A magnetic starch coating solution, its preparation and use, and smoke-generating particles and preparation

By spraying magnetic starch coating on the aerosol particles and using electromagnetic heating, the problem of moisture absorption of the aerosol particles and contact with the heating device is solved, and stability and uniform heating are achieved.

CN115281364BActive Publication Date: 2024-10-25CHINA TOBACCO YUNNAN IND
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202211010078.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-08-22
Publication Date
2024-10-25
Estimated Expiration
2042-08-22

AI Technical Summary

Technical Problem

Aerosol particle products tend to absorb moisture during storage and transportation, resulting in particle adhesion and agglomeration, increased resistance, and poor suction. In addition, the induction heating element of the induction heating device comes into contact with the aerosol particles, causing cleaning and odor absorption effects. problem.

Method used

A magnetic starch coating solution is used, which contains magnetic nanoparticles and starch solution. A coating layer is formed on the surface of the smoking particles through a spray coating method, and uniform heating is achieved under electromagnetic heating.

Benefits of technology

It effectively prevents aerosol particles from absorbing moisture, maintains stability and odor absorption, reduces cleaning problems of heating devices, and the coating process is low-cost and simple to operate.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The present invention belongs to the technical field of heated cigarettes, and specifically relates to a magnetic starch coating solution, its preparation and use, and smoke-generating particles and their preparation. The coating solution contains: magnetic nanoparticles and starch solution. The smoke-generating particles contain: an outer magnetic starch coating layer and internal smoke-generating particles; the magnetic starch coating layer contains starch and a plurality of dispersed magnetic nanoparticles embedded in the starch. The present invention is the first to evenly distribute magnetic nanoparticles in a starch film coating. Compared with ordinary starch film coatings, the moisture-proof ability of aerosol particles is further improved, and it is not easy to absorb water and mildew, which effectively prolongs the shelf life of the particles, while also maintaining the smoking sensory stability of aerosol particle products.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of heated cigarettes, and in particular relates to a magnetic starch coating solution, preparation and use thereof, and smoke-generating particles and preparation thereof. Background Art

[0002] Coating can form a physical barrier on the surface of drugs and foods to prevent environmental factors such as light, oxygen or water vapor from affecting their chemical stability, thereby improving the stability of drugs or foods during manufacturing and storage. Coating is mostly used for various oral solid dosage forms, such as pharmaceutical tablets and capsules. Among them, film coating is the most widely used method to solve various problems encountered during drug production, transportation, storage and clinical use.

[0003] When the drug tablets or granules are stirred in a coating pan or fluidized bed, the coating mixture or coating liquid is sprayed onto the tablets or granules through a nozzle, forming a layer of coating liquid film on the surface of the tablets or granules.

[0004] Existing aerosol particle products use particles made from different granulation processes and different plant materials as the smoke-generating substrate. They are in the shape of regular or irregular particles. In addition to the main plant materials, they also contain smoke-generating agents (such as glycerin and propylene glycol), flavors and fragrances, and other additives. Common aerosol particle products on the market are products similar in appearance to cigarettes made by filling the above-mentioned smoke-generating particles in paper wrapping materials. When in use, the product is placed in a heating device for low-temperature baking and atomization to produce an inhalable aerosol.

[0005] Aerosol particles and aerosol particle products containing the particles are prone to moisture absorption during storage and transportation after manufacturing, which, on the one hand, causes adhesion and agglomeration between particles, resulting in increased resistance when inserting a heating sheet or needle, and poor airflow during inhalation; on the other hand, due to the increase in moisture content, the amount of smoke during inhalation becomes smaller and the inhalation taste becomes lighter. Although commercially available aerosol particle products generally use central resistive heating technology, induction heating technology has the advantages of faster heating rate and more uniform heat distribution compared to resistive heating technology, but the induction heating element of the conventional induction heating device is arranged in the aerosol generating device, and there are problems such as cleaning and affecting the inhalation taste caused by repeated contact between the surface of the induction heating element and the particles in the aerosol particle product. The existing patent (CN108135275A) discloses "coating an aerosol-forming substrate on the core of the sensor material to manufacture aerosol-generating particles", and such "multiple particles form aerosol-forming agglomerates" and aerosol-generating products, and the aerosol-generating products use built-in induction heating to generate inhalable aerosols. The receptor material is a "material that can absorb electromagnetic energy and convert it into heat", preferably a "metal receptor". The aerosol particles obtained by "coating" the aerosol-forming substrate on the receptor described in the patent still have the problem of moisture absorption because the aerosol-forming substrate is directly exposed to the air; on the other hand, the thermal and mechanical properties of the receptor (metal) and the aerosol-forming substrate (plants and organic matter) are quite different, and there may be a problem that the aerosol-forming substrate is not physically adhered tightly to the receptor surface, resulting in the aerosol-forming substrate being separated from the receptor surface or even falling off.

[0006] In order to solve the above-mentioned problems, the present invention is proposed. Summary of the invention

[0007] A first aspect of the present invention provides a magnetic starch coating solution, wherein the coating solution comprises: magnetic nanoparticles and a starch solution.

[0008] Preferably, the magnetic nanoparticles are ferroferric oxide nanoparticles. Of course, the magnetic nanoparticles can also be ferromagnetic iron nanoparticles, cobalt nanoparticles, nickel nanoparticles or other ferrite nanoparticles of ferromagnetism. In order to prevent the iron nanoparticles, cobalt nanoparticles and nickel nanoparticles from being corroded or oxidized, the iron nanoparticles, cobalt nanoparticles and nickel nanoparticles can be surface treated, such as coating a protective layer.

[0009] Preferably, the coating solution further comprises: an auxiliary agent;

[0010] The auxiliary agent is selected from: one or more of a plasticizer, a binder, an anti-adhesive agent and an excipient.

[0011] The second aspect of the present invention provides a method for preparing the magnetic starch coating solution described in the first aspect, wherein the preparation method adopts one of the following methods:

[0012] Method 1:

[0013] Adding an iron salt solution to a starch aqueous solution, mixing well, adding an alkali solution, adjusting the pH to 10-11, heating and mixing well, and further stirring at 80-100 degrees Celsius to promote starch gelatinization to obtain a starch gelatinized solution;

[0014] The starch gelatinized liquid is subjected to ultrasonic treatment, and the first auxiliary agent is added at the same time, and after further constant temperature ultrasonic treatment or homogenization for a certain period of time, degassing is performed to obtain a magnetic starch coating solution;

[0015] Method 2:

[0016] Mix starch and water and stir at 80 to 100 degrees Celsius to prepare a starch aqueous solution;

[0017] Adding magnetic nanoparticles;

[0018] After stirring, ultrasonic treatment is performed, and a second auxiliary agent is added at the same time. After further constant temperature ultrasonic treatment or homogenization for a certain period of time, degassing is performed to obtain a magnetic starch coating solution;

[0019] The first auxiliary agent and the second auxiliary agent are the same or different;

[0020] The first auxiliary agent and the second auxiliary agent are independently selected from: one or more of a plasticizer, a binder, an anti-adhesive agent and an excipient.

[0021] Preferably, the iron salt solution in the above method 1 is a divalent iron salt solution, or a mixed solution of a divalent iron salt solution and a trivalent iron salt solution.

[0022] When the iron salt solution is a divalent iron salt solution, a hydrogen peroxide solution needs to be added for partial oxidation.

[0023] When the iron salt solution is a mixed solution of a divalent iron salt solution and a trivalent iron salt solution, it is not necessary to add a hydrogen peroxide solution for oxidation.

[0024] The purpose of the above degassing is to prevent the presence of bubbles in the coating solution from causing the formation of air holes in the final coating, which affects the coating flatness and strength.

[0025] Preferably, in method 2, the particle size distribution of the magnetic nanoparticles is 10-30 nm. The purity of the magnetic nanoparticles added in method 2 is ≥ 95%.

[0026] The content of magnetic nanoparticles does not exceed 2% of the dry weight of starch.

[0027] The above method 1 is applicable to the case where the magnetic nanoparticles are ferroferric oxide nanoparticles.

[0028] The above method 2 is applicable to all magnetic nanoparticles.

[0029] The third aspect of the present invention provides use of the coating solution described in any one of the first aspects for coating smoky particles and then performing electromagnetic heating.

[0030] The fourth aspect of the present invention provides a smoke-generating particle, the smoke-generating particle comprising: an outer magnetic starch wrapping layer and an inner smoke-generating particle;

[0031] The magnetic starch coating layer comprises starch and a plurality of dispersed magnetic nanoparticles embedded in the starch.

[0032] The fifth aspect of the present invention provides a method for preparing the smoke-generating particles according to the fourth aspect, comprising the following steps:

[0033] Placing the smoke-generating particles in a coating device, spraying the magnetic starch coating solution described in any one of the first aspects from a spray gun disposed in the coating device to form a spray, thereby forming a coating on the surface of the smoke-generating particles;

[0034] The smoky particles coated with magnetic starch are heat treated to obtain the smoky particles.

[0035] The above technical solutions can be freely combined under the premise of no contradiction.

[0036] Compared with the prior art, the present invention has the following beneficial effects:

[0037] (1) Starch is the most commonly used biopolymer, with the advantages of biodegradability, non-toxicity and low cost. However, starch films are sensitive to moisture and brittle. In order to improve their application performance, plasticizers, other materials or even chemical modifications are usually added.

[0038] The present invention is the first to evenly distribute magnetic nanoparticles in a starch film coating, which further improves the moisture resistance of the aerosol particles compared to ordinary starch film coatings, making them less likely to absorb water and mildew, thereby effectively extending the shelf life of the particles while also maintaining the sensory stability of the aerosol particle products when being sucked.

[0039] (2) The coating process has little effect on the weight of aerosol particles, usually only increasing the weight of the particles by 2%-4%, and has little effect on the original properties of aerosol particles and the processing parameters of aerosol particle products.

[0040] (3) Starch and other coating materials are natural, cheap, and used in small amounts. The coating equipment is easy to operate, requires little manpower, and has low costs.

[0041] (4) Starch and other coating materials match the thermal and mechanical properties of plant-based granular materials. The starch film coating can adhere tightly to the surface of aerosol particles, ensuring that the coating will not fall off during transportation, manufacturing, and storage of the particles.

[0042] (5) The magnetic nanoparticles in the film coating are evenly distributed on the entire surface of the aerosol particles. When the alternating electromagnetic field acts on the particles, the magnetic nanoparticles on the surface of the particles induce heat, the coating shrinks due to the heat and peels off from the surface of the particles. The magnetic nanoparticles will directly contact the surface of the particles and heat the particles, which is beneficial to the heating of the outer layer of particles and makes the particles heated more evenly.

[0043] Furthermore, by selecting magnetic nanoparticles of appropriate particle size, adjusting the amount of magnetic nanoparticles added, and preparing starch film coatings of different thicknesses, it is helpful to adjust the heating temperature and heating rate of the aerosol particle product.

[0044] (6) Adding magnetic nanoparticles (such as ferroferric oxide nanoparticles) to starch films will improve the barrier properties and significantly improve the mechanical properties such as tensile strength and elongation at break. DETAILED DESCRIPTION

[0045] The present invention is further described below by way of examples, but is not limited to these examples. Experimental methods without specific conditions in the examples are usually carried out under conventional conditions and conditions described in the manual, or under conditions recommended by the manufacturer. The general equipment, materials, reagents, etc. used can be obtained from commercial sources unless otherwise specified. The raw materials required in the following examples and comparative examples are all commercially available.

[0046] The invention provides a method for preparing a magnetic starch film coating liquid and coating aerosol particles with the coating liquid. The method for preparing the magnetic starch film coating liquid includes a coprecipitation method and a direct addition method.

[0047] Specifically:

[0048] Method 1: Preparation of magnetic starch coating solution by coprecipitation

[0049] The basic principle is that starch (such as cassava starch) molecules have chain-like polar hydroxyl groups -OH, which can adsorb and embed Fe 2+ Ferrous ions and Fe 3+ When an alkaline solution is added to the mixture of starch and iron solution, the divalent iron ions and trivalent iron ions in the alkaline starch solution are instantly hydrolyzed and crystallized to form magnetic iron oxide nanoparticles. The ion equation is as follows:

[0050] Fe 2+ +2Fe 3+ +8OH - →Fe 3 O 4 +4H 2 O

[0051] Specific preparation process:

[0052] Take an appropriate amount of starch, prepare a starch aqueous solution of a certain concentration, add an appropriate amount of iron salt solution, mix well, add alkaline solution, adjust the pH to 10-11, heat to a certain temperature (such as 65°C) at a constant temperature and mix evenly. Further stir vigorously in a constant temperature water bath at about 90°C for a certain time (such as 30-40 minutes) to promote starch gelatinization. Ultrasonic treatment is performed on the starch gelatinized liquid, and a certain proportion of auxiliary agents is added at the same time. After further constant temperature ultrasound or homogenization for a certain period of time, degassing with a vacuum pump obtains a magnetic starch coating solution.

[0053] Method 2: Directly add Fe 3 O 4 Nanoparticles Preparation Magnetic Starch Coating Solution

[0054] A certain concentration of starch aqueous solution was prepared by vigorous stirring in a constant temperature water bath at about 90°C for 30-40 minutes. A certain amount of Fe was added based on the dry weight of starch. 3 O 4 Magnetic nanoparticles. After further vigorous stirring, ultrasonic treatment is performed, and a certain proportion of auxiliary agents are added at the same time. After further constant temperature ultrasonic treatment or homogenization for a certain period of time, degassing is performed with a vacuum pump to obtain a magnetic starch coating solution.

[0055] The preparation method of the magnetic starch coating liquid coated smoky particles is as follows:

[0056] The smoke particles are placed in a coating device (coating pan or fluidized coating machine), and the magnetic starch coating solution is sprayed from a spray gun disposed in the coating device to form a spray, thereby forming a coating on the surface of the smoke particles. The smoke particles coated with the magnetic starch coating are further subjected to heat treatment to obtain the smoke particle product of the present invention.

[0057] The specific process is:

[0058] The coating equipment can be a conventional coating pan, a mesh coating pan or a fluidized bed.

[0059] When coating is performed using a coating pan, the aerosol particles placed on the tablet bed are tumbled and passed through the spray area multiple times by the rotation of the drum on the inclined axis. The mesh coating pan can improve the drying efficiency of the coating because the dry air passes through the tablet bed. When the particles pass through the spray area, the coating liquid droplets are deposited on the surface of the particles to form a coating film. In each cycle, the particles pass through the spray area in different directions, so the surface of the particles facing the spray gun changes frequently, resulting in the coating of the entire surface of the particles. After drying by the hot air flow supplied from the top of the coating pan and the heat conducted from the heated tablet bed, it is beneficial to obtain a smooth and uniform film coating.

[0060] When a fluidized bed coater is used for coating, the coating liquid is atomized into spray droplets through a nozzle, and the coated particles are kept in a fluidized state under the action of hot fluidized air. When the particles pass through the coating area, the spray droplets are sprayed onto the surface of the particles, and the droplets are wetted after contacting with the particles and spread, forming a small piece of coating film on the surface of the particles. As the particles move and dry, the small piece of coating film is repeatedly wrapped, and finally the surface of the particles is completely wrapped until the desired thickness is reached. The coating liquid can be sprayed onto the tumbling aerosol particles by top spraying, bottom spraying (Wurster type) or side spraying, and the particles are continuously circulated and pass through the spraying area many times. Bottom spraying or side spraying is preferred. Bottom spraying can obtain a more uniform film coating thickness, and side spraying increases centrifugal force on the basis of fluidization and gravity, thereby achieving more effective solvent evaporation and higher spray rate. Fluidized bed coating can better provide the energy required for water evaporation, effectively prevent particle agglomeration caused by moisture absorption, and is suitable for coating of starch aqueous dispersions.

[0061] The starch type can be potato starch, wheat starch, sweet potato starch, corn starch, rice starch, kudzu starch, tapioca starch, etc.

[0062] The Fe 3 O 4 The particle size distribution of magnetic nanoparticles is 10-30nm. The Fe 3 O 4 Magnetic nanoparticles purity ≥ 95%. Fe 3 O 4 Magnetic nanoparticles can be deposited on different materials including starch, preventing the spread of water on the starch film surface, forming a highly hydrophobic or super hydrophobic surface, which is beneficial to prevent aerosol particles from absorbing moisture during storage. 3 O 4 The content of magnetic nanoparticles does not exceed 2% of the dry weight of starch. When starch is heated during gelatinization, its double helical conformation is destroyed, which is beneficial to improve the Fe 3 O 4 Distribution of magnetic nanoparticles in starch matrix. 3 O 4 The Curie temperature of magnetic nanoparticles can be controlled at 400-500°C. 3 O 4 The aerosol particles obtained by coating the magnetic nanoparticles with starch are subjected to the external alternating electromagnetic field, and the Fe 3 O 4 The magnetic nanoparticles generate heat by induction, which will cause the starch coating to break and melt, and transfer the heat to the inside of each particle to heat the particle, atomizing and releasing the aerosol formation in the particle. 3 O4 The heating temperature and heating rate of aerosol particle products can be adjusted by adjusting the amount of magnetic nanoparticles added and preparing starch film coatings of different thicknesses.

[0063] The auxiliary agents include plasticizers, binders, anti-adhesive agents and excipients.

[0064] Adding plasticizers to the starch coating solution can reduce the brittleness of the coating and increase the flexibility of the resulting coating, thereby avoiding cracking of the starch coating. The plasticizer should be similar to the structure of starch. The best plasticizer for starch coating usually contains hydroxyl-OH, usually polyols or sugars, such as glycerol, sorbitol, ethylene glycol, polyethylene glycol, xylitol, mannitol, maltitol, glucose, fructose, galactose, and sucrose. One or more of the above plasticizers can be added to the coating solution. Among them, glycerol is preferred as a plasticizer because it is non-toxic, highly safe, and can be used as a smoke generator for aerosol particles. In order to ensure the appropriate viscosity of the coating solution and make the coating sufficiently tough, the proportion of glycerol should be 0.5% to 5% of the dry weight of starch.

[0065] Adding an appropriate amount of adhesive to the starch coating solution is conducive to the good bonding between the starch coating and the surface of the aerosol particles, and improves the film-forming property of the starch. The adhesive is usually a biopolymer, which can enhance the mechanical properties of the starch coating and the barrier effect on water and gas. Cellulose derivatives such as carboxymethyl cellulose (CMC) and / or chitosan can be selected. Among them, chitosan can react with -COOH on the surface of starch and aerosol particles to form an amide bond, connecting the starch and the surface of the particles. At the same time, chitosan also has antibacterial properties, which is beneficial for aerosol particles to extend the shelf life. Hydrophilic colloids such as pectin, gum arabic, galactomannan, carrageenan, guar gum and xanthan gum can also be selected. In addition to bonding starch to particles, they can also reduce the gelatinization temperature of starch. The adhesive accounts for 0.5% to 5% of the dry weight of starch.

[0066] Adding an anti-adhesive agent to the starch coating solution can prevent the aerosol particles from agglomerating during coating and subsequent storage. Preferably, glyceryl monostearate is used as the anti-adhesive agent, accounting for 2% to 10% of the dry weight of the starch.

[0067] A small amount of excipients can also be added to the starch coating solution to minimize direct contact between the coated particles and relieve the squeezing force between the particles to prevent the coating from rupturing. Microcrystalline cellulose is preferably used as an excipient to prevent coating rupture, accounting for 0.1% to 3% of the dry weight of starch.

[0068] Preparation Example of Magnetic Starch Coating Solution:

[0069] Example 1

[0070] The cassava starch aqueous solution was prepared with starch and water in a ratio of 1:3 (weight ratio). Under stirring at 400 rpm, 3 times the volume of the starch solution and a concentration of 1 mol / L of FeCl 3 Solution and FeCl 2 The solution was stirred and a 2 mol / L NaOH solution was added dropwise. The pH was adjusted to 10 with a precision pH meter. The solution was stirred vigorously at 600 rpm for 30 minutes in a 90°C constant temperature water bath to obtain a solution containing Fe. 3 O 4 Pasty starch solution of magnetic nanoparticles. After the paste starch solution is cooled to 65°C, it is placed in an ultrasonic generator at the same temperature and frequency of 20kHz, and 1.5% of the dry weight of starch is added with 99% purity glycerol and 5% of the dry weight of starch monostearate, and the ultrasonic wave is continued for 30 minutes. The obtained coating solution is cooled to room temperature and continuously degassed for 1 hour with a vacuum pump at a pressure of 50mbar to finally obtain a magnetic starch coating solution.

[0071] Example 2

[0072] Corn starch aqueous solution was prepared with starch and water in a ratio of 1:5 (weight ratio). Under stirring at 65 °C and 300 rpm, 0.5 mol / L FeSO was added at a volume of 3 times the starch solution. 4 7H 2 O, add 1 mol / L NaOH solution dropwise while continuing to stir, adjust the pH to 11 with a precision pH meter, and add 30% H 2 O 2 The solution was stirred until the pH was neutral and the oxidation magnetization reaction was maintained for 90 minutes. Then, the solution was stirred vigorously at 600 rpm in a 90°C constant temperature water bath for 30 minutes to obtain a Fe 3 O 4 Pasty starch solution of magnetic nanoparticles. After the paste starch solution is cooled to 65°C, it is placed in an ultrasonic generator at the same temperature and a frequency of 30kHz, and 0.5% of the dry weight of starch is added with 99% purity glycerol, 5% of the dry weight of starch is added with monostearate, 1% of the dry weight of starch is added with chitosan, and 0.2% of the dry weight of starch is added with microcrystalline cellulose, and the ultrasonic treatment is continued for 60 minutes. The obtained coating solution is cooled to room temperature, and a vacuum pump with a pressure of 50mbar is used for continuous degassing for 1 hour to finally obtain a magnetic starch coating solution.

[0073] Embodiment 3:

[0074] The cassava starch aqueous solution was prepared in a ratio of 1:3 (weight ratio) between starch and water, and stirred at 400 rpm for 30 minutes in a 90°C constant temperature water bath to prepare a starch paste. After the starch paste was cooled to 65°C, Fe with a particle size of 20 nm and a starch dry weight of 1.5% was added at a stirring rate of 600 rpm.3 O 4 Magnetic nanoparticles, continue stirring for 30 minutes. Under the same conditions, add glycerol with a purity of 99% accounting for 1% of the dry weight of starch, sorbitol accounting for 0.5% of the dry weight of starch, and CMC accounting for 3% of the dry weight of starch, and continue stirring for 30 minutes. Then place it in an ultrasonic generator at 65°C and a frequency of 30kHz, and continue ultrasonication for 30 minutes. The prepared coating solution is cooled to room temperature and degassed for 1 hour with a vacuum pump at a pressure of 50mbar to finally obtain a magnetic starch coating solution.

[0075] Embodiment 4:

[0076] A potato starch aqueous solution was prepared at a ratio of 1:5 (weight ratio) of starch to water, and stirred at 300 rpm in a 90°C constant temperature water bath for 40 minutes to prepare a starch paste. After the starch paste was cooled to 60°C, Fe 200, which had a particle size of 15 nm and accounted for 2% of the dry weight of starch, was added at a stirring rate of 600 rpm. 3 O 4 Magnetic nanoparticles were stirred for 40 minutes. Under the same conditions, glycerol with a purity of 99% accounting for 0.5% of the dry weight of starch, guar gum accounting for 1.5% of the dry weight of starch, chitosan accounting for 1% of the dry weight of starch, and glyceryl monostearate accounting for 3% of the dry weight of starch were added, and stirring was continued for 30 minutes. Then cooled to room temperature, homogenized for 10 minutes with a rotor-stator homogenizer at 20,000 rpm. The homogenized coating solution was continuously degassed for 1 hour with a vacuum pump at a pressure of 50 mbar to finally obtain a magnetic starch coating solution.

[0077] Example of preparing aerosol particles coated with magnetic starch film:

[0078] Example 5

[0079] The following experiments were carried out using the magnetic starch coating solutions obtained in Examples 1 and 4 respectively:

[0080] Place the newly prepared uncoated aerosol particles in a fluidized coating machine, set the material (coating) temperature to 30-40°C, the fan frequency to 20-30Hz, the atomization pressure to 0.05-0.1MPa, and the peristaltic pump speed to 0.5-1.0mL / min to pump the magnetic starch coating liquid obtained in Examples 1 and 4 respectively, and the coating time is 2h to ensure that all the particles are boiling and fluidized. After the coating is completed, continue to dry at 35°C for 12h. After cooling to room temperature, two types of magnetic starch film-coated aerosol particles with a coating thickness of 40 to 50 microns are obtained respectively.

[0081] Example 6

[0082] The following experiments were carried out using the magnetic starch coating solutions obtained in Examples 2 and 3 respectively:

[0083] Place a suitable amount of newly prepared uncoated aerosol particles in a coating pot, set the material (coating) temperature to 30-50°C, set the air inlet temperature to 75°C, preheat for 5 minutes, start the coating pot, adjust the coating pot speed to 3-5rpm / min, move the spray gun into the coating pot, adjust the magnetic starch coating liquid spray volume obtained in Examples 2 and 3 to 2-3g / min, and start coating. The coating time is 3h, and after the coating is completed, continue to dry at 40°C for 24h. After cooling to room temperature, two types of magnetic starch film-coated aerosol particles with a coating thickness of 20 to 30 microns are obtained.

Claims

1. A magnetic starch coating solution is used for coating smoke-generating particles and then performing electromagnetic heating, characterized in that: The magnetic starch coating solution comprises: magnetic nanoparticles and starch solution, wherein the content of the magnetic nanoparticles does not exceed 2% of the dry weight of the starch; The magnetic nanoparticles are ferroferric oxide nanoparticles, and the particle size distribution of the ferroferric oxide nanoparticles is 10-30 nm; The magnetic starch coating solution further comprises: an auxiliary agent; The auxiliary agent is selected from: one or more of a plasticizer, a binder, an anti-adhesive agent and an excipient; The preparation method of the magnetic starch coating solution adopts one of the following methods: Method 1: Adding an iron salt solution to a starch aqueous solution, mixing well, then adding an alkali solution, adjusting the pH to 10-11, heating and mixing well, and further stirring at 80-100 degrees Celsius to promote starch gelatinization to obtain a starch gelatinized solution; wherein the iron salt solution is a divalent iron salt solution, or a mixed solution of a divalent iron salt solution and a trivalent iron salt solution, when the iron salt solution is a divalent iron salt solution, a hydrogen peroxide solution needs to be added for partial oxidation, and when the iron salt solution is a mixed solution of a divalent iron salt solution and a trivalent iron salt solution, no hydrogen peroxide solution needs to be added for oxidation; Ultrasonic treatment is performed on the starch gelatinized liquid, and a first auxiliary agent is added at the same time, and further constant temperature ultrasonic treatment or homogenization is performed for a certain period of time, followed by degassing to obtain the magnetic starch coating solution; Method 2: Mix starch and water and stir at 80-100 degrees Celsius to prepare a starch aqueous solution; Adding magnetic nanoparticles; After stirring, ultrasonic treatment is performed, and a second auxiliary agent is added at the same time. After further constant temperature ultrasonic treatment or homogenization for a certain period of time, degassing is performed to obtain a magnetic starch coating solution; Wherein, the first auxiliary agent and the second auxiliary agent are the same or different; The first auxiliary agent and the second auxiliary agent are independently selected from: one or more of a plasticizer, a binder, an anti-adhesive agent and an excipient.

2. A smoke-generating particle, characterized in that: The smoke-generating particles comprise: an outer magnetic starch wrapping layer and inner smoke-generating particles; The magnetic starch coating layer comprises starch and a plurality of dispersed magnetic nanoparticles embedded in the starch; The method for preparing the smoke-generating particles comprises the following steps: (1) Preparation of magnetic starch coating solution: It can be prepared by the following two methods: Method 1: Adding an iron salt solution to a starch aqueous solution, mixing well, then adding an alkali solution, adjusting the pH to 10-11, heating and mixing well, and further stirring at 80-100 degrees Celsius to promote starch gelatinization to obtain a starch gelatinized solution; wherein the iron salt solution is a divalent iron salt solution, or a mixed solution of a divalent iron salt solution and a trivalent iron salt solution, when the iron salt solution is a divalent iron salt solution, a hydrogen peroxide solution needs to be added for partial oxidation, and when the iron salt solution is a mixed solution of a divalent iron salt solution and a trivalent iron salt solution, no hydrogen peroxide solution needs to be added for oxidation; Ultrasonic treatment is performed on the starch gelatinized liquid, and a first auxiliary agent is added at the same time, and further constant temperature ultrasonic treatment or homogenization is performed for a certain period of time, followed by degassing to obtain the magnetic starch coating solution; Method 2: Mix starch and water and stir at 80-100 degrees Celsius to prepare a starch aqueous solution; Adding magnetic nanoparticles; After stirring, ultrasonic treatment is performed, and a second auxiliary agent is added at the same time. After further constant temperature ultrasonic treatment or homogenization for a certain period of time, degassing is performed to obtain a magnetic starch coating solution; Wherein, the first auxiliary agent and the second auxiliary agent are the same or different; The first auxiliary agent and the second auxiliary agent are independently selected from: one or more of a plasticizer, a binder, an anti-adhesive agent and an excipient; (2) Preparing smoke-generating particles: placing the smoke-generating particles in a coating device, spraying the magnetic starch coating solution prepared above from a spray gun disposed in the coating device to form a spray, thereby forming a magnetic starch coating on the surface of the smoke-generating particles; The smoky particles coated with magnetic starch are heat treated to obtain the smoky particles.