Forming die and forming method for PVC-O double-socket reducing pipe fittings

By using the forming mold to perform axial stretching and radial stretching of PVC-U pipes, the problem of the inability of existing technology to manufacture high-performance PVC-O double-socket reducing pipe fittings is solved, achieving high strength, toughness and impact resistance. performance of the finished product and simplifies the molding process, ensuring the quality of the finished product and the molding of complex shapes.

CN115008722BActive Publication Date: 2024-10-01YIBIN TIANYI NEW MATERIALS TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210421622.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-04-21
Publication Date
2024-10-01
Estimated Expiration
2042-04-21

AI Technical Summary

Technical Problem

The existing PVC-O double-socket reducer forming technology cannot effectively manufacture high-performance, complex-shaped connectors, and traditional solutions such as steel-plastic pipe fittings have problems such as short service life, high weight, and poor matching.

Method used

A forming mold including an upper module and a lower module is used to perform axial and radial stretching of PVC-U pipes through vacuum channels and guide tubes to form high-performance PVC-O double-socket reducing pipe fittings, using fillet inlays. Blocks and air guide holes ensure molding quality and shape complexity.

Benefits of technology

The molding of PVC-O double-socket reducing pipe fittings with high strength, high toughness, high impact resistance and fatigue resistance is realized. The molding method is simple and convenient, the quality is controllable, meets the usage requirements, and can be taken out without damage through non-contact demoulding.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115008722B_ABST
    Figure CN115008722B_ABST
Patent Text Reader

Abstract

The invention discloses a forming die for a PVC-O double-socket reducing pipe fitting, comprising an upper module and a lower module connected to each other, wherein the two modules each comprise a moving block, an intermediate module and a fixed block which are connected in sequence and provided with an inner cavity, one end of a guide tube provided with a blind hole is connected with the moving blocks of the two modules, the other closed end of the guide tube is placed in the fixed blocks of the two modules, a plurality of radial air guide holes are provided in the middle of the guide tube, and a plug is connected with the fixed blocks of the two modules; the moving block and the fixed block are each provided with a vacuum channel connected with their inner cavities, the inner wall of the intermediate module is each fixedly connected with two or more rounded inserts, the rounded inserts are made of breathable steel, and the outer sides of the rounded inserts are each provided with an exhaust channel connected with the vacuum channel; a flow channel is provided in the intermediate module; the invention also discloses a forming method for a PVC-O double-socket reducing pipe fitting; the invention can prepare a PVC-O double-socket reducing pipe fitting with high performance and complex appearance, and is simple, convenient, and quality-controllable, thus meeting the use requirements.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a forming die and a forming method for a PVC-O double-socket reducing pipe fitting. Background Art

[0002] Biaxially oriented polyvinyl chloride (PVC-O) pipes are PVC-U pipes that are stretched axially and radially under specific conditions, so that the long molecular chains in the pipes are regularly arranged in the biaxial direction, obtaining a new type of PVC pipe with high strength, high toughness, high impact resistance and fatigue resistance. Its performance is far superior to that of ordinary pipes, and it can significantly save raw materials and reduce costs, resulting in an increasing application of biaxially oriented polyvinyl chloride (PVC-O) pipes, which have gradually become the mainstream of the water supply market.

[0003] The matching connectors of PVC-O pipes, especially PVC-O double socket reducers, always solve the demand for PVC-O double socket reducers through other methods different from biaxial orientation.

[0004] The traditional solution is to use steel-plastic pipe fittings. However, due to the shortcomings of steel-plastic pipe fittings such as short service life, high weight, and poor compatibility with PVC-O pipes, the application and promotion of PVC-O pipes have been greatly hindered.

[0005] The existing solution is to adopt the widely used injection molding technology. Since injection molding uses molten material as the starting material and has no orientation, injection molded pipe fittings lack high strength, high toughness, high impact resistance, fatigue resistance and other properties. It is also difficult to manufacture pipe fittings with complex shapes and cannot meet the use requirements. Summary of the invention

[0006] The purpose of the present invention is to provide a molding die and a molding method for a PVC-O double-socket reducing pipe fitting in view of the deficiencies in the prior art, which can be used to prepare high-performance PVC-O double-socket reducing pipe fittings with complex shapes, and is simple, convenient, and quality-controlled, thus meeting use requirements.

[0007] In order to achieve the above-mentioned purpose, the forming mold of the PVC-O double-socket reducing pipe fitting of the present invention comprises an upper module and a lower module connected to each other, both modules comprise a moving block, an intermediate module and a fixed block which are connected in sequence and provided with an inner cavity, one end of a guide tube provided with a blind hole is connected to the moving blocks of the two modules, the other closed end of the guide tube is placed in the fixed blocks of the two modules, a plurality of radial air guide holes are provided in the middle of the guide tube, and a plug is connected to the fixed blocks of the two modules; the characteristic is that: the moving block and the fixed block are both provided with a vacuum channel connected to their inner cavities, the inner wall of the intermediate module is fixedly connected with two or more rounded inserts, the rounded inserts are made of breathable steel, and the outer sides of the rounded inserts are provided with exhaust ducts connected to the vacuum channel; and a flow channel is provided in the intermediate module.

[0008] The molding method of the PVC-O double-socket reducing pipe fittings using the above molding mold comprises the following steps: A) preheating the PVC-U pipe to the molding process temperature; B) introducing a medium into the flow channel to preheat the two middle modules to the molding process temperature; C) transferring the preheated PVC-U pipe to the molding mold, placing the two ends of the pipe in the moving block and the fixed block of the upper module and the lower module respectively, placing the guide pipe in the pipe, locking the two ends of the pipe after the mold is closed, and then using the vacuum channel and the fillet insert of the upper and lower modules to extract the air in the outer space of the pipe to form a negative pressure; D) introducing a gas medium at the process temperature into the guide pipe so that the PVC-U pipe is The C-U pipe is expanded and oriented into a PVC-O double-socket reducing pipe fitting. After maintaining the pressure, a cooling gas medium is introduced into the guide pipe to cool and shape the PVC-O double-socket reducing pipe fitting. E) After the gas outside the double-socket reducing pipe fitting is exhausted, the plug and the guide pipe are withdrawn, the vacuum pumping of the lower module is stopped, and positive pressure gas is introduced through the vacuum channel and the rounded insert of the lower module. The mold is opened, the lower module is removed, the vacuum pumping of the upper module is stopped, and lubricating positive pressure gas is introduced through the vacuum channel and the rounded insert of the upper module. The pipe fitting is withdrawn by its own weight.

[0009] By adopting this molding method, the PVC-O double-socket reducer has high strength, high toughness, high impact resistance, fatigue resistance and other properties because it is formed by orientation; the inner wall of the fillet insert is provided with a fillet and is made of breathable steel, which can form a negative pressure and is easy to deform, and can meet the molding of complex-shaped reducer pipes; the molding method is simple and convenient, the finished product is non-contact demoulding, and is taken out losslessly by gravity, the quality is controllable, and the use requirements are met;

[0010] As a further improvement of the present invention, the inner walls of the movable block and the fixed block are both provided with sealing blocks; the two ends of the PVC-U pipe can be locked and sealed;

[0011] As a further improvement of the present invention, the plug is provided with an inner hole, and the closed end of the guide tube is conical and placed in the inner hole; this can provide support for the guide tube, maintain stability, and improve the quality of orientation molding;

[0012] As a further improvement of the present invention, the plurality of air guide holes in the middle of the guide tube are evenly arranged in the axial direction and the circumference, ensuring that the PVC-U pipe is evenly stressed during orientation, so that the shape and wall thickness of the double-socket reducing pipe fitting after orientation are perfectly controlled, thereby improving the molding quality;

[0013] As a further improvement of the present invention, the gas medium introduced in step D) is compressed gas; rapid orientation is possible;

[0014] As a further improvement of the present invention, the temperature deviation of the preheated PVC-U pipe in step A) does not exceed ±1.5°C to prevent the PVC-U pipe from having a deformed orientation under the same stress when the temperature is uneven;

[0015] In summary, the present invention can prepare high-performance, complex-shaped PVC-O double-socket reducing pipe fittings, and the process is simple, convenient, and quality controllable, thus meeting the use requirements. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 This is a front view of the lower module in the molding die embodiment of the present invention in use.

[0017] Figure 2 This is a diagram of the initial state of the PVC-U pipe used in the present invention.

[0018] Figure 3 This is a finished picture of the PVC-O double-socket reducing pipe fitting obtained by the present invention. DETAILED DESCRIPTION

[0019] In order to more clearly understand the purpose, technical solutions and beneficial effects of the present invention, the present invention is further described below in conjunction with the accompanying drawings, but the protection scope of the present invention is not limited to the following embodiments.

[0020] like Figure 1 As shown, the forming mold of the PVC-O double-socket reducing pipe fitting of the embodiment of the present invention comprises an upper module (not shown) and a lower module 1 connected to each other, and the upper module and the lower module 1 each comprise a moving block 2, an intermediate module 3 and a fixed block 4 which are sequentially connected and provided with an inner cavity, and the structures of the upper module and the lower module 1 are completely the same and symmetrical to each other; one end of a guide tube 5 provided with a blind hole is connected to the moving block 2 of the upper module and the lower module 1, and the other closed end of the guide tube 5 is conical and placed in the fixed block 4 of the upper and lower modules 1, and a plurality of radial air guide holes 6 are provided in the middle of the guide tube 5, and a plurality of guide holes 6 are provided in the middle of the guide tube 5. The air holes 6 are evenly arranged in the axial direction and the circumference; a plug 7 is connected to the fixed blocks 4 of the two modules, and the plug 7 is provided with an inner hole 8, and the conical closed end of the guide tube 5 is placed in the inner hole 8; the inner walls of the moving block 2 and the fixed block 4 of the upper module and the lower module 1 are provided with sealing blocks 9, and the moving block 2 and the fixed block 4 are provided with vacuum channels 10 connected to their inner cavities, and the inner wall of the middle module 3 is fixedly connected with two rounded inserts 11, and the rounded inserts 11 are breathable steel, and the outer side of the rounded inserts 11 is provided with exhaust ducts 12 connected to the vacuum channel 10; the middle module 3 is provided with flow channels 13.

[0021] The molding method of the PVC-O double-socket reducing pipe fittings using the molding die of the present invention comprises the following steps: A) Figure 2The PVC-U pipe 15 shown is placed in an oven and preheated uniformly to the molding process temperature, and the temperature deviation of the PVC-U pipe does not exceed ±1.5℃; B) a medium (such as high-temperature steam) is introduced into the flow channel 13 to preheat the two middle modules 3 to the molding process temperature; C) the preheated PVC-U pipe 15 is transferred to the molding mold, and the two ends of the pipe 15 are respectively placed in the moving block 2 and the fixed block 4 of the upper module and the lower module 1, and the sealing blocks 9 on both sides are sleeved on the outer circle of the two ends of the pipe, and the guide pipe 5 is placed in the pipe. After the mold is closed, the two ends of the pipe are locked, and then the vacuum channel 10, the exhaust channel 12 and the fillet insert 11 of the upper and lower modules 1 are used to extract the air in the outer space of the PVC-U pipe to form a negative pressure; D) a compressed gas medium at the process temperature is introduced into the guide pipe 5 , enter the inner cavity of the pipe through the air guide hole 6, so that the PVC-U pipe expands and is oriented into a PVC-O double-socket reducing pipe fitting 14. After maintaining the pressure, a cooling gas medium is introduced into the guide pipe 5 to cool and shape the PVC-O double-socket reducing pipe fitting 14; E) After the gas outside the double-socket reducing pipe fitting 14 is removed by the vacuum device, the plug 7 and the guide pipe 5 are withdrawn, the vacuuming of the lower module 1 is stopped, and positive pressure gas is introduced through the vacuum channel 10, the exhaust channel 12, and the rounded insert 11 of the lower module 1, the mold is opened, the lower module 1 is removed, and the vacuuming of the upper module is stopped again. The lubricating positive pressure gas is introduced through the vacuum channel and the rounded insert of the upper module. The PVC-O double-socket reducing pipe fitting 14 is separated from the upper module, and the PVC-O double-socket reducing pipe fitting 14 is withdrawn by its own weight;

[0022] PVC-O double socket reducer 14 can be obtained by removing the two clamping ends. Figure 3The PVC-O double-socket reducer finished product 16 is shown; after the mold is closed, the inner cavity size of the mold is slightly larger than the outer size of the PVC-O double-socket reducer 14 after molding, and the amplitude does not exceed 13%, that is, the design dimensions of the inner cavity of the upper and lower modules are larger than the outer diameter of the PVC-O double-socket reducer 14, and the difference between the design dimensions of the inner cavity of the upper and lower modules and the outer diameter of the PVC-O double-socket reducer 124 is equal to the normal shrinkage value of the PVC-O double-socket reducer 14 at the orientation temperature; using this molding method, since the PVC-O double-socket reducer 14 is oriented and molded, it has high strength, high toughness, high impact resistance, fatigue resistance and other properties; the inner wall of the fillet insert 11 is provided with fillets and is transparent The gas steel can form negative pressure on its inner side, which is easy to deform the pipe. During orientation, the rounded corner insert 11 forms an arc-shaped reinforcing rib on the outer circle of the PVC-O double-socket reducer 14, which can meet the molding of complex-shaped reducers. The molding method is simple and convenient, the finished product is non-contact demoulding, and is taken out losslessly by gravity. The quality is controllable and meets the use requirements. The sealing block 9 can lock and seal the two ends of the PVC-U pipe. The closed end of the guide pipe 5 is placed in the inner hole 8, which can provide support for the guide pipe, maintain stability, and improve the orientation molding quality. The air guide hole 6 ensures that the PVC-U pipe is uniformly stressed during orientation, so that the shape and wall thickness of the double-socket reducer after orientation are perfectly controlled, thereby improving the molding quality.

Claims

1. A forming die for a PVC-O double-socket reducing pipe fitting, comprising an upper module and a lower module connected to each other, wherein the two modules each comprise a moving block, an intermediate module and a fixed block which are sequentially connected and provided with an inner cavity, one end of a guide tube provided with a blind hole is connected to the moving blocks of the two modules, the other closed end of the guide tube is placed in the fixed blocks of the two modules, a plurality of radial air guide holes are provided in the middle of the guide tube, and a plug is connected to the fixed blocks of the two modules; the characteristics are as follows: The movable block and the fixed block are both provided with vacuum channels connected to their inner cavities. The inner wall of the intermediate module is fixedly connected with two or more rounded inserts. The inner wall of the rounded insert is provided with rounded corners and is made of breathable steel. The outer side of the rounded insert is provided with an exhaust channel connected to the vacuum channel. A flow channel is provided in the intermediate module.

2. The forming die for the PVC-O double-socket reducing pipe fitting according to claim 1, characterized in that: The inner walls of the moving block and the fixed block are both provided with sealing blocks.

3. The forming die for the PVC-O double-socket reducing pipe fitting according to claim 1 or 2, characterized in that: The plug is provided with an inner hole, and the closed end of the guide tube is conical and is placed in the inner hole.

4. The forming die for the PVC-O double-socket reducing pipe fitting according to claim 3, characterized in that: The plurality of air guide holes in the middle of the guide tube are evenly arranged in the axial direction and the circumference.

5. A method for forming a PVC-O double-socket reducing pipe fitting using the forming mold as claimed in claim 1, comprising the following steps: A) Preheating the PVC-U pipe to the molding process temperature; characterized in that: B) introducing medium into the flow channel to preheat the two middle modules to the molding process temperature; C) transferring the preheated PVC-U pipe to the molding die, placing the two ends of the pipe in the moving block and the fixed block of the upper module and the lower module respectively, placing the guide tube in the pipe, locking the two ends of the pipe after closing the mold, and then using the vacuum channel and the fillet insert of the upper and lower modules to extract the air in the outer space of the pipe to form a negative pressure; D) introducing a gas medium at the process temperature into the guide tube, so that The PVC-U pipe is expanded and oriented into a PVC-O double-socket reducer. After maintaining the pressure, a cooling gas medium is introduced into the guide tube to cool and shape the PVC-O double-socket reducer. E) After the gas outside the double-socket reducer is exhausted, the plug and the guide tube are withdrawn, the vacuum pumping of the lower module is stopped, and positive pressure gas is introduced through the vacuum channel and the rounded insert of the lower module. The mold is opened, the lower module is removed, the vacuum pumping of the upper module is stopped, and lubricating positive pressure gas is introduced through the vacuum channel and the rounded insert of the upper module, and the pipe is withdrawn by its own weight.

6. The molding method of the PVC-O double-socket reducing pipe fitting according to claim 5, characterized in that: The gas medium introduced in step D) is compressed gas.

7. The molding method of the PVC-O double-socket reducing pipe fitting according to claim 5 or 6, characterized in that: The temperature deviation of the preheated PVC-U pipe in step A) shall not exceed ±1.5°C.