Method for preparing chlorine from hydrogen chloride
Through the liquid melt system circulating in three bubbling lift reactors, temperature control is used to react copper ions and chloride ions with oxygen and hydrogen chloride, which solves the problems of melt retention and energy consumption in the existing technology and achieves high efficiency. Chlorine production and improved space-time yield.
Patent Information
- Application Number
- CN202080072253.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-10-18
- Filing Date
- 2020-10-16
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2040-10-16
AI Technical Summary
When the existing technology uses a three-reactor concept, it is difficult to keep the melt in liquid form and recyclable, and there is a problem of high energy consumption, which affects the space-time yield of chlorine.
Using a circulation system including three bubbling lift reactors, the liquid melt of copper ions, alkali cations and chloride ions is contacted with oxygen and hydrogen chloride to form chlorine gas by controlling the temperature in different reactors, avoiding the use of air lift pumps and The pressure difference is required to maintain the melt in liquid form, and the temperature difference is optimized to reduce energy consumption.
Efficient production of chlorine gas is achieved, the space-time yield is improved, and energy consumption is reduced, providing an economical and simple method.
Smart Images

Figure CN114728785B_ABST
Abstract
Description
[0001] The present invention relates to a method for preparing chlorine from hydrogen chloride, which method comprises circulating a catalyst containing copper ions Cu in a reactor system comprising three bubble lift reactors I, II and III. n+ (where n is a value of 1-2), alkali cations and chloride ions Cl - The liquid melt of the first bubbling lift reactor I is made to contain copper ions Cu n+ , alkali cations and chloride ions Cl - The liquid melt is contacted with oxygen (O2) at a temperature of >375°C, so that the molar ratio of Cu in the liquid melt is 2+ :Cu + increases, obtaining Cu with an increased molar ratio 2+ :Cu + (b) circulating the liquid melt obtained in (a) to a reaction zone ii in a second bubbling riser reactor II, wherein the liquid melt is contacted with hydrogen chloride (HCl) at a temperature of >355° C., so that water is formed to obtain a liquid melt rich in chloride anions (Cl) compared to the liquid melt obtained according to (a); - ) a liquid melt obtained in (b); (c) recycling the liquid melt obtained in (b) to a reaction zone iii in a third bubbling riser reactor III, which is operated at a temperature of 400-480° C., so that chlorine (Cl 2 ) is formed, wherein Cl 2 is removed in gaseous form from reaction zone iii and the third bubbling riser reactor III, respectively, leaving a Cl 2-depleted liquid melt compared to the liquid melt obtained according to (b) - of liquid melt.
[0002] The present invention further relates to a reactor system comprising three bubbling riser reactors I, II and III, each bubbling riser reactor comprising reaction zones i, ii and iii; a liquid melt outlet in the top region of each bubbling riser reactor; and a liquid melt inlet in the bottom region of each bubbling riser reactor, wherein the bubbling riser reactors I, II and III are connected by connecting pipelines suitable for liquid melt circulation, so that a) the liquid melt outlet of the first bubbling riser reactor I is connected to the liquid melt inlet of the second bubbling riser reactor II via a connecting pipeline; b) the liquid melt outlet of the second bubbling riser reactor II is connected to the liquid melt inlet of the third bubbling riser reactor III via a connecting pipeline; c) the liquid melt outlet of the third bubbling riser reactor III is connected to the liquid melt inlet of the first bubbling riser reactor I via a connecting pipeline.
[0003] Furthermore, the present invention relates to chlorine obtained or obtainable by the process according to the invention, comprising copper ions Cu n+(where n is a value of 1-2), potassium ion K + and chloride ion Cl - A salt mixture, wherein the salt mixture has a molar ratio Cu of 1:0.60-1:1.45 n+ :K + , and for preparing chlorine from hydrogen chloride these containing copper ions Cu n+ (where n is a value of 1-2), potassium ion K + and chloride ion Cl - A salt mixture, wherein the salt mixture has a molar ratio of Cu of 1:0.60-1:1.45 n+ :K + .
[0004] Hydrogen chloride (HCl) is a waste product in several industrial processes, such as the preparation of isocyanates. HCl can be converted into chlorine (Cl2) by the so-called Deacon process. The Cl2 produced can then be used to make other commercially valuable products, and at the same time, the emission of waste hydrogen chloride is reduced. The Deacon process is based on the gas phase oxidation of hydrogen chloride: 4HCl+O2→2Cl2+2H2O, wherein the reaction is carried out at about 400 to 450°C in the presence of various catalysts, including, for example, copper chloride (CuCl2). The overall process involves three reactions, namely (1) oxidation of CuCl with oxygen to Cu2OCl2 (CuO.CuCl2): 2CuCl+1 / 2O2→Cu2OCl2 (oxidation); (2) reaction of Cu2OCl2 with gaseous HCl to CuCl2 and water: Cu2OCl2+2HCl→2CuCl2+H2O (chlorination); and (3) thermal decomposition of CuCl2 to obtain CuCl and Cl2: 2CuCl2→2CuCl+Cl2 (dechlorination).
[0005] US 2,418,930 A discloses a two-stage Deacon process in molten salts, wherein reaction (1) is carried out in a first stage and reactions (2) and (3) are combined in a second stage.
[0006] Su et al. studied the use of a molten salt mixture containing 45 mol% KCl and 55 mol% CuCl2 as a catalyst for the reaction of HCl with O2 to produce Cl2 in a single reactor consisting of a quartz tube. The conversion of HCl was measured at 400°C and 450°C. (Su S., Mannini D., Metiu H. Gordon MJ, McFarland EW, Ind. Eng. Chem. Res. 2018, 57, 7795-7801).
[0007] Pavel Tokmakov (Pavel Tokmakov: "Untersuchung zur Chemie des Deacon-Prozesses in Salzschmelzen", 2018) gives an overview of the Deacon method. Tokmakov also gave a paper titled "Suggestions for the technology" (" zur Technologie”) schematically outlines a two-reactor concept and a three-reactor concept and concludes that the three-reactor concept would be problematic, particularly from an energy perspective. The temperatures disclosed for the three reactions (i.e. the three reactors) are 360-375° C. (oxidation (1)), 355° C. (chlorination (2)) and >480° C. (dechlorination (3)). The circulation of the liquid melt is considered difficult, particularly from a viewpoint of keeping the melt in liquid form. Relatively large efforts are proposed to overcome the problems associated with the three-reactor concept, i.e. the use of an airlift pump and the use of a pressure difference and the creation of large temperature differences between the reaction zones for the temperatures of the individual reactions.
[0008] US 2,418,931 A discloses a process for producing chlorine from hydrogen chloride, wherein the temperatures in the first, second and third zones range from 200-425° C. (in the first zone), 200-475° C. (in the second zone) and 500-800° C. (in the third zone).
[0009] One object of the present invention is to provide a new and advantageous process for preparing chlorine from hydrogen chloride, which overcomes the above-mentioned problems, in particular a process which uses a three-reactor concept but overcomes the problem of keeping the melt in liquid form and recyclable, while being simpler and more economical than the processes of the prior art. Another object of the present invention is to provide a reactor system for carrying out the process. Another object of the present invention is to provide an improved salt mixture containing copper ions for use in a process for preparing chlorine from hydrogen chloride, which allows a better space-time yield compared to the salt mixtures known in the prior art.
[0010] Therefore, the present invention relates to a process for preparing chlorine from hydrogen chloride, which comprises circulating a catalyst containing copper ions Cu in a reactor system comprising three bubbling riser reactors I, II and III. n+ (where n is a value of 1-2), alkali cations and chloride ions Cl - The liquid melt of each reactor comprises reaction zones i, ii and iii, respectively, wherein:
[0011] (a) In the reaction zone i of the first bubbling lift reactor i, the copper ions Cu n+ , alkali cations and chloride ions Cl- The liquid melt is contacted with oxygen (O2) at a temperature of >375°C, so that the molar ratio of Cu in the liquid melt is 2+ :Cu + increases, obtaining Cu with an increased molar ratio 2+ :Cu + (b) circulating the liquid melt obtained in (a) to a reaction zone ii in a second bubbling riser reactor II, wherein the liquid melt is contacted with hydrogen chloride (HCl) at a temperature of >355° C., so that water is formed to obtain a liquid melt rich in chloride anions (Cl) compared to the liquid melt obtained according to (a); - ) of a liquid melt;
[0012] (c) recycling the liquid melt obtained in (b) to a reaction zone iii in a third bubbling riser reactor III, which is operated at a temperature of 400-480° C., so that chlorine (Cl2) is formed, wherein Cl2 is removed in gaseous form from reaction zone iii and from the third bubbling riser reactor III, respectively, leaving a Cl2-depleted liquid melt compared to the liquid melt obtained according to (b); - of liquid melt.
[0013] Surprisingly, it has been found that this process for preparing chlorine from hydrogen chloride allows an improvement in the space-time yield with respect to the Cl2 obtained. Due to the specific temperature ranges used in (a), (b) and (c), in particular the specific temperature ranges used in (a) and (c), an improved space-time yield can be achieved for the Cl2 obtained and no means such as airlift pumps and / or pressure differences are required to keep the melt in liquid form and recyclable, resulting in an economically advantageous process (smaller temperature differences between the three reaction zones).
[0014] The expression "copper ion Cu n+ (where n is a value of 1-2)" includes Cu 2+ Cations and Cu 1+ cation, where n is Cu in the salt mixture 2+ The molar mass (m2) multiplied by the charge 2 and the Cu in the salt mixture 1+ The molar mass (m1) multiplied by the sum of the charges 1 divided by the Cu in the salt mixture 2+ and Cu 1+ The total molar amount (Cu 2+ Molar amount (m1) + Cu 1+ Molar amount (m1)): n = [m1x1+m2x2] / [m1+m2].
[0015] In one embodiment of the method, the Cl-depleted - The liquid melt is recycled to (a).
[0016] Preferably, at the beginning of the process, a copper ion Cu is used wherein n is 1.5-2.0, preferably 1.8-2.0, more preferably 1.9-2.0, more preferably 2. n+ , alkali cations and chloride ions Cl - The liquid melt of the reaction zone iii of the third bubbling riser reactor III is used as the initial liquid melt and the process is started in step (c). The reaction zone iii of the third bubbling riser reactor III is operated at a temperature of 400-480° C. Chlorine (Cl 2 ) is formed therein, wherein Cl 2 is removed in gaseous form from the reaction zone iii and the third bubbling riser reactor III, respectively, leaving a Cl 2-depleted liquid melt compared to the initial liquid melt. - of liquid melt.
[0017] About copper ions Cu n+ , alkali cations and chloride ions Cl - Preferably, the alkali cations include one or more alkali cations selected from the group consisting of lithium cations, sodium cations and potassium cations, and more preferably include at least potassium cations. Preferably, the liquid melt contains Cu n+ Potassium ion K + and chloride ion Cl - And by the molar ratio of Cu n+ :K + The present invention relates to a salt mixture of 1:0.60-1:1.45, preferably 1:0.60-1:1.40, more preferably 1:0.77-1:1.20, more preferably 1:0.85-1:1.11, preferably obtained or obtainable from a salt mixture comprising Cu(II)Cl and KCl. A lower KCl amount results in a higher CuCl amount, resulting in an improved Cl productivity of the entire method, i.e., an improved space-time yield.
[0018] According to (a), the copper ion Cu n+ , alkali cations and chloride ions Cl - The liquid melt is contacted with oxygen (O2) at a temperature of >375°C in the reaction zone i of the first bubbling riser reactor I, so that the molar ratio Cu in the liquid melt is 2+ :Cu + Preferably, in (a), the copper ion Cu n+ , alkali cations and chloride ions Cl - The liquid melt is contacted with O2 by using a gas phase containing oxygen (O2). According to (a), the wording "the molar ratio of Cu in the liquid melt is 2+ :Cu + Increased" preferably includes due to Cu + Oxidized by O2, Cu 2+ Ions consist of Cu +Ion formation. Preferably, in (a), the liquid melt is contacted with O2 at a temperature of ≥378°C, more preferably ≥380°C, more preferably at a temperature of >375 to 480°C, more preferably 378-480°C, more preferably 380-420°C, more preferably 390-410°C, more preferably 395-405°C.
[0019] According to (b), the liquid melt obtained in (a) is circulated to the reaction zone ii in the second bubbling riser reactor II, wherein the liquid melt is contacted with hydrogen chloride (HCl) at a temperature of >355°C. The contact with HCl in (b) is preferably carried out by using a gas phase containing hydrogen chloride (HCl). Preferably, the liquid melt is contacted with HCl in (b) at a temperature of ≥358°C, more preferably ≥360°C, more preferably at a temperature of >355 to 420°C, more preferably 358-420°C, more preferably 360-420°C, more preferably 380-420°C, more preferably 390-410°C, more preferably 395-405°C.
[0020] According to (c), the liquid melt obtained in (b) is circulated to the reaction zone iii in the third bubbling riser reactor III, which is operated at a temperature of 400-480° C., so that chlorine (Cl2) is formed, wherein Cl2 is removed in gaseous form from the reaction zone iii and the third bubbling riser reactor III, respectively. Preferably, the Cl2 removal according to (c) is carried out by contacting the liquid melt in (c) with an inert gas, such as argon or nitrogen. Preferably, (c) is carried out at a temperature of 410-440° C., more preferably 415-435° C., more preferably 420-430° C.
[0021] According to a preferred embodiment of the process, the liquid melt is contacted with O2 in (a) at a temperature of >375 to 480°C, preferably 378-480°C, more preferably 380-420°C, more preferably 390-410°C, more preferably 395-405°C;
[0022] The contacting with HCl in (b) is carried out at a temperature of >355 to 420°C, preferably 358-420°C, more preferably 360-420°C, more preferably 380-420°C, more preferably 390-410°C, more preferably 395-405°C; and
[0023] The Cl2 removal according to (c), which is preferably carried out by contacting the liquid melt in (c) with an inert gas, such as argon, is carried out at a temperature of 410-440°C, preferably 415-435°C, more preferably 420-430°C.
[0024] According to a more preferred embodiment of the process, the liquid melt is contacted with O2 in (a) at a temperature of 395-405°C, the contact with HCl in (b) is at a temperature of 395-405°C, and the Cl2 removal according to (c) (which is preferably carried out by contacting the liquid melt in (c) with an inert gas, such as argon) is carried out at a temperature of 420-430°C.
[0025] Compared to the state of the art, these preferred embodiments allow for a small temperature difference (delta T) between steps (a), (b) and (c), which is in the range of 35 to 15°C, thereby resulting in less heating and less cooling required for the process compared to prior art processes, which in turn leads to energy savings.
[0026] The liquid melt is preferably circulated between the bubble rise reactors I, II and III via connecting lines.
[0027] Steps (a), (b) and (c) are carried out batchwise or continuously, preferably continuously.
[0028] Step (a), (b) or (c), preferably at least two of (a), (b) and (c), more preferably (a), (b) and (c) are preferably carried out at a pressure of 800-1200 mbar, preferably 900-1100 bar, more preferably 980-1030 mbar, most preferably at atmospheric pressure (1013 mbar).
[0029] According to a preferred embodiment of the process, the liquid melt is contacted with O2 in (a) at a temperature of >375 to 480°C, preferably 378-480°C, more preferably 380-420°C, more preferably 390-410°C, more preferably 395-405°C;
[0030] The contacting with HCl in (b) is carried out at a temperature of >355 to 420°C, preferably 358-420°C, more preferably 360-420°C, more preferably 380-420°C, more preferably 390-410°C, more preferably 395-405°C; and
[0031] The Cl2 removal according to (c) (which is preferably carried out by contacting the liquid melt in (c) with an inert gas, such as argon) is carried out at a temperature of 410-440°C, preferably 415-435°C, more preferably 420-430°C; wherein (a), (b) or (c), preferably at least two of (a), (b) and (c), more preferably (a), (b) and (c) are preferably carried out at a pressure of 980-1030 mbar, most preferably at atmospheric pressure (1013 mbar).
[0032] According to a more preferred embodiment of the process, the liquid melt is contacted with O2 in (a) at a temperature of 395-405°C, the contact with HCl in (b) is carried out at a temperature of 395-405°C, and the Cl2 removal according to (c) (which is preferably carried out by contacting the liquid melt in (c) with an inert gas, such as argon) is carried out at a temperature of 420-430°C, wherein (a), (b) or (c), preferably at least two of (a), (b) and (c), more preferably (a), (b) and (c), are carried out at a pressure of 980-1030 mbar, most preferably at atmospheric pressure (1013 mbar).
[0033] Reactor system
[0034] Furthermore, the present invention also relates to a reactor system comprising three bubbling riser reactors I, II and III, each bubbling riser reactor comprising reaction zones i, ii and iii; a liquid melt outlet in the top region of each bubbling riser reactor; and a liquid melt inlet in the bottom region of each bubbling riser reactor, wherein the bubbling riser reactors I, II and III are connected by connecting pipelines suitable for the circulation of the liquid melt, such that
[0035] a) the liquid melt outlet of the first bubbling lifting reactor I is connected to the liquid melt inlet of the second bubbling lifting reactor II through a connecting pipeline;
[0036] b) the liquid melt outlet of the second bubbling lifting reactor II is connected to the liquid melt inlet of the third bubbling lifting reactor III via a connecting pipeline;
[0037] c) The liquid melt outlet of the third bubbling riser reactor III is connected to the liquid melt inlet of the first bubbling riser reactor I through a connecting pipeline.
[0038] Preferably, one liquid melt outlet is arranged higher (in the vertical direction) than the other two liquid melt outlets, and preferably one liquid melt outlet is arranged higher (in the vertical direction) by 5-10 mm than the other two liquid melt outlets.
[0039] The "top region of the reactor" refers to the upper part of the reactor starting from the (horizontal) middle of the reactor, including the sides of the reactor and the top of the reactor in the upper part; the bottom region of the reactor refers to the lower part of the reactor starting from the (horizontal) middle of the reactor, including the sides of the reactor and the bottom of the reactor in the lower part.
[0040] In one embodiment of the reactor system, at least a portion of each of the three bubbling riser reactors is surrounded by and in heat transfer contact with an independent heating system. Preferably, the independent heating system surrounds at least the lower portion of each bubbling riser reactor, preferably also surrounds a portion of the connecting pipeline and the corresponding liquid melt inlet. In one embodiment, the independent heating system is a furnace.
[0041] In one embodiment of the reactor system, at least 20% by volume, preferably at least 25% by volume, more preferably at least 30% by volume, more preferably 30-50% by volume of the reactor system, preferably part of the upper part of the three bubbling lift reactors, is embedded with a heating medium and in heat transfer contact with the heating medium, wherein the heating medium preferably comprises a heating device. More preferably, the heating medium surrounds at least a portion of the upper part of each bubbling lift reactor (wherein the liquid melt outlet is arranged) and part of the connecting pipeline between the reactors. In one embodiment, the heating medium is a sand bath and the heating device is at least one heating belt. Preferably, at least one heating belt is embedded in the sand bath and surrounds the reactor. Preferably, the heating medium has a temperature of 370-430°C, preferably 380-420°C, more preferably 390-410°C, more preferably 395-405°C.
[0042] Embedding the reactor system, preferably at least part of the upper part of the three bubbling lift reactors and their liquid melt outlets and part of the connecting lines in a heating medium is advantageous because it allows reducing the temperature difference between the inside and outside of the reactor system, for example the connecting lines between the three reactors, thereby improving the fluidity of the liquid melt in the connecting lines. Thus, embedding the heating medium helps to avoid the need for devices such as airlift pumps and / or pressure differences to keep the melt in liquid form and circulatable, thereby obtaining an economically advantageous process.
[0043] Preferably, each bubbling lift reactor comprises a bubbling lift column and has a gas inlet and a gas outlet in the top region of the bubbling lift reactor. The gas inlet is constructed so that the inlet is located in the top region of the reactor, wherein a tube extends from the inlet at the top of the reactor to the bottom of the reactor and is constructed so that the provided gas phase can be released in the bottom region of the reactor.
[0044] Preferably, at least 90% by volume of the reactor system is surrounded by an independent heating system and a heating medium, so that the lower part of each bubbling lift reactor and part of the connecting pipelines and the corresponding liquid melt inlet are surrounded by an independent heating system and at least part of the upper part of the three bubbling lift reactors and their liquid melt outlets and the (remaining) part of the connecting pipelines are surrounded by a heating medium. In this preferred embodiment, only the top region of each bubbling lift reactor, where the gas inlet and gas outlet are arranged, does not contain a heating device.
[0045] Preferably, each bubbling riser reactor is made of a material independently selected from the group of quartz and ceramics, wherein the ceramic is preferably selected from silicon carbide (SiC), magnesia spinel (Mg spinel oxide), Mg-ZrO2, in particular magnesia partially stabilized zirconia (Mg-PSZ) and Y-ZrO2, in particular yttria stabilized tetragonal zirconia polycrystalline (Y-TZP); more preferably, at least one of the three bubbling riser reactors is made of quartz, and more preferably, all three bubbling riser reactors are made of quartz.
[0046] The invention further relates to chlorine obtained or obtainable by the above-described process for preparing chlorine from hydrogen chloride.
[0047] In addition, the present invention also relates to a method comprising copper ions Cu n+ (where n is a value of 1-2), potassium ion K + and chloride ion Cl - A salt mixture wherein the molar ratio of the salt mixture is Cu n+ :K + It is 1:0.60-1:1.45, preferably 1:0.60-1:1.40, more preferably 1:0.77-1:1.20, more preferably 1:0.85-1:1.11, preferably used for preparing chlorine from hydrogen chloride, more preferably used for preparing chlorine from hydrogen chloride with CuCl2 as catalyst, more preferably used for preparing chlorine from hydrogen chloride with CuCl2 as catalyst in the above reactor system.
[0048] In addition, the present invention also relates to a n+ (where n is a value of 1-2), potassium ion K + and chloride ion Cl- in the preparation of chlorine from hydrogen chloride, preferably using CuCl2 as a catalyst to prepare chlorine from hydrogen chloride, more preferably using CuCl2 as a catalyst to prepare chlorine from hydrogen chloride in the above reactor system, wherein the molar ratio of the salt mixture is Cu n+ :K + It is 1:0.60-1:1.45, preferably 1:0.60-1:1.40, more preferably 1:0.77-1:1.20, more preferably 1:0.85-1:1.11.
[0049] The present invention is further illustrated by the following embodiments and combinations of the embodiments as shown by the corresponding reference relationships and back-references. It should be particularly noted that in each example of a series of embodiments mentioned, for example, in the context of a term such as "the method described in any one of embodiments 1-4", it is meant that each embodiment within the scope is clearly disclosed to the technician, that is, the wording of the term should be understood by the technician as synonymous with "the method described in any one of embodiments 1, 2, 3 and 4". In addition, it should be clearly noted that the following group of embodiments is not a claim to determine the scope of protection, but represents an appropriate structural part of the description of the general and preferred aspects of the present invention.
[0050] 1. A method for preparing chlorine from hydrogen chloride, comprising circulating a reaction mixture containing copper ions Cu in a reactor system comprising three bubbling lift reactors I, II and III. n+ (where n is a value of 1-2), alkali cations and chloride ions Cl-, each reactor comprising reaction zones i, ii and iii, wherein: (a) in reaction zone i of the first bubbling lift reactor I, a liquid melt containing copper ions Cu n+ The liquid melt of alkali cations and chloride ions Cl- is contacted with oxygen (O2) at a temperature >375°C, so that the molar ratio of Cu in the liquid melt is 2+ :Cu + increases, obtaining Cu with an increased molar ratio 2+ :Cu + (b) circulating the liquid melt obtained in (a) to reaction zone ii in a second bubbling riser reactor II, wherein the liquid melt is contacted with hydrogen chloride (HCl) at a temperature of >355°C to form water, thereby obtaining a liquid melt enriched in chloride anions (Cl-) compared to the liquid melt obtained according to (a); (c) circulating the liquid melt obtained in (b) to reaction zone iii in a third bubbling riser reactor III, which is operated at a temperature of 400-480°C to form chlorine gas (Cl2), wherein Cl2 is removed in gaseous form from reaction zone iii and the third bubbling riser reactor III, respectively, leaving a liquid melt depleted in Cl- compared to the liquid melt obtained according to (b).
[0051] 2. The method according to embodiment 1, wherein the Cl-depleted liquid melt obtained in (c) is recycled to (a).
[0052] 3. The method of embodiment 1 or 2, wherein at the beginning of the method, a copper ion Cu is used wherein n is 1.5-2, preferably 1.8-2.0, more preferably 1.9-2.0, more preferably 2. n+ A liquid melt of alkali cations and chloride ions Cl- is used as the initial liquid melt and the method is started in step (c).
[0053] 4. The method according to any one of embodiments 1 to 3, wherein the copper ion Cu n+ , alkali cations and chloride ions Cl - The liquid melt contains, as alkali cations, one or more alkali cations selected from the group consisting of lithium cations, sodium cations and potassium cations, and more preferably contains at least potassium cations.
[0054] 5. The method of embodiment 4, wherein the liquid melt comprises Cu n+ Potassium ion K + and chloride ions Cl- and by molar ratio Cu n+ :K + The invention is obtained or obtainable from a salt mixture having a ratio of 1:0.60 to 1:1.45, preferably 1:0.60 to 1:1.40, more preferably 1:0.77 to 1:1.20, more preferably 1:0.85 to 1:1.11, preferably obtained or obtainable from a salt mixture comprising Cu(II)Cl2 and KCl.
[0055] 6. The method of any one of embodiments 1-5, wherein in (a), the liquid melt is contacted with O2 at a temperature ≥378°C, more preferably ≥380°C, more preferably at a temperature of >375 to 480°C, more preferably 378-480°C, more preferably 380-420°C, more preferably 390-410°C, more preferably 395-405°C.
[0056] 7. The process of any one of embodiments 1-6, wherein in (b), the liquid melt is contacted with HCl at a temperature ≥358°C, more preferably ≥360°C, more preferably at a temperature of >355 to 420°C, more preferably 358-420°C, more preferably 360-420°C, more preferably 380-420°C, more preferably 390-410°C, more preferably 395-405°C.
[0057] 8. The method of any one of embodiments 1-7, wherein (c) is carried out at a temperature of 410-440°C, preferably 415-435°C, more preferably 420-430°C.
[0058] 9. The process according to any one of embodiments 1 to 8, wherein the liquid melt is circulated between the bubble riser reactors I, II and III via connecting lines.
[0059] 10. The method of any one of embodiments 1-9, wherein (a), (b) and (c) are carried out in a batch mode or a continuous mode, preferably a continuous mode.
[0060] 11. The method of any one of embodiments 1-10, wherein (a), (b) or (c), preferably at least two of (a), (b) and (c), more preferably (a), (b) and (c) are carried out at a pressure of 800-1200 mbar, preferably 900-1100 bar, more preferably 980-1030 mbar, and most preferably at atmospheric pressure (1013 mbar).
[0061] 12. A reactor system comprising three bubbling riser reactors I, II and III, each bubbling riser reactor comprising a reaction zone i, ii and iii, respectively; a liquid melt outlet in the top region of each bubbling riser reactor; and a liquid melt inlet in the bottom region of each bubbling riser reactor, wherein the bubbling riser reactors I, II and III are connected by a connecting pipeline suitable for liquid melt circulation, such that
[0062] d) the liquid melt outlet of the first bubbling lifting reactor I is connected to the liquid melt inlet of the second bubbling lifting reactor II through a connecting pipeline;
[0063] e) the liquid melt outlet of the second bubbling lifting reactor II is connected to the liquid melt inlet of the third bubbling lifting reactor III through a connecting pipeline;
[0064] f) The liquid melt outlet of the third bubbling riser reactor III is connected to the liquid melt inlet of the first bubbling riser reactor I through a connecting pipeline.
[0065] 13. In the reactor system described in embodiment 12, one liquid melt outlet is arranged higher (in the vertical direction) than the other two liquid melt outlets, and preferably one liquid melt outlet is arranged higher (in the vertical direction) than the other two liquid melt outlets by 5-10 mm.
[0066] 14. The reactor system of embodiment 12 or 13, wherein at least a portion of each of the three bubble lift reactors is surrounded by and in heat transfer contact with an independent heating system.
[0067] 15. The reactor system of any one of embodiments 12-14, wherein at least 20 volume %, preferably at least 25 volume %, more preferably at least 30 volume %, more preferably 30-50 volume % of the reactor system, preferably at least part of the three bubbling lift reactors and their liquid solution outlets and optionally part of the connecting pipelines are embedded with a heating medium and in heat transfer contact with the heating medium, wherein the heating medium preferably includes a heating device.
[0068] 16. The reactor system of any one of embodiments 12-15, wherein each bubbling riser reactor comprises a bubbling riser column and has a gas inlet and a gas outlet in a top region of the bubbling riser reactor.
[0069] 17. The reactor system of any one of embodiments 12-16, wherein each bubbling lift reactor is made of a material independently selected from the group of quartz and ceramics, wherein the ceramic is preferably selected from silicon carbide (SiC), magnesia spinel, Mg-ZrO2, in particular magnesia partially stabilized zirconia (Mg-PSZ) and Y-ZrO2, in particular yttria stabilized tetragonal zirconia polycrystalline (Y-TZP); more preferably, at least one of the three bubbling lift reactors is made of quartz, and more preferably, all three bubbling lift reactors are made of quartz.
[0070] 18. Chlorine obtained or obtainable by the method of any one of embodiments 1-11.
[0071] 19. A method comprising copper ions Cu n+ (where n is a value of 1-2), potassium ion K + and chloride ions Cl-, wherein the molar ratio of the salt mixture is Cu n+ :K + It is 1:0.60-1:1.45, preferably 1:0.60-1:1.40, more preferably 1:0.77-1:1.20, more preferably 1:0.85-1:1.11, preferably used for preparing chlorine from hydrogen chloride, more preferably used for preparing chlorine from hydrogen chloride using CuCl2 as a catalyst, more preferably used for preparing chlorine from hydrogen chloride using CuCl2 as a catalyst in a reactor system according to any one of Embodiments 12-16.
[0072] 20. Contains copper ions Cu n+ (where n is a value of 1-2), potassium ion K + and chloride ion Cl- in the preparation of chlorine from hydrogen chloride, preferably using CuCl2 as a catalyst to prepare chlorine from hydrogen chloride, more preferably using CuCl2 as a catalyst in the preparation of chlorine from hydrogen chloride in a reactor system according to any one of embodiments 12 to 16, wherein the molar ratio of the salt mixture is Cu n+ :K + It is 1:0.60-1:1.45, preferably 1:0.60-1:1.40, more preferably 1:0.77-1:1.20, more preferably 1:0.85-1:1.11.
[0073] The present invention is further illustrated by the following reference examples, comparative examples and examples. Example
[0074] Chemicals
[0075]
[0076] Analytical Instruments
[0077] The chlorine (Cl2) content was determined by introducing the exhaust gas taken from the gas outlet of the bubbling riser reactor III from the corresponding reactor (reference example 1) or from the reactor system (reference example 2) into a conical flask containing 1.0 liter of water and 20 ml of a 5M NaNO3 aqueous solution over a frit. The chloride ion content in the solution was continuously measured by an ISE (ion selective electrode, Cole-Parmer).
[0078] Reference Example 1: Reactor for testing a single reaction step (device 1)
[0079] A cylindrical reactor (all made of quartz) with a gas inlet tube (gas inlet) was used. The gas inlet was constructed so that the inlet was located in the top region of the reactor, wherein the tube extended from the inlet at the top of the reactor to the bottom of the reactor and was constructed so that the provided gas phase could be released in the bottom region of the reactor. The gas outlet was located at the head of the reactor.
[0080] The reactor is filled with the respective salt mixture described below. The gas inlet is then arranged so that its opening is about 1 cm above the salt mixture. The argon flow is started and the temperature is increased to melt the salt mixture. The respective gas inlet tube is then lowered into the liquid melt.
[0081] Reference Example 2: Reactor system for 3-stage continuous testing (device 2)
[0082] The reactor system comprises three independent bubbling riser reactors I, II and III. In use, each bubbling riser reactor contains a molten Cu salt species (the liquid melt contains copper ions Cu n+ (where n is a value of 1-2), potassium ion K + and chloride ion Cl - ), which circulates continuously in and between bubbling lift reactors, and the system can supply and remove independent gases (such as Figure 1 All bubble riser reactors are made of quartz, have an inner diameter of 22 mm and a length of 400 mm. In the following, "bubble riser reactor" is abbreviated as "reactor". A single reactor device is schematically shown in Figure 2 .
[0083] The three independent reactors I, II and III are connected to each other by connecting pipelines, which allow the melt to circulate between the reactors. Each reactor has a liquid melt outlet and a liquid melt inlet. The liquid melt outlet of one reactor is located in its top area and leads to the liquid melt inlet in the bottom area of the next reactor (such as Figure 1 shown in Figure 1In the figure, the gas inlet and gas outlet in the corresponding reactor are represented by simple arrows. Figure 3 A schematic top view showing the reactor system, Figure 4 is a schematic side view of the reactor system).
[0084] In detail, the liquid melt outlet of reactor I located in the top area of reactor I is connected to the liquid melt inlet in the bottom area of reactor II through a connecting pipeline; the liquid melt outlet in the top area of reactor II is connected to the liquid melt inlet in the bottom area of reactor III through a connecting pipeline; and the liquid melt outlet in the top area of reactor III is connected to the liquid melt inlet in the bottom area of reactor I through a connecting pipeline.
[0085] All three reactors I, II and III have in their top region a further inlet suitable for gas supply (gas inlet) and in their reactor head an outlet suitable for discharge of gaseous components (gas outlet). The gas inlet is a tube with a diameter of 2 mm.
[0086] The gas inlet for the gas supply is constructed so that the inlet is located in the reactor top region, wherein a tube extends from the inlet in the reactor top to the bottom of the reactor and is constructed so that the supplied gas phase can be released in the bottom region of the reactor. All three reactors are heated individually by a furnace so that the temperature is adjusted individually for each reactor.
[0087] The liquid melt outlet, the liquid melt inlet and all the connecting pipelines between the three reactors and all the components above the furnace of all three reactors are placed in a sand bath heated by the same heating medium and heating belt (such as Figure 5 ). Figure 4 In the diagram, the heating medium (sand bath) is represented by the square in the upper area and the independent heating system (furnace) is represented by the square in the lower area of each reactor (F1 for reactor I, F2 for reactor II, F3 for reactor III).
[0088] In use, all three reactors are arranged at the same height, and all liquid melt inlets are located at the same height. For one reactor, the liquid melt outlet is 5-10 mm higher than the liquid melt outlets of the two remaining reactors to improve the flow between the reactors (not shown).
[0089] Example 1: Thermal decomposition of CuCl2 in a small-scale reactor (analogously to the reaction in reactor III according to Reference Example 2).
[0090] The CuCl2 thermal decomposition reaction was measured in a reactor as described in Reference Example 1 (Apparatus 1). The reactor had an inner diameter of 9 mm and a length of 300 mm; two different gas inlet tubes were used: one was a ceramic tube with 4 holes and an inner diameter of 0.5 mm; the other was a quartz inlet tube with an inner diameter of 2 mm, which was heat-treated to reduce the outlet diameter.
[0091] The salt mixture has a composition of 36 wt % anhydrous potassium chloride (KCl) and 64 wt % anhydrous copper (II) chloride (CuCl2). 15 g of the salt mixture is heated to 370° C. in a reactor to form a molten salt ("molten salt" is synonymous with "liquid melt") and then further heated to the reaction temperature. The height of the molten salt is 9 cm. 15 sccm (sccm=standard cubic centimeter / minute) of argon is bubbled through the molten salt. The chlorine production rate is measured with a chlorine ISE probe. Using a ceramic tube with 4 holes and an inner diameter of 0.5 mm, the production volume rate of Cl2 at 450° C. is 0.175 mol / m 3 ·s. Using a quartz inlet tube with an inner diameter of 2 mm, which was heat treated to reduce the outlet diameter, the Cl2 production volume rate at 395°C was 0.03 mol / m 3 ·s.
[0092] Example 2: CuCl oxidation reaction (similar to the reaction in reactor 1 according to reference example 2)
[0093] The reactor had an inner diameter of 9 mm and a length of 300 mm, wherein the reactor apparatus was as described in Reference Example 1 (Apparatus 1). The salt mixture had a composition of 28 wt % anhydrous potassium chloride (KCl) and 72 wt % anhydrous copper (I) chloride (CuCl). 20 g of the mixed salt was heated to 350° C. to form a liquid melt. The height of the molten salt was 15 cm. 9 sccm of O2 and 1 sccm of Ar were bubbled through the molten salt through a quartz tube with an inner diameter of 2 mm. The oxygen conversion was 29% at 380° C. When a gas mixture of 16 sccm O2 and 4 sccm of Ar was bubbled through the molten salt through a quartz tube with an inner diameter of 2 mm, the oxygen conversion was 22% at 360° C. and 14% at 400° C.
[0094] Example 3: Chlorination reaction (similar to the reaction in reactor II according to reference example 2)
[0095] The composition of the salt mixture used in the chlorination experiments was 24 wt % anhydrous potassium chloride (KCl), 66 wt % anhydrous copper (II) chloride (CuCl2) and 10 wt % anhydrous copper (II) oxide (CuO). The reactor had an inner diameter of 9 mm and a length of 300 mm. The gas inlet pipe had an inner diameter of 2 mm. The reactor apparatus was as described in Apparatus 1. When the salt mixture was heated to 350°C, KCl and CuCl2 formed a liquid melt. A gas mixture of 20 sccm O2 and 3 sccm HCl was bubbled through the molten salt. The HCl conversion was 97% at 360°C and 94% at 380°C, as measured by a chloride ISE probe.
[0096] Example 4: Cyclic reaction in a reactor system
[0097] The reactor system comprises three independent bubble rising reactors I, II and III, wherein the reactor system apparatus is as described in Reference Example 2 (Apparatus 2).
[0098] For reactor III, T = 425 ° C was set as the operating temperature. For reactors I and II, the temperature was set to T = 400 ° C. The temperatures of reactors I, II and III are the temperatures in reaction zones i, ii, iii. The temperature is measured inside the furnace, approximately halfway between the top and bottom of each reactor. The distance between the temperature probe and the reactor wall containing the molten salt is 1-2 mm. An OMEGA-quick disconnect type thermocouple is used. The error of T is estimated to be + / - 0.1 ° C.
[0099] Start-up phase
[0100] 36 wt % of anhydrous potassium chloride (KCl) and 64 % of anhydrous copper (II) chloride (CuCl ) are mixed to obtain a salt mixture. The salt mixture is introduced into an empty reactor (tightly packed to avoid forming bubbles). The reactor is closed so that the end of the gas inlet pipe is located about 1 mm above the salt mixture. An argon gas flow is started in reactor III. The temperature in the reactor increases at a rate of 100 ℃ per 20-30 minutes, and the operating temperature of each reactor is reached after 1-2 hours and the salt is molten. At the operating temperature, the gas inlet pipe is lowered into the liquid melt until there is a distance of 30 mm between the end of the pipe and the bottom of the reactor.
[0101] Before inserting the gas inlet tubes into reactors I and II, the O2 flow and the HCl / Ar flow were started.
[0102] The pressure in the reactor system was 1 atm (1013 mbar, the system was open to the atmosphere). The gas flow rates of O2, HCl, Ar were each set to 240 ml / min. In the case of HCl, this was generated in situ by bubbling 240 ml / min of argon in a concentrated aqueous HCl solution (360 ml).
[0103] Normal operation stage
[0104] Compared to the three separate reactors of Examples 1-3, the temperature of the cyclic reaction including all three reactions is selected so that the optimum value is reached taking into account the release of Cl2 (which increases with increasing temperature), the vaporization of CuCl2 (which also increases with increasing temperature) and the smallest possible temperature difference between the reaction zones. Therefore, in operation, the reactor III has a temperature of T = 425 ° C, and the temperature is set to T = 400 ° C in the reactors I and II. O2 is supplied to the reactor I through the gas inlet at a flow rate of 240 ml / min, wherein the gas stream containing O2 is removed by the gas outlet of the reactor I. HCl is supplied to the reactor II and the gaseous stream containing HCl and water is removed through the gas outlet of the reactor II. Gaseous argon is supplied to the reactor III at a flow rate of 240 ml / min; the gaseous stream containing Ar and Cl2 leaves the reactor III through the gas outlet and is transferred to a connected conical flask containing 1.0 liter of water and 20 ml of NaNO3 aqueous solution (5M) for analysis.
[0105] Cl2 was continuously formed during the operating time of about 5 hours. It can therefore be shown that the process of the present invention is an advantageous process and a promising candidate for an economical industrial process, wherein in the reaction zone i in the first bubbling riser reactor I, in step (a), the liquid melt is contacted with O2 at a temperature of >375°C; the liquid melt obtained in (a) is circulated to the reaction zone ii in the second bubbling riser reactor II, wherein in step (b), the liquid melt is contacted with hydrogen chloride (HCl) at a temperature of >355°C; and in step (c), the liquid melt obtained in (b) is circulated to the reaction zone iii in the third bubbling riser reactor III, which is operated at a temperature of 400-480°C. BRIEF DESCRIPTION OF THE DRAWINGS
[0107] Figure 1 A reactor system comprising three separate reactors I, II and III is shown. In use, each reactor contains a molten copper salt species, which is continuously circulated in the reactor. The inlet and outlet for the liquid melt and the inlet and outlet for the melt circulation and the corresponding connecting pipelines are indicated by arrows on the sides and between the reactors; the gas inlets and gas outlets for the gas components entering and leaving the reactors are schematically indicated at the bottom and top of the reactors. The reaction zones i, ii and iii in each reactor are not shown.
[0108] Figure 2 The construction of all individual reactors I, II and III is shown in more detail, taking one reactor as an example. The reactor design consists of three parts: the main reactor (1), the insert column (2) and the inlet pipe (3) for conveying gaseous reagents in the reactor system. The main reactor (1) is equipped with a glass joint top, which has a gas inlet and a gas outlet for feeding and removing gaseous reagents and products, as well as a liquid melt inlet and an outlet for liquid melt (circulation). The insert column (2) separates the area exposed to the gas bubbles and allows the liquid to flow back to the main reactor from the holes on the insert top. Figure 2 The black arrows (→) in FIG. 5 show the melt direction in a single reactor, i.e., the melt direction in a single bubbling riser column. The dashed arrows indicate the direction of gas flow.
[0109] Figure 3 A schematic top view of the reactor system is shown, wherein the flow direction of the circulating melt is indicated by arrows.
[0110] Figure 4 A schematic side view of the reactor system is shown, wherein the flow direction of the circulating melt is indicated by arrows. All three reactors I, II and III are placed in a heating medium system, such that the top region of each reactor is embedded in the heating medium, wherein the liquid melt outlet and at least a portion of the connecting pipelines are located in the heating medium (4). All three reactors are further equipped with a separate heating system (F1, F2, F3), such as a furnace, such that a portion of the bottom region of each reactor is surrounded by its separate heating system and is in heat transfer contact with it. Figure 4 As shown, each separate heating system (F1, F2, F3) surrounds at least a portion of the bottom area of each reactor (where the liquid melt inlet is arranged). Preferably, for one reactor, the liquid melt outlet is 5-10 mm higher than the liquid melt outlets of the other two reactors to improve the flow between the reactors (not shown). The arrows at the top of each reactor represent gas inflow and gas outflow.
[0111] Figure 5 The arrangement of the upper part of three bubbling lift reactors in a heating medium (here a sand bath) is shown. The top area of all three reactors is surrounded in the sand bath so that the liquid melt outlet and at least a part of the connecting pipelines are located inside the sand bath. The heating band (5) encloses a large horizontal triangle around the outside of the connecting pipelines and also a small horizontal triangle inside the connecting pipelines.
[0112] Reference numerals
[0113] 1 Main Reactor
[0114] 2 Insert column
[0115] 3 Inlet pipe
[0116] 4 Heating medium / sand bath
[0117] 5 Heating belt
[0118] F1, F2, F3 separate heating system / furnace
[0119] References cited
[0120] -US 2,418,930
[0121] -Su S. et al., Ind.Eng.Chem.Res.2018, 57, 7795-7801
[0122] -Dissertation of Pavel Tokmakov: “Untersuchung zur Chemie des Deacon-Prozesses in Salzschmelzen“, 2018
[0123] -US 2,418,931 A
Claims
1. A method for preparing chlorine from hydrogen chloride, comprising circulating a copper ion Cu containing a value of n of 1 to 2 in a reactor system comprising three bubbling riser reactors I, II and III. n+ , alkali cations and chloride ions Cl - The liquid melt of each reactor comprises reaction zones i, ii and iii, in: (a) In the reaction zone i of the first bubbling lift reactor i, the copper ions Cu n+ , alkali cations and chloride ions Cl - The liquid melt is reacted with oxygen (O 2 ) contact, so that the molar ratio of Cu in the liquid melt 2+ :Cu + increases, obtaining Cu with an increased molar ratio 2+ :Cu + of liquid melt; (b) circulating the liquid melt obtained in (a) to reaction zone ii in a second bubbling riser reactor II, wherein the liquid melt is contacted with hydrogen chloride (HCl) at a temperature of 395-405° C., so that water is formed to obtain a liquid melt rich in chloride anions (Cl) compared to the liquid melt obtained according to (a); - ) of a liquid melt; (c) circulating the liquid melt obtained in (b) to reaction zone iii in a third bubbling riser reactor III, which is operated at a temperature of 420-430° C., so that chlorine (Cl 2 ), where Cl 2 The liquid melt is removed in gaseous form from the third bubbling riser reactor III, leaving a liquid melt depleted in Cl compared to that obtained according to (b). - of liquid melt, The Cl-depleted - The liquid melt is recycled to (a).
2. The method according to claim 1, wherein at the beginning of the method a copper ion Cu is used wherein n is a value of 1.5-2.
0. n+ , alkali cations and chloride ions Cl - A liquid melt of is used as the initial liquid melt and the method is started in step (c).
3. The method according to claim 1, wherein at the beginning of the method, a copper ion Cu is used wherein n is a value of 1.8-2.
0. n+ , alkali cations and chloride ions Cl - A liquid melt of is used as the initial liquid melt and the method is started in step (c).
4. The method according to claim 3, wherein at the beginning of the method, a copper ion Cu is used, wherein n is a value of 1.9-2.
0. n+ , alkali cations and chloride ions Cl - A liquid melt of is used as the initial liquid melt and the method is started in step (c).
5. The method according to claim 4, wherein at the beginning of the method a copper ion Cu is used wherein n is 2. n+ , alkali cations and chloride ions Cl - A liquid melt of is used as the initial liquid melt and the method is started in step (c).
6. The method according to any one of claims 1 to 5, wherein the copper ion Cu n+ , alkali cations and chloride ions Cl - The liquid melt contains, as alkali cations, one or more alkali cations selected from the group consisting of lithium cations, sodium cations and potassium cations.
7. The method according to claim 6, wherein the copper ion Cu n+ , alkali cations and chloride ions Cl - The liquid melt contains at least potassium cations.
8. The method according to claim 7, wherein the liquid melt comprises Cu n+ Potassium ion K + and chloride ion Cl - And by the molar ratio of Cu n+ :K + A salt mixture of 1:0.60-1:1.45 was obtained.
9. The method according to claim 7, wherein the liquid melt comprises Cu n+ Potassium ion K + and chloride ion Cl - And by the molar ratio of Cu n+ :K + A salt mixture of 1:0.60-1:1.40 is obtained.
10. The method according to claim 7, wherein the liquid melt comprises Cu n+ Potassium ion K + and chloride ion Cl - And by the molar ratio of Cu n+ :K + A salt mixture of 1:0.77-1:1.20 was obtained.
11. The method according to claim 7, wherein the liquid melt comprises Cu n+ Potassium ion K + and chloride ion Cl - And by the molar ratio of Cu n+ :K + A salt mixture of 1:0.85-1:1.11 was obtained.
12. The method according to claim 7, wherein the liquid melt comprises Cu n+ Potassium ion K + and chloride ion Cl - and contains Cu(II)Cl 2 and KCl salt mixture.
13. The process according to any one of claims 1 to 5, wherein (a), (b) and (c) are carried out in a batch mode or a continuous mode.
14. The method according to claim 6, wherein (a), (b) and (c) are carried out in a batch mode or a continuous mode.
15. The method according to any one of claims 7 to 12, wherein (a), (b) and (c) are carried out in a batch mode or a continuous mode.
16. The method of claim 15, wherein (a), (b) and (c) are performed in a continuous manner.
17. A reactor system comprising three bubbling riser reactors I, II and III, each bubbling riser reactor comprising a reaction zone i, ii and iii, respectively; a liquid melt outlet in the top region of each bubbling riser reactor; a liquid melt inlet in the bottom region of each bubbling riser reactor, wherein the bubbling riser reactors I, II and III are connected by connecting pipelines suitable for liquid melt circulation, such that a) the liquid melt outlet of the first bubbling riser reactor I is connected to the liquid melt inlet of the second bubbling riser reactor II via a connecting pipeline; b) the liquid melt outlet of the second bubbling lifting reactor II is connected to the liquid melt inlet of the third bubbling lifting reactor III via a connecting pipeline; c) the liquid melt outlet of the third bubbling riser reactor III is connected to the liquid melt inlet of the first bubbling riser reactor I through a connecting pipeline, One of the liquid melt outlets is arranged higher in the vertical direction than the other two liquid melt outlets.
18. The reactor system according to claim 17, wherein one liquid melt outlet is arranged 5-10 mm higher in the vertical direction than the other two liquid melt outlets.
19. The reactor system according to claim 17 or 18, wherein each bubbling riser reactor is made of a material independently selected from the group consisting of quartz and ceramic.
20. The reactor system of claim 19, wherein the ceramic is selected from the group consisting of silicon carbide (SiC), magnesia spinel, Mg-ZrO 2 and Y-ZrO 2 .
21. The reactor system of claim 20, wherein the ceramic is selected from magnesia partially stabilized zirconia (Mg-PSZ).
22. The reactor system of claim 20, wherein the ceramic is selected from yttria-stabilized tetragonal zirconia polycrystals (Y-TZP).
23. The reactor system of claim 21 or 22, wherein at least one of the three bubble riser reactors is made of quartz.
24. The reactor system of claim 23, wherein all three bubble riser reactors are made of quartz.