Semiconductor manufacturing apparatus, semiconductor device, and method for manufacturing semiconductor device
By using an ion implantation device to switch between ionic and neutral component implantation modes in semiconductor manufacturing, the problem of crystallization defects in the impurity diffusion layer was solved, enabling the efficient formation of impurity layers with fewer crystallization defects, thereby improving production efficiency and reducing costs.
Patent Information
- Application Number
- CN202210166664.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2021-08-26
- Filing Date
- 2022-02-23
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2042-02-23
AI Technical Summary
Existing technologies struggle to effectively control crystallization defects in the impurity diffusion layer during semiconductor manufacturing, leading to increased leakage current and low production efficiency.
An ion implantation device is used to switch the implantation modes of ionic and neutral components in the same chamber. An energy filter is used to separate the ionic and neutral components and implant them into the semiconductor substrate with different energies and directions to form impurity layers of different depths and concentrations.
This method enables the formation of multiple impurity layers with fewer crystal defects in a single ion implantation step, improving production efficiency, reducing leakage current, and lowering production costs.
Smart Images

Figure CN115732299B_ABST
Abstract
Description
[0001] [References to related applications]
[0002] This application enjoys priority to Japanese Patent Application No. 2021-138315 (filed on August 26, 2021). This application incorporates the entire contents of the basic application by reference to that basic application. Technical Field
[0003] This embodiment relates to a semiconductor manufacturing apparatus, a semiconductor device, and a method for manufacturing a semiconductor device. Background Technology
[0004] With the miniaturization of semiconductor devices, high-precision control of the impurity diffusion layer is required. For example, when the source or drain layer of a transistor is composed of a single impurity diffusion layer, crystal defects can easily remain in the impurity diffusion layer, leading to increased leakage current. When the source or drain layer is composed of multiple impurity diffusion layers, multiple ion implantation steps need to be repeatedly performed under different conditions. This results in a decrease in yield. Summary of the Invention
[0005] The problem to be solved by the present invention is to provide a semiconductor manufacturing apparatus, a semiconductor device, and a method for manufacturing a semiconductor device that can form an impurity diffusion layer with fewer crystal defects in a shorter number of steps.
[0006] The semiconductor manufacturing apparatus of this embodiment includes a stage for mounting a substrate. A separation unit separates the beam of impurities introduced onto the substrate into ionic and neutral components. A control unit switches between a first mode for introducing ionic components onto the substrate and a second mode for introducing neutral components onto the substrate. Attached Figure Description
[0007] Figure 1 This is a schematic diagram showing an example of the configuration of the ion implantation apparatus according to this embodiment.
[0008] Figure 2A This is a graph showing an example of the power supply voltage in the ion implantation method of this embodiment.
[0009] Figure 2B This is a graph showing an example of the power supply voltage in the ion implantation method of this embodiment.
[0010] Figure 2C This is a graph showing an example of the power supply voltage in the ion implantation method of this embodiment.
[0011] Figure 3 This is a conceptual diagram representing the ionic and neutral components in an energy filter.
[0012] Figure 4This is a conceptual diagram representing the movement of the platform.
[0013] Figure 5 This is a graph representing an example of the acceleration energy of ionic and neutral components.
[0014] Figure 6 It is a graph representing the impurity concentration and depth of the diffusion layer formed by modes 1 and 2.
[0015] Figure 7 This is a cross-sectional view showing an example of the configuration of the transistor in this embodiment.
[0016] Figure 8 It is a graph showing the concentrations of boron, interlattice silicon, and empty lattice generated in the semiconductor substrate W by implanting ionic components of the first mode.
[0017] Figure 9 It is a graph showing the concentrations of boron, interlattice silicon, and empty lattice generated in a semiconductor substrate by implanting ionic components of mode 1 and neutral components of mode 2.
[0018] Figure 10 This is a graph showing the concentrations of boron in the semiconductor substrate after annealing in modes 1 and 2. Detailed Implementation
[0019] Hereinafter, embodiments of the present invention will be described with reference to the accompanying drawings. These embodiments do not limit the scope of the present invention. The drawings are schematic diagrams or conceptual diagrams, and the proportions of the parts may not be the same as actual figures. In the specification and drawings, elements identical to those described in the preceding drawings are labeled with the same symbols, and detailed descriptions are appropriately omitted.
[0020] Figure 1 This is a schematic diagram showing an example configuration of the ion implantation apparatus 1 according to this embodiment. The ion implantation apparatus 1 includes a chamber 3, a stage 5, an ion source 10, an analyzer 20, a Q-lens 30, a scanner 40, a parallel lens 50, acceleration / deceleration electrodes 60, and an energy filter 70. The ion implantation apparatus 1 is a device for doping impurities into a semiconductor substrate W, such as implanting boron (B), phosphorus (P), or arsenic (As) as impurities. In this embodiment, the ion implantation apparatus 1 will be described as an example of an ion implantation apparatus for implanting boron into a semiconductor substrate W.
[0021] Chamber 3 houses the stage 5, ion source 10, analyzer 20, Q-lens 30, scanner 40, parallel lens 50, acceleration / deceleration electrodes 60, and energy filter 70. Chamber 3 is connected to a vacuum pump (not shown) and is configured to depressurize its internal pressure. Chamber 3 has a transfer port for a semiconductor substrate W, through which the semiconductor substrate W is transferred into chamber 3 and mounted on the stage 5. Alternatively, the semiconductor substrate W can be removed from chamber 3 via the transfer port.
[0022] The stage 5 can hold a semiconductor substrate W. The stage 5 is configured to allow the position of the semiconductor substrate W to be moved, or to change the tilt angle of the semiconductor substrate W relative to the ion beam 12. Drive units 80 and 90 are connected to the stage 5. Drive unit 80 is configured to move the stage 5 along a direction substantially parallel to the mounting surface of the stage 5. Drive unit 90 is configured to tilt the mounting surface of the stage 5 relative to the incident angle of the ion beam 12. Thus, the stage 5 can move the semiconductor substrate W within the chamber 3 and adjust its angle relative to the ion beam 12.
[0023] Ion source 10 is, for example, an ion generation source for impurity BF3.
[0024] The aperture 15 is an opening for shaping the impurity beam from the ion source 10.
[0025] The analyzer 20 removes unwanted ions contained in the impurity beam and extracts the desired ion beam 12. For example, in order to extract the ion beam 12 of B+ ions from the impurity beam (B+, F+, BF+, BF2+) generated by the BF3 ion source, the analyzer 20 removes other F+, BF+, and BF2+ ions.
[0026] Q lens 30 is an electromagnetic lens that electromagnetically shapes the desired ion beam (e.g., B+ ions) 12 extracted by analyzer 20.
[0027] The scanner 40 controls the direction of the ion beam 12 to scan B+ ions onto the semiconductor substrate W.
[0028] Parallel lens 50 is an electromagnetic lens that causes the ion beam 12 to contract or disperse.
[0029] The acceleration / deceleration electrode 60 accelerates or decelerates the ion beam 12.
[0030] The ion beam 12 passing through these beamlines (15, 20, 30, 40, 50, 60) is neutralized by the gas remaining in chamber 3. Therefore, the ion beam 12 contains not only the ion beam (ionic component) but also the neutralized neutral beam (neutral component). Hereinafter, the component in the ion beam 12 that remains as ions will be referred to as the ionic component, and the component of ions that has been neutralized will be referred to as the neutral component.
[0031] The energy filter 70 separates the ion components in the ion beam 12 into ionic and neutral components by controlling the ion components. At this time, the energy filter 70 imparts acceleration or deceleration energy to the ionic components, making the injection energy of the ionic components different from that of the neutral components. Thus, the energy filter 70 can separately introduce the ionic and neutral components into the semiconductor substrate W. Furthermore, the energy filter 70 can introduce the ionic components to a first depth in the semiconductor substrate W with one energy, and introduce the neutral components to a second depth in the semiconductor substrate W with another energy. For example, the energy filter 70 can decelerate boron ions (B+) and inject them into the semiconductor substrate W with a relatively low energy, while directly injecting neutralized boron (B) into the semiconductor substrate W with a relatively high energy. Thus, a boron diffusion layer that extends to a deeper location and a boron diffusion layer that extends only to a relatively shallower location can be formed on the semiconductor substrate W. That is, multiple impurity layers of different depths can be formed on the semiconductor substrate W. At this time, the mounting stage 5 can form a deeper boron diffusion layer and a shallower boron diffusion layer at the same position when viewed from above the surface of the semiconductor substrate W by changing the position and slope of the semiconductor substrate W.
[0032] The control unit 100 controls the various components of the ion implantation apparatus 1 and the power supplies 110-130. Power supply 110 supplies power to the energy filter 70 to control the ion composition from the ion beam 12. Power supply 120 supplies power to the drive unit 80, enabling movement of the stage 5. Power supply 130 supplies power to the drive unit 90, allowing adjustment of the tilt angle of the stage 5. The control unit 100 controls the operation of other components of the ion implantation apparatus 1.
[0033] Next, the ion implantation method using ion implantation device 1 will be described.
[0034] Figures 2A to 2C This is a graph showing an example of the voltage of the power supplies 110 to 130 in the ion implantation method of this embodiment. The vertical axis represents the power supply voltage of each power supply 110 to 130. The horizontal axis represents time t. Figure 3 This is a conceptual diagram representing the ionic component 12I and the neutral component 12N in the energy filter 70. Figure 4 This is a conceptual diagram representing the movement of the mounting platform 5.
[0035] first, Figure 1 Ion source 10 generates ions, such as impurity BF3, to form an impurity beam. A aperture 15 shapes and accelerates the impurity beam. Analyzer 20 removes unwanted ions (e.g., F+, BF+, BF2+) from the impurity beam and extracts the desired ion beam 12 (e.g., B+).
[0036] Next, the Q lens 30 electromagnetically shapes the ion beam 12, and the scanner 40 controls the direction of the ion beam.
[0037] Next, the parallel lens 50 causes the ion beam 12 to contract or disperse, and the acceleration / deceleration electrode 60 accelerates or decelerates the ion beam 12.
[0038] The ion beam 12 passing through these beamlines (15, 20, 30, 40, 50, 60) is neutralized by the gas remaining in chamber 3. Therefore, the ion beam 12 contains not only ionic components but also neutral components.
[0039] Therefore, as Figure 2A As shown, after t1, the power supply 110 applies a negative voltage to the energy filter 70. Thus, the energy filter 70 is able to extract the ionic components from the ion beam 12 and separate them from the neutral components.
[0040] For example, such as Figure 3 As shown, the direction of travel of boron ions (B+), which are the ionic component, is bent under the influence of the electric field from the energy filter 70. On the other hand, the direction of travel of boron particles (B), which are the neutral component, remains almost unchanged under the influence of the electric field from the energy filter 70. Thus, the energy filter 70 separates the ionic component 12I from the neutral component 12N.
[0041] Here, as Figure 2B As shown, during the time period t1 to t2, the power supply 120 applies a positive voltage to the drive unit 80, such as... Figure 2C As shown, power supply 130 applies a positive voltage to drive unit 90. Therefore, as... Figure 4 As shown, the drive unit 80 moves the stage 5 in the -Z direction to irradiate the semiconductor substrate W with ionic component 12I, thereby positioning the semiconductor substrate W at position Zi. Furthermore, the drive unit 90 tilts the stage 5 by an angle θ, introducing the ionic component 12I from a direction tilted by an angle θ relative to the direction perpendicular to the surface of the semiconductor substrate W. Angle θ is the tilt angle of the stage 5 relative to a plane approximately perpendicular to the direction of travel of the ionic component 12I.
[0042] At this time, the scanner 40 scans the beam of ion component 12I and neutral component 12N onto the entire semiconductor substrate W by controlling the direction of the ion beam 12. Here, the process of implanting ion component 12I into the semiconductor substrate W at position Zi is referred to as the first mode.
[0043] Next, as Figure 2B As shown, during the period from time t3 to t4, power supply 120 stops supplying positive voltage, as... Figure 2C As shown, power supply 130 stops supplying positive voltage. Therefore, as... Figure 4As shown, the drive unit 80 moves the stage 5 in the +Z direction to return it to its original position, placing the semiconductor substrate W at position Zn, and irradiating the semiconductor substrate W with neutral component 12N. Additionally, the drive unit 90 restores the slope of the stage 5, causing the neutral component 12N to incident from a direction approximately perpendicular to the surface of the semiconductor substrate W. The drive unit 90 sets the slope of the stage 5 so that the neutral component 12N incident from a direction approximately perpendicular to the surface of the semiconductor substrate W. Furthermore, the drive unit 90 can also tilt the stage 5 at an angle different from angle θ. (Not shown), tilted from a direction perpendicular to the surface of the semiconductor substrate W at an angle The direction of introduction of neutral component 12N. Angle The tilt angle of the stage 5 is based on a plane that is approximately perpendicular to the direction of travel of the neutral component 12N. Here, the process of implanting the neutral component 12N into the semiconductor substrate W at position Zn is referred to as the second mode.
[0044] At this time, the scanner 40 scans the beam of ionic component 12I and neutral component 12N onto the entire semiconductor substrate W by controlling the direction of the ion beam 12.
[0045] The control unit 100 switches between mode 1 and mode 2 between t2 and t3, t4 and t5, and t6 and t7. Thus, the drive unit 80 can move the stage 5 between position Zi (for introducing ionic component 12I) in mode 1 and position Zn (for introducing neutral component 12N) in mode 2. The drive unit 90 can adjust the slope of the stage 5 between mode 1 and mode 2. The drive units 80 and 90 synchronously execute the movement of the stage 5 between position Zi and position Zn, and the tilt angle θ of the stage 5 at position Zi and position Zn. Adjustment of the mounting platforms between them.
[0046] Mode 1 and Mode 2 are executed continuously within the same chamber 3. Therefore, multiple impurity layers with different depths and concentrations can be formed.
[0047] Furthermore, during the transition period between Mode 1 and Mode 2 (e.g., t2~t3, t4~t5), the ion implantation device 1 can continuously irradiate the stage 5 with the ion beam 12. Alternatively, the ion implantation device 1 can temporarily interrupt the irradiation of the ion beam 12 after Mode 1 ends, and resume irradiation at the start of Mode 2. Additionally, there is no particular limitation on the execution order of Mode 1 and Mode 2; either one can be executed first.
[0048] Next, the stage 5 rotates the semiconductor substrate W by, for example, 90°, and performs operations t1 to t4 during t5 to t8. Then, the semiconductor substrate W is rotated 180° and 270°, and the operations t1 to t4 are repeated. This introduces the ionic component 12I and the neutral component 12N into the entire surface of the semiconductor substrate W.
[0049] Here, the acceleration energies (keV) of the ionic component 12I and the neutral component 12N are explained.
[0050] Figure 5 This is a graph representing an example of the acceleration energy of the ionic component 12I and the neutral component 12N. The vertical axis represents the acceleration energy (keV), and the horizontal axis represents the position of the ion beam 12, the ionic component 12I, or the neutral component 12N.
[0051] In this embodiment, an ion source 10 is subjected to, for example, approximately +1.0 keV. The ion beam 12 is extracted from the ion source 10 and accelerated in the aperture 15 at, for example, approximately -2.0 keV. Therefore, the acceleration energy of the ion beam 12 is the difference between the potential of the ion source 10 and the potential of the aperture 15, for example, approximately -3.0 keV.
[0052] If the ion beam 12 passes through the beam line (20-60), as described above, the ion beam 12 becomes a mixture of ionic component 12I and neutral component 12N due to the gas in the chamber 3.
[0053] Next, the energy filter 70 separates the ionic component 12I from the neutral component 12N of the ion beam 12. At this time, the energy filter 70 receives power from the power source 110 and applies an electric field to the ion beam 12, changing only the direction of travel of the ionic component 12I. Because the neutral component 12N is electrically neutral, it is unaffected by the electric field, and its direction of travel remains unchanged.
[0054] Furthermore, the energy filter 70 causes the acceleration energies of the ionic component 12I and the neutral component 12N to differ. For example, the energy filter 70 reduces the acceleration energy of the ionic component 12I by, for example, approximately -2.0 keV. Therefore, based on the potential of the ion source 10, the acceleration energy of the ionic component 12I is approximately -1.0 keV. On the other hand, because the neutral component 12N is electrically neutral, it is unaffected by the electric field from the energy filter 70 and maintains an acceleration energy of, for example, approximately -3.0 keV.
[0055] In this way, the energy filter 70 separates the ionic component 12I and the neutral component 12N of the ion beam 12, ensuring that their acceleration energies are different. Thus, the ionic component 12I... Figure 4 It travels at an acceleration energy of approximately -1.0 keV at the lower position Zi. The neutral component 12N... Figure 4 The Zn at the upper position travels with an acceleration energy of approximately -3.0 keV.
[0056] (Mode 1)
[0057] In the first mode, the stage 5 positions the semiconductor substrate W at position Zi, and the stage 5 is tilted at an angle θ. Ionic component 12I is introduced from a direction tilted at an angle θ relative to a direction approximately perpendicular to the surface of the semiconductor substrate W. The acceleration energy of the ionic component 12I is, for example, about -1 keV.
[0058] (Mode 2)
[0059] In the second mode, the stage 5 positions the semiconductor substrate W at position Zn, and the stage 5 is tilted at an angle... The neutral component 12N is tilted at an angle relative to a direction approximately perpendicular to the surface of the semiconductor substrate W. The direction is introduced. In this embodiment, the angle... The angle is approximately 0°. Therefore, the neutral component 12N is introduced from a direction approximately perpendicular to the surface of the semiconductor substrate W. The acceleration energy of the neutral component 12N is, for example, about -3 keV.
[0060] Figure 6 This is a graph showing the impurity concentration and depth of the diffusion layer formed by the first and second modes. The vertical axis represents the concentration of impurities (e.g., boron). The horizontal axis represents the depth from the surface of the semiconductor substrate W. In the first mode, the acceleration energy of the ionic component 12I is, for example, about -1 keV. Therefore, the ionic component (e.g., B+) 12I is introduced to a relatively shallow location from the surface of the semiconductor substrate W. On the other hand, in the second mode, the acceleration energy of the neutral component 12N is, for example, about -3 keV. Therefore, the neutral component 12N (e.g., B) is introduced to a relatively deep location from the surface of the semiconductor substrate W.
[0061] The concentrations of the ionic component 12I and the neutral component 12N in the ion beam 12 vary depending on the pressure within the chamber 3. For example, when the pressure within the chamber 3 is very low and close to a vacuum, the ion beam 12 hardly collides with other gases within the chamber 3. Since the ion beam 12 is neutralized by collisions with other gases, becoming the neutral component 12N, under very low pressure conditions within the chamber 3, most of the ion beam 12 maintains the state of ionic component 12I, while the neutral component 12N remains almost unchanged. In this case, the concentration of ionic component 12I becomes relatively high, and the concentration of neutral component 12N becomes relatively low.
[0062] On the other hand, under relatively high pressure within chamber 3, most of the ion beam 12 collides with other gases within chamber 3. In this situation, most of the ion beam 12 is neutralized into neutral component 12N. Therefore, the concentration of neutral component 12N becomes relatively high, and the concentration of ionic component 12I becomes relatively low.
[0063] The control unit 100 can control the concentrations of ionic component 12I and neutral component 12N by controlling the pressure within the control chamber 3. Therefore, the ion implantation apparatus 1 of this embodiment can control the impurity layers introduced in the first mode and the second mode to the desired concentrations.
[0064] As described above, the ion implantation apparatus 1 of this embodiment continuously switches between a first mode for introducing ionic component 12I into the semiconductor substrate W and a second mode for introducing neutral component 12N into the semiconductor substrate W in the same ion implantation step. Although the first and second modes use the same ion implantation conditions, they can implant ionic component 12I and neutral component 12N with different acceleration energies into the semiconductor substrate W. The energy filter 70 separates the ionic component 12I and neutral component 12N and implants them into the semiconductor substrate W with different acceleration energies. The stage 5 moves the semiconductor substrate W and changes the tilt angle relative to the plane perpendicular to the travel direction of ionic component 12I and neutral component 12N. As a result, a diffusion layer containing multiple impurity layers of different depths and concentrations can be formed on the semiconductor substrate W in a single ion implantation step.
[0065] Figure 7 This is a cross-sectional view showing an example configuration of the transistor Tr in this embodiment. The transistor Tr can be, for example, a transistor of a CMOS (Complementary Metal Oxide Semiconductor) circuit used in controllers such as NAND (Not AND) type flash memory. The transistor Tr is formed on a semiconductor substrate W.
[0066] The transistor Tr comprises a semiconductor substrate W, source diffusion layers 211 and 212, drain diffusion layers 213 and 214, a gate insulating film 230, a gate electrode 240, a capping film 250, a protective film 260, a spacer 270, a pad layer 280, an interlayer insulating film 290, and a contact 295. Hereinafter, the transistor Tr will be described using a P-type MOSFET (MOS Field Effect Transistor) as an example, but the transistor Tr can also be an N-type MOSFET.
[0067] The semiconductor substrate W may be, for example, a silicon substrate. The gate electrode 240 is formed on the surface of the semiconductor substrate W through a gate insulating film 230. The gate electrode 240 may be made of conductive materials such as doped polysilicon or metal. The gate insulating film 230 may be made of a high-dielectric material such as silicon oxide or silicon oxide with a higher relative permittivity.
[0068] Source diffusion layers 211 and 212 are disposed on one side of the gate electrode 240. The source diffusion layers 211 and 212 contain multiple impurity layers 211 and 212 of different depths. Impurity layer 211 is formed by implanting ionic component 12I in the first mode. Impurity layer 212 is formed by implanting neutral component 12N in the second mode. Therefore, impurity layer 212 is formed deeper than impurity layer 211. Impurity layers 211 and 212 can be impurity layers formed by implanting, for example, boron.
[0069] Furthermore, the impurity layer 211 is formed by implanting ionic component 12I from a direction inclined relative to the surface of the semiconductor substrate W. On the other hand, the impurity layer 212 is formed by implanting neutral component 12N from a direction perpendicular to the surface of the semiconductor substrate W. Therefore, the impurity layer 211 protrudes from the impurity layer 212 into the channel region CH below the gate electrode 240, and is disposed closer to the channel region CH than the impurity layer 212.
[0070] Drain diffusion layers 213 and 214 are disposed on the other side of the gate electrode 240. The drain diffusion layers 213 and 214 contain multiple impurity layers 213 and 214 of different depths. Impurity layer 213 is formed simultaneously or continuously with impurity layer 211 by ionic component 12I implanted in the first mode. Impurity layer 214 is formed simultaneously or continuously with impurity layer 212 by neutral component 12N implanted in the second mode. Therefore, impurity layer 214 is formed deeper than impurity layer 213. Impurity layers 213 and 214 can be impurity layers formed by implantation, for example, boron.
[0071] Furthermore, the impurity layer 213 is formed by implanting ionic component 12I from a direction inclined relative to the surface of the semiconductor substrate W. On the other hand, the impurity layer 214 is formed by implanting neutral component 12N from a direction perpendicular to the surface of the semiconductor substrate W. Therefore, the impurity layer 213 protrudes from the impurity layer 214 into the channel region CH below the gate electrode 240, and is disposed closer to the channel region CH than the impurity layer 214.
[0072] Furthermore, an LDD (Lightly Doped Drain) 220 may be provided on the CH side of the channel region of the source diffusion layers 211, 212 and the drain diffusion layers 213, 214. In this embodiment, the source diffusion layer and the drain diffusion layer are each composed of two impurity layers, but they may also be composed of three or more impurity layers.
[0073] A capping film 250 is disposed above the gate electrode 240. The capping film 250 serves as a hard mask for processing the gate electrode 240. The capping film 250 uses an insulating material such as silicon nitride film.
[0074] A protective film 60 is provided to cover the gate electrode 240 and the top cover film 250. The protective film 260 uses an insulating material such as silicon oxide film.
[0075] Spacers 270 are provided on both sides of the gate electrode 240, separated by a protective film 260. The spacers 270 are made of an insulating material such as a silicon oxide film.
[0076] A padding layer 280 is provided to cover the spacer 270 and the protective film 260. The padding layer 280 uses an insulating material such as a silicon nitride film. The padding layer 280 inhibits the penetration of harmful substances such as hydrogen from the outside.
[0077] An interlayer insulating film 290 is provided on the padding layer 280. The interlayer insulating film 290 is made of an insulating material such as a silicon oxide film.
[0078] Contact 295 penetrates the interlayer insulating film 290 and the pad layer 280, and connects to the source diffusion layers 211, 212 or the drain diffusion layers 213, 214. Contact 295 uses a low-resistance metal such as tungsten or copper.
[0079] With this configuration, the transistor Tr electrically connects or disconnects the source diffusion layers 211, 212 and the drain diffusion layers 213, 214 via the channel region CH according to the potential of the gate electrode 240.
[0080] Figure 8 It is a graph showing the concentrations of boron B1, interlattice silicon Si_int1, and empty lattice V1 generated in the semiconductor substrate W by implanting the ionic component 12I of the first mode. Figure 9 It is a graph showing the concentrations of boron B1, B2, interlattice silicon Si_int1, Si_int2, and empty lattice V1, V2 generated in the semiconductor substrate W by implanting the ionic component 12I of the first mode and the neutral component 12N of the second mode. Figure 10These are graphs showing the concentrations of boron B1 and B2 in the semiconductor substrate W after annealing in modes 1 and 2. The vertical axis of these graphs represents the concentration, and the horizontal axis represents the depth Xj from the surface of the semiconductor substrate W.
[0081] like Figure 8 As shown, in Mode 1, boron B1 is implanted to a depth XB1 from the surface of the semiconductor substrate W by implanting ionic component 12I. At this time, under the influence of the implanted ionic component 12I, an empty lattice V1 and interlattice silicon Si_int1 are generated. Interlattice silicon Si_int1 consists of silicon atoms whose self-crystallization bonds break due to collisions between boron B1 and the silicon crystals of the semiconductor substrate W. The empty lattice V1 is the space remaining after the silicon atoms' self-crystallization bonds break. The empty lattice V1 is generated at a depth XV1 from the surface of the semiconductor substrate W. Interlattice silicon Si_int1 is generated at a depth XSi1 from the surface of the semiconductor substrate W.
[0082] Empty lattice V1 and interlattice silicon Si_int1 are generated by collisions between boron B1 and silicon crystals; therefore, XV1 < XB1 < XSi1. Empty lattice V1 is a crystallization defect, so fewer of them are better. Furthermore, the depth positions XB1, XV1, and XSi1 represent the positions of the concentration peaks of boron B1, empty lattice V1, and interlattice silicon Si_int1, respectively.
[0083] like Figure 9 As shown, in the second mode, boron B2 is injected to a depth XB2 from the surface of the semiconductor substrate W by injecting a neutral component 12N. At this time, the injected neutral component 12N causes the formation of an empty lattice V2 and interlattice silicon Si_int2. Interlattice silicon Si_int2 consists of silicon atoms whose self-crystallization bonds break due to collisions between boron B2 and the silicon crystals of the semiconductor substrate W. An empty lattice V2 is the space remaining after the silicon atoms have broken their self-crystallization bonds. For example, an empty lattice V2 is generated at a depth XV2 from the surface of the semiconductor substrate W. Interlattice silicon Si_int2 is generated at a depth XSi2 from the surface of the semiconductor substrate W.
[0084] Empty lattice V2 and interlattice silicon Si_int2 are generated by collisions between boron B2 and silicon crystals; therefore, XV2 < XB2 < XSi2. Empty lattice V2 is a crystallization defect, so fewer of them are better. Furthermore, the depth positions XB2, XV2, and XSi2 represent the positions of the concentration peaks of boron B2, empty lattice V2, and interlattice silicon Si_int2, respectively.
[0085] Here, the depth position XV2 of the empty lattice V2 is close to or approximately equal to the depth position XSi1 of the interlattice silicon Si_int1. Therefore, after annealing, the interlattice silicon Si_int1 is reconfigured within the empty lattice V2, thereby reducing the concentration of both the empty lattice V2 and the interlattice silicon Si_int1. This reduces crystallization defects (EOR (End-Of-Range) defects) in the source diffusion layers 211, 212 and the drain diffusion layers 213, 214. Furthermore, in the second mode, the injection energy of the neutral component 12N is higher, resulting in a widespread and disordered distribution of the interlattice silicon Si_int2, reducing its density. This further reduces crystallization defects in the source diffusion layers 211, 212 and the drain diffusion layers 213, 214.
[0086] After executing modes 1 and 2, annealing is performed. Therefore, as follows... Figure 10 As shown, the empty lattice V1, V2 and the interlattice silicon Si_int1, Si_int2 are reduced as described above, and boron B1, B2 form source diffusion layers 211, 212 and drain diffusion layers 213, 214. At this time, the empty lattice V1, V2 and the interlattice silicon Si_int1, Si_int2 are reduced, and boron B1, B2 form source diffusion layers 211, 212 and drain diffusion layers 213, 214.
[0087] Thus, the ion implantation apparatus 1 and ion implantation method of this embodiment can form a source diffusion layer (or drain diffusion layer) containing multiple impurity layers 211, 212 (or multiple impurity layers 213, 214) with fewer crystal defects in a single, shorter ion implantation step. The drain diffusion layer containing multiple impurity layers 213, 214 with fewer crystal defects can mitigate the electric field near the drain and suppress leakage current and the generation of hot carriers.
[0088] Furthermore, the ion implantation apparatus 1 and the ion implantation method can form a diffusion layer with multiple concentration distributions in a single impurity implantation step. Therefore, this embodiment can increase yield and reduce production costs.
[0089] Furthermore, the concentrations of ion component 12I and neutral component 12N in the ion beam 12 can be controlled by adjusting the pressure within the chamber 3. Therefore, the control unit 100 can control the concentrations of ion component 12I and neutral component 12N by adjusting the pressure within the chamber 3. For example, if the pressure within the chamber 3 is set to 10 times, increasing to 1×10... -3 (Pa)~1×10 -2 If the concentration of ion beam 12 increases (Pa), the probability of collision between ion beam 12 and the correspondingly increased number of particles will increase. Therefore, the amount of neutral component 12N will increase tenfold. Thus, this embodiment can achieve a highly accurate concentration distribution of the diffusion layer by controlling the concentration of neutral component 12N.
[0090] Several embodiments of the present invention have been described, but these embodiments are provided by way of example and are not intended to limit the scope of the invention. These embodiments may be implemented in various other ways, and various omissions, substitutions, and modifications may be made without departing from the spirit of the invention. These embodiments and their variations are included in the scope and spirit of the invention, and likewise included within the scope of the invention as described in the claims and its equivalents.
[0091] [Explanation of Symbols]
[0092] 1: Ion implantation device
[0093] 3: Chamber
[0094] 5: Platform
[0095] 10: Ion source
[0096] 20: Analyzer
[0097] 30:Q lens
[0098] 40: Scanner
[0099] 50: Parallel lens
[0100] 60: Acceleration / Deceleration Electrodes
[0101] 70: Energy Filter
[0102] 80, 90: Drive Unit
[0103] 100: Control Department
[0104] 110~130: Power supply
[0105] W: Semiconductor substrate.
Claims
1. A semiconductor manufacturing apparatus comprising: a stage for mounting a substrate; The separation section separates the beam of impurities introduced into the substrate into ionic and neutral components; and The control unit switches between a first mode that introduces the ionic component into the substrate and a second mode that introduces the neutral component into the substrate; The semiconductor manufacturing apparatus further includes a drive unit that moves the stage to a first position for introducing the ionic component and a second position for introducing the neutral component.
2. The semiconductor manufacturing apparatus according to claim 1, wherein the driving unit adjusts the slope of the stage in such a way that the ionic component is introduced from a direction inclined at a first angle relative to the direction perpendicular to the surface of the substrate, and adjusts the slope of the stage in such a way that the neutral component is introduced from a direction inclined at a second angle relative to the direction perpendicular to the surface of the substrate.
3. The semiconductor manufacturing apparatus according to claim 2, wherein the control unit synchronously executes the movement of the mounting stage between the first position and the second position, and the adjustment of the mounting stage between the first angle and the second angle.
4. The semiconductor manufacturing apparatus according to claim 1, further comprising a chamber for receiving the substrate. The control unit controls the concentration of the ionic component and the neutral component based on the pressure inside the chamber.
5. The semiconductor manufacturing apparatus according to claim 2, further comprising a chamber for receiving the substrate. The control unit controls the concentration of the ionic component and the neutral component based on the pressure inside the chamber.
6. The semiconductor manufacturing apparatus according to claim 1, wherein the separation unit causes the ionic component to have a different energy from the neutral component, introduces the ionic component into the substrate with a first energy, and introduces the neutral component into the substrate with a second energy.
7. The semiconductor manufacturing apparatus according to claim 2, wherein the separation unit causes the ionic component to have a different energy from the neutral component, introduces the ionic component into the substrate with a first energy, and introduces the neutral component into the substrate with a second energy.
8. A method for manufacturing a semiconductor device, the method using a semiconductor manufacturing apparatus, the semiconductor manufacturing apparatus comprising a separation unit and a stage, the separation unit separating a beam of impurities introduced onto a substrate into ionic components and neutral components, and ensuring that the ionic components and the neutral components have different energies, the stage mounting the substrate, and the semiconductor manufacturing apparatus comprising: executing a first mode when the stage is in a first position, moving the stage from the first position to a second position, executing a second mode when the stage is in the second position, and the method for manufacturing the semiconductor device comprising the following steps: The impurity beam is separated into ionic and neutral components. The first mode is executed, which introduces the ionic components into the substrate at a first energy. The second mode is executed, in which the neutral component is introduced into the substrate at a second energy.
9. The method of claim 8, wherein in the first mode, the ionic component is introduced into the substrate from a first angle. In the second mode, the ionic component is introduced into the substrate from a second angle.
10. The method of claim 8, wherein the semiconductor manufacturing apparatus further comprises a chamber for receiving the substrate. The first mode and the second mode are executed consecutively within the same chamber.
11. The method of claim 9, wherein the semiconductor manufacturing apparatus further comprises a chamber for receiving the substrate. The first mode and the second mode are executed consecutively within the same chamber.
Citation Information
Patent Citations
Rail vehicle body structure and method of manufacturing thereof
JP2021138315A
Ion implanter and ion implantation method
CN112242287A
Method and apparatus for neutral beam processing based on gas cluster ion beam technology
US20120045615A1