A device for stripping anti-corrosion coating of glass flakes in service in thermal power plants and a sampling method
By designing a glass flake coating stripping device with stoppers, L-shaped jacking blocks and jacking bolts, and combining the operation process of ultrasonic thickness measurement and handheld grinding wheels, the problem of sampling glass flake coatings in service in thermal power plants has been solved and achieved Safe, easy-to-operate sampling and evaluation ensure the stability and anti-corrosion effect of the anti-corrosion coating.
Patent Information
- Application Number
- CN202210249407.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-03-14
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2042-03-14
AI Technical Summary
It is difficult to effectively evaluate and sample the in-service glass flake anti-corrosion coatings of thermal power plants with existing technology, resulting in the performance degradation of the coatings in corrosive media and shortened anti-corrosion life, and there is a lack of reliable sampling methods and equipment.
A glass flake coating stripping device including a stopper, an L-shaped jacking block and a jacking bolt was designed. By grooving, grinding, and dividing the splines in the sampling area, and using the flake stripping device to peel off the coating one by one, combined with ultrasonic thickness measurement and operating procedures for handheld grinding wheels.
It achieves safe and easy-to-operate sampling and evaluation of glass flake coatings without destroying large-area coatings, fills the gap in sampling methods, and ensures the repair and subsequent anti-corrosion effects of the sampling area.
Smart Images

Figure CN114739761B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of quality assessment of in-service glass flake anti-corrosion coatings of post-furnace environmental protection facilities in thermal power plants, and relates to a device for stripping in-service glass flake anti-corrosion coatings in thermal power plants and a sampling method. Background Art
[0002] Glass flake coating is a non-fiber reinforced resin-based composite material. It is widely used in wet flue gas desulfurization systems of coal-fired power plants due to its excellent anti-corrosion performance and low cost. However, there is currently a lack of product quality standards in the glass flake anti-corrosion industry. The quality of glass flake mortar products and construction quality on the market vary greatly. Even a few months after the construction of glass flake anti-corrosion coating, the tower will be corroded and perforated. Research and engineering practice experience have shown that under the combined effects of corrosive medium immersion, scouring, comprehensive stress, temperature change, etc., glass flake coatings may produce microcracks, resin swelling, resin and glass flake interface damage and other defects inside the organization, resulting in the decline of mechanical properties and corrosion resistance, surface and internal material structure, weakening the anti-corrosion performance of the coating, and shortening the anti-corrosion life. Based on these realities, power plants urgently need to regularly take on-site samples of glass flake coatings in service without damaging the anti-corrosion area, inspect and evaluate their service performance, and provide a basis for further technical transformation or maintenance.
[0003] Difficulties in sampling glass flake coatings:
[0004] 1. The toughness of glass flake coating is poor, requiring professional cutting equipment and reasonable cutting process;
[0005] 2. The adhesion between the glass flake coating and the carbon steel primer is strong, so a special stripping solution is required;
[0006] 3. Glass flake coating is a polymer material with an upper temperature limit of about 80°C. There is a risk of ignition during cutting operation;
[0007] 4. Perform professional repairs on the incision site to prevent leakage at the incision site.
[0008] A reliable sampling method for in-service glass flake coatings is a bottleneck restricting the performance evaluation of glass flake anti-corrosion coatings, and an operational sampling scheme is urgently needed. Summary of the invention
[0009] The technical problem solved by the present invention is as follows: The present invention provides a feasible and easy-to-operate in-service glass flake anti-corrosion coating stripping device and sampling method for the glass flake anti-corrosion coating of the environmental protection facilities behind the furnace of a thermal power plant.
[0010] The technical solution of the present invention:
[0011] A device for stripping glass flake anti-corrosion coatings in service in a thermal power plant comprises a block, an L-shaped top block and a jacking bolt. The block comprises a horizontal section and a vertical section for welding to the surface of a carbon steel substrate. The L-shaped top block also comprises a horizontal section and a vertical section. A threaded hole is provided on the vertical section of the L-shaped top block. The threaded section of the jacking bolt is rotatably arranged in the threaded hole. The nut end of the jacking bolt is arranged between the vertical section of the block and the vertical section of the L-shaped top block. The end of the horizontal section of the L-shaped top block contacts the glass flake coating.
[0012] Preferably, the ends of the horizontal sections of the L-shaped top block are coated with plastic.
[0013] A method for sampling an in-service glass flake anti-corrosion coating of a thermal power plant using a stripping device comprises the following steps:
[0014] S1, select sampling area and sampling site;
[0015] S2, making grooves on the sampling site to divide the sampling site into a sampling area and an instrument fixing area;
[0016] S3, removing glass flakes on the instrument fixing area and then polishing the area;
[0017] S4, processing the glass flake coating on the sampling area into a plurality of sample strips;
[0018] S5, installing a scale stripping device in the instrument fixing area, the scale stripping device is in contact with the end of the sample;
[0019] S6, peeling the specimens from the sampling area one by one using a scale peeling device.
[0020] Preferably, in step S1, the sampling area is selected in the area of the glass flakes that is directly washed by smoke or slurry; the sampling points in the sampling area are selected at points where the glass flake coating has a large color difference and rust marks on the surface, and the sampling points are flat without protrusions or pits; after the sampling points are selected, they are marked and numbered with a marker, and there are no less than 6 sampling points in the glass flake anti-corrosion area of each unit.
[0021] Preferably, in step S2, a "sun"-shaped area is carved on the marked sampling site, and cutting and grooving are performed along the scribed area, wherein the "sun"-shaped area is divided into a sampling area and an instrument fixing area.
[0022] Preferably, before cutting and grooving along the scored area, the thickness of the flake coating in the grooved area is measured with an ultrasonic thickness gauge to ensure that the groove depth is slightly smaller than the thickness of the flake coating in the grooved area; after cutting and grooving along the scored area, the bottom of the groove is grinded at a low speed with a handheld grinding wheel of the same width, with the grinding wheel speed of the grinder being 30 to 50 rpm, to grind off the glass flake base coating to reveal the original color of the steel plate.
[0023] Preferably, step S4 specifically comprises first removing the glass flakes in the fixed area and grinding until the original color of the steel plate is exposed; then opening a plurality of parallel strip grooves on the surface of the glass flake coating in the sampling area, determining the specifications of the strip grooves according to the test requirements, and dividing the glass flake coating into a number of parallel arranged splines.
[0024] Preferably, in step S5, a stopper of the stripping device is spot-welded and fixed on the surface of the polished carbon steel substrate in the instrument fixing area, the screw section of the push bolt is installed into the threaded hole on the vertical section of the L-shaped top block, and then the L-shaped top block of the stripping device is placed on the surface of the carbon steel substrate, ensuring that the vertical section of the L-shaped top block is opposite to the vertical section of the stopper, and the end of the horizontal section of the L-shaped top block is in contact with the spline end of the glass flake coating.
[0025] The preferred step S6 is specifically: first press the glass flakes to prevent the peeled flakes from being cracked due to stress, and then use a tool to rotate the jacking bolt so that the jacking bolt is screwed out to one side of the top block, and the nut end of the jacking bolt squeezes the vertical section of the block, and at the same time the block provides a reverse force to the jacking bolt. After the jacking bolt is subjected to force, it squeezes the L-shaped top block, and the horizontal section end of the L-shaped top block applies force to the glass flake coating, thereby peeling off the glass flake coating.
[0026] Preferably, the method further includes step S7, in which the sampling area is restored; after the sampling is completed, the surface of the sampling area is polished to remove rust and weld nodules, the edge of the scales at the incision is polished to form a 30° groove, two coats of primer are applied, and after the surface is dry, the intermediate coating and the top coating are troweled, and the intermediate coating and the top coating cover the surrounding repair surface to cover the groove.
[0027] Beneficial effects of the invention: The invention provides a device for stripping an in-service glass flake anti-corrosion coating of a thermal power plant and a sampling method, which has the following advantages:
[0028] 1. The sampling method of the in-service glass flake coating of the present invention is easy to implement, filling the blank of glass flake coating sampling.
[0029] 2. The stripping device of the present invention is simple in equipment and easy to operate. It does not damage the base carbon steel material or the large-area anti-corrosion coating and is suitable for sampling and analysis of anti-corrosion plane areas of tens of thousands of square meters.
[0030] 3. The repair process after the sampling method of the present invention is simple, the glass flake coating has good stability after repair, and does not affect the anti-corrosion effect of subsequent service. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] Figure 1 It is a schematic diagram of the slot segmentation of the sampling site;
[0032] Figure 2 It is a schematic diagram of the fixed instrument area stripping at the sampling site;
[0033] Figure 3It is a schematic diagram of spline segmentation of glass flake coating;
[0034] Figure 4 It is a schematic diagram of the peeling of glass flake coating specimen from carbon steel substrate;
[0035] Figure 5 yes Figure 4 A cross-sectional view of
[0036] In the figure: 1-L-type stopper; 2-jacking bolt; 3-L-type top block, 4-glass flake coating, 5-carbon steel substrate. DETAILED DESCRIPTION
[0037] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0038] One embodiment of the present invention: a device for stripping the anti-corrosion coating of glass flakes in service in a thermal power plant, such as Figure 5 As shown, it includes an L-shaped stopper 1, an L-shaped top block 3 and a jacking bolt 2. The L-shaped stopper 1 includes a horizontal section and a vertical section for welding with the surface of a carbon steel substrate 5. The L-shaped top block 3 also includes a horizontal section and a vertical section. The vertical section of the L-shaped top block 3 is provided with an M16 threaded hole. The specification of the jacking bolt is M16, and the bolt length is determined according to the actual spacing. The net distance between the top block and the stopper is 20 to 30 mm. The jacking bolt is matched with the threaded hole of the vertical section of the L-shaped top block. The nut end of the jacking bolt 2 is arranged between the vertical section of the stopper 1 and the vertical section of the L-shaped top block 3. The end of the horizontal section of the L-shaped top block 3 is in contact with the glass flake coating 4, and the end of the horizontal section of the L-shaped top block 3 is plastic-coated.
[0039] Among them, the L-shaped stopper 1 is a 120mm long machined L-shaped structure, and when welded to the surface of the carbon steel substrate 4, 4 to 6 welding points are sufficient; the L-shaped top block 3 is a 12mm wide machined L-shaped top block 3, and the contact surface with the glass flake coating 4 is plastic treated to avoid scratching the glass flake coating 4; the threaded hole opened on the vertical surface of the L-shaped top block 3 is an M16 threaded through hole, which matches the screw section of the M16 jacking bolt 2. When in use, the screw section of the jacking bolt 2 is retracted and supported by the stopper 1. Of course, the size of the L-shaped stopper and the L-shaped top block will be appropriately adjusted according to the requirements of the sampling specimen.
[0040] Another embodiment of the present invention:
[0041] A method for sampling an in-service glass flake anti-corrosion coating of a thermal power plant using a stripping device comprises the following steps:
[0042] S1, Select sampling sites: Select points on the front area scoured by flue gas or slurry where there are large color differences in the color of the scale coating 4 and rust marks on the surface. To meet the site conditions for sampling operations, there should be no protrusions or depressions at the sampling points. After selecting the sampling points, mark them with a marker pen. For each unit, at least 6 points should be selected in the glass flake anti-corrosion area.
[0043] S2, Separate the sampling specimen from the substrate: Use a scale template to draw a "day" - shaped area of 170 - 190 cm × 120 - 130 cm in the marked area. Use a handheld grooving machine to cut and groove along the marked area. Before grooving, use an ultrasonic thickness gauge to measure the thickness of the scale coating in the grooving area. The grooving depth is slightly less than the measured thickness by 50 - 100 μm. For example: If the scale coating at the sampling point is 2.5 mm thick, the grooving depth is 2.4 mm. The rotational speed of the grooving machine is about 50 - 100 revolutions per minute, the forward speed is 2 - 5 cm per minute, and the groove width is 5 mm. After grooving, use a handheld grinding wheel with the same width to grind the bottom of the groove at a low speed. The rotational speed of the grinding wheel of the grinding machine is 100 - 200 revolutions per minute, and grind off the scale primer to expose the natural color of the steel plate, as Figure 1 shown.
[0044] S3, Use a steel pick to铲除 the glass flakes in the area for fixing the instrument, and then use 200 - mesh sandpaper to grind out the natural color of the steel plate of the carbon steel body, separating a sampling area of the glass flake coating 4 with a size of 115 mm × 100 mm, as Figure 2 shown.
[0045] S4, Divide the glass flake specimens into strips. Use the same scribing and cutting method as in step 2 to divide the glass flake coating 4 in the sampling area into 10 - mm - wide strips, as Figure 3 shown.
[0046] S5, Fix the scale peeling device. According to the Figure 4 shown size and position, spot - weld the stop block 1 on the surface of the carbon steel substrate 5. The L - shaped stop block 1 is a machined angle steel with a length of 120 mm, a vertical section thickness of 12 mm, and a horizontal section thickness of 4 mm. 4 - 6 weld points are sufficient. The L - shaped top block 3 is a machined L - shaped top block 3 with a width of 12 mm. The contact surface with the glass flakes is plastic - coated, and a threaded through - hole of M16 is opened at the center of the vertical surface. The M16 screw is back - threaded and顶住 the stop block.
[0047] S6, Implement scale peeling. Use one hand to press the glass flakes with a wooden board to prevent the flakes from cracking under stress, and use an open - ended wrench with the other hand to back off the jacking bolt 2. When the jacking bolt 2 is stressed and retreats one to two thread pitches, the glass flake coating 4 can be peeled off. Therefore, back off the jacking bolt 2 with a moderate force to prevent the glass flakes from splashing instantaneously when peeling off.
[0048] S7, sampling area recovery. After sampling is completed according to the above method, the sampling surface is ground, chamfered, rust and weld nodules are removed, and two coats of primer are applied. After the surface is dry, the middle coat and top coat are applied according to the formula of the glass flake mortar manufacturer. The middle coat and top coat should cover the surrounding flake area.
[0049] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.
[0050] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A device for stripping anti-corrosion coatings on glass flakes in service in thermal power plants, characterized in that: It comprises an L-shaped stopper, an L-shaped top block and a jacking bolt, wherein the L-shaped stopper comprises a horizontal section and a vertical section for spot welding with the surface of a carbon steel substrate; the L-shaped top block also comprises a horizontal section and a vertical section, a threaded hole is arranged on the vertical section of the L-shaped top block, a nut end of the jacking bolt is arranged between the vertical section of the stopper and the vertical section of the L-shaped top block, and the end of the horizontal section of the L-shaped top block contacts the glass flake coating; The method for sampling the in-service glass flake anti-corrosion coating of a thermal power plant using the stripping device comprises the following steps: S1, select the sampling area and sampling point. The sampling area is selected in the area of the glass flakes that is directly washed by smoke or slurry. The sampling point is selected in the sampling area where the glass flake coating has a large color difference and rust marks on the surface, and the sampling point is flat without protrusions or pits. After selecting the sampling point, mark the number with a marker pen. There are no less than 6 sampling points in the glass flake anti-corrosion area of each unit; S2, a wide slot is opened on the sampling site to divide the sampling site into a sampling area and an instrument fixing area; S3, remove the glass flakes on the instrument fixing area, and then grind the area: before cutting and grooving along the scribed area, use an ultrasonic thickness gauge to measure the thickness of the flake coating in the grooved area, adjust the groove depth of the groover, and ensure that the groove depth is slightly smaller than the thickness of the flake coating in the grooved area; after cutting and grooving along the scribed area, use a handheld grinding wheel of the same width to grind the bottom of the groove at a low speed, with the grinding wheel speed of the grinder at 100-200 rpm, and grind off the glass flake primer to reveal the original color of the steel plate; S4, dividing the glass flake coating on the sampling area into a number of standard sample strips; S5, installing a scale stripping device in the instrument fixing area, the scale stripping device is in contact with the end of the sample; S6, use the flake stripping device to strip the sample strips from the sampling area one by one: first press the area of the glass flakes to be sampled and separated by hand to prevent the stripped flakes from being cracked and damaged by falling due to stress, and then use a ratchet wrench to rotate the jacking bolt to make the jacking bolt rotate to the side of the top block, and the nut end of the jacking bolt squeezes the vertical section of the block, and the block provides a reverse force to the jacking bolt. After the jacking bolt is stressed, it squeezes the L-shaped top block, and the horizontal section end of the L-shaped top block applies force to the glass flake coating, and the glass flake coating can be stripped.
2. The device for stripping the anti-corrosion coating of glass flakes in service in a thermal power plant according to claim 1 is characterized in that: The ends of the horizontal sections of the L-shaped top blocks are coated with plastic.
3. The device for stripping the anti-corrosion coating of glass flakes in service in a thermal power plant according to claim 2 is characterized in that: In step S2, a "sun"-shaped area is carved on the marked sampling site, wherein the "sun"-shaped area is divided into a sampling area and an instrument fixing area.
4. The device for stripping the anti-corrosion coating of glass flakes in service in a thermal power plant according to claim 3 is characterized in that: Step S4 specifically involves first removing the glass flakes in a fixed area and grinding until the original color of the steel plate is exposed; then opening a plurality of parallel strip grooves on the surface of the glass flake coating in the sampling area, determining the specifications of the strip grooves according to the test requirements, and dividing the glass flake coating into a number of parallel arranged splines.
5. The device for stripping the anti-corrosion coating of glass flakes in service in a thermal power plant according to claim 4 is characterized in that: In step S5, a fixed stopper is spot-welded on the surface of the polished carbon steel substrate in the fixed area of the instrument, and the position of the stopper is pre-marked and positioned according to the sampling requirements; then the screw section of the jacking bolt is installed into the threaded hole on the vertical section of the L-shaped top block, and then the L-shaped top block of the stripping device is placed on the surface of the carbon steel substrate, ensuring that the vertical section of the L-shaped top block is opposite to the vertical section of the stopper, and the end of the horizontal section of the L-shaped top block is in contact with the spline end of the glass flake coating.
6. The device for stripping the anti-corrosion coating of glass flakes in service in a thermal power plant according to claim 5, characterized in that: It also includes step S7, the sampling area is restored; after the sampling is completed, the surface of the sampling area is polished to remove rust and weld nodules, two coats of primer are applied, and after the surface is dry, the middle coat and the top coat are applied, and the middle coat and the top coat cover the surrounding adjacent glass flake coating areas.
Citation Information
Patent Citations
An impact-resistant anti-corrosion coating
CN102277066A
Preparation method of lamellar powder having coating layer provided to surface of the powder, and thickness measuring method of coating layer using the powder
JP2008203001A