A method for fabricating a semiconductor device and the semiconductor device itself.
By controlling the inward recess of the gate insulating layer and the end of the gate layer to a predetermined length after the etching process, and forming an oxide layer in the re-oxidation process, the problem of reduced effective channel length caused by etching damage is solved, thereby improving the stability of semiconductor devices and reducing leakage current.
Patent Information
- Application Number
- CN202110937661.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-08-16
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2041-08-16
AI Technical Summary
In existing technologies, the etching process causes damage that leads to a reduction in the effective channel length after the re-oxidation process when manufacturing gate stack structures.
After the etching process, the ends of the gate insulating layer and the gate layer are recessed inward by a predetermined length, and an oxide layer is formed in the re-oxidation process so that the oxide layer does not cover the gate insulating layer, thereby maintaining the effective channel length unchanged.
By controlling the oxidation at the gate layer end, the effective channel length reduction caused by the re-oxidation process is avoided, thereby improving the operating stability of the semiconductor device and reducing leakage current.
Smart Images

Figure CN115938923B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor manufacturing, and more particularly to a method for preparing a semiconductor device and the semiconductor device thereof. Background Technology
[0002] The gate stack structure is an indispensable part of a transistor. In existing technologies, the fabrication of a gate stack typically involves first depositing a gate insulating material layer and a gate material layer on a substrate, and then patterning and etching these material layers to form the gate insulating layer and the gate layer. This etching process causes some damage to the substrate surface, the side surfaces of the gate insulating layer and the gate layer. To repair this damage, the conventional approach is to perform a re-oxidation process after the etching process.
[0003] However, the gate stack structure manufactured using the aforementioned existing technology exhibits a reduction in effective channel length after undergoing a re-oxidation process. Summary of the Invention
[0004] In view of the above, embodiments of the present invention provide a method for fabricating a semiconductor device and a semiconductor device to solve at least one problem existing in the background art.
[0005] The technical solution of this invention is implemented as follows:
[0006] This invention provides a method for fabricating a semiconductor device, the method comprising: forming a gate insulating material layer on a substrate;
[0007] A gate material layer is formed on the gate insulating material layer;
[0008] An etching process is performed on the gate material layer and the gate insulating material layer to form the gate layer and the gate insulating layer;
[0009] The gate insulating layer and the gate layer each include a first end and a second end that are opposite to each other in a direction parallel to the channel length. The first end of the gate insulating layer is recessed inward by a predetermined length relative to the first end of the gate layer, and the second end of the gate insulating layer is recessed inward relative to the second end of the gate layer.
[0010] In the above scheme, the method further includes: performing a re-oxidation process, wherein the first end and the second end of the gate layer are oxidized in the re-oxidation process to form an oxide layer.
[0011] In the above scheme, the thickness of the oxide layer in the direction parallel to the channel length is less than or equal to the preset length.
[0012] In the above scheme, the temperature of the re-oxidation process is controlled to be greater than 900°C so that the first end and the second end of the gate layer are fully oxidized to form the oxide layer.
[0013] In the above scheme, the re-oxidation process is controlled to take more than 3 minutes so that the first end and the second end of the gate layer are fully oxidized to form the oxide layer.
[0014] In the above scheme, the etching process performed on the gate material layer and the gate insulating material layer includes: forming a patterned mask layer on the gate material layer;
[0015] Using the patterned mask layer as a mask, an anisotropic etching process is performed on the gate material layer to form the gate layer;
[0016] Using the patterned mask layer as a mask, an isotropic etching process is performed on the gate insulating material layer to form the gate insulating layer.
[0017] In the above scheme, the etching process performed on the gate material layer and the gate insulating material layer includes:
[0018] A patterned mask layer is formed on the gate material layer;
[0019] Using the patterned mask layer as a mask, anisotropic etching is performed on the gate material layer and the gate insulating material layer to form the gate layer and the gate insulating intermediate layer. The gate insulating intermediate layer and the gate layer have the same length in a direction parallel to the channel length.
[0020] A lateral etching process is performed on the gate insulating intermediate layer to form the gate insulating layer.
[0021] In the above scheme, the gate material layer includes a polysilicon material layer and a metal material layer; the gate material layer is formed on the gate insulating material layer, including:
[0022] The polysilicon material layer is formed on the gate insulating material layer; the metal material layer is formed on the polysilicon material layer.
[0023] In the above scheme, the etching process performed on the gate material layer includes: sequentially etching the metal material layer and the polysilicon material layer to obtain a metal layer and a polysilicon layer, wherein the metal layer and the polysilicon layer constitute the gate layer.
[0024] In the above scheme, after forming a gate material layer on the gate insulating material layer, the method further includes: forming a capping material layer on the gate material layer.
[0025] In the above scheme, before performing an etching process on the gate material layer and the gate insulating material layer, the method further includes: performing an etching process on the capping material layer to form a capping layer.
[0026] This invention also provides a semiconductor device, the device comprising: a substrate;
[0027] A gate insulating layer is located on the substrate, the gate insulating layer having a first end and a second end opposite to each other in a direction parallel to the channel length;
[0028] A gate layer, located on the gate insulating layer, the gate layer including a first end and a second end opposite to each other in a direction parallel to the channel length;
[0029] Wherein, the first end of the gate insulating layer is recessed inward by a predetermined length relative to the first end of the gate layer, and the second end of the gate insulating layer is recessed inward relative to the second end of the gate layer.
[0030] In the above scheme, the distance between the first end and the second end of the gate insulating layer is equal to the channel length.
[0031] In the above scheme, both the first end and the second end of the gate layer include an oxide layer formed in the re-oxidation process.
[0032] In the above scheme, the thickness of the oxide layer in the direction parallel to the channel length is less than or equal to the preset length.
[0033] In the above scheme, the gate layer includes a polysilicon layer and a metal layer located on the polysilicon layer, wherein the polysilicon layer and the metal layer have equal lengths in a direction parallel to the channel length.
[0034] In the above scheme, the device further includes a capping layer, which is located on the gate layer.
[0035] The present invention provides a method for fabricating a semiconductor device and a semiconductor device thereof. The method includes: forming a gate insulating material layer on a substrate; forming a gate material layer on the gate insulating material layer; and performing an etching process on the gate material layer and the gate insulating material layer to form a gate layer and a gate insulating layer. The gate insulating layer and the gate layer each include a first end and a second end opposite to each other in a direction parallel to the channel length. The first end of the gate insulating layer relative to the first end of the gate layer, and the second end of the gate insulating layer relative to the second end of the gate layer, are both recessed inward by a predetermined length. Thus, during the subsequent re-oxidation process, the first end and the second end of the gate layer are oxidized to form an oxide layer. This oxide layer does not cover the gate insulating layer, ensuring that the actual gate length is greater than or equal to the length of the gate insulating layer, and preventing a reduction in the effective channel length.
[0036] Additional aspects and advantages of the invention will be set forth in part in the description which follows, and in part will be obvious from the description, or may be learned by practice of the invention. Attached Figure Description
[0037] Figures 1a-1c A process flow diagram of the semiconductor device fabrication method provided in related technologies;
[0038] Figure 2 A flowchart illustrating a method for fabricating a semiconductor device according to an embodiment of the present invention;
[0039] Figures 3a to 3e A process flow diagram of a method for fabricating a semiconductor device provided in an embodiment of the present invention;
[0040] Figures 4a to 4b This is a schematic diagram of etching to form a gate insulating layer and a gate layer according to another embodiment of the present invention;
[0041] Figure 5 This is a schematic diagram of the structure of a semiconductor device provided in an embodiment of the present invention. Detailed Implementation
[0042] Exemplary embodiments of the present invention will now be described in more detail with reference to the accompanying drawings. While exemplary embodiments of the invention are shown in the drawings, it should be understood that the invention can be implemented in various forms and should not be limited to the specific embodiments set forth herein. Rather, these embodiments are provided to enable a more thorough understanding of the invention and to fully convey the scope of the invention to those skilled in the art.
[0043] In the following description, numerous specific details are set forth in order to provide a more thorough understanding of the invention. However, it will be apparent to those skilled in the art that the invention may be practiced without one or more of these details. In other instances, to avoid obscuring the invention, some technical features well-known in the art have not been described; that is, not all features of actual embodiments are described herein, nor are well-known functions and structures described in detail.
[0044] In the accompanying drawings, for clarity, the dimensions of layers, areas, and elements, as well as their relative dimensions, may be exaggerated. The same reference numerals denote the same elements throughout.
[0045] It should be understood that when an element or layer is referred to as "on," "adjacent to," "connected to," or "coupled to" other elements or layers, it may be directly on, adjacent to, connected to, or coupled to other elements or layers, or there may be intervening elements or layers. Conversely, when an element is referred to as "directly on," "directly adjacent to," "directly connected to," or "directly coupled to" other elements or layers, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc., may be used to describe various elements, components, areas, layers, and / or portions, these elements, components, areas, layers, and / or portions should not be limited by these terms. These terms are only used to distinguish one element, component, area, layer, or portion from another element, component, area, layer, or portion. Therefore, without departing from the teachings of this invention, the first element, component, area, layer, or portion discussed below may be referred to as a second element, component, area, layer, or portion. And when a second element, component, area, layer, or portion is discussed, it does not imply that the first element, component, area, layer, or portion necessarily exists in this invention.
[0046] Spatial relation terms such as “below,” “under,” “below,” “under,” “above,” “above,” etc., are used herein for convenience of description to describe the relationship between one element or feature shown in the figure and other elements or features. It should be understood that, in addition to the orientation shown in the figure, spatial relation terms are intended to also include different orientations of the device in use and operation. For example, if the device in the figure is flipped, then the element or feature described as “below,” “under,” or “below” other elements or features will be oriented “above” other elements or features. Therefore, the exemplary terms “below” and “under” can include both above and below orientations. The device may be otherwise oriented (rotated 90 degrees or otherwise) and the spatial descriptive terms used herein will be interpreted accordingly.
[0047] The terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit the invention. When used herein, the singular forms “a,” “an,” and “the” are also intended to include the plural forms unless the context clearly indicates otherwise. It should also be understood that the terms “comprising” and / or “including,” when used in this specification, identify the presence of the stated features, integers, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or groups. When used herein, the term “and / or” includes any and all combinations of the associated listed items.
[0048] Traditional methods for forming gate stack structures include: first, forming a gate insulating material layer and a gate material layer covering the semiconductor substrate on a semiconductor substrate; then, patterning and etching the gate insulating material layer and the gate material layer to form a gate stack structure composed of a gate insulating layer and a gate layer. This etching process can cause some damage to the substrate surface and the side surfaces of the gate stack structure, affecting the integrity and electrical properties of the gate stack structure. For example, a high electric field may be generated in the region near the bottom of the gate insulating layer, affecting the reliability of the gate insulating layer; furthermore, the leakage current between the gate layer and the underlying substrate will also increase.
[0049] In order to repair the etching damage to the gate stack structure in the above etching process, the researchers attempted to perform a re-oxidation process on the etched gate stack structure.
[0050] Figures 1a to 1c This is a process flow diagram for the fabrication of semiconductor devices provided in related technologies.
[0051] First, such as Figure 1a As shown, a gate insulating material layer 11' covering the upper surface of the substrate 10 is first formed on the substrate 10, and then a gate material layer 12' is formed on the gate insulating material layer 11'. After forming the gate material layer 12', a capping material layer 13' may also be formed above the gate material layer 12'.
[0052] Next, as Figure 1b As shown, a patterned etching process is performed on the gate insulating material layer 11', the gate material layer 12', and the capping material layer 13' to form a gate stack structure including the gate insulating layer 11, the gate layer 12, and the capping layer 13. Specifically, before etching, a patterned mask layer (not shown in the figure) can be formed on the capping material layer 13', and then the etching process is performed. The initial length of both the gate insulating layer 11 and the gate layer 12 is L1.
[0053] During the etching process to form the gate stack structure, a certain degree of damage will occur on the surface of the substrate 10 and the side surface of the gate stack structure. This damage will cause changes in the characteristics of the device, such as unstable threshold voltage (Vth) or reduced reliability.
[0054] Therefore, a repair process is needed for the gate stack structure that has suffered etch damage. Currently, the commonly used repair process is gate re-oxidation. This gate re-oxidation process can not only repair the etch damage of the gate stack structure but also increase the thickness of the gate oxide in the gate edge region, thereby reducing GIDL leakage. Figure 1cAs shown, a re-oxidation process is performed on the gate stack structure, and both ends of the gate layer are oxidized to form oxide layers. At this time, the length of the gate insulating layer is L1, and the actual gate length becomes L3, where L3<L1. That is to say, the actual gate length is less than the length of the gate insulating layer, which means the actual channel length is less than the pre-designed channel length, and the effective channel length of the transistor is reduced.
[0055] Based on this, the following technical solutions of the embodiments of the present invention are proposed.
[0056] The embodiments of the present invention provide a method for fabricating a semiconductor device, for details, please refer to Figure 2 . As shown in the figure, the method includes the following steps:
[0057] Step 201: forming a gate insulating material layer on a substrate;
[0058] Step 202: forming a gate material layer on the gate insulating material layer;
[0059] Step 203: performing an etching process on the gate material layer and the gate insulating material layer to form a gate layer and a gate insulating layer;
[0060] Wherein, the gate insulating layer and the gate layer each include a first end and a second end opposite to each other in the direction parallel to the channel length, and the first end of the gate insulating layer is recessed inward by a preset length relative to the first end of the gate layer, and the second end of the gate insulating layer is recessed inward by the preset length relative to the second end of the gate layer.
[0061] In this method, in the direction parallel to the channel length, both ends of the gate layer have protruding length portions relative to both ends of the gate insulating layer, that is, the gate layer has a longer initial length than the gate insulating layer, so that when the subsequent re-oxidation process is performed, the first end and the second end of the gate layer are oxidized to form oxide layers, and the oxide layers will not cover the gate insulating layer, making the actual gate length the same as the preset channel length, and will not cause the reduction of the effective channel length.
[0062] To make the above objects, features and advantages of the present invention more clearly understood, the specific embodiments of the present invention will be described in detail below with reference to the accompanying drawings. In the detailed description of the embodiments of the present invention, for the convenience of explanation, the schematic diagrams may partially enlarge the structure not according to the general scale, and the schematic diagrams are only examples, which should not limit the protection scope of the present invention.
[0063] Figures 3a to 3e is a process flowchart of the method for fabricating a semiconductor device provided by the embodiment of the present invention.
[0064] First, as in Figure 3aAs shown, step 201 is performed to form a gate insulating material layer 21' on the substrate 20. It is understood that in some embodiments, other structures, such as a buffer layer, may be included between the substrate 20 and the gate insulating material layer 21', which is not specifically limited here.
[0065] In the actual process, the substrate is located at the bottom of the gate insulating material layer 21', and can play a supporting role in the subsequent process of forming the stacked structure.
[0066] Here, the substrate can be a semiconductor substrate; specifically, it includes at least one elemental semiconductor material (e.g., a silicon (Si) substrate, a germanium (Ge) substrate, etc.), at least one III-V compound semiconductor material (e.g., a gallium nitride (GaN) substrate, a gallium arsenide (GaAs) substrate, an indium phosphide (InP) substrate, etc.), at least one II-VI compound semiconductor material, at least one organic semiconductor material, or other semiconductor materials known in the art. In one specific embodiment, the substrate is a silicon substrate.
[0067] The gate insulating material layer can be a high dielectric constant material, which provides electrical insulation between the subsequently formed gate layer and the substrate. The gate insulating material layer can be formed from materials such as silicon oxide.
[0068] Next, proceed to step 202, as follows: Figure 3b As shown, a gate material layer 22' is formed on the gate insulating material layer 21'.
[0069] In one embodiment, the gate material layer 22' includes a polysilicon material layer 221' and a metal material layer 222'; forming the gate material layer 22' on the gate insulating material layer 21' includes: forming the polysilicon material layer 221' on the gate insulating material layer 21'; and forming the metal material layer 222' on the polysilicon material 221'. However, this is not a limitation; the gate material layer 22' may also include only one of the polysilicon material layer 221' and the metal material layer 222', i.e., the gate material layer 22' can be either a polysilicon material layer 221' or a metal layer 222'. In a specific embodiment, the metal material layer 222' includes, but is not limited to, tungsten metal, metal silicide, and tungsten nitride, wherein the metal silicide can be TiSi2, CoSi2, and NiSi2, etc.
[0070] In one embodiment, such as Figure 3b As shown, after forming the gate material layer 22', a capping material layer 23' can also be formed on top of the gate material layer 22'. The capping material layer 23' is used to protect the gate material layer 22', and the capping material layer 23' includes, but is not limited to, silicon oxide, silicon nitride, etc.
[0071] The gate insulating material layer 21' and the gate material layer 22' can be formed using one or more thin film deposition processes; specifically, the thin film deposition processes include, but are not limited to, chemical vapor deposition (CVD), plasma enhanced chemical vapor deposition (PECVD), atomic layer deposition (ALD), or combinations thereof.
[0072] Continuing with step 203, an etching process is performed on the gate material layer 22' and the gate insulating material layer 21' to form the gate layer 22 and the gate insulating layer 21, as follows. Figures 3c-3d As shown.
[0073] The gate insulating layer 21 and the gate layer 22 each include a first end and a second end that are opposite to each other in a direction parallel to the channel length. The first end 21a of the gate insulating layer 21 is recessed inward by a predetermined length ΔL relative to the first end 22a of the gate layer 22, and the second end 21b of the gate insulating layer 21 is recessed inward by a predetermined length ΔL relative to the second end 22b of the gate layer 22.
[0074] In one embodiment, an etching process is performed on the gate material layer 22' and the gate insulating material layer 21', including:
[0075] A patterned mask layer (not shown) is formed on the gate material layer 22'; using the patterned mask layer as a mask, an anisotropic etching process is performed on the gate material layer 22' to form the gate layer 22, as shown below. Figure 3c As shown; continuing with the patterned mask layer as a mask, an isotropic etching process is performed on the gate insulating material layer 21' to form the gate insulating layer 21, as shown. Figure 3d As shown.
[0076] In this embodiment, using the same mask layer but different etching methods to etch the gate material layer 22' and the gate insulating material layer 21' allows the two ends 21a and 21b of the finally formed gate insulating layer 21 to be recessed inward by a predetermined length ΔL relative to the two ends 22a and 22b of the gate layer 22. In other words, the first end 21a of the finally formed gate insulating layer 21 is recessed inward by a predetermined length ΔL relative to the first end 22a of the gate layer 22, and the second end 21b of the gate insulating layer 21 is recessed inward by a predetermined length ΔL relative to the second end 22b of the gate layer 22. It should be noted that the value of the predetermined length ΔL is not particularly limited, and it is related to the thickness of the oxide layer formed in the subsequent re-oxidation process.
[0077] In one specific embodiment, an anisotropic etching process is performed on the gate material layer 22', including: sequentially etching the metal material layer 222' and the polysilicon material layer 221' to obtain the metal layer 222 and the polysilicon layer 221. The first end 22a of the gate layer 22 may include the first end 221a of the polysilicon layer 221 and the first end 222a of the metal layer, and the second end 22b of the gate layer 22 may include the second end 221b of the polysilicon layer 221 and the second end 222b of the metal layer, wherein the first end 222a of the metal layer 222 is flush with the first end 221a of the polysilicon layer 221 in the vertical direction, and the second end 222b of the metal layer 222 is flush with the second end 221b of the polysilicon layer 221 in the vertical direction.
[0078] In a specific implementation, the anisotropic etching process includes, but is not limited to, dry etching processes, such as plasma etching. The isotropic etching process includes, but is not limited to, wet etching processes, such as etching with acidic solutions.
[0079] Figures 4a to 4b This is a schematic diagram illustrating the etching process for forming a gate insulating layer 21 and a gate layer 22, according to another embodiment of the present invention. As shown, the etching process performed on the gate material layer 22' and the gate insulating material layer 21' includes:
[0080] A patterned mask layer (not shown) is formed on the gate material layer 22';
[0081] Using the patterned mask layer as a mask, anisotropic etching is performed on the gate material layer 22' and the gate insulating material layer 21' to form the gate layer 22 and the gate insulating intermediate layer 21'. The gate layer 22 and the gate insulating intermediate layer 21' have the same length in the direction parallel to the channel length, such as... Figure 4a As shown;
[0082] A lateral etching process is performed on the gate insulating intermediate layer 21” to form the gate insulating layer 21, as follows: Figure 4b As shown.
[0083] In this embodiment, a two-step etching process is used to etch the gate material layer 22' and the gate insulating material layer 21', which allows the two ends 21a and 21b of the finally formed gate insulating layer 21 to be recessed inward by a predetermined length ΔL relative to the two ends 22a and 22b of the gate layer 22. In other words, the first end 21a of the finally formed gate insulating layer 21 is recessed inward by a predetermined length ΔL relative to the first end 22a of the gate layer 22, and the second end 21b of the gate insulating layer 21 is recessed inward by a predetermined length ΔL relative to the second end 22b of the gate layer 22. It should be noted that the value of the predetermined length ΔL is not particularly limited, and it is related to the thickness of the oxide layer formed in the subsequent re-oxidation process.
[0084] In actual manufacturing processes, the anisotropic etching process can be a plasma etching process. The lateral etching process can be a wet etching process.
[0085] See also Figure 3c In one embodiment, before etching the gate material layer 22' and the gate insulating material layer 21', a step of etching the capping material layer 23' to form the capping layer 23 may be included. The etching process of the capping layer 23 can be the same as the etching process of the gate layer 22, and will not be described in detail here.
[0086] After performing step 203, in one embodiment, as follows: Figure 3e As shown, the method further includes performing a re-oxidation process, in which the first end 22a and the second end 22b of the gate layer 22 are oxidized to form an oxide layer 223. In a specific embodiment, the thickness of the oxide layer 223 in the direction parallel to the channel length is less than or equal to the preset length ΔL. Furthermore, the re-oxidation process can also repair damage to the surface of the substrate 20 and the sidewalls of the gate insulating layer 21, and can also increase the thickness of the oxide layer 223 located at both ends of the gate layer 22, thereby reducing gate-induced drain leakage current (GIDL) leakage.
[0087] In one embodiment, by controlling the re-oxidation temperature to be greater than 900°C, the first end 22a and the second end 22b of the gate layer 22 are sufficiently oxidized to form the oxide layer 223, preventing further oxidation caused by insufficient oxidation of the sidewalls of the gate layer 22 in subsequent processes.
[0088] In another embodiment, by controlling the re-oxidation process time to be greater than 3 minutes, the first end 22a and the second end 22b of the gate layer 22 are sufficiently oxidized to form the oxide layer 223, preventing further oxidation caused by insufficient oxidation of the sidewalls of the gate layer 22 in subsequent processes.
[0089] After the above re-oxidation process, the actual gate length changes due to the formation of the oxide layer, shortening from the initial design length L2 to L3 after the re-oxidation process. By controlling the two ends of the gate insulating layer to be recessed inward by a preset length ΔL relative to the two ends of the gate layer in step 203, the final actual gate length is greater than or equal to the length of the gate insulating layer, i.e., L3≥L1.
[0090] Therefore, through the design of the embodiments of the present invention, the effective channel length of the device will not be reduced due to the formation of oxide layer on the sidewall of the gate layer after the gate stack structure is subjected to the re-oxidation process.
[0091] This invention also provides a semiconductor device, such as... Figure 5 As shown, the semiconductor device includes:
[0092] Substrate 20;
[0093] A gate insulating layer 21 is located on the substrate 20, and the gate insulating layer 21 includes a first end 21a and a second end 21b that are opposite to each other in a direction parallel to the channel length;
[0094] The gate layer 22 is located on the gate insulating layer 21, and the gate layer 21 also includes a first end 22a and a second end 22b that are opposite to each other in a direction parallel to the channel length.
[0095] Wherein, the first end 21a of the gate insulating layer 21 is recessed inward by a predetermined length ΔL relative to the first end 22a of the gate layer 22, and the second end 21b of the gate insulating layer 21 is recessed inward relative to the second end 22b of the gate layer 22.
[0096] In some embodiments, the device further includes a capping layer 23, which is located on the gate layer 22 to protect the gate layer 22, wherein the capping layer 23 includes, but is not limited to, silicon oxide, silicon nitride, etc.
[0097] In some embodiments, a buffer layer or other structure may be formed between the substrate 20 and the gate insulating layer 21, without further restrictions.
[0098] In some embodiments, sidewall structures may be formed on the sidewalls of the gate layer 22 and the gate insulating layer 21 to protect the gate layer 22 and the gate insulating layer 21. Furthermore, the sidewall structures may also be used to maintain electrical insulation between the gate layer 22 and other structures. The sidewall materials include, but are not limited to, silicon nitride (SiN) and silicon carbide (SiC).
[0099] The gate insulating layer 21 and the gate layer 22 can be formed using one or more thin-film deposition processes; specifically, the thin-film deposition processes include, but are not limited to, chemical vapor deposition (CVD), plasma-enhanced chemical vapor deposition (PECVD), atomic layer deposition (ALD), or combinations thereof. The gate insulating layer 21 can be made of a high-dielectric-constant material, including but not limited to silicon oxide, and serves to provide electrical insulation between the subsequently formed gate layer 22 and the substrate 20.
[0100] See also Figure 5 The distance between the first end 21a and the second end 21b of the gate insulating layer 21 is L1, which is equal to the channel length, i.e., the channel length is L1.
[0101] In one embodiment, the gate layer 22 includes a polysilicon layer 221 and a metal layer 222, and the polysilicon layer 221 and the metal layer 222 have equal lengths in a direction parallel to the channel length. Specifically, the first end 22a of the gate layer 22 includes the first end 221a of the polysilicon layer 221 and the first end 222a of the metal layer 222; the second end 22b of the gate layer 22 includes the second end 221b of the polysilicon layer 221 and the second end 222b of the metal layer 222. In this embodiment, the first end 222a of the metal layer 222 is flush with the first end 221a of the polysilicon layer 221 in a vertical direction, and the second end 222b of the metal layer 222 is flush with the second end 221b of the polysilicon layer 221 in a vertical direction, meaning the polysilicon layer 221 and the metal layer 222 have equal lengths. The materials used to form the metal layer 222 include, but are not limited to, tungsten metal, metal silicide, and tungsten nitride, wherein the metal silicide can be TiSi2, CoSi2, and NiSi2.
[0102] In one embodiment, both the first end 22a and the second end 22b of the gate layer 22 include an oxide layer 223 formed in the re-oxidation process. That is, the first end 221a of the polysilicon layer 221 and the first end 222a of the metal layer 222, as well as the second end 221b of the polysilicon layer 221 and the second end 222b of the metal layer 222, all include an oxide layer 223.
[0103] In one embodiment, the thickness of the oxide layer 223 in the direction parallel to the channel length is less than or equal to the preset length ΔL. In this embodiment, the preset length ΔL is the length by which the first end 21a of the gate insulating layer 21 is recessed relative to the first end 22a of the gate layer 22, and the second end 21b of the gate insulating layer 21 is recessed relative to the second end 22b of the gate layer 22.
[0104] It should be understood that the length of the gate layer involved in the embodiments of the present invention, as well as the lengths of the polysilicon layer and metal layer included in the gate layer, are not specifically limited and can be flexibly handled according to actual process requirements. Furthermore, the thickness of the oxide layer formed after the gate layer undergoes a re-oxidation process is not overly limited and can be flexibly handled according to actual process requirements. The gate stack structure involved in the embodiments of the present invention can be applied to DRAM structures or other semiconductor devices, and is not further limited here.
[0105] In summary, in this embodiment of the invention, the two ends of the gate insulating layer are recessed inward by a predetermined length ΔL relative to the two ends of the gate layer. After the re-oxidation process, the oxide layer formed on the sidewall of the gate layer will not cover the gate insulating layer, thereby ensuring that the final gate stack structure will not suffer a reduction in the effective channel length due to the formation of the oxide layer on the sidewall of the gate layer. Figure 1c Compared with the related technical content, the technical solution provided by the embodiments of the present invention solves the problem that the effective channel length is shortened due to the oxidation of the gate layer sidewall after the re-oxidation process, thereby improving the working stability of semiconductor devices.
[0106] In addition, by designing the temperature and time required for the re-oxidation process, the first and second ends of the gate layer can be fully oxidized to form an oxide layer, preventing further oxidation caused by insufficient oxidation of the gate layer sidewalls in subsequent processes.
[0107] It should be noted that the embodiments of the semiconductor device fabrication method provided by the present invention and the embodiments of the semiconductor device belong to the same concept; the technical features in the technical solutions described in each embodiment can be arbitrarily combined without conflict.
[0108] The above description is merely a preferred embodiment of the present invention and is not intended to limit the scope of protection of the present invention. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of the present invention should be included within the scope of protection of the present invention.
Claims
1. A method for fabricating a semiconductor device, characterized in that, The method includes: A gate insulating material layer is formed on the substrate; A gate material layer is formed on the gate insulating material layer; An etching process is performed on the gate material layer and the gate insulating material layer to form the gate layer and the gate insulating layer; The gate insulating layer and the gate layer each include a first end and a second end that are opposite to each other in a direction parallel to the channel length. The first end of the gate insulating layer is recessed inward by a predetermined length relative to the first end of the gate layer, and the second end of the gate insulating layer is recessed inward by a predetermined length relative to the second end of the gate layer. A re-oxidation process is performed, in which the first end and the second end of the gate layer are oxidized to form an oxide layer, the thickness of which in the direction parallel to the channel length is less than or equal to the preset length.
2. The method according to claim 1, characterized in that, The temperature of the re-oxidation process is controlled to be greater than 900°C so that the first end and the second end of the gate layer are fully oxidized to form the oxide layer.
3. The method according to claim 1, characterized in that, The re-oxidation process is controlled to last for more than 3 minutes so that the first and second ends of the gate layer are fully oxidized to form the oxide layer.
4. The method according to claim 1, characterized in that, An etching process is performed on the gate material layer and the gate insulating material layer, including: A patterned mask layer is formed on the gate material layer; Using the patterned mask layer as a mask, an anisotropic etching process is performed on the gate material layer to form the gate layer; Using the patterned mask layer as a mask, an isotropic etching process is performed on the gate insulating material layer to form the gate insulating layer.
5. The method according to claim 1, characterized in that, An etching process is performed on the gate material layer and the gate insulating material layer, including: A patterned mask layer is formed on the gate material layer; Using the patterned mask layer as a mask, anisotropic etching is performed on the gate material layer and the gate insulating material layer to form the gate layer and the gate insulating intermediate layer. The gate insulating intermediate layer and the gate layer have the same length in a direction parallel to the channel length. A lateral etching process is performed on the gate insulating intermediate layer to form the gate insulating layer.
6. The method according to claim 1, characterized in that, The gate material layer includes a polysilicon material layer and a metal material layer; Forming a gate material layer on the gate insulating material layer includes: The polysilicon material layer is formed on the gate insulating material layer; the metal material layer is formed on the polysilicon material layer.
7. The method according to claim 6, characterized in that, An etching process is performed on the gate material layer, including: sequentially etching the metal material layer and the polysilicon material layer to obtain a metal layer and a polysilicon layer, wherein the metal layer and the polysilicon layer constitute the gate layer.
8. The method according to claim 1, characterized in that, After forming a gate material layer on the gate insulating material layer, the method further includes forming a capping material layer on the gate material layer.
9. The method according to claim 8, characterized in that, Before performing an etching process on the gate material layer and the gate insulating material layer, the method further includes: performing an etching process on the capping material layer to form a capping layer.
10. A semiconductor device, characterized in that, The device includes: Substrate; A gate insulating layer is located on the substrate, the gate insulating layer having a first end and a second end opposite to each other in a direction parallel to the channel length; A gate layer is located on the gate insulating layer. The gate layer includes a first end and a second end opposite to each other in a direction parallel to the channel length. Both the first end and the second end of the gate layer include an oxide layer formed in the re-oxidation process. Wherein, the first end of the gate insulating layer is recessed inward by a predetermined length relative to the first end of the gate layer, and the second end of the gate insulating layer is recessed inward by a predetermined length relative to the second end of the gate layer, and the distance between the first end and the second end of the gate insulating layer is equal to the channel length.
11. The device according to claim 10, characterized in that, The thickness of the oxide layer in the direction parallel to the channel length is less than or equal to the preset length.
12. The device according to claim 10, characterized in that, The gate layer includes a polysilicon layer and a metal layer located on the polysilicon layer, wherein the polysilicon layer and the metal layer have equal lengths in a direction parallel to the channel length.
13. The device according to claim 10, characterized in that, The device further includes a capping layer located on the gate layer.
Citation Information
Patent Citations
Semiconductor device and production method thereof
CN103545366A
Transistor element having an anisotropic high-k gate dielectric
CN1692474A