Test device for in-situ study of cracking failure of thin-walled tube surface coating
By designing a multi-axis loading test device and combining an in-situ monitoring system, the problem that the existing technology cannot perform multi-axis loading test of thin-walled tube surface coating under high temperature conditions is solved, and the precise research and strain of the cracking behavior of the coating is achieved. The monitoring of relationships provides multi-axis stress impact analysis of the coating under high temperature conditions.
Patent Information
- Application Number
- CN202310135401.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-02-17
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2043-02-17
AI Technical Summary
The prior art cannot perform multi-axis loading tests for thin-walled tube surface coatings under high temperature conditions, and lacks an in-situ monitoring system, so it is impossible to accurately study the cracking behavior and strain relationship of the coating.
A test device including heating furnace, kettle installation mechanism, in-situ monitoring system, electric push rod system, in-kettle pressure injection system, slow tensile loading system and internal pressure loading system were designed, which can be from room temperature to high temperature range. Multi-axis loading tests are carried out, and mechanical, optical and acoustic signals are collected in real time through in-situ monitoring devices to monitor the strain field and crack characteristics of the coating.
A multi-axis loading test for thin-walled tube surface coating under high temperature conditions is realized, and the coating strain field and crack characteristics are monitored in real time, providing accurate research on the cracking behavior of the coating, and multi-axis stress pairing can be performed in the range of room temperature to high temperature. Study on the impact of coating.
Smart Images

Figure CN116202870B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of material mechanical property testing and experiment, in particular to a testing device for in-situ research on cracking failure of a thin-walled pipe surface coating. Background Art
[0002] Surface coating technology has the advantages of few constraints, strong designability, and a wide range of technology types and material types. It can make the surface of parts have functions such as heat insulation, high-temperature oxidation resistance, corrosion resistance and wear resistance. It is one of the most promising surface engineering methods. For example, surface coating technology can be applied to nuclear reactor fuel cladding, supercritical unit superheaters, and aircraft engine hot end components. Usually, the service conditions of various components are extremely harsh, and they are faced with multiple load coupling effects such as creep, fatigue, and thermal stress for a long time. The stress state is complex, which can easily lead to the initiation, expansion, penetration, and even peeling of cracks in the surface coating, affecting service safety, reliability and overall life.
[0003] At present, there are test devices for studying the cracking behavior of surface coatings in China. The existing technology is "Test device for coating anti-cracking performance and performance test evaluation method". This device can quantitatively evaluate the cracking performance of coatings to a certain extent, such as the maximum strain corresponding to coating cracking, anti-cracking stress, etc., but there are still the following shortcomings: it is not equipped with a heating system, and it is impossible to study the cracking behavior of coatings under high temperature conditions; it does not consider the multi-axial stress state caused by the irregular geometry of engineering components or the diversity of loads under actual service conditions, and it is impossible to carry out multi-axial loading tests; it is not equipped with a comprehensive in-situ monitoring system, and it is unable to achieve a more accurate and immediate correspondence between the damage state of the coating and the strain.
[0004] The existing technology "A method and system for predicting the cracking of brittle coatings" can achieve rapid prediction of the coating damage accumulation stage and evaluate the coating cracking situation. At the same time, the operation is relatively simple and the measurement accuracy is relatively high. However, the device still mainly carries out uniaxial static load tensile tests on plate coating samples and cannot realize multi-axial loading research.
[0005] In summary, it is necessary to provide a test device for in-situ research on cracking failure of thin-walled tube surface coatings that can realize heating, multi-axial loading and in-situ monitoring. Summary of the invention
[0006] In view of the defects in the prior art, the purpose of the present invention is to provide a test device for in-situ research on cracking failure of thin-walled pipe surface coating.
[0007] According to the present invention, a test device for in-situ research on cracking failure of thin-walled pipe surface coating is provided, comprising: a support system, a heating furnace, an in-vessel installation mechanism, an in-situ monitoring system, an electric push rod system, an in-vessel pressure injection system, a slow tensile loading system and an internal pressure loading system;
[0008] The heating furnace and the in-kettle mounting mechanism are mounted on the supporting system, and the electric push rod system is connected to and drives the heating furnace to move up and down.
[0009] The coated thin-walled tube is installed in the in-kettle installation mechanism, the in-situ monitoring system is arranged at the coated thin-walled tube, the in-kettle installation mechanism is connected to the in-kettle pressure injection system, the slow tensile loading system and the internal pressure loading system, and the slow tensile loading system is connected to the coated thin-walled tube.
[0010] Preferably, the in-kettle installation mechanism comprises: an in-kettle pipeline, an in-kettle pull rod, a lower clamping body, an end plug, a ferrule joint, an upper clamping body, a locking bolt and a locking sleeve;
[0011] The two ends of the coated thin-walled tube are clamped by the upper clamping body and the lower clamping body respectively, and locking bolts and locking sleeves are installed between the upper clamping body and the lower clamping body and the coated thin-walled tube respectively;
[0012] The coated thin-walled tube is clamped by the upper clamp at one end and connected to the pipeline in the kettle through the ferrule joint. The coated thin-walled tube is clamped by the lower clamp at one end and blocked by the end plug. The lower clamp faces away from the coated thin-walled tube and is connected to one end of the pull rod in the kettle along the axial direction of the coated thin-walled tube.
[0013] Preferably, the support system comprises: a top beam, a column, a bottom plate and a mounting plate for the cover of the experimental kettle;
[0014] The top beam and the bottom plate are connected via a plurality of the upright posts, and the experimental kettle cover mounting plate is installed between the plurality of the upright posts.
[0015] Preferably, the in-kettle mounting mechanism is mounted on the experimental kettle cover mounting plate, the experimental kettle cover mounting plate is connected to the in-kettle column facing the heating furnace, the in-kettle column is mounted with a clamp support plate facing away from the experimental kettle cover mounting plate, and the upper clamp is fixedly mounted on the clamp support plate.
[0016] Preferably, the heating furnace comprises: an experimental kettle shell, an experimental kettle cover and a sight glass observation window;
[0017] The experimental kettle shell is installed on the experimental kettle cover, the experimental kettle cover is fixedly installed on the experimental kettle cover mounting plate, the experimental kettle shell is placed inside the heating furnace, the experimental kettle shell is connected to the electric push rod system, the sight glass observation window is installed on the side of the experimental kettle shell, and the pull rod inside the kettle passes through the experimental kettle cover and extends in the direction away from the coated thin-walled tube.
[0018] Preferably, the in-kettle pressure injection system is connected to the interior of the experimental kettle shell through an in-kettle pressure injection pipeline.
[0019] Preferably, the slow tensile loading system comprises: a load-bearing frame, a servo motor, a planetary gear reducer, a loading column, an integrated stress loading unit and a load sensor;
[0020] The load-bearing frame includes a first load-bearing frame and a second load-bearing frame, the first load-bearing frame is fixed on the column, and two ends of the loading column are respectively fixed on the first load-bearing frame and the second load-bearing frame;
[0021] Two ends of the integrated stress loading unit are respectively mounted on an upper bearing seat and a lower bearing seat, the lower bearing seat is arranged on the second bearing frame, and the upper bearing seat is arranged on the first bearing frame;
[0022] The planetary gear reducer is installed on the side of the second bearing frame facing away from the first bearing frame, the servo motor is installed on the end of the planetary gear reducer facing away from the second bearing frame, and the output shaft of the planetary gear reducer is connected to the integrated stress loading unit;
[0023] One end of the load sensor is connected to the integrated stress loading unit, and the other end is connected to the pull rod in the kettle.
[0024] Preferably, the in-situ monitoring system comprises: a displacement sensor measuring rod, a high temperature resistant acoustic emission sensor and a CCD camera;
[0025] The displacement sensor measuring rod is connected to the coated thin-walled tube via a fixing clamp, and the displacement sensor is mounted on the displacement sensor measuring rod;
[0026] One or more of the CCD cameras are installed at a position where the lens faces the outer surface of the coated thin-walled tube;
[0027] The high temperature resistant acoustic emission sensor is installed on the coated thin-walled tube.
[0028] Preferably, the internal pressure loading system comprises: a driving gas circuit, a working gas circuit, a sample boosting pipeline, a pressure sensor, a pressure gauge, an accumulator, an exhaust valve, a safety valve, a first one-way valve, a solenoid valve and a gas boosting pump;
[0029] The sample boosting pipeline is connected to the first one-way valve, the pressure sensor and the exhaust valve at one end away from the inner pipeline of the kettle, the pressure sensor is connected to the pressure gauge, the pressure gauge is connected to the safety valve, the first one-way valve is connected to the accumulator, the gas boosting pump and the solenoid valve, the solenoid valve and the gas boosting pump are connected to the working gas circuit, and the gas boosting pump is connected to the driving gas circuit;
[0030] The driving gas circuit includes: a gas pressure regulating valve, an air filter and an air compressor;
[0031] The gas booster pump is connected to the gas pressure regulating valve, the gas pressure regulating valve is connected to the air filter, and the air filter is connected to the air compressor;
[0032] The working gas circuit includes: a stop valve, a second one-way valve, a pressure reducing valve and an argon gas tank;
[0033] The solenoid valve and the gas booster pump are connected to the second one-way valve, the second one-way valve is connected to the pressure reducing valve, the pressure reducing valve is connected to the stop valve, and the stop valve is connected to the argon gas tank.
[0034] Preferably, one end of the coated thin-walled tube is connected to the internal pressure loading system through the kettle pipeline and the sample pressurization pipeline in sequence.
[0035] Compared with the prior art, the present invention has the following beneficial effects:
[0036] 1. The present invention can realize multi-axial loading of coated thin-walled tubes in the range of room temperature to high temperature, that is, simultaneous loading of axial and internal pressure or simultaneous loading of axial and external pressure. The multi-axial stress ratio is controlled by setting the axial load and the pressure difference between the inside and outside of the thin-walled tube, that is, the influence of different axial stresses and hoop stresses on the cracking behavior of the coating on the surface of the thin-walled tube is studied.
[0037] 2. The present invention uses an in-situ monitoring device to synchronously collect the mechanical, optical and acoustic signals of the sample during the loading process, and monitors the strain field distribution, microscopic morphology image and surface crack characteristics of the thin-walled tube surface coating in real time. BRIEF DESCRIPTION OF THE DRAWINGS
[0038] Other features, objects and advantages of the present invention will become more apparent from the detailed description of non-limiting embodiments made with reference to the following drawings:
[0039] Figure 1 It is the overall structure diagram of the test device;
[0040] Figure 2 It is a structural schematic diagram of the slow tensile loading system;
[0041] Figure 3 It is a schematic diagram of the experimental kettle and the in-situ monitoring system structure;
[0042] Figure 4 It is a schematic diagram of the structure of the installation mechanism in the kettle;
[0043] Figure 5 This is a schematic diagram of the connection of the internal pressure loading system;
[0044] As shown in the figure:
[0045]
[0046] DETAILED DESCRIPTION
[0047] The present invention is described in detail below in conjunction with specific embodiments. The following embodiments will help those skilled in the art to further understand the present invention, but are not intended to limit the present invention in any form. It should be noted that, for those of ordinary skill in the art, several changes and improvements can also be made without departing from the concept of the present invention. These all belong to the protection scope of the present invention.
[0048] Example 1
[0049] like Figure 1 As shown, this embodiment includes: a support system 1, a heating furnace 2, a kettle installation mechanism 3, an in-situ monitoring system 5, an electric push rod system 6, a kettle pressure injection system 7, a slow stretching loading system 8 and an internal pressure loading system 9; the heating furnace 2, the kettle installation mechanism 3 and the experimental kettle are installed on the support system 1, the experimental kettle is placed inside the heating furnace 2, and the heating furnace 2 is used to heat the experimental kettle, so as to change the temperature inside the experimental kettle from normal temperature to high temperature, and the electric push rod system 6 connects and drives the experimental kettle and the heating furnace 2 to move up and down. The coating thin-walled tube 4 is installed in the kettle installation mechanism 3, and the coating thin-walled tube 4 is provided with an in-situ monitoring system 5. The kettle installation mechanism 3 is connected to the kettle pressure injection system 7, the slow stretching loading system 8 and the internal pressure loading system 9, and the slow stretching loading system 8 is connected to the coating thin-walled tube 4 and realizes the axial stretching of the coating thin-walled tube 4. The kettle pressure injection system 7 is connected to the inside of the experimental kettle 2 through the kettle pressure injection pipeline 701, and an inert gas of a set pressure is injected into the experimental kettle 2 or a vacuum environment is formed.
[0050] The support system 1 includes: a top beam 101 , columns 102 , a bottom plate 103 and an experimental kettle cover mounting plate 104 ; the top beam 101 and the bottom plate 103 are connected by a plurality of columns 102 , and the experimental kettle cover mounting plate 104 is installed between the plurality of columns 102 .
[0051] like Figure 2As shown, the slow tensile loading system 8 includes: a bearing frame 801, a servo motor 802, a planetary gear reducer 803, a loading column 804, a load sensor 806 and an integrated stress loading unit 807. The upper end portion of the bearing frame 801 is fixed on a plurality of columns 102, and the top and bottom of the loading column 804 are respectively fixed on the upper and lower ends of the bearing frame 801. The integrated stress loading unit 807 includes a ball screw nut and a ball screw, and the top and bottom of the ball screw are respectively installed on the upper bearing seat 808 and the lower bearing seat 805. The loading column 804 and the ball screw are distributed at the lower end portion of the bearing frame 801. The planetary gear reducer 803 is installed below the bearing frame 801, the servo motor 802 is installed below the planetary gear reducer 803, and the output shaft of the planetary gear reducer 803 is connected to the bottom of the ball screw. The servo motor 802 drives the planetary gear reducer 803, and the planetary gear reducer 803 drives the ball screw to rotate. The top of the load sensor 806 is connected to the bottom of the pull rod 304 in the kettle through a connecting block, and the bottom of the load sensor 806 is connected to the integrated stress loading unit 807 through a transition piece.
[0052] like Figure 3 and Figure 4As shown, the experimental kettle in the heating furnace 2 includes: an experimental kettle shell 201, an experimental kettle cover 202 and a sight glass observation window 203; the experimental kettle cover 202 is fixedly mounted on the experimental kettle cover mounting plate 104, the experimental kettle shell 201 is placed inside the heating furnace 2 and connected to the electric push rod system 6, the sight glass observation window 203 is installed on the side of the experimental kettle shell 201 and the heating furnace 2, the inner pull rod 304 passes through the experimental kettle cover 202 and extends in the direction away from the coated thin-walled tube 4, and the slow tensile loading system 8 pulls the coated thin-walled tube 4 through the inner pull rod 304. When the test starts, the experimental kettle shell 201 and the heating furnace 2 system are driven by the electric push rod system 6 to close with the experimental kettle cover 202 to form a closed space. The installation mechanism 3 in the kettle includes: an inner pipeline 301 in the kettle, an inner pull rod 304, a lower clamp body 305, an end plug 306, a ferrule joint 307, an upper clamp body 308, a locking bolt 309 and a locking sleeve 310; both ends of the coated thin-walled tube 4 are clamped by the upper clamp body 308 and the lower clamp body 305 respectively, and the locking bolt 309 and the locking sleeve 310 are respectively installed between the upper clamp body 308 and the lower clamp body 305 and the coated thin-walled tube 4; the coated thin-walled tube 4 is connected to the inner pipeline 301 in the kettle at one end clamped by the upper clamp body 308 through the ferrule joint 307, and the inner pipeline 301 in the kettle away from the coated thin-walled tube 4 is connected to the internal pressure loading system 9 through the sample booster pipeline 901, and the internal pressure loading system 9 inputs gas into the coated thin-walled tube 4 through the inner pipeline 301 in the kettle. The coated thin-walled tube 4 is clamped by the lower clamp body 305, and one end of the end is blocked by the end plug 306. The end of the lower clamp body 305 facing away from the coated thin-walled tube 4 is connected to one end of the pull rod 304 in the kettle along the axial direction of the coated thin-walled tube 4. The kettle installation mechanism 3 is installed on the experimental kettle cover installation plate 104, and the experimental kettle cover installation plate 104 is connected to the kettle column 303 on the side facing the experimental kettle 2. The kettle column 303 is installed with a fixture support plate 302 on the side facing away from the experimental kettle cover installation plate 104, and the upper clamp body 308 is fixedly installed on the fixture support plate 302.
[0053] The in-situ monitoring system 5 includes: a displacement sensor measuring rod 501, a high temperature resistant acoustic emission sensor 502 and a CCD camera 503; the displacement sensor measuring rod 501 is connected to the coated thin-walled tube 4 through a fixing clamp, the displacement sensor is installed on the displacement sensor measuring rod 501, the displacement sensor is used to monitor the axial size of the coated thin-walled tube 4, two CCD cameras 503 are installed at a position where the lens is directly opposite to the outer surface of the coated thin-walled tube 4, the CCD camera 503: a charge coupled device, is an electrical component that can convert optical images into digital signals, the CCD camera 503 can be used in conjunction with an image acquisition card to monitor the strain field and microscopic morphology image of the thin-walled tube surface coating in real time, the coated thin-walled tube 4 is installed with a high temperature resistant acoustic emission sensor 502, the high temperature resistant acoustic emission sensor 502 is a known acoustic emission signal acquisition device, and is used to collect acoustic emission signals related to the thin-walled tube surface coating and crack initiation and expansion during loading.
[0054] like Figure 5 As shown, the internal pressure loading system 9 includes: a driving gas circuit, a working gas circuit, a pressure sensor 902, a pressure gauge 903, an accumulator 904, an exhaust valve 909, a safety valve 910, a first one-way valve 911, an electromagnetic valve 912 and a gas booster pump 913; the sample booster pipeline 901 is connected to the first one-way valve 911, the pressure sensor 902 and the exhaust valve 909 at one end away from the pipeline 301 in the kettle, the pressure sensor 902 is connected to the pressure gauge 903, the pressure gauge 903 is connected to the safety valve 910, the first one-way valve 911 is connected to the accumulator 904, the gas booster pump 913 and the electromagnetic valve 912, and the electromagnetic valve 912 and the gas booster pump 913 are connected to the working Gas circuit, the gas booster pump 913 is connected to the driving gas circuit; the driving gas circuit includes: a gas pressure regulating valve 905, an air filter 906 and an air compressor 907; the gas booster pump 913 is connected to the gas pressure regulating valve 905, the gas pressure regulating valve 905 is connected to the air filter 906, and the air filter 906 is connected to the air compressor 907; the working gas circuit includes: a stop valve 908, a second one-way valve 914, a pressure reducing valve 915 and an argon tank 916; the solenoid valve 912 and the gas booster pump 913 are connected to the second one-way valve 914, the second one-way valve 914 is connected to the pressure reducing valve 915, the pressure reducing valve 915 is connected to the stop valve 908, and the stop valve 908 is connected to the argon tank 916.
[0055] Example 2
[0056] Example 2 is a preferred example of Example 1.
[0057] like Figure 1 As shown, this embodiment includes a slow tensile loading system 8, an internal pressure loading system 9, a heating furnace 2, an experimental kettle, an in-kettle mounting mechanism 3, an in-kettle pressure injection system 7, an in-situ monitoring system 5, a support system 1 and an electric push rod system 6. The support system 1 includes a top beam 101, a column 102 and a bottom plate 103, wherein the top beam 101 and the bottom plate 103 are respectively arranged at the top and bottom of the column 102, and the whole presents a four-column floor-standing structure. The slow tensile loading system 8, the kettle installation mechanism 3, the experimental kettle and the heating furnace are installed between the four columns 102 from bottom to top; the experimental kettle is installed inside the heating furnace 2, presenting an integrated structure, and the overall lifting and lowering of the experimental kettle and the heating furnace 2 are controlled by the electric push rod system 6; the bottom of the kettle pull rod 304 is connected to the slow tensile loading system 8, and the top is connected to the coated thin-walled tube 4 inside the kettle installation mechanism 3; the upper and lower ends of the kettle pipeline 301 are respectively connected to the coated thin-walled tube 4 and the internal pressure loading system 9 to realize the internal pressurization loading of the coated thin-walled tube 4 sample; the kettle pressure injection system 7 can realize the internal pressure injection and control of the experimental kettle; the kettle installation mechanism 3 and the slow tensile loading system 8 are both fixedly connected to the four columns 102.
[0058] like Figure 2As shown, the slow tensile loading system 8 includes: a bearing frame 801, a servo motor 802, a planetary gear reducer 803, a loading column 804, a load sensor 806 and an integrated stress loading unit 807. The upper end portion of the bearing frame 801 is fixed on a plurality of columns 102, and the top and bottom of the loading column 804 are respectively fixed on the upper and lower ends of the bearing frame 801. The integrated stress loading unit 807 includes a ball screw nut and a ball screw, and the top and bottom of the ball screw are respectively installed on the upper bearing seat 808 and the lower bearing seat 805. The loading column 804 and the ball screw are distributed at the lower end portion of the bearing frame 801. The planetary gear reducer 803 is installed below the bearing frame 801, the servo motor 802 is installed below the planetary gear reducer 803, and the output shaft of the planetary gear reducer 803 is connected to the bottom of the ball screw. The servo motor 802 drives the planetary gear reducer 803, and the planetary gear reducer 803 drives the ball screw to rotate. The top of the load sensor 806 is connected to the bottom of the pull rod 304 in the kettle through a connecting block, and the bottom of the load sensor 806 is connected to the integrated stress loading unit 807 through a transition piece.
[0059] like Figure 5 As shown, the internal pressure loading system 9 includes a driving gas circuit, a working gas circuit, a gas booster pump 913, an accumulator 904, a pressure sensor 902 and a corresponding gas outlet pipeline. The driving gas circuit is sequentially connected by an air compressor 907, an air filter 906 and a gas pressure regulating valve 905; the working gas circuit is sequentially connected by an argon tank 916, a stop valve 908, a pressure reducing valve 915 and a second one-way valve 914; an accumulator 904 is arranged at the rear end of the gas booster pump 913 to reduce the internal pressure fluctuation of the coated thin-walled tube 4 and realize precise pressure control; the gas outlet pipeline is connected in parallel with a pressure sensor 902, a pressure gauge 903 and an exhaust valve 909, which are respectively used to display the internal pressure of the sample in real time and discharge the internal gas; a safety valve 910 is arranged on the pipeline to prevent accidents.
[0060] The bottom end of the coated thin-walled tube 4 sample is sealed and welded, and the top end is connected to the kettle pipeline 301 and the sample booster pipeline 901 in sequence through a ferrule joint 307 to achieve internal pressure loading.
[0061] The experimental kettle shell 201 is made of 625 nickel-based alloy, which can meet the requirements of high temperature 600℃ and high pressure 25MPa test. It adopts metal sealing and high-strength bolt locking, and is equipped with safety valve 910 and pressure sensor 902 to provide safety protection. The experimental kettle cover 202 is designed with multiple connection interfaces, which are respectively connected to the pressure injection pipeline 701 and its joints in the kettle, the sample booster pipeline 901 and its joints, the displacement sensor measuring rod 501, etc. The two sides of the experimental kettle shell 201 are provided with sapphire mirror observation windows 203 extending to the outside of the heating furnace body, which are used for digital image correlation monitoring of the strain field of the coated thin-walled tube 4 sample. The installation mechanism 3 in the kettle includes an upper clamp body 308, a lower clamp body 305, a fixture support plate 302, a column 303 in the kettle and a pull rod 304 in the kettle. The upper and lower ends of the coated thin-walled tube 4 are respectively connected to intelligent temperature control instruments for setting and controlling the temperature. The interior of the experimental kettle can be set to a vacuum or inert gas environment, which can form a positive and negative pressure difference with the interior of the coated thin-walled tube 4 sample.
[0062] The in-situ monitoring system 5 includes a displacement sensor, a high temperature resistant acoustic emission sensor 502 and a CCD camera 503. The displacement sensor is used to monitor the axial dimension of the coated thin-walled tube 4 online. The displacement sensor measuring rod 501 installed by the displacement sensor is connected to the coated thin-walled tube 4 through a fixing clamp. The CCD camera 503 is used in conjunction with an image acquisition card to monitor the strain field and microscopic morphology image of the surface coating of the coated thin-walled tube 4 in real time. Two sets of CCD cameras 503 are respectively facing the outer surface of the sample, and the image acquisition card is embedded in the computer. The high temperature resistant acoustic emission sensor 502 is used to collect acoustic emission signals related to the surface coating of the coated thin-walled tube 4 and crack initiation and expansion during loading, and is placed at the lower end of the coated thin-walled tube 4.
[0063] Method for using the device of this embodiment: the coated thin-walled tube 4 is assembled and installed in the heating furnace 2 through the upper clamp body 308, the locking bolt 309, the locking sleeve 310, the lower clamp body 305, etc., and the lower end of the coated thin-walled tube 4 is sealed by the end plug 306 through vacuum electron beam welding, and the axial load is provided by the slow tensile loading system 8; the internal pressure loading system 9 provides argon gas of set pressure to the inside of the coated thin-walled tube 4 through the sample booster pipeline 901, etc., to achieve internal pressure loading; the set pressure is injected into the heating furnace 2 through the pressure injection pipeline 701 in the kettle The inert gas or vacuum environment can form different positive and negative pressure differences with the inside of the coated thin-walled tube 4; during the loading process, the axial size of the coated thin-walled tube 4 is monitored online through the displacement sensor measuring rod 501; the strain field distribution and microscopic morphology image of the coating on the surface of the coated thin-walled tube 4 are collected in real time by the CCD camera 503, and transmitted to the image acquisition card for analysis and processing; the signal data is collected in real time by the high-temperature resistant acoustic emission sensor 502 in the acoustic emission technology, and the analysis and processing is an acoustic emission frequency diagram. The appearance of the initial frequency indicates that cracks have initiated on the surface of the coated thin-walled tube 4.
[0064] In the description of the present application, it should be understood that the terms "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0065] The above describes the specific embodiments of the present invention. It should be understood that the present invention is not limited to the above specific embodiments, and those skilled in the art can make various changes or modifications within the scope of the claims, which does not affect the essence of the present invention. In the absence of conflict, the embodiments of the present application and the features in the embodiments can be combined with each other arbitrarily.
Claims
1. A test device for in-situ study of cracking failure of thin-walled pipe surface coating, characterized in that: include: Support system (1), heating furnace (2), in-vessel mounting mechanism (3), in-situ monitoring system (5), electric push rod system (6), in-vessel pressure injection system (7), slow tensile loading system (8) and internal pressure loading system (9); The heating furnace (2) and the in-kettle mounting mechanism (3) are mounted on the supporting system (1), and the electric push rod system (6) is connected to and drives the heating furnace (2) to move up and down; The coated thin-walled tube (4) is installed in the in-kettle installation mechanism (3), the in-situ monitoring system (5) is arranged at the coated thin-walled tube (4), the in-kettle installation mechanism (3) is connected to the in-kettle pressure injection system (7), the slow tensile loading system (8) and the internal pressure loading system (9), and the slow tensile loading system (8) is connected to the coated thin-walled tube (4); The in-kettle installation mechanism (3) comprises: an in-kettle pipeline (301), an in-kettle pull rod (304), a lower clamp body (305), an end plug (306), a ferrule joint (307), an upper clamp body (308), a locking bolt (309) and a locking sleeve (310); The two ends of the coated thin-walled tube (4) are clamped by the upper clamp body (308) and the lower clamp body (305) respectively, and locking bolts (309) and locking sleeves (310) are installed between the upper clamp body (308) and the lower clamp body (305) and the coated thin-walled tube (4) respectively; One end of the coated thin-walled tube (4) is clamped by the upper clamp body (308) and connected to the pipeline (301) in the kettle through the ferrule joint (307); one end of the coated thin-walled tube (4) is clamped by the lower clamp body (305) and blocked by the end plug (306); one end of the lower clamp body (305) facing away from the coated thin-walled tube (4) is connected to one end of the pull rod (304) in the kettle along the axial direction of the coated thin-walled tube (4); The in-situ monitoring system (5) comprises: a displacement sensor measuring rod (501), a high temperature resistant acoustic emission sensor (502) and a CCD camera (503); The displacement sensor measuring rod (501) is connected to the coated thin-walled tube (4) via a fixing clamp, and the displacement sensor is mounted on the displacement sensor measuring rod (501); One or more CCD cameras (503) are installed at a position where the lens faces the outer surface of the coated thin-walled tube (4); The high temperature resistant acoustic emission sensor (502) is installed on the coated thin-walled tube (4); The support system (1) comprises: a top beam (101), a column (102), a bottom plate (103) and an experimental kettle cover mounting plate (104); The top beam (101) and the bottom plate (103) are connected via a plurality of upright posts (102), and the experimental kettle cover mounting plate (104) is mounted between the plurality of upright posts (102); The in-kettle mounting mechanism (3) is mounted on the experimental kettle cover mounting plate (104); the experimental kettle cover mounting plate (104) is connected to the in-kettle column (303) on the side facing the heating furnace (2); the in-kettle column (303) is mounted with a fixture support plate (302) on the side facing away from the experimental kettle cover mounting plate (104); and the upper fixture body (308) is fixedly mounted on the fixture support plate (302); The heating furnace (2) comprises: an experimental kettle shell (201), an experimental kettle cover (202) and a sight glass observation window (203); The experimental kettle shell (201) is mounted on the experimental kettle cover (202), the experimental kettle cover (202) is fixedly mounted on the experimental kettle cover mounting plate (104), the experimental kettle shell (201) is placed inside the heating furnace (2), the experimental kettle shell (201) is connected to the electric push rod system (6), the sight glass observation window (203) is installed on the side of the experimental kettle shell (201), and the inner kettle pull rod (304) passes through the experimental kettle cover (202) and extends in a direction away from the coated thin-walled tube (4); The in-kettle pressure injection system (7) is connected to the interior of the experimental kettle shell (201) via an in-kettle pressure injection pipeline (701); The internal pressure loading system (9) comprises: a driving gas circuit, a working gas circuit, a sample boosting pipeline (901), a pressure sensor (902), a pressure gauge (903), an accumulator (904), an exhaust valve (909), a safety valve (910), a first check valve (911), a solenoid valve (912) and a gas boosting pump (913); The sample boosting pipeline (901) is connected to the first one-way valve (911), the pressure sensor (902) and the exhaust valve (909) at one end away from the inner pipeline (301) of the kettle, the pressure sensor (902) is connected to the pressure gauge (903), the pressure gauge (903) is connected to the safety valve (910), the first one-way valve (911) is connected to the accumulator (904), the gas boosting pump (913) and the solenoid valve (912), the solenoid valve (912) and the gas boosting pump (913) are connected to the working gas circuit, and the gas boosting pump (913) is connected to the driving gas circuit; The driving gas circuit comprises: a gas pressure regulating valve (905), an air filter (906) and an air compressor (907); The gas booster pump (913) is connected to the gas pressure regulating valve (905), the gas pressure regulating valve (905) is connected to the air filter (906), and the air filter (906) is connected to the air compressor (907); The working gas circuit comprises: a stop valve (908), a second one-way valve (914), a pressure reducing valve (915) and an argon gas tank (916); The solenoid valve (912) and the gas booster pump (913) are connected to the second one-way valve (914), the second one-way valve (914) is connected to the pressure reducing valve (915), the pressure reducing valve (915) is connected to the stop valve (908), and the stop valve (908) is connected to the argon gas tank (916).
2. The test device for in-situ research on cracking failure of thin-walled pipe surface coating according to claim 1 is characterized in that: The slow tensile loading system (8) comprises: a bearing frame (801), a servo motor (802), a planetary gear reducer (803), a loading column (804), an integrated stress loading unit (807) and a load sensor (806); The load-bearing frame (801) comprises a first load-bearing frame and a second load-bearing frame, the first load-bearing frame is fixed on the column (102), and the two ends of the loading column (804) are respectively fixed on the first load-bearing frame and the second load-bearing frame; The two ends of the integrated stress loading unit (807) are respectively mounted on an upper bearing seat (808) and a lower bearing seat (805), the lower bearing seat (805) is arranged on the second bearing frame, and the upper bearing seat (808) is arranged on the first bearing frame; The planetary gear reducer (803) is installed on the side of the second supporting frame facing away from the first supporting frame, the servo motor (802) is installed on the end of the planetary gear reducer (803) facing away from the second supporting frame, and the output shaft of the planetary gear reducer (803) is connected to the integrated stress loading unit (807); One end of the load sensor (806) is connected to the integrated stress loading unit (807), and the other end is connected to the pull rod (304) in the kettle.
3. The test device for in-situ study of cracking failure of thin-walled tube surface coating according to claim 1 is characterized by: One end of the coated thin-walled tube (4) is connected to the internal pressure loading system (9) via the kettle internal pipeline (301) and the sample pressurization pipeline (901) in sequence.