Method and device for deforming metal composite foil

By using multiple plate holders and molds to move in precise directions in the molding equipment, the problems of springback and material thinning during the deformation and molding process of metal composite foils are solved, achieving efficient and low-cost deformation molding, ensuring Improve the safety and energy density of battery cells.

CN114850300BActive Publication Date: 2024-10-18POWERCO SE
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202210092693.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-01-26
Publication Date
2024-10-18
Estimated Expiration
2042-01-26

AI Technical Summary

Technical Problem

In the existing technology, there are problems such as springback, cracks and material thinning during the deformation and molding process of metal composite foils for manufacturing battery cells, which results in high manufacturing costs, long time and affects battery safety.

Method used

A forming equipment and method are used to hold the metal composite foil through multiple sheet holders and molds and deform it at room temperature through precise directional movement and clamping mechanisms to avoid springback and ensure shape accuracy and material stability .

Benefits of technology

It achieves precise deformation and shaping of metal composite foils in a short time and at low cost, avoiding springback, cracks and material thinning, ensuring reliable coating and high energy density of battery cells.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114850300B_ABST
    Figure CN114850300B_ABST
Patent Text Reader

Abstract

The present invention relates to a method for deforming a metal composite foil (7) for a battery cell (33), the method comprising at least the following steps: a) placing the metal composite foil (7) in a forming device (1), the forming device having a plurality of sheet metal holders (2, 11), a plurality of dies (3, 10) and a first punch (4); b) fixing a first fixing area (13) of the metal composite foil (7) by closing the first sheet metal holder (3) and the first die (3); c) fixing a second fixing area (14) of the metal composite foil (7) by closing a second sheet metal holder (11) and a second die (10); d) deforming the second fixing area (14) at least partially along a first direction (16) by moving the second sheet metal holder (11) and the second die (10); and e) deforming a deformation area (15) at least partially along a second direction (19) by moving the punch (4). Furthermore, a forming device (1) is proposed for deforming a metal composite foil (7) for a battery cell.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for deforming a metal composite foil for a battery cell and a battery cell manufactured according to the method. In addition, the present invention also relates to a forming device for deforming a metal composite foil for a battery cell. Background Art

[0002] In order to manufacture battery cells, it is necessary to shape the metal composite foil so that it can form a storage space for a single cell stack structure with a high electrical storage density. In the prior art, for example, so-called pouch foils are known for this purpose, which are made of a composite composed of aluminum and plastic by deformation forming. Here, at least one aluminum layer is connected to other flexible plastic layers to form a pouch foil. However, such aluminum laminated foils sometimes have very poor deep-drawing properties, so that cracks and wrinkles are always generated when the metal composite foil is deformed. In particular, a very large degree of rebound is always observed after the deformation forming process. This is critical because the battery cell composed of electrodes and separators must be continuously and reliably coated, but damage to the coated pouch foil always occurs in highly stressed, i.e., strongly deformed areas.

[0003] Furthermore, today's high-capacity battery cells require the maximum possible number of electrodes to be arranged in a corresponding cell stack of the battery cells, which electrodes are then jointly coated with a metal composite foil. For this purpose, the metal composite foil must be deformed as deeply as possible. However, the deeper the metal composite foil is deformed, the greater the material thinning in critical areas, which can lead to damage.

[0004] If the metal composite foil is deformed using conventional deformation dies, material thinning occurs, in particular in the punch radius and at the webs provided in the die. Such critical areas often lead to cracks in the metal composite foil in these areas of the sheathing and thus threaten the operational safety of the battery cell.

[0005] Therefore, various methods are known from the prior art for deforming metal composite foils. One method is deep-drawing the foil with the aid of a punch. The punch deforms the metal composite foil in the direction of a mold, wherein the desired final shape of the metal composite foil is formed as a negative mold in the mold.

[0006] Three measures are known so far for avoiding springback after deformation forming. The first measure is to connect the two formed metal composite foils to each other by heat input immediately after deformation forming. This is usually achieved by melting. Another measure is to heat the metal composite foil to a temperature of, for example, 80°C during deformation forming in order to reduce the springback after deformation forming by this heat input. However, this is very costly and energy-intensive and slows down the manufacturing process due to the duration required for heat input. As a third measure, the aluminum content of the metal composite foil can be increased, which can be achieved by using a relatively large aluminum foil with a wall thickness of, for example, more than 80 (micrometers or μm). However, this requires the use of a larger amount of relatively expensive aluminum, thereby increasing material costs, the volume and weight of the metal composite foil.

[0007] The solutions known to date have various disadvantages, since they increase the production costs, extend the production time or make the metal composite foil unnecessarily larger or heavier. Summary of the invention

[0008] The technical problem to be solved by the present invention is to at least partially solve the problems arising from the prior art. In particular, a method for processing a metal composite foil should be provided, by which the metal composite foil can be precisely deformed and shaped without springback. At the same time, the process costs and processing time should be reduced. In addition, it should be ensured that the metal composite foil of the finished battery cell does not develop cracks, wrinkles or other damage.

[0009] The technical problem is solved according to the invention by a method for deforming a metal composite foil for a battery cell and a forming device for deforming a metal composite foil for a battery cell. The individual features mentioned in the description can be combined with one another in a technically meaningful manner and can be supplemented by explanatory facts in the description and / or details in the drawings, which show further variant embodiments of the invention.

[0010] A method for producing a metal composite foil for a battery cell is proposed, the method comprising at least the following steps:

[0011] a) placing the metal composite foil in a forming device, the forming device having a plurality of sheet material holders, a plurality of dies and a first punch;

[0012] b) fixing a first fixing region of the metal composite foil by closing a first sheet material holder and a first mold;

[0013] c) fixing the second fixing region of the metal composite foil by closing the second sheet material holder and the second mold;

[0014] d) deforming the second fixing region at least partially in a first direction by moving the second sheet material holder and the second mold;

[0015] e) deforming the deformation region at least partially along a second direction by moving the punch.

[0016] The steps are preferably carried out in the stated order a), b), c), d), e), without it being necessary for the steps to be carried out immediately (directly) one after the other.

[0017] In step a), the metal composite foil is first placed in a forming device. For this purpose, the forming device has a plurality of sheet metal holders and a plurality of molds as well as a first punch.

[0018] In step b), a first fixing region of the metal composite foil is fixed in the forming device by bringing the first sheet metal holder and the first mold closer together. The mutual approach closes the forming device, in particular the first sheet metal holder and the opposing first mold. The first holding region is a region of the metal composite foil which is in direct contact with the first sheet metal holder and the first mold and is fixed by them by clamping (in particular frictional engagement). This fixing is necessary because otherwise the metal composite foil cannot be reliably held in the forming device during the deep-drawing process.

[0019] Step c) provides for fixing the second fixing region of the metal composite foil by closing the second sheet metal holder and the second mold. This is also achieved by the second sheet metal holder and the second mold (correspondingly) being brought closer to each other. The second fixing region is preferably arranged within the first fixing region.

[0020] In step d), the second fixing region is at least partially deformed in the first direction by moving the second sheet metal holder and the second die. For this purpose, the second sheet metal holder and the second die are preferably moved together or simultaneously, so that the fixation of the second fixing region between the two sections is maintained during the deformation process. The first direction is in particular selected in this case so that the two sections are moved in the direction of the first die, wherein the second die moved in this way moves relative to the first die like a second punch. The metal composite foil can be deformed by stretching between the first die and the second die acting as a second punch. If necessary, the second fixing region or a sub-region of the second fixing region can be deformed at the same time. During this deformation, the metal composite foil is stretched in the region between the first and second fixing regions, while in the second deformation region, the metal composite foil is not stretched due to the clamping there.

[0021] In step e), at least a partial deformation of the deformation region is achieved by moving the first punch in the second direction. The deformation region is preferably arranged within the second fixing region and the deformation of the deformation region is selected so that the metal composite foil has a desired shape after being removed from the deformation forming device and after springing back. For this purpose, it is advantageous if the second direction is at least approximately selected so that it is oriented opposite to the first direction. However, larger tolerances in the angular deviation range of, for example, plus or minus 20° to 30° can occur without impairing the invention.

[0022] In particular in the case of applications in which, for reasons of deformation technology, it is not yet desirable to fix the second fixing region by means of the second mold during the deformation, provision can be made for step c) to be carried out after step d).

[0023] The method can be carried out in particular at room temperature. This makes it possible to dispense with a heating device and thus, on the one hand, save costs for the necessary heating energy and, on the other hand, to carry out the deformation forming with particularly short cycle times. Therefore, these cycle times alone can already be made shorter, since no time has to be spent on heating the metal composite foil.

[0024] In particular, it can also be provided that the metal composite foil is at least partially deformed at an angle relative to the extrusion plane on the end face of the second sheet metal holder in the second fixing area. The end face of the second sheet metal holder is here a face that points in the direction of the approaching movement and is in contact with the metal composite foil in order to fix the metal composite foil by clamping. In addition, the extrusion plane is a plane oriented perpendicular to the second direction. If the metal composite foil to be processed has a very large degree of springback, it can be provided that not only a deformation is provided in the deformation area to compensate for the expected springback, but that the second fixing area is also deformed and formed at an angle of, for example, 0°-20° relative to the extrusion plane. The deformation and forming both in the second fixing area and in the deformation area makes it possible to accurately and dimensionally stably process metal composite foils with a large degree of springback characteristics.

[0025] In particular, it can be provided that a holding force is generated in the second fixing region by the second sheet metal holder, which is greater than the tensile force generated by the punch in the deformation region, thereby ensuring that the metal composite foil is securely held in the second fixing region and cannot be moved in an uncontrolled manner, for example by the tensile force generated by the punch.

[0026] It is also advantageous that in the forming device at least during the deformation forming at least the area of ​​the mold that is respectively located behind the metal composite foil in the deformation direction is ventilated. This allows for shorter cycle times for the deformation forming process without having to wait for the ventilation of the mold that would otherwise be required.

[0027] Aluminum composite foils are particularly suitable as metal composite foils, which can be used very well as bag foils. Such aluminum composite foils are already available on the market today and in principle have good properties with regard to durability and accommodation of battery cells. However, this presupposes that damage to the composite foil is avoided during the deep-drawing process, as can be achieved with the invention.

[0028] For this purpose, in particular, metal composite foils with a foil thickness of between 120 μm (micrometers) and 180 μm can be used. Such foils have the required strength and can also be deformed by means of the proposed deep-drawing process. The invention can in principle be implemented with different foil thicknesses, and a particular advantage of the method is that metal composite foils with thin aluminum layers of less than 60 μm (micrometers) or less than 40 μm can also be deformed, while at the same time springback is eliminated or only minimally occurs. This makes it possible to save relatively expensive aluminum during the production process.

[0029] Battery cells with metal composite foils processed in a shaped manner according to the above-described method can thus be produced particularly advantageously. The advantage of the invention is that the metal composite foils shaped in this way are very precise in shape due to the avoidance of spring-back and are free of damage, such as material thinning or cracks. The metal composite foils produced in this way ensure a reliable and permanent covering of the battery cells and avoid the formation of undesirable wrinkles when filling with electrolyte in a vacuum.

[0030] In particular, a motor vehicle also benefits from the invention if it is equipped with at least one battery cell which is surrounded by a metal composite foil which has been preformed according to the proposed method. Such a battery cell can be manufactured more efficiently and is more reliable in long-term operation due to the improved metal composite foil. Furthermore, a higher energy density can be achieved in a battery cell by means of such a metal composite foil, since the foil has a lower weight and better cooling properties.

[0031] Another particularly preferred embodiment of the present invention for solving the technical problem provides a forming device for deforming a metal composite foil for a battery cell. The forming device designed in this way has at least a first sheet metal holder, a first drive device for bringing the first sheet metal holder and the first die closer to each other, a second sheet metal holder, a second die and a first punch. Here, the second sheet metal holder, the second die and the first punch are arranged inside the first sheet metal holder and inside the first die, so that the second die is constructed as a second punch that can be moved into the first die, and the first punch is arranged inside the second sheet metal holder so that the first punch can be moved into the second die. The forming device designed in this way can simultaneously fix the metal composite foil on the first fixing area and the second fixing area and deform it between the two fixing areas in such a way that the second die and the second sheet metal holder are moved together as the second punch into the first die. In addition, a first punch is provided, which performs additional deformation in the deformation area in order to compensate for the springback of the metal composite foil that occurs, so that a metal composite foil with particularly accurate dimensions can be produced at the end of the deformation forming process.

[0032] Furthermore, it is advantageous for reliably holding the metal composite foil during the deformation forming process if the forming device has a second drive device for bringing the second sheet material holder and the second die closer to each other and a third drive device for bringing the first punch and the second die closer to each other. Here, the second drive device can apply a holding force to the metal composite foil that is greater than the tensile force that the third drive device can apply to the metal composite foil via the first punch. The purpose is to resist the tensile force generated by the first punch and acting on the metal composite foil parallel to the pressing plane, so as to prevent the metal composite foil from changing position in the second fixing area.

[0033] In particular, it can also be provided that the first punch deforms the metal composite foil in a direction opposite to the deformation direction of the second punch.

[0034] Furthermore, it can be provided as required that the first punch has a convex punch face. The punch face is the face that comes into contact with the metal composite foil. The convex shaping of the punch face allows the metal composite foil to be formed into a shape that is approximately arched. Due to the springback that occurs after the metal composite foil is removed, it is then possible to achieve that the arch compensates for the springback as much as possible and thus produces a nearly flat surface by appropriately selecting the arch of the convex punch face.

[0035] In particular, it can also be provided that the advance of the second sheet metal holder relative to the first punch is at least 0.5 mm (millimeter), preferably at least 1 mm. This advance ensures that when the segments approach each other, the second sheet metal holder first contacts the second mold before the first punch contacts the metal composite foil. In this way, it is ensured that the second fixing region is first securely fixed between the second sheet metal holder and the second mold before the first punch contacts the metal composite foil and deforms the metal composite foil into shape by applying a tensile force.

[0036] It is particularly advantageous that a gap is provided between the second die and the first die parallel to the direction of relative movement between the second sheet metal holder and the first die, and the gap is designed with a variable gap width. In principle, the gap width considered for this is between 100% and 150% of the material thickness of the metal composite foil. The combination of a variable gap width enables the forming device to be optimally adapted to the corresponding metal composite foil. In practice, an undesirable large elongation of the metal composite foil is observed, especially in the corner region, while in the region located between the corner regions, only very small deformation and thus only relatively small elongation occur in part. Now, with the help of a variable gap width, the elongation generated during deformation forming can be reduced at the corners of the metal composite foil by a larger gap width and increased in the region located between the corners by a gap width smaller than the gap width at the corners. This is achieved, for example, by selecting the gap width in the corner region so that the gap width is greater than the material thickness of the metal composite foil. A suitable value range for the gap width in the corner region is, for example, a gap width between 100% and 150%, and in particular between 110% and 150%, of the material thickness of the metal composite foil. In other regions, where a greater elongation is desired, a gap width at least equal to the material thickness of the metal composite foil can be used. Thus, for example, a gap width between 100% and 120%, and in particular between 100% and 110%, of the material thickness of the metal composite foil can be used in these regions between the corners.

[0037] In particular, the reduced or increased gap width can also be used individually or simultaneously, so that the gap width in at least one section is equal to or greater than the material thickness of the metal composite foil.

[0038] It is particularly advantageous if the gap width or the gap width has a value range of between 100% and 120% of the material thickness of the metal composite foil over at least 60%, preferably at least 80% and in particular at least 90% of the side length of the second mold. For example, the side length between two corners and having such a gap width can thus be deformed with a greater elongation of the metal composite foil than other regions having a greater gap width.

[0039] It is also advantageous if the punch face of the second sheet metal holder is at least partially designed at an angle to the pressing plane, so that the second fixing region can be deformed at an angle to the pressing plane, so that the second fixing region also has the desired shape after the metal composite foil has rebounded and overall compensates for the rebound as completely as possible.

[0040] Furthermore, it can be provided that the metal composite foil comprises at least one layer of PET, aluminum, nylon or PP. Such aluminum composite foils are already available on the market today and in principle have good properties with regard to durability and accommodation of battery cells. However, this presupposes that damage to the composite foil and impairment of the forming accuracy due to springback are avoided during the deep-drawing process, as can be achieved with the invention.

[0041] Finally, it is advantageous if the metal composite foil has an aluminum foil thickness of less than 60 μm (micrometers), preferably at least 40 μm. In connection with the present invention, it is particularly possible to process metal composite foils having particularly thin aluminum, for example 40 μm and below. This allows the use of expensive aluminum to be reduced and the foil thickness of the metal composite foil to be reduced.

[0042] It should be noted that the numbers used here ("first", "second", etc.) are primarily (only) used to distinguish between multiple identical objects, dimensions or processes, and therefore are not in particular mandatory regulations for the correlation and / or order of these objects, dimensions or processes with each other. If a correlation and / or order is required, it will be explicitly stated here or will be obvious to a person skilled in the art when studying the specifically described design. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] The invention and the technical environment are explained in more detail below with reference to the drawings. It should be noted that the invention is not limited to the exemplary embodiments listed. In particular, if not explicitly stated otherwise, it is also possible to extract the factual parts described in the drawings and combine them with other components and concepts in the description. In particular, it should be noted that the drawings and in particular the dimensional ratios shown are only schematic. In the drawings:

[0044] Figure 1 A schematic cross-sectional view of a forming device for opening a metal composite foil according to the prior art is shown;

[0045] Figure 2 A schematic cross-sectional view of a closed forming device for metal composite foil according to the prior art is shown;

[0046] Figure 3 A schematic cross-sectional view of a forming device for a metal composite foil according to the prior art, which is opened after deformation forming;

[0047] Figure 4A schematic cross-sectional view of a molding device according to the present invention in an open state is shown;

[0048] Figure 5 A schematic cross-sectional view of a forming apparatus according to the present invention having a first sheet metal holder close together is shown;

[0049] Figure 6 A schematic cross-sectional view of a forming apparatus according to the present invention having a second sheet metal holder in close proximity is shown;

[0050] Figure 7 A schematic cross-sectional view of a forming device according to the present invention with a second punch approaching;

[0051] Figure 8 A schematic cross-sectional view of a forming device according to the present invention having a second punch and straight and curved dies close to each other;

[0052] Fig. 9 A view showing springback of a bent die;

[0053] Fig.10 A view showing straight die springback;

[0054] Fig.11 A schematic cross-sectional view of a forming device according to the present invention with a first punch approaching in a closed state;

[0055] Fig.12 A schematic cross-sectional view of a forming device in an open state according to the present invention after deformation forming;

[0056] Fig.13 showing a cross-sectional view of a second sheet material holder having a first punch;

[0057] Fig.14 An oblique view showing a first punch having a convex punch face;

[0058] Fig.15 An oblique view showing a first punch having a milled straight punch face;

[0059] Fig.16 showing a top view of a second sheet material holder;

[0060] Fig.17 An oblique view showing a corresponding punch according to the prior art;

[0061] Fig.18 A first embodiment of a first punch is shown;

[0062] Fig.19 A second embodiment of the first punch is shown;

[0063] Fig. 20A first embodiment of a first punch is shown;

[0064] Fig.21 showing a top view of the second punch in the first die; and

[0065] Fig. 22 A schematic diagram of a motor vehicle with a battery cell is shown. DETAILED DESCRIPTION

[0066] Figure 1 A sectional view from the side shows a forming device 1 according to the prior art. The forming device 1 is composed of a first sheet metal holder 2, a first die 3, a first punch 4 and a counter punch 5. The forming device 1 also has a first drive 6 which is suitable for bringing the first sheet metal holder 2 and the first die 3 closer together and thereby fixing a metal composite foil 7 arranged in a pressing plane 8.

[0067] Figure 2 Shown according to Figure 1 The forming device 1 is in a state in which the metal composite foil 7 is deformed by the punch 4 being moved together with the counter punch 5 upwards into the first mold 3 in the drawing plane.

[0068] Figure 3 The situation is shown after the deformation process when the forming device 1 is opened, which means that all sections, namely the sheet metal holder 2, the die 3, the punch 4 and the counter punch 5, have been moved back into their initial position. It can be seen here that the metal composite foil 7 has an undesirable springback 9 in the area deformed by the punch 4.

[0069] Figure 4The forming device 1 is shown in a schematic sectional view. The forming device 1 has a first sheet metal holder 2, a first die 3, a second die 10, a first drive 6, a second sheet metal holder 11, a second drive 12 and a first punch 4. In the opened forming device 1, a metal composite foil 7 has been placed in the extrusion plane 8. The first drive 6 is designed to move the first sheet metal holder 2 toward the first die 3 and clamp the metal composite foil 7 between the first sheet metal holder and the first die. The area in which the clamping is achieved constitutes a first fixing area 13. The second fixing area 14 directly connects the first fixing area 13 in the extrusion plane 8. The second fixing area is an area in which the metal composite foil 7 is held between the second die 10 and the second sheet metal holder 11 by clamping. The second drive 12 is designed so that the second drive can move the second sheet metal holder 11 together with the second die 10 and fix the metal composite foil 7 there. The forming device 1 is configured such that the second die 10 and the second sheet metal holder 11 are arranged inside the first die 3 or inside the first sheet metal holder 2. The first punch 4 is itself arranged inside the second sheet metal holder 11. Below the punch 4 is located a deformation region 15 in which the metal composite foil 7 is deformed by the punch 4.

[0070] Figure 5 Shows the basis of being in a state Figure 4 A forming device 1 is shown in which the first sheet metal holder 2 and the first mold 3 are brought close to one another and in the process fix the metal composite foil 7 in the first fixing region 13 .

[0071] exist Figure 6 In the case shown, the metal composite foil 7 is additionally also fixed in the second fixing area 14. This is achieved by the drive 12 moving the second sheet metal holder 11 and the second mold 10 closer together. The movement of the first sheet metal holder 2 in the direction of the first mold 3 assumes a first direction 16.

[0072] Figure 7The beginning of the deformation forming of the metal composite foil is shown. In the shown state, the metal composite foil 7 has been fixed in the first fixing area 13 and the second fixing area 14, respectively, but has not yet been deformed by the punch 4 in the deformation area 15. In order to ensure that the clamping is reliably achieved in the second fixing area 14 before the first punch contacts the metal composite foil 7, the second sheet metal holder 11 has a geometric advance feed relative to the first punch 4. This geometric advance feed is schematically shown by the distance dimension 17. When approaching, the second sheet metal holder contacts the metal composite foil 7 before the first punch 4 due to the advance feed. It can be clearly seen here that the second mold 10 moves upward into the first mold 3 in the drawing plane and acts like the second punch 18 in this movement. Due to the relative movement caused by this, the first punch 4 moves in the second direction 19 and contacts the metal composite foil 7.

[0073] Figure 8 Two possible embodiments of the invention are shown. The right half shows an embodiment in which the second fixing area 14 is designed parallel to the extrusion plane 8. Figure 7 The above-described implementation modes correspond to the above-described implementation modes.

[0074] On the left half, an embodiment is shown in which the metal composite foil 7 is designed at an angle (α) to the pressing plane 8 in the second fixing region 14. For this purpose, the end face 20 of the second sheet metal holder 11 and the end face 20 of the second mold 10 are arranged inclined at an angle (α) to the pressing plane 8. This design can additionally counteract possible springback of the metal composite foil 7.

[0075] Fig. 9 This effect is again shown by comparing the metal composite foil 7 in the deformed state shown in the upper region of the figure and in the resilient state shown in the lower region of the figure. Undesired resilientness can thus be effectively counteracted by the inclined arrangement of the second fixing region 14 .

[0076] Fig.10 This shows the situation which can occur if the metal composite foil 7 rebounds very strongly if the second fixing region 14 is not arranged at an angle to the pressing plane 8 as shown in the upper region. In this case, a significant undesirable rebound 9 can occur after removal from the forming device 1 .

[0077] Fig.11 Another possible embodiment of the present invention is shown, in which a third drive device 21 is provided in addition to the first drive device 6 and the second drive device 12 in order to move the first punch 4 along the second direction 19. In addition, Fig.11 The structure of the molding device 1 shown is basically combined with the above Figures 4 to 8 The molding equipment 1 is the same.

[0078] Fig.12 Finally, the forming device 1 is shown in the open state, wherein the metal composite foil 7 in the resilient state is shown by the solid line. The contour shown by the dashed line here shows the contour of the deformation that occurs when the forming device 1 is closed.

[0079] Fig.13 A second sheet metal holder 11 with a first punch 4 arranged therein is shown. Unlike the prior art, the present invention does not use a single-component counter-punch, but a double-headed embodiment with a second sheet metal holder 11 combined with a first punch 4. The second sheet metal holder 11 still has a geometric advance feed relative to the first punch 4, which is shown as a distance dimension 17. This distance dimension 17 can be, for example, 0.5 mm, 1 mm or more. The punch 4 has a convexly curved punch face 22 toward the metal composite 7. This makes it possible to deform the metal composite foil 7 in the deformation area 15 into the concavely formed second mold 10 not shown in the figure.

[0080] Fig.14 The first punch 4 is again shown in an oblique view, wherein the convexly shaped punch face 22 can still be clearly seen on the left.

[0081] Fig.15 A possible alternative embodiment of a first punch 4 with a flat punch face 22 is shown, which can be used, for example, when using a metal composite foil 7 with a low degree of springback 9 .

[0082] Fig.16 The second sheet metal holder 11 is shown again in a top view. The second sheet metal holder 11 shown there can be used as required according to Fig.14 or Fig.15 The first punch 4 is shown.

[0083] Fig.17 The counter punch 5 as used in the prior art is shown. The counter punch 5 is characterized by its one-piece design and does not allow deformation and shaping in the second direction. In particular, it is not possible to carry out different deformations in different areas with such a simple counter punch 5, which can be achieved with the second sheet metal holder 11 and the first punch 4 according to the invention, for example in the second fixing area 14 and the deformation area 15.

[0084] Fig.18 A first punch 4 is shown, the punch face 22 of which has a flattened portion in the lower region.

[0085] Fig.19 A further embodiment of a first punch 4 is shown, the punch face 22 of which has a concave section 23 in the lower region.

[0086] In addition, Fig. 20 4 shows a first punch 4 , whose punch face 22 is convex and has an additional projection 24 on the underside.

[0087] In all embodiments of the punch face 22 of the punch 4 , the correspondingly assigned and opposite contact surface of the second mold 10 is preferably designed corresponding to the respective punch face 22 in order to achieve the best deformation forming result.

[0088] In addition Fig.21 , a top view of a first mold 3 is shown, which has a second mold 10 inserted therein. The second mold 10 has a length 25 and a width 26. In the embodiment shown, the second mold 10 has four corners 27 and four longitudinal sides 28 connecting the corners to one another. In addition, a gap 29 is located around the second mold 10 between the second mold 10 and the first mold 3. The surrounding gap 29 has different gap widths. The gap width is greater in the region of the corners 27 than the material thickness of the metal composite foil 7 to be deformed.

[0089] Here, it has also been found that the gap width is selected to be 50%, preferably 120%, and in particular 110% greater than the material thickness of the metal composite film 7. By significantly increasing the gap width in the region of the corners 27 to exceed the material thickness of the metal composite film 7, the metal composite film 7 can flow more easily into these more highly deformed regions during deformation forming and damage to the metal composite film 7 due to excessive elongation is avoided.

[0090] In contrast, the gap width of the gap 29 in the region of the longitudinal side 28 is preferably selected to be 100% to 120%, in particular 100% to 110%, of the material thickness of the metal composite foil 7 to be deformed. The gap width of the gap 29 at the longitudinal side 28 can be selected to be smaller than its gap width in the corner 27. By reducing the gap width in the region of the longitudinal side 28, it is possible to produce a greater degree of elongation of the metal composite foil 7 in these regions, thereby increasing the degree of deformation. The longitudinal side length 30 indicates the region where the gap width is reduced. For this purpose, it can be provided that the longitudinal side length 30 is at least 60%, preferably at least 80% and in particular at least 90% of the length 25 or the width 26. The length 25 or the width 26 can also be referred to as the side length. The region with a smaller gap width is preferably arranged at the same distance from the corner 27 as much as possible.

[0091] Fig. 22Finally, a motor vehicle 31 is shown having a battery 32 which has a plurality of battery cells 33 . The energy stored in the battery 32 is used to drive the motor vehicle 31 .

[0092] Overall, it can be seen that significant advantages can be achieved by the two-piece design of the first punch 4 and the second sheet metal holder 11. As a result, the metal composite foil 7 is reliably fixed by the second sheet metal holder 11 and material flow caused by the first punch 4 during the deformation process is prevented. This has the advantage that the material stretched by the first punch 4 is produced by stretching and reducing the material thickness, so that the additional plastic stretching produces less springback. In addition, the metal composite foil 7 with a particularly thin aluminum layer can be processed reliably and accurately with the help of the present invention. This can also be achieved at normal ambient temperatures, for example, temperatures of 20° C. to 30° C., and energy-consuming heating can be omitted or at least reduced to a minimum.

[0093] Finally, the invention enables better control of the deformation of the metal composite foil 7 by using different gap widths on the longitudinal sides 28 and in the corner regions 27. In this way, very good deformation results can also be achieved on the longitudinal sides, while at the same time the hitherto highly loaded and very critical corner regions 27 have an improved material flow and are therefore less susceptible to damage.

[0094] Reference numerals list

[0095] 1 Molding equipment

[0096] 2 First sheet metal holder

[0097] 3. The first mold

[0098] 4 First Punch

[0099] 5 Corresponding punch

[0100] 6 First drive unit

[0101] 7 Metal composite foil

[0102] 8 Extruded plane

[0103] 9 Rebound

[0104] 10 Second model

[0105] 11 Second sheet material holder

[0106] 12 Second drive unit

[0107] 13 First fixed area

[0108] 14 Second fixed area

[0109] 15 Deformation area

[0110] 16 First Direction

[0111] 17 Distance Dimension

[0112] 18 Second Punch

[0113] 19 Second Direction

[0114] 20 End face

[0115] 21 Third drive unit

[0116] 22 Punch face

[0117] 23 Convex segments

[0118] 24 protrusion

[0119] 25 Length

[0120] 26 Width

[0121] 27 corner

[0122] 28 longitudinal side

[0123] 29 Gap

[0124] 30 Longitudinal side length

[0125] 31 Motor Vehicles

[0126] 32 Batteries

[0127] 33 Battery Cell

Claims

1. A method for deforming a metal composite foil (7) for a battery cell (33), the method comprising at least the following steps: a) placing the metal composite foil (7) in a forming device (1), the forming device having a plurality of sheet material holders (2, 11), a plurality of dies (3, 10) and a first punch (4); b) fixing the first fixing area (13) of the metal composite foil (7) by closing the first sheet material holder (2) and the first mold (3); c) fixing the second fixing area (14) of the metal composite foil (7) by closing the second sheet material holder (11) and the second mold (10); d) deforming the second fixing area (14) at least partially in a first direction (16) by moving the second sheet material holder (11) and the second mold (10); e) deforming the deformation region (15) at least partially in a second direction (19) by moving the punch (4), It is characterized in that A holding force is generated in the second fixing region (14) by the second sheet metal holder (11), which is greater than the tensile force generated in the deformation region by the punch (4).

2. The method according to claim 1, wherein: Step c) is carried out chronologically after step d).

3. The method according to claim 1 or 2, wherein: The metal composite foil (7) is deformed at least partially at an angle (α) relative to the pressing plane (8) on the end face (20) of the second sheet metal holder (11) in the second fixing region (14).

4. The method according to claim 1 or 2, wherein: An aluminum composite foil was used as the metal composite foil (7).

5. The method according to claim 1 or 2, wherein: The wall thickness of the metal composite foil (7) is selected within the range of 100 μm to 180 μm.

6. A battery cell (33) having a metal composite foil (7) produced by the method according to one of the preceding claims.

7. A motor vehicle (31) having at least one battery cell (33) according to claim 6.

8. A forming device (1) for deforming a metal composite foil (7) for a battery cell (33), the forming device comprising at least a first sheet material holder (2), a first drive device (6) for bringing the first sheet material holder (2) and a first die (3) closer to each other, a second sheet material holder (11), a second die (10) and a first punch (4), characterized in that: The second sheet material holder (11), the second die (10) and the first punch (4) are arranged inside the first sheet material holder (2) and inside the first die (3), so that the second die (10) is constructed as a second punch (18) that can be moved into the first die, and the first punch (4) is arranged inside the second sheet material holder (11) so that the first punch can be moved into the second die (10), characterized in that the forming device has a second drive device (12) for bringing the second sheet material holder (11) and the second die (10) closer to each other and a third drive device (21) for bringing the first punch (4) and the second die (10) closer to each other, and the second drive device (12) can apply a holding force to the metal composite foil (7), and the holding force is greater than the pulling force that the third drive device (21) can apply to the metal composite foil (7).

9. The forming device (1) according to claim 8, characterized in that The first punch (4) causes the metal composite foil (7) to deform in a direction opposite to a first deformation direction (16) of the second punch (18).

10. The forming device (1) according to claim 8 or 9, characterized in that: The first punch (4) has a convex punch surface (22).

11. The forming device (1) according to claim 8 or 9, characterized in that: The advance feed amount of the second sheet material holder (11) relative to the first punch (4) is at least 0.5 mm.

12. The forming device (1) according to claim 8 or 9, characterized in that: A gap (29) is provided between the second mold (10) and the first mold (3) parallel to the direction of relative movement between the second sheet metal holder (11) and the first mold (3), and the gap (29) is designed with a variable gap width.

13. The forming device (1) according to claim 8 or 9, characterized in that: The gap width over at least 60% of the side length (25, 26) of the second mold (10) is between 100% and 120% of the material thickness of the metal composite foil (7).

14. The forming device (1) according to claim 8 or 9, wherein: The punch surface (22) of the second sheet metal holder (11) is at least partially designed at an angle (α) relative to the pressing plane (8).

15. The forming device (1) according to claim 8 or 9, characterized in that: The metal composite foil (7) has an aluminum foil thickness of less than 60 μm.

Citation Information

Patent Citations

  • Battery, tab of battery and method of manufacture thereof

    CN1383584A

  • Manufacture of a nestable container

    GB1364879A