A low-temperature superconducting wire welding packaging structure and method for cooling equipment
By adopting the assembly form of low-temperature superconducting wire welding packaging structure in the cooling equipment, the difficulty of superconducting wire processing and welding joint wiring during the welding process is solved, and the compact packaging and insulation of welding joints is achieved, ensuring the high efficiency of the equipment Refrigerate and operate stably.
Patent Information
- Application Number
- CN202110307354.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-03-23
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2041-03-23
AI Technical Summary
In the cooling-conducting equipment, the welding process of superconducting wires has problems such as difficult to process superconducting wires, difficulty in wiring welding joints, large solder joints, difficulty in insulating welding joints packaging, and vulnerability in cooling-conducting insulation materials, which affects welding efficiency and equipment Overall cooling rate.
A low-temperature superconducting wire welding and packaging structure and method are adopted, including an insulated base, an insulated cold conducting substrate, a metal substrate, a metal top cover, an insulated top cover, a first superconducting wire and a second superconducting wire, which is carried out through assembly form Welding operation provides greater bending space and insulation measures to ensure the stability of the solder joints and the cooling effect.
It realizes the convenient processing of superconducting wires and wiring of solder joints, reduces the volume of solder joints, ensures the insulating and the stability of the cold-conducting material, and avoids the problems of excessive space occupied by the equipment and damage to the insulating material.
Smart Images

Figure CN115117645B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of superconducting wire welding and packaging, and in particular to a low-temperature superconducting wire welding and packaging structure and method for cooling equipment. Background Art
[0002] Superconducting wires made of low-temperature metal materials have zero resistance characteristics under extremely low temperature conditions and play an important role in technical and engineering applications that require high currents and strong magnetic fields. In the application of low-temperature superconducting technology, welding problems between superconducting wires are inevitable. Due to the extremely low temperature zero resistance characteristics of superconducting wires, the welding process of superconducting wires is quite different from that of traditional ordinary wires. To ensure the quality of welding, in conduction-cooled superconducting equipment, the welding of superconducting wires must focus on three points: the weld has a good cooling effect, avoids the generation of hot spots inside the weld, and enhances the stability of the weld.
[0003] The conduction-cooled superconducting equipment is completely cooled by the cold conduction of the cold head. Therefore, all the solder joints of the superconducting wires inside the equipment must be in direct contact with the internal mechanical structure to ensure that the external cold energy during equipment cooling quickly enters the solder joints for cooling, and to ensure that the heat generated inside the solder joints can be discharged in time when the equipment is running. Too low a conduction effect will lead to a decrease in the overall cooling rate of the equipment, and the heat generated inside the solder joints cannot be discharged in time, resulting in quenching, etc., affecting the steady-state operation of the entire superconducting equipment.
[0004] The superconducting wire welding process currently widely used in conduction-cooling equipment mainly uses an open metal container as a container for superconducting wires and solder. First, two superconducting wires to be welded are introduced from the wire entry hole at the bottom of the open metal container, and then the two superconducting wires are successively subjected to the removal of the wrapping layer, the coiling operation and the welding operation in the metal container. Finally, the metal container and the conduction-cooling equipment are subjected to cooling and insulation treatment.
[0005] However, the existing welding process has the following disadvantages:
[0006] (1) Superconducting wires are difficult to handle
[0007] During welding, the metal container needs to be fixed in the equipment before subsequent operations are carried out to ensure a stable welding platform. However, the space in the superconducting equipment is limited, which makes it difficult to remove the outer sheath of the superconducting wire. In operations such as pickling and pre-welding of the wire, the narrow operating space will greatly affect the welding efficiency and quality.
[0008] (2) Difficulty in solder joint wiring
[0009] In the superconducting wire welding process, generally 5 to 10 or even more superconducting bare wires need to be welded together. Too many superconducting bare wires have a large wire diameter and a large bending radius. It is difficult to coil all the superconducting bare wires into a metal container, and there is a risk of damaging the superconducting bare wires.
[0010] (3) Large solder joint volume
[0011] When welding a large number of superconducting wires and long bare wires, a large metal container is required to ensure that all bare wires are fully immersed in the container and that there is enough welding material to completely wrap all bare wires. This results in the metal container often having a large volume, which places greater demands on the internal space of the equipment, affecting the compactness of the equipment; while increasing the volume of the equipment, it also reduces the overall cooling rate of the entire system.
[0012] (4) Difficulty in insulating solder joint packaging
[0013] Using metal containers as welding external packages ensures the cooling effect, but the package is very easy to contact with external mechanical structures and cause short circuits. The large volume and irregular shape of the metal container make it difficult to insulate and prone to damage.
[0014] (5) Cooling insulation materials are vulnerable
[0015] The insulating material between the metal container base and the mechanical structure is generally made of aluminum nitride, which is a material with high insulation and high thermal conductivity. The material is generally fixed between the metal container and the mechanical structure of the equipment by bolts. However, the material is fragile and brittle. During installation and equipment operation, the extrusion between the hardware and the friction of the installation bolts will cause the material to break, which poses a hidden danger to the insulation and stable operation of the equipment. Summary of the invention
[0016] The present invention provides a low-temperature superconducting wire welding packaging structure and method for cooling equipment, which can solve the technical problems in the prior art of difficult superconducting wire processing, difficult solder joint wiring, large solder joint volume, difficult solder joint packaging and insulation, and easy damage of cooling insulation materials.
[0017] According to one aspect of the present invention, there is provided a low-temperature superconducting wire welding packaging structure for a cooling device, the packaging structure comprising an insulating base, an insulating cooling substrate, a metal substrate, a metal top cover, an insulating top cover, a first superconducting wire, a second superconducting wire and solder;
[0018] A first through hole is formed on the end surface of the insulating base, an annular groove is formed on the upper end surface of the insulating base, and the axis of the first through hole coincides with the axis of the annular groove;
[0019] The insulating cold-conducting substrate and the metal substrate are both arranged in the first through hole and are both connected to the insulating base, the insulating cold-conducting substrate is arranged on the lower side of the metal substrate, and the lower end surface of the insulating cold-conducting substrate is on the same horizontal plane as the lower end surface of the insulating base;
[0020] The metal top cover and the insulating top cover are both covered in the annular groove, and the insulating top cover is arranged on the outer side of the metal top cover, the metal top cover and the metal base constitute an annular container for containing the solder, a first wiring groove is opened on the bottom of the side wall of the metal top cover, the depth of the first wiring groove is greater than the depth of the annular groove, a second through hole for pouring the solder is opened on the top of the metal top cover, a second wiring groove is opened on the bottom of the side wall of the insulating top cover, the depth of the second wiring groove is greater than the depth of the annular groove, and the positions of the first wiring groove and the second wiring groove are relatively arranged;
[0021] One end of the first superconducting wire is a first superconducting bare wire with the sheath removed, and the other end is a first superconducting busbar with the sheath not removed; one end of the second superconducting wire is a second superconducting bare wire with the sheath removed, and the other end is a second superconducting busbar with the sheath not removed; the first superconducting bare wire and the second superconducting bare wire are mutually wound and coiled into a plurality of turns of annular bare wire, and the diameter of each turn of the annular bare wire is smaller than the inner diameter of the metal top cover; the annular bare wire is arranged in the annular container, and the first superconducting busbar and the second superconducting busbar are arranged outside the annular container;
[0022] The solder is disposed in the annular container and is used for welding the first superconducting wire and the second superconducting wire.
[0023] Preferably, a spiral groove is provided on the inner wall of the metal top cover, and the annular bare wire is embedded in the spiral groove, and the spiral groove is used to limit the vertical displacement of the annular bare wire; the packaging structure also includes a supporting component, and the supporting component is arranged inside the metal top cover, and is used to limit the horizontal displacement of the annular bare wire.
[0024] Preferably, the inner diameter of the metal top cover is greater than or equal to 75 times the outer diameter of the first superconducting busbar and less than or equal to 80 times the outer diameter of the first superconducting busbar, wherein the outer diameter of the first superconducting busbar is the same as the outer diameter of the second superconducting busbar.
[0025] Preferably, the height of the metal top cover is greater than or equal to 8 times the outer diameter of the first superconducting busbar and less than or equal to 10 times the outer diameter of the first superconducting busbar.
[0026] Preferably, the thickness of the metal top cover is greater than or equal to the outer diameter of the first superconducting busbar and less than or equal to 1.5 times the outer diameter of the first superconducting busbar.
[0027] Preferably, the width of the annular groove is equal to the sum of the side wall thickness of the metal top cover and the side wall thickness of the insulating top cover, the inner diameter of the annular groove is the same as the inner diameter of the metal top cover, and the outer diameter of the annular groove is the same as the outer diameter of the insulating top cover.
[0028] Preferably, the diameter of the insulating cooling substrate, the diameter of the metal substrate and the diameter of the first through hole are all the same.
[0029] Preferably, the thickness of the insulating base is equal to the sum of the thickness of the insulating cooling substrate and the thickness of the metal substrate.
[0030] According to another aspect of the present invention, a method for welding and packaging low-temperature superconducting wires for cooling equipment is provided, wherein the packaging structure in the above embodiment is used for welding and packaging, and the method comprises:
[0031] Fixing the insulating base at a preset position, and placing the insulating cooling substrate in the first through hole, so that the lower end surface of the insulating cooling substrate and the lower end surface of the insulating base are on the same horizontal plane;
[0032] Placing the metal substrate on the upper side of the insulating cooling substrate;
[0033] Remove the coating from one end of the first superconducting wire and one end of the second superconducting wire to obtain a first superconducting bare wire and a second superconducting bare wire of preset lengths;
[0034] The first superconducting bare wire and the second superconducting bare wire are wound and pre-welded to connect the first superconducting bare wire and the second superconducting bare wire, and the first superconducting bare wire and the second superconducting bare wire are wound into a ring-shaped bare wire with multiple turns.
[0035] Placing the annular bare wire on the metal base and placing the metal top cover on the annular groove;
[0036] Pour the molten solder from the second through hole into the annular container formed by the metal top cover and the metal base, so that the solder fully immerses the annular bare wire, and cools the solder;
[0037] An insulating top cover is placed on the annular groove to complete the welding of the first superconducting wire and the second superconducting wire.
[0038] According to another aspect of the present invention, a method for welding and packaging low-temperature superconducting wires for cooling equipment is provided, wherein the packaging structure in the above embodiment is used for welding and packaging, and the method comprises:
[0039] Fixing the insulating base at a preset position, and placing the insulating cooling substrate in the first through hole, so that the lower end surface of the insulating cooling substrate and the lower end surface of the insulating base are on the same horizontal plane;
[0040] Placing the metal substrate on the upper side of the insulating cooling substrate;
[0041] Remove the coating from one end of the first superconducting wire and one end of the second superconducting wire to obtain a first superconducting bare wire and a second superconducting bare wire of preset lengths;
[0042] The first superconducting bare wire and the second superconducting bare wire are wound and pre-welded to connect the first superconducting bare wire and the second superconducting bare wire, and the first superconducting bare wire and the second superconducting bare wire are wound into a ring-shaped bare wire with multiple turns.
[0043] Embed the annular bare wire into the spiral groove of the metal top cover, place the supporting component inside the metal top cover to fix the annular bare wire together with the spiral groove, and cover the metal top cover on the annular groove;
[0044] Pour the molten solder from the second through hole into the annular container formed by the metal top cover and the metal base, so that the solder fully immerses the annular bare wire, and cools the solder;
[0045] An insulating top cover is placed on the annular groove to complete the welding of the first superconducting wire and the second superconducting wire.
[0046] Compared with the prior art, the technical solution of the present invention has the following beneficial effects:
[0047] (1) Superconducting wires are easy to handle.
[0048] Since the packaging structure is in the form of assembly, the pretreatment of the superconducting wire (removal of the wrapping layer, pickling, pre-welding, etc.) is not limited by the installation position of the welding container. The wire can be pretreated first, and then placed on the metal substrate for solder pouring and subsequent packaging operations.
[0049] (2) Convenient solder joint wiring
[0050] The package structure is flat in form and has a larger diameter, providing a higher bending space for the coiled wire and making it easier to route the superconducting bare wire inside the solder joint.
[0051] (3) Compact packaging structure
[0052] The package structure is flat with a larger diameter and a smaller height, making it easier for the solder joints to be installed in the gaps inside the device without the need to reserve additional larger solder joint space.
[0053] (4) Perfect insulation packaging
[0054] The insulating base, insulating cooling substrate and insulating top cover ensure that the entire packaging structure has complete insulation measures, ensuring that the entire solder joint will not short-circuit with any external mechanical structure.
[0055] (5) Reliable cooling material
[0056] The insulating cooling substrate at the bottom of the packaging structure is only fixed by the metal substrate on its upper side, and the force is evenly distributed, thus avoiding problems such as material breakage caused by assembly and equipment operation vibration. BRIEF DESCRIPTION OF THE DRAWINGS
[0057] The included drawings are used to provide a further understanding of the embodiments of the present invention, which constitute a part of the specification, are used to illustrate the embodiments of the present invention, and together with the text description, explain the principles of the present invention. Obviously, the drawings in the following description are only some embodiments of the present invention, and for ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0058] Figure 1 A schematic diagram of a low-temperature superconducting wire welding packaging structure for a cooling device provided according to an embodiment of the present invention is shown;
[0059] Figure 2 Shows Figure 1 A top view schematic diagram of the combination of the middle insulating base, the insulating cooling base and the metal base;
[0060] Figure 3 Shows Figure 1 A bottom view schematic diagram of the combination of the middle insulating base, the insulating cooling base and the metal base;
[0061] Figure 4 Shows Figure 1 Schematic diagram of the combination of the middle insulating base, the metal top cover and the insulating top cover;
[0062] Figure 5 A schematic diagram of a metal top cover with a spiral groove provided according to an embodiment of the present invention is shown;
[0063] Figure 6 Shows Figure 5 A schematic diagram of the metal top cover and the supporting components after being assembled;
[0064] Figure 7 A flow chart showing a method for welding and packaging low-temperature superconducting wires for cooling equipment provided in accordance with an embodiment of the present invention is shown;
[0065] Figure 8 A schematic diagram showing two superconducting bare wires wound into a ring-shaped bare wire with multiple turns according to an embodiment of the present invention is shown;
[0066] Fig. 9 A schematic diagram showing a method of placing a ring-shaped bare wire wound into multiple turns on a metal substrate according to an embodiment of the present invention is shown;
[0067] Fig.10 A schematic diagram showing a metal top cover provided in an annular groove according to an embodiment of the present invention is shown;
[0068] Fig.11 A schematic diagram of a package structure after welding is shown according to an embodiment of the present invention;
[0069] Fig.12 A flow chart of a low-temperature superconducting wire welding and packaging method for cooling equipment provided in accordance with another embodiment of the present invention is shown.
[0070] Description of Reference Numerals
[0071] 10. Insulating base; 11. First through hole; 12. Annular groove; 13. Connecting hole;
[0072] 20. Insulated cooling substrate;
[0073] 30. Metal substrate;
[0074] 40. Metal top cover; 41. First wiring groove; 42. Second through hole; 43. Spiral groove;
[0075] 50. Insulation top cover; 51. Second wiring trough;
[0076] 60. a first superconducting wire; 61. a first superconducting bare wire; 62. a first superconducting busbar;
[0077] 70. second superconducting wire; 71. second superconducting bare wire; 72. second superconducting busbar;
[0078] 90. Support components. DETAILED DESCRIPTION
[0079] It should be noted that, in the absence of conflict, the embodiments in this application and the features in the embodiments can be combined with each other. The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. The following description of at least one exemplary embodiment is actually only illustrative and is by no means intended to limit the present invention and its application or use. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0080] It should be noted that the terms used herein are only for describing specific embodiments and are not intended to limit the exemplary embodiments according to the present application. As used herein, unless the context clearly indicates otherwise, the singular form is also intended to include the plural form. In addition, it should be understood that when the terms "comprise" and / or "include" are used in this specification, it indicates the presence of features, steps, operations, devices, components and / or combinations thereof.
[0081] Unless otherwise specifically stated, the relative arrangement of the parts and steps described in these embodiments, numerical expressions and numerical values do not limit the scope of the present invention. At the same time, it should be understood that, for ease of description, the sizes of the various parts shown in the accompanying drawings are not drawn according to the actual proportional relationship. The technology, method and equipment known to ordinary technicians in the relevant field may not be discussed in detail, but in appropriate cases, the technology, method and equipment should be regarded as a part of the authorization specification. In all examples shown and discussed here, any specific value should be interpreted as being merely exemplary, rather than as a limitation. Therefore, other examples of exemplary embodiments may have different values. It should be noted that similar reference numerals and letters represent similar items in the following drawings, so once a certain item is defined in an accompanying drawing, it does not need to be further discussed in subsequent drawings.
[0082] like Figure 1-Figure 4 As shown, the present invention provides a low-temperature superconducting wire welding packaging structure for a cooling device, the packaging structure comprising an insulating base 10, an insulating cooling substrate 20, a metal substrate 30, a metal top cover 40, an insulating top cover 50, a first superconducting wire 60, a second superconducting wire 70 and solder;
[0083] A first through hole 11 is formed on the end surface of the insulating base 10, and an annular groove 12 is formed on the upper end surface of the insulating base 10, wherein the axis of the first through hole 11 coincides with the axis of the annular groove 12;
[0084] The insulating cold-conducting substrate 20 and the metal substrate 30 are both disposed in the first through hole 11 and are both connected to the insulating base 10. The insulating cold-conducting substrate 20 is disposed on the lower side of the metal substrate 30, and the lower end surface of the insulating cold-conducting substrate 20 is on the same horizontal plane as the lower end surface of the insulating base 10.
[0085] The metal top cover 40 and the insulating top cover 50 are both covered in the annular groove 12, and the insulating top cover 50 is arranged on the outer side of the metal top cover 40. The metal top cover 40 and the metal base 30 constitute an annular container for containing the solder. A first wiring groove 41 is opened on the bottom of the side wall of the metal top cover 40, and the depth of the first wiring groove 41 is greater than the depth of the annular groove 12. A second through hole 42 for pouring the solder is opened on the top of the metal top cover 40. A second wiring groove 51 is opened on the bottom of the side wall of the insulating top cover 50, and the depth of the second wiring groove 51 is greater than the depth of the annular groove 12. The positions of the first wiring groove 41 and the second wiring groove 51 are relatively arranged;
[0086] One end of the first superconducting wire 60 is a first superconducting bare wire 61 with the sheath removed, and the other end is a first superconducting busbar 62 with the sheath not removed; one end of the second superconducting wire 70 is a second superconducting bare wire 71 with the sheath removed, and the other end is a second superconducting busbar 72 with the sheath not removed; the first superconducting bare wire 61 and the second superconducting bare wire 71 are mutually intertwined and coiled into a plurality of turns of annular bare wire, and the diameter of each turn of the annular bare wire is smaller than the inner diameter of the metal top cover 40; the annular bare wire is arranged in the annular container, and the first superconducting busbar 62 and the second superconducting busbar 72 are arranged outside the annular container;
[0087] The solder is disposed in the annular container and is used to weld the first superconducting wire 60 and the second superconducting wire 70 .
[0088] Compared with the prior art, the present invention has the following beneficial effects:
[0089] (1) Superconducting wires are easy to handle.
[0090] Since the packaging structure is in the form of assembly, the pretreatment of the superconducting wire (removal of the wrapping layer, pickling, pre-welding, etc.) is not limited by the installation position of the welding container. The wire can be pretreated first, and then placed on the metal substrate for solder pouring and subsequent packaging operations.
[0091] (2) Convenient solder joint wiring
[0092] The package structure is flat in form and has a larger diameter, providing a higher bending space for the coiled wire and making it easier to route the superconducting bare wire inside the solder joint.
[0093] (3) Compact packaging structure
[0094] The package structure is flat with a larger diameter and a smaller height, making it easier for the solder joints to be installed in the gaps inside the device without the need to reserve additional larger solder joint space.
[0095] (4) Perfect insulation packaging
[0096] The insulating base, insulating cooling substrate and insulating top cover ensure that the entire packaging structure has complete insulation measures, ensuring that the entire solder joint will not short-circuit with any external mechanical structure.
[0097] (5) Reliable cooling material
[0098] The insulating cooling substrate at the bottom of the packaging structure is only fixed by the metal substrate on its upper side, and the force is evenly distributed, thus avoiding problems such as material breakage caused by assembly and equipment operation vibration.
[0099] According to an embodiment of the present invention, Figure 5 and Figure 6 As shown, a spiral groove 43 is provided on the inner wall of the metal top cover 40, and the annular bare wire is embedded in the spiral groove 43. The spiral groove 43 is used to limit the displacement of the annular bare wire in the vertical direction; the packaging structure also includes a support component 90, which is arranged inside the metal top cover 40 and is used to limit the displacement of the annular bare wire in the horizontal direction. The fixing of the annular bare wire is achieved through the cooperation of the spiral groove 43 and the support component 90, so that each turn of the annular bare wire is fully immersed in the solder, increasing the contact area with the solder and reducing the contact resistance.
[0100] For example, the support member 90 may be a "X" shaped structure that matches the inner diameter of the metal cover 40, or may be an "*" shaped structure, a "M" shaped structure, or other structures. The present invention does not limit the shape of the support member 90, as long as it can achieve the fixing effect of the annular bare wire.
[0101] According to one embodiment of the present invention, the inner diameter of the metal top cover 40 is greater than or equal to 75 times the outer diameter of the first superconducting busbar 62 and less than or equal to 80 times the outer diameter of the first superconducting busbar 62, wherein the outer diameter of the first superconducting busbar 62 is the same as the outer diameter of the second superconducting busbar 72.
[0102] According to an embodiment of the present invention, the height of the metal top cover 40 is greater than or equal to 8 times the outer diameter of the first superconducting busbar 62 and less than or equal to 10 times the outer diameter of the first superconducting busbar 62 .
[0103] According to an embodiment of the present invention, the thickness of the metal cap 40 is greater than or equal to the outer diameter of the first superconducting busbar 62 and less than or equal to 1.5 times the outer diameter of the first superconducting busbar 62 .
[0104] Through the above arrangement, the packaging structure body has a larger diameter, a smaller height, and a flat structure, which provides a higher bending space for the coiled wire, makes it easier to wire the superconducting bare wire inside the solder joint, and at the same time, makes the solder joint easier to install in the gap inside the equipment without reserving a larger additional solder joint space.
[0105] According to an embodiment of the present invention, the width of the annular groove 12 is equal to the sum of the side wall thickness of the metal top cover 40 and the side wall thickness of the insulating top cover 50, the inner diameter of the annular groove 12 is the same as the inner diameter of the metal top cover 40, and the outer diameter of the annular groove 12 is the same as the outer diameter of the insulating top cover 50. Through the above arrangement, the metal top cover 40 and the insulating top cover 50 can be just stuck in the annular groove 12, which is convenient for installation and fixing.
[0106] The metal top cover 40 and the metal base 30 together form a metal container for holding solder. During the welding process, the metal top cover 40, the metal base 30, the solder and the annular bare wire form an integral structure, which is also the solder joint. Therefore, the metal top cover 40 only needs to be placed in the annular groove 12 without any additional connection operation. The insulating top cover 50, the insulating cold-conducting base 20 and the insulating base 10 together form an insulating housing. The insulating top cover 50 and the insulating base 10 can be assembled by snapping, gluing or interference fit.
[0107] According to an embodiment of the present invention, the diameter of the insulating cooling substrate 20 , the diameter of the metal substrate 30 and the diameter of the first through hole 11 are all the same.
[0108] The insulating cooling substrate 20 and the metal substrate 30 can be assembled with the insulating base 10 by means of snap-fit, gluing or interference fit.
[0109] According to an embodiment of the present invention, the thickness of the insulating base 10 is equal to the sum of the thickness of the insulating cooling substrate 20 and the thickness of the metal substrate 30 .
[0110] According to the actual wiring space requirements, the shape of the packaging structure can be a cylinder or a polygonal prism.
[0111] In the present invention, Wood's metal may be used as the solder.
[0112] Furthermore, the insulating base 10 is also provided with a connecting hole 13, and the connecting hole 13 is used to fix the packaging structure in the cooling device to provide a stable platform for the subsequent welding process.
[0113] Figure 7 A flow chart of a low-temperature superconducting wire welding and packaging method for a cooling device provided in accordance with an embodiment of the present invention is shown. Figure 7As shown, the present invention provides a low-temperature superconducting wire welding packaging method for cooling equipment, which uses the packaging structure in the above embodiment for welding packaging, and the method includes:
[0114] S11, fixing the insulating base 10 at a preset position, and placing the insulating cold-conducting substrate 20 in the first through hole 11, so that the lower end surface of the insulating cold-conducting substrate 20 and the lower end surface of the insulating base 10 are on the same horizontal plane;
[0115] S12, placing the metal substrate 30 on the upper side of the insulating cooling substrate 20;
[0116] S13, removing the coating from one end of the first superconducting wire 60 and one end of the second superconducting wire 70 to obtain a first superconducting bare wire 61 and a second superconducting bare wire 71 of preset lengths;
[0117] S14, pre-welding the first superconducting bare wire 61 and the second superconducting bare wire 71 after winding them, so that the first superconducting bare wire 61 and the second superconducting bare wire 71 are fixedly connected, and the first superconducting bare wire 61 and the second superconducting bare wire 71 after being fixedly connected are coiled into a ring-shaped bare wire with multiple turns, such as Figure 8 As shown;
[0118] S15, placing the ring-shaped bare wire on the metal substrate 30, such as Fig. 9 As shown, the metal cover 40 is placed on the annular groove 12, as shown in FIG. Fig.10 As shown;
[0119] S16, pouring the molten solder from the second through hole 42 into the annular container formed by the metal top cover 40 and the metal base 30, so that the solder fully immerses the annular bare wire, and cooling the solder;
[0120] S17, cover the insulating top cover 50 on the annular groove 12 to complete the welding of the first superconducting wire 60 and the second superconducting wire 70, as shown in FIG. Fig.11 shown.
[0121] Compared with the prior art, the present invention has the following beneficial effects:
[0122] (1) Superconducting wires are easy to handle.
[0123] Since the packaging structure is in the form of assembly, the pretreatment of the superconducting wire (removal of the wrapping layer, pickling, pre-welding, etc.) is not limited by the installation position of the welding container. The wire can be pretreated first, and then placed on the metal substrate for solder pouring and subsequent packaging operations.
[0124] (2) Convenient solder joint wiring
[0125] The package structure is flat in form and has a larger diameter, providing a higher bending space for the coiled wire and making it easier to route the superconducting bare wire inside the solder joint.
[0126] (3) Compact packaging structure
[0127] The package structure is flat with a larger diameter and a smaller height, making it easier for the solder joints to be installed in the gaps inside the device without the need to reserve additional larger solder joint space.
[0128] (4) Perfect insulation packaging
[0129] The insulating base, insulating cooling substrate and insulating top cover ensure that the entire packaging structure has complete insulation measures, ensuring that the entire solder joint will not short-circuit with any external mechanical structure.
[0130] (5) Reliable cooling material
[0131] The insulating cooling substrate at the bottom of the packaging structure is only fixed by the metal substrate on its upper side, and the force is evenly distributed, thus avoiding problems such as material breakage caused by assembly and equipment operation vibration.
[0132] In S11 of the present invention, the insulating cooling substrate 20 is placed on the same horizontal plane as the lower end surface of the insulating base 10 so that the insulating cooling substrate 20 is in contact with the cooling device; the insulating cooling substrate 20 and the insulating base 10 can be assembled by snapping, gluing or interference fit.
[0133] In S12 of the present invention, the metal substrate 30 and the insulating base 10 can be assembled by snapping, gluing or interference fit.
[0134] In S14 of the present invention, in order to increase the contact area of the solder joint, the first superconducting bare wire 61 and the second superconducting bare wire 71 are wound and arranged. In order to ensure that the two superconducting bare wires do not loosen after winding, indium (solder) can be used to pre-weld the two superconducting bare wires after winding so that the two superconducting bare wires are fixed together.
[0135] In S16 of the present invention, the solder may be a Wood's alloy. The annular bare wire is fully immersed in the Wood's alloy, thereby achieving full contact between the Wood's alloy and the annular bare wire, reducing contact resistance; and at the same time avoiding the problem of vacancies inside the solder joint and wire friction. After cooling, the Wood's alloy solidifies, achieving welding of the annular bare wire, that is, welding of the first superconducting wire 60 and the second superconducting wire 70.
[0136] In S17 of the present invention, the insulating top cover 50 and the insulating base 10 can be assembled by snapping, gluing or interference fit.
[0137] Fig.12 A flow chart of a low-temperature superconducting wire welding and packaging method for a cooling device provided in accordance with another embodiment of the present invention is shown. Fig.12 As shown, the present invention also provides a low-temperature superconducting wire welding packaging method for cooling equipment. When the metal top cover 40 has a spiral groove 43, the welding packaging is performed through the following steps:
[0138] S21, fixing the insulating base 10 at a preset position, and placing the insulating cold-conducting substrate 20 in the first through hole 11, so that the lower end surface of the insulating cold-conducting substrate 20 and the lower end surface of the insulating base 10 are on the same horizontal plane;
[0139] S22, placing the metal substrate 30 on the upper side of the insulating cooling substrate 20;
[0140] S23, removing the coating from one end of the first superconducting wire 60 and one end of the second superconducting wire 70 to obtain a first superconducting bare wire 61 and a second superconducting bare wire 71 of preset lengths;
[0141] S24, pre-welding the first superconducting bare wire 61 and the second superconducting bare wire 71 after winding them, so that the first superconducting bare wire 61 and the second superconducting bare wire 71 are fixedly connected, and the first superconducting bare wire 61 and the second superconducting bare wire 71 after being fixedly connected are coiled into a ring-shaped bare wire with multiple turns;
[0142] S25, embed the annular bare wire into the spiral groove 43 of the metal cover 40, place the support component 90 inside the metal cover 40 to fix the annular bare wire together with the spiral groove 43, and cover the metal cover 40 on the annular groove 12;
[0143] S26, pouring the molten solder from the second through hole 42 into the annular container formed by the metal top cover 40 and the metal base 30, so that the solder fully immerses the annular bare wire, and cooling the solder;
[0144] S27 , placing the insulating top cover 50 on the annular groove 12 to complete the welding of the first superconducting wire 60 and the second superconducting wire 70 .
[0145] By adopting the packaging structure or packaging method of the present invention, the contact area between superconducting wires can be increased as much as possible, the contact resistance can be reduced, and wire friction can be avoided, thereby ensuring the stability between the soldering point and the wires in its vicinity, thereby preventing the soldering point from generating local hot spots, thereby avoiding the phenomenon of the entire superconducting circuit being quenched due to the superconducting wire heating up and the normal operation of the equipment being interrupted.
[0146] By adopting the packaging structure or packaging method of the present invention, the solder joint itself is reinforced to prevent the solder joint from being broken due to external mechanical tensile force or tangential force. At the same time, the solder joint itself is insulated and fixed to prevent the solder joint from vibrating during equipment operation and generating friction heat with other external parts or equipment, which further causes the superconducting wire inside the solder joint to quench.
[0147] In the description of the present invention, it is necessary to understand that the directions or positional relationships indicated by directional words such as "front, back, up, down, left, right", "lateral, vertical, perpendicular, horizontal" and "top, bottom" are usually based on the directions or positional relationships shown in the drawings. They are only for the convenience of describing the present invention and simplifying the description. Unless otherwise specified, these directional words do not indicate or imply that the devices or elements referred to must have a specific direction or be constructed and operated in a specific direction. Therefore, they cannot be understood as limiting the scope of protection of the present invention. The directional words "inside and outside" refer to the inside and outside relative to the contours of each component itself.
[0148] For ease of description, spatially relative terms such as "above", "above", "on the upper surface of", "above", etc. may be used here to describe the spatial positional relationship between a device or feature and other devices or features as shown in the figure. It should be understood that spatially relative terms are intended to include different orientations of the device in use or operation in addition to the orientation described in the figure. For example, if the device in the accompanying drawings is inverted, the device described as "above other devices or structures" or "above other devices or structures" will be positioned as "below other devices or structures" or "below other devices or structures". Thus, the exemplary term "above" can include both "above" and "below". The device can also be positioned in other different ways (rotated 90 degrees or in other orientations), and the spatially relative descriptions used here are interpreted accordingly.
[0149] In addition, it should be noted that the use of terms such as "first" and "second" to limit components is only for the convenience of distinguishing the corresponding components. If not otherwise stated, the above terms have no special meaning and therefore cannot be understood as limiting the scope of protection of the present invention.
[0150] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A low-temperature superconducting wire welding packaging structure for cooling equipment, characterized in that: The packaging structure comprises an insulating base (10), an insulating cold-conducting substrate (20), a metal substrate (30), a metal top cover (40), an insulating top cover (50), a first superconducting wire (60), a second superconducting wire (70) and solder; A first through hole (11) is provided on the end surface of the insulating base (10), an annular groove (12) is provided on the upper end surface of the insulating base (10), and the axis of the first through hole (11) coincides with the axis of the annular groove (12); The insulating cold-conducting substrate (20) and the metal substrate (30) are both arranged in the first through hole (11) and are both connected to the insulating base (10); the insulating cold-conducting substrate (20) is arranged on the lower side of the metal substrate (30); and the lower end surface of the insulating cold-conducting substrate (20) and the lower end surface of the insulating base (10) are on the same horizontal plane; The metal cover (40) and the insulating cover (50) are both covered in the annular groove (12), and the insulating cover (50) is arranged on the outer side of the metal cover (40). The metal cover (40) and the metal base (30) form an annular container for containing the solder. A first wiring groove (41) is provided on the bottom of the side wall of the metal cover (40), and the depth of the first wiring groove (41) is greater than the depth of the annular groove (12). A second through hole (42) for pouring the solder is provided on the top of the metal cover (40). A second wiring groove (51) is provided on the bottom of the side wall of the insulating cover (50), and the depth of the second wiring groove (51) is greater than the depth of the annular groove (12). The positions of the first wiring groove (41) and the second wiring groove (51) are relatively arranged. One end of the first superconducting wire (60) is a first superconducting bare wire (61) with the sheath removed, and the other end is a first superconducting busbar (62) with the sheath not removed; one end of the second superconducting wire (70) is a second superconducting bare wire (71) with the sheath removed, and the other end is a second superconducting busbar (72) with the sheath not removed; the first superconducting bare wire (61) and the second superconducting bare wire (71) are mutually intertwined and coiled into a plurality of turns of annular bare wire, the diameter of each turn of the annular bare wire is smaller than the inner diameter of the metal top cover (40); the annular bare wire is arranged in the annular container, and the first superconducting busbar (62) and the second superconducting busbar (72) are arranged outside the annular container; The solder is arranged in the annular container and is used for welding the first superconducting wire (60) and the second superconducting wire (70).
2. The packaging structure according to claim 1, characterized in that: The inner wall of the metal top cover (40) is provided with a spiral groove (43), the annular bare wire is embedded in the spiral groove (43), and the spiral groove (43) is used to limit the displacement of the annular bare wire in the vertical direction; the packaging structure also includes a supporting component (90), and the supporting component (90) is arranged inside the metal top cover (40) and is used to limit the displacement of the annular bare wire in the horizontal direction.
3. The packaging structure according to claim 1, characterized in that: The inner diameter of the metal top cover (40) is greater than or equal to 75 times the outer diameter of the first superconducting busbar (62) and less than or equal to 80 times the outer diameter of the first superconducting busbar (62), wherein the outer diameter of the first superconducting busbar (62) is the same as the outer diameter of the second superconducting busbar (72).
4. The packaging structure according to claim 3, characterized in that: The height of the metal cap (40) is greater than or equal to 8 times the outer diameter of the first superconducting busbar (62) and less than or equal to 10 times the outer diameter of the first superconducting busbar (62).
5. The packaging structure according to claim 4, characterized in that: The thickness of the metal cap (40) is greater than or equal to the outer diameter of the first superconducting busbar (62) and less than or equal to 1.5 times the outer diameter of the first superconducting busbar (62).
6. The packaging structure according to claim 1, characterized in that: The width of the annular groove (12) is equal to the sum of the side wall thickness of the metal top cover (40) and the side wall thickness of the insulating top cover (50), the inner diameter of the annular groove (12) is the same as the inner diameter of the metal top cover (40), and the outer diameter of the annular groove (12) is the same as the outer diameter of the insulating top cover (50).
7. The packaging structure according to claim 1, characterized in that: The diameter of the insulating cooling substrate (20), the diameter of the metal substrate (30) and the diameter of the first through hole (11) are all the same.
8. The packaging structure according to claim 1, characterized in that: The thickness of the insulating base (10) is equal to the sum of the thickness of the insulating cold-conducting substrate (20) and the thickness of the metal substrate (30).
9. A low-temperature superconducting wire welding and packaging method for cooling equipment, characterized in that: The packaging structure according to any one of claims 1 or 3 to 8 is used for welding packaging, and the method comprises: The insulating base (10) is fixed at a preset position, and the insulating cold-conducting substrate (20) is placed in the first through hole (11), so that the lower end surface of the insulating cold-conducting substrate (20) and the lower end surface of the insulating base (10) are on the same horizontal plane; Placing the metal substrate (30) on the upper side of the insulating cooling substrate (20); Removing the coating layer from one end of the first superconducting wire (60) and one end of the second superconducting wire (70) to obtain a first superconducting bare wire (61) and a second superconducting bare wire (71) of a preset length; The first superconducting bare wire (61) and the second superconducting bare wire (71) are wound and then pre-welded to securely connect the first superconducting bare wire (61) and the second superconducting bare wire (71), and the securely connected first superconducting bare wire (61) and the second superconducting bare wire (71) are coiled into a ring-shaped bare wire with multiple turns; Placing the annular bare wire on the metal base (30), and placing the metal top cover (40) on the annular groove (12); Pouring molten solder from the second through hole (42) into an annular container formed by the metal top cover (40) and the metal base (30) so that the solder fully immerses the annular bare wire, and performing a temperature reduction process on the solder; An insulating top cover (50) is placed on the annular groove (12) to complete the welding of the first superconducting wire (60) and the second superconducting wire (70).
10. A low-temperature superconducting wire welding and packaging method for cooling equipment, characterized in that: The packaging structure of claim 2 is used for welding packaging, and the method comprises: The insulating base (10) is fixed at a preset position, and the insulating cold-conducting substrate (20) is placed in the first through hole (11), so that the lower end surface of the insulating cold-conducting substrate (20) and the lower end surface of the insulating base (10) are on the same horizontal plane; Placing the metal substrate (30) on the upper side of the insulating cooling substrate (20); Removing the coating layer from one end of the first superconducting wire (60) and one end of the second superconducting wire (70) to obtain a first superconducting bare wire (61) and a second superconducting bare wire (71) of a preset length; The first superconducting bare wire (61) and the second superconducting bare wire (71) are wound and then pre-welded to securely connect the first superconducting bare wire (61) and the second superconducting bare wire (71), and the securely connected first superconducting bare wire (61) and the second superconducting bare wire (71) are coiled into a ring-shaped bare wire with multiple turns; The annular bare wire is embedded in the spiral groove (43) of the metal top cover (40), the supporting component (90) is placed inside the metal top cover (40) to fix the annular bare wire together with the spiral groove (43), and the metal top cover (40) is placed on the annular groove (12); Pouring molten solder from the second through hole (42) into an annular container formed by the metal top cover (40) and the metal base (30) so that the solder fully immerses the annular bare wire, and performing a temperature reduction process on the solder; An insulating top cover (50) is placed on the annular groove (12) to complete the welding of the first superconducting wire (60) and the second superconducting wire (70).