A waterproof, highly wear-resistant leather material with special light perception and a preparation method thereof

By embedding and fixing reflective particles in the pores of animal leather, and using thermoplastic or thermosetting adhesives to improve the wear resistance and waterproofness of the leather, the problem in the existing technology of the decline in texture of leather materials when increasing performance is solved, and high-quality materials are achieved. Wear-resistant, waterproof and special light effect, while maintaining the original beauty of the leather.

CN115704054BActive Publication Date: 2024-10-18叶小晔
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202110912950.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-08-10
Publication Date
2024-10-18
Estimated Expiration
2041-08-10

AI Technical Summary

Technical Problem

While existing leather materials increase wear resistance, waterproofness and special gloss, they often affect the texture of the leather, and the preparation process is complex and costly.

Method used

Animal leather with pores is used, and reflective particles whose particle size matches the pores are embedded in the pores. The particles are fixed on the leather surface using a thermoplastic or thermosetting adhesive, and the adhesive is cured by heating to improve the wear resistance and waterproofing of the leather. properties while maintaining the texture of leather.

Benefits of technology

The wear resistance and waterproofness of the leather are improved, while the texture of the leather is maintained, the aesthetics and performance of the leather are enhanced, and the prejudice of pore treatment in the existing technology is overcome.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115704054B_ABST
    Figure CN115704054B_ABST
Patent Text Reader

Abstract

The present invention relates to a waterproof, highly wear-resistant leather material with special light perception and a preparation method thereof, the method comprising the following steps: (1) selecting leather with pores; (2) spreading adhesive powder on the leather to allow the adhesive powder to enter the pores; (3) spreading reflective particles of different particle sizes on the leather in descending order and pressing them into the pores; (4) heating the leather to obtain waterproof, highly wear-resistant leather with special light perception. Compared with the prior art, the present invention has the advantages of increasing the wear resistance, waterproofness and special light perception of the leather without affecting the texture of the leather itself.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of leather, and in particular to a waterproof, highly wear-resistant leather material with special light perception and a preparation method thereof. Background Art

[0002] At present, animal leather becomes common leather on the market after a series of processing steps from raw hide to cooked hide. This kind of leather only has its own biological characteristics and structure.

[0003] If you want to obtain leather with different properties, you often add a composite layer or coating to the leather to get different effects, but the leather with the composite layer or coating loses the texture of the leather itself.

[0004] For example, Chinese patent CN108359754A discloses a new type of adjustable luminous leather, including conductive leather and luminescent material, the luminescent material is arranged on the surface of the conductive leather, and the luminescent material is an electroluminescent material. The leather will emit light under external stimulation. This new property expands the application of leather in the electronic field, such as display, lighting, sensing, wearable electronic devices, etc. However, the preparation process is too complicated, and the cost of raw materials is extremely high. The complicated process is bound to have an adverse effect on the texture of the leather itself. Summary of the invention

[0005] The purpose of the present invention is to overcome the defects of the above-mentioned prior art and provide a leather material containing reflective particles and a preparation method thereof that increases the wear resistance, water resistance and special light perception of the leather without affecting the texture of the leather itself.

[0006] The purpose of the present invention can be achieved by the following technical solutions:

[0007] A waterproof, highly wear-resistant leather material with special light perception comprises leather with pores and reflective particles embedded in the pores and having a particle size matching the size of the pores.

[0008] Furthermore, the leather comprises animal leather.

[0009] Furthermore, the particle size of the reflective particles is 200-600 meshes.

[0010] Furthermore, the reflective particles include metals, minerals or gemstones.

[0011] Furthermore, the metal includes tungsten, gold, silver, copper, palladium or aluminum.

[0012] Furthermore, the material also includes an adhesive for bonding the reflective particles in the pores.

[0013] Further, the adhesive comprises a thermoplastic adhesive or a thermosetting adhesive;

[0014] The thermoplastic adhesive comprises EVA resin; the thermosetting adhesive comprises thermosetting phenolic resin raw material.

[0015] A method for preparing the waterproof, highly wear-resistant leather material with special light perception as described above, the method comprising the following steps:

[0016] (1) Select leather with pores;

[0017] (2) Sprinkle the adhesive powder on the leather and gently roll it to allow the adhesive powder to enter the pores, then sweep away the excess powder on the surface;

[0018] (3) Spread reflective particles whose particle sizes match the pore sizes on the leather in descending order of particle size and press them into the pores;

[0019] (4) After the powder floating on the surface is cleaned, the leather is heated for a period of time to obtain a leather material that is waterproof, highly wear-resistant and has a special light sensation.

[0020] The invention utilizes the biological characteristics and structure of animal leather itself, and tans metal or mineral powder of appropriate size into the pores on the leather surface, so that the leather has different effects of its own.

[0021] Animal leather itself has pores and textures, and it also has a certain degree of stretch or elasticity. Different metals or minerals also have different properties. For example, diamond, commonly known as diamond, is the hardest substance in nature. At the same time, diamond has a very high refractive index and strong dispersion performance. The characteristics of diamond determine its uniqueness. Even a powder as small as 600 mesh (23μm) can still sparkle.

[0022] The present invention uses heated resin powder as an adhesive to fix metal or mineral powder in the pores of leather without it falling off at will. The selected phenolic resin powder has high temperature resistance and can maintain the integrity and dimensional stability of its structure at higher temperatures. Phenolic resin is a multifunctional substance that is compatible with various organic and inorganic fillers, so it can be used as a refractory material, friction material and adhesive. Due to its above characteristics, the phenolic resin powder is pressed into the pores of the leather, and then the metal or mineral powder is pressed into it, and heated in a heating box for a few seconds. After the phenolic resin powder is thermoset and cooled, the metal or mineral powder can be well fixed therein without being easy to fall off.

[0023] Furthermore, the leather comprises animal leather.

[0024] Furthermore, the adhesive includes a thermoplastic adhesive or a thermosetting adhesive.

[0025] Furthermore, the thermoplastic adhesive includes EVA resin; and the thermosetting adhesive includes thermosetting phenolic resin raw material.

[0026] The so-called thermosetting phenolic resin raw material is a mixture of phenolic resin powder and 6-10% hexamethylenetetramine.

[0027] Furthermore, the heating temperature is 90-160°C.

[0028] Furthermore, the particle size of the reflective particles is 200-600 meshes.

[0029] Furthermore, the reflective particles include metals, minerals or gemstones.

[0030] Furthermore, the metal includes tungsten, gold, silver, copper, palladium or aluminum, or an alloy, and the gemstone includes diamond, crystal, sapphire, etc.

[0031] Furthermore, the specific operation of step (3) is:

[0032] (3-1) Spread the reflective particles with the largest particle size on the leather and press them into the pores;

[0033] (3-2) Spreading reflective particles with a particle size second only to that of the particles in step (3-1) on the leather and pressing them into the pores;

[0034] (3-3) The reflective particles are sequentially processed in order of particle size from large to small as in step (3-1) until the reflective particles with the smallest particle size are pressed into the pores.

[0035] Furthermore, the heating temperature is 90-160° C. and the heating time is 5-10 seconds.

[0036] Compared with the prior art, the present invention has the following advantages:

[0037] (1) In the present invention, since the pores on the leather surface are filled with hard metal or mineral powder, and the wear resistance of the adhesive is much higher than that of the leather surface layer, the density of the leather surface layer is improved, the hardness is increased, the surface roughness value is reduced, the fatigue wear resistance is increased, and the wear resistance of the leather surface is increased;

[0038] (2) In the present invention, the waterproofness of the leather is related to the tissue structure of the raw leather. Since the pores on the leather surface are filled with reflective particles and adhesive, the leather surface becomes tight and the water-permeable pores become less, thereby improving the waterproofness of the leather;

[0039] (3) In the present invention, the original pores of the leather are filled without losing the texture of the leather itself. At the same time, some sparkling spots can be vaguely seen on the surface of the leather. The effect of this sparkle will vary depending on the metal or mineral powder filled in.

[0040] (4) The pores on the leather are often avoided in the prior art. In many technologies using leather, a set of special processes will be used to remove the pores first to avoid affecting the aesthetics. However, the present invention takes the opposite approach and utilizes the pores that are discarded by the prior art, which not only improves the aesthetics, but also improves the performance of the leather and overcomes technical prejudice. BRIEF DESCRIPTION OF THE DRAWINGS

[0041] Figure 1 This is a photo of the leather material in Example 1. DETAILED DESCRIPTION

[0042] The present invention is described in detail below in conjunction with the accompanying drawings and specific embodiments. This embodiment is implemented based on the technical solution of the present invention, and provides a detailed implementation method and specific operation process, but the protection scope of the present invention is not limited to the following embodiments.

[0043] A method for preparing waterproof, highly wear-resistant leather with special light sensation, the method comprising the following steps:

[0044] (1) Selecting leather with pores; wherein the leather includes animal leather;

[0045] (2) Sprinkle the adhesive powder on the leather, and gently roll it to make the adhesive powder enter the pores, and then sweep away the excess powder on the surface; wherein the adhesive includes a thermoplastic adhesive or a thermosetting adhesive. Thermoplastic adhesives include EVA resins; thermosetting adhesives include thermosetting phenolic resin raw materials; the so-called thermosetting phenolic resin raw materials are a mixture of phenolic resin powder and 6-10% hexamethylenetetramine;

[0046] Thermoplastic adhesives also include polyethylene (PE), melting point 85-110°C or polyaldehyde resin, melting point 88-108°C. It may also be polypropylene, melting point 189°C, softening at around 155°C, and the operating temperature range is -30 to 140°C.

[0047] Thermosetting adhesives also include:

[0048] Melamine formaldehyde resin

[0049] Physical properties: The cured melamine formaldehyde resin is colorless and transparent, stable in boiling water, and can even be used at 150°C. It has self-extinguishing properties, arc resistance, and good mechanical properties. Melamine resin is the abbreviation.

[0050] Chemical properties: The raw materials are melamine (2,4,6-triamino-1,3,5-triazine) and 37% formaldehyde aqueous solution. The molar ratio of formaldehyde to melamine is 2-3. In the first step, different numbers of N-hydroxymethyl substituents are generated, and then further condensed into linear resins. The molecular weight of the product varies with the reaction conditions, ranging from water-soluble to insoluble in water, or even insoluble and infusible solids. The pH value has a great influence on the reaction rate. The resin solution obtained by the above reaction is not suitable for storage. In industry, spray drying is commonly used to make powdered solids. Melamine resin does not cure at room temperature, and is generally cured at 130-150°C. Adding a small amount of acid catalyst can increase the curing speed.

[0051] Or polymethyl methacrylate (PMMA), a high molecular polymer, also known as acrylic or organic glass, with a melting point of 150°C and a glass transition temperature of PMMA of about 105°C;

[0052] (3) Spread reflective particles of different sizes on the leather in descending order and press them into the pores; wherein the reflective particles have a particle size of 200-600 mesh, and the reflective particles include metals, ores or gems. Specifically, the reflective particles are metals (including alloys), ores (including artificial ores, such as artificial diamonds, artificial crystals, etc.), gems (including artificial gems), and jade.

[0053] Reflective particle size: The leather used in the examples is fetal cowhide, that is, the skin of calves born 1-30 days ago, which is the best layer of cowhide, with smooth skin, moderate thickness, and clear tread. However, the pore sizes of leathers from different animals, different varieties of leathers of the same species, and leathers of the same variety grown in different environments or at different growth times may vary greatly. Therefore, if different leathers are used, the range of reflective particle sizes may be larger, and particles larger than 200 mesh may be used;

[0054] (3-1) Sprinkle reflective particles of the largest size (about 200 mesh) on the leather and press them into the pores;

[0055] (3-2) Spreading reflective particles with a particle size second only to that of the particles in step (3-1) on the leather and pressing them into the pores;

[0056] (3-3) The reflective particles are sequentially subjected to the operation of step (3-1) in order of particle size from large to small, until the reflective particles with the smallest particle size (about 600 mesh) are pressed into the pores;

[0057] (4) After the powder floating on the surface is cleaned, the leather is heated at 90-160° C. for 5-10 seconds to obtain waterproof, highly wear-resistant leather with a special glossiness.

[0058] Since the performance of different types of leather and different parts of leather may vary, the leather selected before the implementation of the following embodiments is the middle part of the back of the same whole piece of leather, so as to minimize the difference caused by the selected original leather in subsequent tests.

[0059] The dynamic waterproof performance of the material is tested using the "MAESER Leather Dynamic Waterproof Tester" in accordance with the ASTMD2099-2014 standard. Cut the test piece, install it on the tester, and apply flexure under water to measure the material's penetration resistance index. During the test, as long as the material is penetrated by water, the counting will automatically stop and display the number of times. Under the same conditions and the same flexure frequency, the more times the tester counts, the better the dynamic waterproof performance of the test sample.

[0060] The method for measuring wear resistance is to weigh the leather to 4 decimal places, fix it on the wear tester, and scrape it a certain number of times under the same conditions. The weight after scraping is calculated to calculate the wear rate. The wear resistance of a material is often expressed as the wear rate G, and its calculation formula is:

[0061] G=(m1-m2) / A,

[0062] Where G is the wear rate of the material, g / cm 2 ;

[0063] m1, m2——mass of material before and after wear, g;

[0064] A——wear area of ​​material specimen, cm 2 .

[0065] The lower the wear rate G value of the material, the better the wear resistance of the material.

[0066] Example 1

[0067] A method for preparing waterproof, highly wear-resistant leather with special light sensation, the method comprising the following steps:

[0068] S1. Select leather (original leather) with obvious animal pores.

[0069] S2. Spread a thin layer of phenolic resin powder + 6-10% hexamethylenetetramine (thermosetting phenolic resin raw material) and gently roll it. After the phenolic resin powder enters the pores and is compacted, sweep away the excess phenolic resin powder on the leather surface.

[0070] S3, spread a thin layer of diamond powder of about 200 mesh, and then gently roll it. At this time, the diamond powder of about 200 mesh will be pressed into the larger pores, and the excess powder will be swept away. According to the above steps, press in 300 mesh, 400 mesh, 500 mesh, and 600 mesh diamond powder in turn.

[0071] S4. After cleaning the powder floating on the leather surface, put the leather into a heating box at a temperature of about 150°C. After a few seconds, the leather can be taken out. In this way, the leather containing diamond powder is completed. Figure 1 .

[0072] Example 2

[0073] A method for preparing waterproof, highly wear-resistant leather with special light sensation, the method comprising the following steps:

[0074] S1. Select leather (original leather) with obvious animal pores.

[0075] S2. Spread a thin layer of ethylene-vinyl acetate copolymer powder (EVA resin) and gently roll it. After the EVA resin powder enters the pores and is compacted, sweep away the excess EVA powder on the leather surface.

[0076] S3, spread a thin layer of 200 mesh tungsten gold powder, and then gently roll it. At this time, the 200 mesh tungsten gold powder will be pressed into the larger pores, and the excess powder will be swept away. According to the above steps, press in 300 mesh, 400 mesh, 500 mesh, and 600 mesh tungsten gold powder in turn.

[0077] S4. After cleaning the powder floating on the leather surface, put the leather into a heating box at a temperature of about 100°C. After a few seconds, the leather can be taken out. In this way, the leather containing tungsten gold powder is completed.

[0078] Comparative Example

[0079] This comparative example is a raw hide that is the same as that in Example 1-2.

[0080] Test Examples 1-2 and Comparative Example 1 (original leather) were tested for wear resistance and dynamic waterproof performance. The results are shown in Table 1.

[0081] Table 1 Wear rate G, dynamic waterproofing (times)

[0082] Comparative Example Example 1 Example 2 <![CDATA[Leather abrasion resistance test (g / cm 2 )]]> 0.0075 0.0043 0.0049 Leather dynamic waterproof test (times) 2526 5255 6158

[0083] As can be seen from the table above, since the pores on the leather surface are filled with hard metal or mineral powder, and the wear resistance of the adhesive is much higher than that of the leather surface, the density of the leather surface layer is improved, the hardness is increased, the surface roughness value is reduced, and the fatigue wear resistance is increased, thereby increasing the wear resistance of the leather surface. Since the pores on the leather surface are filled with reflective particles and adhesives, the leather surface becomes compact and the water-permeable pores are reduced, thereby improving the waterproofness of the leather.

[0084] The above is only a preferred embodiment of the present invention, and does not limit the present invention in other forms. Any technician familiar with the profession may use the above disclosed technical content to change or modify it into an equivalent embodiment with equivalent changes. However, any simple modification, equivalent change and modification made to the above embodiment according to the technical essence of the present invention without departing from the technical solution of the present invention still belongs to the protection scope of the technical solution of the present invention.

Claims

1. A method for preparing a waterproof, highly wear-resistant leather material with special light perception, characterized in that: The material includes leather with pores, and reflective particles embedded in the pores and having a particle size matching the size of the pores; The preparation method comprises the following steps: (1) Select leather with pores; (2) Sprinkle the adhesive powder on the leather so that the adhesive powder enters the pores; (3) Spread reflective particles whose particle sizes match the pore sizes on the leather in descending order of particle size and press them into the pores; (4) After heating the leather, a leather material that is waterproof, highly wear-resistant and has a special light feel can be obtained; The specific operations of step (3) are: (3-1) Spread the largest reflective particles on the leather and press them into the pores; (3-2) Spreading reflective particles with a particle size second only to that of the particles in step (3-1) on the leather and pressing them into the pores; (3-3) The reflective particles are sequentially placed in order of particle size from large to small, and the operation is performed as in step (3-1) until the reflective particles with the smallest particle size are pressed into the pores.

2. The method for preparing a waterproof, highly wear-resistant leather material with special light perception according to claim 1, characterized in that: The leather includes animal leather.

3. The method for preparing a waterproof, highly wear-resistant leather material with special light perception according to claim 1, characterized in that: The particle size of the reflective particles is 200-600 meshes.

4. The method for preparing a waterproof, highly wear-resistant leather material with special light perception according to claim 1, characterized in that: The reflective particles include metals and minerals.

5. The method for preparing a waterproof, highly wear-resistant leather material with special light perception according to claim 4, characterized in that: The metal includes tungsten, gold, silver, copper, palladium or aluminum.

6. The method for preparing a waterproof, highly wear-resistant leather material with special light perception according to claim 1, characterized in that: The adhesive powder includes a thermoplastic adhesive or a thermosetting adhesive; The thermoplastic adhesive comprises EVA resin; the thermosetting adhesive comprises thermosetting phenolic resin raw material.

7. The method for preparing a waterproof, highly wear-resistant leather material with special light perception according to claim 1, characterized in that: The heating temperature is 90-160° C. and the heating time is 5-10 seconds.

Citation Information

Patent Citations

  • Novel adjustable lighting leather

    CN108359754A

  • Aqueous leather finishing material and preparation method thereof

    CN111320904A