A cement kiln nitrogen oxide ultra-low emission and monitoring system
By using a technology that combines a foam doser and a cyclone dust collector in the cement kiln denitrification system, the problem of contact between dust in the flue gas and the catalyst is solved, the denitrification efficiency and dust removal effect are improved, the catalyst life is extended, and the operating cost is reduced.
Patent Information
- Application Number
- CN202211273321.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-10-18
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2042-10-18
AI Technical Summary
During the denitrification process of existing cement kilns, the contact between dust in the flue gas and the catalyst leads to wear and poisoning, which affects the denitrification efficiency. The cyclone dust collector is not effective in removing small-diameter particles, resulting in shortened catalyst life and high operating costs.
A foam injector is used to inject foam into the kiln tail flue to absorb dust and aggregate it. It is combined with a cyclone dust collector for dust removal to reduce dust entering the SCR reactor, reduce catalyst wear and poisoning risks, and optimize the distribution of foam through a venturi tube. and breakage to improve dust removal efficiency.
It effectively reduces the wear and poisoning of the catalyst by dust, extends the service life of the catalyst, improves the dust removal effect of small-diameter particles, reduces heat loss, maintains the efficiency of the SCR denitration process, and reduces operating costs.
Smart Images

Figure CN115837214B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of cement production equipment, and in particular to an ultra-low emission and monitoring system of nitrogen oxides from a cement kiln. Background Art
[0002] In the dry cement production process, the rotary kiln is the main source of nitrogen oxides. Among the nitrogen oxides in the flue gas at the kiln tail, the NO content can account for more than 95% of the total, while the NO2 content is relatively small [1]. According to the requirements of the "Emission Standards of Air Pollutants for the Cement Industry", cement production enterprises should limit the emission of nitrogen oxides in tail gas. When no denitrification measures are taken for the flue gas of cement rotary kilns, the emission of nitrogen oxides is about 350 to 2200 mg / Nm 3 , it is difficult to meet the requirements of emission standards, and denitrification measures are generally required.
[0003] At present, the most commonly used denitrification method in cement kilns is selective non-catalytic reduction denitrification, that is, adding a reducing agent (such as ammonia water, urea, etc.) to the decomposition furnace, and at a suitable temperature, the following reaction occurs to reduce NO or NO2 to N2:
[0004] 4NH3+4NO+O2→4N2+6H2O
[0005] 2NO2+4NH3+O2→3N2+6H2O
[0006] However, when the temperature exceeds 1100°C, the oxidation reaction of the reducing agent gradually occurs, reducing the reaction rate of the reducing agent and NO. At this time, the reducing agent even reacts with oxygen to generate more NO, as follows:
[0007] 4NH3+5O2→4NO+6H2O
[0008] Studies have shown that when ammonia is used as a reducing agent, the optimal reaction temperature is 850℃~1100℃, while when urea is used as a reducing agent, the optimal reaction temperature is 900℃~1200℃. At the optimal reaction temperature, the nitrogen oxide emissions of cement kilns can be controlled at 200mg / Nm 3 However, as environmental protection policies become increasingly stringent, 200mg / Nm 3 The emission volume is still higher than the emission requirements in areas with greater environmental pressure. In addition, ammonia is corrosive and easily volatile, while urea is expensive, has low operating costs, and needs to be dissolved into a solution before use.
[0009] The selective catalytic reduction method is a method in which low-temperature flue gas is introduced into the SCR reactor at the outlet pipe of the preheater, ammonia or urea is added to the pipe as a reducing agent, and nitrogen oxides are reduced to nitrogen under the action of a catalyst. This method is to send the low-temperature exhaust gas (about 350°C) from the kiln tail preheater into an SCR reactor equipped with a catalyst to react with the reducing agent. The denitrification efficiency can reach 80% to 90%, and the concentration of nitrogen oxides can be reduced to 100 to 200 mg / Nm 3 The following, such as CN110841475A, adopts this method.
[0010] However, this method requires the use of precious metal catalysts such as V2O5. At the same time, due to the high total dust and alkali metal content in the flue gas, the catalyst is easily blocked and poisoned, resulting in high operating costs. In CN110841475A, a rake-type dust collector is used to prevent dust from accumulating on the catalyst surface, but when dust follows the exhaust gas through the catalyst, it will still cause the dust to contact the catalyst and cause wear and poisoning.
[0011] CN108554144A discloses an SCR denitrification system suitable for high-dust and high-alkali flue gas at the tail of a cement kiln. The system pre-de-dusts the tail flue gas at high temperature by installing an electrostatic precipitator, a cyclone dust collector, a cyclone internal component or a grille, so that the flue gas after pre-de-dust enters the SCR denitrification device for selective catalytic denitrification. In theory, this scheme can reduce the impact of dust on the life of the catalyst. However, due to the large flue gas volume of the cement kiln, to achieve a high dust removal rate, the electrostatic precipitator needs to have a sufficiently large processing capacity, resulting in a huge size and a large footprint of the electrostatic precipitator. If it is installed in front of the inlet of the denitrification device, it will cause a large amount of heat loss. Even if ideal insulation measures are taken, the heat loss generated is unacceptable, causing the temperature of the flue gas after dust removal to drop, affecting the effect of catalytic denitrification. The cyclone dust collector has a poor dust removal effect on particles below 5μm, while the slag ratio of particles below 3.2μm in the flue gas at the tail of a cement kiln can reach 72.3% [2]. The dust removal effect of the cyclone internals and grilles is far inferior to that of the electrostatic precipitator, and the effect of preventing catalyst clogging and poisoning is not ideal.
[0012] [1] Song Zhenghua, Xing Guoliang, Yang Zhengping. New dry process cement kiln nitrogen oxide removal technology [J]. China Cement, 2009(6):73-74.
[0013] [2] Jia Xiaoping, Zhang Kun, Li Shaoping. Analysis and suggestions on the selection of dust removal equipment for kiln systems [J]. Cement, 2014(9):46~48. Summary of the invention
[0014] The purpose of the present invention is to provide a cement kiln nitrogen oxide ultra-low emission and monitoring system, which adopts a selective catalytic reduction method to denitrify the flue gas of the cement kiln, and can reduce the contact between dust in the flue gas and the catalyst, thereby reducing the wear and poisoning effect of dust on the catalyst.
[0015] The technical solution adopted by the present invention is as follows:
[0016] A cement kiln nitrogen oxide ultra-low emission and monitoring system comprises a kiln tail flue, a dust removal device, an SCR reactor, and a waste heat boiler which are connected in sequence, wherein the inlet of the kiln tail flue is connected to a preheater, a reducing agent filling device is provided at the inlet of the SCR reactor, and the reducing agent is ammonia water or urea solution, the dust removal device comprises a foam filler and a cyclone dust collector, the outlet of the foam filler is located on the kiln tail flue, a first dust concentration detector is provided on the kiln tail flue, a second dust concentration detector is provided at the outlet of the cyclone dust collector, and a nitrogen oxide detector is provided at the outlet of the SCR reactor.
[0017] Preferably, the foam filler includes a foaming tank, a bubble injection tube, and a bubbling tube. The foaming tank contains a certain level of foaming liquid, and the bubbling tube injects gas into the foaming liquid. The bubble injection tube is connected to the kiln tail flue and the foaming tank respectively, and the inlet of the bubble injection tube is located in the foam layer in the foaming tank.
[0018] Preferably, the foam filler further comprises a liquid level meter and an acoustic wave level meter, wherein the liquid level meter is used to measure the liquid level of the foaming liquid, and the acoustic wave level meter is installed on the top of the foaming tank to measure the height of the foam layer.
[0019] Preferably, the outlet of the bubble injection pipe is located at the upper side of the kiln tail flue, and the inlet height of the bubble injection pipe is higher than the outlet height.
[0020] Preferably, a first venturi tube is provided at the connection between the bubble injection tube and the kiln tail flue, and the outlet of the bubble injection tube is located in the middle of the first venturi tube.
[0021] Preferably, the foaming liquid comprises the following components by weight: 5% to 22% AEO-12, 0.5% to 2% high carbon alcohols, 1% to 4% methanol, and the remainder water.
[0022] Preferably, a throttle valve is provided on the bubbling tube.
[0023] Preferably, at least three ultrasonic level meters are provided at different positions on the top of the foaming tank.
[0024] Preferably, a second Venturi tube is provided between the outlet of the bubble injection tube and the cyclone dust collector.
[0025] Preferably, the ultrasonic level meter includes a first level meter, a second level meter, and a third level meter, the horizontal distance between the first level meter and the entrance of the bubble tube is L1, the horizontal distance between the second level meter and the bubble tube is L2, the horizontal distance between the third level meter and the entrance of the bubble tube is L3, and L1∈(0,0.25D], L2∈(0,0.30D], L3∈[0.8D,D), where D is the inner diameter of the foaming tank.
[0026] In summary, due to the adoption of the above technical solution, the beneficial effects of the present invention are:
[0027] (1) Placing the dust removal device before the inlet of the SCR reactor can effectively reduce the dust content of the flue gas entering the SCR reactor, thereby greatly reducing the wear and blockage of the catalyst by dust, and avoiding the poisoning of the catalyst by alkaline substances in the dust, which can effectively reduce the loss of the precious metal catalyst used in the SCR reactor and extend its service life;
[0028] (2) A foam injector is used to inject foam into the flue at the tail of the kiln, so that the dust in the flue gas collides with the foam and aggregates into larger particles, which can be removed more effectively after entering the cyclone dust collector, solving the problem that the cyclone dust collector is not effective in removing small-diameter particles in the flue gas. Since the foam carries a small amount of liquid, it has a slight effect on the temperature of the flue gas and will not interfere with the subsequent SCR denitrification process;
[0029] (3) The main component of the foaming agent does not contain metals such as sodium that are toxic to the catalyst and will not affect the performance of the catalyst;
[0030] (4) A first venturi tube is provided at the connection between the bubble injection pipe and the kiln tail flue, so that a low pressure area is generated at the connection between the bubble injection pipe and the kiln tail flue, which is conducive to the foam in the bubble injection pipe entering the kiln tail flue;
[0031] (5) A second Venturi tube is also provided on the flue at the tail of the kiln, which utilizes the change in pressure to break the foam as much as possible before it enters the cyclone dust collector, so that a large number of droplets generated when the foam breaks can diffuse into the flue gas, fully moistening the dust in the flue gas to promote dust aggregation and facilitate dust removal by the cyclone dust collector. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 It is a process flow chart of the present invention.
[0033] Figure 2 This is a structural diagram of the foaming tank.
[0034] Markings in the figure: 100, kiln tail flue; 200, SCR reactor; 300, waste heat boiler; 400, preheater; 500, foam filler; 600, cyclone dust collector; 101, first venturi tube; 102, second venturi tube; 501, foaming tank; 502, bubble injection tube; 503, bubbling tube; 504, liquid level meter; 506, throttle valve; 701, first dust concentration detector; 702, second dust concentration detector; 703, nitrogen oxide detector; 5051, first material level meter; 5052, second material level meter; 5053, third material level meter. DETAILED DESCRIPTION
[0035] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.
[0036] like Figure 1 As shown, the present invention provides a cement kiln nitrogen oxide ultra-low emission and monitoring system, which includes an emission control part and a nitrogen oxide content monitoring part, wherein the emission control part includes a kiln tail flue 100, a dust removal device, an SCR reactor 200, and a waste heat boiler 300 which are connected in sequence, and the inlet of the kiln tail flue 100 is connected to the preheater 400, so that the kiln tail flue gas discharged from the preheater 400 passes through the dust removal device, the SCR reactor 200, and the waste heat boiler 300 in sequence, and after dust removal and denitrification, enters the waste heat boiler 300 to recover heat, and is finally discharged from the chimney.
[0037] A reducing agent filling device is provided at the entrance of the SCR reactor 200. The reducing agent filling device sprays the liquid reducing agent in a mist form, mixes it with the flue gas at the tail of the kiln, and then enters the SCR reactor to reduce the nitrogen oxides in the flue gas at the tail of the kiln and generate nitrogen, thereby reducing the emission of nitrogen oxides. The reducing agent used in the present invention is ammonia water or urea solution, and its specific concentration and filling amount are determined according to the production scale and operating parameters of the cement kiln. The SCR reactor 200 uses molecular sieve loaded V2O5 as a catalyst, and other types of catalysts commonly used in the field can also be used. The structure of the SCR reactor 200, the catalyst type, and the loading method are not the focus of the present invention.
[0038] In addition, the SCR reactor 200 uses a rake-type soot blower, which is provided by the original SCR reactor.
[0039] The dust removal device includes a foam filler 500 and a cyclone dust collector 600. The outlet of the foam filler 500 is located on the kiln tail flue 100. By injecting foam into the kiln tail flue 100, the dust in the kiln tail flue gas is adsorbed, causing it to aggregate and increase in diameter, which is convenient for the cyclone dust collector 600 to remove dust.
[0040] Specifically, the foam filler 500 includes a foaming tank 501, a bubble injection tube 502, and a bubbling tube 503. The foaming tank 501 contains a certain level of foaming liquid, and the lower end of the bubbling tube 503 is inserted into the foaming liquid. By injecting gas into the foaming liquid, a large amount of foam is generated in the foaming liquid, and a foam layer of a certain height is generated in the foaming tank 501. The bubble injection tube 502 is connected to the kiln tail flue 100 and the foaming tank 501 respectively, and the inlet of the bubble injection tube 502 is located in the foam layer in the foaming tank 501, and the outlet of the bubble tube 502 is located on the upper side of the kiln tail flue 100, and the inlet height of the bubble injection tube 502 is higher than its outlet height, so that the foam in the foaming tank 501 can enter the kiln tail flue 100.
[0041] The gas in the bubbling tube 503 is part of the gas discharged from the waste heat boiler 300, and the following factors are mainly considered: the gas flow rate required for bubbling is large, and low-cost gas should be used for bubbling as much as possible; although the cost of using air bubbling is very low, the oxygen content in the air is relatively high, and is higher than the oxygen content in the flue gas at the tail of the kiln, which will affect the reaction balance of the SCR denitrification reaction; the gas temperature discharged from the waste heat boiler 300 still has residual temperature, and is higher than the air temperature, and the temperature difference with the flue gas is smaller, and the impact on the flue gas temperature after mixing into the flue gas is smaller. The reason for not using dust removal flue gas bubbling is that the dust removal flue gas temperature is too high, and the air supply equipment cannot withstand the high temperature of the flue gas. In addition, the high-temperature flue gas will cause the components of the foaming liquid to decompose or oxidize, affecting the foaming effect.
[0042] In order to facilitate the control of the liquid level of the foaming liquid and the height of the foam layer in the foaming tank 501, a liquid level meter 504 and an ultrasonic level meter are also provided on the foaming tank 501, and a throttle valve 506 is provided on the bubbling tube 503. The liquid level meter 504 adopts a float level meter, which can accurately measure the liquid level of the foaming liquid. The ultrasonic level meter is installed on the top of the foaming tank 501 to measure the height of the foam layer.
[0043] Specifically, the sonic level meter includes a first level meter 5051, a second level meter 5052, and a third level meter 5053. The first level meter 5051 is used to measure the foam height H1 at the inlet of the bubble injection tube 502, the second level meter 5052 is used to measure the foam height H2 near the bubble tube 503, and the third level meter 5053 is used to measure the foam height H3 in the area opposite to the inlet of the bubble injection tube 502. The foam height in the foaming tank 501 is H0=(H1+H2+H3) / 3; Specifically, the horizontal distance between the first level meter 5051 and the entrance of the bubble tube 502 is L1, the horizontal distance between the second level meter 5052 and the bubble tube 503 is L2, and the horizontal distance between the third level meter 5053 and the entrance of the bubble tube 502 is L3, and L1∈(0,0.25D], L2∈(0,0.30D], L3∈[0.8D,D), wherein D is the inner diameter of the foaming tank 501, specifically, L1 is 0.1D, L2 is 0.15D, and L3 is 0.95D.
[0044] The first material level meter 5051, the second material level meter 5052, and the third material level meter 5053 use different operating frequencies. Specifically, the operating frequency of the first material level meter 5051 is 32kHz, the operating frequency of the second material level meter 5052 is 34kHz, and the operating frequency of the third material level meter 5053 is 36kHz, so as to avoid mutual interference between the signals of each material level meter.
[0045] In other embodiments, the number of sonic level meters may be greater than 3, and their installation positions should at least include the installation positions of the first level meter 5051, the second level meter 5052, and the third level meter 5053, and the height of the foam layer is still the average value of these sonic level meters.
[0046] When the foaming liquid level in the foaming tank 501 is too low (either H0 or H1 is lower than the lower limit), the configured foaming liquid can be added to the foaming tank 501 through the top feeding port of the foaming tank 501. The replenishment method is manual filling, and an injection pump can also be added to fill through the injection pump; when the height of the foam layer in the foaming tank 501 is too high, the opening of the throttle valve 506 can be reduced to reduce the height of the foam layer; in the present invention, the inlet of the bubble injection tube 502 is located at 40% of the height of the foaming tank 501, and the liquid level of the foaming liquid in the foaming tank 501 is controlled not to be lower than 20% of the height of the foaming tank 501, and is lower than the inlet height of the bubble injection tube 502 by 0.5m, and the foam height H0 does not exceed 80% of the height of the foaming tank 501.
[0047] A first venturi tube 101 is provided at the connection between the bubble injection tube 502 and the kiln tail flue 100. The outlet of the bubble injection tube 502 is located in the middle of the first venturi tube 101. The middle diameter of the first venturi tube 101 is 0.75 times the end diameter. When the kiln tail flue gas passes through the first venturi tube 101, a low-pressure area is generated at the outlet of the bubble injection tube 502, which is beneficial for the foam to enter the kiln tail flue 100 from the foaming tank 501 and reduce the pressure required for the bubbling tube 503 to generate bubbles.
[0048] A second venturi tube 102 is provided between the outlet of the bubble injection tube 502 and the cyclone dust collector 600. The middle diameter of the second venturi tube 102 is 0.5 times the diameter of the end portion. When the bubbles pass through the second venturi tube 102 with the air flow, the pressure outside the bubbles drops suddenly, causing the volume of the bubbles to expand dramatically in a short period of time. Most of the bubbles burst in the process, and the droplets generated during the bursting can further promote the aggregation of dust particles.
[0049] By weight, the foaming liquid used in the present invention includes the following components: AEO-12 accounts for 18%, high carbon alcohol accounts for 1.5%, methanol accounts for 2%, and water accounts for 78.5%. The above components do not contain metal elements, especially Na and heavy metal elements that are toxic to catalysts, and do not contain elements such as sulfur and chlorine.
[0050] In other embodiments, the proportion of AEO-12 can be 5% to 22%, the content of higher carbon alcohols can be 0.5% to 2%, the proportion of methanol can be 1% to 4%, and the balance is water, wherein the proportion of methanol is 1 to 2 times that of higher carbon alcohols.
[0051] The nitrogen oxide content monitoring part of the present invention includes a first dust concentration detector 701, a second dust concentration detector 702, and a nitrogen oxide detector 703, wherein the first dust concentration detector 701 is arranged on the kiln tail flue 100, and is used to measure the dust content in the kiln tail flue gas discharged from the preheater 400, the second dust concentration detector 702 is arranged at the outlet of the cyclone dust collector 600, and is used to measure the dust concentration in the kiln tail flue gas after dust removal, and the nitrogen oxide detector 703 is arranged at the outlet of the SCR reactor 200, and is used to measure the nitrogen oxide content in the kiln tail flue gas after denitrification.
[0052] The flue gas discharged from the preheater 400 enters the kiln tail flue 100, and after mixing with the foam, most of the dust in the flue gas is adsorbed by the foam and aggregated. The foam breaks in the process of moving with the airflow in the kiln tail flue 100 and passing through the second venturi tube 102, generating a large number of droplets and further promoting the aggregation of dust particles. After that, the flue gas enters the cyclone dust collector 600 for dust removal, and the dust particles are discharged from the bottom outlet of the cyclone dust collector 600. The dust-removed flue gas is discharged from the top of the cyclone dust collector 600, and after mixing with the reducing agent, it enters the SCR reactor 200 for denitrification. The flue gas after denitrification enters the waste heat boiler 300 for cooling and is discharged from the chimney. At the same time, a part of the cooled flue gas is sent to the bubbling tube 503 through the blower pipe for bubbling.
[0053] Denitrification of flue gas at the tail of a 2500t / d dry cement kiln was carried out. After measurement, the average flue gas flow rate at the tail of the kiln was 284337Nm 3 / h, the gas flow rate of the bubbling tube 503 is 15000Nm 3 / h, rake soot blower blows soot once a week, the first dust concentration detector 701 reading is 14~32g / Nm 3 The second dust concentration detector 702 reading is 27~183mg / Nm 3 , the reading of nitrogen oxide detector 703 is 19~33mg / Nm 3 (10% O 2The content of nitrogen oxides was 650-800 mg / Nm 3 , the denitrification rate exceeds 95%.
[0054] In addition, the throttle valve 506 was closed and the gas injection through the bubbling tube 503 was stopped to compare the difference in dust removal effect. The second dust concentration detector 702 began to rise and rose rapidly 70 to 110 seconds after the throttle valve 506 was closed, and finally stabilized at 13-17 g / Nm 3 , the dust removal effect of the cyclone dust collector 600 is significantly reduced.
[0055] The above-mentioned cement kiln nitrogen oxide ultra-low emission and monitoring system has been running on a 2500t / d dry process cement kiln for 6 months. The nitrogen oxide content in the flue gas after denitrification is basically maintained at 45mg / Nm 3 Below, the denitrification effect is stable.
[0056] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A cement kiln nitrogen oxide ultra-low emission and monitoring system, comprising a kiln tail flue (100), a dust removal device, an SCR reactor (200), and a waste heat boiler (300) connected in sequence, wherein the inlet of the kiln tail flue (100) is connected to a preheater (400), and a reducing agent filling device is provided at the inlet of the SCR reactor (200), wherein the reducing agent is ammonia water or urea solution, and wherein: The dust removal device comprises a foam filler (500) and a cyclone dust collector (600), the outlet of the foam filler (500) is located on the kiln tail flue (100), the kiln tail flue (100) is provided with a first dust concentration detector (701), the outlet of the cyclone dust collector (600) is provided with a second dust concentration detector (702), and the outlet of the SCR reactor (200) is provided with a nitrogen oxide detector (703); The foam injector (500) comprises a foaming tank (501), a foaming pipe (502), and a bubbling pipe (503); the foaming tank (501) contains a foaming liquid at a certain level; the bubbling pipe (503) injects gas into the foaming liquid; the foaming pipe (502) is connected to the kiln tail flue (100) and the foaming tank (501), respectively, and the inlet of the foaming pipe (502) is located in the foam layer in the foaming tank (501); The gas in the bubbling tube (503) is part of the gas discharged from the waste heat boiler (300); A first venturi tube (101) is provided at the connection between the bubble injection tube (502) and the kiln tail flue (100); the outlet of the bubble injection tube (502) is located in the middle of the first venturi tube (101); when the smoke in the flue passes through the first venturi tube (101), a low-pressure area is generated at the outlet of the bubble injection tube (502), so as to facilitate the foam to enter the kiln tail flue (100) from the foaming tank (501), thereby reducing the pressure required for the bubble tube (503) to generate bubbles; A second venturi tube (102) is also provided between the outlet of the bubble injection tube (502) and the cyclone dust collector (600); The foam filler (500) further comprises a liquid level meter (504) and an acoustic wave level meter. The liquid level meter (504) is used to measure the liquid level of the foaming liquid. The acoustic wave level meter is installed on the top of the foaming tank (501) and is used to measure the height of the foam layer.
2. The ultra-low emission and monitoring system of nitrogen oxides in cement kilns according to claim 1 is characterized in that: The outlet of the bubble injection pipe (502) is located on the upper side of the kiln tail flue (100), and the inlet height of the bubble injection pipe (502) is higher than the outlet height.
3. The ultra-low emission and monitoring system of nitrogen oxides in cement kilns according to claim 1 is characterized in that: The foaming liquid comprises the following components by weight: 5% to 22% of AEO-12, 0.5% to 2% of high carbon alcohol, 1% to 4% of methanol, and the balance is water.
4. The ultra-low emission and monitoring system of nitrogen oxides in cement kilns according to claim 1 is characterized in that: The bubbling tube (503) is provided with a throttle valve (506).
5. The ultra-low emission and monitoring system of nitrogen oxides in cement kilns according to claim 1 is characterized in that: At least three of the sonic level meters are provided at different positions on the top of the foaming tank (501).
6. The ultra-low emission and monitoring system of nitrogen oxides in cement kilns according to claim 5 is characterized in that: The sonic level meter comprises a first level meter (5051), a second level meter (5052), and a third level meter (5053); the horizontal distance between the first level meter (5051) and the entrance of the bubble injection tube (502) is L1; the horizontal distance between the second level meter (5052) and the bubble injection tube (503) is L2; the horizontal distance between the third level meter (5053) and the entrance of the bubble injection tube (502) is L3; and L1∈(0,0.25D], L2∈(0,0.30D], L3∈[0.8D,D), wherein D is the inner diameter of the foaming tank (501).