based on second harmonic for microcrack location includes the following steps:

[0018] Step 6, according to the Lamb wave dispersion curve obtained in step 1, read the fundamental frequency signal and the double frequency signal wave velocity at the excitation frequency from the curve graph;

[0019] Step 7: Consider the sensor on the upper surface of the plane of the board to be tested as an N-element phased array, and consider the transmitting sensor and the receiving sensor as the elements in the phased array. Excite and receive the echo signal of the target area. Let the transmitting element be i, the receiving element be j, S ij That is, it represents the echo signal excited by array element i and received by array element j. The second harmonic signal obtained in step 5 is recorded in the matrix S to obtain echo data of size N×N. The amplitude at any focus point P is defined as

[0020]

[0021]

[0022] where x p ,y p is the coordinate of any focal point P, I p represents the amplitude intensity at the focal point P, t ij It represents the time required for the signal to be excited from the excitation sensor i, pass through the focal point P and finally reach the receiving sensor j. ij (t ij ) represents the receiving response matrix S ij Medium ij The value corresponding to the moment, d ip and d pjThey represent the distance from the excitation sensor i to the focal point P and the distance from the focal point P to the receiving sensor j, respectively. ip and c pj They represent the wave velocity of the fundamental frequency signal from the excitation sensor i to the focus point P and the wave velocity of the second harmonic signal from the focus point P to the receiving sensor j respectively;

[0023] Step 8: According to the I of each focal point P P The imaging map is drawn with the values, the data in the map is normalized, and the maximum amplitude point in the local area of ​​the target area in the imaging map is taken as the microcrack defect location result;

[0024] The improved full focusing algorithm circular hole positioning based on fundamental frequency includes the following steps:

[0025] Step 9: Subtract the second harmonic signal obtained in step 5 from the positive phase damage scattering signal obtained in step 4 to obtain a damage residual signal:

[0026] f r =f s+ -f p ,

[0027] where f s+ is the positive phase damage scattering signal, f p is the second harmonic signal, f r is the obtained residual signal;

[0028] Step 10: The damaged residual signal f obtained in step 9 is r The fundamental frequency component in the response signal is retained by a low-pass filter to obtain a filtered residual signal containing only the fundamental frequency component;

[0029] Step 11: Using the method of step 7, record the damaged residual signal containing only the baseband component obtained in step 10 in the matrix S, and calculate:

[0030]

[0031]

[0032] where c ip and c pj represent the wave speed of the fundamental frequency signal from the excitation sensor i to the focusing point P and from the focusing point P to the receiving sensor j respectively;

[0033] Step 12: According to the I of each focal point P P Draw an imaging diagram with the values, normalize the data in the diagram, exclude the microcrack position obtained in step 8, and take the maximum amplitude point in the local area of ​​the target area in the imaging diagram as the circular hole defect location result;

[0034] The defect prediction result fusion includes the following steps:

[0035] Step 13, integrating the microcrack defect location result obtained in step 8 and the circular hole defect location result obtained in step 12 to obtain the final plate defect location result.

[0036] Furthermore, the method for selecting the excitation signal in step 1 is: according to the dispersion curve, within the range where the second harmonic frequency is less than the cutoff frequency of other modes, select the low-dispersion, fast-speed Lamb wave S 0 The modal signal is used as excitation.

[0037] Furthermore, in step 1, a rectangular window and a Hanning window are used to modulate the Lamb wave excitation signal, and the modulation method is:

[0038]

[0039] Where ε(t) is a step function, f c is the center frequency of the excitation signal, is the phase of the signal, and N is the number of peaks of the modulated sinusoidal signal.

[0040] Furthermore, the method for obtaining the baseline signal and the damage signal in steps 2 and 3 is:

[0041] Two anti-phase signal excitations are launched into the plate to obtain positive and anti-phase response signals:

[0042] Assume the excitation and response of the system is f(t) = a 1 u(t)+a 2 u 2 (t)+a 3 u 3 (t)+…, where u(t) and f(t) are the excitation signal and the corresponding system response, respectively, and a 1 、a 2 、a 3 is the nonlinear coefficient,

[0043] Assume that the positive phase excitation is p(t) and the negative phase excitation is n(t), satisfying n(t) = -p(t). The responses obtained by the two negative phase signal excitations are:

[0044] f + (t) = a 1 p(t)+a 2 p 2 (t)+a 3 p 3 (t)+…

[0045] f - (t) = -a 1 p(t)+a 2 p 2 (t)-a3 p 3 (t)+…

[0046] where f + (t) and is the positive phase response signal, f - (t) is the anti-phase response signal.

[0047] Beneficial Effects

[0048] The method of the present invention proposes an improved full-focus imaging method by utilizing the speed difference of different echo signals on the basis of the traditional full-focus imaging algorithm, thereby improving the precision and accuracy of the focused imaging of different damages in the plate;

[0049] The method of the present invention uses a pulse inversion method to extract the second harmonic from the defect area in the scattering signal and combines it with an improved full-focus imaging method to achieve the classification and positioning of microcracks and circular hole defects in different areas of the plate. The method is stable under various operating and environmental conditions. BRIEF DESCRIPTION OF THE DRAWINGS

[0050] Figure 1 A flowchart of the defect classification and positioning method of the present invention;

[0051] Figure 2 It is a schematic diagram of the all-focusing imaging algorithm of the method of the present invention;

[0052] Figure 3 The excitation signal and its corresponding spectrum diagram used in the method of the present invention;

[0053] Figure 4 It is a simulation model diagram in the method of the present invention;

[0054] Figure 5 A defect area modeling diagram in the method of the present invention;

[0055] Figure 6 This is a comparison of the time domain received signal and its spectrum comparison diagram of the single crack damage method of the present invention;

[0056] Figure 7 The second harmonic extracted from the response signal by the pulse inversion method of the present invention and its corresponding spectrum diagram;

[0057] Figure 8 This is a diagram showing the microcrack damage location results of a single crack model using the method of the present invention;

[0058] Fig. 9 This is a result diagram of damage classification and positioning of a double-crack single circular hole model according to the method of the present invention;

[0059] Fig.10 This is a result diagram of damage classification and positioning of a single crack double circular hole model using the method of the present invention. DETAILED DESCRIPTION

[0060] In order to further understand the content of the present invention, the present invention is described in detail in conjunction with the accompanying drawings and specific implementation methods.

[0061] like Figure 1 As shown, the method of the present invention mainly includes four steps: extracting the second harmonic by pulse inversion method, locating microcracks by improved total focusing algorithm based on second harmonic, locating circular holes by improved total focusing algorithm based on fundamental frequency, and fusing defect prediction results.

[0062] Extraction of Second Harmonic by Pulse Inversion Method

[0063] In this method, a group of linear sensor arrays are first arranged on the upper surface of the aluminum plate, and a transmitting sensor is arranged on the lower surface. In this embodiment, the size of the aluminum plate and the specific position of the upper surface sensor are as follows: Figure 4 As shown (S 1 -S 7 ), after determining the sensor position, the Lamb wave signal is symmetrically incident on the upper and lower surfaces of the aluminum plate through the sensor. The propagation of Lamb wave has dispersion and multi-mode characteristics. According to the dispersion curve, within the range where the double frequency is less than the cutoff frequency of other modes, the Lamb wave S with low dispersion and high speed is selected. 0 The modal signal is used as the excitation; in order to ensure that the appropriate mode is obtained, the center frequency of the excitation signal is selected below the first cutoff frequency in the low-frequency region, so that the Lamb wave has only two basic modes in the composite plate (S 0 and A 0 ) can propagate and no mode transition occurs at the free boundary, and on this basis, the excitation signal is modulated. Rectangular window and Hanning window are usually used to modulate the Lamb wave excitation signal. In this embodiment, Hanning window is used for modulation. For single-frequency excitation, the expression of the excitation signal is as follows:

[0064]

[0065] Where ε(t) is a step function; f c is the center frequency of the excitation signal; is the phase of the signal; N is the number of peaks of the modulated sinusoidal signal. The energy of the modulated signal band is more concentrated, which improves the dispersion of the Lamb wave.

[0066] The positive phase excitation and the reverse phase excitation are applied to the transmitting sensor respectively, and the upper surface sensor is used as the receiving sensor to obtain the response signal. The pulse inversion can filter out the fundamental frequency and odd harmonic components in the response, while the amplitude of the even harmonics will be doubled. Due to the existence of nonlinear damage, the excitation and response of the system can be simplified as follows:

[0067] f(t)=a 1 u(t)+a2 u 2 (t)+a 3 u 3 (t)+… (2)

[0068] Where u(t) and f(t) represent the excitation signal and the corresponding system response, respectively. 1 、a 2 、a 3 is the nonlinear coefficient.

[0069] Assume that the positive phase excitation is p(t) and the negative phase excitation is n(t), satisfying n(t) = -p(t). Then the responses obtained by the two negative phase signal excitations are

[0070]

[0071] where f + (t) and f - (t) represents the positive phase response signal and the negative phase response signal respectively. The two response signals are superimposed to obtain

[0072] f + (t)+f - (t) = 2a 2 p 2 (t)+2a 4 p 4 (t)+… (4)

[0073] After the pulse inversion processing, only the even harmonic components in the response signal are retained, while the fundamental frequency components and odd harmonic components in the original response signal are offset.

[0074] According to the above method, two anti-phase excitations are applied to the intact plate to obtain a positive-phase baseline signal and an anti-phase baseline signal; two anti-phase excitations are applied to the damaged plate to obtain a positive-phase damage signal and an anti-phase damage signal. The positive-phase and anti-phase damage scattering signals can be obtained by subtracting the baseline signal from the damage signal. According to the pulse inversion theory, the pulse inversion result can be obtained by superimposing the two damage scattering signals. The calculation formula for extracting the second harmonic by the pulse inversion method is defined as

[0075]

[0076] where f s+ is the positive phase damage scattering signal, f s- is the anti-phase damage scattering signal, f p is the second harmonic signal.

[0077] After extracting the second harmonic from the Lamb wave response signal using the pulse inversion method, the following will implement classification and positioning for microcracks and circular holes respectively, and finally merge the imaging images of microcracks and circular hole damage to obtain the final classification prediction results.

[0078] Microcrack location based on improved total focusing algorithm based on second harmonic generation

[0079] After extracting the second harmonic related to the microcracks from the response signal, the microcracks can be selectively located by combining it with the improved full focusing method. Figure 2 As shown in the figure, the full focusing algorithm is a data post-processing method based on phased array. It discretizes the target area into grid points, each grid point is used as a virtual focusing point, and the imaging reconstruction is performed using the echo data captured by the full matrix. The amplitude at each point is calculated based on the collected echo data to generate a complete focused image.

[0080] For an N-element phased array, one of the elements is used as the excitation, and all the elements receive the echo signal from the target area. The transmitting element is denoted as i, and the receiving element is denoted as j. The captured time domain signal is recorded in the matrix S, S ij That is, it represents the echo signal excited by array element i and received by array element j, so the echo data of size N×N is obtained. The amplitude I at any focus point P p Defined as

[0081]

[0082]

[0083] Where x p ,y p is the coordinate of any focal point P, I p represents the amplitude intensity at any focal point P, t ij It represents the time required for the sound wave to be excited from the excitation sensor i, pass through the focal point P and finally reach the receiving sensor j. ij (t ij ) represents the receiving response matrix S ij Medium ij The value corresponding to the moment, d ip and d pj They represent the distance from the excitation sensor i to the focal point P and the distance from the focal point P to the receiving sensor j, respectively. ip and c pj They respectively represent the wave velocity of the fundamental frequency signal from the excitation sensor i to the focusing point P and the wave velocity of the second harmonic signal from the focusing point P to the receiving sensor j.

[0084] The excitation signal propagates from the excitation array element to the microcrack at the wave velocity corresponding to the fundamental frequency, and the second harmonic signal is selected for analysis from the microcrack area to the receiving array element. The corresponding wave velocity is the propagation velocity of the second harmonic. The microcrack positioning step first reads the fundamental frequency corresponding to the excitation frequency and the wave velocity corresponding to the second harmonic from the curve according to the Lamb wave dispersion curve; then, the second harmonic extracted based on the pulse inversion method is used to calculate the I of each focus point P using equations (6) and (7). p value; finally, the imaging image is drawn according to the amplitude intensity, the imaging image is normalized, and the maximum amplitude point in the local area of ​​the target area in the imaging image is taken as the microcrack defect positioning result.

[0085] Improved full focusing algorithm for circular hole positioning based on fundamental frequency

[0086] The circular hole positioning step first uses the forward damage scattering signal to subtract the second harmonic signal to obtain the residual signal, as shown in formula (8). The residual signal here contains the fundamental frequency and high-order harmonic components:

[0087] f r =f s+ -f p (8)

[0088] Where f s+ represents the positive phase damage scattering signal, f p represents the second harmonic signal, f r is the obtained residual signal.

[0089] The residual signal is filtered through a low-pass filter to remove the high-order harmonic components, and a filtered residual signal containing only the fundamental frequency is obtained. The defect is imaged using the filtered residual signal containing only the fundamental frequency. The signal propagates from the excitation element to the damage and from the damage to the receiving element at the speed corresponding to the fundamental frequency. Based on equations (6) and (7), I of each focus point P is calculated. p The difference from the microcrack location step is that when the circular hole is located, formula (7) c ip and c pj They represent the wave velocity of the fundamental frequency signal from the excitation sensor i to the focusing point P and from the focusing point P to the receiving sensor j respectively; finally, the imaging diagram is drawn according to the amplitude intensity, the imaging diagram is normalized, and after excluding the microcrack position, the maximum amplitude point in the local area of ​​the target area in the imaging diagram is taken as the circular hole defect positioning result.

[0090] Experimental Results

[0091] Table 1

[0092]

[0093] The sample to be tested in the experiment is an aluminum plate. The specific material performance parameters are shown in Table 1, where ρ represents density, E represents Young's modulus, υ represents Poisson's ratio, and the model size is 600mm×600mm×2mm. In order to reduce the influence of multimodality and dispersion during Lamb wave propagation, anti-phase symmetrical excitation is applied to the upper and lower surfaces of the aluminum plate at the same position to obtain a single S 0 Modal Lamb wave, the excitation signal used in the experiment is a 5-cycle 200kHz Hanning windowed sine wave, its time domain waveform and spectrum are as follows Figure 3 As shown; establish a coordinate system with the center of the aluminum plate as the origin, such as Figure 4 As shown in the figure, a set of seven linear sensor arrays are set on the left and right sides of (0, -50) mm to stimulate and receive signals in turn. The spacing between the sensors is 5 mm, and they are numbered S from left to right. 1 ,S 2 ,……,S 7 A movable transmitting sensor is set on the lower surface to apply symmetrical excitation. Two different defect models are set in the aluminum plate: the microcracks generated in the actual environment are simulated by an elliptical through hole with a major axis length of 3mm and a minor axis length of 1μm. The surface is set to hard contact without friction to produce the CAN effect; circular through holes with diameters of 4mm and 2mm are used to simulate linear scatterers. The area containing these two types of defects is constructed, such as Figure 5 As shown, it is embedded in the designated position of the mainboard, and the specific defect distribution is shown in Table 2. The wave velocity in the improved full-focus imaging algorithm used in this embodiment is the theoretical value in the dispersion curve. According to the Lamb wave dispersion curve, the wave velocities of the 200kHz fundamental frequency and the 400kHz second harmonic in the 2mm thick aluminum plate are approximately 5350m / s and 5230m / s respectively.

[0094] Table 2

[0095]

[0096] The single crack model is used to explore the nonlinear effect of Lamb waves passing through the microcrack area and verify the effectiveness of the pulse inversion method in the present invention to extract the second harmonic and combine it with the improved total focusing algorithm to achieve microcrack location. The microcrack in the model is located at (0,50) mm. For comparative analysis, a circular hole is placed at the same position. Both are compared with the non-destructive case. In the three cases, the S 4 Incentive S 1 The received signal is received and the time domain waveform is plotted on Figure 6 (a). It can be seen from the figure that new and obvious scattered wave packets appear in the lossy plate. The spectrum analysis of the two new scattered wave packets is shown in the following figure. Figure 6As shown in (b), a relatively obvious nonlinear effect appears in the wave packet from the microcrack area, and a large second harmonic signal is generated. However, in the circular hole damaged plate, the scattered wave packet is mainly the fundamental frequency component. Figure 7 (a) shows the time domain superposition results of the forward and reverse phase scattering signals in the single crack model. Figure 7 The corresponding spectrum is plotted in (b). Figure 6 (b) In contrast, the fundamental frequency and triple frequency in the original scattered signal from the microcrack area are eliminated, leaving only the second harmonic component, which verifies the effectiveness of the pulse inversion method in extracting the second harmonic signal. Figure 8 As shown in (a), all data in the figure are normalized to between 0 and 1, and the point with the maximum amplitude in the target area of ​​the image is taken as the position prediction result. Figure 8 (b) shows a comparison between the predicted result and the actual position, where the predicted position is (0,52) mm, which deviates by 2 mm from the actual position (0,50) mm, verifying the effectiveness of the improved total focusing algorithm using second harmonics to locate microcracks in the method of the present invention.

[0097] In the double-crack single-circular-hole model, the two cracks are located at (20,50) mm and (20,-15) mm, and the circular hole is located at (-30,0) mm; while in the single-crack double-circular-hole model, the crack is located at (20,50) mm, and the two circular holes are located at (-30,0) mm and (30,0) mm. Fig. 9 10 and 11 respectively show the classification and positioning effects of two groups of models obtained by using the defect classification and positioning method proposed in the present invention. Fig. 9 There are two highlighted areas in the imaging result of microcracks in (a), which are the two microcrack areas in the model. Fig. 9 (b) is the imaging result obtained by filtering the residual signal, where the only remaining highlight area is the location of the circular hole in the model. The result of the merged imaging is shown in Figure 9(c). The comparison between the classification and positioning prediction results is plotted in Fig. 9 (d) Fig.10 In (a), the microcrack imaging result has only one highlighted area, indicating that there is only one microcrack in this model. Fig.10 (b) is the imaging of the filtered residual signal, which excludes the location of the microcracks. The two local highlighted areas are the locations of the identified circular holes. Fig.10 (c)-(d) show the comparison between the merged imaging results and the predicted results.

[0098] Table 3

[0099]

[0100] The result data of applying this method to the defect classification and location proposed in the present invention for two groups of multi-defect models are summarized in Table 3. The identification results of the types and locations of all defects verify the effectiveness of the defect classification and location method proposed in the present invention.

[0101] The present invention and its embodiments are described schematically above, and the description is not restrictive. The drawings show only one embodiment of the present invention, and the actual structure is not limited thereto. Therefore, if a person skilled in the art is inspired by it and designs a structural method and an embodiment similar to the technical solution without creativity without departing from the purpose of the invention, they shall all fall within the protection scope of the present invention.

Claims

1. Defect classification and location based on Lamb wave pulse inversion and improved total focusing method, characterized by: The method includes the steps of extracting the second harmonic by the pulse inversion method, locating microcracks by the improved total focusing algorithm based on the second harmonic, locating circular holes by the improved total focusing algorithm based on the fundamental frequency, and fusing defect prediction results. The second harmonic extraction by the pulse inversion method includes the following steps: Step S1, obtaining Lamb wave dispersion curve, selecting a suitable mode as an excitation signal and performing modulation; Step S2, a group of linear sensor arrays are arranged on the upper surface at the designated position of the lossless plate, which are sequentially used as excitations and receive echo signals from the target area, and a movable sensor is arranged on the lower surface to apply symmetrical excitations. When each sensor on the upper surface is used as an excitation sensor, the positive phase excitation and negative phase excitation signals of step S1 are symmetrically emitted at the same position on the upper and lower surfaces of the lossless plate where the excitation sensors are arranged, and all sensors in the sensor array are used as receiving sensors and obtain response signals to obtain positive phase baseline signals and negative phase baseline signals; Step S3, executing step S2 on the damaged board to obtain a positive phase damage signal and a negative phase damage signal; Step S4, subtract the positive phase damage signal obtained in step S3 from the positive phase baseline signal obtained in step S2 to obtain the positive phase damage scattering signal f s+ , subtract the inverse phase damage signal obtained in step S3 from the inverse phase baseline signal obtained in step S2 to obtain the inverse phase damage scattering signal f s- ; Step S5, superimposing the positive phase damage scattering signal obtained in step S4 with the reverse phase damage scattering signal to obtain a second harmonic signal in the response signal, the method is as follows: where f s+ is the positive phase damage scattering signal, f s- is the anti-phase damage scattering signal, f p is the second harmonic signal; The microcrack location based on the improved total focusing algorithm of second harmonic includes the following steps: Step S6, reading the fundamental frequency signal and the double frequency signal wave speed at the excitation frequency from the curve graph according to the Lamb wave dispersion curve obtained in step S1; Step S7: regard the sensor on the upper surface of the plane of the plate to be detected as an N-element phased array, regard the transmitting sensor and the receiving sensor as the elements in the phased array, stimulate and receive the echo signal of the target area, and set the transmitting element as i and the receiving element as j. ij That is, the echo signal excited by array element i and received by array element j is recorded in the matrix S in step S5 to obtain echo data of size N×N. The amplitude at any focus point P is defined as: where x p ,y p is the coordinate of any focal point P, I p represents the amplitude intensity at the focal point P, t ij It represents the time required for the signal to be excited from the excitation sensor i, pass through the focal point P and finally reach the receiving sensor j. ij (t ij ) represents the receiving response matrix S ij Medium ij The value corresponding to the moment, d ip and d pj They represent the distance from the excitation sensor i to the focal point P and the distance from the focal point P to the receiving sensor j, respectively. ip and c pj They represent the wave velocity of the fundamental frequency signal from the excitation sensor i to the focus point P and the wave velocity of the second harmonic signal from the focus point P to the receiving sensor j respectively; Step S8: According to the I of each focal point P P The imaging map is drawn with the values, the data in the map is normalized, and the maximum amplitude point in the local area of ​​the target area in the imaging map is taken as the microcrack defect location result; The improved full focusing algorithm circular hole positioning based on fundamental frequency includes the following steps: Step S9, subtract the second harmonic signal obtained in step S5 from the positive phase damage scattering signal obtained in step S4 to obtain a damage residual signal: f r =f s+ -f p , where f s+ is the positive phase damage scattering signal, f p is the second harmonic signal, f r is the obtained residual signal; Step S10: The damaged residual signal f obtained in step S9 is r The fundamental frequency component in the response signal is retained by a low-pass filter to obtain a filtered residual signal containing only the fundamental frequency component; Step S11, using the method of step S7, the damaged residual signal containing only the baseband component obtained in step S10 is recorded in the matrix S, and the following is calculated: where c ip and c pj represent the wave speed of the fundamental frequency signal from the excitation sensor i to the focusing point P and from the focusing point P to the receiving sensor j respectively; Step S12: according to the I of each focal point P P The imaging diagram is drawn with the values, the data in the diagram is normalized, and after excluding the microcrack position obtained in step S8, the maximum amplitude point in the local area of ​​the target area in the imaging diagram is taken as the circular hole defect positioning result; The defect prediction result fusion includes the following steps: Step S13, integrating the microcrack defect location result obtained in step S8 and the circular hole defect location result obtained in step S12 to obtain the final plate defect location result.

2. The defect classification and positioning based on Lamb wave pulse inversion and improved total focusing method according to claim 1, characterized in that: The method for selecting the excitation signal in step S1 is: according to the dispersion curve, within the range where the double frequency is less than the cutoff frequency of other modes, select the low-dispersion, fast-speed Lamb wave S0 mode signal as the excitation.

3. The defect classification and positioning based on Lamb wave pulse inversion and improved total focusing method according to claim 1, characterized in that: The step S1 uses a rectangular window and a Hanning window to modulate the Lamb wave excitation signal, and the modulation method is: Where ε(t) is a step function, f c is the center frequency of the excitation signal, is the phase of the signal, and N is the number of peaks of the modulated sinusoidal signal.

4. The defect classification and positioning based on Lamb wave pulse inversion and improved total focusing method according to claim 1, characterized in that: The method for obtaining the baseline signal and the damage signal in steps S2 and S3 is: Two anti-phase signal excitations are launched into the plate to obtain positive and anti-phase response signals: Assume the excitation and response of the system is f(t)=a1u(t)+a2u 2 (t)+a3u 3 (t)+…, where u(t) and f(t) are the excitation signal and the corresponding system response, respectively, a1, a2, a3 are nonlinear coefficients, Assume that the positive phase excitation is p(t) and the negative phase excitation is n(t), satisfying n(t) = -p(t). The responses obtained by the two negative phase signal excitations are: f + (t)=a1p(t)+a2p 2 (t)+a3p 3 (t)+… f - (t)=-a1p(t)+a2p 2 (t)-a3p 3 (t)+… where f + (t) and is the positive phase response signal, f - (t) is the anti-phase response signal.

Citation Information

Patent Citations

  • Non-linear Lamb wave frequency mixing method for detecting microcrack in plate

    CN105372330A

  • Defect positioning method for condensed laser sensor array based Lamb corrugated plate structure

    CN105527345A

  • Steel plate Lamb wave detection imaging method based on linear array focusing-time reversal

    CN105738478A

  • Nonlinear Lamb wave structure fatigue damage chromatography imaging method based on piezoelectric array

    CN109085244A

  • Method for identifying microcrack direction in plate based on nonlinear frequency mixing technology of Lamb waves

    CN111157629A