A method for synthesizing 2-methyl-1,4-naphthoquinone by oxidation using a cobalt polymerized phthalonitrile catalyst

By catalyzing the oxidation of 2-methylnaphthalene under mild conditions by polymerized phthalonitrile cobalt catalyst, the problems of large amount of catalyst and environmental pollution in the prior art are solved, and high-efficiency and low-cost 2-methyl-1,4-naphthalene are achieved. Quinone preparation, has high conversion and selectivity, and the catalyst is reusable and suitable for industrial production.

CN115974670BActive Publication Date: 2024-11-05NANJING TECH UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310032584.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-01-10
Publication Date
2024-11-05
Estimated Expiration
2043-01-10

AI Technical Summary

Technical Problem

In the prior art, the synthesis process of 2-methyl-1,4-naphthoquinone has problems such as large catalyst usage, low reaction efficiency, and serious environmental pollution, and the catalyst is difficult to recover and separate, resulting in high costs and serious pollution.

Method used

Using polymerized phthalonitrile cobalt catalyst, 2-methyl-1,4-naphthalene quinone was prepared by reacting 2-methylnaphthalene with hydrogen peroxide under mild conditions, and the cobalt mass load of the catalyst was 6.2%-19.7%. And catalyzed by specific solvents and reaction conditions, the catalyst can be reused.

Benefits of technology

It achieves high conversion and high selectivity, mild reaction conditions, low catalyst usage, and has the advantages of green and environmental protection. It is suitable for industrial production, and the catalyst is stable and easy to recover.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004047799430000051
    Figure BDA0004047799430000051
Patent Text Reader

Abstract

The invention relates to a method for synthesizing 2-methyl-1,4-naphthoquinone by oxidation of a polymerized phthalonitrile cobalt catalyst, the method comprising the steps of: using 4,4'-biphenyl diphenol and 4-nitrophthalonitrile to synthesize 4,4'-biphenyl di(3,4-dicyanophenyl) ether as a precursor, coordinating the precursor with cobalt, and obtaining a polymerized cyanine cobalt catalyst. The catalyst has high hydrogen peroxide utilization rate and is easy to recycle. In a solvent, 2-methylnaphthalene, hydrogen peroxide and a polymerized phthalonitrile cobalt catalyst are added, and the product 2-methyl-1,4-naphthoquinone is obtained by reaction at a specific temperature. The process conditions are mild and suitable for industrial production.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a process for preparing 2-methyl-1,4-naphthoquinone by catalytic oxidation of a polymerized cobalt phthalocyanine catalyst. Background Art

[0002] 2-Methyl-1,4-naphthoquinone (2-MNQ for short) is an important intermediate with a wide range of uses in medicine and feed. This compound can be used as an additive to promote livestock growth and development feed; it is also the most important fat-soluble antioxidant in biological systems, which can promote the metabolism of high-energy compounds in the human body, and has the effect of diuresis and enhancing liver detoxification. With the rapid development of the pharmaceutical and animal husbandry industries, V K The demand for 2-MNQ compounds has increased dramatically. Therefore, the research on 2-MNQ synthesis technology has very important practical significance.

[0003] Patent CN 105839134 A discloses a method for preparing 2-MNQ by indirect electro-oxidation. Although this process uses cerium salt oxidation, it requires complex treatment of the cerium salt solution before electrolysis. After heating, 2-MNQ is in an oil phase, while the cerium salt solution is in an aqueous phase. The two-phase reaction contact surface is small, the reaction time is long, and it is easy to cause partial 2-MNQ peroxidation. The process is complicated, not conducive to industrialization, and the cost is high; Patent CN 101575276 proposes a method for synthesizing 2-methyl-1,4-naphthoquinone using an ionic liquid as a catalyst. This method solves environmental pollution and other problems, but it is difficult to completely separate the ionic liquid from the reaction product, and the residual catalyst will cause pollution to the product.

[0004] The most commonly used method for synthesizing 2-MNQ in industry is: 2 SO 4 Under acidic conditions, CrO 3 Direct oxidation of 2-methylnaphthalene to prepare 2-MNQ (RUS 2420512; IN 2004DE 00669; Med. Chem.

[0005] Comm, 2014, 5, 923). The final conversion rate is 42-65%, but during the reaction, the generation of chromium-containing wastewater and chromium-containing solid wastes causes serious environmental pollution, making it unsuitable for industrial application.

[0006] Urus Serhan et al. synthesized a novel graphene oxide (GO) loaded with bis(diphenylphosphinoethyl)amino [GO@CHONHRN(CH 2 PPh 2 ) 2] type ligand and its palladium (II) and platinum (II) complexes (Chem. Eng. J. 2016, 306, 961), directly oxidize 2-methylnaphthalene to 2-MNQ, and can achieve 95% conversion rate and 60% selectivity. However, the preparation method of the catalyst is complicated and the economic cost is high.

[0007] Guoli Zi et al. used lanthanum-doped MCM-41 as a catalyst for liquid-phase oxidation of 2-methylnaphthalene to 2-methyl-1,4-naphthoquinone (Catalysis Communications 49 (2014) 10–14). Although a high conversion rate of the substrate (95.8%) was achieved, the selectivity was poor (69.3%). Lanthanum is a precious rare earth element with a high price. At the same time, lanthanum is highly toxic to organisms.

[0008] Therefore, the preparation of low-cost, green, stable and reusable catalysts is particularly important for industrial needs. Summary of the invention

[0009] The purpose of the present invention is to improve the deficiencies of the prior art and provide a method for synthesizing 2-methyl-1,4-naphthoquinone by oxidation using a cobalt polyphthalonitrile catalyst. The present invention aims to solve the problems of large catalyst dosage, low reaction efficiency and serious environmental pollution in the prior art, and provides a method for preparing 2-methyl-1,4-naphthoquinone by oxidation using 2-methylnaphthalene, which has mild reaction conditions, high reaction yield, low catalyst dosage and is environmentally friendly.

[0010] The technical solution of the present invention is: a method for synthesizing 2-methyl-1,4-naphthoquinone by oxidation of a polymerized cobalt phthalonitrile catalyst, the specific steps of which are as follows:

[0011] A. Preparation of polymerized phthalonitrile cobalt catalyst: In an inert gas, 4,4'-biphenol and 4-nitrophthalonitrile are dissolved in N,N-dimethylformamide, anhydrous potassium carbonate is added, stirred, filtered, washed, and dried to obtain a precursor; the precursor and a cobalt compound are heated and reacted in a soluble solvent, and after cooling, filtered, washed, and dried to obtain a catalyst, wherein the mass loading of cobalt is 6.2%-19.7%;

[0012] B. Add 2-methylnaphthalene, hydrogen peroxide and polymerized cobalt phthalonitrile catalyst into a solvent, and react in an oil bath at 30-50° C. for 8-12 hours to obtain the product 2-methyl-1,4-naphthoquinone.

[0013] After stopping heating, the mixture is cooled to room temperature, and the conversion rate of 2-methylnaphthalene and the selectivity of 2-methyl-1,4-naphthoquinone are detected by gas chromatography. Finally, the catalyst is separated by centrifugation, and the catalyst is washed with acetonitrile and dried in vacuum before being reused.

[0014] Preferably, the cobalt compound in step A is cobalt acetate; the soluble solvent is N,N-dimethylethanolamine; and the inert gas is argon.

[0015] Preferably, the stirring time described in step A is 10-48h; the filtration temperature is 0-30°C; the heating reaction temperature is 120°C-160°C; the heating reaction time is 6-10h; the molar ratio of 4,4'-biphenol to 4-nitrophthalonitrile is 1:(0.8-3); the ratio of anhydrous potassium carbonate to 4,4'-biphenol is 1:1-3:1; and the molar ratio of the precursor to the cobalt compound is 1:(0.25-1).

[0016] Preferably, the solvent in step B is acetonitrile; the amount of the cobalt polyphthalonitrile catalyst is 28%-43% of the substrate mass; the oxidant is hydrogen peroxide, and the molar amount of the oxidant is 4-8 times the equivalent of the substrate 2-methylnaphthalene.

[0017] Beneficial effects:

[0018] The catalyst provided by the invention has good stability and high activity. The catalyst has high activity and high selectivity for preparing 2-methyl-1,4-naphthoquinone from 2-methylnaphthalene, is easy to recycle and reuse, and the reaction has the advantages of being green and environmentally friendly, and is very suitable for industrial production. DETAILED DESCRIPTION

[0019] Implementation Case 1:

[0020] In an Ar atmosphere, 0.02mmol (3.74mg) of 4,4'-biphenyldiphenol and 0.04mmol (6.9mg) of 4-nitrophthalonitrile were dissolved in 20ml of N,N-dimethylformamide and stirred for 10min. 0.06mmol of anhydrous potassium carbonate was added to the reaction solution and stirred for 10h. The yellow precipitate was filtered out at 0℃ and washed with deionized water and anhydrous ether until neutral. The precursor was obtained by vacuum drying at 60℃ for 12h. 1mmol (440mg) of the precursor and 0.25mmol (62.25mg) of cobalt acetate were added to 6ml of N,N-dimethylethanolamine. The reaction was carried out at 160℃ in a reactor for 6h, and the mixture was cooled to room temperature and filtered. The filtrate was washed with anhydrous methanol, acetone and deionized water until the filtrate was colorless, and dried in a vacuum oven at 60℃ for 12h to obtain catalyst M1 (6.2% Co).

[0021] Implementation Case 2:

[0022] In an Ar atmosphere, 0.02mmol (3.74mg) of 4,4'-biphenyldiphenol and 0.06mmol (10.35mg) of 4-nitrophthalonitrile were dissolved in 30ml of N,N-dimethylformamide and stirred for 10min. 0.06mmol of anhydrous potassium carbonate was added to the reaction solution and stirred for 24h. The yellow precipitate was filtered out at 30℃ and washed with deionized water and anhydrous ether until neutral. The precursor was obtained by vacuum drying at 60℃ for 8h. 1mmol (440mg) of the precursor and 0.75mmol (186.75mg) of cobalt acetate were added to 10ml of N,N-dimethylethanolamine. The reaction was carried out at 130℃ in a reactor for 10h, and the reaction was cooled to room temperature and filtered. The filtrate was washed with anhydrous methanol, acetone and deionized water until the filtrate was colorless, and dried in a vacuum oven at 80℃ for 6h to obtain catalyst M2 (15.4% Co).

[0023] Implementation Case 3:

[0024] In an Ar atmosphere, 0.04mmol (7.48mg) of 4,4'-biphenyldiphenol and 0.05mmol (8.625mg) of 4-nitrophthalonitrile were dissolved in 25ml of N,N-dimethylformamide and stirred for 60min. 0.04mmol of anhydrous potassium carbonate was added to the reaction solution and stirred for 48h. The yellow precipitate was filtered out at 0℃ and washed with deionized water and anhydrous ether until neutral. The precursor was obtained by vacuum drying at 80℃ for 5h. 1mmol (440mg) of the precursor and 1mmol (249mg) of cobalt acetate were added to 15ml of N,N-dimethylethanolamine. The reaction was carried out at 120℃ in a reactor for 10h, and the mixture was cooled to room temperature and filtered. The filtrate was washed with anhydrous methanol, acetone and deionized water until the filtrate was colorless, and dried in a vacuum oven at 60℃ for 6h to obtain catalyst M3 (19.7% Co).

[0025] Implementation Case 4:

[0026] In an Ar atmosphere, 0.04mmol (7.48mg) of 4,4'-biphenyldiphenol and 0.05mmol (8.625mg) of 4-nitrophthalonitrile were dissolved in 50ml of DMF, and 0.08mmol of anhydrous potassium carbonate was added to the reaction solution and stirred for 15h. The yellow precipitate was filtered out at 0℃ and washed with deionized water and anhydrous ether until neutral. The precursor was obtained by vacuum drying at 60℃ for 10h. 1mmol (440mg) of the precursor and 0.25mmol (62.25mg) of cobalt acetate were added to 6ml of N,N-dimethylformamide. The reaction was carried out at 160℃ in a reactor for 6h, and the reaction was cooled to room temperature and filtered. The filtrate was washed with anhydrous methanol, acetone and deionized water until the filtrate was colorless, and dried in a vacuum oven at 60℃ for 12h to obtain catalyst M4 (7.5% Co).

[0027] Implementation Case 5:

[0028] In an Ar atmosphere, 0.03mmol (5.61mg) of 4,4'-biphenyldiphenol and 0.06mmol (10.35mg) of 4-nitrophthalonitrile were dissolved in 50ml of DMF and stirred for 10min. 0.06mmol of anhydrous potassium carbonate was added to the reaction solution and stirred for 24h. The yellow precipitate was filtered out at 25°C and washed with deionized water and anhydrous ether until neutral. The precursor was obtained by vacuum drying at 60°C for 12h. 1mmol (440mg) of the precursor and 0.5mmol (124.5mg) of cobalt acetate were added to 6ml of N, N-dimethylethanolamine. The reaction was carried out at 160°C in a reactor for 6h, and the reaction was cooled to room temperature and filtered. The filtrate was washed with anhydrous methanol, acetone and deionized water until the filtrate was colorless, and dried in a vacuum oven at 60°C for 12h to obtain catalyst M5 (10.5% Co).

[0029] Implementation Case 6:

[0030] In an Ar atmosphere, 0.03mmol (5.61mg) of 4,4'-biphenyldiphenol and 0.08mmol (13.8mg) of 4-nitrophthalonitrile were dissolved in 50ml of DMF and stirred for 10min. 0.06mmol of anhydrous potassium carbonate was added to the reaction solution and stirred for 36h. The yellow precipitate was filtered out at 0℃ and washed with deionized water and anhydrous ether until neutral. The precursor was obtained by vacuum drying at 100℃ for 3h. 1mmol (440mg) of the precursor and 0.25mmol (62.25mg) of cobalt acetate were added to 6ml of N, N-dimethylethanolamine. The reaction was carried out at 130℃ in a reactor for 10h, and the reaction was cooled to room temperature and filtered. The filtrate was washed with anhydrous methanol, acetone and deionized water until the filtrate was colorless, and dried in a vacuum oven at 100℃ for 3h to obtain catalyst M6 (6.3% Co).

[0031] Implementation Case 7: The prepared catalyst is used for the preparation of 2-methyl-1,4-naphthoquinone.

[0032] In a Shrek tube, add 1mmol (142mg) 2-methylnaphthalene, 5mmol hydrogen peroxide, 1ml acetonitrile and catalyst M3, and the amount of catalyst is 50mg. Put a balloon on the branch to release the pressure. Place it in a 50℃ oil pan to react for 12h. After the reaction is completed, take out the tube and cool it to room temperature, centrifuge it, and use anhydrous magnesium sulfate to remove water from the clarified supernatant. Use gas chromatography to detect the conversion rate of 2-methylnaphthalene and the selectivity of 2-methyl-1,4-naphthoquinone. Finally, filter and wash the catalyst with ethanol, and it can be reused after drying. The reaction formula is as follows:

[0033]

[0034] The processes using catalysts M2, M3, M4, M5, and M6 are consistent with the process flow of M1, and the reaction results are listed in Table 1.

[0035] Table 1:

[0036] catalyst 2-Methylnaphthalene conversion Yield of 2-methyl-1,4-naphthoquinone M1 55% 47% M2 46% 38% M3 52% 42% M4 43% 32% M5 49% 40% M6 40% 33%

[0037] Catalyst M3 was used in Example 8, the reaction temperature was changed, and the results are listed in Table 2.

[0038] Table 2:

[0039] temperature 2-Methylnaphthalene conversion Yield of 2-methyl-1,4-naphthoquinone 30℃ 45% 36% 40℃ 52% 46% 50℃ 50% 43%

[0040] Catalyst M1 was used in Example 7, and the molar amount of hydrogen peroxide was changed. The results are listed in Table III.

[0041] Table 3:

[0042] Amount of hydrogen peroxide 2-Methylnaphthalene conversion Yield of 2-methyl-1,4-naphthoquinone 4mmol 46% 38% 6mmol 55% 47% 8mmol 50% 42%

[0043] Catalyst M1 was used in Example 7, and the reaction time was changed. The results are listed in Table 4.

[0044] Table 4:

[0045] Reaction time 2-Methylnaphthalene conversion Yield of 2-methyl-1,4-naphthoquinone 8h 50% 42% 10h 52% 43% 12h 52% 43%

[0046] Implementation Case 8:

[0047] In a Shrek tube, add 1mmol (142mg) 2-methylnaphthalene, 5mmol hydrogen peroxide, 1ml acetonitrile, and 40mg of catalyst M1, and use a balloon to release the pressure at the branch. Place in a 40℃ oil pan to react for 8h. After the reaction is completed, take out the tube and cool it to room temperature, centrifuge it, and use anhydrous magnesium sulfate to remove water from the clarified supernatant. Use gas chromatography to detect the conversion rate of 2-methylnaphthalene and the selectivity of 2-methyl-1,4-naphthoquinone.

[0048] Implementation Case 9:

[0049] In a Shrek tube, add 1mmol (142mg) 2-methylnaphthalene, 5mmol hydrogen peroxide, 1ml acetonitrile and catalyst M1, and the amount of catalyst is 50mg. Put a balloon at the branch to release the pressure. Place it in a 40℃ oil pan to react for 8h. After the reaction is completed, take out the tube and cool it to room temperature, centrifuge it, and use anhydrous magnesium sulfate to remove water from the clarified supernatant. Use gas chromatography to detect the conversion rate of 2-methylnaphthalene and the selectivity of 2-methyl-1,4-naphthoquinone.

[0050] Implementation Case 10:

[0051] In a Shrek tube, add 1mmol (142mg) 2-methylnaphthalene, 5mmol hydrogen peroxide, 1ml acetonitrile and catalyst M1, and the amount of catalyst is 60mg. Put a balloon at the branch to release the pressure. Place it in a 40℃ oil pan to react for 8h. After the reaction is completed, take out the tube and cool it to room temperature, centrifuge it, and use anhydrous magnesium sulfate to remove water from the clarified supernatant. Use gas chromatography to detect the conversion rate of 2-methylnaphthalene and the selectivity of 2-methyl-1,4-naphthoquinone.

[0052] Implementation Cases The amount of catalyst 2-Methylnaphthalene conversion Yield of 2-methyl-1,4-naphthoquinone 8 40mg 46% 35% 9 50mg 55% 46% 10 60mg 58% 49%

[0053] The recycling and use of catalyst M1 is shown in the following table:

[0054] Recycling times 2-Methylnaphthalene conversion Yield of 2-methyl-1,4-naphthoquinone 1 55% 46% 2 52% 43.5% 3 54% 44% 4 54% 39% 5 52% 43%

Claims

1. A method for synthesizing 2-methyl-1,4-naphthoquinone by oxidation using a polymerized cobalt phthalocyanine catalyst, the specific steps of which are as follows: A. Preparation of polymerized cobalt phthalocyanine catalyst: In an inert gas, 4,4'-biphenol and 4-nitrophthalonitrile are dissolved in N,N-dimethylformamide, anhydrous potassium carbonate is added, stirred, filtered, washed, and dried to obtain a precursor; the precursor and a cobalt compound are heated and reacted in a soluble solvent, and after cooling, filtered, washed, and dried to obtain a catalyst, wherein the mass loading of cobalt in the catalyst is 6.2%-19.7%; B. Add 2-methylnaphthalene, an oxidant and a polymerized cobalt phthalocyanine catalyst into a solvent, and react at 30-50° C. for 8-12 hours to obtain the product 2-methyl-1,4-naphthoquinone; the solvent in step B is acetonitrile; The oxidant is hydrogen peroxide.

2. The method according to claim 1, characterized in that The cobalt compound described in step A is cobalt acetate; the soluble solvent is N,N-dimethylethanolamine; and the inert gas is argon.

3. The method according to claim 1, characterized in that The stirring time described in step A is 10-48h; the filtration temperature is 0-30°C; the heating reaction temperature is 120°C-160°C; and the heating reaction time is 6-10h.

4. The method according to claim 1, characterized in that The molar ratio of 4,4'-biphenol to 4-nitrophthalonitrile in step A is 1:(0.8-3); the ratio of anhydrous potassium carbonate to 4,4'-biphenol is 1-3:1; and the molar ratio of the precursor to the cobalt compound is 1:(0.25-1).

5. The method according to claim 1, characterized in that The amount of the polymerized cobalt phthalocyanine catalyst used in step B is 28%-43% of the substrate mass; the molar amount of the oxidant is 4-8 times the equivalent of the substrate 2-methylnaphthalene.