Flexible Cover Window

By forming an elastic buffer layer on the rear surface of the window substrate of the flexible display, absorbing the slight deformation of the folded part, the problem of layering or buckling in the prior art is solved, extending the service life and adapting to the needs of various folding methods.

CN114822241BActive Publication Date: 2024-11-05UTI INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210101592.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2021-01-28
Filing Date
2022-01-27
Publication Date
2024-11-05
Estimated Expiration
2042-01-27

AI Technical Summary

Technical Problem

The cover windows of existing flexible displays are prone to layering or buckling when folded repeatedly, resulting in screen distortion and shortening of service life. The choice of material thickness and hardness is limited, making it difficult to meet the strength characteristics of various folding methods.

Method used

The elastic buffer layer is formed on the rear surface of the window substrate, absorbing the micro-deformation of the folded part through the design of a single structure or multi-layer structure, reducing the elongation difference between the window substrate and the display panel, preventing layering or buckling, and improving resistance Impactness.

Benefits of technology

It extends the service life of the cover window, reduces screen distortion in the folded part, reduces the limitations of material thickness and hardness, is suitable for flexible displays in various folding modes, and improves impact resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114822241B_ABST
    Figure CN114822241B_ABST
Patent Text Reader

Abstract

A flexible cover window is proposed, which includes a window substrate and an elastic buffer layer having a single-layer structure or a multi-layer structure. The elastic buffer layer is provided on the rear surface of the window substrate to absorb deformation occurring in the folding portion. The flexible cover window is a glass-based cover window for protecting a foldable, rollable, slidable or stretchable flexible display. In addition, the flexible cover window has an elastic buffer layer on the rear surface of the window substrate to reduce the elongation difference between the window substrate and the display panel, so that delamination or buckling due to micro-deformation at the folding portion of the flexible cover window can be prevented. Therefore, the service life of the flexible cover window is extended and image distortion on the screen at the folding portion can be prevented.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS

[0002] This application claims priority to Korean Patent Application No. 10-2021-0012012, filed on January 28, 2021, which is hereby incorporated by reference in its entirety for all purposes. Technical Field

[0003] The present disclosure relates to a flexible cover window, and more particularly to a flexible cover window having an elastic buffer layer on a rear surface of a substrate thereof to absorb micro deformation occurring in a folded portion to prevent delamination or buckling in the folded portion. Background Art

[0004] In recent years, electrical and electronic technologies have developed rapidly, and various types of display products have emerged to meet the needs of the new era and the demands of various types of consumers.

[0005] In the case of flexible displays, research is being conducted on displays that can be bent, rolled, and stretched from a folded state. A cover window for protecting a display panel as well as the display panel should be formed to be flexible.

[0006] Such a flexible cover window should have good flexibility, and should not produce marks on the folded portion even when folded repeatedly, and should not have distortion in image quality.

[0007] For existing cover windows of flexible displays, polymer films such as PI or PET have been used on the surface of the display panel.

[0008] However, in the case of a polymer film, the polymer film is used only to prevent scratches on a display panel due to its weak mechanical strength, is weak in impact resistance, has low transmittance, and is known to be relatively expensive.

[0009] In addition, in the case of such a polymer film, as the number of folding times of the display increases, marks are left on the folded portion, resulting in damage to the folded portion. For example, during the evaluation of the folding limit (usually 200,000 times), the polymer film may be squeezed or torn.

[0010] Recently, in order to overcome the limitations of cover windows having polymer films, various studies have been conducted on glass-based cover windows.

[0011] Such a glass-based cover window needs to have physical properties that satisfy folding characteristics, not cause screen distortion, and have sufficient strength even under repeated contact and pressure by a touch pen or the like.

[0012] Recently, as consumer demand for flexible displays in various folding modes such as foldable, rollable, slidable and stretchable modes increases, research is actively being conducted. Attention is also focused on research on cover windows for protecting such display (OLED) panels.

[0013] In the case of polymer films such as CPI or PET or glass as materials of existing cover windows, when folded repeatedly, delamination or buckling phenomena often occur depending on the difference in elongation of the folded parts, such as Figure 1 and Figure 2 as shown in .

[0014] When the cover window is thicker or has a higher hardness, this phenomenon will be more serious. Therefore, when selecting the material of the cover window, the thickness and hardness of the cover window are limited.

[0015] That is, when the cover window is relatively thin, the deformation during bending is small, and thus the above-mentioned delamination or buckling phenomenon does not occur much. However, as the thickness of the cover window increases and the hardness increases, the deformation during folding increases, making the cover window difficult to apply.

[0016] Additionally, regardless of the material covering the window, delamination or buckling issues are more likely to occur as the number of folds increases.

[0017] As described above, there is a need to study a cover window that does not distort the screen while solving the deformation problem in the folded portion and satisfying strength characteristics and folding characteristics for various folding methods for a flexible display. Summary of the invention

[0018] An object of the present disclosure is to provide a flexible cover window which forms an elastic buffer layer on a rear surface of a window substrate to absorb micro deformation occurring in a folded portion so that there is no delamination or buckling in the folded portion.

[0019] In order to achieve the above-mentioned purpose, the technical point of the present disclosure is to provide a flexible cover window, characterized in that the flexible cover window includes an elastic buffer layer formed on a window substrate and a rear surface of the window substrate in a single structure or a multi-layer structure to absorb deformation occurring in a folded portion.

[0020] In addition, when the elastic buffer layer is formed in a single structure, it is preferred that the elastic buffer layer is sequentially formed as an upper adhesive layer, an elastic film layer at a lower portion of the upper adhesive layer, and a lower adhesive layer at a lower portion of the elastic film layer.

[0021] In addition, when the elastic buffer layer is formed in a multi-layer structure, preferably, an upper adhesive layer, a plurality of elastic film layers formed in a laminated structure through an intermediate adhesive layer below the upper adhesive layer, and a lower adhesive layer located below the elastic film layer laminated structure are sequentially formed.

[0022] In addition, the elastic film layer may preferably be any one of an elastic polyurethane (EPU) film, a thermoplastic polyurethane (TPU) film, and a polyolefin (PO) film.

[0023] In addition, for the upper adhesive layer and the lower adhesive layer, an optically clear adhesive (OCA) or an optically clear resin (OCR) is preferably used.

[0024] In addition, the thickness of the elastic film layer is preferably 25 μm to 150 μm, and the thickness of the upper adhesive layer and the lower adhesive layer is preferably 10 μm to 150 μm.

[0025] In addition, the window substrate is preferably a polymer film or glass, and the window substrate has a thickness of 30 μm to 400 μm, and a CPI film or a PET film may be used.

[0026] Here, the flexible cover window may be laminated on the upper side of a flexible display panel in which a CPI film or a PET film is attached to the front surface, or the flexible cover window is laminated on the upper side of a flexible display panel in which a CPI film or a PET film is attached to the front surface and an AF coating is formed on the upper layer of the CPI film or the PET film. Preferably, a functional layer is formed on the front surface of the window substrate.

[0027] In addition, in the flexible cover window, preferably, a CPI film or a PET film is formed on the front surface of the window substrate, and preferably, a functional layer is formed on the front surface of the CPI film or the PET film.

[0028] The present disclosure relates to a cover window for protecting a flexible display. The present disclosure provides a glass-based cover window for protecting a flexible display in a foldable, rollable, slidable and stretchable manner.

[0029] In particular, by forming an elastic buffer layer on the rear surface of the window substrate, the elongation difference between the window substrate and the display panel is alleviated to prevent delamination or buckling in the folding portion, thereby improving the service life of the cover window and minimizing screen distortion in the folding portion.

[0030] In addition, the present disclosure minimizes restrictions on the material, thickness, and hardness of the window substrate by forming an elastic buffer layer on the rear surface of the window substrate, so that window substrates made of various materials can be used according to the folding method or product specifications of the flexible display.

[0031] In addition, the present disclosure is implemented as a composite material formed of glass and a resin material to enhance the flexibility, resilience, elasticity, and strength characteristics of the resin material while maintaining the texture of the glass as much as possible. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] Figure 1 and Figure 2 is a schematic diagram showing a lifting and buckling phenomenon in a folding portion of a conventional flexible cover window;

[0033] Figure 3 is a schematic diagram of a flexible cover window according to an embodiment of the present disclosure;

[0034] Figure 4 It shows that Figure 3 A schematic diagram of an example of applying an embodiment of the present invention to a flexible display panel;

[0035] Figure 5 is a schematic diagram of a flexible cover window according to another embodiment of the present disclosure;

[0036] Figure 6 is a schematic diagram of a flexible cover window according to another embodiment of the present disclosure; and

[0037] Figure 7 It shows that Figure 6 Schematic diagram of an example of an embodiment of the present invention being applied to a flexible display panel. DETAILED DESCRIPTION

[0038] The present disclosure relates to a cover window for protecting a flexible display and a glass-based cover window for protecting a flexible display in a foldable, rollable, slidable and stretchable manner.

[0039] In particular, the present disclosure improves the service life of the cover window and minimizes screen distortion at the folding portion by forming an elastic buffer layer on the rear surface of the window substrate to prevent delamination or buckling at the folding portion due to micro-deformation caused by the elongation difference between the glass substrate and the display panel.

[0040] In addition, by forming an elastic buffer layer on the rear surface of the window substrate, restrictions on the material, thickness, and hardness of the window substrate can be minimized, and window substrates made of various materials can be used according to the folding method or product specifications of the flexible display.

[0041] In addition, by forming an elastic buffer layer on the rear surface of the window substrate, impact resistance is improved by absorbing and dispersing impact force such as a pen drop, and a flexible cover window with ensured strength characteristics and folding characteristics is provided.

[0042] Hereinafter, the present disclosure will be described in detail with reference to the accompanying drawings. Figure 3 is a schematic diagram of a flexible cover window according to an embodiment of the present disclosure, Figure 4 It shows that Figure 3 A schematic diagram of an example of an embodiment of the present invention being applied to a flexible display panel, Figure 5 is a schematic diagram of a flexible cover window according to another embodiment of the present disclosure, Figure 6 is a schematic diagram of a flexible cover window according to another embodiment of the present disclosure, and Figure 7 It shows that Figure 6 Schematic diagram of an example of an embodiment of the present invention being applied to a flexible display panel.

[0043] As shown, the flexible cover window according to the present disclosure includes a window substrate 100 and an elastic buffer layer 200 formed on a rear surface of the window substrate 100 in a single structure or a multi-layer structure to absorb deformation generated by a folded portion.

[0044] In the present disclosure, the term "front surface" refers to a surface that a user can touch, and refers to a surface that a touch pen or the like contacts, and refers to a surface facing upward in the drawings. In addition, the "rear surface" in the present disclosure refers to a surface opposite to the touch surface, that is, a surface in a direction toward the display panel, and refers to a surface in a downward direction in the drawings.

[0045] According to the present disclosure, the cover window is used to protect the flexible display panel 10 in a foldable, rollable, slidable and stretchable manner. The cover window is laminated (attached) on the front surface of the flexible display panel 10.

[0046] A region of the cover window corresponding to the folded or rolled portion of the flexible display panel 10 is referred to as a folded portion, and a region other than the folded portion is referred to as a planar portion.

[0047] As the window substrate 100 in the present disclosure, a polymer film or glass may be used. The thickness of the window substrate 100 is preferably 30 μm to 400 μm.

[0048] In the case of a polymer film, any transparent material may be used, and a thick polymer film of 40 μm or more or a hard plastic film may be applied. For example, a CPI film or a PET film may also be used as the flexible cover window according to the present disclosure.

[0049] Previously, in order to be adopted as a cover window for various folding types (foldable, rollable, slidable and stretchable), both folding characteristics and hardness characteristics must be satisfied, so their application on thick or hard materials is limited. As mentioned above, delamination or buckling occurs at the folding portion, or the folding and strength characteristics are deteriorated.

[0050] In the present disclosure, by forming the elastic buffer layer 200 on the rear surface of the window substrate 100, the restrictions on the material, thickness and hardness of the window substrate can be minimized, and the window substrate made of various materials can be used according to the folding method or product specifications of the flexible display. Therefore, the restrictions on material selection can be minimized.

[0051] In the present disclosure, a glass substrate is used as an embodiment of a window substrate, and the following description will focus on this.

[0052] In one embodiment of the present disclosure, the glass substrate 100 may be formed to have a uniform thickness in all regions of the plane portion, and the folded portion or folded portion may be formed to be thinner than the plane portion by thinning. In this case, generally speaking, the thickness of the plane portion of the glass substrate 100 is 30 μm to 400 μm, and the thickness of the folded portion is about 10 μm to 100 μm, and the folded portion is formed by processing a very thin glass plate. The glass substrate 100 in the present disclosure is enhanced in strength by performing a chemical strengthening process.

[0053] The glass substrate in the present disclosure is formed on the front surface of the display panel 10 to protect the display panel 10 by maintaining folding and strength characteristics, and may also be disposed on a transparent polyimide (CPI) film cover for protecting the CPI film.

[0054] As shown in the figures, the present disclosure includes a glass substrate 100 and an elastic buffer layer 200 formed on a rear surface of the glass substrate 100 in a single structure or a multi-layer structure to absorb deformation generated by a folded portion.

[0055] In particular, the present disclosure improves the service life of the cover window and minimizes distortion of the screen at the folded portion by forming an elastic buffer layer 200 on the rear surface of the window substrate 100 to prevent delamination or buckling at the folded portion due to micro-deformation caused by the elongation difference between the glass substrate 100 and the display panel 10.

[0056] In addition, by forming the elastic buffer layer 200 on the back surface of the glass substrate 100, impact resistance is improved by absorbing and dispersing impact force such as a pen drop, and a flexible cover window having ensured strength characteristics and folding characteristics is provided.

[0057] Conventionally, cumbersome operations such as a mask process or an etching process have been performed to form a special pattern or a folding portion (F) on the glass substrate 100 in order to improve strength characteristics and folding characteristics. However, by controlling the material, thickness, and physical properties of the elastic buffer layer 200 to disperse and absorb impact force, the process can be simplified without the above cumbersome work.

[0058] Generally speaking, when an impact such as a pen drop acts on the cover window, the impact force transmitted vertically is stronger than the impact force transmitted horizontally. According to the present disclosure, the elastic buffer layer 200 is formed on the rear surface of the glass substrate 100 to effectively disperse or absorb the vertical impact force and to hold the glass substrate 100, thereby improving the pen drop characteristics.

[0059] According to the display or product specifications and folding methods, the elastic buffer layer 200 can be formed in a single structure or a multi-layer structure.

[0060] Figure 3 A case is shown in which the elastic buffer layer 200 is formed in a single structure.

[0061] When the elastic buffer layer 200 is formed in a single structure, the elastic buffer layer 220 is sequentially formed as an upper adhesive layer 210, an elastic film layer 220 at a lower portion of the upper adhesive layer 210, and a lower adhesive layer 230 at a lower portion of the elastic film.

[0062] That is, the adhesive layer is formed on both surfaces of the elastic film layer 220 to be laminated on the rear surface of the glass substrate 100 and attached to the front surface of the display panel 10 to reduce the elongation difference between the glass substrate 100 and the display panel 10, thereby preventing delamination or buckling at the folded portion.

[0063] The upper adhesive layer 210 fixes the glass substrate 100 and the elastic film layer 220 , the lower adhesive layer 230 fixes the display panel 10 and the elastic film layer 220 , and the elastic film layer 220 is used to mitigate the elongation difference between the flexible cover window and the display panel 10 .

[0064] In a conventional manner, when a cover window formed of a glass substrate 100 is laminated with an adhesive layer without an elastic buffer layer 200 structure, micro deformation occurs due to a difference in elongation between an upper structure or a lower structure in the folded portion, thereby easily causing delamination or buckling in the folded portion.

[0065] In the present disclosure, by forming an adhesive layer on both sides of the elastic film layer 220 to realize the elastic buffer layer 200, and laminating the elastic buffer layer between the glass substrate 100 and the display panel 10, the elongation difference between the display panel 10 and the glass substrate 100 is alleviated, thereby eliminating delamination or buckling of the glass substrate 100 in the folded portion.

[0066] As the elastic film layer 220 , any material in the form of a transparent and elastic film may be used, and in an embodiment of the present disclosure, an elastic polyurethane (EPU) film, a thermoplastic polyurethane (TPU) film, and a polyolefin (PO) film may be used.

[0067] According to an embodiment of the present disclosure, the thickness of the elastic film layer 220 is preferably 25 μm to 150 μm, more preferably 50 μm to 100 μm. When the thickness is thinner than the above thickness range, the buffering function of elongation and the impact force absorption function are insufficient. When the thickness is thicker than the above thickness range, the thickness of the cover window may become thicker, and the folding characteristics may be reduced.

[0068] The following table shows an example of elastic properties of the elastic film layer 220 , and is physical property data that can mitigate the difference in elongation between the thin glass substrate 100 and the display panel 10 .

[0069]

[0070]

[0071] In addition, the surface of the elastic film layer 220 is subjected to plasma surface treatment or the like to improve wettability of the surface of the elastic film layer 220 , thereby improving coating performance of the adhesive layer on the surface of the elastic film layer 220 and enabling uniform and precise coating.

[0072] For the upper adhesive layer and the lower adhesive layer in the present disclosure, an optically clear adhesive (OCA) or an optically clear resin (OCR) can be used, which is a transparent resin having a refractive index almost equal to that of glass 1.5, and for example, acrylic, epoxy resin, silicone resin, urethane, urethane composite material, urethane acrylic composite material, mixed sol-gel, silicone composite material, etc. can be used.

[0073] The thickness of the upper and lower adhesive layers is preferably 10 μm to 150 μm, the thickness of the upper adhesive layer 210 is more preferably 25 μm to 75 μm, and the thickness of the lower adhesive layer 230 is more preferably 10 μm to 50 μm.

[0074] If the thickness is thinner than the above thickness, the fixing effect of the adhesive may be deteriorated, and if the thickness is thicker than the above thickness, the folding property and transparency may be deteriorated, or the adhesive force may be wasted without improvement.

[0075] like Figure 4 As shown in , the flexible cover window can be laminated on the upper side of the flexible display panel 10 in which the existing CPI film or PET film 20 is attached to the front side, or the flexible cover window can be laminated on the flexible display panel 10 in which the CPI film or PET film 20 is attached to the front surface and the AF coating is formed on the upper layer of the CPI film or PET film 20.

[0076] In this case, a functional layer may be formed on the front surface of the glass substrate 100. The functional layer may enhance the anti-scattering function and surface scratch resistance (3H) of the glass substrate 100, and the thickness of the functional layer is suitably about 2 μm to 20 μm.

[0077] A transparent resin having a refractive index almost the same as that of glass (1.5), such as an optically clear resin (OCR), can be used as a functional layer, and for example, acrylic, epoxy resin, silicone resin, urethane, urethane composite material, urethane acrylic composite material, mixed sol-gel and silicone, etc. can be used.

[0078] In addition, the functional layer may be implemented by providing an anti-fingerprint (AF) function or an anti-reflection (AR) function, synthesizing a resin having such a function, or forming various patterns, for example, forming a pattern such as a moth eye.

[0079] In another embodiment of the present disclosure, Figure 5 As shown in , when the elastic buffer layer 200 is formed in a multi-layer structure, the upper adhesive layer 210 is formed in the upper part of the elastic buffer layer 200, a plurality of elastic film layers 221, 222 are formed in a laminated structure through the middle adhesive layer 240 below the upper adhesive layer 210, and the lower adhesive layer 230 is formed in the lower part of the elastic film layer laminated structure.

[0080] When the elastic buffer layer 200 is formed in a multi-layer structure, the plurality of elastic film layers may be formed of the same material, the same hardness, and the same thickness. According to the folding method or product specifications of the display, the plurality of elastic film layers may be formed to have a lower elongation (elasticity) when the plurality of elastic film layers are closer to the glass substrate (folded inward), or to have a higher elongation (elasticity) when the plurality of elastic film layers are closer to the glass substrate (folded outward).

[0081] Therefore, a laminated structure including the same or different elastic film layers is implemented according to various folding methods of the display, thereby alleviating the elongation difference in the folded portion and minimizing defects such as delamination or buckling in the folded portion.

[0082] In this disclosure, Figure 6 As shown in , a CPI film or a PET film 20 may be formed on the front surface of a glass substrate 100 , and a functional layer 300 may be formed on the front surface of the CPI film or the PET film 20 .

[0083] In this case, if Figure 7 As shown in FIG. 1 , the protective CPI film or PET film 20 formed on the front surface of the conventional flexible display panel 10 is omitted, and the CPI film or PET film 20 is formed on the front surface of the glass substrate 100, and thereafter, a functional layer may be formed as needed.

[0084] According to the present disclosure, the cover window is directly laminated on the flexible display panel 10. A CPI film or a PET film 20 is formed on the cover window, and then a functional layer 300 is formed as needed.

[0085] Therefore, the present disclosure relates to a cover window for protecting a flexible display, and provides a cover window for protecting a flexible display in a foldable, rollable, slidable, and stretchable manner.

[0086] In particular, by forming an elastic buffer layer on the rear surface of the window substrate, the elongation difference between the window substrate and the display panel is alleviated to prevent delamination or buckling in the folding part, thereby improving the service life of the cover window and minimizing screen distortion in the folding part.

[0087] In addition, by forming an elastic buffer layer on the rear surface of the window substrate, impact resistance is improved by absorbing and dispersing impact force such as a pen falling, and a flexible cover window having ensured strength characteristics and folding characteristics is provided.

[0088] In addition, the present disclosure minimizes restrictions on the material, thickness, and hardness of the window substrate by forming an elastic buffer layer on the rear surface of the window substrate, so that a window substrate made of various materials can be used according to the folding method or product specifications of the flexible display. Therefore, restrictions on material selection can be minimized.

[0089] In addition, in an embodiment of the present disclosure, when the window substrate is used as glass, the present disclosure is implemented as a composite material formed of glass and a resin material to enhance the flexibility, resilience, elasticity and strength characteristics of the resin material while maintaining the texture of the glass as much as possible.

Claims

1. A flexible cover window, comprising: Window substrate; as well as an elastic buffer layer, the elastic buffer layer being disposed on the rear surface of the window substrate, the elastic buffer layer playing a role of absorbing deformation occurring in the folded portion, Wherein, the elastic buffer layer includes the following structure (A) or structure (B): (A) an upper adhesive layer; an elastic film layer, the elastic film layer being disposed below the upper adhesive layer; and a lower adhesive layer, the lower adhesive layer being disposed below the elastic film layer; or (B) an upper adhesive layer above the laminate; the laminate comprising a first elastic film layer above the intermediate adhesive layer and a second elastic film layer below the intermediate adhesive layer; and a lower adhesive layer disposed below the laminate, The elastic film layer of configuration (A) and the first elastic film layer and the second elastic film layer of configuration (B) have a Young's modulus of 2.0 to 5.0 MPa and a haze of less than 3.0%.

2. The flexible cover window according to claim 1, wherein: The elastic film layer of construction (A) is selected from any one of an elastic polyurethane (EPU) film, a thermoplastic polyurethane (TPU) film, and a polyolefin (PO) film.

3. The flexible cover window according to claim 1, wherein: The first elastic film layer and the second elastic film layer of configuration (B) are respectively selected from any one of an elastic polyurethane (EPU) film, a thermoplastic polyurethane (TPU) film, and a polyolefin (PO) film.

4. The flexible cover window according to claim 1, wherein: In configuration (A), the upper adhesive layer and the lower adhesive layer are respectively selected from an optically clear adhesive (OCA) or an optically clear resin (OCR).

5. The flexible cover window according to claim 1, wherein: In configuration (B), the upper adhesive layer and the lower adhesive layer are respectively selected from an optically clear adhesive (OCA) or an optically clear resin (OCR).

6. The flexible cover window according to claim 1, wherein: In configuration (A), the elastic film layer has a thickness of 25 μm to 150 μm.

7. The flexible cover window according to claim 1, wherein: In configuration (B), the first elastic film layer and the second elastic film layer each have a thickness of 25 μm to 150 μm.

8. The flexible cover window according to claim 1, wherein: In configuration (A), the upper adhesive layer and the lower adhesive layer each have a thickness of 10 μm to 150 μm.

9. The flexible cover window according to claim 1, wherein: In configuration (B), the upper adhesive layer and the lower adhesive layer each have a thickness of 10 μm to 150 μm.

10. The flexible cover window according to claim 1, wherein: The window substrate is made of a polymer film or glass.

11. The flexible cover window according to claim 10, wherein: The window substrate has a thickness of 30 μm to 400 μm.

12. The flexible cover window according to claim 10, wherein: The polymer film is a CPI film or a PET film.

13. The flexible cover window according to claim 1, wherein: The flexible cover window is applied on the upper surface of the flexible display panel where a CPI film or a PET film is attached to the front surface of the flexible display panel, or the flexible cover window is applied on the upper surface of the flexible display panel where a CPI film or a PET film is attached to the front surface of the flexible display panel and an anti-fingerprint (AF) coating is provided on the upper surface of the CPI film or the PET film. 14 . The flexible cover window of claim 13 , further comprising a functional layer on a front surface of the flexible cover window. 15 . The flexible cover window of claim 1 , further comprising a CPI film or a PET film on a front surface of the flexible cover window. 16 . The flexible cover window of claim 15 , further comprising a functional layer disposed on a front surface of the CPI film or the PET film.