A signal transmission coaxial composite cable for gate lifting
By using a multi-layer shielding structure and a wear-resistant sheath in the gate signal transmission cable, the problems of cable anti-interference, safety and flexibility are solved, and efficient signal transmission and wear-resistant performance are improved.
Patent Information
- Application Number
- CN202211228072.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-10-09
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2042-10-09
AI Technical Summary
The signal transmission cable of the gate needs to be anti-interference, highly safe, wear-resistant and easy to bend when used, but the existing technology is difficult to meet these requirements.
Use a coaxial composite cable including six voice lines and three signal lines, using foamed polyethylene insulation layer, tinned copper wire individual shielding layer, fine aramid yarn wrapping layer, aluminum-plastic composite tape shielding layer, and tinned copper wire Braided total shielding layer and wear-resistant and flexible polyurethane sheath, combined with tinned copper wire drain wire, enhance shielding and flexibility.
Significantly improves the anti-interference ability, safety of use, wear resistance and bending performance of signal transmission, meeting the needs of flexible movement and dragging of the gate.
Smart Images

Figure CN115394474B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field, and in particular to a signal transmission coaxial composite cable for gate lifting. Background Art
[0002] The gate is a channel blocking device. The requirements for cables in the process of controlling its automatic lifting are different from those of ordinary cables. The electromagnetic waves that control the gate action radiate electromagnetic waves to the outside world while being transmitted longitudinally in the cable. The external electromagnetic field can also interfere with the inside of the cable. At the same time, the signal transmission cable used in the gate needs to be highly flexible when used, and can be flexibly moved or dragged with the lifting and lowering of the gate. Therefore, it is particularly important to improve the anti-interference performance, safety of use, and wear resistance and flexibility of the cable. Summary of the invention
[0003] Based on the technical problems existing in the background technology, the present invention proposes a signal transmission coaxial composite cable for gate lifting.
[0004] The technical solution adopted by the present invention is:
[0005] A signal transmission coaxial composite cable for gate lifting and lowering, comprising a cable core, the cable core comprising six voice lines and three signal lines, the voice lines comprising a voice line conductor and a polyolefin insulation layer coated on the outside of the voice line conductor; the signal line comprising a signal line conductor, the outside of the signal line conductor is coated with a foamed polyethylene insulation layer, a tinned copper wire individual shielding layer, and a fine aramid yarn winding layer in sequence from the inside to the outside; a plurality of fine aramid yarn ropes are filled between the six voice lines and the three signal lines, the six voice lines and the three signal lines are twisted to form a cable core, the outside of the cable core is overlapped and wrapped with two layers of aluminum-plastic composite tape shielding layers, the conductive surface of the aluminum-plastic composite tape shielding layers faces inward and a ground wire is dragged longitudinally, the ground wire is a tinned copper wire drainage wire; the aluminum-plastic composite tape shielding layer is coated with a tinned copper wire braided total shielding layer, the outside of the tinned copper wire braided total shielding layer is extruded with a polyurethane sheath, and the outer surface of the polyurethane sheath is serrated.
[0006] Furthermore, the voice line conductor and the signal line conductor are both made of tinned alloy copper foil wire twisted conductors. The tinned copper wire separate shielding layer is made of Φ0.008mm tinned copper wire wound together.
[0007] Furthermore, the foamed polyethylene insulation layer comprises the following raw materials in parts by weight:
[0008] AC foaming agent 7-10, high density polyethylene 130-150, lignin 10-15, 4-dimethylaminopyridine 10-20, 2-bromo-2-methylpropionyl bromide 30-40, triglycidyl isocyanurate 2-4, trifluoroethyl methacrylate 40-50, tert-butyl p-diphenol 0.5-1, nano silicon dioxide 6-10, cuprous chloride 1-2, triethylamine 2-3.
[0009] The method for preparing the foamed polyethylene insulation layer comprises the following steps:
[0010] (1) taking triglycidyl isocyanurate, adding it to 80-90 times its weight of dimethylformamide, stirring evenly, adding trifluoroethyl methacrylate, stirring evenly, to obtain a monomer dispersion;
[0011] (2) Take lignin, add it to 30-40 times of its weight of N,N-dimethylformamide, send it into a stirring kettle, add 4-dimethylaminopyridine, stir evenly, place it in an ice water bath, add 2-bromo-2-methylpropionyl bromide, let it stand for 3-5 hours, discharge it, stir it at room temperature for 15-20 hours, vacuum filter it, wash the filter cake with water, and vacuum dry it at 50-55° C. to obtain an initiator;
[0012] (3) Mix triethylamine and nano-silicon dioxide, add to 30-40 times the weight of the mixture of N,N-dimethylformamide, and perform ultrasonication for 1-2 hours to obtain a silicon dispersion;
[0013] (4) Take an initiator, add it to the above-mentioned monomer dispersion, send it into a reactor, introduce nitrogen, adjust the temperature of the reactor to 70-80° C., add cuprous bromide, stir and react for 3-4 hours, add the above-mentioned silicon dispersion, increase the temperature to 120-130° C., stir and react for 1.5-2 hours, discharge the material, and remove dimethylformamide by rotary evaporation to obtain a modified filler;
[0014] (5) taking the modified filler, mixing it with high-density polyethylene and tert-butyl-p-diphenol, stirring it evenly, feeding it into an extruder, melting and extruding it, cooling it, and obtaining a premixed masterbatch;
[0015] (6) Take the above premixed masterbatch, mix it with ac foaming agent, steam heat it at 120-130°C for 1-2 hours, and cool it to room temperature to obtain.
[0016] The advantages of the present invention are:
[0017] In the present invention, the insulating layers of the signal line and the voice line are made of foamed polyethylene and low-smoke halogen-free flame-retardant polyolefin respectively, which greatly improves their flame retardant properties and ensures that they have a certain degree of softness;
[0018] In the present invention, a variety of shielding structures are adopted, including a tinned copper wire single shielding layer, a two-layer aluminum-plastic composite tape shielding layer, and a tinned copper wire braided total shielding layer, which further ensures smooth transmission of signals without external interference and has strong anti-interference ability;
[0019] In the present invention, a tinned copper wire drainage line is added to ensure the safety of the cable in places with large flow of people such as gates;
[0020] In the present invention, a wear-resistant, flexible and flame-retardant polyurethane sheath is adopted, and the outer surface of the polyurethane sheath is serrated, so that the cable meets the requirements of soft, flexible and wear-resistant performance.
[0021] The foamed polyethylene insulation layer added in the present invention uses lignin as a raw material to prepare a cellulose-based ATRP initiator, and then initiates the polymerization of trifluoroethyl methacrylate, thereby improving the toughness and strength of the polymer. The present invention treats the monomer with triglycidyl isocyanurate, and then blends it with an amine-modified silica dispersion liquid, promotes epoxy crosslinking at high temperature, and realizes effective dispersion of silica and lignin in the polymer matrix, thereby improving the mechanical stability of the finished material. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 It is a structural schematic diagram of the present invention.
[0023] In the figure: voice line conductor 1, polyolefin insulation layer 2, signal line conductor 3, foamed polyethylene insulation layer 4, tinned copper wire separate shielding layer 5, fine aramid yarn wrapping layer 6, fine aramid yarn rope 7, aluminum-plastic composite tape shielding layer 8, ground wire 9, tinned copper wire braided overall shielding layer 10, polyurethane sheath 11. DETAILED DESCRIPTION
[0024] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.
[0025] Example 1.
[0026] like Figure 1As shown, a signal transmission coaxial composite cable for gate lifting and lowering includes a cable core, the cable core includes six voice lines and three signal lines, the voice line includes a voice line conductor 1 and a polyolefin insulation layer 2 coated on the outside of the voice line conductor; the signal line includes a signal line conductor 3, and the signal line conductor 3 is coated with a foamed polyethylene insulation layer 4, a tinned copper wire separate shielding layer 5, and a fine aramid yarn winding layer 6 from the inside to the outside in sequence; a plurality of fine aramid yarn ropes 7 are filled between the six voice lines and the three signal lines, and the six voice lines and the three signal lines are twisted to form a cable core, and two layers of aluminum-plastic composite tape shielding layers 8 are overlapped and wrapped around the outside of the cable core, and the conductive surface of the aluminum-plastic composite tape shielding layer 8 faces inward and a ground wire 9 is dragged longitudinally, and the ground wire 9 is a tinned copper wire drainage line; the aluminum-plastic composite tape shielding layer 8 is coated with a tinned copper wire braided total shielding layer 10, and the tinned copper wire braided total shielding layer 10 is extruded with a polyurethane sheath 11, and the outer surface of the polyurethane sheath 11 is serrated.
[0027] The voice line conductor 1 and the signal line conductor 3 are both made of tinned alloy copper foil wire twisted conductors. The tinned copper wire separate shielding layer 5 is made of Φ0.008mm tinned copper wire wound.
[0028] The foamed polyethylene insulation layer 4 comprises the following raw materials in parts by weight:
[0029] AC foaming agent 7, high density polyethylene 130, lignin 10, 4-dimethylaminopyridine 10, 2-bromo-2-methylpropionyl bromide 30, triglycidyl isocyanurate 2, trifluoroethyl methacrylate 40, tert-butyl p-diphenol 0.5, nano silicon dioxide 6, cuprous chloride 1-2, triethylamine 2.
[0030] The method for preparing the foamed polyethylene insulation layer 4 comprises the following steps:
[0031] (1) taking triglycidyl isocyanurate, adding it to 80 times its weight of dimethylformamide, stirring evenly, adding trifluoroethyl methacrylate, stirring evenly, to obtain a monomer dispersion;
[0032] (2) Take lignin, add it to 30 times its weight of N,N-dimethylformamide, send it into a stirring tank, add 4-dimethylaminopyridine, stir evenly, place it in an ice water bath, add 2-bromo-2-methylpropionyl bromide, let it stand for 3 hours, discharge it, stir it at room temperature for 15 hours, vacuum filter it, wash the filter cake with water, and vacuum dry it at 55°C to obtain an initiator;
[0033] (3) Mix triethylamine and nano-silicon dioxide, add to N,N-dimethylformamide (30 times the weight of the mixture), and perform ultrasonication for 1 hour to obtain a silicon dispersion;
[0034] (4) Take an initiator, add it to the above monomer dispersion, send it into a reactor, introduce nitrogen, adjust the temperature of the reactor to 70° C., add cuprous bromide, stir and react for 3 hours, add the above silicon dispersion, increase the temperature to 120° C., stir and react for 1.5 hours, discharge the material, and remove dimethylformamide by rotary evaporation to obtain a modified filler;
[0035] (5) taking the modified filler, mixing it with high-density polyethylene and tert-butyl-p-diphenol, stirring it evenly, feeding it into an extruder, melting and extruding it, cooling it, and obtaining a premixed masterbatch;
[0036] (6) Take the above premixed masterbatch, mix it with ac foaming agent, steam heat it at 120°C for 1 hour, and cool it to room temperature to obtain.
[0037] Example 2.
[0038] like Figure 1 As shown, a signal transmission coaxial composite cable for gate lifting and lowering includes a cable core, the cable core includes six voice lines and three signal lines, the voice line includes a voice line conductor 1 and a polyolefin insulation layer 2 coated on the outside of the voice line conductor; the signal line includes a signal line conductor 3, and the signal line conductor 3 is coated with a foamed polyethylene insulation layer 4, a tinned copper wire separate shielding layer 5, and a fine aramid yarn winding layer 6 from the inside to the outside in sequence; a plurality of fine aramid yarn ropes 7 are filled between the six voice lines and the three signal lines, and the six voice lines and the three signal lines are twisted to form a cable core, and two layers of aluminum-plastic composite tape shielding layers 8 are overlapped and wrapped around the outside of the cable core, and the conductive surface of the aluminum-plastic composite tape shielding layer 8 faces inward and a ground wire 9 is dragged longitudinally, and the ground wire 9 is a tinned copper wire drainage line; the aluminum-plastic composite tape shielding layer 8 is coated with a tinned copper wire braided total shielding layer 10, and the tinned copper wire braided total shielding layer 10 is extruded with a polyurethane sheath 11, and the outer surface of the polyurethane sheath 11 is serrated.
[0039] The voice line conductor 1 and the signal line conductor 3 are both made of tinned alloy copper foil wire twisted conductors. The tinned copper wire separate shielding layer 5 is made of Φ0.008mm tinned copper wire wound.
[0040] The foamed polyethylene insulation layer includes the following raw materials in parts by weight:
[0041] AC foaming agent 10, high density polyethylene 150, lignin 15, 4-dimethylaminopyridine 20, 2-bromo-2-methylpropionyl bromide 40, triglycidyl isocyanurate 4, trifluoroethyl methacrylate 50, tert-butyl p-diphenol 1, nano silicon dioxide 10, cuprous chloride 2, and triethylamine 3.
[0042] The method for preparing a foamed polyethylene insulation layer comprises the following steps:
[0043] (1) taking triglycidyl isocyanurate, adding it to 90 times its weight of dimethylformamide, stirring evenly, adding trifluoroethyl methacrylate, stirring evenly, to obtain a monomer dispersion;
[0044] (2) Take lignin, add it to 40 times of its weight of N,N-dimethylformamide, send it into a stirring tank, add 4-dimethylaminopyridine, stir evenly, place it in an ice water bath, add 2-bromo-2-methylpropionyl bromide, let it stand for 5 hours, discharge it, stir it at room temperature for 20 hours, vacuum filter it, wash the filter cake with water, and vacuum dry it at 55°C to obtain an initiator;
[0045] (3) Mix triethylamine and nano-silicon dioxide, add to 40 times the weight of the mixture of N, N-dimethylformamide, and sonicate for 2 hours to obtain a silicon dispersion;
[0046] (4) Take an initiator, add it to the above-mentioned monomer dispersion, send it into a reactor, introduce nitrogen, adjust the temperature of the reactor to 80° C., add cuprous bromide, stir and react for 4 hours, add the above-mentioned silicon dispersion, increase the temperature to 130° C., stir and react for 2 hours, discharge the material, and remove dimethylformamide by rotary evaporation to obtain a modified filler;
[0047] (5) taking the modified filler, mixing it with high-density polyethylene and tert-butyl-p-diphenol, stirring it evenly, feeding it into an extruder, melting and extruding it, cooling it, and obtaining a premixed masterbatch;
[0048] (6) Take the above premixed masterbatch, mix it with ac foaming agent, steam heat it at 130°C for 1-2 hours, and cool it to room temperature to obtain.
[0049] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A signal transmission coaxial composite cable for gate lifting, characterized in that: The invention comprises a cable core, wherein the cable core comprises six voice lines and three signal lines, wherein the voice lines comprise a voice line conductor (1) and a polyolefin insulation layer (2) coated on the outside of the voice line conductor; the signal line comprises a signal line conductor (3), wherein the outside of the signal line conductor (3) is coated with a foamed polyethylene insulation layer (4), a tinned copper wire separate shielding layer (5), and a fine aramid yarn wrapping layer (6) in sequence from the inside to the outside; a plurality of fine aramid yarn ropes (7) are filled between the six voice lines and the three signal lines, and the six voice lines and the three signal lines are twisted to form a A cable core, wherein two layers of aluminum-plastic composite tape shielding layers (8) are wrapped around the outside of the cable core, the conductive surface of the aluminum-plastic composite tape shielding layer (8) faces inward and a ground wire (9) is dragged longitudinally, and the ground wire (9) is a tinned copper wire drainage wire; the aluminum-plastic composite tape shielding layer (8) is coated with a tinned copper wire braided total shielding layer (10), and the tinned copper wire braided total shielding layer (10) is extruded with a polyurethane sheath (11), and the outer surface of the polyurethane sheath (11) is serrated; the foamed polyethylene insulation layer comprises the following raw materials in parts by weight: AC foaming agent 7-10, high density polyethylene 130-150, lignin 10-15, 4-dimethylaminopyridine 10-20, 2-bromo-2-methylpropionyl bromide 30-40, triglycidyl isocyanurate 2-4, trifluoroethyl methacrylate 40-50, tert-butyl p-diphenol 0.5-1, nano silicon dioxide 6-10, cuprous chloride 1-2, triethylamine 2-3; The method for preparing the foamed polyethylene insulation layer comprises the following steps: (1) taking triglycidyl isocyanurate, adding it to 80-90 times its weight of dimethylformamide, stirring evenly, adding trifluoroethyl methacrylate, stirring evenly, to obtain a monomer dispersion; (2) Take lignin, add it to 30-40 times of its weight of N,N-dimethylformamide, send it into a stirring kettle, add 4-dimethylaminopyridine, stir evenly, place it in an ice water bath, add 2-bromo-2-methylpropionyl bromide, let it stand for 3-5 hours, discharge it, stir it at room temperature for 15-20 hours, vacuum filter it, wash the filter cake with water, and vacuum dry it at 50-55° C. to obtain an initiator; (3) Mix triethylamine and nano-silicon dioxide, add to 30-40 times the weight of the mixture of N,N-dimethylformamide, and perform ultrasonication for 1-2 hours to obtain a silicon dispersion; (4) Take an initiator, add it to the above-mentioned monomer dispersion, send it into a reactor, introduce nitrogen, adjust the temperature of the reactor to 70-80° C., add cuprous bromide, stir and react for 3-4 hours, add the above-mentioned silicon dispersion, increase the temperature to 120-130° C., stir and react for 1.5-2 hours, discharge the material, and remove dimethylformamide by rotary evaporation to obtain a modified filler; (5) taking the modified filler, mixing it with high-density polyethylene and tert-butyl-p-diphenol, stirring it evenly, feeding it into an extruder, melting and extruding it, cooling it, and obtaining a premixed masterbatch; (6) Take the above premixed masterbatch, mix it with ac foaming agent, steam heat it at 120-130°C for 1-2 hours, and cool it to room temperature to obtain.
2. A signal transmission coaxial composite cable for gate lifting according to claim 1, characterized in that: The voice line conductor (1) and the signal line conductor (3) are both made of tinned alloy copper foil twisted conductors.
3. A signal transmission coaxial composite cable for gate lifting according to claim 1, characterized in that: The tinned copper wire separate shielding layer (5) is formed by winding tinned copper wires with a diameter of 0.008 mm.