A method for accurately measuring the contour of a cut blank
By arranging 3D laser sensors and thermal imaging cameras on the movement path of the billet, combined with the calibration matrix and ICP algorithm, the precise measurement of the hot billet profile is achieved, which solves the problem of insufficient manual measurement speed and accuracy and is suitable for harsh environments. Improved detection efficiency and data management efficiency.
Patent Information
- Application Number
- CN202211282317.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-10-17
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2042-10-17
AI Technical Summary
In the existing technology, automatic detection systems for contour parameters of hot cast slabs are relatively scarce. Manual measurement speed and accuracy cannot match the production speed, and it is difficult to measure for a long time in harsh environments such as high temperature, dust, and noise, resulting in difficulty in data processing.
Using a non-contact online measurement method of all billet contours, by arranging 4 3D laser sensors and 1 thermal imager on the movement path of the billet, combined with the calibration matrix and ICP algorithm, the precise splicing and parameter calculation of the billet contour is achieved, and the acquisition The width, thickness and sickle bend parameters of each section of the slab.
It improves the detection efficiency and the scale of measurement parameters, saves human resources, is suitable for harsh environments, is simple and convenient to operate, and has efficient data management and traceability.
Smart Images

Figure CN115493520B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of automatic detection, and in particular provides a device and method for accurately measuring the contour of a cut blank on-line. Background Art
[0002] A continuous casting ingot is a cast ingot formed after flame cutting after the continuous casting ingot is put on the production line. At present, the automatic detection system for the contour parameters of a continuous casting ingot is relatively rare in the industry. For the production of hot casting ingots, fast and accurate measurement of contour parameters is extremely important for controlling the quality of the entire production process.
[0003] At present, there is considerable pressure on manual measurement. On the one hand, the speed of manual inspection cannot match the production speed, and the measurement accuracy is greatly affected by external conditions. On the other hand, the magnitude of measurement data cannot be compared with that of automatic measurement equipment, and subsequent data processing also has certain difficulties. The measurement environment of high temperature, dust and noise is not conducive to long-term manual measurement. Summary of the invention
[0004] In view of the above problems, the present invention proposes a contactless online measurement method for all blank contours. The research object is all hot blank contour parameters, which can realize automatic acquisition of all blank contour parameters and provide a data basis for the production process.
[0005] The method for accurately measuring the profile of a blank of the present invention comprises the following specific steps:
[0006] Step 1: Arrange acquisition equipment on the motion path of the ingot, including four 3D laser sensors radiating outward from the four edges on the circumference of the ingot, and a thermal imager on the top of the ingot; the four 3D laser sensors and the thermal imager are respectively connected to the POE network port of the switch through a network cable, and the switch is connected to the network port of the industrial computer through a network cable.
[0007] Step 2: Calibrate the actual installation position of the sensor;
[0008] (1) A cubic calibration block is fixed at the center of the rectangle formed by the four sensor layout positions, so that the four circumferential edges of the calibration block are parallel to the direction of motion of the billet, so that each laser sensor can scan a plane of the calibration block, thereby forming a point cloud contour in each 3D laser sensor and obtaining the endpoint coordinates of the point cloud contour.
[0009] (2) With the center of the calibration block as the origin of the coordinate system, the calibration block coordinate system is established to further determine the edge and corner coordinates of the calibration block.
[0010] (3) Open the four 3D laser sensors to scan the calibration block and directly generate a point cloud contour. Perform a rigid body affine transformation on the endpoint coordinates of the point cloud contour in each 3D laser sensor and the coordinates of the endpoint of the scanned position of the calibration block in the calibration block coordinate system to obtain the relative position of each 3D laser sensor and the calibration block. At this point, the spatial positions of the four 3D laser sensors are acquired, and the coordinate transformation matrix obtained during the calibration process is stored.
[0011] Step 3: Collect the ingot contour data and perform preliminary splicing.
[0012] The ingot is scanned by four 3D laser sensors to generate a point cloud contour, and the calibration matrix obtained in step 3 is called to perform contour splicing to obtain a preliminary splicing contour.
[0013] Step 4: Based on the preliminary splicing of the ingot contour in step 3, further correct the calibration matrix to complete the fine splicing of the ingot cross-sectional contours.
[0014] The point cloud contours of the overlapping parts are used to perform calculation iterations using ICP to reduce the gaps in the point cloud contours of the overlapping parts. During the process, the first ingot cross-section data collected at the beginning is used for fine splicing, and a fine splicing matrix is iterated to correct the calibration matrix. Subsequent cross-section splicing is all done using the correction matrix.
[0015] Step 5: Calculate the width and thickness of the ingot cross section.
[0016] Generate horizontal and vertical line segments to intersect the point cloud contour, and then calculate the distance between the intersection points to obtain the width and thickness of the ingot section.
[0017] Step 6, determine the sickle bend parameter C.
[0018] Record the coordinates of the two corner points on the upper side of the cross section measured for the entire ingot to determine the concave and convex sides; on the concave side, connect the corner point on the first measured cross section of the ingot with the corner point on the last measured cross section to form a straight line, and calculate the distance between the most concave upper corner point and this straight line as C.
[0019] The advantages of the present invention are:
[0020] 1. The invention provides a method for accurately measuring the profile of a blank, which effectively improves the detection efficiency, increases the scale of measurement parameters, and makes data management and tracing efficient;
[0021] 2. The method for accurately measuring the contour of all blanks of the present invention saves human resources, is suitable for harsh environments, and is simple and convenient to operate. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 This is a schematic diagram of the billet structure.
[0023] Figure 2 This is a flow chart of the method for accurately measuring the profile of a blank according to the present invention.
[0024] Figure 3 This is a layout diagram of the acquisition equipment used in the method for accurately measuring the contour of a cut piece of the present invention.
[0025] Figure 4 This is a schematic diagram of the calibration process of the method for accurately measuring the profile of a blank according to the present invention.
[0026] Figure 5 This is a hardware system connection diagram of the method for accurately measuring the contour of a cut blank according to the present invention.
[0027] Figure 6 This is a flow chart of the application process of the method for accurately measuring the contour of a blank according to the present invention. DETAILED DESCRIPTION
[0028] The present invention is further described in detail below with reference to the accompanying drawings.
[0029] like Figure 1 As shown in FIG. 1 , the method for accurately measuring the profile of a billet according to the present invention is for billets with a thickness between 190 and 250 mm at positions Tl and Tr, a width between 1530 and 2000 mm at positions Wup and Wdown, and a length L between 4600 and 11000 mm. Figure 1 As shown. During the production process of the slab, the contours of both sides of multiple end faces of the slab are scanned, and then the collected contour data are spliced and processed. The contour specific position parameter information is solved according to the needs for analysis, judgment, and storage to meet the needs of long-term data measurement / display / storage / playback / export. The above-mentioned Tl position is the Y (about 50mm) distance position from the left side of the slab to the right, and the Tr position is a mirror image of Tl; Wup is the X (about 40mm) distance position downward from the upper surface of the slab, and the Wdown position is a mirror image of Wup; Figure 1 C in the middle is the maximum curvature of the side of the ingot.
[0030] The hardware used in the method for accurately measuring the profile of a blank of the present invention includes a 3D laser sensor, a thermal imager, an air pump, and a gas cooling dryer. The overall measurement method is as follows: Figure 2 As shown, the details are as follows:
[0031] Step 1: Arrange the collection equipment on the billet moving path.
[0032] Arrange 5 profile parameter acquisition devices, including 4 3D laser sensors and 1 thermal imager, to collect the profile parameters of the ingot. The spatial position is as follows: Figure 3 shown.
[0033] The four 3D laser sensors are arranged circumferentially, and are respectively located in the directions of the four edges radiating outward on the circumference of the ingot. At the same time, the four 3D laser sensors are arranged in the same plane, and the plane is perpendicular to the direction of movement of the ingot. It is necessary to ensure that the collection area of the upper left laser sensor covers part of the left side and part of the top surface of the ingot, and the collection area of the lower left laser sensor covers part of the left side and part of the bottom surface of the ingot, and the collection areas of the two laser sensors on the left side have overlapping parts on the left side of the ingot. Similarly, it is ensured that the collection area of the upper right laser sensor covers part of the right side and part of the top surface of the ingot, and the collection area of the lower right laser sensor covers part of the right side and part of the bottom surface of the ingot. Further, the collection areas of the two upper 3D laser sensors on the upper surface of the ingot do not overlap, and the collection areas of the two lower 3D laser sensors on the lower surface of the ingot do not overlap.
[0034] The 3D laser sensor in the present invention adopts the C5-1600CS series, each contour contains 1600 points, the scanning speed is up to 25000Hz, the IP67-level closed shell, the X-direction resolution is about 0.3mm, the Z-direction resolution is about 15μm, the field of view range is 350mm-650mm, the working distance is 700mm, and the line laser color can be selected as 405nm blue and 660nm red. A protective cover is installed on the outside of each 3D laser sensor; the protective cover includes a back cover and a front cover; wherein the back cover is fixed to the laser sensor by screws, and a cooling gas inlet hole is designed on the back cover to be connected to a cooling dryer, and the cooling dryer is connected to an air pump; the air pump generates gas with water vapor at room temperature, and the gas passes through the cooling dryer and enters the protective cover through the inlet hole. The front cover covers the laser sensor and is fixed to the rear cover by screws in the circumferential direction. The front cover is embedded with a light outlet hole for the laser to emit a line laser to the surface of the ingot. The glass window is used for the laser sensor to collect the diffuse reflected light of the line laser. In addition, an air outlet is provided to discharge the hot air in the protective cover.
[0035] The arrangement position of the thermal imager is coplanar with the four 3D laser sensors and is located directly above the ingot, and is used to collect temperature change data at different positions on the surface of the ingot during its movement. The temperature measurement range of the thermal imager in the present invention is 100-1200℃, the accuracy index is 100-750℃ less than or equal to 2%, 750-1200℃ less than or equal to 1.5%, and the operating temperature is -10-60℃. The outside of the thermal imager is designed with a cylindrical protective cover; an air inlet is left on the outer wall of the cylindrical protective cover, and the air inlet is connected to a cooling dryer, and the cooling dryer is connected to an air pump; the air pump generates gas with water vapor at room temperature, and after the gas passes through the cooling dryer, it passes into the protective cover of the equipment through the air inlet. The end face window of the cylindrical protective cover is directly opposite to the acquisition end of the thermal imager, and an air outlet is left on the circumference of the window to discharge the hot air in the cylindrical protective cover.
[0036] The above four 3D laser sensors and one thermal imager are connected to the POE network port of the switch through a network cable, and the switch is connected to the network port of the industrial computer through a network cable. Figure 4 As shown. The switch uses Hikvision DS-3E0510P-S, 8 network ports, maximum power of 20W per port, maximum power of 110W for the whole machine, switching capacity of 20Gbps, packet forwarding rate of 14.88Mpps, working temperature of 0℃~40℃, and desktop installation. The industrial computer uses Lenovo Tianqi win10 home Chinese version, I7-8700CPU, 8G memory, 1T mechanical hard disk + 256G solid state hard disk, Dell U2720QM 4K monitor. At the same time, an encoder is installed in the drive motor carrying the billet movement. The encoder generates pulse signals at equal time intervals when the drive motor is working, and connects to 5 acquisition devices respectively, so that the acquisition devices trigger the acquisition at the same time, ensuring that all devices collect data of the same section of the billet at the same time. The encoder in the present invention uses OMRON incremental rotary encoder E6B2-CWZ6C, diameter 40mm 2M NPN 5-24VDCE6B2-CWZ6C 1000P / R pulse. The encoder and the aforementioned air cooling equipment (cooling dryer and air pump) are powered separately, and the control circuit is connected to the industrial computer.
[0037] Step 2: Calibrate the actual installation position of the sensor.
[0038] Since the precise installation positions of the four 3D laser sensors are not easy to obtain, a calibration method is used to obtain the actual position of each sensor. The method is as follows:
[0039] (1) Figure 5 As shown in the figure, a 100x100x100mm metal cube calibration block is used and fixed at the center of the rectangle formed by the four sensor layout positions, so that the four circumferential edges of the calibration block are parallel to the movement direction of the billet, so that each laser sensor can scan a plane of the calibration block, thereby forming a point cloud contour in each 3D laser sensor and obtaining the endpoint coordinates of the point cloud contour.
[0040] (2) With the center of the calibration block as the origin of the coordinate system, the calibration block coordinate system is established to further determine the edge and corner coordinates of the calibration block.
[0041] (3) Open the four 3D laser sensors to scan the calibration block and directly generate the point cloud contour. Perform a rigid body affine transformation on the endpoint coordinates of the point cloud contour in each 3D laser sensor and the coordinates of the scanned position of the calibration block in the calibration block coordinate system to obtain the relative position of each 3D laser sensor and the calibration block. At this point, the spatial position of the four 3D laser sensors is acquired, and the coordinate conversion calibration matrix obtained in the calibration process is stored. When measuring each cross section of the billet, the calibration matrix can be directly called for processing to obtain the initial billet contour of the spliced billet.
[0042] Step 3: Collect the ingot contour data and perform preliminary splicing.
[0043] The point cloud contour is generated by scanning the ingot by four 3D laser sensors. Since each 3D laser sensor can only collect a part of the point cloud contour data of the ingot, they are arranged in disorder when integrated together; therefore, the calibration matrix obtained in step 3 is called at this time to perform contour splicing to obtain a preliminary spliced contour.
[0044] Step 4: Based on the preliminary splicing of the ingot contour in step 3, further correct the calibration matrix to complete the fine splicing of the ingot cross-sectional contours.
[0045] Since there are two 3D laser sensors on the left and right sides of the billet, and the acquisition surfaces covered by the two 3D laser sensors on each side overlap, the point cloud contours of the overlapping parts are calculated and iterated using ICP (i.e., the closest point iteration algorithm) to minimize the gap between the point cloud contours of the overlapping parts. In the process of fine splicing of each section of the billet, the first billet section data collected at the beginning is used for fine splicing, and the fine splicing matrix is iterated to correct the calibration matrix; thus, all subsequent section splicing can be spliced using the correction matrix to ensure the consistency of the entire billet section splicing.
[0046] Step 5: Calculate the width and thickness of the ingot cross section.
[0047] Since the measurement of the ingot focuses on the thickness and width of the ingot, the middle of the upper and lower surfaces can be ignored. Therefore, the shape of the ingot point cloud contour obtained by the above method after splicing is similar to a bracket, and the point cloud contour in the middle of the upper and lower surfaces is discontinuous. Therefore, when measuring the statistical thickness and width, it is only necessary to generate horizontal and vertical line segments that intersect with the point cloud contour, and then calculate the distance of the intersection point.
[0048] Step 6, determine the sickle bend parameter C.
[0049] According to the sickle bay parameter C, the coordinates of the two corner points on the upper side of the cross section (the cross section perpendicular to the direction of motion of the billet) of the entire billet are recorded to determine the concave and convex sides. The determination method is: use the coordinates of the upper left and right corner points of all cross sections to draw quadratic curves respectively. The concave side is concave if the middle of the curve is concave, and vice versa for convex. On the concave side, connect the upper corner point of the first cross section measured by the billet with the upper corner point of the last cross section measured to form a straight line, and calculate the distance between the most concave upper corner point and this straight line as C.
[0050] The method for accurately measuring the profile of a casting blank of the present invention is as follows: Figure 6 The actual application process is as follows:
[0051] A. Power on the data collection equipment and perform self-test;
[0052] B. Start the air pump and cooling dryer to output cold air to the protective cover of each acquisition device. Manually input the parameter information of the current ingot (including batch number, specification, quality, destination, tolerance, etc.) in the industrial computer system interface, adjust the scanning density parameters, and set the measurement position X, Y;
[0053] C. Check that there is no object to be measured in the measurement field of view, click the start measurement button, drive the working track to run, the billet moves, the encoder outputs pulse signals at equal intervals, the two laser sensors on the upper side scan the measurement area, the billet enters the field of view, and the data collected by the two laser sensors will rise and jump. At this time, the measurement system in the industrial computer receives the rising jump signal to control the 5 acquisition devices to start running immediately and refresh the start measurement time;
[0054] D. During the current billet measurement process, the system will complete the temperature measurement of each section of the billet, scan the contour to form point cloud data, splice the contour, and solve the thickness and width information of each section; refresh and display each end face measurement data in the software interface, judge whether it is qualified or not and mark the unqualified information, and display the temperature curve changing with time. After the single billet measurement is completed, all measurement data will be automatically stored;
[0055] E. When the current billet measurement is completed, the data collected by the two sensors on the upper side will jump downward. When the industrial computer receives the downward jump signal, it stops data processing and refreshes the end measurement time;
[0056] If the current billet measurement is not completed, click the End Measurement button, and the measurement software will automatically store the data and stop after the current measurement process is completed to prevent misoperation; if there is no object to be measured in the measurement field of view at this time, you can directly click the End Measurement button. If you do not click the End Measurement button after the measurement of the object to be measured is completed, the system will be online all the time but will not process or store data, waiting for the next measurement process to arrive.
[0057] After each ingot measurement is completed, the sickle bend parameter C is calculated, and a line graph of the temperature data and ingot size parameters is drawn and refreshed on the software interface. Finally, the data is stored in the database, and the measurement end button is clicked. The system stops running, and the air cooling equipment stops running after a delay of 10 minutes.
[0058] F. Handling of abnormal situations: If an abnormal situation occurs during the measurement process, you can click the emergency stop button to clear the measured data of the current slab and end the measurement process.
[0059] G. Data export function: click the data export button, a page will pop up, select the start time and end time, and you can export the historical data of this time period to the Output folder.
Claims
1. A method for accurately measuring the profile of a cut blank, characterized by: The specific steps are: Step 1: Arrange acquisition equipment on the motion path of the ingot, including four 3D laser sensors in the direction of the four edges radiating outward on the circumference of the ingot, and a thermal imager on the upper part of the ingot; the four 3D laser sensors and the thermal imager are respectively connected to the POE network port of the switch through a network cable, and the switch is connected to the network port of the industrial computer through a network cable; Step 2: Calibrate the actual installation position of the sensor; (1) A cubic calibration block is fixed at the center of the rectangle formed by the four sensor arrangement positions, so that the four circumferential edges of the calibration block are parallel to the direction of motion of the billet, so that each laser sensor can scan a plane of the calibration block, thereby forming a point cloud contour in each 3D laser sensor and obtaining the endpoint coordinates of the point cloud contour; (2) Taking the center of the calibration block as the origin of the coordinate system, establish the calibration block coordinate system, and further determine the edge and corner coordinates of the calibration block; (3) Open the four 3D laser sensors to scan the calibration block and directly generate a point cloud contour. Perform a rigid body affine transformation on the endpoint coordinates of the point cloud contour in each 3D laser sensor and the coordinates of the endpoint of the scanned position of the calibration block in the calibration block coordinate system to obtain the relative position of each 3D laser sensor and the calibration block. At this point, the spatial positions of the four 3D laser sensors are acquired, and the coordinate transformation matrix obtained in the calibration process is stored. Step 3: Collect the billet profile data and perform preliminary splicing; The ingot is scanned by four 3D laser sensors to generate a point cloud contour, and the calibration matrix obtained in step 3 is called to perform contour splicing to obtain a preliminary splicing contour; Step 4: Based on the preliminary splicing of the billet profile in step 3, further correct the calibration matrix to complete the fine splicing of the billet profiles; The point cloud contours of the overlapping parts are used to perform calculation iterations using ICP to reduce the gaps between the point cloud contours of the overlapping parts. During the process, the first ingot cross-section data collected at the beginning is used for fine splicing, and then a fine splicing matrix is iterated to correct the calibration matrix. Subsequent cross-section splicing is all done using the correction matrix. Step 5: Calculation of the width and thickness of the ingot section; Generate horizontal and vertical line segments to intersect the point cloud contour, and then calculate the distance between the intersection points to obtain the width and thickness of the ingot cross section; Step 6, determining the sickle bend parameter C; Record the coordinates of the two corner points on the upper side of the cross section measured for the entire ingot to determine the concave and convex sides; on the concave side, connect the corner point on the first measured cross section of the ingot with the corner point on the last measured cross section to form a straight line, and calculate the distance between the most concave upper corner point and this straight line as C.
2. A method for accurately measuring a cut blank profile as claimed in claim 1, characterized in that: The four 3D laser sensors and thermal imagers are arranged in a plane perpendicular to the direction of motion of the billet.
3. A method for accurately measuring a cut blank profile as claimed in claim 1, characterized in that: A protective cover is installed outside the 3D laser sensor; the protective cover includes a back cover and a front cover; the back cover is fixed to the laser sensor by screws, and a cooling gas inlet hole is designed on the back cover to be connected to a cooling dryer, and the cooling dryer is connected to an air pump; the air pump generates gas with water vapor at room temperature, and the gas passes through the cooling dryer and enters the protective cover through the inlet hole; the front cover covers the laser sensor and is fixed to the back cover by screws in the circumferential direction, and a light outlet hole is embedded in the front cover for the laser to emit a line laser to the surface of the ingot, and a glass window is used for the laser sensor to collect diffusely reflected light of the line laser, and an air outlet hole is also provided to discharge the hot air in the protective cover.
4. A method for accurately measuring a cut blank profile as claimed in claim 1, characterized in that: A cylindrical protective cover is designed on the outside of the thermal imager; an air inlet is left on the outer wall of the cylindrical protective cover, the air inlet is connected to a cooling dryer, and the cooling dryer is connected to an air pump; the air pump generates gas with water vapor at room temperature, and after the gas passes through the cooling dryer, it enters the equipment protective cover through the air inlet; the end face window of the cylindrical protective cover faces the acquisition end of the thermal imager, and air outlets are left around the window to discharge the hot air in the cylindrical protective cover.
5. A method for accurately measuring a cut blank profile as claimed in claim 1, characterized in that: An encoder is installed in the driving motor that carries the ingot. The encoder generates pulse signals at equal time intervals when the driving motor is working. The pulse signals are connected to 5 collection devices respectively, so that the collection devices trigger collection at the same time, ensuring that all devices collect data of the same cross-section of the ingot at the same time.
6. A method for accurately measuring a cut blank profile as claimed in any one of claims 1 to 5, characterized in that: The application process is as follows: A. Power on the data collection equipment and perform self-test; B. Start the air pump and cooling dryer to output cold air to the protective covers of each acquisition device; manually input the parameter information of the current ingot in the industrial computer system interface, adjust the scanning density parameters, and set the measurement position; C. Check that there is no object to be measured in the measurement field of view, click the start measurement button, drive the working track to run, the billet moves, the encoder outputs pulse signals at equal intervals, the two laser sensors on the upper side scan the measurement area, the billet enters the field of view, and the data collected by the two laser sensors will rise and jump. At this time, the measurement system in the industrial computer receives the rising jump signal to control the 5 acquisition devices to start running immediately and refresh the start measurement time; D. During the current billet measurement process, the system will complete the temperature measurement of each section of the billet, scan the contour to form point cloud data, splice the contour, and solve the thickness and width information of each section; refresh and display each end face measurement data in the software interface, judge whether it is qualified or not and mark the unqualified information, and display the temperature curve changing with time. After the single billet measurement is completed, all measurement data will be automatically stored; E. When the current billet measurement is completed, the data collected by the two sensors on the upper side will jump downward. When the industrial computer receives the downward jump signal, it stops data processing and refreshes the end measurement time; After each ingot measurement is completed, the sickle bend parameter C is calculated, and a line graph of the temperature data and ingot size parameters is drawn and refreshed on the software interface. Finally, the data is stored in the database, and the measurement end button is clicked. The system stops running and the air cooling equipment stops running after a delay of 10 minutes.
7. A method for accurately measuring a cut blank profile as claimed in claim 6, characterized in that: If the current billet measurement is not completed, click the End Measurement button to automatically store the data and stop after the current measurement process is completed; if there is no object to be measured in the measurement field of view at this time, you can directly click the End Measurement button. If you do not click the End Measurement button after the measurement of the object to be measured is completed, the system will remain online but will not process or store data, waiting for the next measurement process to arrive.
8. A method for accurately measuring a cut blank profile as claimed in claim 6, characterized in that: If an abnormal situation occurs during the measurement process, click the emergency stop button, the measured data of the current slab will be cleared, and the measurement process will end.
Citation Information
Patent Citations
Contour form control
CN103358574A
Slab contour detection system
CN106123800A
Cabin section contour accurate measurement method based on line laser
CN113554697A
Apparatus and method for measuring width and profile of slabs
KR1020130024349A
Method and apparatus for the determination of the contour of sheet metal blanks
US20020033885A1