Method for preparing array substrate and display panel
By forming a protective layer in the binding area of the OLED display and wrapping the binding pins, the short circuit problem caused by metal ion replacement during the anode etching process is solved, ensuring the normal operation and display effect of the binding pins.
Patent Information
- Application Number
- CN202211142696.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-09-20
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2042-09-20
AI Technical Summary
During the anode etching process of OLED displays, metal ions are easily replaced, resulting in a short circuit between the binding pins, affecting the display effect.
A protective layer is formed in the binding area, including a first protective layer and a second protective layer, wrapping the binding pins to prevent the etching liquid from reacting with the pins and avoiding short circuits. The first protective layer is made of gallium nitride material, and the second protective layer is arranged on the same layer as the planarization layer, wrapping the top protective part, and the side protective part surrounds the binding pins to prevent erosion of the anode etching liquid.
Effectively prevent short circuits between bound pins, ensure normal operation of the pins, improve display effect, avoid metal precipitation of the anode etching liquid, and ensure normal display of the display panel.
Smart Images

Figure CN115497880B_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the field of display technology, and specifically relates to a method for preparing an array substrate and a display panel. Background Art
[0002] In recent years, organic light-emitting diode (OLED) displays have attracted more and more attention from the industry due to their excellent performance. Compared with liquid crystal displays (LCD), which currently occupy a major market share, OLED displays have a series of advantages such as light weight, small thickness, low power consumption, bright colors, fast response speed, wide viewing angle, and flexible display.
[0003] Bonding is an important step in the manufacturing process of OLED displays. It refers to the process of connecting the bonding pins in the bonding area of the OLED panel and the driver integrated circuit (IC), flexible printed circuit (FPC) or touch IC according to a certain workflow and conducting them. However, during the anodic etching process, the metal ions in the etching solution are easily replaced by metal and gathered between adjacent bonding pins, resulting in a short circuit between the bonding pins and display abnormalities. Summary of the invention
[0004] The purpose of the present application is to provide a method for preparing an array substrate and a display panel, which can protect the binding pins during the anode etching process, ensure the normal operation of the binding pins, and improve the display effect.
[0005] A first aspect of the present application provides a method for preparing an array substrate, comprising:
[0006] Providing a base substrate, the base substrate comprising a display area and a binding area;
[0007] A driving layer and a planarization layer are sequentially formed in the display area, wherein the driving layer includes a plurality of transistors, and the planarization layer has a via hole exposing a first electrode of the transistor, wherein the first electrode is a source electrode or a drain electrode;
[0008] forming binding pins and a protective layer wrapping the binding pins in sequence in the binding area;
[0009] After the protection layer is formed, an anode is formed on the planarization layer of the display area, and the anode is connected to the first electrode of the transistor through the via hole.
[0010] In an exemplary embodiment of the present application, after forming an anode on the planarization layer of the display area, the method for preparing the array substrate further includes:
[0011] The protective layer on the binding pins is removed to expose the binding pins.
[0012] In an exemplary embodiment of the present application, the protective layer includes a first protective layer, wherein before the planarization layer is formed in the display area, the first protective layer covering the binding pins is formed in the binding area.
[0013] In an exemplary embodiment of the present application, the first protective layer wraps the binding pin.
[0014] In an exemplary embodiment of the present application, the first protective layer includes:
[0015] A top protection portion, the top protection portion is located at a side of the binding pin away from the substrate base;
[0016] A side protection portion is formed on the driving layer and arranged around the binding pin, the side protection portion is connected to the top protection portion, and a surface of the side protection portion away from the base substrate is lower than a surface of the top protection portion away from the base substrate.
[0017] In an exemplary embodiment of the present application, the binding pins are provided in plurality and are spaced apart from each other;
[0018] The material of the first protective layer is gallium nitride, a plurality of first protective layers are provided and adjacent ones are disconnected from each other, and the first protective layers are provided in a one-to-one correspondence with the binding pins.
[0019] In an exemplary embodiment of the present application, the protective layer further includes a second protective layer, and the material of the second protective layer is different from that of the first protective layer, wherein:
[0020] After forming the first protection layer, the second protection layer is formed in the binding area, and the second protection layer at least wraps the top protection part.
[0021] In an exemplary embodiment of the present application, the orthographic projection of the second protection layer on the base substrate is located within the orthographic projection of the first protection layer on the base substrate, so that the side surface of the side protection portion is exposed.
[0022] In an exemplary embodiment of the present application, the second protection layer and the planarization layer are arranged in the same layer and are spaced from each other; and / or
[0023] The binding pin is arranged at the same layer as the source and drain of the transistor; and / or
[0024] The anode is a sandwich structure of indium tin oxide, silver and indium tin oxide.
[0025] A second aspect of the present application provides a display panel, comprising a cathode, a light-emitting layer, and an array substrate manufactured by any of the above-mentioned manufacturing methods, wherein the light-emitting layer is arranged between the cathode and the anode.
[0026] This application scheme has the following beneficial effects:
[0027] The present application scheme includes a method for preparing an array substrate. By forming a protective layer that completely covers the binding pins in the binding area, the binding pins can be protected from reacting with the etching solution during the anodic etching process, thereby preventing the etching solution from precipitating metal between adjacent binding pins, ensuring that adjacent pins are disconnected from each other, and preventing adjacent binding pins from being connected and causing a short circuit. In addition, the present application scheme also includes a display panel. The protective layer can effectively prevent short circuits between binding pins, ensuring the normal operation of the binding pins, thereby ensuring the display effect of the display panel.
[0028] Other features and advantages of the present application will become apparent from the following detailed description, or may be learned in part by the practice of the present application.
[0029] It should be understood that the foregoing general description and the following detailed description are exemplary and explanatory only and are not restrictive of the present application. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] The drawings herein are incorporated into the specification and constitute a part of the specification, illustrate embodiments consistent with the present application, and together with the specification are used to explain the principles of the present application. Obviously, the drawings described below are only some embodiments of the present application, and for ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0031] Figure 1 A schematic diagram showing a process of a method for preparing an array substrate provided in Embodiment 1 of the present application is shown;
[0032] Figure 2 A schematic structural diagram of a substrate provided in Embodiment 1 of the present application is shown;
[0033] Figure 3 A schematic diagram of the process of forming a source electrode, a drain electrode and a binding pin provided in the first embodiment of the present application is shown;
[0034] Figure 4 A schematic structural diagram showing a buffer layer provided in the first embodiment of the present application and arranged on the substrate;
[0035] Figure 5A schematic diagram of a structure in which an active layer is provided on a buffer layer according to a first embodiment of the present application is shown;
[0036] Figure 6 A schematic diagram of a structure in which a gate insulating layer is provided on a buffer layer according to a first embodiment of the present application is shown;
[0037] Figure 7 A schematic diagram of a structure in which a gate provided in Embodiment 1 of the present application is disposed on a gate insulating layer is shown;
[0038] Figure 8 A schematic structural diagram of forming a first insulating layer on a gate insulating layer provided in the first embodiment of the present application is shown;
[0039] Fig. 9 A schematic diagram of a structure in which a first groove hole and a second groove hole are provided in the first embodiment of the present application is shown;
[0040] Fig.10 A schematic diagram of the structure of forming a source electrode, a drain electrode and a binding pin provided in the first embodiment of the present application is shown;
[0041] Fig.11 A schematic diagram of the process structure of forming a protective layer provided in the first embodiment of the present application is shown;
[0042] Fig.12 A schematic diagram of a structure in which a first protective layer is formed on a binding pin provided in the first embodiment of the present application is shown;
[0043] Fig.13 A schematic diagram of a structure in which a planarization layer is formed in a display area and a binding area according to Embodiment 1 or Embodiment 2 of the present application is shown;
[0044] Fig.14 A schematic diagram of a structure for forming an anode on a display area provided in Embodiment 1 or Embodiment 2 of the present application is shown;
[0045] Fig.15 A schematic diagram of a process for removing a protective layer provided in Embodiment 1 of the present application is shown;
[0046] Fig.16 A schematic diagram of the structure of removing the protective layer provided in the first embodiment of the present application is shown;
[0047] Fig.17 A schematic diagram showing the structure of the display area and the binding area provided in the first embodiment of the present application is shown;
[0048] Fig.18 A schematic diagram of the structure of the cathode, light-emitting layer and anode provided in Example 2 of the present application is shown.
[0049] Description of reference numerals:
[0050] 10. Array substrate; 10a. Via hole; 10b. First groove hole; 10c. Second groove hole; 101. Base substrate; 101a. Display area; 101b. Binding area; 102. Planarization layer; 1031. Source; 1032. Drain; 104. Buffer layer; 105. Active layer; 106. Gate insulating layer; 107. Gate; 108. First insulating layer; 109. Binding pin; 110. Protective layer; 1101. First protective layer; 1102. Second protective layer; 20. Anode; 30. Cathode; 40. Light-emitting layer. DETAILED DESCRIPTION
[0051] Example embodiments will now be described more fully with reference to the accompanying drawings. However, example embodiments can be implemented in a variety of forms and should not be construed as limited to the examples set forth herein; rather, these embodiments are provided so that this application will be more comprehensive and complete and fully convey the concept of the example embodiments to those skilled in the art.
[0052] In this application, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0053] In this application, unless otherwise clearly specified and limited, the terms "assembly", "connection" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0054] In addition, described feature, structure or characteristic can be combined in one or more embodiments in any suitable manner. In the following description, many specific details are provided to provide a full understanding of the embodiments of the present application. However, those skilled in the art will appreciate that the technical scheme of the present application can be put into practice without one or more of the specific details, or other methods, components, devices, steps, etc. can be adopted. In other cases, known methods, devices, realizations or operations are not shown or described in detail to avoid blurring the various aspects of the application.
[0055] Embodiment 1
[0056] Embodiment 1 of the present application provides a method for preparing an array substrate 10, see Figure 1As shown, it includes the following steps:
[0057] Step S100: See Figure 2 As shown, a base substrate 101 is provided, and the base substrate 101 includes a display area 101a and a binding area 101b.
[0058] For example, the shape of the base substrate 101 can be circular, square, oval, etc., and its shape is not specifically limited; in addition, the base substrate 101 can be made of organic glass, resin, quartz or metal, etc., and its material is not specifically limited.
[0059] Step S200 : forming a driving layer and a planarization layer 102 in the display area 101 a in sequence, wherein the driving layer includes a plurality of transistors, and the planarization layer 102 has a via hole 10 a exposing a first electrode of the transistor, wherein the first electrode is a source electrode 1031 or a drain electrode 1032 .
[0060] The driving layer includes a plurality of transistors arranged in an array, and the transistors include a first electrode and a second electrode, the first electrode and the second electrode are spaced apart from each other and both overlap the active layer 105; by way of example, the first electrode can be the drain 1032, and the second electrode can be the source 1031; of course, in different implementations, the first electrode can also be the source 1031, and the second electrode can be the drain 1032.
[0061] In this embodiment, the first electrode represents the drain 1032 , and the second electrode represents the source 1031 .
[0062] The steps of sequentially forming transistors in the display area 101a specifically include the following steps, see Figure 3 As shown:
[0063] Step S201, see Figure 4 As shown, a buffer layer 104 is formed on the base substrate 101 in the display area 101a and the binding area 101b. The buffer layer 104 can be made of materials such as silicon nitride (SiNx) and silicon oxide (SiOx).
[0064] Step S202, see Figure 5 As shown, an active layer 105 is formed on the buffer layer 104 of the display area 101a; the active layer 105 is made of polycrystalline silicon (Poly-Si);
[0065] Step S203, see Figure 6 As shown, a gate insulating layer 106 is formed on the buffer layer 104 in the display area 101a and the binding area 101b, and the gate insulating layer 106 completely covers the active layer 105; the gate insulating layer 106 is made of materials such as silicon nitride (SiNx) and silicon oxide (SiOx).
[0066] Step S204, see Figure 7As shown, a gate electrode 107 is formed on the gate insulating layer 106 in the display region 101a.
[0067] For example, a first metal layer is coated on the gate insulating layer 106, and the first metal layer is patterned (illuminated and etched) to form a gate 107 on the gate insulating layer 106. The gate 107 is used to control the on and off of the transistor. The first metal layer can be made of metal materials such as aluminum (Al), copper (Cu), and molybdenum (Mo).
[0068] Step S205, see Figure 8 As shown, a first insulating layer 108 is formed on the gate insulating layer 106 in the display area 101a and the binding area 101b, and the first insulating layer 108 in the display area 101a completely covers the gate 107; the first insulating layer 108 can be made of the same material as the gate insulating layer 106, for example, silicon nitride (SiNx) and silicon oxide (SiOx), but not limited thereto.
[0069] Step S206, see Fig. 9 As shown, the first insulating layer 108 and the gate insulating layer 106 are patterned in the display area 101a to form a first recessed hole 10b and a second recessed hole 10c to expose a portion of the active layer 105;
[0070] For example, the first insulating layer 108 and the gate insulating layer 106 are subjected to light irradiation and pattern etching to form a first recess hole 10 b and a second recess hole 10 c on the left and right sides of the gate 107 , which respectively expose a portion of the active layer 105 .
[0071] Step S207, see Fig.10 As shown, a second metal layer is coated in the display area 101a, and the second metal layer is patterned (illuminated and etched) to form a corresponding pattern.
[0072] For example, when a second metal layer is coated in the display area 101a, the metal in the second metal layer flows into the first groove hole 10b and the second groove hole 10c, overlaps with the active layer 105, and then forms the source 1031 and the drain 1032 of the transistor respectively through patterning.
[0073] It should be noted that the second metal layer can be a sandwich structure of titanium (Ti) / aluminum (Al) / titanium (Ti), wherein Al is easily oxidized and Ti is not easily oxidized, and thus, adding Ti on both sides of Al can prevent oxidation of Al.
[0074] It is worth mentioning that the transistor in the embodiment of the present application adopts a top gate type; of course, a bottom gate type may also be adopted in other embodiments. It is understandable that when the bottom gate type is adopted, the gate 107 is located below the active layer 105.
[0075] Step S300, see Figure 1 and Fig.10 As shown, a binding pin 109 and a protection layer 110 wrapping the binding pin 109 are sequentially formed in the binding area 101 b.
[0076] For example, the second metal layer in the above step S207 is patterned to obtain a plurality of non-adjacent binding pins 109, that is, the binding pins 109 are arranged on the same layer as the source 1031 and the drain 1032 of the transistor; one end of the binding pin 109 is used to connect and conduct with the pin of the driving integrated circuit (AI for short) via anisotropic conductive glue, and the other end is used to connect signal lines such as data line (Date) and scan line (Gate).
[0077] It should be noted that "same-layer arrangement" refers to the use of the same film-forming process to form a film layer for forming a specific pattern, and then using the same mask to form a layer structure through a single patterning process. That is, one patterning process corresponds to a mask (also called a photomask). Depending on the specific pattern, a single patterning process may include multiple exposure, development or etching processes, and the specific pattern in the formed layer structure may be continuous or discontinuous, and these specific patterns may also be at different heights or have different thicknesses. This simplifies the manufacturing process, saves manufacturing costs, and improves production efficiency.
[0078] In addition, a protective layer 110 is formed on the first insulating layer 108, and the protective layer 110 wraps the binding pin 109 to prevent the metal from being replaced by an oxidation-reduction reaction between the etching liquid of the anode 20 and the binding pin 109, thereby ensuring that adjacent binding pins 109 are disconnected from each other and that there is no short circuit between the binding pins 109, thereby ensuring the normal information transmission function of the binding pin 109.
[0079] It is worth mentioning that the protection layer 110 in the binding area 101 b can be formed before the anode 20 is formed on the planarization layer 102 in the display area 101 a , so as to better protect the binding pins 109 .
[0080] In addition, the protection layer 110 can be a single-layer or multi-layer structure, which can well protect the binding pins 109 and is not easy to react with the etching solution.
[0081] When the protective layer 110 adopts a one-layer structure, the protective layer 110 wraps the binding pin 109, and the protective layer 110 can be made of a material that does not react with the etching solution of the anode 20, which can be specifically designed according to different embodiments.
[0082] When the protective layer 110 adopts a two-layer structure, the specific implementation method may be as follows:
[0083] For example, the protective layer 110 in the binding area 101b includes a first protective layer 1101 and a second protective layer 1102. The forming of the protective layer 110 in the binding area 101b includes the following steps:
[0084] Step S301, see Fig.11 and Fig.12 As shown, a first protection layer 1101 is formed on the first insulating layer 108 to wrap the binding pin 109 .
[0085] Optionally, a film is deposited on the first insulating layer 108 by metal organic chemical vapor deposition (MOCVD), and patterned by photolithography and etching to form a first protection layer 1101 that wraps the binding pin 109 .
[0086] Step S302, see Fig.13 As shown, after the first protection layer 1101 is formed, a second protection layer 1102 is formed in the binding area 101 b , and the second protection layer 1102 at least wraps the top protection portion.
[0087] It should be noted that the first protective layer 1101 and the second protective layer 1102 are made of different materials; for example, the first protective layer 1101 is made of gallium nitride (GaN).
[0088] In addition, the second protective layer 1102 in the binding area 101b and the second protective layer 1102 in the display area 101a can be arranged in the same layer, that is, the second protective layer 1102 uses the same material as the planarization layer 102, and the same layer arrangement is the same as the above description, which will not be repeated here.
[0089] It can be understood that the second protection layer 1102 in the binding area 101 b and the planarization layer 102 in the display area 101 a are formed by the same mask process (formed by light irradiation and etching).
[0090] In this way, by wrapping the first protective layer 1101 around the outside of the binding pin 109, the binding pin 109 can be well prevented from reacting with the anode 20 etching solution, thereby avoiding a short circuit between the binding pins 109 and ensuring the signal transmission efficiency of the binding pin 109. In addition, the first protective layer 1101 can be protected by the second protective layer 1102 to prevent the first protective layer 1101 from being etched by the anode 20 etching solution, thereby better protecting the binding pin 109. In addition, by manufacturing the second protective layer 1102 while manufacturing the planarization layer 102, the manufacturing process is reduced, thereby reducing the manufacturing cost.
[0091] It is worth mentioning that see Fig.12As shown, the first protection layer 1101 and the second protection layer 1102 are arranged in one-to-one correspondence with the binding pins 109; and the longitudinal section of the first protection layer 1101 on the binding pins 109 can be in an arch bridge shape or a step shape.
[0092] For example, the longitudinal section of the first protective layer 1101 is stepped, and the first protective layer 1101 includes a top protection portion (not shown in the figure) and a side protection portion (not shown in the figure); wherein, the two sides of the first protective layer 1101 are side protection portions, and the middle portion is a top protection portion, that is, the top protection portion is located on the side of the binding pin 109 away from the base substrate 101, the side protection portion is formed on the driving layer and arranged around the binding pin 109, and the surface of the side protection portion away from the base substrate 101 is lower than the surface of the top protection portion away from the base substrate 101.
[0093] In this way, the first protective layer 1101 adopts a stepped structure, which can increase the coverage width of the bottom of the first protective layer 1101, prevent the anode 20 etching solution from etching the first protective layer 1101, thereby preventing the binding pins 109 from leaking out and better protecting the binding pins 109.
[0094] It should be noted that the side protection portion is connected to the top protection portion and is made in one piece to better protect the binding pins 109 .
[0095] In addition, the second protective layer 1102 may partially wrap the top protective portion, or may completely wrap the top protective portion, and the two ends of the second protective layer 1102 are respectively overlapped on the side protective portions on both sides. Furthermore, the second protective layer 1102 may overlap with the edge position of the side protective portion, or the orthographic projection of the second protective layer 1102 on the base substrate 101 may be smaller than the orthographic projection of the first protective layer 1101 on the base substrate 101, that is, it does not overlap with the edge position of the side protective portion.
[0096] Understandably, see Fig.13 As shown, the orthographic projection of the second protective layer 1102 on the base substrate 101 is smaller than the orthographic projection of the first protective layer 1101 on the base substrate 101, which can avoid the second protective layer 1102 directly contacting the first insulating layer 108, making it easier to peel off the second protective layer 1102 in the binding area 101b.
[0097] Step S400, see Figure 1 and Fig.14 As shown, after forming the protection layer 110, an anode 20 is formed on the planarization layer 102 of the display area 101a, and the anode 20 is connected to the first electrode of the transistor through the via hole 10a.
[0098] For example, a film is formed on the planarization layer 102 by physical vapor deposition (PVD), and the anode 20 is formed by photolithography and wet etching; the anode 20 can be a sandwich structure of ITO (indium tin oxide), Ag (silver), and ITO (indium tin oxide). Ag (silver) is easily oxidized, and adding ITO (indium tin oxide) on the upper and lower sides of Ag for protection can effectively prevent the oxidation of Ag.
[0099] It can be understood that during the wet etching process of the anode 20, the binding pin 109 can be protected by the protective layer 110 to prevent the aluminum (Al) from being exposed to the etching solution, so that the aluminum (Al) will not provide electrons to the etching solution, thereby preventing the Ag+ (silver ions) in the etching solution of the anode 20 from acting on the aluminum in the binding pin 109 and causing silver (Ag) precipitation.
[0100] Further, see Fig.15 As shown, the method for preparing the array substrate 10 further includes the following steps:
[0101] Step S500, see Fig.16 and Fig.17 As shown, the protection layer 110 on the binding pins 109 is removed to expose the binding pins 109 .
[0102] For example, a 266nm / 248nm laser is used to irradiate the first protective layer 1101 to remove the first protective layer 1101 and the second protective layer 1102 on the binding pins 109 , so that the binding pins 109 are exposed to facilitate binding with the driver integrated circuit.
[0103] Among them, the first protective layer 1101 can be made of materials that are easily decomposed by laser, such as gallium nitride (GaN), gallium oxide (GaO) and other materials; in this way, the protective layer 110 on the binding pin 109 can be better removed, and the removal is more convenient and quick, and it is not easy to damage the binding pin 109, thereby ensuring the transmission of information.
[0104] It is understandable that when the laser is used to irradiate the first protective layer 1101, the first protective layer 1101 and the second protective layer 1102 located on the binding pins 109 are peeled off at the same time. In this way, a process can be saved, and the production cost can be saved.
[0105] In addition, gallium nitride (GaN) or gallium oxide (GaO) will form conductive metal gallium after being decomposed by laser, and if it is not cleaned thoroughly, it will cause a short circuit between adjacent binding pins 109; therefore, in order to avoid the residual metal gallium causing a short circuit between the binding pins 109, the first protective layer 1101 and the second protective layer 1102 on each binding pin 109 are disconnected from each other.
[0106] In addition to the method of removing the protective layer 110 by laser irradiation, the second protective layer 1102 on the first protective layer 1101 can be first removed by exposure and development, and then the first protective layer 1101 can be removed by laser irradiation. In this way, when the second protective layer 1102 is removed, the binding pins 109 can be protected by the first protective layer 1101 to prevent the binding pins 109 from being damaged.
[0107] It should be noted that the protective layer 110 adopts the two structures of the first protective layer 1101 and the second protective layer 1102, which is mainly based on: if only the second protective layer 1102 or other materials are used for protection, since the cured second protective layer 1102 or other materials cannot be directly removed by development, they need to be removed by coating photoresist, exposure, and dry etching, and the dry etching method has low selectivity, so it is difficult to remove the second protective layer 1102 or other materials at the binding position, and the binding pin 109 will be damaged to a certain extent when the second protective layer 1102 or other materials at the binding position are removed by dry etching. If only the first protective layer 1101 is used, the etching solution may partially etch the first protective layer 1101, causing the binding pin 109 to be exposed, thereby causing the binding pin 109 to short-circuit. Therefore, based on the above two considerations, the embodiment of the present application adopts a combination of the first protective layer 1101 and the second protective layer 1102 to protect the binding pin 109.
[0108] In addition, after removing the first protective layer 1101 and the second protective layer 1102 under laser irradiation, the residual protective layer 110 on the binding pin 109 is removed by cleaning to avoid affecting the normal operation of the binding pin 109.
[0109] It is worth mentioning that in the present embodiment, the array substrate 10 adopts a low-temperature polycrystalline silicon LTPS-TFT driving backplane; of course, in different embodiments, the array substrate 10 may also adopt other driving backplanes, and the preparation method thereof is the same as that in the embodiment of the present application, and will not be repeated here one by one.
[0110] Embodiment 2
[0111] A second embodiment of the present application provides a display panel, which is an organic light-emitting diode display panel (Organic Light-Emitting Diode, OLED); wherein the organic light-emitting diode display panel is a top emission type.
[0112] See also Fig.18The organic light emitting diode display panel shown includes a cathode 30, a light emitting layer 40 and an array substrate 10 manufactured using the preparation method in Example 1, wherein the light emitting layer 40 is located between the cathode 30 and the anode 20; under the drive of an external voltage, the electrons injected into the cathode 30 and the holes injected into the anode 20 recombine in the light emitting layer 40 to form electron-hole pairs at a bound energy level, i.e., excitons, which radiate and excite to emit photons, generate visible light, and the display panel can then realize display.
[0113] Among them, see Fig.13 and Fig.14 As shown, by forming a protective layer 110 between the anodes 20, the binding pins 109 in the binding area 101b are protected to avoid short circuits between the binding pins 109, ensure normal transmission of the binding pins 109, ensure normal generation of holes in the anode 20, and further ensure normal generation of visible light by the light-emitting layer 40, thereby ensuring the display effect of the display panel.
[0114] In the description of this specification, the description with reference to the terms "some embodiments", "exemplarily", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present application. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, without contradiction.
[0115] Although the embodiments of the present application have been shown and described above, it can be understood that the above embodiments are exemplary and cannot be understood as limitations on the present application. Ordinary technicians in this field can change, modify, replace and modify the above embodiments within the scope of the present application. Therefore, any changes or modifications made in accordance with the claims and description of the present application should fall within the scope of the patent of this application.
Claims
1. A method for preparing an array substrate, It is characterized in that include: A base substrate is provided, the base substrate comprising a display area and a binding area; a driving layer and a planarization layer are sequentially formed in the display area, the driving layer comprising a plurality of transistors, the planarization layer having a via hole exposing a first electrode of the transistor, the first electrode being a source electrode or a drain electrode, the driving layer comprising a first insulating layer disposed on the base substrate, the first insulating layer being disposed on a side of the planarization layer close to the base substrate; A binding pin and a protective layer wrapping the binding pin are sequentially formed in the binding area, the protective layer comprising a first protective layer and a second protective layer, wherein before the planarization layer is formed in the display area, the first protective layer covering the binding pin is formed in the binding area, the first protective layer comprising a top protective portion and a side protective portion, the top protective portion being located on a side of the binding pin away from the base substrate; the first protective layer is formed on the driving layer and arranged around the binding pin, the side protective portion is connected to the top protective portion, and a surface of the side protective portion away from the base substrate is lower than a surface of the top protective portion away from the base substrate; the second protective layer is arranged on a side of the first protective layer away from the first insulating layer, the second protective layer is arranged in the same layer as the planarization layer, the orthographic projection of the second protective layer on the base substrate is located within the orthographic projection of the first protective layer on the base substrate, so that the side surface of the side protective portion is exposed; After forming the protective layer, an anode is formed on the planarization layer of the display area, and the anode is connected to the first electrode of the transistor through the via hole; wherein, after forming the anode on the planarization layer of the display area, the method for preparing the array substrate further includes: The first protection layer and the second protection layer on the binding pin are removed simultaneously by laser irradiation to expose the binding pin.
2. The method for preparing an array substrate according to claim 1, It is characterized in that The first protection layer wraps the binding pins.
3. The method for preparing an array substrate according to claim 1, It is characterized in that The binding pins are arranged in plurality and are spaced apart from each other; The material of the first protective layer is gallium nitride, a plurality of first protective layers are provided and adjacent ones are disconnected from each other, and the first protective layers are provided in a one-to-one correspondence with the binding pins.
4. The method for preparing an array substrate according to claim 1, It is characterized in that The protective layer further includes a second protective layer, the second protective layer and the first protective layer are made of a different material, wherein: After forming the first protection layer, the second protection layer is formed in the binding area, and the second protection layer at least wraps the top protection part.
5. The method for preparing the array substrate according to claim 4, It is characterized in that The second protection layer and the planarization layer are arranged in the same layer and are spaced from each other; and / or The binding pin is arranged at the same layer as the source and drain of the transistor; and / or The anode is a sandwich structure of indium tin oxide, silver and indium tin oxide.
6. A display panel, It is characterized in that The invention comprises a cathode, a light-emitting layer and an array substrate manufactured by the manufacturing method according to any one of claims 1 to 5, wherein the light-emitting layer is arranged between the cathode and the anode.