An ultra-small diameter ultra-hard micro-blade milling and grinding composite ball head tool and a preparation method thereof

By designing ultra-small diameter ultra-hard micro-blade milling and grinding composite ball head tools, using multi-micro-blade structures and abrasive layers, combined with laser cutting and high-frequency welding and other technologies, the problem of difficult processing of micro-structure parts is solved, and high efficiency and precision is achieved Processing and high-quality cutting.

CN115383668BActive Publication Date: 2024-11-12BEIJING INST OF TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210546241.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-05-18
Publication Date
2024-11-12
Estimated Expiration
2042-05-18

AI Technical Summary

Technical Problem

It is difficult to achieve efficient precision machining of existing microstructured parts, especially the cutting performance and processing quality of difficult-to-machines materials are affected, and the existing tool design and preparation methods have defects, resulting in low wear and machining efficiency.

Method used

Designed an ultra-small diameter ultra-hard micro-edge milling and grinding composite ball head tool, including multi-micro-edge structure and abrasive grain layer, and is prepared using laser cutting, high-frequency welding, laser diameter reduction and precision grinding technology, suitable for high-end precision Processing of parts.

Benefits of technology

It improves the mechanical properties, machining stability and cutting performance of the tool, reduces the difficulty of preparation, achieves efficient precision machining, extends the tool life and improves the processing quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115383668B_ABST
    Figure CN115383668B_ABST
Patent Text Reader

Abstract

The present invention relates to an ultra-small diameter ultra-hard micro-blade milling composite ball head tool and a preparation method thereof, belonging to the field of micro-tool processing technology. It includes a tool head involved in the cutting part and a transitional tool neck, a welding area, a transitional tool handle, a tool neck and a tool handle that play a connecting and supporting role, wherein the tool head includes a plurality of micro-blades, each of which includes a tool back face, a cutting edge, a front face and a chip groove, and a micro-abrasive layer is formed on the back face by precision grinding with a grinding wheel or an electroplating process. The material of the tool head is polydiamond or polycrystalline cubic boron nitride, and the tool head diameter d is 50-500μm. The micro-groove structure is adopted to improve the rigidity and strength of the tool, and it has the characteristics of extremely small size, which can meet the processing requirements of high-end micro-precision parts. At the same time, the micro-blade multi-blade structure adopted can effectively improve the anti-collapse property of the cutting edge and ensure the cutting stability of the tool.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to an ultra-small diameter ultra-hard micro-blade milling and grinding composite ball head tool and a preparation method thereof, belonging to the technical field of micro-tool processing. Background Art

[0002] With the development of high-end manufacturing industries such as aerospace, the requirements for efficient and precise processing of tiny structural parts are getting higher and higher. However, the difficult-to-process materials such as high-temperature alloys, cemented carbides, SiC, etc. used in tiny structural parts are very easy to cause tool wear, affecting the processing efficiency and processing quality of tiny structural parts. Superhard tool materials, such as PCD, PCBN, etc., have become the main materials for high-end precision tools due to their high hardness, high wear resistance and better cutting performance. However, with the reduction of tool size and changes in tool materials, there are many problems in the design and preparation of tiny superhard tools. Unreasonable tool structure will not only reduce the cutting performance of the tool, but also make the tool difficult to prepare. Unreasonable preparation methods will cause defects such as cracks and pits on the tool surface, affecting the service life of the tool. At the same time, the existing grinding tool needs to be replaced for surface polishing after milling of tiny components. Replacing the tool is not only not conducive to improving the processing accuracy of tiny components, but the tool change operation also reduces the processing efficiency.

[0003] Therefore, in response to the demand for efficient and precise machining of tiny structural parts, the present invention proposes an ultra-small diameter super-hard micro-blade milling and grinding composite ball head tool and a preparation method thereof. Summary of the invention

[0004] The invention provides an ultra-small diameter ultra-hard micro-blade milling and grinding composite ball head tool and a preparation method thereof, which is used for precise and efficient machining of difficult-to-machine materials, and is particularly suitable for finishing machining of high-end precision parts.

[0005] The technical solution for implementing the present invention is as follows:

[0006] An ultra-small diameter ultra-hard micro-blade milling composite ball-end tool, characterized in that it comprises a tool head for a cutting part and a transitional tool neck, a welding area, a transitional tool handle, a tool neck and a tool handle that play a connecting and supporting role, wherein the tool head comprises a plurality of micro-blades, each of which comprises a tool back face, a cutting edge, a front face and a chip groove, a micro-abrasive layer is formed on the back face by a grinding wheel precision grinding or electroplating process, the material of the tool head is polydiamond (PCD) or polycrystalline cubic boron nitride (PCBN), and the tool head diameter d is 50-500 μm;

[0007] The micro-blade is designed as a planar cutting edge curve, and its mathematical expression is:

[0008]

[0009] Among them, r is the tool radius, θ is the tool height angle, and γ0 is the angle between the plane where the cutting edge curve is located and the tool plane.

[0010] The flank surface adopts a circular arc flank surface structure, which is obtained by rotating the generating line by an angle δ, and its mathematical expression is:

[0011]

[0012] Where l is the length of the flank line, δ is the rotation angle of the flank formed by the line, α0 is the normal flank angle of the micro-edge milling tool, and l∈[0,0.08],

[0013] Furthermore, the number of micro blades is 3-10.

[0014] Furthermore, the geometric parameters of the tool are: overall tool length L0 = 60 mm, micro-edge groove length L = 0.2 mm, tool head length L1 = 1 mm, transition tool neck taper angle α m =20°, transition handle length L2 = 1.5mm, tool neck taper angle α n =15°, handle diameter D=3-6mm.

[0015] Furthermore, the front angle is set to 0-6° for plastic materials such as titanium alloy and stainless steel, and is set to -6-0° for hard and brittle materials such as SiC and sapphire.

[0016] A method for preparing an ultra-small diameter ultra-hard micro-edge milling and grinding composite ball head tool is as follows:

[0017] Step S1: laser / electric spark cutting of superhard composite sheets, using high-power laser or electric spark to cut the superhard composite sheets into composite sheet round blocks with a diameter of 0.5-3 mm for subsequent preparation of superhard tool bars, the material of the superhard composite sheets is polydiamond (PCD) or polycrystalline cubic boron nitride (PCBN);

[0018] Step S2: high-frequency brazing of the superhard composite sheet and the substrate, using high-frequency induction brazing technology to perform high-frequency welding on the superhard composite sheet cut in step S1 and the cemented carbide substrate to obtain a superhard tool bar blank;

[0019] Step S3: Laser reduction of the superhard tool bar stock blank, using laser to reduce the diameter of the superhard tool bar stock blank in step S2 to form a five-section overall structure of the superhard tool;

[0020] Step S4: Precision grinding of superhard tools, using precision grinding technology to prepare ultra-small diameter tool blades, and completing the precision preparation of ultra-small diameter superhard micro-blade milling and grinding composite ball-end tools through multi-axis linkage precision grinding and multi-axis linkage precision compensation technology. The precision grinding of the superhard tools mainly includes spherical grinding, micro-blade grinding and cylindrical grinding, wherein spherical grinding forms the tool back face, micro-blade grinding forms the tool front face and chip groove, and cylindrical grinding ensures the geometric dimensional accuracy of the tool involved in the cutting part;

[0021] Step S5: Preparation of an abrasive layer on the back face of a superhard tool. In order to realize a milling and grinding composite processing, an abrasive layer is prepared on the back face of the tool based on step S4. The abrasive layer on the back face is prepared by the same precision grinding as micro-blade grinding, or by electroplating.

[0022] Furthermore, the spherical grinding of the superhard tool is completed by parallel grinding wheel end faces. The grinder makes the center of the tool ball located on the W-axis rotation center through five-axis linkage of X, Y, Z, A and W axes, and then realizes spherical grinding through A-axis rotation and W-axis indexing rotation.

[0023] Furthermore, the micro-edge grinding of the superhard tool is completed by a bevel grinding wheel. First, the tool center point is positioned by the X, Y, Z and W axes, and then the micro-edge grinding of the milling tool is completed by the four-axis linkage of the X, Z, W and A axes.

[0024] Furthermore, in the cylindrical grinding of the superhard tool, the grinding process is to move to the processing position through X and Z. After the grinding starts, the parallel grinding wheel end face is fed through the X axis, and the Y axis controls the grinding depth to grind the tool bar to a specified size.

[0025] Furthermore, the precision grinding method for preparing the abrasive layer on the back face of the superhard tool utilizes the characteristics of materials such as PCD and PCBN that are sintered with superhard abrasives and a binder, and grinds the back face of the tool through a multi-axis linkage CNC grinding method to expose the abrasive grains on the back face to form an abrasive layer. The principle of back face grinding is to position the tool and the grinding wheel to the grinding position through the linkage of the X, Y, Z and W axes, and then complete the grinding of the back face through the linkage of the X, Z, A and W axes.

[0026] Furthermore, the electroplating process is used to prepare the abrasive layer on the back face of the superhard tool. The tool is used as the cathode, and a layer of abrasive is plated on the back face by the method of nickel-abrasive co-deposition. Compared with precision grinding, the back face abrasive prepared by the electroplating process is not limited by the tool material, and abrasives of different particle sizes and concentrations can be plated as needed.

[0027] Beneficial effects of the present invention:

[0028] (1) The five-section structure of the ultra-small diameter superhard ball-end tool proposed in the present invention can increase the welding area of ​​the superhard tool during the welding process between the superhard composite sheet and the substrate, thereby improving the overall mechanical properties and processing stability of the micro ball-end tool;

[0029] (2) The ultra-small diameter super-hard ball-end tool proposed in the present invention abandons the spiral groove structure which has no significant effect and adopts the micro-groove structure according to the size characteristics and processing requirements of the tool. It can improve the rigidity and strength of the tool without affecting the cutting performance of the tool and reduce the difficulty of tool preparation;

[0030] (3) The ultra-small diameter super-hard ball-end tool proposed in the present invention has the characteristics of extremely small size, which can meet the processing requirements of high-end micro-precision parts. At the same time, the micro-edge multi-edge structure adopted can effectively improve the anti-collapse property of the cutting edge and ensure the cutting stability of the tool, which is very suitable for the precision processing of high-hardness materials;

[0031] (4) The ultra-small diameter super-hard ball-end tool proposed in the present invention has an abrasive layer prepared on the back face, which can form a micro-grinding effect during the processing, forming a milling and grinding composite processing method combining micro-edge cutting and back face grinding, which can improve the tool processing efficiency and processing quality;

[0032] (5) The present invention proposes a method and process for preparing an ultra-small diameter superhard micro-blade milling composite ball head tool, which can realize the precise preparation of the tool of the present invention and other similar superhard tools, and can improve the preparation efficiency and preparation quality of the tool. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] Figure 1 Schematic diagram of the geometric structure of an ultra-small diameter super-hard micro-edge milling and grinding composite ball head tool of the present invention

[0034] Figure 2 The mathematical model of the ball head of an ultra-small diameter ultra-hard micro-blade milling composite ball head tool of the present invention is

[0035] Figure 3 Schematic diagram of the mathematical model of the tool head of an ultra-small diameter ultra-hard micro-blade milling composite ball head tool of the present invention

[0036] Figure 4 The overall manufacturing process of an ultra-small diameter ultra-hard micro-blade milling and grinding composite ball head tool of the present invention;

[0037] Figure 5 A process for precision grinding of a cutter head of an ultra-small diameter ultra-hard micro-blade milling and grinding composite ball-end tool according to the present invention;

[0038] Figure 6 It is a schematic diagram of the multi-axis linkage grinding principle of a super-small diameter super-hard micro-blade milling composite ball-end tool head of the present invention;

[0039] Figure 7 A schematic diagram of the preparation principle of abrasive grains on the back face of an ultra-small diameter super-hard micro-edge milling composite ball-end tool of the present invention;

[0040] Figure 8 A physical picture of a super-small diameter super-hard micro-edge milling and grinding composite ball-end tool head of the present invention;

[0041] 1-blade head, 2-transition blade neck, 3-welding area, 4-transition blade handle, 5-blade neck, 6-blade handle;

[0042] 101-flank face, 102-cutting edge, 103-front face, 104-chip groove; Specific implementation methods

[0043] The present invention will be further described below in conjunction with the accompanying drawings.

[0044] like Figure 1 As shown, an ultra-small diameter super-hard micro-blade milling composite ball head tool is characterized in that it mainly includes a tool head-1 participating in the cutting part and a transition tool neck-2, a welding area-3, a transition tool handle-4, a tool neck-5, and a tool handle-6 that play a connecting and supporting role, wherein the tool head part mainly includes a tool back face-101, a cutting edge-102, a front face-103, and a chip groove-104.

[0045] Furthermore, the ultra-small diameter superhard milling composite tool material is a superhard material such as polycrystalline diamond (PCD) and polycrystalline cubic boron nitride (PCBN). In this specific implementation case, PCBN material of Element Six with a grade of DBW85 is used, and the matrix material is UF09 material of IMC.

[0046] Furthermore, the ultra-small diameter superhard milling and grinding composite ball-end tool is characterized in that the diameter d of the tool head is generally 50-500 μm, the diameter D of the tool handle is generally 3-6 mm, and the number of micro-edges is generally 3-10;

[0047] Furthermore, the geometrical parameters of the ultra-small diameter ultra-hard micro-edge milling composite ball-end tool designed and manufactured in this specific implementation case are: overall tool length L0 = 60 mm, micro-edge groove length L = 0.2 mm, tool head length L1 = 1 mm, transition tool neck taper angle α m =20°, transition handle length L2 = 1.5mm, tool neck taper angle α n =15°, handle diameter D = 3mm, micro blade diameter d = 0.2mm, number of micro blades is 5;

[0048] Furthermore, the rake angle of the ultra-small diameter super-hard milling composite ball-end tool can be adaptively designed according to the processing material. This specific implementation case selects a 6° positive rake angle for titanium alloy and stainless steel materials;

[0049] Figure 2 The figure is a schematic diagram of the mathematical model of the ball head of an ultra-small diameter PCBN micro-blade milling composite ball head tool. The origin O of the coordinate system is located at the center of the micro-blade milling composite tool, the OZ axis coincides with the tool axis, and the OX is tangent to the tool rake face. The cutting edge of the micro-blade milling composite tool can be expressed as:

[0050]

[0051] Among them, r is the tool radius, θ is the tool height angle, and γ0 is the angle between the plane where the cutting edge curve is located and the tool plane.

[0052] The flank surface adopts an arc flank surface structure, so any point E on the flank surface can be obtained by rotating any point C on the generating line BC around the line segment OA by δ, and the coordinate of point C is C=[0,-lcosα0,r-lsinα0], where l is the length of the generating line of the flank surface, that is, the length of the line segment BC, δ is the rotation angle of the generating line to form the flank surface, α0 is the normal flank angle of the micro-edge milling tool, and l∈[0,0.08],

[0053] Therefore, the mathematical expression of the back cutting edge can be expressed as:

[0054]

[0055] Figure 3 The invention discloses an overall manufacturing process of an ultra-small diameter PCBN micro-blade milling and grinding composite ball-end tool, including laser / electric spark cutting of PCBN composite sheets, high-frequency brazing of PCBN composite sheets and cemented carbide substrates, laser diameter reduction of PCBN tool bar blanks and precision grinding of PCBN tools.

[0056] Furthermore, the preparation method of the ultra-small diameter PCBN milling and grinding composite ball head tool is as follows:

[0057] Step S1: PCBN composite sheet laser / electric spark cutting. Use high-power laser or electric spark to cut the superhard composite sheet into PCBN composite sheet round blocks with a diameter of 1 mm for subsequent preparation of PCBN tool bars;

[0058] Step S2: high-frequency brazing of the PCBN composite piece and the cemented carbide substrate. Taking advantage of the high-frequency induction brazing technology, such as fast heating speed and simple equipment, the PCBN composite piece cut in step S1 is high-frequency welded with the cemented carbide substrate to obtain a superhard tool bar blank, wherein the solder is silver-copper solder, argon is used as the protective gas, the welding pressure is 0.5-2MPa, the welding temperature is 700℃, and the temperature is kept for 10s;

[0059] Step S3: Laser reduction of superhard bar stock. Taking advantage of the high efficiency and non-contact processing characteristics of laser, the superhard bar stock in step S2 is laser reduced to form a five-section overall structure of superhard tool. The laser uses a picosecond laser with a laser pulse width of 15ps, a rate of 800kHz, and an average power of 20W. The diameter of the formed PCBN bar stock cutter head is 0.21mm, leaving a processing allowance for subsequent precision grinding.

[0060] Step S4: Precision grinding of ultra-small diameter PCBN tools. Precision grinding technology can eliminate the heat-affected layer generated by laser processing, and has the characteristics of high processing accuracy and good quality, which can improve the surface quality of tool processing. Therefore, the ultra-small diameter tool is sharpened and prepared using the Makino Precision Machinery six-axis CNC tool grinder to complete the preparation of the ultra-small diameter PCBN micro-blade milling and grinding composite ball head tool.

[0061] Step S5: Preparation of abrasive layer on the back face of superhard tool. In order to realize the milling and grinding composite processing, an abrasive layer is prepared on the back face of the tool based on step S4, which can form a milling and grinding composite processing together with the cutting edge micro-milling. The preparation of the abrasive layer on the back face is achieved by two methods: precision grinding or electroplating process.

[0062] Furthermore, the superhard tool precision grinding, such as Figure 4 As shown, it mainly includes spherical grinding, micro-edge grinding and cylindrical grinding. Spherical grinding forms the back face of the tool, micro-edge grinding forms the front face and chip groove of the tool, and cylindrical grinding ensures the geometric dimensional accuracy of the tool involved in the cutting part. Makino Seiki six-axis CNC tool grinder was selected, and a PCBN micro-edge milling and grinding composite ball head tool with a diameter of 0.2 mm was obtained according to the grinding process of rough machining - grinding speed 20 m / s, feed speed 60 mm / min, grinding depth 10 μm and fine machining - grinding speed 20 m / s, feed speed 10 mm / min, grinding depth 3 μm.

[0063] Furthermore, the superhard tool precision grinding is completed using a Makino Seiki six-axis CNC grinder, such as Figure 5 As shown, the machine tool can realize five-axis (X, Y, Z, A, W axis) linkage and has high flexibility. The existence of the U axis ensures the positioning accuracy of tool grinding.

[0064] Figure 6 This is the principle diagram of multi-axis CNC grinding of ultra-small diameter ultra-hard micro-blade tools, in which spherical grinding is completed by parallel grinding wheel end faces. The grinder completes the preparation before grinding through the five-axis linkage of X, Y, Z, A and W axes, and then realizes spherical grinding through the rotation of A and W axes; micro-blade grinding is completed by beveled grinding wheels. First, the center point of the tool is positioned through the X, Y, Z and W axes, and then the micro-blade grinding of the milling tool is completed through the four-axis linkage of X, Z, W and A axes; cylindrical grinding is moved to the processing position through X and Z. After the grinding starts, the parallel grinding wheel end faces are fed through the X axis, and the Y axis controls the grinding depth to grind the tool bar to the specified size.

[0065] Furthermore, the abrasive layer on the back face of the superhard tool is prepared by a precision grinding or precision electroplating method, such as Figure 7 As shown. The principle of precision grinding is to use the characteristics of materials such as PCD and PCBN, that is, PCD, PCBN and other materials are sintered by super-hard abrasives and binders. The back face of the tool is ground by a multi-axis linkage CNC grinding method, so that the abrasive grains on the back face are exposed to form an abrasive layer. The principle of back face grinding is to position the tool and the grinding wheel to the grinding position through the linkage of the X, Y, Z and W axes, and then complete the grinding of the first back face through the linkage of the X, Z, A and W axes; the principle of the precision electroplating method is to use the electroplating process, with the tool as the cathode, and a layer of abrasive grains is plated on the back face by the nickel-abrasive co-deposition method. Compared with precision grinding, the back face abrasive grains prepared by the electroplating process are not limited by the tool material, and can be plated with abrasive grains of different particle sizes and concentrations as needed, which is more suitable for different processing conditions.

[0066] Figure 8 This is a photo of a PCBN micro-blade milling composite ball head tool with a diameter of 0.2 mm and a front angle of 6° that was successfully prepared according to the designed structure and preparation process in the above steps, in which the abrasive layer on the back face of the tool was precisely ground.

[0067] Finally, it should be noted that the above specific embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. An ultra-small diameter ultra-hard micro-blade milling composite ball head tool, characterized in that: The tool head includes a cutting part, a transitional tool neck, a welding area, a transitional tool handle, a tool neck and a tool handle that play a connecting and supporting role, wherein the tool head includes a plurality of micro blades, each of which includes a tool back face, a cutting edge, a front face and a chip groove, and a tiny abrasive layer is formed on the back face by precision grinding with a grinding wheel or electroplating process, the material of the tool head is polydiamond (PCD) or polycrystalline cubic boron nitride (PCBN), and the tool head diameter d is 50-500μm; The micro-blade is designed as a planar cutting edge curve, and its mathematical expression is: Where r is the tool radius, θ is the tool height angle, and γ0 is the angle between the plane where the cutting edge curve is located and the tool plane; The flank surface adopts a circular arc flank surface structure, which is obtained by rotating the generating line by an angle δ, and its mathematical expression is: Where l is the length of the flank line, δ is the rotation angle of the flank formed by the line, α0 is the normal flank angle of the micro-edge milling tool, and l∈[0,0.08], The number of the micro blades is 3-10; The geometric parameters of the tool are: overall tool length L0 = 60 mm, micro-edge groove length L = 0.2 mm, tool head length L1 = 1 mm, transition tool neck taper angle α m =20°, transition handle length L2 = 1.5mm, tool neck taper angle α n =15°, handle diameter D = 3-6mm; For titanium alloy and stainless steel plastic materials, the front angle is set to 0~6°, and for SiC and sapphire hard and brittle materials, the front angle is set to -6~0°.

2. The method for preparing an ultra-small diameter ultra-hard micro-blade milling composite ball-end tool according to claim 1, characterized in that: The method is specifically as follows: Step S1: laser / electric spark cutting of superhard composite sheets, using high-power laser or electric spark to cut the superhard composite sheets into composite sheet round blocks with a diameter of 0.5-3 mm for subsequent preparation of superhard tool bars, the material of the superhard composite sheets is polydiamond (PCD) or polycrystalline cubic boron nitride (PCBN); Step S2: high-frequency brazing of the superhard composite sheet and the substrate, using high-frequency induction brazing technology to perform high-frequency welding on the superhard composite sheet cut in step S1 and the cemented carbide substrate to obtain a superhard tool bar blank; Step S3: Laser reduction of the superhard tool bar stock blank, using laser to reduce the diameter of the superhard tool bar stock blank in step S2 to form a five-section overall structure of the superhard tool; Step S4: Precision grinding of superhard tools, using precision grinding technology to prepare ultra-small diameter tool blades, and completing the precision preparation of ultra-small diameter superhard micro-blade milling and grinding composite ball-end tools through multi-axis linkage precision grinding and multi-axis linkage precision compensation technology. The precision grinding of the superhard tools mainly includes spherical grinding, micro-blade grinding and cylindrical grinding, wherein spherical grinding forms the tool back face, micro-blade grinding forms the tool front face and chip groove, and cylindrical grinding ensures the geometric dimensional accuracy of the tool involved in the cutting part; Step S5: Preparation of an abrasive layer on the back face of a superhard tool. In order to realize a milling and grinding composite processing, an abrasive layer is prepared on the back face of the tool based on step S4. The abrasive layer on the back face is prepared by the same precision grinding as micro-blade grinding, or by electroplating.

3. The method for preparing an ultra-small diameter ultra-hard micro-blade milling composite ball-end tool according to claim 2, characterized in that: The spherical grinding of the superhard tool is completed by parallel grinding wheel end faces. The grinding machine makes the tool ball center on the W-axis rotation center through five-axis linkage of X, Y, Z, A and W axes, and then realizes spherical grinding through A-axis rotation and W-axis indexing rotation.

4. The method for preparing an ultra-small diameter ultra-hard micro-edge milling and grinding composite ball-end tool according to claim 3, characterized in that: The micro-edge grinding of the superhard tool is completed by a bevel grinding wheel. First, the tool center point is positioned by the X, Y, Z and W axes, and then the micro-edge grinding of the milling tool is completed by the four-axis linkage of the X, Z, W and A axes.

5. The method for preparing an ultra-small diameter ultra-hard micro-edge milling and grinding composite ball-end tool according to claim 4, characterized in that: The cylindrical grinding of the superhard tool is performed by moving the tool to the processing position through X and Z. After the grinding starts, the parallel grinding wheel end face is fed through the X axis, and the Y axis controls the grinding depth to grind the tool bar to a specified size.

6. The method for preparing an ultra-small diameter ultra-hard micro-edge milling and grinding composite ball-end tool according to claim 5, characterized in that: The precision grinding method for preparing the abrasive layer on the back face of the superhard tool utilizes the characteristics of PCD and PCBN materials that are sintered with superhard abrasives and a binder. The back face of the tool is ground by a multi-axis linkage CNC grinding method to expose the abrasive grains on the back face to form an abrasive layer. The back face grinding principle is to position the tool and the grinding wheel to the grinding position through the linkage of the X, Y, Z and W axes, and then complete the grinding of the back face through the linkage of the X, Z, A and W axes.

7. The method for preparing an ultra-small diameter ultra-hard micro-edge milling and grinding composite ball-end tool according to claim 6, characterized in that: The electroplating process is used to prepare the abrasive layer on the back face of the superhard tool. The tool is used as the cathode, and a layer of abrasive is plated on the back face by the nickel-abrasive co-deposition method. Compared with precision grinding, the back face abrasive prepared by the electroplating process is not limited by the tool material, and abrasives of different particle sizes and concentrations can be plated as needed.