Preparation and application of a 3D printed double gel capable of loading fat-soluble and water-soluble active substances
By using 3D printed double gel composed of vegetable oil, the problem of insufficient application and complex preparation of food double gels in the field of 3D printing in the prior art is solved, and low-cost and efficient double gel preparation is achieved, with good stability Sex and printing characteristics, suitable for fat-suppressing and functional food applications.
Patent Information
- Application Number
- CN202211179578.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-09-27
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2042-09-27
AI Technical Summary
The existing food double gels have few applications in the field of 3D printing, the preparation process is complex, and the oil gel agent content is high, making it difficult to meet the low-cost and efficient 3D printing needs.
3D printed double gel composed of vegetable oil, drinking water, hydrogel agent, oilgel agent and emulsifier are used to form a uniform double gel through stirring and homogenization, and the preparation process is simplified. Suitable for 3D printing.
It realizes low-cost and efficient 3D printed double gel preparation, has good stability and printing characteristics, is suitable for large-scale production, suitable for the application of fat-supervised and functional foods, and meets personalized nutritional needs.
Smart Images

Figure CN115644263B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of food processing, and particularly relates to a 3D printed double gel capable of loading fat-soluble and water-soluble active substances, and a preparation method and application thereof. Background Art
[0002] 3D food printing uses food materials with specific characteristics, and deposits them layer by layer through a food-grade nozzle using a 3D food printer according to the set 3D template to obtain the corresponding 3D graphic food. By changing the composition and ratio of food materials, 3D food printing can achieve customized food shape, color, texture, flavor or nutrition and other personalized needs, and has shown unique advantages in leading the production of personalized precision nutritious food. For example, according to the nutritional needs of different groups of people such as the elderly and patients with specific gastrointestinal diseases, customized diets that meet personal nutrition and appearance needs can be customized.
[0003] In recent years, the number of people suffering from many diseases such as hypertension, hyperlipidemia, and obesity has been increasing, which is closely related to a high-fat and high-calorie diet. Low-sugar and low-fat foods are becoming more and more popular, and reducing the fat and calorie content of food has become an important trend in food preparation. As a uniform and stable composite system containing both oil gel and hydrogel, the food double gel contains not only the rich beneficial unsaturated fatty acids in liquid oil, but also has the texture characteristics of solid fat without the advantages of producing trans fatty acids, as well as the characteristics of encapsulating and dissolving a variety of fat-soluble active substances; at the same time, the hydrogel contained in it has the advantages of high compatibility with food, good fusion, and the ability to dissolve a variety of water-soluble bioactive substances. In addition, compared with simple oil gel and hydrogel, the double gel exhibits better stability and texture properties, and is more suitable for food processing. Therefore, food double gel has great application potential in the development of fat-reducing foods and functional foods, especially as a load and embedding of fat-soluble and water-soluble active substances.
[0004] Although a small number of food double gel systems have been developed, they are rarely used in food, and there are very few double gel systems for food 3D printing, and their preparation is relatively complicated. Chinese patent application (CN202210433829.5-A double gel with a printable protein network and its preparation method and application) discloses a double gel with a printable protein network and its preparation method and application, and provides a 3D printable double gel prepared by an emulsion template method. The preparation process is relatively complicated and requires the use of plant protein, hydrogel, salt solution, oil gel and other gelling agents or gel adjuvants to form a double gel with printing characteristics, which is mainly used in the field of artificial meat. Chinese patent application (CN202111434454.6-A temperature-sensitive simulation of plastic fat, oral texture and digestive behavior controllable double gel and its preparation and application) discloses a temperature-sensitive simulation of plastic fat, oral texture and digestive behavior controllable double gel and its preparation and application. Its hydrogel preparation process is relatively complicated, requiring the use of two types of hydrogels, and the application of double gel in the field of food 3D printing has not been developed. The Chinese patent application (CN202111538724.8-A method for preparing a food-grade dual gel based on grease gel and hydrogel) discloses a method for preparing a food-grade dual gel based on grease gel and hydrogel. The oil gel content used is high, and the application of the dual gel in the field of food 3D printing has not been developed. Summary of the invention
[0005] In order to overcome the shortcomings and deficiencies of the above-mentioned prior art, the primary purpose of the present invention is to provide a 3D printing food-grade double gel with fewer types of required gelling agents, low oil gelling agent content, simple preparation method, stable product, and excellent 3D printing properties, so that food-grade double gel can be used in food 3D printing at a lower cost and higher efficiency.
[0006] Another object of the present invention is to provide a method for preparing the above-mentioned 3D printed double gel capable of loading fat-soluble and water-soluble active substances.
[0007] Another object of the present invention is to provide the application of the above-mentioned 3D printing double gel that can load fat-soluble and water-soluble active substances in 3D printing fat substitutes and functional foods, so as to meet people's needs for oil-water double gels to encapsulate different types of active substances and be suitable for 3D printing.
[0008] The purpose of the present invention is achieved through the following solutions:
[0009] A 3D printing double gel capable of loading fat-soluble and water-soluble active substances, wherein the raw materials include the following components in weight percentage: 25% to 80% vegetable oil, 25% to 75% drinking water, 1% to 5% hydrogel, 0.5% to 5% oil gel, and 0% to 2% emulsifier.
[0010] The raw materials of the 3D printing double gel capable of loading fat-soluble and water-soluble active substances also include the following raw materials in weight percentage: 0.01% to 0.5% of water-soluble active substances and 0.01% to 0.5% of fat-soluble active substances.
[0011] Preferably, the raw materials of the 3D printed double gel capable of loading fat-soluble and water-soluble active substances include the following raw materials in weight percentage: 25% to 80% vegetable oil, 25% to 75% drinking water, 1% to 4% hydrogel, 0.5% to 4% oil gel, 0% to 1.5% emulsifier, 0.01% to 0.2% water-soluble plant polyphenols, and 0.01% to 0.2% fat-soluble plant polyphenols.
[0012] The vegetable oil is at least one of rapeseed oil, soybean oil, sunflower oil, peanut oil, olive oil and corn oil.
[0013] The hydrogel is at least one of gelatin, pectin, konjac gum and guar gum.
[0014] The oil gel is at least one of candelilla wax, beeswax, rice bran wax and monoglyceride, wherein the monoglyceride is at least one of monostearate glyceryl, monolaurate glyceryl and monopalmitate glyceryl.
[0015] The emulsifier is at least one of glyceryl stearate, polyglyceryl ricinoleate, lecithin and stearic acid.
[0016] The fat-soluble active substances include but are not limited to at least one of quercetin, orange peel flavonoids, curcumin, resveratrol, lycopene, and β-carotene, and the hydrophilic active substances include but are not limited to at least one of ferulic acid, gallic acid, catechins, and anthocyanins.
[0017] A method for preparing the above-mentioned 3D printed dual gel capable of loading fat-soluble and water-soluble active substances comprises the following steps:
[0018] (1) Preparation of the oil gel mixture: adding the oil gelling agent and the emulsifier to the vegetable oil, heating and stirring to dissolve, obtaining the oil gel mixture, and keeping it warm for later use;
[0019] (2) Preparation of a hydrogel mixture: adding a hydrogel agent to water, heating and stirring to dissolve, obtaining a hydrogel mixture, and keeping the mixture warm for later use;
[0020] (3) adding a fat-soluble active substance to the oil gel mixture obtained in step (1), heating and stirring until dissolved, and setting aside; at the same time, adding a hydrophilic active substance to the hydrogel mixture obtained in step (2), heating and stirring until dissolved, and setting aside;
[0021] (4) preparing a 3D printed dual gel capable of loading fat-soluble and water-soluble active substances: homogenizing the oil gel mixture containing the oil-soluble active substance and the hydrogel mixture containing the hydrophilic active substance obtained in step (3), and then cooling and solidifying to obtain a dual gel;
[0022] (5) 3D printing: The above-mentioned dual gel is added into a 3D printer for printing, thereby obtaining a 3D printed dual gel capable of delivering active substances.
[0023] The amount of the oil gel in step (1) is preferably 1% to 6% by weight of the oil gel mixture, preferably 3% to 6%.
[0024] The heating temperature in step (1) is maintained at 85-120° C., the heating time is 1-3 hours, and the stirring speed is 200 rpm-600 rpm.
[0025] The heating temperature in step (2) is 50-95° C. and the heating time is 40-70 min. The next step can be performed only after all the hydrogel is fully dissolved.
[0026] The temperature of heating and stirring when adding the fat-soluble active substance in step (3) is 85-95°C; the temperature of heating and stirring when adding the hydrophilic active substance in step (3) is 50-60°C.
[0027] The homogenizing speed in step (4) is 9000 rpm to 12000 rpm, the homogenizing time is 1 to 5 min, and the homogenizing temperature is 15 to 30° C., preferably 20 to 25° C.
[0028] The double gel in step (4) is stored at 0-10°C, preferably 4°C.
[0029] In the 3D printing process described in step (5), the printing speed is 50-90 mm / s, the extrusion speed is 100-170 mm / s, and the printing material temperature is 15-30°C, preferably 20-25°C.
[0030] The above-mentioned 3D printed dual gel capable of loading fat-soluble and water-soluble active substances is used in 3D printed fat substitutes and functional foods.
[0031] Compared with the prior art, the present invention has the following advantages and beneficial effects:
[0032] The present invention uses an oleogel to gel the liquid vegetable oil, uses a hydrogel to fix water molecules to form a hydrogel, adds an embedded active substance when preparing the oleogel and the hydrogel, and then forms a uniform double gel by stirring and homogenizing. Different types of double gels can be obtained by mixing in different proportions. While delivering active substances, it can also meet the requirements of being used as a 3D printing material.
[0033] The 3D printing double gel of the present invention, which can load fat-soluble and water-soluble active substances, requires few types of gelling agents, has a simple preparation method and low cost, and has stable active substances and good printing properties in the 3D printing double gel, which is suitable for large-scale production. The prepared double gel has low calories, is green and safe, and has good properties of replacing saturated fatty acids. Fat-soluble or water-soluble nutrients or functional active substances are subsequently added to develop 3D printing functional nutritional foods with rich nutritional functionality to meet the personalized nutritional needs of consumers. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Figure 1 This is a picture of the double gel effect of 3D printed food obtained in Example 1.
[0035] Figure 2 This is a double gel microscope image of the 3D printed food obtained in Example 1.
[0036] Figure 3 This is the 3D printed food double gel effect diagram obtained in Example 2.
[0037] Figure 4 This is a double gel microscope image of the 3D printed food obtained in Example 2.
[0038] Figure 5 This is the double gel effect diagram of 3D printed food obtained in Example 3.
[0039] Figure 6 This is a double gel microscope image of the 3D printed food obtained in Example 3.
[0040] Figure 7 This is the 3D printed food double gel effect diagram obtained in Example 4.
[0041] Figure 8 This is a double gel microscope image of the 3D printed food obtained in Example 4.
[0042] Fig. 9 This is the 3D printed food double gel effect diagram obtained in Comparative Example 1.
[0043] Fig.10 This is the appearance of the double gel obtained in Comparative Example 2.
[0044] Fig.11 This is the appearance of the double gel obtained in Comparative Example 3.
[0045] Fig.12 This is the appearance of the double gel obtained in Comparative Example 4.
[0046] Fig.13 This is the appearance of the double gel obtained in Comparative Example 5.
[0047] Fig.14 This is the appearance of the double gel obtained in Comparative Example 6. DETAILED DESCRIPTION
[0048] The present invention is further described in detail below in conjunction with the examples and drawings, but the embodiments of the present invention are not limited thereto. If specific conditions are not specified in the examples, they are carried out according to conventional conditions or conditions recommended by the manufacturer. If the manufacturer of the reagents or instruments used is not specified, they are all conventional products that can be purchased commercially.
[0049] Unless otherwise specified, the reagents used in the examples can be purchased from the market.
[0050] The contents of each component used in Examples 1-4 and Comparative Examples 1-6 are expressed as a percentage by mass of the final dual gel.
[0051] Example 1
[0052] 1) Preparation of oil gel mixture: 33.56% high oleic sunflower oil, 0.35% stearyl glyceride, and 1.05% candelilla wax were weighed, and dissolved by stirring at 90° C. for 90 min at a speed of 300 rpm to obtain an oil gel mixture, which was kept warm for later use.
[0053] 2) Preparation of hydrogel mixture: 3.25% gelatin and 61.69% deionized water were taken at room temperature, stirred and dissolved at 60° C. for 60 min, with a rotation speed of 220 rpm, and stirred and mixed evenly to obtain a hydrogel mixture, which was kept warm for later use.
[0054] 3) Adding active substances: Weigh 0.03% quercetin, add it to the oil gel, continue heating and stirring at 90° C. until it is completely dissolved; weigh 0.07% catechin, add it to the hydrogel, continue heating and stirring at 60° C. until it is completely dissolved, and keep the stirring speed unchanged.
[0055] 4) The oil gel mixture and the hydrogel mixture to which the active substance has been added are homogeneously mixed at room temperature at a rotation speed of 10000 rpm for 1 min to obtain a uniform oil hydrogel mixture.
[0056] 5) The oil-water gel mixture obtained in the previous step is placed at 4° C. for cooling and storage to obtain a double gel encapsulating the active substance.
[0057] 6) Add the above-mentioned dual gel into a 3D printer, adjust the printing speed to 50 mm / s, the extrusion speed to 100 mm / s, the printing material temperature to 25° C., and print to obtain a 3D printed dual gel that can load fat-soluble and water-soluble active substances.
[0058] Figure 1 and Figure 2They are the 3D printed food double gel effect picture and microscope picture obtained in Example 1. It can be seen from the picture that under this condition, the double gel has good printing characteristics and can form a uniform and stable double gel structure.
[0059] Example 2
[0060] 1) Preparation of oil gel mixture: Weigh 62.33% rapeseed oil, 0.65% lecithin, and 1.95% beeswax, stir and dissolve them at 100° C. for 150 min at a speed of 300 rpm to obtain an oil gel mixture, and keep it warm for use.
[0061] 2) Preparation of hydrogel mixture: 1.75% pectin and 33.21% deionized water were taken at room temperature, stirred and dissolved at 70° C. for 60 min, with a rotation speed of 220 rpm, and stirred and mixed evenly to obtain a hydrogel mixture, which was kept warm for later use.
[0062] 3) Adding active substances: Weigh 0.07% resveratrol, add it to the oil gel, continue heating at 85° C. and stirring until it is completely dissolved; weigh 0.04% gallic acid, add it to the hydrogel, continue heating at 55° C. and stirring until it is completely dissolved, with the stirring speed unchanged.
[0063] 4) The oil gel mixture and the hydrogel mixture to which the active substance has been added are mixed and homogenized at room temperature at a rotation speed of 9000 rpm for 5 minutes to obtain a uniform oil-hydrogel mixture.
[0064] 5) The oil-water gel mixture obtained in the previous step is placed at 0° C. for cooling and storage to obtain a double gel encapsulating the active substance.
[0065] 6) Add the above-mentioned dual gel into a 3D printer, adjust the printing speed to 90 mm / s, the extrusion speed to 170 mm / s, the printing material temperature to 25° C., and print to obtain a 3D printed dual gel that can load fat-soluble and water-soluble active substances.
[0066] Figure 3 and Figure 4 They are the 3D printed food double gel effect picture and microscope picture obtained in Example 2. It can be seen from the picture that under this condition, the double gel has good printing characteristics and can form a uniform and stable double gel structure.
[0067] Example 3
[0068] 1) Preparation of oil gel mixture: Weigh 47.95% soybean oil, 0.50% glyceryl monostearate, and 1.50% stearic acid, and dissolve them by stirring at 85° C. for 90 min at a speed of 300 rpm to obtain an oil gel mixture, which is kept warm for later use.
[0069] 2) Preparation of hydrogel mixture: 2.50% konjac gum and 47.45% deionized water were added at room temperature, stirred and dissolved at 50° C. for 60 min, with a rotation speed of 220 rpm, and the mixture was stirred and mixed evenly to obtain a hydrogel mixture, which was kept warm for use.
[0070] 3) Adding active substances: Weigh 0.05% of curcumin, add it to the oil gel, continue heating and stirring at 85° C. until it is completely dissolved; weigh 0.05% of anthocyanidin, add it to the hydrogel, continue heating and stirring at 50° C. until it is completely dissolved, and keep the stirring speed unchanged.
[0071] 4) The oil gel mixture and the hydrogel mixture to which the active substance has been added are mixed and homogenized at room temperature at a rotation speed of 12000 rpm for 1 min to obtain a uniform oil-hydrogel mixture.
[0072] 5) The oil-water gel mixture obtained in the previous step is placed at 6° C. for cooling and storage to obtain a double gel encapsulating the active substance.
[0073] 6) Add the above-mentioned dual gel into a 3D printer, adjust the printing speed to 70 mm / s, the extrusion speed to 130 mm / s, the printing material temperature to 30° C., and print to obtain a 3D printed dual gel that can load fat-soluble and water-soluble active substances.
[0074] Figure 5 and Figure 6 They are the 3D printed food double gel effect picture and microscope picture obtained in Example 3. It can be seen from the picture that under this condition, the double gel has good printing characteristics and can form a uniform and stable double gel structure.
[0075] Example 4
[0076] 1) Preparation of oil gel mixture: Weigh 28.77% peanut oil, 0.30% polyglycerol castoryl ester, and 0.9% rice bran wax, stir and dissolve them at 120° C. for 90 min at a speed of 300 rpm to obtain an oil gel mixture, and keep it warm for use.
[0077] 2) Preparation of hydrogel mixture: 3.50% guar gum and 66.43% deionized water were added at room temperature, stirred and dissolved at 95° C. for 60 min at a speed of 220 rpm, and the mixture was stirred and mixed evenly to obtain a hydrogel mixture, which was kept warm for later use.
[0078] 3) Adding active substances: Weigh 0.03% lycopene, add it to the oil gel, continue heating at 85° C. and stirring until it is completely dissolved; weigh 0.07% ferulic acid, add it to the hydrogel, continue heating at 50° C. and stirring until it is completely dissolved, with the stirring speed unchanged.
[0079] 4) The oil gel mixture and the hydrogel mixture to which the active substance has been added are mixed and homogenized at room temperature at a rotation speed of 11000 rpm for 3 minutes to obtain a uniform oil hydrogel mixture.
[0080] 5) The oil-water gel mixture obtained in the previous step is placed at 4° C. for cooling and storage to obtain a double gel encapsulating the active substance.
[0081] 6) Add the above-mentioned dual gel into a 3D printer, adjust the printing speed to 80 mm / s, the extrusion speed to 160 mm / s, the printing material temperature to 15° C., and print to obtain a 3D printed dual gel that can load fat-soluble and water-soluble active substances.
[0082] Figure 7 and Figure 8 They are the 3D printed food double gel effect picture and microscope picture obtained in Example 4. It can be seen from the picture that under this condition, the double gel has good printing characteristics and can form a uniform and stable double gel structure.
[0083] Comparative Example 1
[0084] The steps and conditions of Example 1 are referred to, except that the printing speed is adjusted to 100 mm / s and the extrusion speed is adjusted to 30 mm / s in step 6. Under the comparative conditions, the printed double gel pattern has poor effect.
[0085] Fig. 9 This is the 3D printed double gel obtained in Comparative Example 1. Under this condition, the printed double gel cannot maintain the 3D printed three-dimensional structure well, and the graphic effect is poor.
[0086] Comparative Example 2
[0087] Referring to the steps and conditions of Example 2, the difference is that in step 1), rapeseed oil is 91.10%, lecithin is 0.95%, and beeswax is 2.85%; in step 2), pectin is 0.24%, and deionized water is 4.75%. Under these comparative conditions, the formed double gel cannot maintain a solid structure well and is not suitable for 3D printing.
[0088] Fig.10 This is the 3D printing double gel obtained in Comparative Example 2. At this ratio, the prepared double gel has poor stability. After the sample is inverted, some sagging will occur. Such flow characteristics of the sample will cause the 3D printed pattern to collapse, and it is not suitable for 3D printing.
[0089] Comparative Example 3
[0090] The steps and conditions of Reference Example 3 are different in that in step 1), soybean oil is 4.79%, monoglyceride is 0.05%, stearic acid is 0.15%, and in step 2), konjac gum is 7.6%, and deionized water is 87.31%. Under these comparative conditions, the printed double gel graphics have poor effect.
[0091] Fig.11 This is the 3D printing double gel obtained in Comparative Example 3. Under this ratio, the prepared double gel has poor stability. After the sample is inverted, it will sag. Such flow characteristics of the sample will cause the 3D printed pattern to collapse, and it is not suitable for 3D printing.
[0092] Comparative Example 4
[0093] Referring to the steps and conditions of Example 1, the difference is that whey protein is used as the hydrogel in step 2. Under this comparative condition, a stable double gel cannot be formed.
[0094] Fig.12 This is the double gel obtained in Comparative Example 4. Under this condition, the double gel prepared has poor stability, stratification, poor sample uniformity, and is not suitable for 3D printing.
[0095] Comparative Example 5
[0096] Referring to the steps and conditions of Example 1, the difference is that carrageenan is used as the hydrogel in step 2), and under this comparative condition, a stable double gel cannot be formed.
[0097] Fig.13 This is the double gel obtained in Comparative Example 5. Under this condition, the double gel prepared has poor stability, stratification, poor sample uniformity, and is not suitable for 3D printing.
[0098] Comparative Example 6
[0099] Referring to the steps and conditions of Example 2, the difference is that in step 1), the content of beeswax is 16%, in step 2), carrageenan is used as the hydrogel, and the content of deionized water is 18.86%. Under this comparative condition, a stable double gel cannot be formed.
[0100] Fig.14 This is the double gel obtained in Comparative Example 6. Under this ratio, the prepared double gel has poor stability. After the sample is inverted, it will sag. Such flow characteristics of the sample will cause the 3D printed pattern to collapse, and it is not suitable for 3D printing.
[0101] The above embodiments are preferred implementation modes of the present invention, but the implementation modes of the present invention are not limited to the above embodiments. Any other changes, modifications, substitutions, combinations, and simplifications that do not deviate from the spirit and principles of the present invention should be equivalent replacement methods and are included in the protection scope of the present invention.
Claims
1. A 3D printed double gel capable of loading fat-soluble and water-soluble active substances, characterized in that The raw materials include the following components in weight percentage: vegetable oil 28.77% to 33.56%, drinking water 61.69% to 66.43%, hydrogel 1.75% to 3.5%, oil gel 0.5% to 1.95%, emulsifier 0.3% to 1.5%, water-soluble active substance 0.04% to 0.07%, fat-soluble active substance 0.03% to 0.07%; The emulsifier is at least one of glyceryl stearate, polyglyceryl ricinoleate, lecithin, and stearic acid; The hydrogel is one of gelatin, pectin, konjac gum, and guar gum; The oil gel is at least one of candelilla wax, beeswax, rice bran wax, and monoglyceride; The fat-soluble active substance is at least one of quercetin, curcumin, resveratrol, and lycopene, and the hydrophilic active substance is at least one of ferulic acid, gallic acid, catechin, and anthocyanidin; The 3D printed double gel capable of loading fat-soluble and water-soluble active substances is prepared by the following method: (1) Preparation of the oil gel mixture: adding the oil gelling agent and the emulsifier to the vegetable oil, heating and stirring to dissolve, obtaining the oil gel mixture, and keeping it warm for later use; (2) Preparation of a hydrogel mixture: adding a hydrogel agent to water, heating and stirring to dissolve, obtaining a hydrogel mixture, and keeping the mixture warm for later use; (3) adding a fat-soluble active substance to the oil gel mixture obtained in step (1), heating and stirring until dissolved, and setting aside; at the same time, adding a hydrophilic active substance to the hydrogel mixture obtained in step (2), heating and stirring until dissolved, and setting aside; (4) preparing a 3D printed dual gel capable of loading fat-soluble and water-soluble active substances: homogenizing the oil gel mixture containing the oil-soluble active substance and the hydrogel mixture containing the hydrophilic active substance obtained in step (3), and then cooling and solidifying to obtain a dual gel; (5) 3D printing: adding the above-mentioned dual gel into a 3D printer for printing, thereby obtaining a 3D printed dual gel capable of delivering active substances; The homogenization temperature in step (4) is 15-30°C.
2. The 3D printed dual gel capable of loading fat-soluble and water-soluble active substances according to claim 1, characterized in that: The vegetable oil is at least one of rapeseed oil, soybean oil, sunflower oil, peanut oil, olive oil and corn oil.
3. The 3D printed dual gel capable of loading fat-soluble and water-soluble active substances according to claim 1, characterized in that: The amount of the oil gel in step (1) is 1% to 6% by weight of the oil gel mixture.
4. The 3D printed dual gel capable of loading fat-soluble and water-soluble active substances according to claim 1, characterized in that: In the 3D printing process described in step (5), the printing speed is 50-90 mm / s and the extrusion speed is 100-170 mm / s.
5. Application of the 3D printed double gel capable of loading fat-soluble and water-soluble active substances according to any one of claims 1-2 in 3D printed fat substitutes and functional foods.
Citation Information
Cited By
Supramolecular co-melt adhesive, preparation and application thereof, pigment-loaded supramolecular co-melt adhesive and application of pigment-loaded supramolecular co-melt adhesive
CN120349573A