A test knot and its application, fabrication and cutting method

By designing a test junction with a covering film and a positioning film in the Josephson junction, the problem of accurately determining the cutting position during the cutting process was solved, enabling efficient and precise cutting and high-quality observation of the barrier layer cross-section.

CN116490056BActive Publication Date: 2026-11-17ORIGIN QUANTUM COMPUTING TECH (HEFEI) CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202310618837.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-05-25
Publication Date
2026-11-17
Estimated Expiration
2043-05-25

AI Technical Summary

Technical Problem

When using focused ion beams to cut Josephson junctions, it is difficult to accurately determine the expected cutting location, especially the electron barrier layer, leading to inaccurate cutting and potential damage.

Method used

Design a test junction including a cover layer and a positioning layer. The cover layer protects the electron barrier layer, and the positioning layer indicates the cutting stop position, thereby protecting the barrier layer and improving cutting accuracy during the cutting process.

Benefits of technology

By protecting the electron barrier layer and providing a cutting stop position indicator, the accuracy and efficiency of cutting are improved, unnecessary cutting times are reduced, and high-quality barrier layer cross-section observation and analysis are ensured.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116490056B_ABST
    Figure CN116490056B_ABST
Patent Text Reader

Abstract

This application discloses a test junction and its application, fabrication, and dicing methods, belonging to the field of quantum chip fabrication. The example test junction includes two superconducting layers providing a Josephson junction and an electron barrier layer between them, as well as a cover layer that covers at least the region where the Josephson junction is located. It also has a positioning film layer at least partially disposed within the first and / or second superconducting layers. This positioning film layer is positioned away from the overlapping region and is positioned to be diced together with the electron barrier layer by a positioning plane. This test junction can be used in embodiments where cutting is performed to observe the cross-section protected by the electron barrier layer, providing a higher dicing success rate and improving dicing efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application belongs to the field of quantum information, especially the field of quantum chip fabrication. In particular, this application relates to a test junction and its application, fabrication and cutting methods. Background Technology

[0002] Josephson junctions are key structures in superconducting quantum chips. Typically, a Josephson junction is a weakly connected structure of two superconductors. In a superconducting quantum chip, a Josephson junction can be constructed as two superconducting aluminum atoms and an oxide / alumina layer bonded between them. Studying the oxide layer will aid in the fabrication and design of Josephson junctions.

[0003] Currently, transmission electron microscopy (TEM) can be used to study the structure and properties of the oxide layer in the junction region of the Josephson junction. To study this oxide layer via TEM, a focused ion beam (FIB) can be used beforehand to precisely cut the target oxide layer and to thin the junction sample.

[0004] However, it is difficult to determine whether the cut has reached the intended position when using FIB for cutting. Summary of the Invention

[0005] This application provides an example of a test junction and its application, fabrication, and cutting method. It can be used to determine the stopping point during the cutting of a Josephson junction, so as to accurately cut to the barrier layer of the Josephson junction, thereby enabling analysis of its fabrication quality through the cross-section exposed by the cutting of the barrier layer.

[0006] The solution presented in this application is implemented through the following steps.

[0007] In a first aspect, this application presents an example of a test conclusion. It includes:

[0008] The first superconductor layer has a junction-forming surface;

[0009] An electron barrier layer is formed on the junction surface of the first superconducting layer;

[0010] The second superconducting layer partially overlaps with the first superconducting layer, and the overlapping region is aligned with the barrier layer, thereby forming a Josephson junction in the overlapping region by the first superconducting layer, the electronic barrier layer, and the first superconducting layer.

[0011] A cover film is aligned to cover the overlapping region, such that at least in the overlapping region, the first superconductor layer, the electron barrier layer, and the first superconductor layer are covered; and

[0012] The positioning film layer based on the positioning of the electronic barrier layer is at least partially disposed within the first superconductor layer and / or the second superconductor layer, and the positioning film layer is separated from the overlapping region;

[0013] The test junction is defined with a positioning plane, which allows the positioning plane to cut both the positioning film and the electron barrier layer when the positioning film is positioned based on the electron barrier layer.

[0014] The test junction includes a Josephson junction, a capping layer, and a positioning layer. The capping layer covers the region where the Josephson junction is located, i.e., the overlapping region or more regions, thereby protecting the electron barrier layer in the Josephson junction.

[0015] Therefore, by protecting the electron barrier layer as described above, the electron barrier layer can be protected from unwanted damage during the subsequent cutting of the test junction, which facilitates obtaining a higher quality electron barrier layer cross-section and makes it easier to observe and analyze the electron barrier layer cross-section later.

[0016] The positioning film layer can be used to indicate the stop position during the cutting process, thereby improving the accuracy of cutting and reducing unnecessary cutting operations.

[0017] According to some examples of this application, the first superconducting layer and the second superconducting layer are configured in a cross-sectional arrangement;

[0018] Alternatively, the superconductor layer has grooves, and the positioning film layer is at least partially located within the grooves;

[0019] Alternatively, the positioning film layer may not be covered by the covering film layer;

[0020] Alternatively, the superconducting layer has a length dimension and a width dimension, with the length dimension being greater than the width dimension and appearing as a long, narrow strip. The superconducting layer has a centerline defined along the direction of the defined length dimension, and the positioning film layers are distributed in a manner that crosses the centerline laterally.

[0021] According to some examples in this application, the first superconducting layer and the second superconducting layer are made of the same material;

[0022] Alternatively, at least one of the first superconducting layer and the second superconducting layer is an aluminum film;

[0023] Alternatively, the electronic barrier layer can be aluminum oxide;

[0024] Alternatively, the positioning film layer is a platinum film;

[0025] Alternatively, the positioning film layer and the covering film layer can be made of the same material.

[0026] In a second aspect, examples of this application present a test junction comprising:

[0027] A first aluminum film extending along a first direction has positioning surfaces distributed along the first direction, and the positioning surfaces have grooves;

[0028] An aluminum oxide film is formed on a portion of the positioning surface but not in the area where the groove is located, and the aluminum oxide film has a preset thickness.

[0029] The second aluminum film extends along a second direction that intersects the first direction, and covers an aluminum oxide film in the area overlapping with the first aluminum film. The overlapping area avoids the groove and is separated from the groove by a predetermined distance along the first direction. The predetermined thickness is defined by the direction from the first aluminum film to the second aluminum film.

[0030] A positioning film layer is at least partially embedded in a groove, the region of the positioning film layer within the groove having a preset depth measured along the groove depth direction.

[0031] According to some examples in this application, the test result has one or more features selected from the following:

[0032] First characteristic: The positioning film layer is made of platinum;

[0033] Second feature: The positioning film layer is flush with the positioning surface;

[0034] Third feature: The test junction is defined with a cutting surface that half-slits the alumina film along the first direction, and the positioning film layer is positioned to be half-slit by the cutting surface.

[0035] Fourth feature: The positioning film layer fills the entire depth of the groove.

[0036] According to some examples in this application, the preset depth is at least an order of magnitude greater than the preset thickness;

[0037] And / or, the preset depth is greater than the preset thickness, the preset depth is on the order of micrometers, and the preset thickness is on the order of nanometers.

[0038] In a third aspect, this application provides an example of a method for fabricating a test knot. The method includes:

[0039] A Josephson junction formed on a substrate is provided, including a first electrode, a second electrode, and a barrier layer connected to and located between the first electrode and the second electrode, the first electrode and the second electrode being cross-configured, wherein the first electrode contacts the substrate within an extended trajectory, the substrate defining a junction region and an outside region, the projection of the barrier layer in the direction opposite to the substrate being located in the junction region, and at least the first electrode having an outside segment in the outside region.

[0040] Optionally, a protective film layer is configured, which is located in the junction region and covers the portions of the first electrode and the second electrode in the junction region, and the protective film layer does not cover the outer region of the junction.

[0041] Positioning elements are obtained in an optional order and positioned within the outer segment of the junction. The positioning elements have a height dimension defined by a given depth extending from the surface of the outer segment into the interior.

[0042] In a fourth aspect, this application provides an example of the application of the aforementioned test junction in the fabrication of a Josephson junction, wherein the Josephson junction comprises two superconducting layers and a weakly connected layer connecting and located between the two superconducting layers.

[0043] According to some examples of this application, test knots are used to determine the cutting stop position during the cutting operation of Josephson knots, where the Josephson knot cut at the cutting stop position exposes a cross section provided by the weakly connected layer, and the fabrication process is evaluated or adjusted based on the analysis of the cross section.

[0044] In a fifth aspect, this application provides an example of a method for cutting a test knot with a Josephson knot, the cutting method comprising:

[0045] A Josephson junction is provided, having two cross-distributed electrodes and a barrier layer connected between the two cross-distributed electrodes, wherein one or both electrodes are configured with an embedded film of a given thickness at a location away from the barrier layer.

[0046] Optionally, perform either the first operation or the second operation:

[0047] The first operation includes: when only one electrode is configured to embed the film, gradually etching the Josephson junction along the extension direction of the other electrode, and the etching range includes the area where the barrier layer and the embedded film are located, and stopping the etching when the cross-section exposes the embedded film.

[0048] The second operation includes: when the two electrodes are each configured with an embedded film, gradually etching the Josephson junction along the extension direction of either electrode, and the etching range includes the area where the barrier layer and the embedded film are located, and stopping the etching when the cross-section exposes the embedded film.

[0049] Optionally, in the first operation, the etching operation is performed synchronously from both the front and rear sides toward the barrier layer along the extension direction of the other electrode.

[0050] Optionally, in the second operation, the etching operation is performed synchronously from both the front and rear sides towards the barrier layer along the extension direction of any electrode.

[0051] Beneficial effects:

[0052] In a Josephson junction, the electron barrier layer is bonded between the top and bottom superconducting electrodes. Therefore, the Josephson junction can be cut (e.g., by etching) to achieve the desired cross-section of the electron barrier layer. However, because the electron barrier layer is very thin, such as on the nanometer scale, it is relatively fragile. Therefore, to obtain a high-quality electron barrier layer, it can be protected, for example, by configuring a capping film. Given the presence of the protective capping film and the very small thickness of the electron barrier layer, configuring a positioning film makes it easier to identify whether the desired cut has been made during cutting compared to cutting without a positioning film. This helps improve cutting efficiency and accuracy, and reduces unnecessary multiple cutting operations. Attached Figure Description

[0053] To illustrate this more clearly, the accompanying drawings used in the description will be briefly introduced below.

[0054] Figure 1 This is a schematic diagram of the structure of a quantum bit on a quantum chip in related technologies;

[0055] Figure 2 This is a schematic diagram of the Josephson knot structure in the example of this application;

[0056] Figure 3 This is a schematic diagram of the structure of the first test junction in this application example from one viewpoint (excluding the barrier layer);

[0057] Figure 4 for Figure 3 A cross-sectional view of the test junction (excluding the covering membrane layer);

[0058] Figure 5 This is a schematic diagram of the structure of the second type of test junction in the example of this application from one perspective;

[0059] Figure 6 This illustration shows a schematic diagram of etching thinning from both sides to the center of a Josephson junction-based test junction, as shown in an example of this application.

[0060] Explanation of reference numerals in the attached figures: 100-Test junction; 101-First superconductor layer; 102-Second superconductor layer; 103-Covering film layer; 104-Positioning film layer; 105-Electron barrier layer. Detailed Implementation

[0061] Currently, the key component of superconducting quantum chips—superconducting qubits—is mainly based on the Josephson structure.

[0062] Figure 1 This is a schematic diagram of the Josephson junction-based qubit structure arranged on a superconducting quantum chip in related technologies. Figure 1As shown, the structure of a qubit often employs a single capacitor to ground, and a superconducting quantum interference device with one end grounded and the other end connected to that capacitor. Furthermore, this capacitor is often a cross-shaped parallel-plate capacitor.

[0063] See Figure 1 As shown, the cross-shaped capacitor plate C q (i.e., bit capacitor) is surrounded by the ground plane (GND), and the cross-shaped capacitor plate C q There is a gap (usually an air gap, for insulation) between it and the ground plane (GND).

[0064] One end of the superconducting quantum interference device (SQUID) is connected to a cross-shaped capacitor plate C. q (One end of a capacitor arm, as mentioned later in the first part), and the other end is connected to the ground plane (GND).

[0065] Due to the cross-shaped capacitor plate C q The first end is typically used to connect to a superconducting quantum interference device, while the second end is used for coupling with the readout resonant cavity. The cross-shaped capacitor plate C... q The other two ends are used for coupling with adjacent qubits to achieve bit expansion. A certain amount of space is usually reserved near the first and second ends for arranging microwave transmission lines such as drive control signal lines (xy) and flux modulation signal lines (Z). Similarly, a certain amount of space is usually reserved near the resonant cavity for arranging readout signal transmission lines that are coupled to the resonant cavity.

[0066] When performing quantum computing, the frequency of the qubit is first adjusted to the working frequency (initial state creation) by using the magnetic flux control signal on the magnetic flux control signal line. Then, the quantum state control signal is applied to the qubit in the initial state by driving the control signal line to control the quantum state. Finally, the quantum state of the controlled qubit is read out by using a resonant cavity.

[0067] In superconducting quantum chips, Josephson junctions provide nonlinear inductance in quantum circuits / quantum devices. By connecting them in parallel with a capacitor (which can typically be described as a shunt capacitor), a nonlinear oscillator that can function as a superconducting quantum bit can be formed.

[0068] Generally, a Josephson junction consists of two superconductor layers sandwiching an extremely thin insulator. This insulator layer is only a few nanometers thick, thus enabling significant electron-pair tunneling, the Josephson effect. The insulator layer forms a weak connection between the two superconductor layers. This insulator layer can also serve as a barrier layer, and can be a normal-state metal, a weakened superconductor layer, or a semiconductor. The Josephson junction currently widely used in superconducting quantum computing is based on aluminum / alumina / aluminum; and aluminum oxide is used as the barrier layer in the form of an insulating layer. (See also...) Figure 2 .

[0069] Overall, Josephson junctions are relatively small in size. For example, some typical Josephson junctions are around 100 to 300 nanometers in size. Therefore, Josephson junctions are mostly fabricated using micro- and nanofabrication techniques widely used in semiconductor technology. For example, Josephson junctions are fabricated based on Dolan Bridge combined with dual-angle evaporation / oblique evaporation processes.

[0070] Furthermore, in practice, high-resistivity silicon or sapphire is often used as the substrate, and the Josephson junction is then fabricated onto the substrate. The barrier layer in the junction is formed by oxidizing the superconductor layer. Subsequently, micro / nano fabrication techniques can be used to fabricate various components, quantum circuits, etc.

[0071] It is known that the barrier layer formed by the ultrathin insulator in the middle of the Josephson junction is the key to achieving coherence of the superconducting electrodes on both sides. As mentioned above, the commonly used alumina barrier layer can be formed by in-situ thermal oxidation, which diffuses oxygen to the aluminum surface to form AlO. x And due to the self-limiting nature of this reaction (AlO... x The aluminum layer (which hinders oxygen atoms from diffusing further into the underlying aluminum) blocks oxygen atoms, preventing them from diffusing further to the Al surface, and consequently also hindering the diffusion of AlO₂. x The layer has grown to its maximum thickness.

[0072] Furthermore, considering the difficulty in controlling the oxygen partial pressure during thermal oxidation in the actual fabrication process, controlling the thickness and uniformity of the resulting barrier layer is challenging. Annealing is also typically used to further refine the AlO₂ layer. x The transformation into high-quality alumina may lead to defects such as oxygen vacancies, which could adversely affect the performance of qubits, such as shortening the coherence time.

[0073] Therefore, during the process development, it is necessary to consider quality monitoring or analysis of the fabricated Josephson junction, especially the study of its barrier layer. By analyzing the structure and properties of the oxide layer, the fabrication process of the Josephson junction can be examined in order to improve and optimize the process.

[0074] The inventors of this application used TEM, as mentioned above, to study the structure and properties of the oxide layer in the junction region. Furthermore, the inventors selected a cross-section of the barrier layer and then used TEM to "observe" this cross-section. However, because focused ion beams (FIBs) can cause significant damage to Josephson junctions (JJs), a material is applied to the JJ region as a protective layer before FIB cutting. This protective layer can be, for example, Pt or carbon.

[0075] On the one hand, the opaque nature of the Pt / carbon protective layer makes it difficult to conveniently determine whether the desired position has been cut during the FIB dicing process. On the other hand, the barrier layer in the junction is very thin (typically a few nanometers in size, such as 1 nm to 3 nm; generally, the thickness is less than or equal to the coherence length of Cooper pairs). Therefore, identifying the barrier layer using SEM (scanning electron microscopy) is also relatively more difficult.

[0076] Based on this understanding, the inventors of this application propose a solution that can overcome the problem of difficulty in observing and identifying the barrier layer, and also correspondingly improve the success rate and accuracy of cutting.

[0077] In the example, this solution uses a pre-designed positioning structure, or what is described as a marker. Based on this, the positioning structure can be easily identified during the cutting process to determine the desired cut location. One advantage is that the thickness of the barrier layer cross-section during cutting, for example, is only a few nanometers, making it relatively difficult to distinguish. Furthermore, the presence of a protective layer, such as platinum, also affects identification. Therefore, this solution allows for the configuration of a thicker (e.g., micrometer) positioning structure within the cross-section, positioned away from the protective layer without being obscured, enabling convenient and efficient identification and thus determining the desired cut location—creating a barrier layer cross-section for observation.

[0078] Therefore, the test junction 100, which will be mentioned below, can be used in the fabrication of a Josephson junction comprising two superconducting layers and a weakly connected layer between the two superconducting layers. One application is, for example, the test junction 100 used to determine the slitting stop position during a slitting operation on the Josephson junction. At the slitting stop position, the slidable Josephson junction exposes a cross-section provided by the weakly connected layer, and the fabrication process is evaluated or adjusted based on the analysis of the cross-section. For example, when cross-sectional analysis reveals uneven thickness in the weakly connected layer, adjustments to the fabrication method of the weakly connected layer, such as the temperature of thermal oxidation or the oxygen partial pressure, can be considered.

[0079] In some examples, such as Figure 3 and Figure 4 ( Figure 4 The test junction 100 shown (not illustrated in the diagram) includes a first superconductor layer 101 and an electron barrier layer 105. Figure 3 (Not shown), second superconductor layer 102, cover film layer 103 and positioning film layer 104.

[0080] In terms of manufacturing efficiency, consistency and quality, the first superconductor layer 101 and the second superconductor layer 102 can generally be made of the same material (other examples may be different), such as aluminum, and can also be made using the same equipment.

[0081] Since the oxide layer on the surface of the superconductor layer can have adverse effects on the performance of the superconductor, the electron barrier layer 105 can be limited to the location where the Josephson junction is configured, although this may place higher demands on the fabrication process.

[0082] exist Figure 3 In this configuration, the first superconducting layer 101 and the second superconducting layer are arranged in a crisscross pattern. Therefore, there are overlapping positions between them. The electron barrier layer 105 can then be positioned at these locations. Consequently, a junction surface—a region for the electron barrier layer 105 to be attached—can be pre-defined on the superconducting layer as a positioning point. For example, a rectangular region (e.g., the midpoint between the two ends of the extended trajectory) can be defined as the junction surface on the surface / top surface of the first superconducting layer 101.

[0083] An electron barrier layer 105 is disposed on the junction surface of the first superconducting layer 101. Simultaneously, the second superconducting layer overlaps with the first superconducting layer at corresponding positions on the barrier layer. It is understood that a Josephson junction is formed at this overlap. In other words, the second superconducting layer and the first superconducting layer partially overlap in a certain region. Furthermore, this overlapping region is aligned with the barrier layer (top and bottom), thereby forming a Josephson junction in the overlapping region by the first superconducting layer 101, the electron barrier layer 105, and the first superconducting layer 101.

[0084] The electron barrier layer can be configured only in the overlapping region of the projection of the second superconductor layer with that of the first superconductor layer. Alternatively, in other examples, based on considerations such as fabrication process and efficiency, the electron barrier layer can be configured on a complete surface of the second superconductor layer, such as the top surface, after a portion of the electron barrier layer is removed by an appropriate method such as etching, thus exposing some surfaces not covered by the electron barrier layer.

[0085] To avoid damage to the barrier layer caused by cutting to observe its cross-section, a capping layer 103 is also provided in the example for protection. In this example, the capping layer 103 is aligned with the overlapping region (primarily the location of the electron barrier layer 105). The capping layer 103 covers at least the first superconductor layer 101, the electron barrier layer 105, and the first superconductor layer 101 in the overlapping region. In other examples, the capping layer 103 can be configured to be larger (both length and width extended) or longer or wider. For example, the capping layer 103 in other examples has a larger... Figure 3 The covering membrane layer 103 has a larger area. For example, a longer covering membrane layer 103 indicates a larger area in the middle. Figure 3 The horizontal dimension is increased as shown. For example, a wider cover film layer 103 indicates that... Figure 3 The vertical dimension shown is increased.

[0086] Due to the presence of the capping layer 103, when dicing is performed using FIB, the capping layer 103 can prevent the ion beam from damaging the electron barrier layer 105 at undesirable locations. It is worth noting that the capping layer 103 acts as a structure that protects the junction, more specifically, the electron barrier layer 105, and does not mean that it completely prevents dicing of the junction.

[0087] The capping layer 103 can be made of various suitable materials depending on the cutting method used. For example, in the examples of this application, a focused ion beam is used for cutting (or etching), so the capping layer 103 can be platinum or carbon. This allows the fabrication of the capping layer to be achieved using the focused ion beam equipment, thereby improving process efficiency and consistency. Other materials can also be selected in other examples, such as organic films, other inorganic films, or other metal deposition films.

[0088] In addition, the test junction 100 also includes a positioning film layer 104. This positioning film layer 104 is used to determine the stopping position when cutting the electron barrier layer 105, i.e., the cutting stop position. Therefore, it can be understood that the positioning film layer 104 is positioned based on the position of the electron barrier layer 105 within the Josephson junction. That is, the position and spatial distribution of the positioning film layer 104 within the Josephson junction can be designed and fabricated based on the position and spatial distribution of the electron barrier layer 105 within the Josephson junction.

[0089] Based on this positioning requirement, a positioning plane can be defined for the test junction 100. Furthermore, when the positioning film 104 is positioned relative to the electron barrier layer 105, the positioning plane can simultaneously cut through both the positioning film 104 and the electron barrier layer 105. Thus, by observing the relative positional relationship between the positioning plane and the positioning film 104 and the electron barrier layer 105, it can be clearly determined that the positioning film 104 and the electron barrier layer 105 are distributed along a linear direction.

[0090] For example, in Figure 3 In the middle, the rectangular covering film 103, at the midpoint of its width feature in the vertical direction, shares a common axis of symmetry with the positioning film 104. Figure 3The dashed line in the diagram represents the centerline of the rectangular covering film 103; therefore, L1 = L2. It can also be understood that the positioning plane can be the plane defined by this centerline. In other examples, the axis of symmetry of the positioning film 104 may also deviate from the centerline.

[0091] Alternatively, the superconducting layer may be long and narrow, with both length and width dimensions, such that the length dimension of the superconducting layer is greater than its width dimension. Simultaneously, the superconducting layer has a centerline defined along the direction of the defined length dimension, and the positioning film layers 104 are distributed laterally across this centerline.

[0092] The distribution of the positioning film 104 in some dimensions has been described above. The distribution of the positioning film 104 relative to the superconducting layer will be explained below. In the example, the positioning film 104 can be configured to the first superconducting layer 101, such as... Figure 3 As shown. Alternatively, the positioning film layer 104 can also be configured on the second superconductor layer 102. Even more specifically, the first superconductor layer 101 and the second superconductor layer 102 can each be configured with a positioning film layer 104.

[0093] Furthermore, the positioning film 104 is at least partially located within the superconducting layer. It may be exposed on the surface of the superconducting layer or completely embedded within the superconducting layer. Alternatively, the positioning film 104 may be located within the superconducting layer but may also be partially exposed; for example, the superconducting layer may have open trenches, holes, or pits, and the positioning film 104 may be configured into the structure.

[0094] In short, the positioning film 104 is at least partially disposed within either or both of the first superconductor layer 101 and the second superconductor layer 102. In this application example, the superconductor layer has grooves, and the positioning film 104 is at least partially located within the grooves. Therefore, in some examples, the positioning film 104 may have a portion protruding above the surface of the superconductor layer.

[0095] In particular, when the positioning film 104 is made of the same material, it is expected to simplify the process and improve the quality of the fabricated test junction 100. For example, in the case of cutting / etching using FIB, the grooves for the positioning film 104 can be fabricated by etching using FIB, as well as the cover film 103 and the positioning film 104. Therefore, the grooves, the cover film 103, and the positioning film 104 can be fabricated in the same equipment, thereby avoiding frequent changes in processing equipment and simplifying the process.

[0096] Additionally, the positioning film layer 104 is positioned away from the overlapping area. For example, in Figure 3In this configuration, the positioning film 104 is located at the left end of the first superconducting layer 101, while the overlapping area is located approximately in the middle of the first superconducting layer 101; and the two have a spacing that is appropriately selected as needed (but not particularly limited). That is, the positioning film 104 is not masked by the cover film 103. However, in other examples, if there is a need, the positioning film 104 may be selected to be covered and masked by the cover film 103; this usually means that a larger cover film 103 is required. If there is no specific need or additional benefit, then it is generally not necessary to specially configure the cover film 103 to cover the positioning film 104.

[0097] In the above description, the first superconducting layer 101 and the second superconducting layer 102 of the test junction 100 are configured in a crisscross pattern; for example, they are distributed in a crisscross pattern in the horizontal and vertical directions, i.e., they are distributed at approximately a 90-degree angle. In other examples, the first superconducting layer 101 and the second superconducting layer 102 may also be distributed at other angles. Alternatively, in other examples, the first superconducting layer 101 and the second superconducting layer 102 may also be arranged in the same direction, such as... Figure 5 As shown. And in Figure 5 The example shown is where the positioning film 104 is located in one of the superconducting layers, while in other examples, the positioning film 104 may be configured in two superconducting layers respectively.

[0098] In other examples, the inventors have also proposed a test junction 100 that allows for convenient observation of the barrier layer cross-section of a Josephson junction exposed by cutting using methods such as FIB.

[0099] The test junction 100 includes a Josephson junction and a positioning film layer 104. The Josephson junction includes a first aluminum film, a second aluminum film, and an aluminum oxide film located between the first aluminum film and the second aluminum film.

[0100] The components of the Josephson knot will be described in detail below.

[0101] In the Josephson junction, a first aluminum film extends along a first direction and has positioning surfaces distributed along the first direction, the positioning surfaces having grooves. These positioning surfaces are, for example, the substrate-facing surface of a thin film fabricated by methods such as photolithography, etching, or deposition when the test junction 100 is fabricated on a substrate. Furthermore, the first aluminum film also has grooves formed on the positioning surfaces; these grooves are used to house the positioning film layer 104.

[0102] The positioning film layer 104, exemplarily selected as platinum, can be completely disposed within the groove, with its top located within the groove. In some examples, the top of the positioning film layer 104 is on the same plane as the surface of the first aluminum film, i.e., the positioning film layer 104 is flush with the positioning surface; or a portion (or referred to as the embedded portion) of the positioning film layer 104 is within the groove, while the remainder (or referred to as the protrusion) extends outside the groove. In such examples, it is known that the positioning film layer 104 fills the entire depth of the groove.

[0103] To describe the burial depth of the positioning membrane 104, its region within the groove can be defined to have a preset depth measured along the groove depth direction, such as... Figure 4 D2 in the text describes the preset depth of the positioning film 104 within the groove. In some examples, this preset depth can be at least an order of magnitude greater than the preset thickness of the alumina. For example, the preset depth is ten times the preset thickness. Alternatively, for better identification of the alumina cross-section, the preset depth can be on the order of micrometers, while the preset thickness is on the order of nanometers.

[0104] The alumina film in the Josephson junction (having, for example) Figure 4 The thickness (D1 as described in the text) is formed on a portion of the positioning surface of the first aluminum film, and is not located in the area where the groove is situated. Therefore, it can be understood that the alumina film is far removed from the groove. For ease of description and comparison, the example assumes that the alumina film has a preset thickness. The alumina film can be formed by oxidizing the first aluminum film, or by combining oxidation under heating conditions, i.e., thermal oxidation; furthermore, it can be combined with annealing.

[0105] The second aluminum foil in the Josephson knot extends along a second direction that intersects the first direction. Therefore, in some examples, this type of Josephson knot can be described as a cross knot.

[0106] In the example, the first and second aluminum films are interlaced and overlap each other, so the second aluminum film covers the alumina film in the area where it overlaps with the first aluminum film. Since the fabrication is performed by a method such as evaporation deposition, the two aluminum films can partially contact each other in the overlapping area and are partially separated by alumina. Simultaneously, the overlapping area avoids the groove (and thus the positioning film layer 104), and the overlapping area is located a predetermined distance away from the groove along a first direction. Based on this, the predetermined thickness of the alumina film is determined and defined by measurement along the direction from the first aluminum film to the second aluminum film.

[0107] Combination Figure 3 and Figure 4The test junction 100 is defined with a cutting surface that partially bisects the alumina film along a first direction, and the positioning film layer 104 is positioned to be partially bisected by the cutting surface. Thus, when the test junction 100 is cut, the cross-section can be exposed from the middle position of the alumina film when the cut reaches the desired position.

[0108] To facilitate those skilled in the art in implementing the scheme of this application example, a method for manufacturing test junction 100 is also provided in the example.

[0109] The production method includes:

[0110] A Josephson junction is provided formed on a substrate. The substrate defines a junction region and an off-junction region, and the Josephson junction is selectively configured accordingly. The Josephson junction includes a first electrode, a second electrode, and a barrier layer connected to and located between the first and second electrodes. The first and second electrodes are arranged in an alternating configuration. To define the fabrication order of the first and second electrodes, it can be determined that the first electrode contacts the substrate within an extended trajectory range. Therefore, the barrier layer is formed on a local surface of the first electrode, and the second electrode covers the barrier layer at a corresponding location on that local surface.

[0111] Furthermore, as an explanation of the location-based characteristics, the projection of the barrier layer in the direction directly opposite to the substrate is located in the junction region, while one or both of the first and second electrodes have an outer segment in the outer region of the junction. Thus, corresponding structures can be fabricated in both the junction region and the outer region.

[0112] For example, in some examples, a protective film layer can be optionally configured (while in other examples, a protective film layer can be omitted). The protective film layer is located in the junction region and covers portions of the first and second electrodes within that junction region, but does not cover the outer junction region.

[0113] As mentioned above, in the extrajunctival region, one or both of the first and second electrodes have an extrajunctival segment. Therefore, a positioning element can be fabricated in an optional sequence. This positioning element is positioned within the extrajunctival segment, and it has a height dimension defined by a given depth extending from the surface of the extrajunctival segment into its interior.

[0114] The phrase "optional order" indicates that the positioning element can be fabricated during the fabrication of the Josephson junction (e.g., the first electrode and / or the second electrode), for example, by fabricating the electrode with a groove and then fabricating the positioning element into that groove. Alternatively, the positioning element can be fabricated after the Josephson junction is fabricated and before the protective film layer is fabricated (if needed). Or, the positioning element can be fabricated after the protective film layer is fabricated.

[0115] Based on the test knot 100 that was fabricated, an example of cutting the test knot 100 with a Josephson knot is also proposed.

[0116] The cutting method includes:

[0117] A Josephson junction is provided, wherein the Josephson junction has two cross-distributed electrodes and a barrier layer connected to and located between the two cross-distributed electrodes. An embedded film of a given thickness is disposed on either or both electrodes away from the barrier layer. Typically, to reduce processing steps and potential damage to the Josephson junction, the embedded film is fabricated on one electrode instead of two electrodes.

[0118] Based on the Josephson junction described above, the cutting method also includes different operations depending on the embedded membrane being produced.

[0119] For example, a first operation is performed. This first operation includes: when only one of the two cross-distributed electrodes is configured with an embedded film, gradually etching the Josephson junction along the extension direction of the other of the two cross-distributed electrodes. The etching range includes the region containing the barrier layer and the embedded film, and etching stops when a cross-section is reached, exposing the embedded film.

[0120] For example, a second operation is performed. The second operation includes: when two cross-distributed electrodes are each configured with an embedded film, gradually etching the Josephson junction along the extension direction of either electrode, and the etching range includes the area where the barrier layer and the embedded film are located, and stopping the etching when the cross-section is reached and the embedded film is exposed.

[0121] Furthermore, during the etching process, etching can be performed from one end of the electrode extension path to the other. Alternatively, etching can be performed from both ends of the electrode extension path towards the middle. That is, in the first operation, the etching operation is performed simultaneously from both sides of the barrier layer along the extension direction of the other electrode. Alternatively, in the second operation, the etching operation is performed simultaneously from both sides of the barrier layer along the extension direction of any one electrode.

[0122] For example, Figure 6 The document describes a superconducting quantum interference device (QFID). This interferometer has two Josephson junctions, one of which is protected by a platinum coating. Two arrows indicate gradual etching from the two junctions towards the midpoint; that is, according to… Figure 6 The etching is performed from top to bottom and from bottom to top, with the two etching positions located in the middle of the junction, approximately in the middle of the barrier layer of the Josephson junction along the vertical direction shown in the diagram.

[0123] The embodiments described above with reference to the accompanying drawings are exemplary and are only used to explain this application, and should not be construed as limiting this application.

[0124] To make the objectives, technical solutions, and advantages of the embodiments of this application clearer, one or more embodiments have been described above with reference to the accompanying drawings. Throughout the description, similar reference numerals are used to denote similar components. In the foregoing description, numerous specific details have been set forth for illustrative purposes in order to provide a more thorough understanding of one or more embodiments. However, it will be apparent that one or more embodiments may be practiced in various circumstances without these specific details, and the embodiments may be combined with and referenced to each other without contradiction.

[0125] It should be noted that the terms "first," "second," etc., in the specification, claims, and accompanying drawings of this application are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that such data can be interchanged where appropriate so that the embodiments of this application described herein can be implemented in orders other than those illustrated or described herein. Furthermore, the terms "comprising" and "having," and any variations thereof, are intended to cover non-exclusive inclusion; for example, a process, method, system, product, or apparatus that comprises a series of steps or units is not necessarily limited to those steps or units explicitly listed, but may include other steps or units not explicitly listed or inherent to such processes, methods, products, or apparatus.

[0126] Additionally, it should be understood that when a layer (or film), region, pattern, or structure is referred to as being "on" a substrate, layer (or film), region, and / or pattern, it can be located directly on another layer or substrate, and / or intercalation layers may also be present. Furthermore, it should be understood that when a layer is referred to as being "under" another layer, it can be located directly under that layer, and / or one or more intercalation layers may also be present. Additionally, references to "on" and "under" the layers may be made based on the accompanying drawings.

[0127] The above description, based on the embodiments shown in the drawings, details the structure, features, and effects of this application. The above description is only a preferred embodiment of this application, but this application does not limit the scope of implementation to what is shown in the drawings. Any changes made in accordance with the concept of this application, or modifications to equivalent embodiments, that do not exceed the spirit covered by the specification and drawings, should be within the protection scope of this application.

Claims

1. A test junction, characterized in that, include: The first superconductor layer has a junction-forming surface; An electron barrier layer is formed on the junction surface of the first superconducting layer; The second superconducting layer partially overlaps with the first superconducting layer, and the overlapping region is aligned with the electron barrier layer, thereby forming a Josephson junction in the overlapping region by the first superconducting layer, the electron barrier layer, and the first superconducting layer. A covering film is aligned with the overlapping region to cover at least the first superconductor layer, the electron barrier layer, and the first superconductor layer in the overlapping region; as well as The positioning film layer, based on the positioning of the electron barrier layer, is at least partially disposed within the first superconductor layer and / or the second superconductor layer, and the positioning film layer is located away from the overlapping region; The test junction is defined with a positioning plane, which allows the positioning plane to cut both the positioning film and the electron barrier layer when the positioning film is positioned based on the electron barrier layer. The rectangular covering film, located at the midpoint of its width in the vertical direction, shares a common axis of symmetry with the positioning film. The positioning plane is a plane defined by the axis of symmetry, and the positioning film layer and the electron barrier layer are distributed along a linear direction; The positioning film layers are distributed laterally across the axis of symmetry.

2. The test junction of claim 1, wherein, The first and second superconducting layers are arranged in a crisscross pattern. Alternatively, the superconductor layer has grooves, and the positioning film layer is at least partially located within the grooves; Alternatively, the positioning film layer may not be covered by the covering film layer; Alternatively, the superconducting layer has a length dimension and a width dimension, with the length dimension being greater than the width dimension, resulting in a long and narrow strip shape, and the superconducting layer having a centerline determined along the direction of the defined length dimension.

3. The test result according to claim 1 or 2, characterized in that, The first and second superconductor layers are made of the same material; Alternatively, at least one of the first superconducting layer and the second superconducting layer is an aluminum film; Alternatively, the electronic barrier layer can be aluminum oxide; Alternatively, the positioning film layer is a platinum film; Alternatively, the positioning film layer and the covering film layer can be made of the same material.

4. A test junction, characterized in that, include: A first aluminum film extending along a first direction has positioning surfaces distributed along the first direction, the positioning surfaces having grooves; An aluminum oxide film is formed on a portion of the positioning surface but not in the area where the groove is located, and the aluminum oxide film has a preset thickness. The second aluminum film extends along a second direction intersecting the first direction, and covers an aluminum oxide film in the area overlapping with the first aluminum film. The overlapping area avoids the groove and is located a predetermined distance away from the groove along the first direction. The predetermined thickness is defined by the direction from the first aluminum film to the second aluminum film. A positioning film layer is at least partially embedded in the groove, and the area of ​​the positioning film layer in the groove has a preset depth measured along the groove depth direction; The positioning film layer has an axis of symmetry; The test result is defined with a cross section that half-splits the alumina film along a first direction, and the positioning film layer is positioned to be half-split by the cross section. The cutting plane is defined by the axis of symmetry, and the positioning film and alumina are distributed along a linear direction; The positioning film layers are distributed laterally across the axis of symmetry.

5. The test result according to claim 4, characterized in that, The test junction has one or more of the following characteristics: First characteristic: The positioning film layer is made of platinum; Second feature: The positioning film layer is flush with the positioning surface; Fourth feature: The positioning film layer fills the entire depth of the groove.

6. The test result according to claim 4 or 5, characterized in that, The preset depth is at least one order of magnitude greater than the preset thickness; And / or, the preset depth is greater than the preset thickness, the preset depth is on the order of micrometers, and the preset thickness is on the order of nanometers.

7. A method for fabricating a test junction, characterized in that, The production method includes: A Josephson junction formed on a substrate is provided, including a first electrode, a second electrode, and a barrier layer connected to and located between the first electrode and the second electrode, the first electrode and the second electrode being cross-configured, wherein the first electrode contacts the substrate within an extended trajectory, the substrate defining a junction region and an outside region, the projection of the barrier layer in a direction opposite to the substrate being located in the junction region, and at least the first electrode having an outside segment in the outside region. A protective film layer is configured, which is located in the junction region and covers the portions of the first electrode and the second electrode in the junction region, but does not cover the outer region of the junction. The positioning element is obtained in an optional order and positioned within the outer segment of the nodule. The positioning element has a height dimension defined by a given depth extending from the surface of the outer segment into the interior. The protective film layer has an axis of symmetry; The first electrode is provided with a positioning plane that cuts the positioning element and the barrier layer together, and the positioning plane is a plane defined by the axis of symmetry; The positioning element is positioned based on the barrier layer, and the positioning element and the barrier layer are distributed along a linear direction; The positioning elements are distributed laterally across the axis of symmetry.

8. The application of a test junction as described in any one of claims 1 to 6 in the fabrication of a Josephson junction, wherein the Josephson junction comprises two superconducting layers and a weakly connected layer connecting and located between the two superconducting layers.

9. The application of the test knot according to claim 8 in the fabrication of Josephson knots, characterized in that, The test junction is used to determine the cutting stop position during the cutting operation of the Josephson junction. At the cutting stop position, the Josephson junction is cut to expose a cross section provided by the weak connection layer, and the fabrication process is evaluated or adjusted based on the analysis of the cross section.

10. A method for cutting a test knot with a Josephson knot, characterized in that, The cutting method includes: A Josephson junction is provided having two cross-distributed electrodes and a barrier layer connected to and located between the two cross-distributed electrodes, wherein one or both electrodes are configured with an embedded film of a given thickness at a location away from the barrier layer. The embedded membrane has an axis of symmetry; The Josephson junction defines a positioning plane that cuts the barrier layer and the embedded film together, the positioning plane being a plane defined by the axis of symmetry; The embedded membrane is positioned based on the barrier layer, and the embedded membrane and the barrier layer are distributed along a linear direction; The embedded membranes are distributed laterally across the axis of symmetry; Perform the first or second operation: The first operation includes: when only one electrode is configured to embed the film, gradually etching the Josephson junction along the extension direction of the other electrode, and the etching range includes the barrier layer and the region where the embedding film is located, and stopping the etching when the cross-section is reached and the embedding film is exposed; The second operation includes: when the two electrodes are each configured with an embedded film, gradually etching the Josephson junction along the extension direction of either electrode, and the etching range includes the area where the barrier layer and the embedded film are located, and stopping the etching when the cross-section is reached and the embedded film is exposed.

11. The method for cutting a test knot with a Josephson knot according to claim 10, characterized in that, In the first operation, the etching operation is performed synchronously from both sides of the barrier layer along the extension direction of the other electrode.

12. The method for cutting a test knot with a Josephson knot according to claim 10, characterized in that, In the second operation, the etching operation is performed synchronously from both sides of the barrier layer along the extension direction of any electrode.

Citation Information

Patent Citations

  • Buffer layer to prevent etching by photoresist developer

    CN109844642A

  • Josephson junction and preparation method of superconducting quantum interference device

    CN111244259A